Preparation method and application of sandwich type photoelectrochemical immunosensor based on Bi2MoO6 / Co3O4 composite material
Through the combination of Bi2MoO6/Co3O4 composite materials and Cu/CoS2-Ag NPs, the problem of low response efficiency of photoelectrochemical immunosensors in visible light is solved, and CEA detection with high sensitivity and strong specificity is achieved, and a new clinical detection method is provided.
Patent Information
- Application Number
- CN202411205666.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-12-06
AI Technical Summary
The existing photoelectrochemical immunosensors are inefficient in visible light response. Due to the relatively positive conduction band position, weak reduction power, poor dispersion, and unsatisfactory visible light adsorption, Bi2MoO6 material has limited its application in photoelectrochemical sensors, and electron transfer is space-transferred. The steric resistance affects the signal attenuation.
Bi2MoO6/Co3O4 composite material is used as the substrate to prepare Bi2MoO6 with superior performance by hydrothermal method, and optimize the photoelectric conversion activity through composite modification, combined with Cu/CoS2-Ag NPs as a label for signal amplification, and build a sandwich photoelectrochemical immunosensor. Optoelectronic performance is improved by using the energy band matching of Co3O4 and Bi2MoO6.
It realizes ultra-sensitive detection under visible light conditions, short response time, low detection limit, wide linear range and good stability, providing a high sensitivity and strong specificity CEA detection method, providing an early clinical detection of CEA New analysis methods.
Abstract
Description
Technical Field
[0001] The present invention relates to a preparation method and application of a photoelectrochemical immunosensor based on a Bi2MoO6 / Co3O4 composite material, and specifically to a sandwich-type photoelectrochemical immunosensor for sensitively detecting CEA using the Bi2MoO6 / Co3O4 composite material as a substrate material, belonging to the technical field of new functional materials and biosensor detection. Background Art
[0002] The photoelectric conversion process of photoelectrochemical (PEC) immunosensors is achieved through photoelectrically active materials. When excited by light, electrons in the materials jump from the valence band to the conduction band, generating electron-hole pairs. The separation of electrons and holes generates photovoltage, which forms a photocurrent in the external circuit, converting the light signal into an electrical signal. Based on this principle, it is crucial to seek photoelectrically active materials with high conversion performance, high stability, and non-toxicity for the construction of photoelectrochemical sensors. Currently, the most studied TiO2 can only respond to ultraviolet light (<400 nm), which accounts for only 4% of the total energy of sunlight, due to its wide bandgap. The development of visible light-responsive photoelectric materials is one of the most important ways to achieve efficient photoelectric conversion. Bi2MoO6 is a typical semiconductor compound with many unique properties, such as characteristic layered structure, sufficient chemical stability, tunable band gap and excellent photocatalytic activity. However, Bi2MoO6 is limited in its application in photoelectrochemical sensors due to its small specific surface area, relatively positive conduction band position, weak reduction power, poor dispersion, unsatisfactory visible light adsorption, and short lifetime of photoinduced electron-hole pairs. The band gap of Co3O4 can be well matched with the energy band of Bi2MoO6, resulting in better photoelectric performance, improved light utilization, and enhanced excitation of optical signals.
