An electrolyte injection amount determination method, device, equipment and storage medium
By calculating the basic electrolyte injection volume and the permeation loss model of the power battery, the target electrolyte injection volume is determined to compensate for electrolyte permeation and side reaction losses, thus solving the problem of insufficient electrolyte at the end of the power battery's life and achieving a long battery life and high energy density.
Patent Information
- Application Number
- CN202611413810.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-11
- Publication Date
- 2026-11-10
AI Technical Summary
In existing technologies, the loss of electrolyte due to long-term use of power batteries cannot be observed or compensated, resulting in insufficient electrolyte at the end of the battery's life, causing a drop in capacity. Furthermore, excessive electrolyte injection will sacrifice energy density and increase costs.
By determining the basic electrolyte injection volume, expected permeation loss, and safety factor of the power battery, and combining the electrolyte permeation loss model, the target electrolyte injection volume is calculated to compensate for permeation and side reaction losses, ensuring that the electrolyte is sufficient throughout the entire life cycle.
This effectively avoids the sudden drop in performance caused by insufficient electrolyte at the end of the battery's life, ensuring the battery's long lifespan and reliability, while also improving energy density and economy.
Smart Images

Figure CN123073370A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of battery electrolyte filling technology, and in particular to a method, apparatus, equipment and storage medium for determining the electrolyte filling volume. Background Technology
[0002] For power batteries, there will be a significant loss of total electrolyte volume in the cells during long-term use. This loss mainly occurs through long-term, slow physical penetration and diffusion in the form of vapor or liquid phase through the sealed interface of the battery. Even if the airtightness test is passed, this penetration loss cannot be eliminated.
[0003] Traditional battery electrolyte filling designs generally overlook long-term seepage losses. This can lead to insufficient electrolyte levels and a significant drop in capacity towards the end of the battery's lifespan. Conversely, excessive electrolyte filling to compensate for these seepage losses sacrifices energy density and increases manufacturing costs. Summary of the Invention
[0004] The main objective of this application is to provide a method, apparatus, device, and storage medium for determining the electrolyte injection volume, aiming to solve the problem that the long-term electrolyte permeation loss cannot be observed when the battery is in a sealed state, and to avoid the technical problem of a sudden drop in performance due to insufficient electrolyte at the end of the battery's life.
[0005] To achieve the above objectives, this application provides a method for determining the electrolyte injection volume, the steps of which include: The basic electrolyte injection volume of the power battery is determined based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions. Based on the expected operating temperature profile of the sealing system of the power battery, the preset full life cycle and the preset electrolyte permeation loss model, the expected permeation loss corresponding to the electrolyte permeation of the sealing system is determined. The target electrolyte injection volume for the power battery is determined based on the basic injection volume, the expected permeation loss, and the preset safety factor.
[0006] In one embodiment, after determining the basic injection volume, the following steps are further included: The electrolyte injection process parameters of the power battery are determined based on the target electrolyte injection volume. Power battery samples were prepared based on the liquid injection process parameters, and accelerated aging tests were conducted on the power battery samples. The actual amount of electrolyte remaining in the tested power battery samples was measured using a solvent extraction method. Based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, the model parameters of the preset electrolyte permeation loss model are adjusted until the difference in remaining amount is lower than the preset first threshold, so that the expected permeation loss calculated by the preset electrolyte permeation loss model after updating the model parameters is close to the actual permeation loss of the electrolyte.
[0007] In one embodiment, before the step of adjusting the model parameters of the preset electrolyte permeation loss model based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, the method further includes: The expected amount of electrolyte remaining is determined based on the expected permeation loss, expected consumption, and target injection volume.
[0008] In one embodiment, the step of determining the basic electrolyte injection volume of the power battery, based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions, includes: Obtain the preset liquid storage space parameters of the power battery, and determine the minimum liquid injection volume based on the preset liquid storage space parameters. The preset liquid storage space parameters include the electrode parameters of the battery cell and the separator parameters. Based on the preset side reaction parameters and preset electrochemical aging model of the power battery, the expected consumption is determined. The preset side reaction parameters include at least the target cycle life and target storage life of the power battery. The base injection volume is determined based on the minimum injection volume and the expected consumption.
[0009] In one embodiment, the electrode parameters include the electrode coating amount, electrode compaction density, and electrode material density, and the diaphragm parameters include the diaphragm volume and diaphragm porosity. Determining the minimum injection volume based on preset liquid storage space parameters includes the following steps: The porosity of the electrode coating is determined based on the electrode compaction density and the electrode material density. The electrode pore volume is determined based on the coating porosity and the electrode coating amount. The pore volume of the diaphragm is determined based on the diaphragm volume and the diaphragm porosity. The minimum injection volume is determined based on the electrode pore volume and the diaphragm pore volume.
[0010] In one embodiment, the method for constructing a preset electrolyte permeation loss model specifically includes the following steps: Long-term storage tests were conducted on the sealing system of the power battery, and the actual effective permeability of the sealing system to electrolyte at different temperatures was determined based on the test results. By fitting the actual effective permeability at different temperatures, the Arrhenius equation is used to determine the permeation activation energy and pre-exponential factor of the sealed system. A pre-defined electrolyte permeation loss model was established based on the osmotic activation energy and the pre-exponential factor.
[0011] In one embodiment, after establishing the preset electrolyte permeation loss model, the following steps are also included: Material-level permeation tests were conducted on the sealing materials used in the sealing system, and the steady-state permeability of the sealing materials to electrolyte at different temperatures was determined based on the test results. When the error between the steady-state permeability at the preset temperature and the actual effective permeability exceeds the preset error, the method for constructing the preset electrolyte permeation loss model is re-executed.
[0012] Furthermore, to achieve the above objectives, this application also provides an electrolyte injection volume determination device, which includes: The basic electrolyte injection assessment module is used to determine the basic electrolyte injection amount of the power battery based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions. The permeation prediction module is used to determine the expected permeation loss corresponding to electrolyte permeation in the sealing system based on the expected operating temperature profile of the power battery sealing system, the preset full life cycle, and the preset electrolyte permeation loss model. The liquid injection volume calculation module is used to determine the target liquid injection volume of the power battery based on the basic liquid injection volume, the expected permeation loss, and the preset safety factor.
