Modularized prefabrication method for converter suitable for overseas transportation

By performing modular prefabrication and strict inspection of the conversion furnace in China, a highly integrated 'assembly' has been formed, which solves the problems of difficult construction, long construction period and unstable quality in ocean transportation and overseas construction, and achieves efficient and safe Construction and transportation.

CN119077303AInactive Publication Date: 2024-12-06SHANGHAI BAOYE GRP CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411588979.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-08
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing technology has low integration of the modular construction methods of converter furnaces under ocean transportation and overseas construction conditions, resulting in high construction difficulty, long construction period, unstable quality, and safety risks.

Method used

Modular prefabrication method is adopted to carry out complicated assembly processes in China to form a highly integrated 'assembly', and then transport it overseas in roll-to-roll, reducing on-site assembly, and through strict area division, material cutting splicing, welding, and non-destructive testing , pre-assembly inspection, rust removal and coating and marking steps to ensure the high precision and stability of the module.

Benefits of technology

It reduces the complexity and uncertainty of overseas construction, shortens the project cycle, improves construction efficiency and safety, reduces transportation risks, and adapts to the construction environment and regulatory requirements of different countries and regions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119077303A_ABST
    Figure CN119077303A_ABST
Patent Text Reader

Abstract

The invention discloses a converter modular prefabrication method suitable for overseas transportation, and belongs to the technical field of converter prefabrication. In order to solve the problems that the integration level is not high, and economical, efficient and high-quality modular construction cannot be realized when overseas projects are undertaken, the complicated assembly process is completed in an environment with better domestic conditions, so that the installation difficulty and the construction period of an overseas site are reduced; the components can be assembled with high precision and high quality in a factory through modular prefabrication, so that the construction period of the whole project is shortened, the complicated assembly process of the reformer is carried out in China with loose conditions, and then the reformer is transported to an overseas project location in a roll-roll mode through a highly-integrated'assembly ', so that the construction period is shortened, and the construction period is shortened. And then the converter can be installed and put into production only through a small amount of field assembly operation, so that the influence on the local environment, the labor condition and the like is small during overseas operation, and batch assembly, wharf final assembly and assembly rolling assembly are facilitated, so that the converter is suitable for ocean transportation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of reformer prefabrication, and in particular to a reformer modular prefabrication method suitable for overseas transportation. Background Art

[0002] The reformer is a large, complex, systematic equipment widely used in chemical industry, metallurgy and other fields. It is mainly used to convert hydrocarbons or other raw materials into synthesis gas or other valuable chemicals in the presence of catalysts. The design and operation of the reformer involves knowledge from multiple disciplines, including chemical engineering, thermodynamics, materials science, etc.

[0003] The working principle of the reformer usually involves chemical reactions under high temperature and pressure, which requires precise control of parameters such as temperature, pressure, and gas flow. Therefore, during the design and operation process, advanced control technology and monitoring systems need to be adopted to ensure the stable operation and efficient conversion of the reformer.

[0004] The reformer is a large, complex, systematic equipment. For this type of equipment, the domestic method of off-site local manufacturing and on-site specific assembly is currently adopted. The patent with announcement number CN104976894B discloses an overall modular structure and construction method of an industrial furnace, which adopts overall modular design, workshop modular manufacturing and overall assembly, overall transportation, and on-site overall installation for the industrial furnace, which reduces the construction difficulty and ensures manufacturing accuracy and construction progress. However, there are still the following problems in actual operation: The existing methods are based on the conditions of near-shore and near-sea transportation. Since there are almost no restrictions on transportation conditions and on-site construction conditions, the modular method is not highly integrated. When undertaking overseas projects, the current modular construction method cannot achieve economical, efficient, and high-quality modular construction due to many restrictions such as ocean transportation conditions, local laws and regulations of the project location, and labor conditions. Summary of the invention

[0005] The object of the present invention is to provide a modular prefabrication method of a reformer suitable for overseas transportation, so as to solve the problems raised in the above background technology.