[0003] During the preparation of PEC immunosensors, the transfer of electrons is hindered due to steric hindrance. Therefore, most PEC immunosensors are of the signal attenuation type; nanozymes can be used as good signal tags for connecting detection antibodies Ab2 for signal amplification due to their advantages such as good biocompatibility, high stability, low cost, poor conductivity and easy modification; and the Ag-NH2 bond between silver nanoparticles (Ag NPs) and antibodies can effectively increase the number of Ab2 molecules on the surface of the composite material; Ag NPs can be formed in situ on the surface of Bi2MoO6 / Co3O4 composite materials to obtain Cu / CoS2-Ag NPs; Through the specific binding of antigen and antibody, different levels of CEA were fixed on the electrode, and then the fixed concentration of Cu / CoS2-Ag NPs-Ab2 was bound to the electrode through the specific reaction of CEA and Ab2, which significantly reduced the photocurrent; the proposed sandwich PEC immunosensor has ultra-high sensitivity, good reproducibility and acceptable specificity Summary of the invention
[0004] One of the purposes of the present invention is to obtain Bi2MoO6 materials with superior performance by a hydrothermal method, and to further optimize the photoelectric conversion activity by modification such as compounding; The second purpose of the present invention is to prepare a sandwich-type photoelectrochemical immunosensor with high sensitivity, strong specificity and fast detection speed based on Bi2MoO6 / Co3O4 composite material, so as to realize ultra-sensitive detection of CEA under visible light conditions;
[0005] 1. A method for preparing a sandwich-type photoelectrochemical immunosensor based on a Bi2MoO6 / Co3O4 composite material, characterized in that it comprises the following steps: 1) Cut the ITO conductive glass into 1.6×0.6 cm 2 , ultrasonically cleaned with detergent powder, acetone, ethanol and ultrapure water for 0.5 h in sequence, and dried under nitrogen; 2) Take 6 µL of 1 ~ 6 mg / mL Bi2MoO6 / Co3O4 solution and drop it onto the conductive surface of ITO conductive glass and dry it at room temperature; 3) Add 1 ~ 5 mg / mL carcinoembryonic antigen (CEA) Ab1 solution to the modified electrode surface, incubate at 4 °C for 1 h, then rinse with ultrapure water and dry naturally until a wet film is formed. 4) Add 6 µL of 1% to 3% bovine serum albumin solution to the modified electrode surface, rinse the electrode surface with ultrapure water after 0.5 h, and dry in a refrigerator at 4 °C until it becomes a wet film; 5) Add 6 µL of CEA standard solution at different concentrations, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water; 6) Add 6 µL of Cu / CoS2-silver nanoparticle-conjugated CEA antibody (Cu / CoS2-Ag NPs-Ab2) standard solution, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water to prepare a working electrode.
[0006] 2. The CEA antibody solution with a concentration of 1 μg / mL as claimed in claim 1 is obtained by diluting a 1 mg / mL CEA antibody solution purchased from Nanjing GenScript Biotechnology Co., Ltd. with phosphate buffer.
[0007] 3. The fixed concentration Cu / CoS2-Ag NPs-Ab2 solution as described in claim 1 is prepared by dissolving 3 to 6 mg Cu / CoS2-Ag NPs in 1 mL PBS (pH = 7.4), then adding 1 mg / mL CEA antibody standard solution purchased from Nanjing GenScript Biotechnology Co., Ltd., and diluting with phosphate buffer.
[0008] 4. The phosphate buffer as claimed in claim 1 is prepared by mixing 0.1 mol / L disodium hydrogen phosphate solution and 0.1 mol / L potassium dihydrogen phosphate, and the pH value thereof is adjusted to 7.4.
[0009] 5. The Cu / CoS2-Ag NPs solution as claimed in claim 3 is prepared by gradually adding 1 wt% to 5 wt% ammonia water to a 10 mg / mL AgNO3 solution to obtain a silver ammonia solution as an Ag NPs precursor solution; dissolving 50 mg to 80 mg Cu / CoS2 powder in more than 40 mL of the solution and continuously stirring the mixture in the dark at room temperature.
[0010] 6. The Cu / CoS2 powder as claimed in claim 5 is 0.8 mmol ammonium vanadate dissolved in a mixture of 19 mL deionized water and 1 mL ammonia water; 88 mg Cu / Co-ZIF nanocubes are dispersed in 80 mL ethanol, ultrasonically treated for 5 min, and then the ammonium vanadate aqueous solution is quickly injected into the Cu / Co-ZIF solution and stirred continuously for 20 s; the product Cu / Co-ZIF / polyvanadate is collected by centrifugation; Cu / Co-ZIF / polyvanadate is dispersed in 80 mL ethanol, heated at 50°C, 20 mL water is poured into the dispersion for 4 h, and the resulting product Cu / Co-vanadate is dispersed in 90 mL ethanol, heated at 90°C, and 5 mL thioacetamide is added after mechanical stirring; after 4 h, the product is collected by centrifugation and annealed in an Ar atmosphere for 2 h.
