Sensing film, manufacturing method thereof and electronic equipment testing assembly

By using induction films of flexible base layer and light reflective layer in electronic equipment, the problem of inaccurate stress simulation in mechanical reliability test is solved, and the accurate recording and identification of the stress conditions of electronic equipment is achieved, which is suitable for the design of internal space of electronic equipment. .

CN119024476APending Publication Date: 2024-11-26HONOR DEVICE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310601002.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-24
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In the mechanical reliability test of the prior art, the stress simulation results of various parts of the electronic equipment differ from the actual results, resulting in inaccurate stress simulation and affecting the internal space design of the electronic equipment.

Method used

Using an induction film including a flexible base layer and a light reflective layer, the light reflective layer consists of a plurality of first dielectric bodies and a second dielectric bodies, displays structural colors under natural light through the Bragg reflection effect, records and recognizes external stresses, and the induction film is Reusable.

Benefits of technology

It improves the accuracy of recording stress conditions in various parts of electronic equipment in mechanical reliability testing, and can detect external pressure and tension at the same time. It is highly applicable and suitable for the design of internal space of electronic equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119024476A_ABST
    Figure CN119024476A_ABST
Patent Text Reader

Abstract

The invention provides an induction film, a manufacturing method thereof and an electronic equipment testing assembly, relates to the technical field of testing, and is used for solving the problem that the recording effect of stress conditions borne by all parts of electronic equipment in a mechanical reliability test is poor. The induction film comprises a flexible substrate layer and a light reflection layer. The light reflecting layer is located on one side of the flexible substrate layer. The light reflection layer comprises a plurality of first dielectric bodies and a plurality of second dielectric bodies, the first dielectric bodies are arranged at intervals at least in the first direction, and the first direction is parallel to the flexible substrate layer. The second medium bodies are located between the two adjacent first medium bodies. The refractive index of the first medium body is different from that of the second medium body.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of testing technology, and in particular to a sensing film and a manufacturing method thereof, and an electronic equipment testing component. Background Art

[0002] In order to improve the reliability of electronic equipment, electronic equipment manufacturers usually simulate the stress conditions that various parts of electronic equipment will be subjected to in real-life usage scenarios during the research and development stage to provide a reference for the design of the internal space of the electronic equipment.

[0003] However, after conducting multiple mechanical reliability tests on electronic devices (such as drop tests, roller tests, etc.), it was found that the stress simulation results obtained for each part of the electronic device are usually different from the actual results, and the stress simulation results are not conducive to the internal space design of the electronic device. Therefore, recording the stress on each part of the electronic device during the mechanical reliability test is of great reference significance for the internal space design of the electronic device.

[0004] Currently, there is an urgent need for a product that can record the stresses on various parts of electronic equipment during mechanical reliability testing. Summary of the invention

[0005] The embodiments of the present application provide a sensing film and a method for manufacturing the same, and an electronic device testing component, which are used to solve the problem of poor recording effect of stress conditions on various parts of an electronic device during a mechanical reliability test.

[0006] To achieve the above objectives, the embodiments of the present application adopt the following technical solutions:

[0007] In a first aspect, a sensing film is provided. The sensing film includes a flexible substrate layer and a light reflecting layer. The light reflecting layer is located on one side of the flexible substrate layer. The light reflecting layer includes a plurality of first dielectric bodies and a second dielectric body, wherein the plurality of first dielectric bodies are arranged at least in a first direction and spaced from each other, and the first direction is parallel to the flexible substrate layer. The second dielectric body is located between two adjacent first dielectric bodies. The refractive index of the first dielectric body is different from the refractive index of the second dielectric body.

[0008] The light reflecting layer may include a first dielectric body and a second dielectric body. The refractive index of the first dielectric body is different from the refractive index of the second dielectric body. Exemplarily, the material included in the first dielectric body and the material included in the flexible base layer may be the same, and the material included in the second dielectric body and the material included in the flexible ground layer may be different, for example, the dielectric constant of the material included in the second dielectric body is different from the dielectric constant of the material included in the flexible base layer. Exemplarily again, the material included in the first dielectric body and the material included in the flexible base layer may also be different.

[0009] The plurality of first dielectric bodies are arranged at intervals from each other along the first direction. Exemplarily, the first dielectric body is a strip structure extending along the second direction, and the plurality of first dielectric bodies are arranged at intervals from each other along the first direction. The plurality of first dielectric bodies may be arranged at equal intervals, or the spacing between the plurality of first dielectric bodies in the local area may be different from the spacing between the plurality of first dielectric bodies in other areas due to stress in the local area.

[0010] A plurality of first dielectric bodies and a plurality of second dielectric bodies form a periodic structure arranged alternately in a first direction on the flexible substrate layer. Since the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, the plurality of first dielectric bodies and the plurality of second dielectric bodies together form a photonic crystal with a one-dimensional structure. When light propagates in the photonic crystal, Bragg reflection occurs, so that light with a wavelength approximately equal to D1 cannot pass through the photonic crystal and is reflected, so that the light reflection layer presents the color of the reflected light in the photonic crystal under natural light. This color can be called the structural color or physical color of the light reflection layer.

[0011] The structural color of the light reflecting layer is directly related to the periodic structure formed by the multiple first dielectric bodies and the multiple second dielectric bodies. When D1 of the photonic crystal changes under the action of an external force, the structural color exhibited by the light reflecting layer also changes accordingly.

[0012] In this way, the sensing film can repeatedly perform mechanical reliability tests on different electronic devices or components to be tested to record the external stress conditions to which the electronic devices or components to be tested are subjected.

[0013] In a possible implementation manner of the first aspect, the plurality of first dielectric bodies are further arranged at intervals from each other along a second direction, and the second direction is parallel to the flexible base layer and intersects with the first direction.

[0014] The plurality of first dielectric bodies are arranged at intervals from each other along the first direction and at intervals from each other along the second direction. The plurality of first dielectric bodies may be arranged at equal intervals in the first direction or the second direction, or the spacing between the plurality of first dielectric bodies in the local area may be different from the spacing between the plurality of first dielectric bodies in other areas due to local stress.

[0015] Exemplarily, the first dielectric body is a block structure, and a plurality of first dielectric bodies are arranged in an array along the first direction and the second direction on the flexible base layer.

[0016] A plurality of first dielectric bodies and a plurality of second dielectric bodies form a periodic structure alternately arranged along a first direction and a periodic structure alternately arranged along a second direction on the flexible substrate layer. Since the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, the plurality of first dielectric bodies and the plurality of second dielectric bodies together form a photonic crystal with a two-dimensional structure. When light propagates in the photonic crystal, Bragg reflection occurs, so that light with a wavelength approximately equal to D1 in the first direction cannot pass through the photonic crystal and is reflected, so that the photonic crystal presents the color of reflected light with a wavelength corresponding to D1 within the viewing angle range corresponding to the first direction under natural light; similarly, light with a wavelength approximately equal to D5 in the second direction cannot pass through the photonic crystal and is reflected, so that the photonic crystal presents the color of reflected light with a wavelength corresponding to D5 within the viewing angle range corresponding to the second direction under natural light.

[0017] In this way, the sensing film can repeatedly perform mechanical reliability tests on different electronic devices or components to be tested to record the external stress conditions to which the electronic devices or components to be tested are subjected.

[0018] In a possible implementation manner of the first aspect, in the first direction, a spacing distance D1 between mutually approaching edges of two adjacent first dielectric bodies satisfies 100 nm≤D1≤1000 nm.

[0019] In the first direction, the spacing distance D1 between the edges of two adjacent first dielectric bodies that are close to each other may satisfy 100 nm≤D1≤1000 nm. For example, D1 may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm or 1000 nm.

[0020] D1 covers the range of visible light, and the change of D1 can be represented by different colors in visible light, so as to facilitate the identification of the sensing effect of the reaction film on stress.

[0021] In a possible implementation of the first aspect, in the first direction, a size D2 of the first dielectric body satisfies 100 nm≤D2≤1000 nm. For example, D2 may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm or 1000 nm.

[0022] D2 covers the range of visible light, and the change of D2 can be represented by different colors in visible light, so as to facilitate the identification of the sensing effect of the reaction film on the stress.

[0023] In a possible implementation of the first aspect, in a direction perpendicular to the flexible base layer, a dimension D3 of the first dielectric body satisfies D3≤1 mm. For example, D3 is 1 mm, 0.9 mm, 0.8 mm, 0.7 mm, 0.6 mm, 0.5 mm, 0.4 mm, 0.3 mm, 0.2 mm, or 0.1 mm.

[0024] Since the first dielectric body is smaller in size in the third direction, it can change its shape more sensitively when receiving external stress, thereby improving the sensitivity of the light reflection layer to external stress. Furthermore, since the number of film layers of the sensing functional layer is small (two layers, namely the flexible base layer and the light reflection layer), the thickness is thinner than the above-mentioned pressure-sensitive paper, and the sensing functional layer can fit the component to be tested inside the electronic device without occupying too much space inside the electronic device, thereby improving the applicability of the sensing film.

