Film bulk acoustic resonator preparation method, film bulk acoustic resonator and filter
By introducing an intermediate metal layer during the fabrication of the thin-film bulk acoustic wave resonator to protect the piezoelectric material layer, and using photolithography and dry etching techniques to form a mass load, the problems of limited process options and poor flexibility in mass load formation are solved, thereby improving the performance of the thin-film bulk acoustic wave resonator and filter.
Patent Information
- Application Number
- CN202310611022.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-06
- Filing Date
- 2023-05-26
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing technology, the mass load formation process of thin-film bulk acoustic resonators has limited options and poor flexibility, resulting in poor filter sensitivity.
By introducing an intermediate metal layer during the fabrication of the thin-film bulk acoustic resonator, the piezoelectric material layer is protected from subsequent processes, thereby forming a mass load under the top electrode. The final mass load layer is formed using photolithography and dry etching techniques.
The increased process options improve the flexibility and accuracy of mass load formation for thin-film bulk acoustic resonators and filters, thereby enhancing filter performance.
Smart Images

Figure CN118944624A_ABST
Abstract
Description
[Technical field]
[0001] Various embodiments of the present invention relate to the technical field of resonators, and in particular, to a method for preparing a thin film bulk acoustic wave resonator, a thin film bulk acoustic wave resonator, and a filter. [Background technology]
[0002] Piezoelectric crystals have been used as frequency control components for radio communication devices for decades because of their ability to generate stable resonant frequency signals during operation. Typically, the resonant frequency of a particular piezoelectric crystal can be tuned by changing the mass loading of the piezoelectric crystal, specifically by increasing or decreasing the mass of the electrode portion of the piezoelectric crystal.
[0003] However, in the related art, a method for preparing a thin film bulk acoustic wave resonator on a substrate having a top electrode deposited on a piezoelectric material layer uses a mass load lift-off process, and it is impossible to form a mass load on and below the top electrode because the lift-off process cannot be performed directly on the piezoelectric material layer made of aluminum nitride due to losses in subsequent processes, resulting in fewer process options, poor mass load formation of the thin film bulk acoustic wave resonator and flexibility in a filter having the thin film bulk acoustic wave resonator, and poor sensitivity in the filter.
[0004] Therefore, it is necessary to provide a method for preparing a thin film bulk acoustic wave resonator to solve the above problems. [Summary of the invention]
[0005] The object of the present invention is to provide a method for preparing a thin film bulk acoustic wave resonator, a thin film bulk acoustic wave resonator, and a filter to solve the problems of fewer process options and poor flexibility in mass load formation of a thin film bulk acoustic wave resonator and a filter having a thin film bulk acoustic wave resonator.
[0006] According to one aspect of the present invention, a method for preparing a thin film bulk acoustic wave resonator is provided. The method comprises: providing a substrate having a top surface; forming a dielectric material layer on the top surface of the substrate; forming a bottom electrode on the surface of the dielectric material layer away from the substrate; forming a piezoelectric material layer on the surface of the bottom electrode away from the substrate; forming an intermediate metal layer on the surface of the piezoelectric material layer away from the substrate; forming a mass load layer on the surface of the intermediate metal layer away from the substrate; and forming a top electrode on the surface of the mass load layer away from the substrate. The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.
[0007] As an improvement, forming the dielectric material layer on the top surface of the substrate includes: forming and patterning a sacrificial layer on the substrate; forming the dielectric material layer on the sacrificial layer, wherein the dielectric material layer can be an aluminum nitride layer, a silicon nitride layer or any suitable dielectric film layer.
[0008] As an improvement, forming the intermediate metal layer on the surface of the piezoelectric material layer away from the substrate includes: performing metal deposition on the surface of the piezoelectric material layer away from the substrate to form the intermediate metal layer.
[0009] As an improvement, after forming the top electrode on the mass loading layer, the method further comprises dry etching the top electrode to form a final mass loading layer.
[0010] As an improvement, forming the mass load layer on the surface of the intermediate metal layer away from the substrate comprises:
[0011] coating a photoresist on the intermediate metal layer;
[0012] performing photolithographic patterning on the photoresist to obtain a pattern on the intermediate metal layer;
[0013] performing metal deposition on the intermediate metal layer; and
[0014] The intermediate metal layer is peeled off to form the mass loading layer.