[0011] 7. The Cu / Co-ZIF as claimed in claim 6 is prepared by dissolving 219 mg of cobalt nitrate hexahydrate and 121 mg of copper nitrate in 20 mL of deionized water containing 10 mg of hexadecyltrimethylammonium bromide; then the solution is quickly injected into an aqueous solution containing 9.08 g of 2-methylimidazole, stirred at room temperature for 20 min, and collected by centrifugation.
[0012] 8. The Bi2MoO6 / Co3O4 solution according to claim 1, characterized in that the preparation steps are as follows: 3.0 g of 2-methylimidazole and 1.5 g of cobalt nitrate hexahydrate were dispersed in 40 mL of methanol, respectively, and ultrasonicated for 10 min; the 2-methylimidazole solution was then mixed with the cobalt nitrate solution, and the resulting mixture was stirred at room temperature for 24 h; the resulting mixture was collected by centrifugation and named ZIF-67; then, ZIF-67 was calcined at 550 °C for 2 h in an air atmosphere to obtain Co3O4 derived from ZIF-67; 122 mg Co3O4 was uniformly dispersed in 30 mL ethylene glycol and stirred vigorously for 20 min; then 100 mg sodium oleate, 485 mg bismuth nitrate pentahydrate and 121 mg sodium molybdate dihydrate were added to completely dissolve; then the mixture was transferred to a 100 mL polytetrafluoroethylene-lined container and stored at 140 °C for 24 h; the precipitate was collected by centrifugation and washed several times with deionized water and ethanol; then it was dried at 80 °C overnight to obtain Bi2MoO6 / Co3O4 material, and the Bi2MoO6 / Co3O4 powder was dispersed in deionized water to obtain a Bi2MoO6 / Co3O4 solution.
[0013] 9. A sandwich-type photoelectrochemical immunosensor based on Bi2MoO6 / Co3O4 composite material prepared by the preparation method according to claim 1, used for the detection of CEA, characterized in that the detection steps are as follows: 1) The test was carried out using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and a modified ITO electrode as the working electrode in 15 mL of a phosphate buffer solution with a pH of 5.0 to 8.0 and a concentration of ascorbic acid of 0.05 to 0.25 mol / L; 2) Use the time-current method to detect the CEA standard solution, set the voltage to 0 V, the running time to 120 s, and the light source wavelength to 400 ~ 500 nm; 3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; 4) Use the CEA sample solution to be tested instead of the CEA standard solution for testing.
[0014] 1. The present invention uses Bi2MoO6 material to construct a PEC sensing model for the first time, and solves the problem of low photoelectric conversion efficiency when the material is used alone through the compounding of Co3O4. The composite material has great application potential in photoelectric conversion; 2. The sandwich-type photoelectrochemical immunosensor prepared by the present invention is used for the detection of CEA, has a short response time, a low detection limit, a wide linear range, and good stability, and can achieve simple, rapid, highly sensitive and specific detection, providing a new analytical method for the early clinical detection of CEA. Specific implementation plan
[0015] Example 1 A method for preparing a sandwich-type photoelectrochemical immunosensor based on Bi2MoO6 / Co3O4 composite material: 1) Cut the ITO conductive glass into 1.6×0.6 cm 2, ultrasonically cleaned with detergent powder, acetone, ethanol and ultrapure water for 0.5 h in sequence, and dried under nitrogen; 2) Take 6 µL of 1 mg / mL Bi2MoO6 / Co3O4 solution and drop it onto the conductive surface of ITO conductive glass and let it dry at room temperature; 3) Add 5 mg / mL carcinoembryonic antigen (CEA) Ab1 solution to the modified electrode surface, incubate at 4 °C for 1 h, then rinse with ultrapure water and dry naturally until a wet film is formed; 4) Add 6 μL of 2% bovine serum albumin solution to the modified electrode surface, rinse the electrode surface with ultrapure water after 0.5 h, and dry it in a refrigerator at 4 °C until it becomes a wet film; 5) Add 6 µL of CEA standard solution at different concentrations, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water; 6) Add 6 µL of Cu / CoS2-silver nanoparticle-conjugated CEA antibody (Cu / CoS2-Ag NPs-Ab2) standard solution, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water to prepare a working electrode.