[0025] In a possible implementation of the first aspect, in a direction perpendicular to the flexible base layer, a dimension D4 of the second dielectric body satisfies D4≤1 mm. D4 is 1 mm, 0.9 mm, 0.8 mm, 0.7 mm, 0.6 mm, 0.5 mm, 0.4 mm, 0.3 mm, 0.2 mm or 0.1 mm.

[0026] Since the second dielectric body is smaller in size in the third direction, it can change its shape more sensitively when receiving external stress, thereby improving the sensitivity of the light reflecting layer to external stress. Furthermore, since the number of film layers of the sensing functional layer is small (two layers, namely the flexible base layer and the light reflecting layer), the thickness is thinner than the above-mentioned pressure-sensitive paper, and the sensing functional layer can fit the component to be tested inside the electronic device without occupying too much space inside the electronic device, thereby improving the applicability of the sensing film.

[0027] In a possible implementation manner of the first aspect, the shape of the first dielectric body includes at least one of a regular polygon, a rectangular body, a hemispherical body, a spherical body, a rhombus body, and an ellipsoidal body.

[0028] In a possible implementation of the first aspect, the second dielectric body includes air, which can reduce the cost of the second dielectric body, thereby reducing the manufacturing cost and manufacturing steps of the sensing film.

[0029] In a possible implementation manner of the first aspect, the structural colors displayed by the sensing film include green and / or yellow.

[0030] When the structural color of the light reflecting layer shows green or yellow, the human eye can determine that the light reflecting layer is subjected to external pressure and D1 is reduced by discerning that the light reflecting layer appears blue; and the human eye can determine that the light reflecting layer is subjected to external pressure and D1 is expanded by discerning that the light reflecting layer appears red.

[0031] Therefore, when the structural color of the light reflecting layer shows green and / or yellow, the sensing film can detect external pressure and external tension at the same time, which can increase the diversity of the sensing film's sensing of external stress and expand the use scenarios of the sensing film.

[0032] In a possible implementation of the first aspect, the sensing film further includes a release paper, which is located on a side of the flexible base layer away from the light reflecting layer and is laminated to the flexible base layer.

[0033] The release paper can be directly attached to the surface of the sensing functional layer to prevent external dust or other substances from being adsorbed on the surface of the sensing functional layer, thereby reducing the adhesion between the subsequent sensing functional layer and the electronic device to be tested or the components to be tested inside the electronic device to be tested (such as mainboards, chips and other structural parts). The release paper needs to have a hard texture and is not easy to deform, so a smooth paper material can be selected for the release paper. In addition, a layer of pressure-sensitive adhesive can be coated on the surface of the release paper to facilitate the release paper to be bonded to the sensing functional layer through the pressure-sensitive adhesive.

[0034] In actual use scenarios, the release paper is first peeled off from the surface of the sensing function layer, and then the sensing function layer is attached to the surface of the electronic device or component to be tested. Therefore, the release paper can improve the firmness of the attachment of the sensing function layer to the surface of the electronic device or component to be tested.

[0035] In a possible implementation manner of the first aspect, the sensing film further includes a protective film, which is located on a side of the light reflecting layer away from the flexible base layer and is laminated to the light reflecting layer.

[0036] The protective film can be directly attached to the surface of the sensing functional layer to prevent external stress from being directly applied to the sensing functional layer, thereby reducing or even preventing the influence of external stress on the structural color displayed by the sensing functional layer. In actual use scenarios, the protective film can be peeled off from the surface of the sensing functional layer first, and then the sensing functional layer can be attached to the surface of the electronic device or component to be tested; or, the sensing functional layer can be attached to the surface of the electronic device or component to be tested first, and then the protective film can be peeled off from the surface of the sensing functional layer.

[0037] The protective film may include one or more polymer materials selected from polyethylene, polyethylene terephthalate and o-phenylphenol. Of course, the protective film may also include other suitable materials, which are not limited herein.

[0038] In a possible implementation of the first aspect, the flexible substrate layer and the first dielectric body include the same material and are connected as an integral structure, so that the flexible substrate layer and the first dielectric body can be manufactured at the same time, simplifying the manufacturing steps of the sensing film and improving the manufacturing efficiency of the sensing film.

[0039] In a possible implementation of the first aspect, the flexible base layer may include a soft polymer material. For example, the flexible base layer may include one or more of polydimethylsiloxane, thermoplastic polyurethane elastomer, thermoplastic elastomer, thermoplastic polyester elastomer (also known as polyester rubber), polyacrylates with long chain alkyl side chains, and rubber polymers, which are not limited here.

[0040] The flexible substrate has the characteristics of dimensional stability at room temperature, moderate cross-linking degree, plastic deformation, and rebound after deformation.

[0041] In a second aspect, a method for manufacturing a sensing film is also provided. The method includes: providing a hard template. Using the hard template to shape the material to be formed to form a sensing film; the sensing film includes a flexible substrate layer and a light reflecting layer located on one side of the flexible substrate layer; the light reflecting layer includes a plurality of first dielectric bodies and a second dielectric body, the plurality of first dielectric bodies are arranged at least in a first direction and spaced apart from each other, and the second dielectric body is located between two adjacent first dielectric bodies; the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, and the first direction is parallel to the flexible substrate layer.

[0042] First, a hard template can be produced. The hard template may include a rigid material, and the rigid material may include metal, ceramic, glass, quartz, hard polymer material, etc., which are not limited here. The hard template can be prepared by masking and electron beam etching the rigid material, and of course, it can also be prepared by other suitable methods, which are not limited here.

[0043] The hard template may include a base portion and a protrusion. The protrusion may be located on one side of the base portion, and the protrusion includes a plurality of protrusion sub-portions. In some examples, each protrusion sub-portion may be a long strip structure extending along the second direction, and the plurality of protrusion sub-portions may be a one-dimensional structure spaced apart along the first direction. In other examples, the plurality of protrusion sub-portions may be a block structure, and the plurality of protrusion sub-portions may be a two-dimensional structure spaced apart along the first direction and along the second direction.

[0044] After the hard template is manufactured, the hard template can be used to emboss the first dielectric material to be formed, so that the first dielectric material to be formed is formed. Afterwards, the formed first dielectric material can be cured, so that the cured first dielectric material forms a sensing function layer.

[0045] One set of hard templates can form a sensing functional layer exhibiting one initial structural color, and multiple sets of hard templates can form sensing functional layers exhibiting multiple initial structural colors.

[0046] The sensing functional layer obtained by hard template stamping, the first dielectric body and the flexible base layer may include the same material. For example, the first dielectric body and the flexible base layer are both made of the first dielectric material to be formed, and the first dielectric body and the flexible base layer are an integrated structure connected to each other.

[0047] The method of imprinting the first dielectric material to be formed by a hard template so that the first dielectric material to be formed is formed and forms a sensing film can improve the stability of the shape and spacing of each first dielectric body on the sensing film, and obtain a sensing film with excellent sensing performance. In addition, the method has a simple process and low cost, and can facilitate large-scale production of sensing films.

[0048] In a possible implementation of the second aspect, a material to be molded is molded using a hard template to form a sensing film, including: providing a substrate. Coating a first dielectric material to be molded on the substrate. Imprinting the first dielectric material to be molded using the hard template to form a molded first dielectric material layer matching the shape of the hard template. Curing the molded first dielectric material layer. After the molded first dielectric material layer is cured, the substrate is removed to form a first dielectric body, the first dielectric body having a periodic structure. A second dielectric body is filled in the gap of the periodic structure to form a sensing film.

[0049] In some feasible implementations, before the hard template performs imprinting on the first dielectric material to be formed, a substrate may be provided, which may include a rigid substrate, such as a quartz substrate, a glass substrate, etc., which is not limited here.

[0050] The first dielectric material to be formed is coated on the substrate, and then the protrusion of the hard template is facing the first dielectric material to be formed and the hard template is pressed into the first dielectric material to be formed, so that the first dielectric material to be formed is formed on the substrate to form a first dielectric material layer that matches the shape of the hard template. The coating of the first dielectric material to be formed can be specifically carried out by at least one of spin coating, spray coating, scraping coating or drip coating.

[0051] Afterwards, the first dielectric material layer formed on the substrate is cured, and the substrate is removed from the cured first dielectric material layer to form a first dielectric body, wherein the first dielectric body has a periodic structure. The curing of the molding material layer can be performed by ultraviolet light curing or thermal curing. When the molding material layer is cured by UV light, the hard template can include a light-transmitting material such as glass.

[0052] Afterwards, the second dielectric body can be filled in the gaps of the periodic structure of the first dielectric body to form a sensing functional layer. The shape of the second dielectric body in the sensing functional layer can be matched with the shape of the protrusions in the hard template.

[0053] Exemplarily, the sensing functional layer formed above can be a sensing functional layer with air as the second dielectric body. In some other examples, the first dielectric material layer formed after curing serves as the first dielectric body, and the second dielectric body can be further formed after the first dielectric body is formed, so that the first dielectric body and the second dielectric body together form a light reflection layer of the sensing functional layer.

[0054] It can be understood that when the multiple protrusions on the hard template form a one-dimensional structure, the light reflection layer formed by the hard template is also a one-dimensional structure of the corresponding shape. Similarly, when the multiple protrusions on the hard template form a two-dimensional structure, the light reflection layer formed by the hard template is also a two-dimensional structure of the corresponding shape.

