Method for manufacturing blind groove with high precision and depth control
By using copper clad plate with consistent dielectric layer thickness, laser ablation, tin filling, stacking and tin removal methods on the printed circuit board, the problems of blind groove processing accuracy and copper layer etching residues in the prior art are solved, and the problem of blind groove processing is realized. High precision and rapid and thorough blind slot production ensures the stability of electrical connections.
Patent Information
- Application Number
- CN202411176200.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-12-03
AI Technical Summary
In the existing blind groove processing methods for printed circuit boards, poor mechanical depth control accuracy or residual copper layer etching leads to poor quality, which cannot effectively ensure high accuracy and electrical connection stability.
Using copper clad plate with the thickness of the intermediate dielectric layer and the depth of the blind groove, the preliminary groove body is formed by laser ablation, filled with tin and overflow, overlapping the semi-cured sheet and copper layer, exposing the etching line, and finally retracting the tin to form a blind groove to ensure high accuracy and no metal residue.
The production of high-precision deep-controlled blind grooves is realized, which avoids metal residue problems, improves processing efficiency and electrical connection reliability.
Smart Images

Figure CN119072027A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of printed circuit board manufacturing technology, and in particular to a method for manufacturing a blind groove with high-precision depth control. Background Art
[0002] Circuit board is also called printed circuit board or printed circuit board, also often referred to as PCB. It is an important electronic component, a support for electronic components, and a provider of electrical connections for electronic components. It is a basic component used to support and connect electronic components. Reliable electrical connections can be achieved between electronic components through PCB, so that the equipment can operate normally.
[0003] During PCB production, blind slots, holes and other structures are often processed on the board. The existing PCB slot processing mostly adopts the following two methods: One method is to process the slot by mechanical depth-controlled drilling and milling. This processing method is not only complicated and inefficient, but also has poor depth control accuracy during processing, which easily leads to poor quality of the formed slot. The other method is to first lay copper on the bottom of the slot, then ablate the copper layer by laser, and then remove the copper layer by etching copper to form the slot. Although this method has high depth control accuracy, the etched copper layer often has residues, which easily affects the electrical connection function of the slot. Summary of the invention
[0004] Based on this, it is necessary to provide a blind groove manufacturing method with high-precision depth control to address the deficiencies in the prior art.
[0005] A method for making a blind groove with high precision and controlled depth comprises the following steps:
[0006] Step 1: Cut the material, and cut a copper-clad board with a dielectric layer in the middle and copper layers on the upper and lower sides. The thickness of the dielectric layer is consistent with the depth of the blind groove to be processed;
[0007] Step 2: Ablation, single-sided etching of the top copper layer of the copper-clad laminate, and then partial ablation of the dielectric layer exposed after etching using a laser device until the bottom copper layer is exposed, so that it is initially formed into a slot body;
[0008] Step 3: Fill tin, fill tin in the ablated slot and reflow it to completely fill the slot;
[0009] Step 4: Laminating, laminating the prepreg and the copper layer on the upper surface of the dielectric layer of the copper clad laminate in sequence, and completely pressing the two together and attaching them to the copper clad laminate;
[0010] Step 5: Circuit, the copper layer on the surface of the copper clad board is exposed, developed and etched to produce the circuit of the circuit board, and the slot is exposed while the circuit is produced;
[0011] Step 6: Strip the tin to remove the tin filled in the slot body to form it into the final blind slot structure.
[0012] Furthermore, after the tin filling in step 3, the unevenness on the surface of the copper clad laminate can be smoothed.
[0013] Furthermore, the prepreg and the copper layer stacked after step 4 may be multiple layers.
[0014] To sum up, the beneficial effect of the high-precision depth-controlled blind groove production method of the present invention is that: by designing a method of filling the groove body with tin and then stripping the tin, the manufactured blind groove can ensure extremely high depth control accuracy, and at the same time, the tin stripping operation is faster and more thorough than conventional bottom copper etching, which can effectively avoid the problem of metal residue in the blind groove; the present invention is highly practical and has a strong promotion significance. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic cross-sectional structure diagram of the process from step 1 to step 6 in a method for making a blind groove with high precision and controlled depth according to the present invention. DETAILED DESCRIPTION
[0016] In order to further understand the features, technical means and specific objectives and functions achieved by the present invention, and analyze the advantages and spirit of the present invention, a further understanding is obtained through the following detailed description of the present invention in combination with the accompanying drawings and specific implementation methods.