[0006] To achieve the above object, the present invention provides the following technical solution: a modular prefabrication method of a reformer suitable for overseas transportation, comprising the following steps: Production area division: according to the project schedule and progress, the team divides the area according to the project, material, and type of work; Material cutting and splicing: cutting the materials, spot welding the parts and assembling them after cutting; Material welding, welding of assembled and spliced ​​component parts; Non-destructive testing: conduct flaw detection on all fully penetrated welds of all profiles and issue a report; Pre-assembly inspection: perform pre-assembly inspection on the contents that need to be pre-assembled, wherein the contents that need to be pre-assembled include the radiation section bottom plate, wall panels, top plate, components connected between the bottom plate and the top plate, convection section modules, chimneys, air ducts connected with steel flange surfaces, and flues; Pre-assembly construction, precise measurement and benchmark wire testing of component hoisting, recording assembly dimensions and marking repair points; Rust removal and painting of components: rust removal of components as a whole, painting of components after rust removal and testing of painting quality; Component identification: After assembly, the components are stamped and numbered, where the depth of the stamp is less than or equal to 5 mm; Inspection point: inspect the appearance, welding and dimensions of components. After the inspection is completed, fill in the component inspection form and submit it. Pre-assembly inspection will be carried out after pre-assembly of components, and the number of components will be counted before delivery. The material cutting and splicing comprises the following steps: When the length of the material cannot meet the length requirements of the component parts, the material is spliced; Directly splice angle steel, channel steel with a cross-sectional height less than 150mm, H-shaped steel and I-shaped steel and perform full penetration welding on the butt joints; For channel steel, H-shaped steel and I-shaped steel with a cross-sectional height greater than or equal to 150mm, Z-shaped splicing is performed and full penetration welding is performed on the butt joints. The splicing length is 1.5 times the cross-sectional height. At the same time, stress relief holes are reserved according to the welding drawing. The diameter of the stress relief holes is 8mm. The stress relief holes are welded closed during splicing; The shortest splicing length for H-shaped steel is 1000mm, and the shortest splicing length for diagonal steel and channel steel with width and height greater than 100mm is 500mm.

[0007] Furthermore, the material cutting and splicing further comprises the following steps: Confirm the material and process requirements before cutting, number the materials according to the layout drawing, parts list, parts drawing and computer sample drawing, and lay out based on the welding shrinkage allowance of the components and the cutting and planing allowances, and cut the materials after confirmation; Remove oil, rust and moisture from the surface of the parent material, and straighten the plate after cutting; When cutting steel, plasma cutting is selected. When the thickness of the steel plate is less than or equal to 12mm, shearing machine is selected for cutting. When the thickness of the steel plate is greater than 12mm, automatic cutting machine is selected for cutting. When the steel is small-shaped steel, grinding wheel cutting machine is selected for cutting. When the steel is large-shaped steel, automatic and semi-automatic cutting machines are selected for cutting. After cutting, remove slag and spatter; Check the number, material, size, quantity and processing accuracy of the assembly parts. After the inspection, spot weld and assemble the parts.

[0008] Furthermore, the material welding further comprises the following steps: Remove the oxide scale, slag scale, moisture, oil, rust and burrs within 50mm-80mm around the welding area; The welding is performed on the same component in a way that the heat is dispersed and distributed symmetrically, and the long welds are welded by skip welding, so that the welds and the base material have a smooth transition.

[0009] Furthermore, the nondestructive testing further includes the following steps: Carry out PT flaw detection on the position of the lifting lug; Conduct PT test on the butt joint of channel steel and angle steel L100*100*10; Conduct PT test on H-beam butt welds; UT test is carried out on H-beams with web and flange thickness greater than 12mm.

[0010] Furthermore, the pre-assembly construction further includes the following steps: Clean the platform and use a level to check and calibrate the platform for flatness; Find the component number that needs to be pre-assembled according to the layout drawing, and hoist and stack the components according to the drawing; Measure the overall dimensions, diagonal and flatness of the component, use chalk lines to draw the bolt hole edges of the two wall panels as reference lines, and check the alignment of the bolt holes after the wall panels are connected based on the reference lines; Fill in the assembly dimensions according to the assembly records and mark the areas that need repair.

[0011] Furthermore, the component rust removal and coating further comprises the following steps: The components are derusted by shot blasting machine. The abrasives used by the shot blasting machine are steel shot and cut shot. The diameter of the steel shot and cut shot is 0.5-1.0mm. The small parts and parts that cannot be derusted by shot blasting are derusted manually and with power tools; Check the name, model and color of the paint; After sandblasting and rust removal, the first coat of primer shall be sprayed within 4 hours, and the next coat shall be painted after the coating reaches surface dryness. The interval between coating spraying shall not be less than 4 hours; After painting is completed, spray the component number and positioning mark on the component.

[0012] Furthermore, before the power tool is rust-removed, the speed value range of the power tool is set, including: The diameter of the extracted steel shot; The first adjustment coefficient is obtained by using the diameter of the steel shot; wherein the first adjustment coefficient is obtained by the following formula: Wherein, k represents the first adjustment coefficient; n represents the number of types of steel shots with different diameters included; D i Indicates the diameter value corresponding to the i-th steel shot; D z Indicates the middle value of the diameter of the steel shot; D max Indicates the maximum diameter of the steel shot; D min Indicates the minimum diameter of the steel shot; Extract the sawtooth angle of the cut shot; The second adjustment coefficient is obtained by using the sawtooth angle of the cut shot; wherein the second adjustment coefficient is obtained by the following formula: Wherein, s represents the second adjustment coefficient; m represents the number of types of sawtooth angles of the cut shot; α i Indicates the specific angle value corresponding to the i-th angle; α z Indicates the middle value of the angle; α max Indicates the maximum angle; α min Indicates the minimum angle; The first adjustment coefficient and the second adjustment coefficient are used to set the rotation speed value range of the power tool.

