Method and device for monitoring, regulating and controlling wet oxidation aperture of VCSEL (Vertical Cavity Surface Emitting Laser) chip
By responding to the oxidation pore size optimization request at the user's end, the oxidation pore shape parameters and uniform coefficients of the VCSEL chip are collected and predicted, and appropriate wet oxidation control parameters are selected, which solves the problem of insufficient control accuracy of wet oxidation pore size of the VCSEL chip, and achieves a higher level of oxidation pore size accuracy and beam quality.
Patent Information
- Application Number
- CN202411484599.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-10-23
AI Technical Summary
In the prior art, there is insufficient accuracy control for the control of the wet oxidation pore size of VCSEL chips, which affects the stability and consistency of the product.
By responding to the oxidation pore size optimization request at the user's end, the oxidation pore shape parameters and uniform coefficients are collected, the prediction parameters are generated using the beam quality predictor, the wet oxidation control parameters that meet the expected beam parameters are selected, and real-time monitoring and adjustment are carried out to achieve accurate quantification control.
The accuracy control level of VCSEL chip oxidation pore size is improved, ensuring that the beam quality meets expectations, and improving the stability and consistency of the product.
Smart Images

Figure CN119009679A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of vertical cavity surface emitting lasers, and in particular to a method and device for monitoring and controlling the wet oxidation aperture of a VCSEL chip. Background Art
[0002] With the rapid development of optoelectronics technology, vertical-cavity surface-emitting lasers (VCSELs), as high-performance laser light sources, have shown broad application prospects in a variety of fields, including optical communications, data storage, lidar, and 3D sensing. The performance of VCSEL chips, particularly their laser emission quality, is directly affected by the precise control of their internal structure, with precise control of the oxide aperture being particularly critical. The oxide aperture not only determines the laser beam's emission path but also directly influences key parameters such as the beam's diameter, divergence angle, profile, and power distribution, thereby impacting the VCSEL's overall performance and application effectiveness. Traditionally, the production of VCSEL chips relies primarily on empirical methods for the formation of the oxide aperture and its wet oxidation control. This approach typically relies on engineers' accumulated experience and repeated adjustments to process parameters, lacking scientific quantitative standards and systematic control methods. This results in insufficient precision control, impacting product stability and consistency.
[0003] In the current related technologies, there is a technical problem of insufficient precision control in the wet oxidation aperture control of VCSEL chips. Summary of the Invention
[0004] The present application provides a method and apparatus for monitoring and controlling the wet oxidation aperture of a VCSEL chip. The method responds to a user's request for optimization of the oxidation aperture of the VCSEL chip, clarifies the desired parameters of the light beam, collects the shape parameters and uniformity coefficient of the oxidation aperture according to the application scenario type of the VCSEL chip, and maps them through a beam quality predictor to generate predicted beam parameters. Based on the prediction results, wet oxidation control parameters that meet the desired beam parameters are selected as benchmark parameters for monitoring and control, and real-time monitoring and adjustment are performed. Through precise quantitative control and real-time monitoring, the method achieves the technical effect of improving the precision control level of the oxidation aperture of the VCSEL chip.
[0005] This application provides a method for monitoring and controlling the aperture of a VCSEL chip wet oxidation process, comprising: In response to a VCSEL chip oxidation aperture optimization request submitted by a user end, an expected beam diameter, an expected beam divergence angle, an expected beam profile, and an expected power in the barrel are obtained; according to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request, oxidation aperture shape parameters and an oxidation aperture uniformity coefficient are collected; according to the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient, mapping is performed through a beam quality predictor to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile, and a predicted power in the barrel; according to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel, wet oxidation control parameters that meet the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel are selected and set as monitoring and control benchmark parameters; and wet oxidation monitoring is performed according to the monitoring and control benchmark parameters.
[0006] In a possible implementation, according to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request, the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient are collected, and the following processing is performed: According to the application scenario type of the VCSEL chip, a one-to-one corresponding historical cross-sectional dataset of oxidation pore shape parameters and a historical cross-sectional dataset of oxidation pore uniformity coefficient are collected; the historical cross-sectional dataset of oxidation pore shape parameters is preprocessed by removing outliers to obtain the distribution interval of oxidation pore shape parameters; the historical cross-sectional dataset of oxidation pore uniformity coefficient is preprocessed by removing outliers to obtain the distribution interval of oxidation pore uniformity coefficient; random assignment is performed according to the distribution interval of oxidation pore shape parameters and the distribution interval of oxidation pore uniformity coefficient to obtain the oxidation pore shape parameters and the oxidation pore uniformity coefficient.
[0007] In a possible implementation, according to the application scenario type of the VCSEL chip, a one-to-one corresponding historical cross-sectional dataset of oxidation hole shape parameters and a historical cross-sectional dataset of oxidation hole uniformity coefficient are collected, and the following processing is performed: Obtaining oxidation pore shape parameter attributes and oxidation pore uniformity coefficient attributes, wherein the oxidation pore shape parameter attributes include oxidation pore major diameter, oxidation pore minor diameter, and oxidation pore depth, and the oxidation pore uniformity coefficient attributes include oxidation pore distribution spacing and oxidation pore distribution quantity; and collecting historical cross-sectional data of the VCSEL chip application scenario type based on the oxidation pore major diameter, the oxidation pore minor diameter, the oxidation pore depth, the oxidation pore distribution spacing, and the oxidation pore distribution quantity to obtain the oxidation pore shape parameter historical cross-sectional data set and the oxidation pore uniformity coefficient historical cross-sectional data set.
[0008] In a possible implementation, mapping is performed by a beam quality predictor based on the oxidation hole shape parameter and the oxidation hole uniformity coefficient to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile, and a predicted power in the barrel, and the following processing is performed: According to the oxidation hole long diameter parameter and the oxidation hole short diameter parameter of the oxidation hole shape parameter, mapping is performed through the beam diameter prediction channel of the beam quality predictor to obtain the predicted beam diameter; according to the oxidation hole shape parameter, mapping is performed through the beam divergence angle prediction channel of the beam quality predictor to obtain the predicted beam divergence angle; according to the oxidation hole uniformity coefficient, mapping is performed through the beam profile prediction channel of the beam quality predictor to obtain the predicted beam profile; according to the oxidation hole uniformity coefficient, mapping is performed through the barrel power prediction channel of the beam quality predictor to obtain the predicted barrel power.
[0009] In a possible implementation, based on the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel, a wet oxidation control parameter that satisfies the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel is selected and set as a monitoring and control benchmark parameter, and the following processing is performed: The predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the expected power in the barrel are verified according to the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel to obtain a beam quality verification result; when the beam quality verification result is passed, the wet oxidation control parameters are optimized according to the oxidation hole shape parameters and the oxidation hole uniformity coefficient to obtain target wet oxidation control parameters; the target wet oxidation control parameters are set as the monitoring and control benchmark parameters; when the beam quality verification result is failed, the oxidation hole shape parameters and the oxidation hole uniformity coefficient are updated according to the application scenario type of the VCSEL chip.