[0055] In a possible implementation of the second aspect, a material to be molded is molded using a hard template to form a sensing film, including: coating a first dielectric material to be molded on the hard template to form a molded first dielectric material matching the shape of the hard template. Curing the molded first dielectric material. After the molded first dielectric material is cured, the hard template is removed to form a first dielectric body, the first dielectric body having a periodic structure. A second dielectric body is filled in the gap of the periodic structure to form a sensing film.

[0056] In some feasible implementations, the first dielectric material to be formed can also be directly coated on the base of the hard template and cover the protrusions, so that the first dielectric material to be formed is formed on the hard template to form a formed first dielectric material layer matching the shape of the hard template.

[0057] Afterwards, the first dielectric material layer formed on the hard template is cured, and after the hard template is removed from the cured first dielectric material layer, a first dielectric body is formed, and the first dielectric body has a periodic structure. Specifically, the first dielectric material layer can be cured by ultraviolet light curing or thermal curing. When UV light is used to cure the molded material layer, the hard template can include a light-transmitting material such as glass.

[0058] Afterwards, the second dielectric body can be filled in the gaps of the periodic structure of the first dielectric body to form a sensing functional layer. The shape of the second dielectric body in the sensing functional layer can be matched with the shape of the protrusions in the hard template.

[0059] Exemplarily, the sensing functional layer formed above is a sensing functional layer with air as the second dielectric body. In some other examples, the first dielectric material layer formed after curing is used as the first dielectric body, and the second dielectric body can be formed after the first dielectric body is formed, so that the first dielectric body and the second dielectric body together form the light reflection layer of the sensing functional layer.

[0060] It can be understood that when the multiple protrusions on the hard template form a one-dimensional structure, the light reflection layer 22 formed by the hard template is also a one-dimensional structure of the corresponding shape. Similarly, when the multiple protrusions on the hard template form a two-dimensional structure, the light reflection layer formed by the hard template is also a two-dimensional structure of the corresponding shape.

[0061] In a third aspect, a method for manufacturing a sensing film is also provided. The method includes: forming a flexible substrate layer. Forming a plurality of first dielectric bodies spaced apart from each other at least along a first direction on the flexible substrate layer, and a second dielectric layer located between two adjacent first dielectric bodies, forming a light reflection layer, and the flexible substrate layer and the light reflection layer together constitute the sensing film. The refractive index of the first dielectric body is different from the refractive index of the second dielectric body, and the first direction is parallel to the flexible substrate layer.

[0062] The flexible substrate layer can be produced by coating a flexible substrate material. The flexible substrate layer may include a soft polymer material. Exemplarily, the flexible substrate layer may include one or more of polydimethylsiloxane, thermoplastic polyurethane elastomer, thermoplastic elastomer, thermoplastic polyester elastomer, polyacrylates with long chain alkyl side chains, and rubber polymers, which are not limited here. In this way, the flexible substrate layer can have good flexibility and stretchability.

[0063] The present application can obtain various sensing films by first manufacturing a flexible base material and then manufacturing a light reflecting layer with a one-dimensional structure or a two-dimensional structure on the flexible base material.

[0064] In a possible implementation of the third aspect, a plurality of first medium bodies arranged at least at intervals from each other along a first direction are formed on a flexible base layer, including: printing a plurality of ink droplets on the flexible base layer, and the plurality of ink droplets arranged at least at intervals from each other along the first direction form a plurality of first medium bodies on the flexible base layer.

[0065] After the flexible base layer is manufactured, a plurality of ink droplets may be printed on the flexible base layer by using an inkjet printing process. The plurality of ink droplets may be arranged at intervals from each other at least along a first direction.

[0066] The ink droplets may include one or more of microsphere emulsion, humectant (such as ethylene glycol), surfactant, and deionized water. In addition, the ink droplets may also include other suitable materials, which are not limited herein.

[0067] The microsphere emulsion may include monodisperse polymer materials (such as polystyrene), metal materials, ceramic materials (such as silicon dioxide) and other suitable materials, which are not limited here. In addition, the proportion of deionized water in the ink droplets can adjust the viscosity between the ink droplets and the flexible substrate layer.

[0068] The microspheres in the ink droplets react with the flexible substrate layer and are fixed on the flexible substrate layer, thereby forming a plurality of first dielectric bodies arranged at intervals from each other at least along a first direction on the flexible substrate layer.

[0069] It should be noted that the orderly spacing between the multiple ink droplets printed on the flexible substrate layer can be achieved by inducing the formation of non-covalent interaction forces through the evaporation of the solvent in the ink droplets. The non-covalent interaction force is a force that is spontaneously formed between the ink droplets due to thermodynamic reasons, and can automatically achieve the orderly spacing between the multiple ink droplets without the help of other external forces.

[0070] A two-dimensional structure extending along the first direction and the second direction may be formed between the plurality of first dielectric bodies. The plurality of first dielectric bodies close to each other may be arranged in a rectangular shape, an equilateral triangle shape, or a regular hexagon shape.

[0071] The spacing distance between the edges of two adjacent first dielectric bodies on the flexible base layer that are close to each other will decrease due to the contraction of the flexible base layer, and will also increase due to the extension of the flexible base layer.

[0072] The method of forming a sensing film by printing ink droplets on a flexible substrate layer through an inkjet printing process can adjust the distance between multiple ink droplets on the flexible substrate layer by controlling the spacing degree of the solvent volatilization in the ink droplets to induce self-assembly, thereby adjusting the distance between multiple first dielectric bodies. It has the advantage of easy adjustment of the initial structural color of the sensing film, and can produce sensing films with different initial structural colors according to actual needs. In addition, this method does not require an additional hard template, which can reduce the cost of the hard template in the process of manufacturing the sensing film, thereby reducing the manufacturing cost of the sensing film.

[0073] In a fourth aspect, an electronic device test assembly is also provided. The electronic device test assembly includes a sensing film and an identification mechanism. The sensing film is any of the above sensing films. The sensing film is used to fit the outer surface of the electronic device and / or the outer surface of the internal components of the electronic device. The identification mechanism is used to identify the color on the sensing film after the electronic device completes the mechanical reliability test.

[0074] Since the electronic device testing assembly provided in the present application includes the sensing film described in any one of the embodiments of the first aspect above, the two can solve the same technical problems and achieve the same effects. BRIEF DESCRIPTION OF THE DRAWINGS

[0075] Figure 1 Schematic diagram of the structure of pressure-sensitive paper in some schemes;

[0076] Figure 2 A schematic diagram of the structure of the sensing film provided in some embodiments of the present application;

[0077] Figure 3 A schematic diagram of the product form of the sensing film provided in some embodiments of the present application;

[0078] Figure 4 Schematic diagram of the product form of the sensing film provided in other embodiments of the present application;

[0079] Figure 5 A side view of a sensing functional layer provided for some embodiments of the present application;

[0080] Figure 6 for Figure 5 A schematic diagram of a three-dimensional structure of a corresponding sensing functional layer;

[0081] Figure 7 for Figure 6 A schematic diagram of a three-dimensional structure in which the spacing between the edges of two adjacent first dielectric bodies close to each other in the sensing functional layer is in different sizes;

[0082] Figure 8 for Figure 5 Another schematic diagram of the three-dimensional structure of the corresponding sensing functional layer;

[0083] Fig. 9 for Figure 5 Another schematic diagram of the three-dimensional structure of the corresponding sensing functional layer;

[0084] Fig.10 for Fig. 9 A top view of the sensing functional layer shown;

[0085] Fig.11 for Fig.10 A schematic diagram of a three-dimensional structure in which the spacing between the edges of two adjacent first dielectric bodies close to each other in the sensing functional layer is in different sizes;

[0086] Fig.12 It is a schematic diagram of the structure of one side surface of the electronic device to be tested;

[0087] Fig.13 A schematic diagram of the structure of the sensing functional layer provided in some embodiments of the present application after being attached to the surface of the electronic device to be tested;

[0088] Fig.14 A schematic diagram of the manufacturing process of the sensing film provided in some embodiments of the present application;

[0089] Fig.15 A schematic diagram of a manufacturing process of a sensing film provided in other embodiments of the present application;

[0090] Fig.16 A schematic diagram of a one-dimensional photonic crystal structure of an optical disc and a local part of the optical disc;

[0091] Fig.17 A schematic diagram of a manufacturing process of a sensing film provided in other embodiments of the present application;

[0092] Fig.18 for Fig.17 A top view of a sensing film manufactured by the sensing film manufacturing method shown. DETAILED DESCRIPTION

[0093] In the embodiments of the present application, the terms "first", "second", and "third" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or more of the features.

[0094] In the embodiments of the present application, the terms "include", "comprises" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element.

[0095] In order to improve the reliability of electronic equipment, electronic equipment manufacturers will conduct multiple mechanical reliability tests on electronic equipment (such as drop tests, roller tests, etc.) during the design and development process to simulate the stress conditions that various parts of the electronic equipment are subjected to in actual usage scenarios, and provide a reference for the internal space design of the electronic equipment.