[0013] Further, using the first adjustment coefficient and the second adjustment coefficient to set the speed value range of the power tool includes: extracting the first adjustment coefficient and the second adjustment coefficient; The friction force generated by the combined action of the steel shot and the cut shot is obtained by using the first adjustment coefficient and the second adjustment coefficient, wherein the friction force is obtained by the following formula: Where F represents the friction force generated by the combined action of steel shot and cut shot; μ 01 Indicates the friction coefficient of steel shot; μ 02 represents the friction coefficient of the cut shot; k represents the first adjustment coefficient; s represents the second adjustment coefficient; N represents the average value of the normal force of the steel shot and the cut shot on the component; Extract the power frequency of the power tool; The rotation speed value range of the power tool is set by utilizing the friction force generated by the steel shot and the cut shot in combination with the power frequency of the power tool, wherein the rotation speed value range of the power tool is obtained by the following formula: Among them, V upIndicates the upper limit value corresponding to the speed range of the power tool; V down Indicates the lower limit of the speed range of the power tool; F max and F min They represent the maximum friction and minimum friction required for rust removal respectively; F represents the friction generated by the combined action of steel shot and cut shot; f max and f min They respectively represent the maximum and minimum values ​​of the power supply frequency; P represents the number of pole pairs of the power tool's motor.

[0014] Furthermore, the component rust removal and coating further comprises the following steps: Before painting, the surface treatment of the components and each process of the painting work shall be checked and recorded. After the paint film is completely dry, the dry film thickness shall be tested with a dry film thickness gauge; Among them, when testing the dry film thickness, select no less than five measuring points, select three points at each measuring point for testing and take the average value, and compare the average value based on the standard coating thickness; The minimum thickness value of the measuring points shall not be less than 80% of the standard value, and more than 90% of the measuring points reaching the standard coating thickness are considered qualified.

[0015] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention allows the complicated assembly process of the converter to be carried out in the country where conditions are relaxed, and then the highly integrated "assembly" is transported to the overseas project site by roll-on / roll-off. After that, the converter can be installed and put into production through only a small amount of on-site assembly work. In this way, the impact on the local environment, labor conditions, etc. during overseas operations is relatively small, and it is convenient for batch assembly, dock assembly, and assembly roll-on / roll-off, so it is suitable for ocean transportation.

[0016] 2. The present invention reduces the difficulty and duration of installation at overseas sites by completing the complex assembly process under relatively good domestic conditions. Modular prefabrication enables each component to be assembled with high precision and quality in the factory, thereby shortening the construction period of the overall project. At the same time, modular prefabrication reduces the complexity and uncertainty of overseas construction sites, such as the impact of factors such as weather, environment, and differences in labor skills on construction progress and quality. At the same time, it also reduces the safety risks that may be encountered in overseas construction.

[0017] 3. After the pre-assembly construction is completed in the factory, the integrity and stability of the converter module are significantly improved, which helps to reduce the risk caused by module deformation or damage during transportation. At the same time, the pre-assembly construction can also reduce the workload and difficulty of on-site installation, and reduce the risk of safety accidents during installation. During the pre-assembly construction process, the size, shape and connection accuracy of the components are strictly inspected and recorded, which helps to discover and promptly deal with problems in the component manufacturing process. Through quality control and repair measures in the factory, it can be ensured that the quality of the components meets the design requirements and relevant standards. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the modular prefabrication process of the present invention; Figure 2 It is a schematic diagram of the pre-assembly process of the present invention. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0020] In order to solve the problem that the existing technology is carried out under the conditions of near-shore and near-sea transportation, and the transportation conditions and on-site construction conditions are almost unlimited, the modular method has a low degree of integration. When undertaking overseas projects, under the conditions of ocean transportation, local laws and regulations of the project location, employment conditions and many other restrictions, the current modular construction method cannot achieve economic, efficient and high-quality conversion to modular construction. Please refer to Figure 1-2 , the present invention provides the following technical solutions: The modular prefabrication method of the reformer suitable for overseas transportation includes the following steps: Production area division: according to the project schedule and progress, the team divides the area according to the project, material, and type of work; Material cutting and splicing: cutting the materials, spot welding the parts and assembling them after cutting; Material welding, welding of assembled and spliced ​​component parts; Non-destructive testing: conduct flaw detection on all fully penetrated welds of all profiles and issue a report; Pre-assembly inspection: perform pre-assembly inspection on the contents that need to be pre-assembled, wherein the contents that need to be pre-assembled include the radiation section bottom plate, wall panels, top plate, components connected between the bottom plate and the top plate, convection section modules, chimneys, air ducts connected with steel flange surfaces, and flues; Pre-assembly construction, precise measurement and benchmark wire testing of component hoisting, recording assembly dimensions and marking repair points; Rust removal and painting of components: rust removal of components as a whole, painting of components after rust removal and testing of painting quality; Component identification: After assembly, the components are stamped and numbered, where the depth of the stamp is less than or equal to 5 mm; At the inspection point, the appearance, welding and size of the components are inspected. After the inspection is completed, the component inspection form is filled in and submitted. Among them, pre-assembly inspection is carried out for components that need to be pre-assembled after pre-assembly, and the number of components is counted before shipment.

