Hot melting drill machining extrusion force prediction method and equipment based on needle type extrusion and medium
By quickly predicting the extrusion pressure in hot melt drilling processing based on the material elastic-plastic mechanics and spherical centripetal continuous velocity field theory, the problem of low calculation time and accuracy in the prior art is solved, and the hot melt drilling processing is realized The squeeze pressure during the process is predicted quickly and accurately.
Patent Information
- Application Number
- CN202411154373.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-12-03
AI Technical Summary
During hot melt drilling processing, existing finite element methods require a lot of pre-processing when calculating extrusion pressure, which takes a long time, making it difficult to quickly and accurately predict extrusion pressures for different processing materials and process parameters, especially in micropore processing The tool breakage occurs.
Based on the material's elastic-plastic mechanics theory and spherical centripetal continuous velocity field theory, combined with the needle extrusion stress theory, the average strain speed and deformation resistance of the processed material are calculated by obtaining the structure of the hot melt drill tool, processing process parameters and cooling and lubrication factors. and friction factor to determine the extrusion stress state coefficient, and then quickly predict the extrusion pressure during hot melt drilling processing.
The tedious pre-processing steps in the finite element method are avoided, and the fast and accurate prediction of extrusion pressure in hot melt drilling is achieved, which reduces the calculation time and improves the prediction accuracy.
Smart Images

Figure CN119066810A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of mechanical processing technology, and in particular to a method, device and medium for predicting extrusion force of hot melt drilling processing based on needle extrusion. Background Art
[0002] The melt drill process refers to the process of using a high-speed rotating melt drill to contact the surface of the product and apply downward axial pressure. The melt drill head rubs against the metal and generates high temperature, causing the processed material in the vicinity to soften rapidly. While the melt drill squeezes and penetrates, it stretches the softened material into a boss.
[0003] During the melt drilling process, accompanied by severe extrusion pressure and friction heat, melt drill tool breakage often occurs, especially when hot melt processing is performed on micro-holes. Therefore, during the design of the melt drill, it is necessary to calibrate the tool strength for different processing materials and process parameters, and the calibration calculation requires reliable extrusion pressure data. During the melt drilling process, the extrusion pressure on the tool is different under different tool structures, process parameters and cooling and lubrication factors. The existing finite element method often requires a lot of pre-processing when calculating the extrusion pressure, and it takes a considerable amount of time. Therefore, it is necessary to propose a set of standardized extrusion pressure calculation methods to quickly solve the extrusion force prediction problem in melt drilling processing. Summary of the invention
[0004] The purpose of the present application is to provide a method, device and medium for predicting the extrusion force of a hot melt drill processing based on needle extrusion, which can quickly and accurately predict the extrusion force during the hot melt drill processing.
[0005] To achieve the above objectives, this application provides the following solutions:
[0006] In a first aspect, the present application provides a method for predicting extrusion force of hot melt drilling processing based on needle extrusion, comprising:
[0007] Obtain the melt drill tool structure, processing parameters and processing cooling and lubrication factors;
[0008] Based on the material elastic-plastic mechanics theory, the average strain velocity of the processed material is determined according to the hot melt drill tool structure and processing parameters;
[0009] Based on the strain velocity coefficient diagram of material deformation resistance, the deformation resistance of the processed material is determined according to the average strain velocity of the processed material and the processing parameters;
[0010] Based on the assumption that the friction stress on the contact surface is uniformly distributed, the friction factor between the hot melt drill and the processed material is determined according to the processing cooling and lubrication factors;
[0011] Based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters.
[0012] Based on the needle extrusion stress theory, the axial extrusion force on the tool during the hot melt drilling process is determined according to the extrusion stress state coefficient of the processed material, deformation resistance and hot melt drill tool structure.