[0016] Example 2 A method for preparing a sandwich-type photoelectrochemical immunosensor based on Bi2MoO6 / Co3O4 composite material: 1) Cut the ITO conductive glass into 1.6×0.6 cm 2 , ultrasonically cleaned with detergent powder, acetone, ethanol and ultrapure water for 0.5 h in sequence, and dried under nitrogen; 2) Take 6 µL of 3 mg / mL Bi2MoO6 / Co3O4 solution and drop it onto the conductive surface of ITO conductive glass and dry it at room temperature; 3) Add 3 mg / mL carcinoembryonic antigen (CEA) Ab1 solution to the modified electrode surface, incubate at 4 °C for 1 h, then rinse with ultrapure water and dry naturally until a wet film is formed. 4) Add 6 μL of 1% bovine serum albumin solution to the modified electrode surface, rinse the electrode surface with ultrapure water after 0.5 h, and dry it in a refrigerator at 4 °C until it becomes a wet film; 5) Add 6 µL of CEA standard solution at different concentrations, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water; 6) Add 6 µL of Cu / CoS2-silver nanoparticle-conjugated CEA antibody (Cu / CoS2-Ag NPs-Ab2) standard solution, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water to prepare a working electrode.
[0017] Example 3 A method for preparing a sandwich-type photoelectrochemical immunosensor based on Bi2MoO6 / Co3O4 composite material: 1) Cut the ITO conductive glass into 1.6×0.6 cm 2 , ultrasonically cleaned with detergent powder, acetone, ethanol and ultrapure water for 0.5 h in sequence, and dried under nitrogen; 2) Take 6 µL of 6 mg / mL Bi2MoO6 / Co3O4 solution and drop it onto the conductive surface of ITO conductive glass and let it dry at room temperature; 3) Add 1 mg / mL carcinoembryonic antigen (CEA) Ab1 solution to the modified electrode surface, incubate at 4 °C for 1 h, then rinse with ultrapure water and dry naturally until a wet film is formed. 4) Add 6 μL of 3% bovine serum albumin solution to the modified electrode surface, rinse the electrode surface with ultrapure water after 0.5 h, and dry it in a refrigerator at 4 °C until it becomes a wet film; 5) Add 6 µL of CEA standard solution at different concentrations, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water; 6) Add 6 µL of Cu / CoS2-silver nanoparticle-conjugated CEA antibody (Cu / CoS2-Ag NPs-Ab2) standard solution, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water to prepare a working electrode.
[0018] Example 4 Preparation of Bi2MoO6 / Co3O4 composite material: 3.0 g of 2-methylimidazole and 1.5 g of cobalt nitrate hexahydrate were dispersed in 40 mL of methanol, respectively, and ultrasonicated for 10 min; the 2-methylimidazole solution was then mixed with the cobalt nitrate solution, and the resulting mixture was stirred at room temperature for 24 h; the resulting mixture was collected by centrifugation and named ZIF-67; then, ZIF-67 was calcined at 550 °C for 2 h in an air atmosphere to obtain Co3O4 derived from ZIF-67; 122 mg Co3O4 was uniformly dispersed in 30 mL ethylene glycol and stirred vigorously for 20 min; then 100 mg sodium oleate, 485 mg bismuth nitrate pentahydrate and 121 mg sodium molybdate dihydrate were added to completely dissolve; then the mixture was transferred to a 100 mL polytetrafluoroethylene-lined container and stored at 140 °C for 24 h; the precipitate was collected by centrifugation and washed several times with deionized water and ethanol; then it was dried at 80 °C overnight to obtain Bi2MoO6 / Co3O4 material, and the ground powder was prepared into an aqueous solution with a concentration of 3 mg / mL.
[0019] Example 5 Preparation of Bi2MoO6 / Co3O4 composite material: 1.0 g of 2-methylimidazole and 0.5 g of cobalt nitrate hexahydrate were dispersed in 40 mL of methanol, respectively, and ultrasonicated for 10 min; the 2-methylimidazole solution was then mixed with the cobalt nitrate solution, and the resulting mixture was stirred at room temperature for 24 h; the resulting mixture was collected by centrifugation and named ZIF-67; then, ZIF-67 was calcined at 550 °C for 2 h in an air atmosphere to obtain Co3O4 derived from ZIF-67; 61 mg Co3O4 was evenly dispersed in 30 mL ethylene glycol and stirred vigorously for 20 min; then 50 mg sodium oleate, 247.5 mg bismuth nitrate pentahydrate and 60.5 mg sodium molybdate dihydrate were added to completely dissolve; then transferred to a 100 mL polytetrafluoroethylene-lined container and stored at 140 °C for 24 h; the precipitate was collected by centrifugation and washed several times with deionized water and ethanol; then dried at 80 °C overnight to obtain Bi2MoO6 / Co3O4 material, and the ground powder was configured into an aqueous solution with a concentration of 2 mg / mL.