[0021] Specifically, this technical solution allows the complicated assembly process of the converter to be carried out in the country where conditions are relaxed, and then the highly integrated "assembly" is transported to the overseas project site by roll-on / roll-off. After that, the converter can be installed and put into production through only a small amount of on-site assembly work. In this way, the impact on the local environment, labor conditions, etc. during overseas operations is relatively small, which facilitates batch assembly, dock assembly, and assembly roll-on / roll-off, making it suitable for ocean transportation.

[0022] In the above embodiment, by completing the complex assembly process in a domestic environment with better conditions, the difficulty and duration of installation at the overseas site are reduced. Modular prefabrication enables each component to be assembled with high precision and quality in the factory, thereby shortening the construction period of the overall project. At the same time, modular prefabrication reduces the complexity and uncertainty of overseas construction sites, such as the impact of factors such as weather, environment, and differences in labor skills on construction progress and quality. At the same time, it also reduces the safety risks that may be encountered in overseas construction.

[0023] In the above embodiment, in a domestic factory environment, more advanced equipment and technology can be used for precision processing and quality control to ensure that each module meets the design requirements. Steps such as non-destructive testing and pre-assembly inspection further ensure the welding quality and assembly accuracy of the components. Through modular prefabrication, multiple components are integrated into an "assembly" for transportation, reducing the number of transportation times and the use of packaging materials, thereby reducing transportation costs. In addition, the roll-on / roll-off transportation method also improves transportation efficiency.

[0024] In the above embodiment, the modular design enables the reformer to better adapt to the construction environment and regulatory requirements of different countries and regions. By adjusting the combination and configuration of the modules, it can quickly adapt to various project requirements, carry out modular prefabrication in China, reduce construction waste and pollution emissions at overseas sites, and is conducive to environmental protection and sustainable development. At the same time, it also promotes the development of related industries and technological progress in China.

[0025] Material cutting and splicing also includes the following steps: Confirm the material and process requirements before cutting, number the materials according to the layout drawing, parts list, parts drawing and computer sample drawing, and lay out based on the welding shrinkage allowance of the components and the cutting and planing allowances, and cut the materials after confirmation; Remove oil, rust and moisture from the surface of the parent material, and straighten the plate after cutting; When cutting steel, plasma cutting is selected. When the thickness of the steel plate is less than or equal to 12mm, shearing machine is selected for cutting. When the thickness of the steel plate is greater than 12mm, automatic cutting machine is selected for cutting. When the steel is small-shaped steel, grinding wheel cutting machine is selected for cutting. When the steel is large-shaped steel, automatic and semi-automatic cutting machines are selected for cutting. After cutting, remove slag and spatter; Check the number, material, size, quantity and processing accuracy of the assembly parts. After the inspection, spot weld and assemble the parts.

[0026] When the length of the material cannot meet the length requirements of the component parts, the material is spliced; Directly splice angle steel, channel steel with a cross-sectional height less than 150mm, H-shaped steel and I-shaped steel and perform full penetration welding on the butt joints; For channel steel, H-shaped steel and I-shaped steel with a cross-sectional height greater than or equal to 150mm, Z-shaped splicing is performed and full penetration welding is performed on the butt joints. The splicing length is 1.5 times the cross-sectional height. At the same time, stress relief holes are reserved according to the welding drawing. The diameter of the stress relief holes is 8mm. The stress relief holes are welded closed during splicing; The shortest splicing length for H-shaped steel is 1000mm, and the shortest splicing length for diagonal steel and channel steel with width and height greater than 100mm is 500mm.

[0027] In the above embodiment, the accuracy and rationality of cutting are ensured by confirming the material and process, numbering, and laying out before cutting, thereby reducing material waste and improving material utilization. At the same time, the precise cutting and splicing process ensures the dimensional accuracy and shape accuracy of the components, providing a good foundation for subsequent welding and assembly. Different splicing methods and welding requirements are adopted for steels with different cross-sections, such as direct splicing of diagonal steels and small steel sections, and Z-shaped splicing of large steel sections with reserved stress release holes. These measures effectively enhance the strength and stability of the components and ensure the overall performance of the converter.

[0028] In the above embodiments, during the material cutting and splicing process, strict inspection and quality control are carried out, such as checking the number, material, size, quantity and processing accuracy of the assembly parts, to ensure that each component meets the design requirements, which not only improves the construction quality, but also reduces the workload of subsequent repairs and rework, and improves construction efficiency. Through precise cutting and splicing, the size and weight of the components are more reasonable, which is convenient for transportation and installation. Especially in overseas transportation, reasonable component size and weight can reduce transportation costs and risks, while reducing the difficulty and cost of installation at overseas sites.

[0029] Material welding specifically includes the following steps: Remove the oxide scale, slag scale, moisture, oil, rust and burrs within 50mm-80mm around the welding area; The welding is performed on the same component in a way that the heat is dispersed and distributed symmetrically, and the long welds are welded by skip welding, so that the welds and the base material have a smooth transition.