[0017] like Figure 1 As shown, the present invention provides a method for making a blind groove with high precision and controlled depth, comprising the following steps:
[0018] Step 1: Cutting a copper-clad board with a dielectric layer 10 in the middle and copper layers 20 on the upper and lower sides, wherein the thickness of the dielectric layer 10 is consistent with the depth of the blind groove 60 to be processed;
[0019] Step 2: ablation, single-sided etching of the top copper layer 20 of the copper-clad laminate, and then partial ablation of the dielectric layer 10 exposed after etching using a laser device until the bottom copper layer 20 is exposed, so as to preliminarily form a slot body 30;
[0020] Step 3: Filling with tin, filling tin 40 in the ablated slot 30 and reflowing, so that the tin 40 completely fills the slot 30, after filling with tin, the uneven surface of the copper clad laminate can be smoothed;
[0021] Step 4: laminating, laminating the prepreg 50 and the copper layer 20 on the upper surface of the dielectric layer 10 of the copper clad laminate in sequence, and completely pressing and attaching the two to the copper clad laminate. Specifically, in this embodiment, only one layer of prepreg 50 and one layer of copper layer 20 are laminated. It can be understood that more layers can be laminated in other embodiments to meet more complex circuit board production requirements;
[0022] Step 5: Circuit, exposing, developing and etching the copper layer 20 on the surface of the copper clad board to produce the circuit of the circuit board, and exposing the slot body 30 while producing the circuit;
[0023] Step 6: Stripping the tin 40 , removing the tin 40 filled in the slot body 30 to form the final blind slot 60 structure.
[0024] In summary, the beneficial effect of the high-precision depth-controlled blind groove manufacturing method of the present invention is that: by designing a method of filling the groove body 30 with tin 40 and then stripping the tin, the manufactured blind groove 60 can ensure extremely high depth control accuracy, and at the same time, the tin stripping operation is faster and more thorough than conventional bottom copper etching, which can effectively avoid the problem of metal residue in the blind groove 60; the present invention is highly practical and has a strong promotion significance.
[0025] The above-mentioned embodiment only expresses one implementation method of the invention, and its description is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the inventive concept, which all belong to the protection scope of the invention. Therefore, the protection scope of the invention patent shall be based on the attached claims.
Claims
1. A method for making a blind groove with high precision and controlled depth, characterized in that: The steps include: Step 1: Cut the material, and cut a copper-clad board with a dielectric layer in the middle and copper layers on the upper and lower sides. The thickness of the dielectric layer is consistent with the depth of the blind groove to be processed; Step 2: Ablation, single-sided etching of the top copper layer of the copper-clad laminate, and then partial ablation of the dielectric layer exposed after etching using a laser device until the bottom copper layer is exposed, so that it is initially formed into a slot body; Step 3: Fill tin, fill tin in the ablated slot and reflow it to completely fill the slot; Step 4: Laminating, laminating the prepreg and the copper layer on the upper surface of the dielectric layer of the copper clad laminate in sequence, and completely pressing the two together and attaching them to the copper clad laminate; Step 5: Circuit, the copper layer on the surface of the copper clad board is exposed, developed and etched to produce the circuit of the circuit board, and the slot is exposed while the circuit is produced; Step 6: Strip the tin to remove the tin filled in the slot body to form it into the final blind slot structure.
2. The method for making a blind groove with high precision and controlled depth as claimed in claim 1, characterized in that: After the tin filling in step 3, the uneven surface of the copper clad laminate can be smoothed.
3. The method for making a blind groove with high precision and controlled depth as claimed in claim 1, characterized in that: The prepreg and copper layer stacked after step 4 may be multiple layers.