[0010] In a possible implementation, the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel are verified according to the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel to obtain a beam quality verification result, and the following processing is performed: When the diameter deviation between the expected diameter of the light beam and the predicted diameter of the light beam is less than or equal to the diameter deviation threshold, and the divergence angle deviation between the expected divergence angle of the light beam and the predicted divergence angle of the light beam is less than or equal to the divergence angle deviation threshold, and the contour shape deviation between the expected profile of the light beam and the predicted profile of the light beam is less than or equal to the contour shape deviation threshold, and the bucket power deviation between the expected power in the barrel and the predicted power in the barrel is less than or equal to the bucket power deviation threshold, a first-level verification pass signal is generated; a first multiplication factor of the expected diameter of the light beam and the expected divergence angle of the light beam is calculated, and a second multiplication factor of the predicted diameter of the light beam and the predicted divergence angle of the light beam is calculated to obtain A third product factor of a diffraction-limited Gaussian beam diameter and a diffraction-limited Gaussian beam divergence angle of the same wavelength is obtained; a ratio of the first product factor to the third product factor is calculated and set as an expected beam quality factor; a ratio of the second product factor to the third product factor is calculated and set as a predicted beam quality factor; when a beam quality factor deviation between the expected beam quality factor and the predicted beam quality factor is less than or equal to a beam quality factor deviation threshold, a secondary verification pass signal is generated; when both the primary verification pass signal and the secondary verification pass signal are passed, the beam quality verification result is passed; otherwise, the beam quality verification result is failed.
[0011] In a possible implementation, when the beam quality verification result is passed, wet oxidation control parameter optimization is performed based on the oxidation hole shape parameter and the oxidation hole uniformity coefficient to obtain target wet oxidation control parameters, and the following processing is performed: Obtain a wet oxidation control parameter distribution constraint interval, wherein the wet oxidation control parameter distribution constraint interval includes an oxidation temperature distribution constraint interval, an oxidation time distribution constraint interval, a nitrogen flow rate distribution constraint interval, a nitrogen concentration distribution constraint interval, a water vapor flow rate distribution constraint interval, and a water vapor concentration distribution constraint interval; based on the VCSEL chip model and the wet oxidation equipment model, collect a wet oxidation control historical cross-sectional data set that meets the oxidation pore shape parameters and the oxidation pore uniformity coefficient through an online network; perform normalized dimensionality reduction distribution on the wet oxidation control historical cross-sectional data set based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval to obtain wet oxidation control particle distribution coordinates; perform outlier coordinate removal on the wet oxidation control particle distribution coordinates to obtain wet oxidation control particle concentrated coordinates; extract the wet oxidation control parameter distribution interval of the wet oxidation control particle concentrated coordinates and set it as the target wet oxidation control parameter.
[0012] In a possible implementation, based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval, the wet oxidation control historical cross-section data set is normalized and dimensionally reduced to obtain wet oxidation control particle distribution coordinates, and the following processing is performed: Obtain oxidation temperature history section data of the first wet oxidation control history section data of the wet oxidation control history section data set; calculate the first deviation modulus of the oxidation temperature history section data and the minimum value of the oxidation temperature distribution constraint interval; calculate the second deviation modulus of the maximum value and the minimum value of the oxidation temperature distribution constraint interval; calculate the ratio of the first deviation modulus to the second deviation modulus, and set it as the oxidation temperature normalized coordinate; with the same processing process, obtain the oxidation time normalized coordinate, nitrogen flow normalized coordinate, nitrogen concentration normalized coordinate, water vapor flow normalized coordinate, and water vapor concentration normalized coordinate; obtain the first particle distribution coordinate according to the oxidation temperature normalized coordinate, the oxidation time normalized coordinate, the nitrogen flow normalized coordinate, the nitrogen concentration normalized coordinate, the water vapor flow normalized coordinate, and the water vapor concentration normalized coordinate, and add it to the wet oxidation control particle distribution coordinate.
[0013] The present application also provides a device for monitoring and controlling the aperture of a VCSEL chip wet oxidation process, comprising: The oxidation aperture optimization request response module is used to respond to the VCSEL chip oxidation aperture optimization request submitted by the user end, and obtain the expected beam diameter, expected beam divergence angle, expected beam profile and expected power in the barrel; the oxidation aperture parameter acquisition module is used to collect the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient according to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request; the beam quality prediction module is used to predict the beam quality based on the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient. The predictor performs mapping to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile and a predicted power in the barrel; a monitoring and control benchmark parameter acquisition module is used to select wet oxidation control parameters that meet the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel according to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel, and set them as monitoring and control benchmark parameters; a wet oxidation monitoring module is used to perform wet oxidation monitoring according to the monitoring and control benchmark parameters.
[0014] The method and device for monitoring and controlling the wet oxidation aperture of a VCSEL chip proposed in this application first respond to a VCSEL chip oxidation aperture optimization request submitted by a user end, obtain the desired beam diameter, desired beam divergence angle, desired beam profile, and desired power in the barrel, then collect the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient according to the VCSEL chip application scenario type in the VCSEL chip oxidation aperture optimization request, then map the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient through a beam quality predictor to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile, and a predicted power in the barrel, then select wet oxidation control parameters that meet the desired beam diameter, the desired beam divergence angle, the desired beam profile, and the expected power in the barrel based on the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel, and set them as monitoring and control benchmark parameters. Finally, wet oxidation monitoring is performed based on the monitoring and control benchmark parameters, thereby achieving the technical effect of improving the precision control level of the oxidation aperture of the VCSEL chip. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings of the embodiments of the present invention are briefly introduced below. Flowcharts are used in this application to illustrate the operations performed by the apparatus according to the embodiments of the present application. It should be understood that the preceding or following operations are not necessarily performed in precise order. Instead, various steps may be processed in reverse order or simultaneously as needed. Furthermore, other operations may be added to these processes, or one or more operations may be removed from these processes.
[0016] Figure 1 A schematic flow chart of a method for monitoring and controlling the aperture of a VCSEL chip wet oxidation process provided in an embodiment of the present application.
[0017] Figure 2 Schematic diagram of the structure of the device for monitoring and controlling the wet oxidation aperture of a VCSEL chip provided in an embodiment of the present application.
[0018] Explanation of the accompanying symbols: oxidation aperture optimization request response module 10, oxidation aperture parameter acquisition module 20, beam quality prediction module 30, monitoring and control benchmark parameter acquisition module 40, wet oxidation monitoring module 50. DETAILED DESCRIPTION
[0019] The above description is only an overview of the technical solution of the present application. In order to more clearly understand the technical means of the present application, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are listed below.
[0020] In order to make the purpose, technical solutions and advantages of this application clearer, the application will be further described in detail below with reference to the accompanying drawings. The described embodiments should not be regarded as limiting this application. All other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0021] In the following description, reference is made to “some embodiments”, which describes a subset of all possible embodiments, but it will be understood that “some embodiments” may be the same subset or different subsets of all possible embodiments and may be combined with each other without conflict, and the terms “first\second” involved are merely used to distinguish similar objects and do not represent a specific ordering of the objects. The terms “including” and “having” and any variations are intended to cover non-exclusive inclusions. For example, a process, method, device, product or server that includes a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or modules that are not clearly listed or inherent to these processes, methods, products or devices. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application belongs. The terms used herein are for the purpose of describing the embodiments of this application only.
[0022] The present application provides a method for monitoring and controlling the aperture of a VCSEL chip wet oxidation process, such as Figure 1 As shown, the method includes: Step S100: In response to a VCSEL chip oxidation aperture optimization request submitted by a user, the desired beam diameter, desired beam divergence angle, desired beam profile, and desired power in the barrel are obtained. Specifically, a VCSEL chip oxidation aperture optimization request is received from the user, and the desired beam diameter, desired beam divergence angle, desired beam profile, and desired power in the barrel parameters contained in the request are parsed. The oxidation aperture is a specific aperture formed on the chip during the VCSEL chip manufacturing process through techniques such as wet oxidation, and is used to control the output characteristics of the light beam. The desired beam diameter is the diameter of the beam that the user desires the VCSEL chip to output; the desired beam divergence angle is the angle of the beam that the user desires the VCSEL chip to diverge; the desired beam profile is the shape of the beam profile that the user desires the VCSEL chip to output; and the desired power in the barrel is the power that the user desires the VCSEL chip to output within a specific area (e.g., the barrel area of the optical receiver).