[0030] In the above embodiment, by removing impurities in the welding area and its vicinity, the cleanliness of the weld joint is ensured, thereby improving the welding quality. A clean welding surface helps to reduce welding defects such as pores and slag inclusions, improve the strength and sealing of the weld, and the use of heat dispersion and symmetrical distribution for welding, as well as skip welding technology at long welds, helps to reduce thermal stress and deformation generated during welding. This welding method can balance the heat input during welding, avoid deformation and stress concentration caused by local overheating, and thus maintain the geometric shape and dimensional accuracy of the component.

[0031] Nondestructive testing also includes the following steps: Carry out PT flaw detection on the position of the lifting lug; Conduct PT test on the butt joint of channel steel and angle steel L100*100*10; Conduct PT test on H-beam butt welds; UT test is carried out on H-beams with web and flange thickness greater than 12mm.

[0032] In the above embodiment, the non-destructive testing technology can detect internal defects or cracks without destroying the components, thereby ensuring the quality of the components. During the modular prefabrication process of the converter, non-destructive testing of key parts can effectively avoid performance degradation or safety hazards caused by internal defects of the components. By performing non-destructive testing on key parts such as the lug positions and butt welds, the connection strength and sealing of these parts can be ensured, thereby improving the reliability of the components.

[0033] In the above embodiments, the application of non-destructive testing technology can optimize the construction process, reduce rework and repair work caused by welding defects, and avoid problems in subsequent installation and commissioning by timely discovering and handling welding defects, thereby improving construction efficiency. The overseas transportation environment is complex and changeable, and has higher requirements on the quality and stability of components. It is ensured that the components are not easily damaged or deformed during transportation, thereby reducing transportation risks. At the same time, high-quality components are also more likely to meet the acceptance standards of overseas projects.

[0034] Pre-assembly construction also includes the following steps: Clean the platform and use a level to check and calibrate the platform for flatness; Find the component number that needs to be pre-assembled according to the layout drawing, and hoist and stack the components according to the drawing; Measure the overall dimensions, diagonal and flatness of the component, use chalk lines to draw the bolt hole edges of the two wall panels as reference lines, and check the alignment of the bolt holes after the wall panels are connected based on the reference lines; Fill in the assembly dimensions according to the assembly records and mark the areas that need repair.

[0035] In the above embodiment, the platform is cleaned, leveled, inspected and calibrated to ensure that the basic environment of the pre-assembly construction meets the accuracy requirements. On this basis, the components are hoisted and stacked according to the layout drawings, and the overall dimensions, diagonals and flatness of the components are strictly measured. The alignment of the bolt holes after the wall panels are connected is detected by the reference wire. These steps together ensure the high accuracy of the pre-assembly construction, which can significantly improve the overall quality and installation efficiency of the converter module and reduce the workload of on-site adjustments and corrections. The pre-assembly construction advances part of the assembly work to the factory. Through reasonable construction organization and process arrangement, the construction efficiency can be significantly improved. At the same time, problems found during the pre-assembly process and parts that need to be repaired can be dealt with in time in the factory, avoiding shutdowns and delays caused by waiting for repairs during on-site construction, which helps to shorten the project cycle and improve the overall benefits of the project.

[0036] In the above embodiment, after the pre-assembly construction is completed in the factory, the integrity and stability of the converter module are significantly improved, which helps to reduce the risk caused by module deformation or damage during transportation. At the same time, the pre-assembly construction can also reduce the workload and difficulty of on-site installation and reduce the risk of safety accidents during installation. During the pre-assembly construction process, the size, shape and connection accuracy of the components are strictly inspected and recorded, which helps to discover and promptly deal with problems in the component manufacturing process. Through quality control and repair measures in the factory, it can be ensured that the quality of the components meets the design requirements and relevant standards.

[0037] The rust removal and painting of components also includes the following steps: The components are derusted by shot blasting machine. The abrasives used by the shot blasting machine are steel shot and cut shot. The diameter of the steel shot and cut shot is 0.5-1.0mm. The small parts and parts that cannot be derusted by shot blasting are derusted manually and with power tools; Check the name, model and color of the paint; After sandblasting and rust removal, the first coat of primer shall be sprayed within 4 hours, and the next coat shall be painted after the coating reaches surface dryness. The interval between coating spraying shall not be less than 4 hours; After painting is completed, spray the component number and positioning mark on the component.

[0038] Before painting, the surface treatment of the components and each process of the painting work shall be checked and recorded. After the paint film is completely dry, the dry film thickness shall be tested with a dry film thickness gauge; Among them, when testing the dry film thickness, select no less than five measuring points, select three points at each measuring point for testing and take the average value, and compare the average value based on the standard coating thickness; The minimum thickness value of the measuring points shall not be less than 80% of the standard value, and more than 90% of the measuring points reaching the standard coating thickness are considered qualified.