[0015] As an improvement, forming the top electrode on the mass load layer comprises:
[0016] Depositing metal on the surface of the mass load layer away from the substrate to form the top electrode metal layer;
[0017] applying the mass loading layer;
[0018] patterning at least one parallel resonator;
[0019] The mass load layer and the top electrode metal layer are dry etched to form the top electrode on the at least one parallel resonator.
[0020] As an improvement, the metal deposition includes physical vapor deposition (PVD), chemical vapor deposition (CVD), electroplating and other suitable processes.
[0021] As an improvement, the total thickness includes the thickness of the intermediate metal layer and the thickness of the top electrode, the total thickness is adjusted according to the frequency range of the thin film bulk acoustic wave resonator, and the thickness of the top metal layer is 100 nm to 1000 nm.
[0022] As an improvement, the thickness of the intermediate metal layer is 5 nm to 1000 nm.
[0023] As an improvement, the material of the substrate includes any one of quartz, aluminum nitride, silicon, silicon carbide, sapphire, glass and polymer materials.
[0024] As an improvement, the material of the piezoelectric material layer includes any one of lithium niobate, aluminum nitride, zinc oxide or lead zirconate titanate.
[0025] As an improvement, the material of the intermediate metal layer includes any one of tungsten, platinum, titanium, molybdenum and aluminum, as well as other suitable metals.
[0026] As an improvement, the material of the top electrode includes any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable metals.
[0027] According to another aspect of the present invention, there is provided a thin film bulk acoustic wave resonator, comprising: a substrate having a top surface; a dielectric material layer formed on the top surface of the substrate; a bottom electrode formed on a surface of the dielectric material layer away from the substrate; a piezoelectric material layer formed on the substrate; an intermediate metal layer formed on a surface of the piezoelectric material layer away from the substrate; a mass load layer formed on a surface of the intermediate metal layer away from the substrate; and a top electrode formed on a surface of the mass load layer away from the substrate. The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on a surface of the intermediate metal layer away from the substrate and when the top electrode is formed on a surface of the mass load layer away from the substrate.
[0028] As an improvement, the thickness of the intermediate metal layer is 5 nm to 1000 nm.
[0029] As an improvement, the FBAW resonator further includes a final mass loading layer formed by dry etching the top electrode.
[0030] As an improvement, the total thickness includes the thickness of the intermediate metal layer and the thickness of the top electrode, the total thickness is adjusted according to the frequency range of the thin film bulk acoustic wave resonator, and the thickness of the top metal layer is 100 nm to 1000 nm.
[0031] As an improvement, the material of the substrate includes any one of quartz, aluminum nitride, silicon, silicon carbide, sapphire, glass and polymer materials; the material of the piezoelectric material layer includes any one of lithium niobate, aluminum nitride, zinc oxide or lead zirconate titanate.
[0032] As an improvement, the material of the intermediate metal layer includes any one of tungsten, platinum, titanium, molybdenum and aluminum, as well as other suitable metals; the material of the top electrode includes any one of tungsten, platinum, titanium, molybdenum and aluminum, as well as other suitable metals.
[0033] According to another aspect of the present invention, a filter is provided, comprising: a first film bulk acoustic wave resonator group and a second film bulk acoustic wave resonator group, wherein the first film bulk acoustic wave resonator group is a combination of at least two film bulk acoustic wave resonators formed on the same substrate and connected in series with a predetermined circuit, and the second film bulk acoustic wave resonator group is a combination of at least two film bulk acoustic wave resonators formed on another substrate and connected in parallel with another predetermined circuit. Wherein, each of the at least two film bulk acoustic wave resonators in the first film bulk acoustic wave resonator group and the at least two film bulk acoustic wave resonators in the second film bulk acoustic wave resonator group comprises: a substrate having a top surface; a dielectric material layer formed on the top surface of the substrate; a bottom electrode formed on a surface of the dielectric material layer away from the substrate; a piezoelectric material layer formed on the substrate; an intermediate metal layer formed on a surface of the piezoelectric material layer away from the substrate; a mass load layer formed on a surface of the intermediate metal layer away from the substrate; and a top electrode formed on a surface of the mass load layer away from the substrate. The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.