[0023] Step S200 collects oxidation pore shape parameters and oxidation pore uniformity coefficients based on the VCSEL chip application scenario type requested for the VCSEL chip oxidation pore diameter optimization. Specifically, the data collection scope is determined based on the VCSEL chip application scenario type (e.g., communications, sensing, projection, etc.). Historical data for oxidation pore shape parameters and oxidation pore uniformity coefficients corresponding to the current application scenario type is collected from a historical database. Oxidation pore shape parameters describe the geometric characteristics of oxidation pores, such as major diameter, minor diameter, and depth; oxidation pore uniformity coefficients describe the uniformity of oxidation pore distribution, such as the spacing and number of distributed pores.
[0024] In one possible implementation, based on the VCSEL chip application scenario type requested for the VCSEL chip oxidation aperture optimization, oxidation pore shape parameters and oxidation pore uniformity coefficients are collected. Step S200 further includes step S210: based on the VCSEL chip application scenario type, a corresponding historical cross-sectional dataset of oxidation pore shape parameters and a historical cross-sectional dataset of oxidation pore uniformity coefficients are collected. Specifically, a specific application scenario of the VCSEL chip is identified, such as high-speed data transmission, 3D sensing, or LiDAR. For a specific application scenario, historical data of oxidation pore shape parameters (such as diameter and shape factor) and oxidation pore uniformity coefficient (a measure of oxidation pore size consistency) related to the application scenario is retrieved from a historical database. This data is obtained from previous design iterations, testing, or production records. Step S220: Outlier removal preprocessing is performed on the historical cross-sectional dataset of oxidation pore shape parameters to obtain a distribution range for the oxidation pore shape parameters. Specifically, each data point in the historical cross-sectional dataset of oxidation pore shape parameters is examined to identify and remove abnormal values (outliers) that significantly deviate from the majority of data points. These values may be caused by measurement errors, equipment failures, or other atypical factors. Statistical analysis is performed on the cleaned dataset to calculate statistical quantities such as the mean and standard deviation to determine the data distribution. Based on the results of the statistical analysis, a reasonable distribution interval is determined, encompassing the majority (e.g., 95% or 99%) of the data points, which serves as a reference range for subsequent random assignment. Step S230 preprocesses the oxidation pore uniformity coefficient historical cross-sectional dataset by removing outliers to obtain an oxidation pore uniformity coefficient distribution interval. Specifically, the process is similar to step S220, but is applied to the oxidation pore uniformity coefficient historical cross-sectional dataset. By removing outliers and performing statistical analysis, a reasonable oxidation pore uniformity coefficient distribution interval is determined. Step S240 randomly assigns values based on the oxidation pore shape parameter distribution interval and the oxidation pore uniformity coefficient distribution interval to obtain the oxidation pore shape parameter and the oxidation pore uniformity coefficient. Specifically, within the distribution intervals determined in steps S220 and S230, random sampling is used to generate values for the oxidation pore shape parameter and the oxidation pore uniformity coefficient. The randomly generated parameter values are assigned to the current VCSEL chip optimization process to explore possible optimal performance in a given application scenario. This implementation method collects and analyzes historical cross-sectional data sets to determine which oxidation pore shape parameters and uniformity coefficients are more ideal in different application scenarios. By randomly assigning values within these distribution ranges, it ensures that the new optimization is close to the optimal solution from the beginning, thereby achieving the technical effect of accelerating the optimization process and improving optimization efficiency.
[0025] In one possible implementation, based on the application scenario type of the VCSEL chip, a one-to-one corresponding historical cross-sectional dataset of oxidation pore shape parameters and a historical cross-sectional dataset of oxidation pore uniformity coefficient are collected. Step S210 further includes step S211, where oxidation pore shape parameter attributes and oxidation pore uniformity coefficient attributes are obtained. The oxidation pore shape parameter attributes include the oxidation pore major diameter, the oxidation pore minor diameter, and the oxidation pore depth, and the oxidation pore uniformity coefficient attributes include the oxidation pore distribution spacing and the number of oxidation pores distributed. Specifically, the oxidation pore shape parameter attributes and oxidation pore uniformity coefficient attributes to be collected are determined. The oxidation pore shape parameter attributes include the oxidation pore major diameter (the maximum diameter of the oxidation pore in a direction perpendicular to the light emission direction), the minor diameter (the diameter in a direction perpendicular to the major diameter if the shape is not completely circular), and the depth (the distance from the chip surface to the bottom of the oxidation pore). These parameters directly affect the light emission pattern and efficiency. The oxide hole uniformity coefficient attributes include the distribution spacing of the oxide holes on the chip (the distance between adjacent oxide holes, which affects light uniformity and resolution) and the distribution number of oxide holes (the total number of oxide holes in a specific area, which affects light intensity and coverage). These parameters determine light uniformity and overall performance. These attributes are recorded in a data structure for subsequent data collection and processing. Step S212: Historical cross-sectional data for the VCSEL chip application scenario type is collected based on the oxide hole major diameter, the oxide hole minor diameter, the oxide hole depth, the oxide hole distribution spacing, and the oxide hole distribution number, to obtain a historical cross-sectional dataset for the oxide hole shape parameters and a historical cross-sectional dataset for the oxide hole uniformity coefficient. Specifically, a historical database storing VCSEL chip design, manufacturing, and testing data is accessed. Based on the application scenario and the attributes defined in step S211, historical data for the oxide hole shape parameters and oxide hole uniformity coefficient related to the current application scenario is filtered from the database. The filtered data is categorized and organized according to the application scenario and attributes to form a historical cross-sectional dataset for the oxide hole shape parameters and a historical cross-sectional dataset for the oxide hole uniformity coefficient. This implementation method achieves the technical effect of improving the targetedness and effectiveness of VCSEL chip optimization by accurately defining and collecting historical data on the oxide pore shape parameters and uniformity coefficient properties that are closely related to the application scenarios of VCSEL chips.
[0026] Step S300: Mapping the oxidation hole shape parameters and the oxidation hole uniformity coefficient using a beam quality predictor generates a predicted beam diameter, predicted beam divergence angle, predicted beam profile, and predicted in-barrel power. Specifically, the beam quality predictor is a machine learning-based prediction tool used to predict beam quality based on oxidation hole parameters. The oxidation hole shape parameters and the oxidation hole uniformity coefficient are input into the beam quality predictor, which uses the mapping relationship to predict the beam diameter, divergence angle, profile, and in-barrel power based on the input parameters.
[0027] In one possible implementation, mapping is performed through a beam quality predictor according to the oxidation hole shape parameter and the oxidation hole uniformity coefficient to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile and a predicted power in the barrel. Step S300 further includes step S310, mapping through a beam diameter prediction channel of the beam quality predictor according to the oxidation hole long diameter parameter and the oxidation hole short diameter parameter of the oxidation hole shape parameter to obtain the predicted beam diameter; step S320, mapping through a beam divergence angle prediction channel of the beam quality predictor according to the oxidation hole shape parameter to obtain the predicted beam divergence angle; step S330, mapping through a beam profile prediction channel of the beam quality predictor according to the oxidation hole uniformity coefficient to obtain the predicted beam profile; step S340, mapping through a barrel power prediction channel of the beam quality predictor according to the oxidation hole uniformity coefficient to obtain the predicted power in the barrel.