[0020] Example 6 Preparation of Bi2MoO6 / Co3O4 composite material: 6.0 g of 2-methylimidazole and 3.0 g of cobalt nitrate hexahydrate were dispersed in 40 mL of methanol, respectively, and ultrasonicated for 10 min; the 2-methylimidazole solution was then mixed with the cobalt nitrate solution, and the resulting mixture was stirred at room temperature for 24 h; the resulting mixture was collected by centrifugation and named ZIF-67; then, ZIF-67 was calcined at 550 °C for 2 h in an air atmosphere to obtain Co3O4 derived from ZIF-67; 244 mg Co3O4 was evenly dispersed in 30 mL ethylene glycol and stirred vigorously for 20 min; then 200 mg sodium oleate, 970 mg bismuth nitrate pentahydrate and 242 mg sodium molybdate dihydrate were added to completely dissolve; then the mixture was transferred to a 100 mL polytetrafluoroethylene-lined container and stored at 140 °C for 24 h; the precipitate was collected by centrifugation and washed several times with deionized water and ethanol; then it was dried at 80 °C overnight to obtain Bi2MoO6 / Co3O4 material, and the ground powder was prepared into an aqueous solution with a concentration of 5 mg / mL.
[0021] Example 7 Preparation of Cu / CoS2-Ag NPs-Ab2 solution: Cu / Co-ZIF was prepared by dissolving 219 mg of cobalt nitrate hexahydrate and 121 mg of copper nitrate in 20 mL of deionized water containing 10 mg of hexadecyltrimethylammonium bromide. The solution was then quickly injected into an aqueous solution containing 9.08 g of 2-methylimidazole, stirred at room temperature for 20 min, and collected by centrifugation. Cu / CoS2 powder was prepared by dissolving 0.8 mmol ammonium vanadate in a mixture of 19 mL deionized water and 1 mL ammonia water; 88 mg Cu / Co-ZIF nanocubes were dispersed in 80 mL ethanol and ultrasonically treated for 5 min, then the ammonium vanadate aqueous solution was quickly injected into the Cu / Co-ZIF solution and stirred continuously for 20 s; the product Cu / Co-ZIF / polyvanadate was collected by centrifugation; Cu / Co-ZIF / polyvanadate was dispersed in 80 mL ethanol, heated at 50 °C, 20 mL water was poured into the dispersion for 4 h, and the resulting product Cu / Co-vanadate was dispersed in 90 mL ethanol, heated at 90 °C, and 5 mL thioacetamide was added after mechanical stirring; after 4 h, the product was collected by centrifugation and annealed in an Ar atmosphere for 2 h; 1 wt% ammonia water was gradually added to 10 mg / mL AgNO3 solution to obtain a silver ammonia solution as the Ag NPs precursor solution; 80 mg Cu / CoS2 powder was dissolved in 40 mL or more of the solution, stirred continuously in the dark at room temperature; 3 mg Cu / CoS2-Ag NPs were dissolved in 1 mL PBS (pH = 7.4), and then 1 mg / mL CEA antibody standard solution was added and diluted with phosphate buffer.