[0013] In addition, to achieve the above objectives, this application also provides an electrolyte injection volume determination device, which includes: a memory, a processor, and an electrolyte injection volume determination program stored in the memory and executable on the processor. The electrolyte injection volume determination program is configured to implement the steps of the electrolyte injection volume determination method as described above.
[0014] In addition, to achieve the above objectives, this application also provides a storage medium, which is a computer-readable storage medium, and stores an electrolyte injection volume determination program on the computer-readable storage medium. When the electrolyte injection volume determination program is executed by a processor, it implements the steps of the electrolyte injection volume determination method as described above.
[0015] This application provides a method, apparatus, equipment, and storage medium for determining the electrolyte injection volume. The method first calculates a base injection volume based on the cell's immersion requirements and electrolyte side reaction losses. Then, by inputting the expected operating temperature profile of the power battery and a preset full lifespan into a preset electrolyte permeation loss model, it predicts the expected permeation loss due to prolonged permeation. Simultaneously, a preset safety factor, considering individual differences, corrects the expected permeation loss as compensation for the base injection volume, thus obtaining the target injection volume for the power battery. This target volume serves as the basis for setting the injection process parameters. During the power battery electrolyte injection volume design stage, the expected permeation loss due to electrolyte side reactions is included in the total electrolyte volume calculation. This prevents the power battery from experiencing a capacity drop at the end of its lifespan due to insufficient electrolyte caused by long-term electrolyte side reaction losses, ensuring the long lifespan and reliability of the power battery. Attached Figure Description
[0016] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this application and, together with the description, serve to explain the principles of this application.
[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1 A flowchart illustrating an embodiment of the electrolyte injection volume determination method of this application; Figure 2 A flowchart illustrating an embodiment of the electrolyte injection volume determination method of this application; Figure 3 This is a flowchart illustrating an embodiment of the method for determining the electrolyte injection volume in this application. Figure 4 A flowchart illustrating an embodiment of the electrolyte injection volume determination method of this application; Figure 5 A flowchart illustrating an embodiment of the electrolyte injection volume determination method of this application; Figure 6 A schematic diagram of the module structure provided for an embodiment of the electrolyte injection volume determination device of this application; Figure 7 This is a schematic diagram of the structure of the electrolyte injection volume determination device provided in this application.
[0019] The purpose, features, and advantages of this application will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0020] It should be understood that the specific embodiments described herein are merely illustrative of the technical solutions of this application and are not intended to limit this application.
[0021] To better understand the technical solution of this application, a detailed description will be provided below in conjunction with the accompanying drawings and specific implementation methods.
[0022] The electrolyte injection volume determination method provided in this application can be executed by a device with data processing capabilities, specifically a processor within that device. This electronic device is primarily used during the design and manufacturing process of power batteries to provide corresponding electrolyte injection process parameters for different types of power batteries, thereby controlling the volume of electrolyte injected into the semi-finished power battery product and ensuring that the battery product's performance meets standards and exhibits excellent consistency.
[0023] It's easy to understand that if the electrolyte in a power battery cannot fill all the pores of the electrodes and separator, dry areas will form, preventing the lithium battery from conducting properly. These dry areas can lead to localized overcharging and lithium plating, resulting in a sharp drop in capacity or even internal short circuits. Throughout the entire lifespan of a power battery, the electrolyte will decompose due to long-term infiltration or internal side reactions, resulting in a certain amount of loss. In the design of electrolyte injection volume, electrolyte loss caused by side reaction decomposition is a process that follows electrochemical kinetics and can be accurately predicted using chemical principles. However, electrolyte loss due to long-term infiltration is a continuous, invisible physical diffusion process that cannot be directly observed after the battery has been manufactured and used for a long time. Therefore, electrolyte loss due to long-term infiltration is usually ignored, leading to a significant capacity drop at the end of the battery's life due to insufficient total electrolyte volume, severely impacting battery reliability and lifespan.
[0024] Based on the above, this application proposes a first embodiment of a method for determining the electrolyte injection volume. Please refer to [the relevant documentation]. Figure 1 The method for determining the electrolyte injection volume includes the following steps: Step S10: Determine the basic electrolyte injection volume of the power battery based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions.
[0025] It should be noted that, in this embodiment, the minimum electrolyte injection volume refers to the physical requirement that can just submerge and fill all the pores of the battery cell (including the pores of the electrode active material, the pores of the separator, etc.); the expected consumption volume refers to the amount of chemical loss that can be made up for by the electrolyte during the entire life cycle of the battery due to side reactions; and the basic electrolyte injection volume refers to the total volume that can just meet the above physical and chemical requirements during the entire life cycle of the battery, without considering that the battery sealing system will be permeated for a long time.
[0026] It is easy to understand that in this embodiment, the minimum amount of electrolyte that can just submerge the battery cell in the new battery state can be determined first by the internal design structure of the power battery. Then, the estimated amount of electrolyte that will inevitably be consumed due to side reactions during the entire battery life cycle is used as compensation, and finally the above-mentioned basic amount of electrolyte can be calculated.
[0027] Specifically, the formula for calculating the basic injection volume is as follows: ; in, Basic injection volume; Minimum injection volume; This represents the expected consumption.
[0028] Furthermore, please combine Figure 2 To understand this, in this embodiment, the steps for determining the basic electrolyte injection volume of the power battery, based on the minimum amount of electrolyte required to fully wet the battery cell and the expected consumption of electrolyte due to internal side reactions, include: Step S11: Obtain the preset liquid storage space parameters of the power battery, and determine the minimum liquid injection volume based on the preset liquid storage space parameters. The preset liquid storage space parameters include the electrode parameters of the battery cell and the separator parameters.
[0029] It should be noted that, in this embodiment, the preset electrolyte storage space parameters refer to the size-related parameters of the power battery in the electrolyte storage design, which may include at least electrode parameters and separator parameters. Electrode parameters are quantifiable parameters used to describe the physical properties of the electrode (positive and / or negative electrode) coating and its electrolyte storage capacity, while separator parameters are quantifiable parameters used to describe the physical structure of the separator and its electrolyte storage capacity.
[0030] Electrode parameters and separator parameters determine the spatial dimensions of the electrode coating and separator, which indirectly determines the required volume of electrolyte used to fill the electrode and separator pores. In this embodiment, the dimensional parameters corresponding to the space for storing electrolyte formed by the physical structure of the power battery can be determined based on the dimensional parameters related to the physical structure design, i.e., preset electrolyte storage space parameters. This allows for the determination of the minimum electrolyte injection volume required to precisely submerge these key physical structures.