Brief Description of the Drawings
[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work, among which:
[0035] Figure 1 is a schematic diagram of a cross-sectional structure of a thin film bulk acoustic resonator in the related art;
[0036] Figure 2 yes Figure 1 A schematic diagram of forming mass loading of a thin film bulk acoustic wave resonator in the related art is shown;
[0037] Figure 3 is a flow chart of a method for preparing a thin film bulk acoustic resonator according to some embodiments of the present invention;
[0038] Figure 4is a flow chart of a method for preparing a thin film bulk acoustic resonator according to some embodiments of the present invention;
[0039] Figure 5 is a schematic cross-sectional structure diagram of a thin film bulk acoustic resonator provided according to some embodiments of the present invention;
[0040] Figure 6 is a schematic diagram of the structure of a filter provided according to some embodiments of the present invention;
[0041] Figure 7 is a schematic diagram of a mass loading pattern formed in a filter according to some embodiments of the present invention. [Specific implementation method]
[0042] In order to make the purpose, technical solutions and advantages of the present invention more obvious and easy to understand, the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention and the accompanying drawings, wherein the same or similar reference numerals represent the same or similar elements or elements with the same or similar functions from beginning to end. It should be understood that the embodiments of the present invention described below are only used to explain the present invention, but not to limit the present invention, that is, based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without performing creative work should fall within the scope of protection of the present invention. In addition, the technical features involved in each embodiment of the present invention described below can be combined as long as there is no conflict between them.
[0043] refer to Figure 1 The FBAR 100 in the related art includes a piezoelectric layer 130 , an upper electrode 140 and a lower electrode 120 disposed on the upper and lower surfaces of the piezoelectric layer, respectively, and a seed layer 110 supporting the lower electrode 120 on a substrate 10 .
[0044] The film bulk acoustic resonator 100 uses bulk longitudinal acoustic waves in the piezoelectric layer 130. When an electric field is generated between two electrodes by an applied voltage, the piezoelectric layer 130 converts part of the electrical energy into mechanical energy in the form of acoustic waves. The acoustic waves propagate in the same direction as the electric field and are reflected from the electrode / air interface.
[0045] The resonance frequency, which is one of the resonance characteristics of the thin film bulk acoustic wave resonator 100, varies according to the thickness t1 of the piezoelectric layer 130. In recent small-sized thin film resonators, a new technology is adopted to adjust the resonance frequency using the so-called mass loading effect, which causes the mass to vary according to the thickness t2 of the upper electrode 140 without changing the thickness t1 of the piezoelectric layer 130, which results in a greater variation in the resonance frequency.
[0046] In the film bulk acoustic wave resonator 100 of the related art, the lower electrode 120 is subjected to chemical and mechanical impacts during repeated deposition and etching during the preparation process of the film bulk acoustic wave resonator 100. In order to withstand such chemical and mechanical impacts, the lower electrode 120 should be made of a material with high chemical and mechanical strength, such as molybdenum (Mo) or tungsten (W), rather than a light metal such as aluminum. However, molybdenum and tungsten have greater vibration transmission losses than aluminum due to their high damping factors and are not easy to process. These materials increase the preparation cost and complicate the preparation process, while reducing the overall efficiency of the film bulk acoustic wave resonator 100.
[0047] like Figure 2 As shown, in a conventional FBAW resonator, in the case of the above structure, a mass load can only be formed on the top electrode by processes such as applying a pattern mask and etching the top electrode. Since processes such as etching and stripping affect or even destroy the piezoelectric layer, a mass load cannot be formed under the top electrode or on the piezoelectric layer, which results in fewer process options, poor flexibility in mass load formation of a FBAW resonator and a filter having a FBAW resonator, and poor accuracy of the filter.
[0048] refer to Figure 3 According to some embodiments of the present invention, the method for preparing a thin film bulk acoustic wave resonator includes the following steps 301 to 307.
[0049] In step 301 , a substrate having a top surface is provided.
[0050] In some embodiments, the material of the substrate includes any one of silicon, silicon carbide, sapphire, and glass.
[0051] In step 302, a dielectric material layer is formed on a top surface of a substrate.