[0022] Example 8 Preparation of Cu / CoS2-Ag NPs-Ab2 solution: Cu / Co-ZIF was prepared by dissolving 219 mg of cobalt nitrate hexahydrate and 121 mg of copper nitrate in 20 mL of deionized water containing 10 mg of hexadecyltrimethylammonium bromide. The solution was then quickly injected into an aqueous solution containing 9.08 g of 2-methylimidazole, stirred at room temperature for 20 min, and collected by centrifugation. Cu / CoS2 powder was prepared by dissolving 0.8 mmol ammonium vanadate in a mixture of 19 mL deionized water and 1 mL ammonia water; 44 mg Cu / Co-ZIF nanocubes were dispersed in 80 mL ethanol and ultrasonically treated for 5 min, then the ammonium vanadate aqueous solution was quickly injected into the Cu / Co-ZIF solution and stirred continuously for 20 s; the product Cu / Co-ZIF / polyvanadate was collected by centrifugation; Cu / Co-ZIF / polyvanadate was dispersed in 80 mL ethanol, heated at 50 °C, 20 mL water was poured into the dispersion for 4 h, and the resulting product Cu / Co-vanadate was dispersed in 90 mL ethanol, heated at 90 °C, and 5 mL thioacetamide was added after mechanical stirring; after 4 h, the product was collected by centrifugation and annealed in an Ar atmosphere for 2 h; 3 wt% ammonia water was gradually added to 10 mg / mL AgNO3 solution to obtain a silver ammonia solution as the Ag NPs precursor solution; 50 mg Cu / CoS2 powder was dissolved in 40 mL or more of the solution, stirred continuously in the dark at room temperature; 6 mg Cu / CoS2-Ag NPs were dissolved in 1 mL PBS (pH = 7.4), and then 1 mg / mL CEA antibody standard solution was added and diluted with phosphate buffer.
[0023] Example 9 Preparation of Cu / CoS2-Ag NPs-Ab2 solution: Cu / Co-ZIF was prepared by dissolving 219 mg of cobalt nitrate hexahydrate and 121 mg of copper nitrate in 40 mL of deionized water containing 10 mg of hexadecyltrimethylammonium bromide. The solution was then quickly injected into an aqueous solution containing 9.08 g of 2-methylimidazole, stirred at room temperature for 20 min, and collected by centrifugation. Cu / CoS2 powder was prepared by dissolving 1.6 mmol ammonium vanadate in a mixture of 19 mL deionized water and 1 mL ammonia water; 88 mg Cu / Co-ZIF nanocubes were dispersed in 80 mL ethanol, ultrasonically treated for 5 min, and then the ammonium vanadate aqueous solution was quickly injected into the Cu / Co-ZIF solution and stirred continuously for 20 s; the product Cu / Co-ZIF / polyvanadate was collected by centrifugation; Cu / Co-ZIF / polyvanadate was dispersed in 80 mL ethanol, heated at 50 °C, 20 mL water was poured into the dispersion for 4 h, and the resulting product Cu / Co-vanadate was dispersed in 90 mL ethanol, heated at 90 °C, and 5 mL thioacetamide was added after mechanical stirring; after 4 h, the product was collected by centrifugation and annealed in an Ar atmosphere for 2 h. 2 wt% ammonia water was gradually added to 10 mg / mL AgNO3 solution to obtain silver ammonia solution as Ag NPs precursor solution; 60 mg Cu / CoS2 powder was dissolved in more than 40 mL of solution and stirred continuously in the dark at room temperature; 6 mg Cu / CoS2-Ag NPs were dissolved in 1 mL PBS (pH = 7.4), and then 1 mg / mL CEA antibody standard solution was added and diluted with phosphate buffer.
[0024] Example 10 Detection of CEA: (1) The test was carried out using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode. The test was carried out in 15 mL of PBS buffer solution with a pH of 5.5 and a concentration of 0.1 mol / L ascorbic acid. (2) Use the time-current method to detect the CEA standard solution, set the voltage to 0 V, the running time to 120 s, and the light source wavelength to 400 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Use the CEA sample solution to be tested instead of the CEA standard solution for testing.
[0025] Example 11 Detection of CEA: (1) The test was carried out using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode. The test was carried out in 15 mL of PBS buffer solution with a pH of 7.4 and a concentration of 0.2 mol / L ascorbic acid. (2) Use the time-current method to detect the CEA standard solution, set the voltage to 0 V, the running time to 120 s, and the light source wavelength to 450 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Use the CEA sample solution to be tested instead of the CEA standard solution for testing.