[0031] Specifically, please combine Figure 3 To understand, in this embodiment, the electrode parameters include the electrode coating amount, electrode compaction density, and electrode material density, and the diaphragm parameters include the diaphragm volume and diaphragm porosity. Determining the minimum injection volume based on preset liquid storage space parameters includes the following steps: Step S111: Determine the coating porosity of the electrode coating based on the electrode compaction density and the electrode material density.
[0032] Step S112: Determine the electrode pore volume based on the coating porosity and the electrode coating amount.
[0033] It should be noted that, in this embodiment, the actual density of the electrode sheet refers to the apparent density of the electrode coating after compression by the rolling process; the density of the electrode material refers to the theoretical true density of the inherent components in the electrode coating after mixing; the porosity of the electrode sheet refers to the proportion of the pore volume in the electrode coating to the total volume of the coating, which characterizes the density of the coating; the electrode coating amount refers to the total amount of all solid components, such as active materials, contained in the electrode coating; and the electrode pore volume refers to the total volume of all micropores inside the electrode coating that can be filled by the electrolyte.
[0034] It should be understood that, in this embodiment, the electrode coating may include a positive electrode coating and a negative electrode coating, which typically differ in material selection and structural design. Therefore, the aforementioned electrode compaction density, electrode material density, coating porosity, electrode coating amount, and electrode pore volume can also be divided into two sets of parameters corresponding to the positive and negative electrodes, respectively.
[0035] It is easy to understand that, in this embodiment, for any type of electrode, the mass remains essentially unchanged before and after the rolling process. Therefore, the porosity of the electrode coating, i.e., the aforementioned coating porosity, can be determined using the electrode sheet compaction density and the electrode sheet material density. The electrode sheet coating volume can be calculated using the known electrode sheet coating amount and electrode sheet compaction density. Finally, the electrode pore volume corresponding to the electrode sheet can be determined by multiplying the coating porosity and the electrode sheet coating volume.
[0036] Step S113: Determine the pore volume of the diaphragm based on the diaphragm volume and the diaphragm porosity.
[0037] It should be noted that in this embodiment, the membrane volume refers to the geometric volume occupied by the membrane structure; the membrane porosity refers to the proportion of the membrane structure volume occupied by the pores inside the membrane. Both are structural parameters of the membrane itself and are known quantities provided by the membrane product at the time of manufacture; the membrane pore volume refers to the total volume occupied by all connected or semi-connected microchannels inside the membrane, that is, the part of the apparent geometric volume of the membrane that can be filled by electrolyte.
[0038] It is easy to understand that, in this embodiment, the diaphragm void volume can be directly determined by the product of the known diaphragm volume and the diaphragm porosity.
[0039] Step S114: Determine the minimum injection volume based on the electrode pore volume and the diaphragm pore volume.
[0040] It is easy to understand that the electrode pore volume reflects the volume of electrolyte that can be stored in the electrode structure, while the membrane pore volume reflects the volume of electrolyte that can be stored in the membrane structure. Together, they constitute the main space size inside the battery cell that can store electrolyte. In this embodiment, the electrode pore volume (including the positive electrode pore volume and the negative electrode pore volume) can be added to the membrane pore volume to obtain the minimum amount of electrolyte that can just wet the battery cell and the membrane.
[0041] Specifically, the formula for calculating the minimum injection volume is as follows: ; in, This represents the positive electrode pore volume; The negative electrode pore volume; This represents the pore volume of the diaphragm.
[0042] Step S12: Based on the preset side reaction parameters of the power battery and the preset electrochemical aging model, determine the expected consumption. The preset side reaction parameters include at least the target cycle life and target storage life of the power battery.
[0043] It should be noted that, in this embodiment, the preset electrochemical aging model refers to a side reaction kinetic model established based on the Arrhenius equation. It is mainly used to estimate the volume of electrolyte consumed by the battery during cycling and storage due to internal side reactions such as solid electrolyte interphase (SEI) film growth and electrolyte decomposition, i.e., the aforementioned expected consumption. The preset side reaction parameters refer to relevant parameters for electrolyte side reactions, including at least the battery's target cycle life, target storage life, average operating temperature, electrode surface area (specifically, negative electrode surface area), SEI model growth rate constant, SEI model growth activation energy, and electrolyte decomposition reaction rate.
[0044] Average operating temperature refers to the average temperature of the battery when used under normal operating conditions, which is a known quantity that can be obtained in advance based on operating condition statistics; electrode surface area refers to the area of the negative electrode surface where side reactions can occur, which is a known quantity that can be obtained in advance based on electrode design; SEI film growth rate constant refers to the reference rate of SEI film growth per unit area, which is a known quantity that can be obtained through aging tests; SEI film growth activation energy refers to the energy barrier that needs to be overcome during the growth process, which is a known quantity that can be calculated based on the material system characteristic parameters; electrolyte decomposition reaction rate refers to the decomposition rate of the electrolyte, which is a known quantity that can be measured and calibrated through high-temperature tests.
[0045] It should be noted that, in this embodiment, the target cycle life refers to the number of standard charge-discharge cycles that the power battery is expected to complete from the start of use until its capacity decays to the preset failure threshold under the design conditions; the target storage life refers to the time that the power battery is expected to experience from the start of storage until its capacity decays to the preset failure threshold under specific storage conditions.
[0046] It is worth noting that in this embodiment, in the preset electrochemical aging model, cycle consumption and storage consumption are calculated independently and then summed. It is not necessary to forcibly convert the number of cycles into time; only an integration upper limit needs to be set for each. The target storage lifetime can usually be equal to the preset total lifetime, serving as the upper limit boundary for calculating the storage consumption portion; while the target cycle lifetime can serve as the upper limit boundary for the cycle consumption portion.
[0047] It is easy to understand that, in this embodiment, the target cycle life and target storage life (preset full life cycle) of the battery design, as well as the other known quantities mentioned above, can be substituted into the preset electrochemical aging model to calculate the expected consumption of electrolyte due to internal side reactions within the preset full life cycle of the battery.
[0048] Step S13: Determine the base injection volume based on the minimum injection volume and the expected consumption volume.