[0028] Specifically, the beam quality predictor is a machine learning model that integrates multiple prediction channels, used to predict beam quality based on oxidation aperture parameters. The beam diameter prediction channel inputs the major and minor diameters of the oxidation aperture and outputs the predicted beam diameter; the beam divergence prediction channel inputs the oxidation aperture shape parameters and outputs the predicted beam divergence angle; the beam profile prediction channel inputs the oxidation aperture uniformity coefficient and outputs the predicted beam profile; and the in-bucket power prediction channel inputs the oxidation aperture uniformity coefficient and receiving area parameters and outputs the predicted in-bucket power. The following uses the beam diameter prediction channel as an example to illustrate the model training process: A large amount of data on oxidation aperture parameters and corresponding beam diameters after wet oxidation of VCSEL chips is collected. The data is cleaned to remove noise and outliers, and the collected data is normalized. A neural network model is selected based on data characteristics, trained using preprocessed data, and prediction performance is optimized by adjusting model parameters and training strategies. A test set is used to evaluate the model's prediction accuracy and generalization ability to ensure that the model meets practical requirements. Finally, the trained model is deployed in the beam quality predictor for real-time beam quality prediction. This implementation utilizes specialized prediction channels to process different beam quality parameters. Each channel is optimized for its specific task. Through training with a large amount of historical data, it can capture complex optical phenomena and physical laws, thereby more accurately predicting the quality characteristics of the beam, achieving the technical effect of improving the accuracy and efficiency of the prediction.
[0029] Step S400, based on the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel, select the wet oxidation control parameters that meet the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel, and set them as monitoring and control benchmark parameters. Specifically, the predicted beam diameter, divergence angle, profile and power in the barrel are compared with the user's expected values. The oxidation pore shape parameters and oxidation pore uniformity coefficient corresponding to the predicted beam quality parameters that can meet the user's expected values are selected, and the wet oxidation control parameters corresponding to the oxidation pore shape parameters and oxidation pore uniformity coefficient are obtained, and set them as monitoring and control benchmark parameters. Among them, the wet oxidation control parameters are parameters used to control the shape and uniformity of the oxidation pores during the wet oxidation process, such as oxidation temperature, oxidation time, gas flow rate and concentration, etc.
[0030] In one possible implementation, based on the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel, wet oxidation control parameters that meet the desired beam diameter, the desired beam divergence angle, the desired beam profile, and the desired power in the barrel are selected and set as monitoring and control benchmark parameters. Step S400 further includes step S410, in which the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel are verified based on the desired beam diameter, the desired beam divergence angle, the desired beam profile, and the desired power in the barrel to obtain a beam quality verification result. Specifically, the expected value and the predicted value of the beam are compared one by one, and the difference or deviation between them is calculated using mathematical methods. If all predicted values are within a certain tolerance range of the expected values, the verification result is passed; otherwise, it is failed. In step S420, if the beam quality verification result is passed, the wet oxidation control parameters are optimized based on the oxidation hole shape parameter and the oxidation hole uniformity coefficient to obtain the target wet oxidation control parameters. Specifically, based on the verified oxidation hole shape parameters and uniformity coefficients, as well as the wet oxidation control parameter range, an optimization algorithm is used to search within the control parameter range to find a set of control parameters that brings the beam quality (predicted value) closest to the expected value, namely, the target wet oxidation control parameters. In step S430, the target wet oxidation control parameters are set as the monitoring and control benchmark parameters. Specifically, the target wet oxidation control parameters obtained through optimization are set as the monitoring and control benchmark parameters during the wet oxidation process. In step S440, if the beam quality verification result fails, the oxidation hole shape parameters and the oxidation hole uniformity coefficient are updated based on the VCSEL chip application scenario. Specifically, if the beam quality verification result fails, the oxidation hole shape parameters and the oxidation hole uniformity coefficient are readjusted based on the specific application scenario of the VCSEL chip. Beam quality prediction and verification are then performed again based on the updated oxidation hole shape parameters and oxidation hole uniformity coefficient until the beam quality verification result passes. This implementation ensures that the wet oxidation process more accurately meets the expected beam quality requirements through beam quality verification, thereby achieving the technical effect of improving product performance and quality.
[0031] In one possible implementation, the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel are verified based on the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel to obtain a beam quality verification result. Step S410 further includes step S411, when the diameter deviation between the expected beam diameter and the predicted beam diameter is less than or equal to a diameter deviation threshold, and the divergence angle deviation between the expected beam divergence angle and the predicted beam divergence angle is less than or equal to a divergence angle deviation threshold, and the contour shape deviation between the expected beam profile and the predicted beam profile is less than or equal to a contour shape deviation threshold, and the bucket power deviation between the expected power in the barrel and the predicted power in the barrel is less than or equal to a bucket power deviation threshold, a first-level verification pass signal is generated. Specifically, the diameter deviation, divergence angle deviation, contour shape deviation, and bucket power deviation respectively represent the difference between the actual predicted value and the expected value. If all deviations meet the threshold conditions, a first-level verification pass signal is generated.
[0032] Step S412, calculate the first product factor of the expected beam diameter and the expected beam divergence angle, calculate the second product factor of the predicted beam diameter and the predicted beam divergence angle, and obtain the third product factor of the diffraction-limited Gaussian beam diameter and the diffraction-limited Gaussian beam divergence angle of the same wavelength; Step S413, calculate the ratio of the first product factor to the third product factor, set it as the expected beam quality factor, calculate the ratio of the second product factor to the third product factor, and set it as the predicted beam quality factor; Step S414, when the beam quality factor deviation between the expected beam quality factor and the predicted beam quality factor is less than or equal to the beam quality factor deviation threshold, generate a secondary verification pass signal.
[0033] Specifically, the first product factor (the product of the expected beam diameter and the expected beam divergence angle) and the second product factor (the product of the predicted beam diameter and the predicted beam divergence angle) are calculated. Simultaneously, the diameter and divergence angle of a diffraction-limited Gaussian beam of the same wavelength are obtained, and their product is calculated as the third product factor. The ratio of the first product factor to the third product factor (the expected beam quality factor) and the ratio of the second product factor to the third product factor (the predicted beam quality factor) are calculated, respectively. These two ratios are parameters used to quantify beam quality, reflecting the degree of closeness of the beam quality to the quality of a diffraction-limited Gaussian beam. The closer the value is to 1, the better the beam quality and the closer it is to an ideal diffraction-limited Gaussian beam (an ideal beam model with optimal beam quality). The beam quality factor deviation between the expected beam quality factor and the predicted beam quality factor is calculated, and a determination is made as to whether it is less than or equal to a beam quality factor deviation threshold. If so, a secondary verification pass signal is generated.
[0034] Step S415: When both the first-level verification pass signal and the second-level verification pass signal pass, the beam quality verification result is passed; Step S416: Otherwise, the beam quality verification result is failed. Specifically, if both the first-level verification pass signal and the second-level verification pass signal are generated, the beam quality verification result is passed. If any first-level verification fails, the beam quality verification result is failed. This implementation method comprehensively evaluates the quality of the beam through conventional beam parameter comparison and beam quality factor comparison, ensuring that the predicted beam performance meets actual needs, and achieving the technical effect of improving the accuracy of beam quality verification.