[0096] Pressure-sensitive paper is widely used to record stress sources during the reliability test phase of electronic equipment. During the mechanical reliability test of electronic equipment, pressure-sensitive paper is first attached to the surface of the electronic equipment or the surface of the component to be tested inside the electronic equipment; then the electronic equipment with pressure-sensitive paper attached is subjected to mechanical reliability test. After the mechanical reliability test, the pressure-sensitive paper can represent the stress-bearing part of the electronic equipment by the color displayed, and the depth of the color displayed by the pressure-sensitive paper can represent the magnitude of the force on the stress-bearing part of the electronic equipment.

[0097] Figure 1The schematic diagram of the structure of the pressure-sensitive paper is shown. The working principle of the pressure-sensitive paper 00 is that when the pressure-sensitive paper is subjected to external stress, the microcapsule 01 will rupture, and the color-forming material in the microcapsule 01 will react with the external color-developing material 02 to produce a color (for example, red). The degree of rupture of the microcapsule is different under different degrees of stress, so different depths of color representing different stress magnitudes can be presented.

[0098] However, due to the limitation of the working principle of pressure-sensitive paper 00, firstly, whether pressure or tension is applied to pressure-sensitive paper 00, it will cause microcapsule 01 to rupture. Therefore, it is impossible to identify whether the stress is pressure or tension from the color display of pressure-sensitive paper 00. Secondly, the number of film layers of pressure-sensitive paper 00 is large, and there is a problem of large thickness of pressure-sensitive paper 00, which makes it difficult to fit the components to be tested inside the electronic device. In addition, the stress pressure displayed by pressure-sensitive paper 00 must cause the microcapsule to rupture, and there is a problem of low sensitivity to stress sensing. The above multiple situations lead to the poor recording effect of pressure-sensitive paper on the stress conditions of various parts of electronic equipment in mechanical reliability testing.

[0099] Based on this, the embodiments of the present application provide a sensing film and a manufacturing method thereof, and an electronic device testing assembly, which are used to overcome the problem of poor recording of stress conditions of various parts of electronic devices in mechanical reliability testing. Detailed descriptions are given below.

[0100] Figure 2 A schematic diagram of the structure of the sensing film provided in some embodiments of the present application; Figure 3 A schematic diagram of the product form of the sensing film provided in some embodiments of the present application; Figure 4 Schematic diagram of the product form of the sensing film provided in other embodiments of the present application.

[0101] like Figure 2 As shown, the sensing film 100 may include a release paper 10, a sensing function layer 20 and a protective film 30. The release paper 10, the sensing function layer 20 and the protective film 30 may be stacked in sequence, and the sensing function layer 20 is located between the release paper 10 and the protective film 30.

[0102] The sensing functional layer 20 may include a flexible substrate layer and a light reflecting layer. The light reflecting layer is located on one side of the flexible substrate layer. The release paper 10 may be located on the side of the flexible substrate layer away from the light reflecting layer, and the protective film 30 may be located on the side of the light reflecting layer away from the flexible substrate layer. The light reflecting layer may reflect light of a specific wavelength to display a structural color of a corresponding color. The structural color displayed by the light reflecting layer may also be referred to as the structural color displayed by the sensing functional layer 20. The sensing functional layer 20 will be described in detail later.

[0103] The release paper 10 can be directly attached to the surface of the sensing function layer 20 to prevent dust or other substances from being adsorbed on the surface of the sensing function layer 20, thereby reducing the adhesion between the subsequent sensing function layer 20 and the electronic device to be tested or the components to be tested inside the electronic device to be tested (such as mainboards, chips and other structural parts). The release paper 10 needs to have a hard texture and is not easy to deform, so a smooth paper material can be selected for the release paper 10. In addition, a layer of pressure-sensitive adhesive can be coated on the surface of the release paper 10 so that the release paper 10 can be bonded to the sensing function layer 20 through the pressure-sensitive adhesive.

[0104] In actual use scenarios, the release paper 10 is first peeled off from the surface of the sensing function layer 20, and then the sensing function layer 20 is attached to the surface of the electronic device or component to be tested. Therefore, the release paper 10 can improve the firmness of the attachment of the sensing function layer 20 to the surface of the electronic device or component to be tested.

[0105] The protective film 30 can be directly attached to the surface of the sensing functional layer 20 to prevent external stress from being directly applied to the sensing functional layer 20, thereby reducing or even preventing the influence of external stress on the structural color displayed by the sensing functional layer 20. In actual use scenarios, the protective film 30 can be peeled off from the surface of the sensing functional layer 20 first, and then the sensing functional layer 20 can be attached to the surface of the electronic device or component to be tested; or, the sensing functional layer 20 can be attached to the surface of the electronic device or component to be tested first, and then the protective film 30 can be peeled off from the surface of the sensing functional layer 20.

[0106] The protective film 30 may include one or more polymer materials selected from polyethylene (PE), polyethylene terephthalate (PET) and o-phenylphenol (OPP). Of course, the protective film 30 may also include other suitable materials, which are not limited here.

[0107] Among them, the sensing film 100 actually only has the sensing functional layer 20 for sensing external stress, so the sensing functional layer 20 can also be called the sensing film with the release paper 10 and the protective film 30 removed. There are three ways to bond the sensing functional layer 20 to the surface of the electronic device or the component to be tested. In the first bonding method, the sensing functional layer 20 is directly bonded to the surface of the structural part (the electronic device or the component to be tested) by the adhesion of its own material, without the need for additional adhesive materials; in the second bonding method, the surface of the release paper 10 is coated with a pressure-sensitive adhesive, and after the release paper 10 is removed, at least part of the pressure-sensitive adhesive remains on the sensing functional layer 20, and the sensing functional layer 20 is bonded to the surface of the structural part through the pressure-sensitive adhesive; in the third bonding method, a layer of non-viscous liquid (such as water or alcohol) is coated on the surface of the structural part, and the surface tension of the non-viscous liquid is used to adsorb the sensing functional layer 20 on the surface of the structural part, and in the third bonding method, after the stress test of the structural part, the sensing functional layer 20 is easier to remove from the surface of the structural part.

[0108] like Figure 3 As shown, the sensing film 100 can be in the form of multiple independent thin sheets during the sales and transportation process. The multiple sensing films 100 can include a uniform size or a variety of different sizes to match electronic devices of different sizes and their internal components. In addition, as Figure 4 As shown, the sensing film 100 can also be in a continuous and curved roll form during the sales and transportation process. Users can cut the roll-shaped sensing film 100 according to actual use needs to obtain the sensing film 100 in the form of sheets of various sizes.

[0109] It should be noted that the sensing film 100 may include both the release paper 10 and the protective film 30, or only one of them, which is not limited here. In addition, in the roll-shaped sensing film 100, the release paper 10 in the outer circle of the sensing film 100 can be reused as the protective film of the inner circle of the sensing film 100. Therefore, in this case, the sensing film 100 can only include the release paper 10 and the sensing function layer 20, and there is no need to set up the protective film 30 additionally.

[0110] The sensing functional layer 20 is described in detail below:

[0111] Figure 5 A side view of a sensing functional layer provided for some embodiments of the present application; Figure 6 for Figure 5 A schematic diagram of a three-dimensional structure of a corresponding sensing functional layer; Figure 7 for Figure 6 The three-dimensional structural schematic diagrams are shown in which the spacing distances between the edges of two adjacent first dielectric bodies in the sensing functional layer are in different sizes.

[0112] like Figure 5As shown, the sensing functional layer 20 may include a flexible base layer 21 and a light reflecting layer 22. In the third direction Z, the light reflecting layer 22 is located on one side of the flexible base layer 21.

[0113] The flexible substrate layer 21 may include a soft polymer material. For example, the flexible substrate layer 21 may include one or more of polydimethylsiloxane (PDMS), thermoplastic polyurethane (TPU), thermoplastic elastomer (TPE), thermoplastic polyester elastomer (TPEE, also known as polyester rubber), polyacrylates with long chain alkyl side chains, and rubber polymers, which are not limited here.

[0114] The flexible substrate layer 21 has the characteristics of being dimensionally stable at room temperature, having a moderate degree of cross-linking, being plastically deformable, and being able to rebound after deformation.

[0115] The light reflection layer 22 may include a first dielectric body 221 and a second dielectric body 222. The refractive index of the first dielectric body 221 is different from the refractive index of the second dielectric body 222. Exemplarily, the material included in the first dielectric body 221 and the material included in the flexible base layer 21 may be the same, and the material included in the second dielectric body 222 and the material included in the flexible ground layer 21 may be different, for example, the dielectric constant of the material included in the second dielectric body 222 is different from the dielectric constant of the material included in the flexible base layer 21. Exemplarily, the material included in the first dielectric body 221 and the material included in the flexible base layer 21 may also be different.

[0116] For example, the first dielectric body 221 may include a light-transmitting resin material. The second dielectric body 222 may include air. This can reduce the cost of the second dielectric body, thereby reducing the manufacturing cost and manufacturing steps of the sensing film. Of course, the first dielectric body 221 and the second dielectric body 222 may also be made of light-transmitting resin materials, but their refractive indices are different.