[0049] It is easy to understand that the minimum injection volume ensures the initial physical wetting requirements of the cell, while the expected consumption volume compensates for subsequent electrolyte chemical losses caused by internal side reactions. Neither of these factors involves physical permeation losses from the sealing system. In this embodiment, combining the minimum injection volume with the expected consumption volume yields the basic injection volume without considering electrolyte permeation during sealing.
[0050] Step S20: Based on the expected operating temperature profile of the sealing system of the power battery, the preset full life cycle, and the preset electrolyte permeation loss model, determine the expected permeation loss corresponding to electrolyte permeation in the sealing system.
[0051] It should be noted that, in this embodiment, the sealing system refers to the sealing interface formed between the battery terminals and the cover plate of the aforementioned power battery by an elastic sealing ring material (such as fluororubber); the preset full life cycle refers to the target operating time or equivalent operating time of the power battery from the start of use to the end of its life, determined during the design phase. It can also be understood as the design life index of the battery. For example, the power battery of electric vehicles is usually set to 15 years or the equivalent number of charge-discharge cycles (5000 times); the expected operating temperature profile refers to the correlation function of the thermodynamic temperature of the sealing interface of the power battery changing with time within its preset full life cycle; the preset electrolyte permeation loss model is a dynamic model constructed based on the physical characteristics of the sealing system itself, with temperature and time as the core variables, which can reflect the law of electrolyte permeation change with temperature and time.
[0052] Electrolyte permeation in a sealed system is a long-term, continuous physical process. It can occur primarily through vapor evaporation and diffusion from the sealant, or through liquid seepage through the micropores of the sealing material. Regardless of the method, the organic solvent components in the electrolyte will continuously seep out under temperature-driven conditions, and the permeation rate is significantly affected by temperature.
[0053] Electrolyte permeation rate exhibits an exponential relationship with temperature, following the Arrhenius law. Therefore, when calculating the expected permeation loss, the temperature variation trend throughout the battery's lifespan needs to be considered. In this embodiment, to address the above situation, the expected operating temperature profile can be input as a temperature variable into a pre-established electrolyte permeation loss model, while a pre-defined lifespan can be input as a time variable. This transforms the previously invisible, minute losses caused by long-term electrolyte permeation into a quantifiable predictable value, which is the aforementioned expected permeation loss.
[0054] Step S30: Determine the target liquid injection volume of the power battery based on the basic liquid injection volume, the expected permeation loss, and the preset safety factor.
[0055] It should be noted that, in this embodiment, the target liquid injection volume refers to the total volume that can ensure the battery meets both the physical and chemical requirements throughout its entire life cycle, taking into account the long-term permeation of the battery sealing system. The preset safety factor is an engineering boundary that is pre-quantified based on multiple batches of test data of the material / structure system, with a preset statistical confidence level (e.g., 99.5%) as a constraint. It is used to cover the uncertainty and individual differences of the model's predicted values, and its value range can be [1.0, 2.0].
[0056] In this embodiment, by multiplying the expected permeation loss by a preset safety factor as a permeation loss prediction value with high confidence and incorporating it into the forward design, and then superimposing it with the basic electrolyte injection volume, the total electrolyte injection volume (target electrolyte injection volume) covering all major loss pathways throughout the entire life cycle of the power battery can be obtained, thus realizing the scientific calculation of the total electrolyte volume.
[0057] Specifically, the formula for calculating the target injection volume is as follows: ; in, Preset safety factor; The target injection volume; Basic injection volume; This represents the expected penetration loss.
[0058] It is worth noting that in this embodiment, the method for determining the preset safety factor is as follows: First, long-term test data of n different batches of sealing systems are collected to determine the actual permeability of each group and the permeability distribution. Then, the predicted permeability calculated by the preset electrolyte permeation loss model is compared with the actual permeability of each group, ensuring that the two satisfy the following relationship: ; in, To predict penetration rate; This represents the true penetration rate. To preset the statistical confidence level, for example, it can be set to 99.5%.
[0059] Thus, the solution is obtained This refers to the preset safety factor set for this type of power battery.
[0060] Based on the above-mentioned electrolyte injection control method, the basic electrolyte injection volume is determined by first comprehensively considering the physical wetting requirements of the battery cell (minimum injection volume) and the chemical consumption of internal side reactions (expected consumption). Then, the expected operating temperature profile of the sealing system of the power battery and the preset full life cycle are substituted into the pre-constructed preset electrolyte permeation loss model to predict the expected permeation loss of the sealing system during the full life cycle. Finally, the expected permeation loss is corrected for probability distribution by a preset safety factor and then added to the basic electrolyte injection volume to obtain the target electrolyte injection volume that comprehensively considers the physical wetting requirements, chemical losses, and physical permeation losses.
[0061] Compared to traditional electrolyte injection quantity design methods that only consider basic wetting requirements and / or electrochemical reaction losses, the electrolyte injection quantity determination method provided in this application can simultaneously complete the scientific compensation for electrolyte losses at both the chemical reaction and physical penetration levels during the injection quantity design stage. This avoids insufficient capacity and a sharp drop in performance at the end of the battery's life due to insufficient electrolyte, thus ensuring the long life and reliability of the power battery and avoiding unnecessary excessive injection during the production stage, thereby improving energy density and economy.
[0062] This application provides a method for determining the electrolyte injection volume. The method first determines the basic injection volume based on the cell's immersion requirements and electrolyte side reaction losses. Then, it inputs the expected operating temperature profile of the power battery and a preset full lifespan into a preset electrolyte permeation loss model to predict the expected permeation loss due to prolonged permeation. Simultaneously, a preset safety factor, considering individual differences, is used to correct the expected permeation loss as compensation for the basic injection volume, thus obtaining the target injection volume for the power battery. During the power battery electrolyte injection volume design stage, the expected permeation loss due to electrolyte side reactions is included in the calculation of the total electrolyte volume. This overcomes the risk of capacity drop due to insufficient electrolyte at the end of the power battery's lifespan caused by long-term electrolyte side reaction losses, ensuring the long lifespan and reliability of the power battery.
[0063] Based on the first embodiment of the electrolyte injection volume determination method of this application, in the second embodiment of the electrolyte injection volume determination method of this application, the content that is the same as or similar to the first embodiment of the electrolyte injection volume determination method described above can be referred to the above description, and will not be repeated hereafter. Based on this, please refer to... Figure 4 In this embodiment, after determining the basic injection volume, the following steps are also included: Step S41: Determine the electrolyte injection process parameters of the power battery based on the target electrolyte injection volume of the power battery.