[0035] In one possible implementation, when the beam quality verification result passes, wet oxidation control parameters are optimized based on the oxidation pore shape parameter and the oxidation pore uniformity coefficient to obtain target wet oxidation control parameters. Step S420 further includes step S421, whereby target wet oxidation control parameter distribution constraints are obtained. The target wet oxidation control parameter distribution constraints include oxidation temperature distribution constraints, oxidation duration distribution constraints, nitrogen flow rate distribution constraints, nitrogen concentration distribution constraints, water vapor flow rate distribution constraints, and water vapor concentration distribution constraints. Specifically, based on process knowledge, equipment specifications, and experimental data, reasonable distribution constraint constraints are set for each wet oxidation control parameter (oxidation temperature, oxidation duration, nitrogen flow rate, nitrogen concentration, water vapor flow rate, and water vapor concentration). These constraints define the range of parameter adjustment, ensuring that operations are performed within a safe and effective range. The constraint interval for each parameter is recorded as a basis for subsequent data processing and optimization. Step S422: Based on the VCSEL chip model and the wet oxidation equipment model, a historical cross-sectional wet oxidation control dataset that satisfies the oxidation pore shape parameters and the oxidation pore uniformity coefficient is collected online. Specifically, the range of historical data to be collected is determined based on the VCSEL chip model and the wet oxidation equipment model. Through a network connection to a database or data warehouse, historical wet oxidation control data that meets the requirements is automatically or manually downloaded. This data includes control parameters and results from multiple experiments or production processes. The collected data is organized to form a historical cross-sectional wet oxidation control dataset, with each cross-sectional wet oxidation control dataset representing the control parameters and results from a single experiment or production process. Step S423: Based on the oxidation temperature distribution constraint interval, the oxidation duration distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval, the wet oxidation control particle distribution coordinates are obtained by normalizing the wet oxidation control particle distribution coordinates. Specifically, each control parameter in the historical cross-sectional wet oxidation control dataset is normalized according to its distribution constraint interval, i.e., the actual value is converted into a relative value between 0 and 1. Perform distribution analysis on the normalized data to determine the distribution of each control parameter, providing a basis for subsequent optimization. Step S424, delete the outlier coordinates of the wet oxidation control particle distribution coordinates to obtain the wet oxidation control particle centralized coordinates. Specifically, perform density distribution analysis on each control parameter point to calculate its density or frequency in the data set. Based on the density analysis results, identify those points with low density and a long distance from other points as outliers. Delete the identified outliers from the data set to obtain more centralized and representative wet oxidation control particle centralized coordinates.Step S425, extract the wet oxidation control parameter distribution interval of the concentrated coordinates of the wet oxidation control particles, and set it as the target wet oxidation control parameter. Specifically, the concentrated coordinates of the wet oxidation control particles are analyzed to determine the distribution of each control parameter. According to the analysis results, reasonable distribution intervals of each control parameter are extracted. These intervals can cover most of the concentrated coordinate points and meet the requirements of the oxidation pore shape parameters and the oxidation pore uniformity coefficient. The extracted wet oxidation control parameter distribution interval is set as the target wet oxidation control parameter to guide subsequent experiments or production processes. This implementation method scientifically and systematically determines the target wet oxidation control parameters by setting reasonable distribution constraint intervals for each control parameter, collecting historical data, performing normalized dimensionality reduction distribution, deleting outlier coordinates, etc., and achieves the technical effect of improving the accuracy and reliability of the wet oxidation control parameter optimization results.
[0036] In one possible implementation, the wet oxidation control historical cross-section data set is normalized and dimensionally reduced based on the oxidation temperature distribution constraint interval, the oxidation duration distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval to obtain wet oxidation control particle distribution coordinates. Step S423 further includes step S4231: obtaining oxidation temperature historical cross-section data of a first wet oxidation control historical cross-section data set in the wet oxidation control historical cross-section data set. Specifically, the first wet oxidation control historical cross-section data set (any record in the data set) is extracted from the wet oxidation control historical cross-section data set. Oxidation temperature-related data is separated from the historical cross-section data to form oxidation temperature historical cross-section data. Step S4232: Calculate a first deviation modulus between the oxidation temperature historical cross-section data and the minimum value of the oxidation temperature distribution constraint interval. Specifically, the minimum value (i.e., the lower temperature limit) of the oxidation temperature distribution constraint interval is determined. The absolute value of the difference between the temperature value in the oxidation temperature historical cross-section data set and the lower temperature limit is calculated to obtain the first deviation modulus. Step S4233: Calculate the second deviation modulus of the maximum and minimum values within the oxidation temperature distribution constraint interval. Specifically, determine the maximum value (i.e., the upper temperature limit) and minimum value (i.e., the lower temperature limit) within the oxidation temperature distribution constraint interval. Calculate the absolute value of the difference between the upper temperature limit and the lower temperature limit to obtain the second deviation modulus. Step S4234: Calculate the ratio of the first deviation modulus to the second deviation modulus and set it as the normalized oxidation temperature coordinate. Specifically, divide the first deviation modulus by the second deviation modulus to obtain a ratio, and map this ratio to the interval [0, 1] to obtain the normalized oxidation temperature coordinate.
[0037] In step S4235, the normalized coordinates of the oxidation time, the normalized coordinates of the nitrogen flow rate, the normalized coordinates of the nitrogen concentration, the normalized coordinates of the water vapor flow rate, and the normalized coordinates of the water vapor concentration are obtained using the same processing process. Specifically, the process of steps S4231 to S4234 is repeated, but the oxidation time, nitrogen flow rate, nitrogen concentration, water vapor flow rate, and water vapor concentration control parameters are processed separately to calculate the corresponding normalized coordinates for each control parameter. In step S4236, the first particle distribution coordinates are obtained based on the normalized coordinates of the oxidation temperature, the normalized coordinates of the oxidation time, the normalized coordinates of the nitrogen flow rate, the normalized coordinates of the nitrogen concentration, the normalized coordinates of the water vapor flow rate, and the normalized coordinates of the water vapor concentration, and are added to the wet oxidation control particle distribution coordinates. Specifically, the normalized coordinates of all control parameters are combined to form a multidimensional vector. This multidimensional vector is used as the first particle distribution coordinate and added to the wet oxidation control particle distribution coordinate set. This implementation method converts the wet oxidation control historical cross-section data set into a form that is easier to process and analyze through normalization and dimensionality reduction processing, reducing computational complexity and achieving the technical effect of improving optimization efficiency.
[0038] Step S500, wet oxidation monitoring is performed according to the monitoring and control benchmark parameters. Specifically, a wet oxidation process is started on the VCSEL chip, and chemical etching is performed according to the monitoring and control benchmark parameters to form the required oxidation pore size. During the wet oxidation process, various sensors and monitoring equipment are used to monitor the shape parameters (such as long diameter, short diameter), uniformity coefficient and other key parameters (such as temperature, concentration, etc.) of the oxidation pores in real time. If it is found that the actual oxidation process deviates from the monitoring and control benchmark parameters, or the shape and uniformity of the oxidation pores do not meet the requirements, the control parameters of the wet oxidation are adjusted in time to restore or optimize the oxidation process. When the wet oxidation process reaches the predetermined target and the shape and uniformity of the oxidation pores meet the requirements, the wet oxidation process is stopped. The embodiments of the present application respond to a user-end request for optimization of the oxidation aperture of a VCSEL chip, clarify the desired parameters of the light beam, collect the shape parameters and uniformity coefficient of the oxidation aperture according to the application scenario type of the VCSEL chip, and map them through a beam quality predictor to generate predicted beam parameters. Based on the prediction results, wet oxidation control parameters that meet the desired beam parameters are selected as benchmark parameters for monitoring and regulation, and real-time monitoring and adjustment are performed. Through precise quantitative control and real-time monitoring, the technical effect of improving the precision control level of the oxidation aperture of the VCSEL chip is achieved.