[0013] Optionally, based on the material elastic-plastic mechanics theory, the average strain velocity of the processed material is determined according to the melt drill tool structure and processing parameters, specifically including:
[0014] According to the hot melt drill tool structure, the extrusion deformation ratio λ of the processed material is calculated, and the formula ε e =lnλ Calculate the average true extension strain ε of the processed material e ;
[0015] According to the hot melt drill tool structure and processing parameters, the formula is used Calculate the time t that the hot melt drill stays in the processing area s ; where α is the working cone angle of the hot melt drill tool, D t is the maximum diameter of the hot melt drill working cone section, d is the maximum diameter of the hot melt drill pressing cone section, V j is the axial feed speed of the hot melt drill;
[0016] According to the average true extension strain ε of the processed material e and the time t that the hot melt drill stays in the processing area s , using the formula Calculate the average strain rate of the processed material
[0017] Optionally, based on the strain velocity coefficient diagram of the material deformation resistance, the deformation resistance of the processed material is determined according to the average strain velocity of the processed material and the processing parameters, specifically including:
[0018] According to the average strain velocity of the processed material and the processing parameters, the strain velocity coefficient Cv of the processed material is determined from the strain velocity coefficient diagram of the material deformation resistance;
[0019] According to the strain velocity coefficient Cv of the processed material, the formula σ k =C v σ s Calculate the deformation resistance σ of the processed material k ; Among them, σ s It is the yield stress of the processed material when it is statically stretched at the deformation temperature.
[0020] Optionally, the melt drill tool structure includes a pressing cone section, a working cone section and a transition cone section; the pressing cone section is a cone section where the melt drill extrudes the material to plastically deform after contacting the material to be processed, and includes a drill tip portion and a main body portion; the working cone section is a cone section where the melt drill contacts the material to be processed to form a processing surface; the transition cone section is a cone section connecting the working cone section and the melt drill clamping portion; the friction factor between the melt drill and the material to be processed specifically includes: a friction factor m between the material to be processed in the processing area and the pressing cone section of the melt drill, a friction factor m between the material to be processed in the processing area and the working cone section of the melt drill t and the friction factor m between the material being processed and the transition cone section of the hot melt drill in the processing area d .
[0021] Optionally, based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters, specifically including:
[0022] According to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and processing parameters, the formula Calculate the extrusion stress state coefficient n of the processed material σ ; Among them, m, m t and m d are the friction factors between the hot melt drill and the processed material, L t The maximum length of relative motion between the hot melt drill tool and the material being processed, l d is the axial length of the hot melt drill pressed into the cone section, α is the hot melt drill tool working cone angle, β is the prefabricated cone angle of the workpiece, t t is the difference between the maximum radius of the hot melt drill working cone section and the maximum radius of the drill tip of the pressed cone section, t d It is the difference between the hole diameter of the material being processed and the maximum diameter of the hot melt drill's pressed cone section.
[0023] Optionally, based on the needle extrusion stress theory, the extrusion stress state coefficient of the processed material, the deformation resistance and the hot melt drill tool structure are used to determine the extrusion force on the tool in the axial direction during the hot melt drill processing, specifically including:
[0024] According to the extrusion stress state coefficient n of the processed material σ and the deformation resistance of the processed material σ k , using the formula P = n σ ·σ k Calculate the axial stress P during hot melt drilling;
[0025] According to the structure of the hot melt drill tool, calculate the end area S of the hot melt drill pressed into the cone section;
[0026] According to the axial stress P during the hot melt drilling process and the end area S of the hot melt drill pressed into the cone section, the formula F=P·S is used to calculate the axial extrusion force F exerted on the tool during the hot melt drilling process.
[0027] Optionally, the processing parameters include: hot melt drill processing temperature and hot melt drill axial feed speed.
[0028] Optionally, the machining cooling and lubrication factor is non-lubricated machining or lubricated machining;
[0029] In the case of non-lubricated processing, the friction factor between the hot melt drill and the processed material is:
[0030]
[0031] During lubrication processing, the friction factor between the hot melt drill and the processed material is:
[0032]
[0033] In a second aspect, the present application provides a computer device, comprising: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the method for predicting the extrusion force of hot melt drilling processing based on needle extrusion.
[0034] In a third aspect, the present application provides a computer-readable storage medium having a computer program stored thereon, which, when executed by a processor, implements the method for predicting the extrusion force of hot melt drilling processing based on needle extrusion.