[0064] As is easily understood, electrolyte injection process parameters refer to a series of quantifiable and controllable process conditions set during the electrolyte injection process of a power battery to achieve the target injection volume and ensure that the electrolyte fully and uniformly wets the internal pores of the battery cell. In this embodiment, after calculating the target injection volume, it can be used as an input condition to set or adjust a series of quantifiable and controllable parameters in the electrolyte injection supply and demand, namely the aforementioned electrolyte injection process parameters. This ensures that the electrolyte can be accurately and reliably injected into the battery cell according to the target injection volume, and achieves sufficient and uniform wettability of the battery cell, electrodes, and separator by the electrolyte.
[0065] Step S42: Based on the liquid injection process parameters, a power battery sample is prepared and an accelerated aging test is performed on the power battery sample.
[0066] Step S43: The actual remaining amount of electrolyte in the tested power battery sample is measured by solvent extraction.
[0067] It should be noted that, in this embodiment, the power battery sample refers to a test sample of a power battery manufactured for verification based on the injection process parameters specified by the preliminarily calculated target injection volume; accelerated aging test refers to an equivalent full life cycle accelerated experiment conducted under high temperature conditions (such as 60℃~85℃) or high rate cycling conditions (such as periodic power pulse transmission and reception); the actual electrolyte remaining volume refers to the actual electrolyte volume remaining in the cell after the accelerated aging test is completed, measured by disassembling the power battery sample and using the solvent extraction method. The solvent extraction method is an experimental method that utilizes the principle that the target substance has high solubility in a specific organic solvent. The test material is immersed in a specific organic solvent, allowing the target substance in the test material to be transferred to the liquid phase, and then the components of the target substance in the liquid phase are quantitatively analyzed.
[0068] It is easy to understand that, in this embodiment, the electrolyte injection process parameters (including injection volume, vacuum degree, and immersion time, etc.) can be specified based on the calculated target injection volume, and a power battery sample for accelerated aging testing can be prepared according to the injection process parameters. Subsequently, the power battery sample can be subjected to accelerated aging testing to simulate the entire life cycle of the power battery sample, and after the accelerated aging test is completed, the actual remaining electrolyte volume inside the power battery sample, i.e., the actual remaining electrolyte amount, can be extracted by solvent extraction.
[0069] Step S44: Based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, adjust the model parameters of the preset electrolyte permeation loss model until the difference in remaining amount is lower than the preset first threshold, so that the expected permeation loss calculated by the preset electrolyte permeation loss model after updating the model parameters is close to the actual permeation loss of the electrolyte.
[0070] As is easily understood, the expected remaining electrolyte volume refers to the volume of electrolyte that should remain in the battery cell when the battery reaches its preset full lifespan, based on the prediction results of the preset electrolyte permeation loss model. In this embodiment, by comparing the actual remaining electrolyte volume obtained from actual measurement with the expected remaining electrolyte volume corresponding to the prediction results of the preset electrolyte permeation loss model, the prediction deviation of the model can be evaluated. This allows for adaptive adjustments to the model parameters based on the magnitude of the prediction deviation, continuously optimizing the prediction model so that the final predicted result (expected permeation loss) continuously approaches the actual permeation loss of the electrolyte.
[0071] It should be noted that in this embodiment, the model parameters mainly refer to the aforementioned pre-exponential factor and / or osmotic activation energy. The pre-exponential factor is directly proportional to the predicted osmotic loss, while the osmotic activation energy is temperature-dependent. The preset first threshold is a value greater than 0 (its specific value can be adaptively adjusted according to the actual application environment). It is used to characterize that the difference between the actual remaining electrolyte and the expected remaining electrolyte is sufficiently small, within a tolerable error range, and can be ignored. If the difference in remaining electrolyte is lower than the preset first threshold, it indicates that the electrolyte remaining amount predicted by the model is very close to the actual measured electrolyte remaining amount, meaning the predicted value and the actual value are highly similar. When the actual remaining electrolyte amount deviates significantly from the expected remaining electrolyte amount only under different temperature adjustments, the osmotic activation energy can be adjusted accordingly first. However, when the influence of temperature is relatively small, if the actual remaining electrolyte amount still deviates significantly from the expected remaining amount, the pre-exponential factor is continuously adjusted proportionally according to the deviation ratio until the difference in remaining amount is lower than the preset first threshold. Then, the above-mentioned cyclic update process is terminated, and the final optimized model parameters are retained.
[0072] Based on the above closed-loop mechanism, the preset electrolyte permeation loss model can be continuously optimized so that the target electrolyte injection volume output by the model is closer to the actual electrolyte injection volume required by the battery.
[0073] Furthermore, in this embodiment, before the step of adjusting the model parameters of the preset electrolyte permeation loss model based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, the method further includes: Step S4401: Determine the expected remaining electrolyte amount based on the expected permeation loss, expected consumption, and target injection volume.
[0074] It is easy to understand that calculating the expected remaining electrolyte requires considering both the predicted electrolyte permeation loss and the predicted electrolyte consumption due to side reactions. In this embodiment, the formula for calculating the expected remaining electrolyte is as follows: ; in, This represents the expected remaining electrolyte level. The target injection volume; This represents the expected consumption amount. This represents the expected penetration loss.
[0075] Based on the first and / or second embodiments of the electrolyte injection volume determination method of this application, in the third embodiment of the electrolyte injection volume determination method of this application, the content that is the same as or similar to the first and / or second embodiments of the electrolyte injection volume determination method described above can be referred to the above description and will not be repeated hereafter. Based on this, please refer to... Figure 5In this embodiment, the method for determining the electrolyte injection volume further includes a method for constructing a preset electrolyte permeation loss model. The method for constructing the preset electrolyte permeation loss model specifically includes the following steps: Step S201: Conduct a long-term storage test on the sealing system of the power battery, and determine the actual effective permeability of the sealing system for electrolyte at different temperatures based on the test results of the long-term storage test.
[0076] Step S202: Fit the actual effective permeability at different temperatures, and use the Arrhenius equation to determine the permeation activation energy and pre-exponential factor of the sealing system.