[0039] In the above embodiment, the rust on the component is removed by a shot blasting machine, especially using steel shots and cut shots with a diameter of 0.5-1.0 mm, which can efficiently and thoroughly remove the rust and oxide layer on the surface of the component, providing a good base for subsequent painting. For small parts and parts that cannot be rusted by shot blasting, manual and power tools are used to remove rust to ensure that the surface of the component is completely clean, thereby improving the adhesion and corrosion resistance of the coating, which is especially important for harsh environments such as humidity and salt spray that may be encountered during overseas transportation, and can effectively extend the service life of the converter module.

[0040] In the above embodiment, the paint is strictly inspected before painting to ensure that the name, model and color of the paint meet the design requirements, thereby avoiding painting quality defects caused by paint problems. At the same time, the painting interval and the number of coating layers are strictly controlled to ensure that the coating thickness is uniform and dense, thereby improving the protective performance of the coating. After painting, the component number and positioning mark are sprayed on the component to facilitate subsequent installation, maintenance and traceability.

[0041] In the above embodiment, shot blasting rust removal is efficient and automated, which can significantly improve the rust removal efficiency. At the same time, the inspection and record-keeping work during the painting process helps to discover and solve problems in a timely manner, avoiding rework and delays caused by painting quality problems. In addition, reasonable painting technology and strict quality control measures can also help improve construction efficiency and shorten project cycles. High-quality painting can effectively prevent components from being corroded and damaged during transportation, reducing transportation risks caused by component damage, which is especially important for overseas transportation. Because the transportation distance is long, the time is long, and the environment is complex and changeable, higher requirements are placed on the protective performance of the components.

[0042] Specifically, before the power tool is rust-removed, the speed value range of the power tool is set, including: The diameter of the extracted steel shot; The first adjustment coefficient is obtained by using the diameter of the steel shot; wherein the first adjustment coefficient is obtained by the following formula: Wherein, k represents the first adjustment coefficient; n represents the number of types of steel shots with different diameters included; D i Indicates the diameter value corresponding to the i-th steel shot; D z Indicates the middle value of the diameter of the steel shot; D max Indicates the maximum diameter of the steel shot; D min Indicates the minimum diameter of the steel shot; Extract the sawtooth angle of the cut shot; The second adjustment coefficient is obtained by using the sawtooth angle of the cut shot; wherein the second adjustment coefficient is obtained by the following formula: Wherein, s represents the second adjustment coefficient; m represents the number of types of sawtooth angles of the cut shot; α i Indicates the specific angle value corresponding to the i-th angle; α z Indicates the middle value of the angle; α max Indicates the maximum angle; α min Indicates the minimum angle; The first adjustment coefficient and the second adjustment coefficient are used to set the rotation speed value range of the power tool.

[0043] The technical effect of the above technical solution is: by extracting the diameter of the steel shot and the sawtooth angle of the cut shot, and calculating the first adjustment coefficient and the second adjustment coefficient respectively, the speed value range of the power tool can be adjusted more accurately according to the characteristics of the abrasive used. This personalized setting helps to improve the efficiency and effect of rust removal, while reducing unnecessary energy consumption and tool wear. The diameter of the steel shot and the sawtooth angle of the cut shot are key factors affecting the rust removal effect. The technical solution sets the speed by considering these factors, which can ensure that the power tool is in the best state during operation, thereby more effectively removing rust and improving the surface treatment quality. Different rust removal tasks may require the use of steel shots of different diameters and cut shots with sawtooth angles. The technical solution provides a flexible method to quickly adjust the speed of the power tool according to specific task requirements, enhancing the adaptability and versatility of the tool. By accurately setting the speed value range, the power tool can be prevented from running at too high or too low a speed, thereby reducing unnecessary mechanical stress and helping to extend the service life of the tool.

[0044] In summary, this technical solution optimizes the speed setting of the power tool by comprehensively considering the physical properties of the abrasive, thereby improving the rust removal effect, enhancing the adaptability of the tool and extending the tool life.

[0045] Specifically, using the first adjustment coefficient and the second adjustment coefficient to set the speed value range of the power tool includes: extracting the first adjustment coefficient and the second adjustment coefficient; The friction force generated by the combined action of the steel shot and the cut shot is obtained by using the first adjustment coefficient and the second adjustment coefficient, wherein the friction force is obtained by the following formula: Where F represents the friction force generated by the combined action of steel shot and cut shot; μ 01 Indicates the friction coefficient of steel shot; μ 02 represents the friction coefficient of the cut shot; k represents the first adjustment coefficient; s represents the second adjustment coefficient; N represents the average value of the normal force of the steel shot and the cut shot on the component; Extract the power frequency of the power tool; The rotation speed value range of the power tool is set by utilizing the friction force generated by the steel shot and the cut shot in combination with the power frequency of the power tool, wherein the rotation speed value range of the power tool is obtained by the following formula: Among them, V up Indicates the upper limit value corresponding to the speed range of the power tool; V down Indicates the lower limit of the speed range of the power tool; Fmax and F min They represent the maximum friction and minimum friction required for rust removal respectively; F represents the friction generated by the combined action of steel shot and cut shot; f max and f min They respectively represent the maximum and minimum values ​​of the power supply frequency; P represents the number of pole pairs of the power tool's motor.