[0026] Example 12 Detection of CEA: (1) The test was carried out using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and the prepared ITO modified electrode as the working electrode. The test was carried out in 15 mL of PBS buffer solution with a pH of 8.0 and a concentration of 1.5 mol / L ascorbic acid. (2) Use the time-current method to detect the CEA standard solution, set the voltage to 0 V, the running time to 120 s, and the light source wavelength to 500 nm; (3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; (4) Use the CEA sample solution to be tested instead of the CEA standard solution for testing.
Claims
1. A Bi-based 2 MoO 6 / Co 3 O 4 Preparation method of sandwich-type photoelectrochemical immunosensor of composite materials, It is characterized in that The following steps are involved: 1) Cut the ITO conductive glass into 1.6×0.6 cm 2 , ultrasonically cleaned with detergent powder, acetone, ethanol and ultrapure water for 0.5 h in sequence, and dried under nitrogen; 2) Take 6 µL of 1 ~ 6 mg / mL Bi 2 MoO 6 / Co 3 O 4 The solution was dripped onto the conductive surface of the ITO conductive glass and dried at room temperature; 3) Add 1 ~ 5 mg / mL of carcinoembryonic antigen (CEA) Ab to the surface of the modified electrode 1 The solution was incubated at 4 °C for 1 h, then washed with ultrapure water and dried naturally until a wet film was formed; 4) Add 6 µL of 1% to 3% bovine serum albumin solution to the modified electrode surface, rinse the electrode surface with ultrapure water after 0.5 h, and dry in a refrigerator at 4 °C until it becomes a wet film; 5) Add 6 µL of CEA standard solution at different concentrations, incubate at 4 °C for 4 h, and then rinse the electrode surface with ultrapure water; 6) Add 6 µL Cu / CoS 2 - CEA antibody conjugated with silver nanoparticles (Cu / CoS 2 -Ag NPs-Ab 2 ) standard solution, incubate at 4℃ for 4 h, and then rinse the electrode surface with ultrapure water to prepare the working electrode.
2. A Bi-based 2 MoO 6 / Co 3 O 4 Preparation method of sandwich-type photoelectrochemical immunosensor of composite materials, It is characterized in that The Bi 2 MoO 6 / Co 3 O 4 , the preparation steps are as follows: 1) 3.0 g of 2-methylimidazole and 1.5 g of cobalt nitrate hexahydrate were dispersed in 40 mL of methanol and ultrasonicated for 10 min. The 2-methylimidazole solution was then mixed with the cobalt nitrate solution, and the resulting mixture was stirred at room temperature for 24 h. The resulting mixture was collected by centrifugation and named ZIF-67. Then, ZIF-67 was calcined at 550 °C for 2 h in an air atmosphere to obtain Co derived from ZIF-67. 3 O 4 ; 2) 122 mg Co 3 O 4 The mixture was uniformly dispersed in 30 mL of ethylene glycol and stirred vigorously for 20 min. Then, 100 mg of sodium oleate, 485 mg of bismuth nitrate pentahydrate and 121 mg of sodium molybdate dihydrate were added to completely dissolve the mixture. The mixture was then transferred to a 100 mL polytetrafluoroethylene-lined container and stored at 140 °C for 24 h. The precipitate was collected by centrifugation and washed several times with deionized water and ethanol. The precipitate was then dried at 80 °C overnight to obtain Bi 2 MoO 6 / Co 3 O 4 Material.
3. A Bi-based 2 MoO 6 / Co 3 O 4 Composite sandwich-type photoelectrochemical immunosensor, It is characterized in that The sensor is used for carcinoembryonic antigen (CEA) detection. The detection steps are as follows: 1) The test was carried out using an electrochemical workstation with a three-electrode system, with a saturated calomel electrode as the reference electrode, a platinum wire electrode as the auxiliary electrode, and a sandwich photoelectrochemical immunosensor as the working electrode. The test was carried out in 15 mL of a phosphate buffer solution with a pH of 5.0 to 8.0 and a concentration of ascorbic acid of 0.05 to 0.25 mol / L. 2) Use the time-current method to detect the CEA standard solution, set the voltage to 0 V, the running time to 120 s, and the light source wavelength to 400 ~ 500 nm; 3) After the electrodes are placed, turn on the light every 20 seconds for 20 seconds, record the photocurrent, and draw a working curve; 4) Use the CEA sample solution to be tested instead of the CEA standard solution for testing.