[0035] According to the specific embodiments provided in this application, this application discloses the following technical effects:
[0036] The present application provides a method, device and medium for predicting the extrusion force of melt drill processing based on needle extrusion. The method is based on the material elastic-plastic mechanics theory, and solves the average strain velocity of the processed material according to the melt drill tool structure and processing parameters; based on the strain velocity coefficient diagram of the material deformation resistance, the deformation resistance of the processed material is determined according to the average strain velocity of the processed material and the processing parameters; based on the assumption that the friction stress of the contact surface is uniformly distributed, the friction factor between the melt drill and the processed material is determined according to the processing cooling and lubrication factors; based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the melt drill and the processed material, the melt drill tool structure and the processing parameters. Finally, based on the needle extrusion stress theory, the predicted value of the extrusion force of the melt drill processing is calculated by combining the extrusion stress state coefficient of the processed material, the deformation resistance and the melt drill tool structure. The present application avoids a large number of pre-processing steps in the finite element method, and can quickly and accurately predict the extrusion force during the melt drill processing process. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0038] Figure 1 A flow chart of the method for predicting the extrusion force of hot melt drilling processing based on needle extrusion provided in this application;
[0039] Figure 2 Schematic diagram of the hot melt drill tool outline provided for this application;
[0040] Figure 3 This is a graph showing the measurement results of the extrusion force during hot melt drilling processing provided in this application. DETAILED DESCRIPTION
[0041] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0042] In view of the above-mentioned deficiencies in the prior art, the present application proposes a method, device and medium for predicting the extrusion force of a hot melt drill based on needle extrusion. According to the hot melt drill tool structure, processing parameters and processing cooling and lubrication factors, the extrusion stress state coefficient and deformation resistance of the processed material are calculated, and based on the needle extrusion stress theory, the extrusion force during the hot melt drill processing is quickly and accurately predicted.
[0043] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0044] In an exemplary embodiment, Figure 1 As shown, the present application provides a method for predicting the extrusion force of hot melt drilling based on needle extrusion, which is executed by a computer device, specifically, it can be executed by a computer device such as a terminal or a server alone, or it can be executed by a terminal and a server together, including the following steps 1 to 6. Among them:
[0045] Step 1: Obtain the hot melt drill tool structure, processing parameters and processing cooling and lubrication factors.
[0046] Among them, Figure 2The figure shows the outline of the hot melt drill tool. The hot melt drill is an integral tool, and the tool outline includes three parts, namely, the pressing cone section, the working cone section and the transition cone section. The pressing cone section is the cone section where the hot melt drill squeezes the material to plastically deform after contacting the material to be processed, and includes the drill tip and the main body; the working cone section is the cone section where the hot melt drill contacts the material to be processed to form the processing surface; and the transition cone section is the cone section connecting the working cone section and the hot melt drill clamping part.
[0047] The processing parameters include: hot melt drill processing temperature and hot melt drill axial feed speed. Taking the carbide hot melt drill tool processing TC4 titanium alloy material as an example, the hot melt drill processing temperature is 450°C; the hot melt drill axial feed speed is 25mm / min.
[0048] The machining cooling and lubrication factors include non-lubricated machining and lubricated machining.
[0049] Step 2: Based on the elastic-plastic mechanics theory of materials, determine the average strain velocity of the processed material according to the hot melt drill tool structure and processing parameters.
[0050] Specifically, the extrusion deformation ratio λ (i.e., the ratio of the maximum diameter to the minimum diameter of the main part of the pressed cone section) of the processed material is calculated according to the hot melt drill tool structure, and the formula ε is used. e =lnλ Calculate the average true extension strain ε of the processed material e ; According to the hot melt drill tool structure and processing parameters, the formula is used Calculate the time t that the hot melt drill stays in the processing area s ; where α is the working cone angle of the hot melt drill tool, D t is the maximum diameter of the hot melt drill working cone section, d is the maximum diameter of the hot melt drill pressing cone section, V j is the axial feed speed of the hot melt drill; according to the average true extension strain ε of the processed material e and the time t that the hot melt drill stays in the processing area s , using the formula Calculate the average strain rate of the processed material
[0051] For example, the extrusion deformation ratio λ is calculated to be 3.935 according to the hot melt drill tool structure, and the average true extension strain ε e is 1.370. The time t that the hot melt drill stays in the processing area of TC4 titanium alloy material is calculated. s The average strain velocity of the processed material during hot melt drilling is calculated by applying the elastic-plastic mechanics theory of materials. 1.2436s -1 .