[0039] In the above, refer to Figure 1 The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to an embodiment of the present invention is described in detail. Figure 2A device for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to an embodiment of the present invention is described.
[0040] The apparatus for monitoring and controlling the aperture of a VCSEL chip wet oxidation process according to an embodiment of the present invention is designed to address the technical problem of insufficient precision control in existing VCSEL chip wet oxidation aperture control methods, thereby improving the precision control level of the VCSEL chip oxidation aperture. The apparatus for monitoring and controlling the aperture of a VCSEL chip wet oxidation process includes an oxidation aperture optimization request response module 10, an oxidation aperture parameter acquisition module 20, a beam quality prediction module 30, a monitoring and control reference parameter acquisition module 40, and a wet oxidation monitoring module 50.
[0041] The oxidation aperture optimization request response module 10 is used to respond to the VCSEL chip oxidation aperture optimization request submitted by the user end, and obtain the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel; the oxidation aperture parameter acquisition module 20 is used to collect the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient according to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request; the beam quality prediction module 30 is used to map the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient through a beam quality predictor to generate a predicted beam diameter, a predicted beam divergence angle, a predicted beam profile and a predicted power in the barrel; the monitoring and control reference parameter acquisition module 40 is used to select the wet oxidation control parameters that meet the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel according to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel, and set them as monitoring and control reference parameters; the wet oxidation monitoring module 50 is used to perform wet oxidation monitoring according to the monitoring and control reference parameters.
[0042] The specific configuration of the oxidation pore parameter acquisition module 20 will be described in detail below. As described above, based on the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request, the oxidation pore shape parameter and the oxidation pore uniformity coefficient are collected. The oxidation pore parameter acquisition module 20 may further include: a historical cross-sectional data set acquisition unit for collecting a one-to-one corresponding historical cross-sectional data set of the oxidation pore shape parameter and the oxidation pore uniformity coefficient according to the VCSEL chip application scenario type; an oxidation pore shape parameter distribution interval acquisition unit for performing outlier removal preprocessing on the oxidation pore shape parameter historical cross-sectional data set to obtain the oxidation pore shape parameter distribution interval; an oxidation pore uniformity coefficient distribution interval acquisition unit for performing outlier removal preprocessing on the oxidation pore uniformity coefficient historical cross-sectional data set to obtain the oxidation pore uniformity coefficient distribution interval; and a random assignment unit for performing random assignment based on the oxidation pore shape parameter distribution interval and the oxidation pore uniformity coefficient distribution interval to obtain the oxidation pore shape parameter and the oxidation pore uniformity coefficient.
[0043] Among them, according to the type of application scenario of the VCSEL chip, a one-to-one corresponding historical cross-sectional data set of oxidation pore shape parameters and a historical cross-sectional data set of oxidation pore uniformity coefficient are collected, and the historical cross-sectional data set collection unit may further include: an attribute acquisition subunit for obtaining oxidation pore shape parameter attributes and oxidation pore uniformity coefficient attributes, wherein the oxidation pore shape parameter attributes include oxidation pore long diameter, oxidation pore short diameter, oxidation pore depth, and the oxidation pore uniformity coefficient attributes include oxidation pore distribution spacing and oxidation pore distribution number; a historical cross-sectional data collection subunit is used to collect historical cross-sectional data of the VCSEL chip application scenario type according to the oxidation pore long diameter, the oxidation pore short diameter, the oxidation pore depth, the oxidation pore distribution spacing, and the oxidation pore distribution number, to obtain the oxidation pore shape parameter historical cross-sectional data set and the oxidation pore uniformity coefficient historical cross-sectional data set.
[0044] The specific configuration of the beam quality prediction module 30 will be described in detail below. As described above, according to the oxidation hole shape parameter and the oxidation hole uniformity coefficient, mapping is performed through the beam quality predictor to generate a beam predicted diameter, a beam predicted divergence angle, a beam predicted profile, and a barrel predicted power. The beam quality prediction module 30 may further include: a beam predicted diameter acquisition unit for mapping the oxidation hole long diameter parameter and the oxidation hole short diameter parameter of the oxidation hole shape parameter through the beam diameter prediction channel of the beam quality predictor to obtain the beam predicted diameter; a beam predicted divergence angle acquisition unit for mapping the oxidation hole shape parameter through the beam divergence angle prediction channel of the beam quality predictor to obtain the beam predicted divergence angle; a beam predicted profile acquisition unit for mapping the oxidation hole uniformity coefficient through the beam profile prediction channel of the beam quality predictor to obtain the beam predicted profile; and a barrel predicted power acquisition unit for mapping the oxidation hole uniformity coefficient through the barrel power prediction channel of the beam quality predictor to obtain the barrel predicted power.
[0045] The specific configuration of the monitoring and control reference parameter acquisition module 40 will be described in detail below. As described above, according to the beam predicted diameter, the beam predicted divergence angle, the beam predicted profile and the predicted power in the barrel, the wet oxidation control parameters that meet the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel are selected and set as monitoring and control reference parameters. The monitoring and control reference parameter acquisition module 40 may further include: a beam quality verification unit for verifying the predicted beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel according to the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel. The predicted power in the bucket is verified to obtain a beam quality verification result; the wet oxidation control parameter optimization unit is used to optimize the wet oxidation control parameters according to the oxidation hole shape parameter and the oxidation hole uniformity coefficient when the beam quality verification result is passed, and obtain the target wet oxidation control parameters; the monitoring and control benchmark parameter determination unit is used to set the target wet oxidation control parameters to the monitoring and control benchmark parameters; the oxidation hole parameter updating unit is used to update the oxidation hole shape parameter and the oxidation hole uniformity coefficient according to the application scenario type of the VCSEL chip when the beam quality verification result is failed.
[0046] Wherein, the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel are verified according to the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel to obtain a beam quality verification result, and the beam quality verification unit may further include: a first-level verification pass signal generating subunit for generating a first-level verification pass signal when the diameter deviation between the expected beam diameter and the predicted beam diameter is less than or equal to a diameter deviation threshold, and the divergence angle deviation between the expected beam divergence angle and the predicted beam divergence angle is less than or equal to a divergence angle deviation threshold, and the contour shape deviation between the expected beam profile and the predicted beam profile is less than or equal to a contour shape deviation threshold, and the bucket power deviation between the expected power in the barrel and the predicted power in the barrel is less than or equal to a bucket power deviation threshold; a multiplication factor obtaining subunit for calculating the beam period The first product factor of the expected beam diameter and the expected divergence angle of the beam is calculated, and the second product factor of the predicted beam diameter and the predicted divergence angle of the beam is calculated to obtain a third product factor of the diffraction-limited Gaussian beam diameter and the diffraction-limited Gaussian beam divergence angle of the same wavelength; the beam quality factor calculation subunit is used to calculate the ratio of the first product factor to the third product factor, set it as the expected beam quality factor, calculate the ratio of the second product factor to the third factor, and set it as the predicted beam quality factor; the secondary verification pass signal generation subunit is used to generate a secondary verification pass signal when the beam quality factor deviation between the expected beam quality factor and the predicted beam quality factor is less than or equal to the beam quality factor deviation threshold; the verification subunit is used to, when both the first verification pass signal and the second verification pass signal are passed, the beam quality verification result is passed, otherwise, the beam quality verification result is failed.