[0117] like Figure 5As shown, the dimension D3 of the first dielectric body 221 perpendicular to the flexible substrate layer 21 (third direction Z) can satisfy D3≤1mm. For example, D3 is 1mm, 0.9mm, 0.8mm, 0.7mm, 0.6mm, 0.5mm, 0.4mm, 0.3mm, 0.2mm or 0.1mm. Similarly, the dimension D4 of the second dielectric body 222 perpendicular to the flexible substrate layer 21 can also satisfy D4≤1mm. For example, D4 ​​is 1mm, 0.9mm, 0.8mm, 0.7mm, 0.6mm, 0.5mm, 0.4mm, 0.3mm, 0.2mm or 0.1mm. Among them, the dimension D3 of the first dielectric body 221 perpendicular to the flexible substrate layer 21 and the dimension D4 of the second dielectric body 222 perpendicular to the flexible substrate layer 21 can be substantially equal.

[0118] Since the first dielectric body 221 and / or the second dielectric body 222 are relatively small in size in the third direction Z, they can be more sensitive to morphological changes when receiving external stress, thereby improving the sensitivity of the light reflecting layer 22 to external stress. Furthermore, since the number of film layers of the sensing functional layer 20 is small (two layers, namely the flexible base layer 21 and the light reflecting layer 22), the thickness is thinner than the above-mentioned pressure-sensitive paper, and the sensing functional layer 20 can be attached to the component to be tested inside the electronic device without occupying too much space inside the electronic device, thereby improving the applicability of the sensing film 100.

[0119] On the basis that the dimension D3 of the first dielectric body 221 in the third direction Z is ≤1 mm, the dimension D7 of the sensing functional layer 20 in the third direction Z may satisfy D7≤2 mm. For example, D7 is 0.5 mm, 0.8 mm, 1 mm, 1.2 mm, 1.4 mm, 1.6 mm, 1.8 mm or 2 mm.

[0120] Since the dimension D7 of the sensing functional layer 20 in the third direction Z is relatively small, the sensing functional layer 20 can be attached to the internal component to be tested of the electronic device to perform stress sensing on the internal component to be tested, thereby improving the applicability of the sensing film 100 .

[0121] In some possible implementations, such as Figure 5 and Figure 6 As shown, a plurality of first dielectric bodies 221 are arranged at intervals along the first direction X. Exemplarily, the first dielectric body 221 is a strip structure extending along the second direction Y, and the plurality of first dielectric bodies 221 are arranged at intervals along the first direction X. The plurality of first dielectric bodies 221 may be arranged at equal intervals, or the spacing between the plurality of first dielectric bodies 221 in the local area may be different from the spacing between the plurality of first dielectric bodies 221 in other areas due to stress in the local area.

[0122] For example, Figure 5As shown, in the first direction X, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 that are close to each other may satisfy 100nm≤D1≤1000nm. For example, D1 may be 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 700nm, 800nm, 900nm or 1000nm.

[0123] D1 covers the range of visible light, and the change of D1 can be represented by different colors in the visible light, so as to facilitate identification of the sensing effect of the reaction film 100 on the stress.

[0124] Of course, the plurality of first dielectric bodies 221 may also be arranged at intervals along the second direction Y. Exemplarily, the first dielectric body 221 is a strip structure extending along the first direction X, and the plurality of first dielectric bodies 221 are arranged at intervals along the second direction Y. This is not limited here.

[0125] The first dielectric body 221 and the flexible base layer 21 are connected to each other and fixed in position. For example, the first dielectric body 221 and the flexible base layer 21 include the same material and are an integrally formed structure.

[0126] like Figure 5 and Figure 6 As shown, the second dielectric body 222 is located between two adjacent first dielectric bodies 221. It can be understood that the plurality of second dielectric bodies 222 are arranged in a spaced relationship along the first direction X, wherein the spacing distance between the edges of two adjacent second dielectric bodies 222 that are close to each other in the first direction X is equal to the dimension D2 of the first dielectric body 221 in the first direction X.

[0127] For example, Figure 5 As shown, in the first direction X, the size D2 of the first dielectric body 221 may satisfy 100 nm≤D2≤1000 nm. For example, D2 may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm or 1000 nm.

[0128] D2 covers the range of visible light, and the change of D2 can be represented by different colors in the visible light, so as to facilitate identification of the sensing effect of the reaction film 100 on the stress.

[0129] In this way, Figure 5 and Figure 6As shown, a plurality of first dielectric bodies 221 and a plurality of second dielectric bodies 222 are arranged alternately in a first direction X on the flexible base layer 21, and because the refractive index of the first dielectric body 221 is different from the refractive index of the second dielectric body 222, the plurality of first dielectric bodies 221 and the plurality of second dielectric bodies 222 together form a photonic crystal with a one-dimensional structure. When light propagates in the photonic crystal, Bragg reflection occurs, so that light with a wavelength approximately equal to D1 cannot pass through the photonic crystal and is reflected, so that the photonic crystal of the light reflection layer 22 presents the color of the reflected light under natural light. This color can be called the structural color or physical color of the light reflection layer 22.

[0130] The structural color of the light reflecting layer 22 is directly related to the periodic structure formed by the plurality of first dielectric bodies 221 and the plurality of second dielectric bodies 222 . When D1 of the photonic crystal changes under the action of an external force, the structural color exhibited by the light reflecting layer 22 also changes accordingly.

[0131] For example, when the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 that are close to each other is approximately equal to 580 nm, Figure 7 In the sensing functional layer 20 shown in (b), the light reflecting layer 22 exhibits a yellow structural color. On this basis, if the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 approaching each other increases to 630 nm under the action of external tension, as Figure 7 The light reflecting layer 22 in the sensing functional layer 20 shown in (c) shows a red structural color. Alternatively, if the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 approaching each other is reduced to 450nm under the action of external pressure, as shown in FIG. Figure 7 In the sensing functional layer 20 shown in (a), the light reflecting layer 22 exhibits a blue structural color.

[0132] It should be noted that due to the characteristics of the cross-linking degree of the flexible substrate layer 21, when the light reflective layer 22 is subjected to external stress causing the D1 in the light reflective layer 22 to change, so that the structural color presented by the light reflective layer 22 changes, the flexible substrate layer 21 can make the structural color presented by the light reflective layer 22 after the D1 changes be maintained for 10min-20min. Afterwards, the flexible substrate layer 21 drives the D1 of the light reflective layer 22 to be restored to the previous D1, and the structural color of the light reflective layer 22 can be restored to the structural color presented before. By maintaining the structural color presented by the light reflective layer 22 after the change through the cross-linking degree of the flexible substrate layer 21, it is possible to conveniently record the stress-bearing parts of the electronic equipment in the mechanical reliability test, and whether each stress-bearing part is subjected to tensile stress or compressive stress, through the color distribution of the sensing film.

[0133] In this way, the sensing film 100 can repeatedly perform mechanical reliability tests on different electronic devices or components to be tested, so as to record the external stress conditions to which the electronic devices or components to be tested are subjected.

[0134] Figure 8 for Figure 5 Another schematic diagram of the three-dimensional structure of the corresponding sensing functional layer; Fig. 9 for Figure 5 Another schematic diagram of the three-dimensional structure of the corresponding sensing functional layer; Fig.10 for Fig. 9 A top view of the sensing functional layer shown; Fig.11 for Fig.10 The three-dimensional structural schematic diagrams are shown in which the spacing distances between the edges of two adjacent first dielectric bodies in the sensing functional layer are in different sizes.

[0135] In some possible implementations, such as Figure 8 and Fig. 9 As shown, the plurality of first dielectric bodies 221 are arranged at intervals along the first direction X and at intervals along the second direction Y. The plurality of first dielectric bodies 221 may be arranged at equal intervals in the first direction X or the second direction Y, or the spacing between the plurality of first dielectric bodies 221 in the local area may be different from the spacing between the plurality of first dielectric bodies 221 in other areas due to local stress.

[0136] For example, Fig.10 As shown, in the first direction X, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 close to each other can satisfy 100nm≤D1≤1000nm. For example, D1 can be 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 700nm, 800nm, 900nm or 1000nm. In the second direction Y, the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 close to each other can satisfy 100nm≤D5≤1000nm. For example, D5 can be 100nm, 200nm, 300nm, 400nm, 500nm, 600nm, 700nm, 800nm, 900nm or 1000nm.

[0137] The spacing distance D1 between the edges of two adjacent first dielectric bodies 221 in the first direction X and the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 in the second direction Y may be substantially equal or unequal.

[0138] Exemplarily, the first dielectric body 221 is a block structure, and a plurality of first dielectric bodies 221 are arranged in an array on the flexible base layer 21 along the first direction X and the second direction Y. Figure 8 As shown, the shape of the first dielectric body 221 includes a regular polygon (such as a rectangular body, a regular pentagonal prism or a regular hexagonal prism, etc.), a rectangular body (such as a long strip), a hemispherical body, a spherical body, a rhombus, an ellipsoid, a cylinder (such as Fig. 9 At least one of the ones shown).

[0139] The first dielectric body 221 and the flexible base layer 21 are connected to each other and fixed in position. For example, the first dielectric body 221 and the flexible base layer 21 include the same material and are an integrally formed structure.

[0140] like Figure 8 , Fig. 9 and Fig.10 As shown, the second dielectric body 222 is located between two adjacent first dielectric bodies 221 .