[0052] Step 3: Based on the strain velocity coefficient diagram of the material deformation resistance, determine the deformation resistance of the processed material according to the average strain velocity of the processed material and the processing parameters.
[0053] Specifically, according to the average strain velocity of the processed material and the processing parameters, the strain velocity coefficient Cv of the processed material is determined from the strain velocity coefficient diagram of the material deformation resistance; according to the strain velocity coefficient Cv of the processed material, the formula σ k =C v σ s Calculate the deformation resistance σ of the processed material k ; Among them, σ s It is the yield stress of the processed material when it is statically stretched at the deformation temperature.
[0054] Exemplarily, the average strain velocity is determined Finally, according to the hot melt drilling processing temperature of 450℃, the strain velocity coefficient diagram of the material deformation resistance at this temperature is consulted. The abscissa of the strain velocity coefficient diagram is the average strain velocity. The vertical axis is the strain velocity coefficient Cv, which determines the average strain velocity of the processed material. 1.2436s -1 The strain velocity coefficient Cv is 1.02. For the processed material TC4 titanium alloy, the yield stress σ s is 750Mpa, determine the deformation resistance of the processed material σ k It is 765Mpa.
[0055] Step 4: Based on the assumption that the friction stress on the contact surface is uniformly distributed, the friction factor between the hot melt drill and the processed material is determined according to the processing cooling and lubrication factors.
[0056] The friction factor between the hot melt drill and the processed material specifically includes: the friction factor m between the processed material in the processing area and the hot melt drill pressing cone section, the friction factor m between the processed material in the processing area and the hot melt drill working cone section t and the friction factor m between the material being processed and the transition cone section of the hot melt drill in the processing area d .
[0057] For example, during non-lubricated machining, the friction factor between the hot melt drill and the machined material is: During lubrication processing, the friction factor between the hot melt drill and the processed material is:
[0058] Step 5: Based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters.
[0059] Specifically, based on the spherical centripetal continuous velocity field theory, according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters, the formula is used Calculate the extrusion stress state coefficient n of the processed material σ ; Among them, m, m t and m d are the friction factors between the hot melt drill and the processed material, L t The maximum length of relative motion between the hot melt drill tool and the material being processed, l d is the axial length of the hot melt drill pressed into the cone section, α is the hot melt drill tool working cone angle, β is the prefabricated cone angle of the workpiece, t t is the difference between the maximum radius of the hot melt drill working cone section and the maximum radius of the drill tip of the pressed cone section, t d It is the difference between the hole diameter of the material being processed and the maximum diameter of the hot melt drill's pressed cone section.
[0060] For example, the maximum length L of relative motion between the hot melt drill tool and the material being processed is t The axial length of the hot melt drill pressed into the cone section is l d The difference between the maximum radius of the hot melt drill working cone section and the maximum radius of the drill tip of the pressed cone section is 0.2 mm. t is 0.335 mm, the difference between the processing hole diameter of the processed material and the maximum diameter of the hot melt drill pressed into the cone section t d is 0.25mm. During the extrusion process, the velocity vector of the processed material always points outward from the hot melt drill, which meets the theoretical requirements of the spherical centripetal continuous velocity field. The volume of the processed material remains unchanged during the processing, and the upper limit law can be used to determine the approximate solution of the deformation load according to the kinematic permissible velocity field. In this case, the extrusion stress state coefficient n of the processed material during the hot melt drill processing is calculated σ It is 4.9471.
[0061] Step 6: Based on the needle extrusion stress theory, the extrusion stress state coefficient of the processed material, the deformation resistance and the hot melt drill tool structure are used to determine the axial extrusion force on the tool during the hot melt drill process.
[0062] Specifically, according to the extrusion stress state coefficient n of the processed material σ and the deformation resistance of the processed material σ k , using the formula P = n σ ·σ k Calculate the axial stress P during the hot melt drilling process; calculate the end area S of the hot melt drill pressed into the cone section according to the hot melt drill tool structure; according to the axial stress P during the hot melt drilling process and the end area S of the hot melt drill pressed into the cone section, use the formula F=P·S to calculate the axial extrusion force F exerted on the tool during the hot melt drilling process.