[0052] In some embodiments, forming a dielectric material layer on a surface of the substrate remote from the substrate includes forming and patterning a sacrificial layer on the substrate, and forming the dielectric material layer on the sacrificial layer. The sacrificial layer is made of a material that is easier to etch than thermal oxides used in prior art methods.
[0053] A dielectric material layer is formed on a substrate by metal deposition to support the entire FBAR on the substrate. The dielectric material layer vibrates together with the vibration of the piezoelectric material layer. The dielectric material layer can be made of silicon nitride (Si3N4), silicon dioxide (SiO2) or other insulating materials. Preferably, the thickness of the dielectric material layer should be adjusted within a predetermined thickness range according to the limitations in the preparation process.
[0054] In this case, the resonant frequency of the FBAW resonator can be precisely adjusted without causing any damage to the bottom electrode. During the deposition and etching of the piezoelectric material layer and the top electrode, the chemical and mechanical impact transmitted to the bottom electrode can be reduced, enabling free selection of the material used for the bottom electrode.
[0055] In step 303 , a bottom electrode is formed on a surface of the dielectric material layer away from the substrate.
[0056] In some embodiments, the bottom electrode is made of a metal material having a Young's modulus greater than that of the dielectric material layer, thereby improving the overall rigidity of the dielectric material layer, thereby preventing deformation of the dielectric material layer, and improving the stability and reliability of the dielectric material layer.
[0057] In step 304, a piezoelectric material layer is formed on a surface of the bottom electrode facing away from the substrate.
[0058] In some embodiments, the material of the piezoelectric material layer includes lithium niobate, aluminum nitride, zinc oxide, lead zirconate titanate, or any other suitable material.
[0059] In step 305 , an intermediate metal layer is formed on a surface of the piezoelectric material layer away from the substrate.
[0060] In some embodiments, forming an intermediate metal layer on a surface of the piezoelectric material layer away from the substrate includes performing metal deposition on the surface of the piezoelectric material layer away from the substrate to form an intermediate metal film. The intermediate metal layer is configured to protect the piezoelectric material layer from being affected in subsequent steps, such as forming a mass load layer on the surface of the intermediate metal layer away from the substrate, and forming a top electrode on the mass load layer.
[0061] By forming an intermediate metal layer between the piezoelectric material layer and the mass load layer, a mass load can be formed under the top electrode. In addition, the intermediate metal layer is configured to protect the piezoelectric material layer from subsequent processes such as stripping and dry etching. That is, the processing options for forming the mass load are increased, and the mass load can be easily formed under the top electrode by stripping or dry etching, which increases the process options and increases the flexibility of mass load formation of the thin film bulk acoustic wave resonator and the filter having the thin film bulk acoustic wave resonator, thereby increasing the accuracy of the filter.
[0062] Preferably, the material of the intermediate metal layer includes any one of tungsten, platinum, titanium, molybdenum and aluminum, and other suitable materials.
[0063] In step 306 , a mass loading layer is formed on a surface of the intermediate metal layer remote from the substrate.
[0064] In some embodiments, forming a mass loading layer on a surface of the intermediate metal layer away from the substrate includes coating a photoresist on the intermediate metal, photolithographically patterning the photoresist to obtain a pattern on the intermediate metal layer, performing metal deposition on the intermediate metal layer, and stripping the metal layer to form the mass loading layer.
[0065] In some embodiments, for the mass loading layer, it is preferred to select a material that causes a small change in the resonant frequency of the FBAW resonator according to a change in the thickness of the FBAW resonator.
[0066] In step 307 , a top electrode is formed on a surface of the mass loading layer facing away from the substrate.
[0067] In some embodiments, forming a top electrode on the mass load layer includes performing metal deposition on a surface of the mass load away from the substrate to form a top electrode metal layer, applying the mass load layer, coating a photoresist on at least one parallel resonator, and dry etching the mass load layer and the top electrode metal layer to form a top electrode on at least one parallel resonator.
[0068] Preferably, the material of the top electrode includes any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable materials.
[0069] refer to Figure 4 In some embodiments, after forming the top electrode on the mass loading layer, the method further includes step 308 .
[0070] In step 308, the top electrode is dry etched to form a final mass loading layer.