[0141] The spacing distance between the edges of two adjacent second dielectric bodies 222 that are close to each other in the first direction X is equal to the size of the first dielectric body 221 in the first direction X. For example, Fig.10 As shown, in the first direction X, the size D2 of the first dielectric body 221 may satisfy 100 nm≤D2≤1000 nm. For example, D2 may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm or 1000 nm.

[0142] The spacing distance between the edges of two adjacent second dielectric bodies 222 that are close to each other in the second direction Y is equal to the dimension D6 of the first dielectric body 221 in the second direction Y. For example, Fig.10 As shown, in the second direction Y, the dimension D6 of the first dielectric body 221 may satisfy 100 nm≤D6≤1000 nm. For example, D2 may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm or 1000 nm.

[0143] In this way, Figure 8 and Fig. 9As shown, a plurality of first dielectric bodies 221 and a plurality of second dielectric bodies 222 are arranged on the flexible base layer 21 to form a periodic structure alternately arranged along the first direction X and a periodic structure alternately arranged along the second direction Y. Since the refractive index of the first dielectric body 221 is different from that of the second dielectric body 222, the plurality of first dielectric bodies 221 and the plurality of second dielectric bodies 222 together form a photonic crystal with a two-dimensional structure. When light propagates in the photonic crystal, Bragg reflection occurs, so that light having a wavelength substantially equal to D1 cannot pass through the photonic crystal in the first direction X and is reflected, so that the photonic crystal presents the color of reflected light corresponding to the wavelength D1 within the viewing angle range corresponding to the first direction X under natural light; similarly, light having a wavelength substantially equal to D5 cannot pass through the photonic crystal in the second direction X and is reflected, so that the photonic crystal presents the color of reflected light corresponding to the wavelength D5 within the viewing angle range corresponding to the second direction Y under natural light.

[0144] For example, Fig.10 As shown, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 approaching each other in the first direction X can be equal to 450nm, and at this time, the photonic crystal of the light reflecting layer 22 appears blue within the viewing angle range corresponding to the first direction X under natural light; the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 approaching each other in the second direction Y can be equal to 530nm, and at this time, the photonic crystal of the light reflecting layer 22 appears green within the viewing angle range corresponding to the second direction Y under natural light.

[0145] Of course, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 in the first direction X can be substantially equal to the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 in the second direction Y, so that the light reflecting layer 22 presents the same color at different viewing angles under natural light.

[0146] like Fig.11 As shown in (b), the spacing distances D1 and D5 between the edges of two adjacent first dielectric bodies 221 that are close to each other are both equal to 530nm. If the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 that are close to each other increases to 630nm under the action of external tension, as shown in Fig.11 As shown in (c), the light reflecting layer 22 shows a red structural color in the viewing angle range corresponding to the first direction X under natural light; or, if the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 approaching each other is reduced to 450nm under the action of external pressure, as shown in Fig.11As shown in (a), the light reflecting layer 22 exhibits a blue structural color in the viewing angle range corresponding to the first direction X under natural light. At the same time, if the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 approaching each other increases to 630nm under the action of external tension, the light reflecting layer 22 exhibits a red structural color in the viewing angle range corresponding to the second direction Y under natural light; or, if the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 approaching each other decreases to 450nm under the action of external pressure, the light reflecting layer 22 exhibits a blue structural color in the viewing angle range corresponding to the second direction Y under natural light.

[0147] Regardless of whether the photonic crystal is a one-dimensional structure or a two-dimensional structure. When the structural color of the light-reflecting layer 22 shows blue, when the light-reflecting layer 22 is subjected to external pressure and D1 is reduced, the color presented by the light-reflecting layer 22 exceeds the range of visible light and cannot be distinguished by the human eye. Only when the light-reflecting layer 22 is subjected to external tension and D1 is expanded, the light-reflecting layer 22 shows green, yellow or red, so that the human eye can determine that the sensing film 100 is subjected to external tension by identifying the color of the light-reflecting layer 22. Similarly, when the structural color of the light-reflecting layer 22 shows red, when the light-reflecting layer 22 is subjected to external pressure and D1 is expanded, the color presented by the light-reflecting layer 22 exceeds the range of visible light and cannot be distinguished by the human eye. Only when the light-reflecting layer 22 is subjected to external pressure and D1 is reduced, the light-reflecting layer 22 shows yellow, green or blue, so that the human eye can determine that the sensing film 100 is subjected to external pressure by identifying the color of the light-reflecting layer 22.

[0148] When the structural color of the light reflecting layer 22 is green or yellow, the human eye can determine that the light reflecting layer 22 is subjected to external pressure and D1 is reduced by discerning that the light reflecting layer 22 appears blue; and the human eye can determine that the light reflecting layer 22 is subjected to external pressure and D1 is expanded by discerning that the light reflecting layer 22 appears red.

[0149] Therefore, when the structural color of the light reflecting layer 22 shows green and / or yellow, the sensing film can detect external pressure and external tension at the same time, which can increase the diversity of the sensing film 100 sensing external stress and expand the application scenarios of the sensing film 100.

[0150] It should be noted that due to the characteristics of the cross-linking degree of the flexible substrate layer 21, when the light reflective layer 22 is subjected to external stress causing D1 and / or D2 in the light reflective layer 22 to change, so that the structural color presented by the light reflective layer 22 changes, the flexible substrate layer 21 can make the structural color presented by the light reflective layer 22 after the change of D1 and / or D2 be maintained for 10min-20min. Afterwards, the flexible substrate layer 21 drives D1 and / or D2 of the light reflective layer 22 to be restored to the previous D1 and / or D2, and the structural color of the light reflective layer 22 can be restored to the structural color presented before. By maintaining the structural color presented by the light reflective layer 22 after the change of the cross-linking degree of the flexible substrate layer 21, it is convenient to record the stress-bearing parts of the electronic equipment in the mechanical reliability test, and whether each stress-bearing part is subjected to tensile stress or compressive stress, through the color distribution of the sensing film.

[0151] In this way, the sensing film 100 can repeatedly perform mechanical reliability tests on different electronic devices or components to be tested, so as to record the external stress conditions to which the electronic devices or components to be tested are subjected.

[0152] In some other feasible implementations, the light reflecting layer 22 may further include a plurality of functional sublayers stacked along the third direction Z, each functional sublayer including a first dielectric body and a second dielectric body. The structure of the functional sublayer is similar to that of the above-mentioned one-dimensional photonic crystal or two-dimensional photonic crystal, and will not be described in detail here.

[0153] Fig.12 A schematic diagram of the structure of the sensing functional layer provided in some embodiments of the present application after being attached to the surface of the electronic device to be tested; Fig.13 It is a schematic diagram of the structure of one side surface of the electronic device to be tested.

[0154] The sensing function layer 20 with the release paper 10 and the protective film 30 removed is attached to the surface of the electronic device to be tested. The initial structural color of the sensing function layer 20 is green. Through the reliability test of the electronic device to be tested, it can be found that the sensing function layer 20 is Fig.12 The position of the middle circle is shown in blue, and the sensing functional layer 20 is Fig.12 The location of the middle oval is shown in red.

[0155] It can be understood that in the circular part of the sensing functional layer 20, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 close to each other becomes narrower, and the structural color of the sensing functional layer 20 in the part covering the circle changes from green to blue. The human eye can judge that the sensing functional layer 20 is subjected to compressive stress in the part covering the circle based on the color change of this part. Similarly, in the elliptical part of the sensing functional layer 20, the spacing distance D1 between the edges of two adjacent first dielectric bodies 221 close to each other becomes wider, and the structural color of the sensing functional layer 20 in the part covering the elliptical part changes from green to red. The human eye can judge that the sensing functional layer 20 is subjected to tensile stress in the part covering the elliptical protrusion based on the color change of this part.

[0156] Finally Fig.13 As shown, after the sensing functional layer 20 is torn off, it can be found that the surface of the electronic device to be tested includes a circular concave portion and an elliptical convex portion.

[0157] In summary, after the sensing functional layer 20 of the sensing film 100 provided by the embodiment of the present application is attached to the surface of the electronic device or the component to be tested, the human eye and the machine can determine the corresponding compressive stress or tensile stress of each part on the sensing functional layer 20 through the change of the structural color presented at each part of the sensing functional layer 20, thereby improving the convenience of detecting the surface external stress of the electronic device or the component to be tested; at the same time, the sensing film 100 has been described as having the characteristics of good sensitivity, thin thickness and strong applicability. Therefore, the sensing film 100 provided by the embodiment of the present application has a better effect of recording the stress conditions of each part of the electronic device in the mechanical reliability test.

[0158] The embodiment of the present application further provides a test assembly of an electronic device. The test assembly of an electronic device may include a driving mechanism, an identification mechanism, and a sensing film. The sensing film may be the sensing film 100 provided in any of the above embodiments.

[0159] The electronic device may be a laptop computer, a mobile phone, a smart phone, a tablet computer, a smart vehicle-mounted device, a navigator, a sports camera, a smart home appliance, an artificial intelligence device, a wearable device, or a virtual reality / augmented reality / mixed reality device, etc., and the embodiments of the present application are not limited to this.

