Method for preparing recycled concrete aggregate test specimen, testing device and testing method

By using dilute hydrochloric acid etching and cyclic impregnation with a composite regulating solution, a stable active regulating layer is formed, which solves the problem of integrated design of surface activity regulation and specimen structure in the preparation of recycled concrete aggregate specimens, and ensures the accuracy of bonding performance testing.

CN122409291APending Publication Date: 2026-07-17江苏创驰新材料科技有限公司

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
江苏创驰新材料科技有限公司
Filing Date
2026-05-29
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing methods for preparing recycled concrete aggregate specimens lack integrated design of surface activity regulation and specimen structure, leading to instability in the interfacial transition zone and affecting the accuracy of bond performance test results.

Method used

The recycled aggregate is activated by acid etching with dilute hydrochloric acid, and a composite regulating solution is prepared for cyclic impregnation treatment to form a stable active regulating layer. During the drying and activation curing process, a continuous active regulating layer is formed, which is then directly mixed with cement and fine aggregate to form a mold.

Benefits of technology

This design achieves true integration of surface activity regulation and specimen structure, ensuring the stability of the interface transition zone and the accuracy of adhesion performance testing, and preventing the regulation layer from falling off or being damaged during the molding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122409291A_ABST
    Figure CN122409291A_ABST
Patent Text Reader

Abstract

本发明涉及再生混凝土骨料技术领域,具体涉及一种再生混凝土骨料试件制备方法、测试装置和测试方法:首先,稀盐酸酸蚀活化去除了骨料表面松散杂质并暴露微观粗糙基底;其次,配制的复合调控液中含有硅酸钠活性基团与纳米二氧化硅填充组分,可实现化学活化与物理填充的协同效应;再次,循环浸渍处理使调控液深度渗透入骨料表层孔隙,形成机械互锁锚固;然后,分段干燥固化在骨料表面形成连续稳定的活性调控层;最后,经表面干燥与活化固化后的骨料直接与水泥、细骨料、水及外加剂混合搅拌并浇筑成型。本技术方案实现了表面活性调控与试件结构的真正一体化设计,避免了调控层在后续成型过程中的脱落或破坏。