[0071] In some embodiments, metal deposition includes physical vapor deposition (PVD), chemical vapor deposition (CVD), electroplating, and other suitable processes.
[0072] In some embodiments, the total thickness includes the thickness of the intermediate metal layer and the thickness of the top electrode, the total thickness is adjusted according to the frequency range of the thin film bulk acoustic wave resonator, and the thickness of the top metal layer is 100nm to 1000nm. Preferably, the thickness of the intermediate metal layer is 5nm to 1000nm.
[0073] refer to Figure 5According to some embodiments of the present invention, a thin film bulk acoustic wave resonator 500 provided includes a substrate 510 having a top surface; a dielectric material layer 520 formed on the top surface of the substrate 510; a bottom electrode 530 formed on a surface of the dielectric material layer 520 away from the substrate 510; a piezoelectric material layer 540 formed on the bottom electrode 530; an intermediate metal layer 550 formed on a surface of the piezoelectric material layer 540 away from the substrate 510; a mass load layer 560 formed on a surface of the intermediate metal layer 550 away from the substrate 510; and a top electrode 570 formed on a surface of the mass load layer 560 away from the substrate 510.
[0074] In some embodiments, the FBAW resonator 500 further includes a final mass load layer 580 formed by dry etching the top electrode 570. The intermediate metal layer 550 is configured to protect the piezoelectric material layer 540 from being affected when the mass load layer 560 is formed on the surface of the intermediate metal layer 550 away from the substrate 510 and the top electrode 570 is formed on the surface of the mass load layer 560 away from the substrate 510.
[0075] according to Figure 3 and Figure 4 The steps shown in FIG. 5 are used to provide a thin film bulk acoustic wave resonator 500. Therefore, for the relevant contents of the thin film bulk acoustic wave resonator 500, reference can be made to the above-mentioned Figure 3 and Figure 4 Description.
[0076] like Figure 6As shown, according to some embodiments of the present invention, a filter 600 is provided, comprising a first film bulk acoustic wave resonator group and a second film bulk acoustic wave resonator group, wherein the first film bulk acoustic wave resonator group is a combination of at least two film bulk acoustic wave resonators formed on the same substrate and connected in series with a predetermined circuit (series film bulk acoustic wave resonators), and the second film bulk acoustic wave resonator group is a combination of at least two film bulk acoustic wave resonators formed on another substrate and connected in parallel with another predetermined circuit (parallel film bulk acoustic wave resonators). Each of the at least two film bulk acoustic wave resonators in the first film bulk acoustic wave resonator group and the at least two film bulk acoustic wave resonators in the second film bulk acoustic wave resonator group comprises a substrate having a top surface; a dielectric material layer formed on the top surface of the substrate; a bottom electrode formed on a surface of the dielectric material layer away from the substrate; a piezoelectric material layer formed on the substrate; an intermediate metal layer formed on a surface of the piezoelectric material layer away from the substrate; a mass load layer formed on a surface of the intermediate metal layer away from the substrate; and a top electrode formed on a surface of the mass load layer away from the substrate. The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.
[0077] The thickness and / or pattern of each mass-loading layer in at least two FBARs of the first FBAR group and at least two FBARs of the second FBAR group can be the same or different.
[0078] In some embodiments, the number of the FBARs in the first FBAR group and the number of the FBARs in the second FBAR group are both exemplarily three. Figure 6 As shown. Specifically, the first film bulk acoustic resonator group includes three film bulk acoustic resonators, for example, film bulk acoustic resonator A, film bulk acoustic resonator B, and film bulk acoustic resonator C, and the second film bulk acoustic resonator group includes three film bulk acoustic resonators, for example, film bulk acoustic resonator D, film bulk acoustic resonator E, and film bulk acoustic resonator F. However, the number of film bulk acoustic resonators in the first film bulk acoustic resonator group and the number of film bulk acoustic resonators in the second film bulk acoustic resonator group are not limited to the above-mentioned examples, as long as the number is equal to or greater than two, so that a group of resonators can be formed.
[0079] refer to Figure 7 , describes an example of mass load formation in a filter. In this example, mass loads are formed on the six FBARs described above in different ways.