[0077] It should be noted that, in this embodiment, the long-term storage test refers to filling the interior of the simulated test piece containing a complete sealed structure with electrolyte and sealing it, then placing it at a series of constant temperatures (such as 45°C, 60°C, and 75°C) for a continuous storage experiment for thousands of hours (e.g., more than 2000 hours); the test result of the long-term storage test refers to the data on the change of mass loss of the test piece at each temperature over time during the above test period; the actual effective permeability refers to the permeability actually exhibited by the whole in the real sealed system (including the pole, cover plate, sealing ring assembly, etc.).
[0078] In this embodiment, the test results typically include an initial stabilization phase and a linear loss phase. The slope of the curve at the corresponding temperature during the linear loss phase can be interpreted as the actual effective permeability.
[0079] It should be noted that, in this embodiment, the penetration activation energy refers to the minimum energy required for the electrolyte to overcome the intermolecular forces, free volume energy barrier, and interfacial barrier within the sealing material matrix, thereby enabling diffusion and migration. It is a quantitative indicator used to describe the sensitivity of permeability to temperature changes. The Arrhenius equation is an exponential function expression describing the relationship between chemical reaction rate (or physical diffusion rate) and temperature, and the pre-exponential factor refers to the frequency factor in the Arrhenius equation. When using the Arrhenius equation to characterize the change in the permeation rate of the electrolyte through the sealing interface with temperature, it can be specifically described as follows: ; in, This represents the actual effective penetration rate. It is a pre-exponential factor used to reflect the intrinsic frequency of electrolyte molecules colliding with and successfully penetrating the sealing material at a reference temperature; It is the osmotic activation energy; It is the gas constant; For temperature.
[0080] It is easy to understand that, in this embodiment, several complete sealing systems can be fabricated into standard samples, immersed in an electrolyte, and subjected to accelerated aging conditions (such as 85-90°C or other conditions higher than room temperature) for long-term storage testing. During this period, the samples can be periodically removed, and their total weight loss can be continuously monitored using an ultra-micro balance to obtain test results, i.e., data on the change of mass loss of the test piece over time at each temperature. Subsequently, linear fitting can be performed on the data points corresponding to the linear loss stage in the test results to obtain a fitting equation: ; in, The total mass of the test specimen lost due to electrolyte penetration during storage; It represents the mass loss per unit time and can also be used to characterize the actual effective permeability of a sealing system at a certain temperature; Storage time; The intercept of the fitted straight line is used to compensate for systematic deviations caused by zero-point drift or initial weighing errors in the balance measurement.
[0081] Subsequently, each temperature corresponds to an actual effective permeability. At this point, the Arrhenius equation is used again to calculate the actual effective permeability at various temperatures. Take the natural logarithm and the reciprocal of temperature. By performing a linear fit, another fitting equation is obtained: ; At this point, the intercept is... The slope is The osmotic activation energy can be obtained from the slope of the equation. The pre-exponential factor is obtained from the slope. .
[0082] Step S203: Based on the osmotic activation energy and the pre-exponential factor, establish a preset electrolyte osmotic loss model.
[0083] It is readily understood that, in this embodiment, after calculating the osmotic activation energy and pre-exponential factor, these two parameters can be substituted into the Arrhenius equation to obtain a osmotic loss rate model describing the change of electrolyte permeability with temperature. Subsequently, by integrating the loss rate model over time, a preset electrolyte osmotic loss model can be obtained, which ultimately describes the relationship between electrolyte osmotic loss and temperature and time.
[0084] Furthermore, in this embodiment, after establishing the preset electrolyte permeation loss model, the following steps are also included: Step S204: Perform a material-level permeation test on the sealing material used in the sealing system, and determine the steady-state permeation rate of the sealing material for electrolyte at different temperatures based on the test results of the material-level permeation test.
[0085] It should be noted that, in this embodiment, material-level permeability testing refers to an experimental method for determining the permeability characteristics of the sealing material used in the sealing system. It is mainly used to obtain the steady-state permeability of the sealing material to various key components in the electrolyte. Steady-state permeability refers to the mass or volume of electrolyte molecules that permeates through the sealing material per unit time, unit area, unit thickness (or unit pressure difference) after the diffusion process through the sealing material reaches a stable state. It is used to characterize the barrier performance of the sealing material.
[0086] As is readily understood, in this embodiment, a specific sealing material can be prepared into a standard sample, immersed in an electrolyte, and placed at an accelerated aging temperature (e.g., 85°C, 90°C). The sample is periodically removed, and its weight change is measured using a high-precision gravimetric analyzer. Gas chromatography-mass spectrometry (GC-MS) is then used to analyze the vapor components permeating through the sample, i.e., the test results of the material-level test. Subsequently, by fitting Fick's diffusion law, the steady-state permeability and diffusion coefficient of the sealing material to the key components in the electrolyte, as a function of temperature, are obtained.
[0087] Step S205: When the error between the steady-state permeability and the actual effective permeability at the preset temperature exceeds the preset error, the method for constructing the preset electrolyte permeation loss model is re-executed.
[0088] It should be noted that, in this embodiment, the preset error refers to the maximum permissible deviation in the results of material-level and system-level penetration tests that is set in advance.
[0089] It is easy to understand that in this embodiment, given the material-level steady-state permeability and the system-level actual effective permeability, the two can be compared. If the error between the two exceeds a preset error, it indicates that the system-level test may have permeation caused by non-intrinsic factors such as interface defects or assembly defects. In this case, the system-level test results should be used to construct the aforementioned preset electrolyte permeation loss model. Alternatively, steps S201-S203 can be re-executed, and if it is confirmed that the error between the retest result and the steady-state permeability does not exceed the preset error, the aforementioned preset electrolyte permeation loss model can be constructed based on the system-level retest results.
[0090] This application also provides an electrolyte injection volume determination device. Please refer to... Figure 6 The electrolyte injection volume determination device includes: The basic electrolyte injection assessment module 10 is used to determine the basic electrolyte injection amount of the power battery based on the minimum amount of electrolyte required for the battery cell to be fully immersed and the expected amount of electrolyte consumed due to internal side reactions.
[0091] The permeation prediction module 20 is used to determine the expected permeation loss corresponding to electrolyte permeation in the sealing system based on the expected operating temperature profile of the power battery-based sealing system, the preset full life cycle, and the preset electrolyte permeation loss model.