[0046] The technical effect of the above technical solution is: by extracting the first adjustment coefficient and the second adjustment coefficient, and combining the physical properties of steel shot and cut shot (such as friction coefficient) and the friction generated by their joint action, the technical solution can more finely control the speed range of the power tool. This control not only takes into account the characteristics of the abrasive, but also combines the power frequency and motor parameters of the power tool itself, thereby achieving a more accurate speed setting. By accurately setting the speed range of the power tool, the technical solution can ensure that the power tool runs at the optimal speed during the rust removal process, thereby maximizing the rust removal efficiency and improving the rust removal effect. At the same time, considering the friction factor helps to ensure effective contact between the abrasive and the surface of the component, further improving the quality of rust removal.

[0047] This technical solution sets the speed range of the power tool by taking into account multiple factors (such as abrasive characteristics, power frequency, motor parameters, etc.), thereby enhancing the adaptability and stability of the power tool under different working conditions. This helps reduce the problem of tool damage or poor rust removal due to improper speed. By accurately controlling the speed range, this technical solution helps reduce the situation where the power tool runs at too high or too low speed, thereby reducing mechanical stress and extending the service life of the tool.

[0048] In summary, this technical solution optimizes the rust removal efficiency and effect, enhances the adaptability and stability of the power tool, and extends the service life of the tool by comprehensively considering multiple factors to accurately set the speed range of the power tool.

[0049] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A modular prefabrication method of a reformer suitable for overseas transportation, comprising the following steps: Production area division: according to the project schedule and progress, the team divides the area according to the project, material, and type of work; Material cutting and splicing: cutting the materials, spot welding the parts and assembling them after cutting; Material welding, welding of assembled and spliced ​​component parts; Non-destructive testing: conduct flaw detection on all fully penetrated welds of all profiles and issue a report; Pre-assembly inspection: perform pre-assembly inspection on the contents that need to be pre-assembled, wherein the contents that need to be pre-assembled include the radiation section bottom plate, wall panels, top plate, components connected between the bottom plate and the top plate, convection section modules, chimneys, air ducts connected with steel flange surfaces, and flues; Pre-assembly construction, precise measurement and benchmark wire testing of component hoisting, recording assembly dimensions and marking repair points; Rust removal and painting of components: rust removal of components as a whole, painting of components after rust removal and testing of painting quality; Component identification: After assembly, the components are stamped and numbered, where the depth of the stamp is less than or equal to 5 mm; Inspection point: inspect the appearance, welding and dimensions of components. After the inspection is completed, fill in the component inspection form and submit it. Pre-assembly inspection will be carried out after pre-assembly of components, and the number of components will be counted before delivery. It is characterized in that the material cutting and splicing comprises the following steps: When the length of the material cannot meet the length requirements of the component parts, the material is spliced; Directly splice angle steel, channel steel with a cross-sectional height less than 150mm, H-shaped steel and I-shaped steel and perform full penetration welding on the butt joints; For channel steel, H-shaped steel and I-shaped steel with a cross-sectional height greater than or equal to 150mm, Z-shaped splicing is performed and full penetration welding is performed on the butt joints. The splicing length is 1.5 times the cross-sectional height. At the same time, stress relief holes are reserved according to the welding drawing. The diameter of the stress relief holes is 8mm. The stress relief holes are welded closed during splicing; The shortest splicing length for H-shaped steel is 1000mm, and the shortest splicing length for diagonal steel and channel steel with width and height greater than 100mm is 500mm.

2. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 1, characterized in that: The material cutting and splicing specifically further includes the following steps: Confirm the material and process requirements before cutting, number the materials according to the layout drawing, parts list, parts drawing and computer sample drawing, and lay out based on the welding shrinkage allowance of the components and the cutting and planing allowances, and cut the materials after confirmation; Remove oil, rust and moisture from the surface of the parent material, and straighten the plate after cutting; When cutting steel, plasma cutting is selected. When the thickness of the steel plate is less than or equal to 12mm, shearing machine is selected for cutting. When the thickness of the steel plate is greater than 12mm, automatic cutting machine is selected for cutting. When the steel is small-shaped steel, grinding wheel cutting machine is selected for cutting. When the steel is large-shaped steel, automatic and semi-automatic cutting machines are selected for cutting. After cutting, remove slag and spatter; Check the number, material, size, quantity and processing accuracy of the assembly parts. After the inspection, spot weld and assemble the parts.

3. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 1, characterized in that: The material welding specifically further comprises the following steps: Remove the oxide scale, slag scale, moisture, oil, rust and burrs within 50mm-80mm around the welding area; The welding is performed on the same component in a way that the heat is dispersed and distributed symmetrically, and the long welds are welded by skip welding, so that the welds and the base material have a smooth transition.

4. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 1, characterized in that: The nondestructive testing specifically further comprises the following steps: Carry out PT flaw detection on the position of the lifting lug; Conduct PT test on the butt joint of channel steel and angle steel L100*100*10; Conduct PT test on H-beam butt welds; UT test is carried out on H-beams with web and flange thickness greater than 12mm.

5. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 1, characterized in that: The pre-assembly construction specifically further comprises the following steps: Clean the platform and use a level to check and calibrate the platform for flatness; Find the component number that needs to be pre-assembled according to the layout drawing, and hoist and stack the components according to the drawing; Measure the overall dimensions, diagonal and flatness of the component, use chalk lines to draw the bolt hole edges of the two wall panels as reference lines, and check the alignment of the bolt holes after the wall panels are connected based on the reference lines; Fill in the assembly dimensions according to the assembly records and mark the areas that need repair.

6. The modular prefabrication method of a reformer suitable for overseas transportation according to claim 1, characterized in that: The component rust removal and coating process specifically further comprises the following steps: The components are derusted by shot blasting machine. The abrasives used by the shot blasting machine are steel shot and cut shot. The diameter of the steel shot and cut shot is 0.5-1.0mm. The small parts and parts that cannot be derusted by shot blasting are derusted manually and with power tools; Check the name, model and color of the paint; After sandblasting and rust removal, the first coat of primer shall be sprayed within 4 hours, and the next coat shall be painted after the coating reaches surface dryness. The interval between coating spraying shall not be less than 4 hours; After painting is completed, spray the component number and positioning mark on the component.

7. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 6, characterized in that: Before removing rust from power tools, set the speed range of the power tools, including: The diameter of the extracted steel shot; The first adjustment coefficient is obtained by using the diameter of the steel shot; wherein the first adjustment coefficient is obtained by the following formula: Wherein, k represents the first adjustment coefficient; n represents the number of types of steel shots with different diameters included; D i Indicates the diameter value corresponding to the i-th steel shot; D z Indicates the middle value of the diameter of the steel shot; D max Indicates the maximum diameter of the steel shot; D min Indicates the minimum diameter of the steel shot; Extract the sawtooth angle of the cut shot; The second adjustment coefficient is obtained by using the sawtooth angle of the cut shot; wherein the second adjustment coefficient is obtained by the following formula: Wherein, s represents the second adjustment coefficient; m represents the number of types of sawtooth angles of the cut shot; α i Indicates the specific angle value corresponding to the i-th angle; α z Indicates the middle value of the angle; α max Indicates the maximum angle; α min Indicates the minimum angle; The first adjustment coefficient and the second adjustment coefficient are used to set the rotation speed value range of the power tool.

8. The modular prefabrication method of the reformer suitable for overseas transportation according to claim 7, characterized in that: Using the first adjustment coefficient and the second adjustment coefficient to set the speed value range of the power tool includes: extracting the first adjustment coefficient and the second adjustment coefficient; The friction force generated by the combined action of the steel shot and the cut shot is obtained by using the first adjustment coefficient and the second adjustment coefficient, wherein the friction force is obtained by the following formula: Where F represents the friction force generated by the combined action of steel shot and cut shot; μ 01 Indicates the friction coefficient of steel shot; μ 02 represents the friction coefficient of the cut shot; k represents the first adjustment coefficient; s represents the second adjustment coefficient; N represents the average value of the normal force of the steel shot and the cut shot on the component; Extract the power frequency of the power tool; The rotation speed value range of the power tool is set by utilizing the friction force generated by the steel shot and the cut shot in combination with the power frequency of the power tool, wherein the rotation speed value range of the power tool is obtained by the following formula: Among them, V up Indicates the upper limit value corresponding to the speed range of the power tool; V down Indicates the lower limit of the speed range of the power tool; F max and F min They represent the maximum friction and minimum friction required for rust removal respectively; F represents the friction generated by the combined action of steel shot and cut shot; f max and f min They respectively represent the maximum and minimum values ​​of the power supply frequency; P represents the number of pole pairs of the power tool's motor.

9. The method for modular prefabrication of a reformer suitable for overseas transportation according to claim 6, characterized in that: The component rust removal and coating process specifically further comprises the following steps: Before painting, the surface treatment of the components and each process of the painting work shall be checked and recorded. After the paint film is completely dry, the dry film thickness shall be tested with a dry film thickness gauge; Among them, when testing the dry film thickness, select no less than five measuring points, select three points at each measuring point for testing and take the average value, and compare the average value based on the standard coating thickness; The minimum thickness value of the measuring points shall not be less than 80% of the standard value, and more than 90% of the measuring points reaching the standard coating thickness are considered qualified.

Citation Information

Patent Citations

  • An overall modular structure and construction method of an industrial furnace

    CN104976894B

  • Automobile gear ruggedization shot-blasting machine

    CN101157203A

  • Steel structure machining process

    CN109079438A

  • Bridge steel shell tower section machining and assembling technology

    CN117484201A

  • H-shaped steel processing technology

    CN118342221A