[0080] Specifically, the mass load layer is formed by peeling between the intermediate metal layer and the top electrode in the film bulk acoustic resonator A, the film bulk acoustic resonator B, and the film bulk acoustic resonator C. The only difference between the film bulk acoustic resonator A and the film bulk acoustic resonator B is that the thickness of the mass load layer gradually increases from the film bulk acoustic resonator A to the film bulk acoustic resonator C. The mass load layer is formed by peeling between the intermediate metal layer and the top electrode in the film bulk acoustic resonator D, the film bulk acoustic resonator E, and the film bulk acoustic resonator F, and the final mass load layer is further formed on the top electrode by dry etching. The thickness of the mass load layer gradually increases from the film bulk acoustic resonator D to the film bulk acoustic resonator F, and the thickness of the final mass load layer also gradually increases from the film bulk acoustic resonator D to the film bulk acoustic resonator F.
[0081] In some embodiments, the thickness and / or pattern of the mass load layer of each of at least two film bulk acoustic resonators in the first film bulk acoustic resonator group and at least two film bulk acoustic resonators in the second film bulk acoustic resonator group are the same, and the thickness and / or pattern of the mass load layer of each of at least two film bulk acoustic resonators in the second film bulk acoustic resonator group are different. That is, the thickness and / or pattern of the mass load layer within the filter or between filter designs can be flexibly controlled. Therefore, the processing options for forming the mass load are increased, and the mass load can be easily formed under the top electrode by stripping or dry etching, which increases the process options, increases the flexibility of mass load formation of the film bulk acoustic resonator and the filter having the film bulk acoustic resonator, thereby increasing the accuracy of the filter.
[0082] It should be noted that the embodiments herein are described in a progressive manner. Each embodiment focuses on its differences from other embodiments, and reference can be made to the same or similar parts between these embodiments. For the product embodiments, since they are similar to those method embodiments, the description is simple, and reference can be made to the description of the method embodiments for the relevant content.
[0083] It should also be noted that, in the context of the present invention, relational terms such as first and second are used only to distinguish one entity or step from another entity or step, and do not necessarily require or imply any such actual relationship or order between these entities or steps. In addition, the terms "comprises", "includes" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only these elements, but also other elements not explicitly listed, or elements inherent to the process, method, article or device. Without further limitation, an element preceding the statement "comprises..." does not exclude the presence of other identical elements in the process, method, article or device that includes the element.
[0084] The description of the above disclosed embodiments may enable those skilled in the art to implement or use the present application. Various modifications to the embodiments will be apparent to those skilled in the art, and the general principles herein may be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application is not limited to the embodiments described herein, but should conform to the broadest scope consistent with the principles and novel features disclosed herein.
Claims
1. A method for preparing a thin film bulk acoustic wave resonator, comprising: providing a substrate having a top surface; forming a dielectric material layer on the top surface of the substrate; forming a bottom electrode on a surface of the dielectric material layer away from the substrate; forming a piezoelectric material layer on a surface of the bottom electrode away from the substrate; forming an intermediate metal layer on a surface of the piezoelectric material layer away from the substrate; forming a mass loading layer on a surface of the intermediate metal layer away from the substrate; and forming a top electrode on a surface of the mass loading layer remote from the substrate; The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.
2. The preparation method according to claim 1, wherein forming the dielectric material layer on the top surface of the substrate comprises: forming and patterning a sacrificial layer on the substrate; The dielectric material layer is formed on the sacrificial layer, wherein the dielectric material layer may be an aluminum nitride layer, a silicon nitride layer or any suitable dielectric film layer.
3. The preparation method according to claim 1, wherein forming the intermediate metal layer on the surface of the piezoelectric material layer away from the substrate comprises: Metal deposition is performed on the surface of the piezoelectric material layer away from the substrate to form the intermediate metal layer. 4 . The preparation method according to claim 1 , wherein after forming the top electrode on the mass load layer, the method further comprises dry etching the top electrode to form a final mass load layer.
5. The preparation method according to claim 1, wherein forming the mass load layer on the surface of the intermediate metal layer away from the substrate comprises: coating a photoresist on the intermediate metal layer; performing photolithographic patterning on the photoresist to obtain a pattern on the intermediate metal layer; Depositing metal on the intermediate metal layer; and The intermediate metal layer is peeled off to form the mass loading layer.