[0092] The liquid injection volume calculation module 30 is used to determine the target liquid injection volume of the power battery based on the basic liquid injection volume, the expected permeation loss volume, and the preset safety factor.
[0093] The electrolyte injection volume determination device provided in this application, employing the electrolyte injection volume determination method described in the above embodiments, can solve the problem of not being able to observe long-term electrolyte permeation loss due to the battery being in a sealed state, thus avoiding the technical problem of a sudden performance drop due to insufficient electrolyte at the end of the battery's lifespan. Compared with the prior art, the beneficial effects of the electrolyte injection volume determination device provided in this application are the same as those of the electrolyte injection volume determination method provided in the above embodiments, and other technical features in the electrolyte injection volume determination device are the same as those disclosed in the methods of the above embodiments, and will not be repeated here.
[0094] This application provides an electrolyte injection volume determination device, which includes: at least one processor; and a memory communicatively connected to the at least one processor; wherein the memory stores instructions executable by the at least one processor, and the instructions are executed by the at least one processor to enable the at least one processor to perform the electrolyte injection volume determination method in the above embodiment 1.
[0095] The following is for reference. Figure 7 The diagram illustrates a structural schematic suitable for implementing the electrolyte injection volume determination device in the embodiments of this application. The electrolyte injection volume determination device in the embodiments of this application may include, but is not limited to, fixed terminals such as vehicle-mounted terminals. Figure 7 The electrolyte injection volume determination device shown is merely an example and should not impose any limitations on the functionality and scope of use of the embodiments of this application.
[0096] like Figure 7As shown, the electrolyte injection volume determination device may include a processing unit 1001 (e.g., a central processing unit, a graphics processing unit, etc.), which can perform various appropriate actions and processes according to a program stored in a read-only memory (ROM) 1002 or a program loaded from a storage device 1003 into a random access memory (RAM) 1004. The RAM 1004 also stores various programs and data required for the operation of the electrolyte injection volume determination device. The processing unit 1001, ROM 1002, and RAM 1004 are interconnected via a bus 1005. An input / output (I / O) interface 1006 is also connected to the bus. Typically, the following devices can be connected to I / O interface 1006: input devices 1007 including, for example, a touchscreen, touchpad, keyboard, mouse, image sensor, microphone, accelerometer, gyroscope, etc.; output devices 1008 including, for example, a liquid crystal display (LCD), speaker, vibrator, etc.; storage devices 1003 including, for example, magnetic tape, hard disk, etc.; and communication devices 1009. Communication device 1009 allows the electrolyte volume determination device to exchange data with other devices wirelessly or via wired communication. Although an electrolyte volume determination device with various devices is shown in the figure, it should be understood that it is not required to implement or possess all of the devices shown. More or fewer devices may be implemented or possessed alternatively.
[0097] Specifically, according to the embodiments disclosed in this application, the processes described above with reference to the flowcharts can be implemented as computer software programs. For example, embodiments disclosed in this application include a computer program product comprising a computer program carried on a computer-readable medium, the computer program containing program code for performing the methods shown in the flowcharts. In such embodiments, the computer program can be downloaded and installed from a network via a communication device, or installed from storage device 1003, or installed from ROM 1002. When the computer program is executed by processing device 1001, it performs the functions defined in the methods of the embodiments disclosed in this application.
[0098] The electrolyte injection volume determination device provided in this application, employing the electrolyte injection volume determination method described in the above embodiments, can solve the problem of not being able to observe long-term electrolyte permeation loss due to the battery being in a sealed state, thus avoiding the technical problem of a sudden performance drop due to insufficient electrolyte at the end of the battery's lifespan. Compared with the prior art, the beneficial effects of the electrolyte injection volume determination device provided in this application are the same as those of the electrolyte injection volume determination method provided in the above embodiments, and other technical features of this electrolyte injection volume determination device are the same as those disclosed in the previous embodiment method, and will not be repeated here.
[0099] It should be understood that the various parts disclosed in this application can be implemented using hardware, software, firmware, or a combination thereof. In the description of the above embodiments, specific features, structures, materials, or characteristics can be combined in any suitable manner in one or more embodiments or examples.
[0100] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of protection of the above claims.
[0101] This application provides a computer-readable storage medium having computer-readable program instructions (i.e., a computer program) stored thereon, the computer-readable program instructions being used to execute the electrolyte injection volume determination method in the above embodiments.
[0102] The computer-readable storage medium provided in this application may be, for example, a USB flash drive, but is not limited to, electrical, magnetic, optical, electromagnetic, infrared, or semiconductor devices, apparatuses, or any combination thereof. More specific examples of computer-readable storage media may include, but are not limited to: electrical connections having one or more wires, portable computer disks, hard disks, random access memory (RAM), read-only memory (ROM), erasable programmable read-only memory (EPROM), optical fibers, portable compact disk read-only memory (CD-ROM), optical storage devices, magnetic storage devices, or any suitable combination thereof. In this embodiment, the computer-readable storage medium may be any tangible medium containing or storing a program that can be used by or in conjunction with an instruction execution apparatus, device, or device. The program code contained on the computer-readable storage medium may be transmitted using any suitable medium, including but not limited to: wires, optical cables, radio frequency (RF), etc., or any suitable combination thereof.
[0103] The aforementioned computer-readable storage medium may be included in the electrolyte injection volume determination device; or it may exist independently and not assembled into the electrolyte injection volume determination device.
[0104] The aforementioned computer-readable storage medium carries one or more programs. When these programs are executed by the electrolyte injection quantity determining device, the electrolyte injection quantity determining device: determines the basic electrolyte injection quantity of the power battery based on the minimum injection quantity required for the battery cell to be fully immersed and the expected consumption of the electrolyte due to internal side reactions; determines the expected permeation loss corresponding to electrolyte permeation in the sealing system based on the expected operating temperature profile of the power battery's sealing system, a preset full life cycle, and a preset electrolyte permeation loss model; and determines the target electrolyte injection quantity of the power battery based on the basic injection quantity, the expected permeation loss, and a preset safety factor.