[0160] The driving mechanism may include a mechanism for performing a mechanical reliability test on the electronic device. For example, the driving mechanism may include a mechanism for performing a roller test on the electronic device; and / or, the driving mechanism may include a mechanism for performing a drop test on the electronic device. Of course, the driving mechanism may also be other mechanisms capable of performing a mechanical reliability test on the electronic device, which is not limited here.

[0161] After the release paper 10 and the protective film 30 are removed from the sensing film 100, the sensing film 100 is attached to the surface of the electronic device and / or the component to be tested. The electronic device with the sensing film attached is placed on a driving mechanism so that the driving mechanism performs a mechanical reliability test on the electronic device.

[0162] After the mechanical reliability test is completed, the color displayed by the recognition mechanism sensing functional layer 20 can be used to determine the stress-bearing parts of the electronic device and / or the component to be tested, and whether the stress at each stress-bearing part is tensile stress or compressive stress.

[0163] To summarize, the test assembly of the electronic device provided in the embodiment of the present application, the identification mechanism can determine the stress-bearing parts of the electronic device and / or the component to be tested, and whether the stress at each stress-bearing part is tensile stress or compressive stress by sensing the changes in the structural color presented at various parts of the functional layer 20, thereby improving the convenience of detecting the surface external stress of the electronic device to be tested or the component to be tested, and facilitating the recording of the stress conditions of various parts of the electronic device during the mechanical reliability test.

[0164] The embodiment of the present application also provides a method for manufacturing a sensing film. The method for manufacturing the sensing film can be performed by nanoimprinting, and the sensing functional layer 20 provided in any of the above embodiments can be obtained by the manufacturing method.

[0165] Fig.14 A schematic diagram of the manufacturing process of the sensing film provided in some embodiments of the present application.

[0166] First, a hard template X1 can be manufactured. The hard template X1 may include a rigid material, and the rigid material may include metal, ceramic, glass, quartz, a hard polymer material, etc., which is not limited here. The hard template X1 can be prepared by masking and electron beam etching the rigid material, and of course, it can also be prepared by other suitable methods, which is not limited here.

[0167] like Fig.14 As shown, the hard template X1 may include a base portion and a protrusion. The protrusion may be located on one side of the base portion, and the protrusion includes a plurality of protrusion sub-portions. In some examples, each protrusion sub-portion may be a long strip structure extending along the second direction Y, and the plurality of protrusion sub-portions may be a one-dimensional structure arranged at intervals along the first direction X. In other examples, the plurality of protrusion sub-portions may be a block structure, and the plurality of protrusion sub-portions may be a two-dimensional structure arranged at intervals along the first direction X and along the second direction Y.

[0168] After the hard template is manufactured, the hard template can be used to emboss the first dielectric material to be formed, so that the first dielectric material to be formed can be formed. Afterwards, the formed first dielectric material can be cured, so that the cured first dielectric material forms the sensing function layer 20 .

[0169] Exemplarily, the first dielectric material to be molded may include liquid resin.

[0170] In some possible implementations, such as Fig.14 As shown, before the hard template X1 is used to imprint the first dielectric material to be formed, a substrate X2 may be provided. The substrate X2 may include a rigid substrate, such as a quartz substrate, a glass substrate, etc., which is not limited here.

[0171] The first dielectric material X3 to be formed is coated on the substrate X2, and then the protrusion of the hard template X1 faces the first dielectric material X3 to be formed and the hard template X1 is pressed into the first dielectric material X3 to be formed, so that the first dielectric material X3 to be formed is formed on the substrate to form a first dielectric material layer that matches the shape of the hard template X1. The coating of the first dielectric material to be formed can be specifically carried out by at least one of spin coating, spray coating, scraping coating or drip coating.

[0172] Afterwards, the first dielectric material layer formed on the substrate X2 is cured, and the substrate X2 is removed from the cured first dielectric material layer to form a first dielectric body 221, which has a periodic structure. Specifically, the curing of the molding material layer can be performed by ultraviolet (UV) light curing or thermal curing. When UV light is used to cure the molding material layer, the hard template can include a light-transmitting material such as glass.

[0173] Afterwards, the second dielectric body may be filled in the gaps of the periodic structure of the first dielectric body 221 to form the sensing functional layer 20. The shape of the second dielectric body 222 in the sensing functional layer 20 may be adapted to the shape of the protrusions in the hard template.

[0174] For example, Fig.14 The sensing functional layer 20 formed above is a sensing functional layer 20 with air as the second dielectric body 222. In some other examples, the first dielectric material layer formed after curing is used as the first dielectric body 221, and the second dielectric body 222 can be formed after the first dielectric body 221 is formed, so that the first dielectric body 221 and the second dielectric body 222 together form the light reflection layer 22 of the sensing functional layer 20.

[0175] It can be understood that when the multiple protrusions on the hard template form a one-dimensional structure, the light reflection layer 22 formed by the hard template is also a one-dimensional structure of the corresponding shape. Similarly, when the multiple protrusions on the hard template form a two-dimensional structure, the light reflection layer 22 formed by the hard template is also a two-dimensional structure of the corresponding shape.

[0176] Fig.15Schematic diagram of the manufacturing process of the sensing film provided in other embodiments of the present application.

[0177] In some possible implementations, such as Fig.15 As shown, the first dielectric material X3 to be formed can also be directly coated on the base of the hard template X1 and cover the protrusions, so that the first dielectric material X3 to be formed is formed on the hard template X1 to form a formed first dielectric material layer that matches the shape of the hard template X1.

[0178] Afterwards, the first dielectric material layer formed on the hard template X1 is cured, and after the hard template X1 is removed from the cured first dielectric material layer, a first dielectric body 221 is formed, and the first dielectric body 221 has a periodic structure. Specifically, the first dielectric material layer can be cured by ultraviolet (UV) light curing or thermal curing. When UV light is used to cure the molded material layer, the hard template can include a light-transmitting material such as glass.

[0179] Afterwards, the second dielectric body may be filled in the gaps of the periodic structure of the first dielectric body 221 to form the sensing functional layer 20. The shape of the second dielectric body 222 in the sensing functional layer 20 may be adapted to the shape of the protrusions in the hard template.

[0180] For example, Fig.15 The sensing functional layer 20 formed above is a sensing functional layer 20 with air as the second dielectric body 222. In some other examples, the first dielectric material layer formed after curing is used as the first dielectric body 221, and the second dielectric body 222 can be formed after the first dielectric body 221 is formed, so that the first dielectric body 221 and the second dielectric body 222 together form the light reflection layer 22 of the sensing functional layer 20.

[0181] It can be understood that when multiple protrusions on the hard template X1 form a one-dimensional structure, the light reflection layer 22 formed using the hard template X1 is also a one-dimensional structure of corresponding shape. Similarly, when multiple protrusions on the hard template X1 form a two-dimensional structure, the light reflection layer 22 formed using the hard template X1 is also a two-dimensional structure of corresponding shape. One set of hard templates X1 can form a sensing functional layer 20 presenting one initial structural color, and multiple sets of hard templates X1 can respectively form sensing functional layers 20 presenting multiple initial structural colors.

[0182] The sensing functional layer 20 obtained by embossing the hard template X1, the first dielectric body 221 and the flexible base layer 21 may include the same material. For example, the first dielectric body 221 and the flexible base layer 21 are both made of the first dielectric material to be formed, and the first dielectric body 221 and the flexible base layer 21 are an integrated structure connected to each other.

[0183] The method of imprinting the first dielectric material to be formed by the hard template X1 so that the first dielectric material to be formed X3 is formed and forms a sensing film can improve the stability of the shape and spacing of each first dielectric body 221 on the sensing film, and obtain a sensing film with excellent sensing performance. In addition, the method has simple process and low cost, and can facilitate large-scale production of sensing films.

[0184] In some embodiments, Fig.16 An optical disc and a local one-dimensional photonic crystal structure of the optical disc are shown. Scanning electron microscope (SEM) can be used to find that the local structure of the optical disc has a one-dimensional photonic crystal structure. Using the local structure of the optical disc as the above-mentioned hard template X1, PDMS (such as Corning DC184 PDMS) AB glue as the substrate (wherein A glue and B glue are mixed in a ratio of 10:1), thermal curing is adopted for curing, and the curing temperature is 150°C. A sensing functional layer 20 with a one-dimensional photonic crystal structure can be produced, and the initial structural color of the sensing functional layer 20 can be green.

[0185] Fig.17 A schematic diagram of a manufacturing process of a sensing film provided in other embodiments of the present application; Fig.18 for Fig.17 A top view of a sensing film manufactured by the sensing film manufacturing method shown.

[0186] First, if Fig.17 As shown, the flexible substrate layer 21 can be made by coating a flexible substrate material. The flexible substrate layer 21 may include a soft polymer material. Exemplarily, the flexible substrate layer 21 may include one or more of polydimethylsiloxane, thermoplastic polyurethane elastomer, thermoplastic elastomer, thermoplastic polyester elastomer, polyacrylates with long-chain alkyl side chains, and rubber polymers, which are not limited here. In this way, the flexible substrate layer can have good flexibility and stretchability.

[0187] After the flexible substrate 21 is manufactured, Fig.17 As shown, an ink jet printing process (IJP) can also be used to print a plurality of ink droplets X5 on the flexible substrate layer 21. The plurality of ink droplets X5 can be arranged at intervals from each other at least along the first direction.