[0063] For example, according to the needle extrusion stress theory, the axial stress P during the hot melt drilling process is calculated to be 3.785 GPa. According to the hot melt drilling tool structure, the axial extrusion force F=P·S during the hot melt drilling process is solved, and the axial extrusion force on the tool is calculated to be 695.8N.
[0064] In summary, the extrusion force prediction of TC4 titanium alloy material processed by cemented carbide hot melt drilling is completed.
[0065] According to the above example processing environment, experimental verification is carried out and the following results are obtained: Figure 3 The axial force test data shown in the figure shows that the maximum axial forces detected are 739N, 734N, 724N, 704N, 745N, and 725N, respectively, with errors of 5.85%, 5.20%, 3.9%, 1.16%, 6.6%, and 4.03% compared with the predicted results. The average cutting force of the machining test is 728.5N, with an error of 4.49% compared with the predicted results.
[0066] In an exemplary embodiment, the present application further provides a computer device, including a memory and a processor, wherein a computer program is stored in the memory, and the processor implements the steps in the above-mentioned method embodiments when executing the computer program.
[0067] In an exemplary embodiment, the present application further provides a computer-readable storage medium storing a computer program, which implements the steps in the above-mentioned method embodiments when executed by a processor.
[0068] In an exemplary embodiment, the present application further provides a computer program product, including a computer program, which implements the steps in the above-mentioned method embodiments when executed by a processor.
[0069] It should be noted that the user information (including but not limited to user device information, user personal information, etc.) and data (including but not limited to data used for analysis, stored data, displayed data, etc.) involved in this application are all information and data authorized by the user or fully authorized by all parties, and the collection, use and processing of relevant data must comply with relevant regulations.
[0070] Those skilled in the art can understand that all or part of the processes in the above-mentioned embodiment methods can be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to the memory, database or other medium used in the embodiments provided in the present application can include at least one of non-volatile and volatile memory. Non-volatile memory can include read-only memory (ROM), magnetic tape, floppy disk, flash memory, optical memory, high-density embedded non-volatile memory, resistive random access memory (ReRAM), magnetic random access memory (MRAM), ferroelectric random access memory (FRAM), phase change memory (PCM), graphene memory, etc. Volatile memory can include random access memory (RAM) or external cache memory, etc. By way of illustration and not limitation, RAM may be in various forms, such as static random access memory (SRAM) or dynamic random access memory (DRAM).
[0071] The database involved in each embodiment provided in this application may include at least one of a relational database and a non-relational database. The non-relational database may include a distributed database based on blockchain, etc., but is not limited thereto. The processor involved in each embodiment provided in this application may be a general-purpose processor, a central processing unit, a graphics processor, a digital signal processor, a programmable logic device, a data processing logic device based on quantum computing, etc., but is not limited thereto.
[0072] The technical features of the above embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0073] This article uses specific examples to illustrate the principles and implementation methods of this application. The description of the above embodiments is only used to help understand the method and core ideas of this application. At the same time, for those skilled in the art, according to the ideas of this application, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting this application.
Claims
1. A method for predicting the extrusion force of hot melt drilling based on needle extrusion, characterized in that: include: Obtain the melt drill tool structure, processing parameters and processing cooling and lubrication factors; Based on the material elastic-plastic mechanics theory, the average strain velocity of the processed material is determined according to the hot melt drill tool structure and processing parameters; Based on the strain velocity coefficient diagram of material deformation resistance, the deformation resistance of the processed material is determined according to the average strain velocity of the processed material and the processing parameters; Based on the assumption that the friction stress on the contact surface is uniformly distributed, the friction factor between the hot melt drill and the processed material is determined according to the processing cooling and lubrication factors; Based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters. Based on the needle extrusion stress theory, the axial extrusion force on the tool during the hot melt drilling process is determined according to the extrusion stress state coefficient of the processed material, deformation resistance and hot melt drill tool structure.
2. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: Based on the material elastic-plastic mechanics theory, the average strain velocity of the processed material is determined according to the hot melt drill tool structure and processing parameters, including: According to the hot melt drill tool structure, the extrusion deformation ratio λ of the processed material is calculated, and the formula ε e =lnλ Calculate the average true extension strain ε of the processed material e ; According to the hot melt drill tool structure and processing parameters, the formula is used Calculate the time t that the hot melt drill stays in the processing area s ; Among them, α is the working cone angle of the hot melt drill tool, D t is the maximum diameter of the hot melt drill working cone section, d is the maximum diameter of the hot melt drill pressing cone section, V j is the axial feed speed of the hot melt drill; According to the average true extension strain ε of the processed material e and the time t that the hot melt drill stays in the processing area s , using the formula Calculate the average strain rate of the processed material 3. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: Based on the strain velocity coefficient diagram of material deformation resistance, the deformation resistance of the processed material is determined according to the average strain velocity of the processed material and the processing parameters, including: According to the average strain velocity of the processed material and the processing parameters, the strain velocity coefficient Cv of the processed material is determined from the strain velocity coefficient diagram of the material deformation resistance; According to the strain velocity coefficient Cv of the processed material, the formula σ k =C v σ s Calculate the deformation resistance σ of the processed material k ; Among them, σ s It is the yield stress of the processed material when it is statically stretched at the deformation temperature.
4. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: The melt drill tool structure includes a pressing cone section, a working cone section and a transition cone section; the pressing cone section is a cone section where the melt drill extrudes the material to plastically deform after contacting the material to be processed, and includes a drill tip portion and a main body portion; the working cone section is a cone section where the melt drill contacts the material to be processed to form a processing surface; the transition cone section is a cone section connecting the working cone section and the melt drill clamping portion; the friction factor between the melt drill and the material to be processed specifically includes: the friction factor m between the material to be processed in the processing area and the pressing cone section of the melt drill, the friction factor m between the material to be processed in the processing area and the working cone section of the melt drill t and the friction factor m between the material being processed and the transition cone section of the hot melt drill in the processing area d .
5. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: Based on the spherical centripetal continuous velocity field theory, the extrusion stress state coefficient of the processed material is determined according to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and the processing parameters, including: According to the friction factor between the hot melt drill and the processed material, the hot melt drill tool structure and processing parameters, the formula Calculate the extrusion stress state coefficient n of the processed material σ ; Among them, m, m t and m d are the friction factors between the hot melt drill and the processed material, L t The maximum length of relative motion between the hot melt drill tool and the material being processed, l d is the axial length of the hot melt drill pressed into the cone section, α is the hot melt drill tool working cone angle, β is the prefabricated cone angle of the workpiece, t t is the difference between the maximum radius of the hot melt drill working cone section and the maximum radius of the drill tip of the pressed cone section, t d It is the difference between the hole diameter of the material being processed and the maximum diameter of the hot melt drill's pressed cone section.
6. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: Based on the needle extrusion stress theory, the extrusion stress state coefficient of the processed material, the deformation resistance and the hot melt drill tool structure are used to determine the axial extrusion force on the tool during the hot melt drill process, including: According to the extrusion stress state coefficient n of the processed material σ and the deformation resistance of the processed material σ k , using the formula P = n σ ·σ k Calculate the axial stress P during hot melt drilling; According to the structure of the hot melt drill tool, calculate the end area S of the hot melt drill pressed into the cone section; According to the axial stress P during the hot melt drilling process and the end area S of the hot melt drill pressed into the cone section, the formula F=P·S is used to calculate the axial extrusion force F exerted on the tool during the hot melt drilling process.
7. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 1 is characterized in that: The processing parameters include: hot melt drill processing temperature and hot melt drill axial feed speed.
8. The method for predicting the extrusion force of hot melt drilling based on needle extrusion according to claim 4 is characterized in that: The processing cooling and lubrication factor is non-lubricated processing or lubricated processing; In the case of non-lubricated processing, the friction factor between the hot melt drill and the processed material is: During lubrication processing, the friction factor between the hot melt drill and the processed material is:
9. A computer device comprising: A memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the method for predicting the extrusion force of a hot melt drill based on needle extrusion according to any one of claims 1 to 8.
10. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, the method for predicting the extrusion force of hot melt drilling based on needle extrusion according to any one of claims 1 to 8 is implemented.