6. The preparation method according to claim 1, wherein forming the top electrode on the mass load layer comprises: Depositing metal on the surface of the mass load layer away from the substrate to form the top electrode metal layer; applying the mass loading layer; patterning at least one parallel resonator; The mass load layer and the top electrode metal layer are dry etched to form the top electrode on the at least one parallel resonator.
7. The preparation method according to claim 6, wherein: The metal deposition includes physical vapor deposition (PVD), chemical vapor deposition (CVD), electroplating and other suitable processes.
8. The preparation method according to claim 6, wherein: The total thickness includes the thickness of the intermediate metal layer and the thickness of the top electrode, the total thickness is adjusted according to the frequency range of the thin film bulk acoustic wave resonator, and the thickness of the top metal layer is 100 nm to 1000 nm.
9. The preparation method according to claim 8, wherein: The thickness of the intermediate metal layer is 5nm to 1000nm.
10. The preparation method according to claim 1, wherein: The material of the substrate includes any one of quartz, aluminum nitride, silicon, silicon carbide, sapphire, glass and polymer materials.
11. The preparation method according to claim 1, wherein: The material of the piezoelectric material layer includes any one of lithium niobate, aluminum nitride, zinc oxide or lead zirconate titanate and other suitable metals.
12. The preparation method according to claim 1, wherein: The material of the intermediate metal layer includes any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable metals.
13. The preparation method according to claim 1, wherein The material of the top electrode includes any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable metals.
14. A thin film bulk acoustic wave resonator, comprising: a substrate having a top surface; a layer of dielectric material formed on the top surface of the substrate; a bottom electrode formed on a surface of the dielectric material layer away from the substrate; a piezoelectric material layer formed on the substrate; an intermediate metal layer formed on a surface of the piezoelectric material layer away from the substrate; a mass loading layer formed on a surface of the intermediate metal layer remote from the substrate; and a top electrode formed on a surface of the mass loading layer remote from the substrate; The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.
15. The thin film bulk acoustic wave resonator according to claim 14, wherein: The thickness of the intermediate metal layer is 5nm to 1000nm.
16. The FBAW resonator of claim 14, further comprising a final mass loading layer formed by dry etching the top electrode.
17. The thin film bulk acoustic wave resonator according to claim 14, wherein: The total thickness includes the thickness of the intermediate metal layer and the thickness of the top electrode, the total thickness is adjusted according to the frequency range of the thin film bulk acoustic wave resonator, and the thickness of the top metal layer is 100 nm to 1000 nm.
18. The thin film bulk acoustic wave resonator according to claim 14, wherein the material of the substrate comprises any one of quartz, aluminum nitride, silicon, silicon carbide, sapphire, glass and polymer materials; the material of the piezoelectric material layer comprises any one of lithium niobate, aluminum nitride, zinc oxide or lead zirconate titanate and other suitable metals.
19. The thin film bulk acoustic wave resonator according to claim 18, wherein the material of the intermediate metal layer comprises any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable metals; the material of the top electrode comprises any one of tungsten, platinum, titanium, molybdenum, aluminum and other suitable metals.
20. A filter comprising a first film bulk acoustic wave resonator group and a second film bulk acoustic wave resonator group, wherein: The first FBAW resonator group is a combination of at least two FBAW resonators formed on the same substrate and connected in series with a predetermined circuit, and the second FBAW resonator group is a combination of at least two FBAW resonators formed on another substrate and connected in parallel with another predetermined circuit; Wherein, each of the at least two FBARs in the first FBAR group and the at least two FBARs in the second FBAR group comprises: a substrate having a top surface; a layer of dielectric material formed on the top surface of the substrate; a bottom electrode formed on a surface of the dielectric material layer away from the substrate; a piezoelectric material layer formed on the substrate; an intermediate metal layer formed on a surface of the piezoelectric material layer away from the substrate; a mass loading layer formed on a surface of the intermediate metal layer remote from the substrate; and a top electrode formed on a surface of the mass loading layer remote from the substrate; The intermediate metal layer is configured to protect the piezoelectric material layer from being affected when the mass load layer is formed on the surface of the intermediate metal layer away from the substrate and the top electrode is formed on the surface of the mass load layer away from the substrate.