[0188] The ink droplet X5 may include one or more of microsphere emulsion, moisturizing agent (such as ethylene glycol), surfactant, and deionized water. In addition, the ink droplet X5 may also include other suitable materials, which are not limited here.

[0189] The microsphere emulsion may include monodisperse polymer materials (such as polystyrene (PS)), metal materials, ceramic materials (such as silicon dioxide SiO2) and other suitable materials, which are not limited here. In addition, the proportion of deionized water in the ink droplet X5 can adjust the viscosity between the ink droplet X5 and the flexible substrate layer 21.

[0190] The microspheres in the ink droplet X5 react with the flexible base layer 21 and are fixed on the flexible base layer 21 , thereby forming a plurality of first dielectric bodies 221 arranged at intervals from each other at least along a first direction on the flexible base layer 21 .

[0191] It should be noted that the orderly spacing between the multiple ink droplets X5 printed on the flexible substrate layer 21 can be achieved by inducing the formation of non-covalent interaction forces through the evaporation of the solvent in the ink droplets X5. The non-covalent interaction force is a force that is spontaneously formed between the ink droplets X5 due to thermodynamic reasons, and can automatically achieve the orderly spacing between the multiple ink droplets X5 without the help of other external forces.

[0192] The size of the first dielectric body 221 in the first direction X may be between 100 nm and 1000 nm. For example, the size of the first dielectric body 221 in the first direction X may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm, or 1000 nm. Similarly, the size of the first dielectric body 221 in the second direction Y may also be between 100 nm and 1000 nm. For example, the size of the first dielectric body 221 in the second direction Y may be 100 nm, 200 nm, 300 nm, 400 nm, 500 nm, 600 nm, 700 nm, 800 nm, 900 nm, or 1000 nm.

[0193] A plurality of first dielectric bodies 221 may form a two-dimensional structure extending along the first direction X and along the second direction Y. Fig.18 As shown, the plurality of first dielectric bodies 221 close to each other may be arranged in a rectangular shape, in a regular triangle shape, or in a regular hexagon shape.

[0194] The spacing between the edges of two adjacent first dielectric bodies 221 on the flexible base layer 21 that are close to each other will decrease due to the contraction of the flexible base layer 21 , and will also increase due to the extension of the flexible base layer 21 .

[0195] For example, when the sensing film is subjected to external tension, the portion of the flexible substrate layer subjected to the external tension stretches in the first direction X. When the distance D1 between the edges of the two adjacent first dielectric bodies 221 is increased to 630 nm, the sensing film exhibits a red structural color in the viewing angle range corresponding to the first direction X under natural light. Alternatively, when the sensing film is subjected to external pressure, the portion of the flexible substrate layer subjected to the external pressure shrinks in the first direction X. When the distance D1 between the edges of the two adjacent first dielectric bodies 221 is reduced to 450 nm, the sensing film exhibits a blue structural color in the viewing angle range corresponding to the first direction X under natural light. At the same time, when the sensing film is subjected to external tension, the portion of the flexible base layer subjected to the external tension stretches in the second direction Y, and when the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 close to each other increases to 630nm, the sensing film exhibits a red structural color in the viewing angle range corresponding to the second direction Y under natural light; or, when the sensing film is subjected to external tension, the portion of the flexible base layer subjected to external pressure shrinks in the second direction Y, and when the spacing distance D5 between the edges of two adjacent first dielectric bodies 221 close to each other decreases to 450nm, the sensing film exhibits a blue structural color in the viewing angle range corresponding to the second direction Y under natural light.

[0196] The method of forming a sensing film by printing ink droplets on a flexible substrate layer by IJP can adjust the distance between multiple ink droplets on the flexible substrate layer by controlling the spacing degree of the solvent volatilization in the ink droplets to induce self-assembly, thereby adjusting the distance between multiple first dielectric bodies. It has the advantage of easy adjustment of the initial structural color of the sensing film, and can produce sensing films with different initial structural colors according to actual needs. In addition, the method does not require an additional hard template, which can reduce the cost of the hard template in the process of manufacturing the sensing film, thereby reducing the manufacturing cost of the sensing film.

[0197] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.

[0198] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.

Claims

1. A sensing film, characterized in that: include: A flexible base layer; A light reflecting layer is located on one side of the flexible base layer; the light reflecting layer includes a plurality of first dielectric bodies and a second dielectric body, the plurality of first dielectric bodies are arranged at intervals from each other at least along a first direction, and the second dielectric body is located between two adjacent first dielectric bodies; the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, and the first direction is parallel to the flexible base layer.

2. The sensing film according to claim 1, characterized in that: The plurality of first dielectric bodies are also arranged in a spaced relationship from one another along a second direction, and the second direction is parallel to the flexible base layer and intersects with the first direction.

3. The sensing film according to claim 1 or 2, characterized in that: In the first direction, a spacing distance D1 between two adjacent edges of the first dielectric bodies that are close to each other satisfies 100 nm ≤ D1 ≤ 1000 nm; and / or, In the first direction, a size D2 of the first dielectric body satisfies 100 nm≤D2≤1000 nm.

4. The inductive film according to any one of claims 1 to 3, characterized in that: In a direction perpendicular to the flexible base layer, a dimension D3 of the first dielectric body satisfies D3≤1 mm; and / or, In a direction perpendicular to the flexible base layer, a dimension D4 of the second dielectric body satisfies D4≤1 mm.

5. The inductive film according to any one of claims 1 to 4, characterized in that: The shape of the first dielectric body includes at least one of a regular polygon, a rectangular body, a hemispherical body, a spherical body, a rhombus body, and an ellipsoidal body.

6. The inductive film according to any one of claims 1 to 5, characterized in that: The second medium includes air.

7. The inductive film according to any one of claims 1 to 6, characterized in that: The structural colors displayed by the sensing film include green and / or yellow.

8. The inductive film according to any one of claims 1 to 7, characterized in that: Also includes: A release paper is located on a side of the flexible base layer away from the light reflecting layer and is attached to the flexible base layer; and / or, The protective film is located on a side of the light reflecting layer away from the flexible base layer and is attached to the light reflecting layer.

9. The inductive film according to any one of claims 1 to 8, characterized in that: The flexible base layer and the first dielectric body include the same material and are connected in an integral structure.

10. The inductive film according to any one of claims 1 to 9, characterized in that: The flexible base layer includes one or more of polydimethylsiloxane, thermoplastic polyurethane elastomer, thermoplastic elastomer, thermoplastic polyester elastomer, polyacrylate with long-chain alkyl side chain and rubber polymer.

11. A method for manufacturing a sensing film, characterized in that: The method comprises: Provide hard templates; The hard template is used to shape the material to be formed to form a sensing film; the sensing film includes a flexible base layer and a light reflecting layer located on one side of the flexible base layer; the light reflecting layer includes a plurality of first dielectric bodies and a second dielectric body, the plurality of first dielectric bodies are arranged at intervals from each other at least along a first direction, and the second dielectric body is located between two adjacent first dielectric bodies; the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, and the first direction is parallel to the flexible base layer.

12. The method according to claim 11, characterized in that The method of using the hard template to shape the material to be formed into a sensing film includes: providing a substrate; coating a first dielectric material to be formed on the substrate; Using the hard template to emboss the first dielectric material to be formed, so as to form a first dielectric material layer that matches the shape of the hard template; curing the formed first dielectric material layer; After the formed first dielectric material layer is solidified, the substrate is removed to form a first dielectric body, wherein the first dielectric body has a periodic structure; A second dielectric body is filled in the gaps of the periodic structure to form a sensing film.

13. The method according to claim 11, characterized in that The method of using the hard template to shape the material to be formed into a sensing film includes: Coating a first dielectric material to be formed on the hard template to form a formed first dielectric material matching the shape of the hard template; curing the formed first dielectric material; After the molded first dielectric material is solidified, the hard template is removed to form a first dielectric body, wherein the first dielectric body has a periodic structure; A second dielectric body is filled in the gaps of the periodic structure to form a sensing film.

14. A method for manufacturing a sensing film, characterized in that: The method comprises: forming a flexible base layer; A plurality of first dielectric bodies arranged at intervals from each other at least along a first direction and a second dielectric layer located between two adjacent first dielectric bodies are formed on the flexible base layer to form a light reflecting layer, and the flexible base layer and the light reflecting layer together constitute a sensing film; the refractive index of the first dielectric body is different from the refractive index of the second dielectric body, and the first direction is parallel to the flexible base layer.

15. The method according to claim 14, characterized in that The method of forming a plurality of first dielectric bodies spaced apart from each other at least along a first direction on the flexible base layer comprises: A plurality of ink droplets are printed on the flexible base layer, and the plurality of ink droplets are arranged at intervals from each other at least along a first direction to form a plurality of first medium bodies on the flexible base layer.

16. An electronic equipment testing assembly, characterized in that: include: The sensing film is the sensing film according to any one of claims 1 to 10; The sensing film is used to adhere to the outer surface of the electronic device and / or the outer surface of the internal components of the electronic device; The identification mechanism is used to identify the color on the sensing film after the electronic device completes the mechanical reliability test.