[0047] Wherein, when the beam quality verification result is passed, the wet oxidation control parameter optimization is performed according to the oxidation hole shape parameter and the oxidation hole uniformity coefficient to obtain the target wet oxidation control parameter, and the wet oxidation control parameter optimization unit may further include: a wet oxidation control parameter distribution constraint interval acquisition subunit for obtaining the wet oxidation control parameter distribution constraint interval, wherein the wet oxidation control parameter distribution constraint interval includes the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow distribution constraint interval, and the water vapor concentration distribution constraint interval; a wet oxidation control history cross-section data set acquisition subunit for collecting, based on the VCSEL chip model and the wet oxidation equipment model, the data that meets the oxidation hole shape parameter and the oxidation hole uniformity coefficient. The wet oxidation control historical cross-sectional data set is a wet oxidation control particle distribution coordinate acquisition subunit, which is used to perform normalized dimensionality reduction distribution on the wet oxidation control historical cross-sectional data set based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval to obtain the wet oxidation control particle distribution coordinates; the wet oxidation control particle concentrated coordinate acquisition subunit is used to delete outlier coordinates on the wet oxidation control particle distribution coordinates to obtain the wet oxidation control particle concentrated coordinates; the wet oxidation control parameter distribution interval extraction subunit is used to extract the wet oxidation control parameter distribution interval of the wet oxidation control particle concentrated coordinates, and set it as the target wet oxidation control parameter.
[0048] Among them, based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow distribution constraint interval, and the water vapor concentration distribution constraint interval, the wet oxidation control history section data set is normalized and dimensionally reduced to obtain the wet oxidation control particle distribution coordinates. The wet oxidation control particle distribution coordinate acquisition subunit may further include: an oxidation temperature history section data acquisition microunit for obtaining oxidation temperature history section data of the first wet oxidation control history section data of the wet oxidation control history section data set; a first deviation modulus calculation microunit for calculating the first deviation modulus of the oxidation temperature history section data and the minimum value of the oxidation temperature distribution constraint interval; a second deviation modulus calculation microunit for calculating Calculate the second deviation modulus of the maximum and minimum values of the oxidation temperature distribution constraint interval; the oxidation temperature normalized coordinate setting microunit is used to calculate the ratio of the first deviation modulus to the second deviation modulus, and set it as the oxidation temperature normalized coordinate; the other parameter normalized coordinate acquisition microunit is used to obtain the oxidation time normalized coordinate, nitrogen flow normalized coordinate, nitrogen concentration normalized coordinate, water vapor flow normalized coordinate, and water vapor concentration normalized coordinate with the same processing process; the first particle distribution coordinate acquisition microunit is used to obtain the first particle distribution coordinate according to the oxidation temperature normalized coordinate, the oxidation time normalized coordinate, the nitrogen flow normalized coordinate, the nitrogen concentration normalized coordinate, the water vapor flow normalized coordinate, and the water vapor concentration normalized coordinate, and add it to the wet oxidation control particle distribution coordinate.
[0049] The device for monitoring and controlling the aperture of a VCSEL chip wet oxidation process provided in an embodiment of the present invention can execute the method for monitoring and controlling the aperture of a VCSEL chip wet oxidation process provided in any embodiment of the present invention, and has the corresponding functional modules and beneficial effects of the execution method.
[0050] Although the present application makes various references to certain modules in the apparatus according to the embodiments of the present application, any number of different modules may be used and run on the user terminal and / or server, and the various units and modules included are only divided according to functional logic, but are not limited to the above division, as long as the corresponding functions can be achieved; in addition, the specific names of the functional units are only for the convenience of distinguishing each other and are not used to limit the scope of protection of the present invention.
[0051] The above specific embodiments do not constitute a limitation to the scope of protection of this application. It should be understood by those skilled in the art that various modifications, combinations and substitutions can be made according to design requirements and other factors. Any modifications, equivalent replacements and improvements made within the spirit and principles of this application should be included in the scope of protection of this application. In some cases, the actions or steps recorded in this application can be performed in an order different from that in the embodiments and can still achieve the desired results. In addition, the processes depicted in the accompanying drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.
Claims
1. A method for monitoring and controlling the aperture of a VCSEL chip wet oxidation, characterized in that: include: In response to a VCSEL chip oxidation aperture optimization request submitted by a user, obtain a desired beam diameter, a desired beam divergence angle, a desired beam profile, and a desired power in the barrel; According to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request, collecting oxidation aperture shape parameters and oxidation aperture uniformity coefficients; According to the oxidation hole shape parameter and the oxidation hole uniformity coefficient, mapping is performed through a beam quality predictor to generate a beam prediction diameter, a beam prediction divergence angle, a beam prediction profile and a barrel prediction power; According to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel, a wet oxidation control parameter satisfying the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel is selected and set as a monitoring and control benchmark parameter; Wet oxidation monitoring is performed according to the monitoring and regulating benchmark parameters.
2. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 1, characterized in that: According to the VCSEL chip application scenario type of the VCSEL chip oxidation aperture optimization request, the oxidation aperture shape parameters and the oxidation aperture uniformity coefficient are collected, including: According to the application scenario type of the VCSEL chip, a one-to-one corresponding historical cross-sectional data set of oxidation hole shape parameters and a historical cross-sectional data set of oxidation hole uniformity coefficient are collected; Performing outlier removal preprocessing on the oxidation pore shape parameter historical cross-section data set to obtain the oxidation pore shape parameter distribution interval; Performing outlier removal preprocessing on the oxidation pore uniformity coefficient historical cross-section data set to obtain the oxidation pore uniformity coefficient distribution interval; Random assignment is performed according to the oxidation pore shape parameter distribution interval and the oxidation pore uniformity coefficient distribution interval to obtain the oxidation pore shape parameter and the oxidation pore uniformity coefficient.
3. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 2, characterized in that: According to the application scenario type of the VCSEL chip, a one-to-one corresponding historical cross-sectional data set of oxidation hole shape parameters and a historical cross-sectional data set of oxidation hole uniformity coefficient are collected, including: Obtaining oxidation pore shape parameter attributes and oxidation pore uniformity coefficient attributes, wherein the oxidation pore shape parameter attributes include oxidation pore long diameter, oxidation pore short diameter, and oxidation pore depth, and the oxidation pore uniformity coefficient attributes include oxidation pore distribution spacing and oxidation pore distribution quantity; According to the oxidation hole long diameter, the oxidation hole short diameter, the oxidation hole depth, the oxidation hole distribution spacing, and the oxidation hole distribution number, historical cross-sectional data of the VCSEL chip application scenario type are collected to obtain the oxidation hole shape parameter historical cross-sectional data set and the oxidation hole uniformity coefficient historical cross-sectional data set.
4. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 1, characterized in that: According to the oxidation hole shape parameter and the oxidation hole uniformity coefficient, mapping is performed through a beam quality predictor to generate a beam prediction diameter, a beam prediction divergence angle, a beam prediction profile and a barrel prediction power, including: According to the oxidation hole long diameter parameter and the oxidation hole short diameter parameter of the oxidation hole shape parameter, mapping is performed through the beam diameter prediction channel of the beam quality predictor to obtain the beam prediction diameter; According to the oxidation hole shape parameters, mapping is performed through the beam divergence angle prediction channel of the beam quality predictor to obtain the beam predicted divergence angle; According to the oxidation hole uniformity coefficient, mapping is performed through a beam profile prediction channel of the beam quality predictor to obtain the beam prediction profile; According to the oxidation hole uniformity coefficient, mapping is performed through the barrel power prediction channel of the beam quality predictor to obtain the barrel predicted power.
5. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 1, characterized in that: According to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel, a wet oxidation control parameter satisfying the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel is selected and set as a monitoring and control benchmark parameter, including: Verify the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel according to the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel to obtain a beam quality verification result; When the beam quality verification result is passed, optimizing the wet oxidation control parameters according to the oxidation hole shape parameters and the oxidation hole uniformity coefficient to obtain target wet oxidation control parameters; Setting the target wet oxidation control parameter as the monitoring and regulation reference parameter; When the beam quality verification result is failed, the oxidation hole shape parameter and the oxidation hole uniformity coefficient are updated according to the application scenario type of the VCSEL chip.
6. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 5, characterized in that: The predicted beam diameter, the predicted beam divergence angle, the predicted beam profile, and the predicted power in the barrel are verified according to the expected beam diameter, the expected beam divergence angle, the expected beam profile, and the expected power in the barrel to obtain a beam quality verification result, including: When the diameter deviation between the expected diameter of the light beam and the predicted diameter of the light beam is less than or equal to the diameter deviation threshold, and the divergence angle deviation between the expected divergence angle of the light beam and the predicted divergence angle of the light beam is less than or equal to the divergence angle deviation threshold, and the contour shape deviation between the expected profile of the light beam and the predicted profile of the light beam is less than or equal to the contour shape deviation threshold, and the power deviation in the bucket between the expected power in the bucket and the predicted power in the bucket is less than or equal to the power deviation threshold, a first-level verification pass signal is generated; Calculating a first product factor of the expected beam diameter and the expected beam divergence angle, calculating a second product factor of the predicted beam diameter and the predicted beam divergence angle, and obtaining a third product factor of the diffraction-limited Gaussian beam diameter and the diffraction-limited Gaussian beam divergence angle of the same wavelength; Calculating a ratio of the first multiplication factor to the third multiplication factor, setting the ratio as an expected beam quality factor, calculating a ratio of the second multiplication factor to the third multiplication factor, setting the ratio as a predicted beam quality factor; When a beam quality factor deviation between the expected beam quality factor and the predicted beam quality factor is less than or equal to a beam quality factor deviation threshold, generating a secondary verification pass signal; When both the first-level verification pass signal and the second-level verification pass signal pass, the beam quality verification result is passed; Otherwise, the beam quality verification result is failed.
7. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 5, characterized in that: When the beam quality verification result is passed, optimizing the wet oxidation control parameters according to the oxidation hole shape parameter and the oxidation hole uniformity coefficient to obtain the target wet oxidation control parameters includes: Obtaining a wet oxidation control parameter distribution constraint interval, wherein the wet oxidation control parameter distribution constraint interval includes an oxidation temperature distribution constraint interval, an oxidation time distribution constraint interval, a nitrogen flow distribution constraint interval, a nitrogen concentration distribution constraint interval, a water vapor flow distribution constraint interval, and a water vapor concentration distribution constraint interval; According to the VCSEL chip model and the wet oxidation equipment model, online collection of wet oxidation control historical cross-section data sets that meet the oxidation hole shape parameters and the oxidation hole uniformity coefficient; Based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow rate distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow rate distribution constraint interval, and the water vapor concentration distribution constraint interval, the wet oxidation control historical cross-section data set is normalized and reduced in dimension to obtain wet oxidation control particle distribution coordinates; Deleting outlier coordinates of the wet oxidation control particle distribution coordinates to obtain concentrated coordinates of the wet oxidation control particles; The wet oxidation control parameter distribution interval of the concentrated coordinates of the wet oxidation control particles is extracted and set as the target wet oxidation control parameter.
8. The method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to claim 7, characterized in that: Based on the oxidation temperature distribution constraint interval, the oxidation time distribution constraint interval, the nitrogen flow distribution constraint interval, the nitrogen concentration distribution constraint interval, the water vapor flow distribution constraint interval, and the water vapor concentration distribution constraint interval, the wet oxidation control historical cross-section data set is normalized and reduced in dimension to obtain the wet oxidation control particle distribution coordinates, including: Obtain oxidation temperature historical section data of the first wet oxidation control historical section data of the wet oxidation control historical section data set; Calculating a first deviation modulus value between the oxidation temperature historical cross-section data and a minimum value of the oxidation temperature distribution constraint interval; Calculating a second deviation modulus value of a maximum value and a minimum value of the oxidation temperature distribution constraint interval; Calculate the ratio of the first deviation modulus value to the second deviation modulus value and set it as the oxidation temperature normalized coordinate; Using the same processing process, the normalized coordinates of oxidation time, nitrogen flow rate, nitrogen concentration, water vapor flow rate, and water vapor concentration are obtained; According to the normalized coordinates of the oxidation temperature, the normalized coordinates of the oxidation time, the normalized coordinates of the nitrogen flow, the normalized coordinates of the nitrogen concentration, the normalized coordinates of the water vapor flow, and the normalized coordinates of the water vapor concentration, the first particle distribution coordinates are obtained and added to the wet oxidation control particle distribution coordinates.
9. A monitoring and control device for the wet oxidation aperture of a VCSEL chip, characterized in that: The device is used to implement the method for monitoring and controlling the aperture of a VCSEL chip wet oxidation according to any one of claims 1 to 8, and the device comprises: An oxidation aperture optimization request response module, wherein the oxidation aperture optimization request response module is used to respond to a VCSEL chip oxidation aperture optimization request submitted by a user end, and obtain an expected beam diameter, an expected beam divergence angle, an expected beam profile, and an expected power in the barrel; An oxidation hole parameter collection module, the oxidation hole parameter collection module is used to collect oxidation hole shape parameters and oxidation hole uniformity coefficients according to the VCSEL chip application scenario type of the VCSEL chip oxidation hole optimization request; A beam quality prediction module, the beam quality prediction module is used to generate a beam prediction diameter, a beam prediction divergence angle, a beam prediction profile and a barrel prediction power by mapping the oxidation hole shape parameters and the oxidation hole uniformity coefficient through a beam quality predictor; A monitoring and control reference parameter acquisition module, wherein the monitoring and control reference parameter acquisition module is used to select a wet oxidation control parameter that satisfies the expected beam diameter, the expected beam divergence angle, the expected beam profile and the expected power in the barrel according to the predicted beam diameter, the predicted beam divergence angle, the predicted beam profile and the predicted power in the barrel, and set it as a monitoring and control reference parameter; A wet oxidation monitoring module is used to perform wet oxidation monitoring according to the monitoring and control benchmark parameters.
Citation Information
Patent Citations
Perpendicular cavity surface emitting laser device stable in single transverse mode polarization
CN103414105A
A high power and high speed vertical cavity surface emitting laser with double oxide apertures
CN109038215A
Oxidation hole generation method and vertical cavity surface emitting laser device
CN113809637A
Phase array oxide-confined vcsels
JP2005045243A
Vertical cavity surface emitting laser diode and method for manufacturing the same
US20050121678A1
Cited By
Vertical cavity surface emitting laser and oxidation aperture control method thereof
CN121307636A