[0105] Computer program code for performing the operations of this application can be written in one or more programming languages or a combination thereof, including object-oriented programming languages such as Java, Smalltalk, and C++, as well as conventional procedural programming languages such as "C" or similar programming languages. The program code can be executed entirely on the user's computer, partially on the user's computer, as a standalone software package, partially on the user's computer and partially on a remote computer, or entirely on a remote computer or server. In cases involving remote computers, the remote computer can be connected to the user's computer via any type of network—including a Local Area Network (LAN) or a Wide Area Network (WAN)—or can be connected to an external computer (e.g., via the Internet using an Internet service provider).
[0106] The flowcharts and block diagrams in the accompanying drawings illustrate the architecture, functionality, and operation of possible implementations of apparatus, methods, and computer program products according to various embodiments of this application. In this regard, each block in a flowchart or block diagram may represent a module, segment, or portion of code containing one or more executable instructions for implementing a specified logical function. It should also be noted that in some alternative implementations, the functions indicated in the blocks may occur in a different order than those indicated in the drawings. For example, two consecutively indicated blocks may actually be executed substantially in parallel, and they may sometimes be executed in reverse order, depending on the functions involved. It should also be noted that each block in the block diagrams and / or flowcharts, and combinations of blocks in the block diagrams and / or flowcharts, can be implemented using dedicated hardware-based apparatus to perform the specified function or operation, or using a combination of dedicated hardware and computer instructions.
[0107] The modules described in the embodiments of this application can be implemented in software or hardware. The names of the modules do not necessarily limit the functionality of the unit itself.
[0108] The readable storage medium provided in this application is a computer-readable storage medium that stores computer-readable program instructions (i.e., a computer program) for executing the above-described method for determining the electrolyte injection volume. This solves the problem that long-term electrolyte permeation loss cannot be observed because the battery is in a sealed state, thus avoiding the technical problem of a sudden performance drop due to insufficient electrolyte at the end of the battery's lifespan. Compared with the prior art, the beneficial effects of the computer-readable storage medium provided in this application are the same as those of the electrolyte injection volume determination method provided in the above embodiments, and will not be repeated here.
[0109] The above are merely preferred embodiments of this application and do not limit the patent scope of this application. Any equivalent structural or procedural transformations made using the content of this application's specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent scope of this application.
Claims
1. A method for determining the electrolyte injection volume, characterized in that, The steps of the method for determining the electrolyte injection volume include: The basic electrolyte injection volume of the power battery is determined based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions. Based on the expected operating temperature profile of the sealing system of the power battery, the preset full life cycle, and the preset electrolyte permeation loss model, the expected permeation loss corresponding to the electrolyte permeation of the sealing system is determined. The target electrolyte injection volume for the power battery is determined based on the basic injection volume, the expected permeation loss, and the preset safety factor.
2. The method for determining the electrolyte injection volume as described in claim 1, characterized in that, After determining the basic injection volume, the following steps are also included: The electrolyte injection process parameters of the power battery are determined based on the target electrolyte injection volume. Based on the aforementioned liquid injection process parameters, a power battery sample was prepared, and the power battery sample was subjected to accelerated aging test. The actual amount of electrolyte remaining in the tested power battery samples was measured using a solvent extraction method. Based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, the model parameters of the preset electrolyte permeation loss model are adjusted until the difference in remaining amount is lower than a preset first threshold, so that the expected permeation loss calculated by the preset electrolyte permeation loss model after updating the model parameters approaches the actual permeation loss of the electrolyte.
3. The method for determining the electrolyte injection volume as described in claim 2, characterized in that, Before the step of adjusting the model parameters of the preset electrolyte permeation loss model based on the difference between the actual remaining electrolyte amount and the expected remaining electrolyte amount, the method further includes: The expected remaining electrolyte amount is determined based on the expected permeation loss, the expected consumption, and the target injection volume.
4. The method for determining the electrolyte injection volume as described in claim 1, characterized in that, The steps for determining the basic electrolyte injection volume of a power battery, based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions, include: Obtain the preset liquid storage space parameters of the power battery, and determine the minimum liquid injection volume based on the preset liquid storage space parameters. The preset liquid storage space parameters include the electrode parameters of the battery cell and the separator parameters. Based on the preset side reaction parameters and preset electrochemical aging model of the power battery, the expected consumption is determined. The preset side reaction parameters include at least the target cycle life and target storage life of the power battery. The base injection volume is determined based on the minimum injection volume and the expected consumption.
5. The method for determining the electrolyte injection volume as described in claim 4, characterized in that, The electrode parameters include the electrode coating amount, electrode compaction density, and electrode material density; the diaphragm parameters include the diaphragm volume and diaphragm porosity. Determining the minimum injection volume based on the preset liquid storage space parameters includes the following steps: The porosity of the electrode coating is determined based on the electrode compaction density and the electrode material density. The electrode pore volume is determined based on the coating porosity and the electrode coating amount. The pore volume of the diaphragm is determined based on the diaphragm volume and the diaphragm porosity. The minimum injection volume is determined based on the electrode pore volume and the diaphragm pore volume.
6. The method for determining the electrolyte injection volume as described in claim 1, characterized in that, The method for constructing the preset electrolyte permeation loss model specifically includes the following steps: A long-term storage test was conducted on the sealing system of the power battery, and the actual effective permeability of the sealing system to the electrolyte at different temperatures was determined based on the test results of the long-term storage test. The actual effective permeability at different temperatures was fitted, and the permeation activation energy and pre-exponential factor of the sealing system were determined using the Arrhenius equation. Based on the osmotic activation energy and the pre-exponential factor, a preset electrolyte osmotic loss model is established.
7. The method for determining the electrolyte injection volume as described in claim 6, characterized in that, Following the step of establishing a preset electrolyte permeation loss model, the following steps are also included: The sealing material used in the sealing system is subjected to a material-level permeability test, and the steady-state permeability of the sealing material to the electrolyte at different temperatures is determined based on the test results of the material-level permeability test. When the error between the steady-state permeability at the preset temperature and the actual effective permeability exceeds the preset error, the method for constructing the preset electrolyte permeation loss model is re-executed.
8. A device for determining the amount of electrolyte injected, characterized in that, The electrolyte injection volume determination device includes: The basic electrolyte injection assessment module is used to determine the basic electrolyte injection amount of the power battery based on the minimum amount of electrolyte required to fully wet the battery cell and the expected amount of electrolyte consumed due to internal side reactions. The permeation prediction module is used to determine the expected permeation loss corresponding to electrolyte permeation in the sealing system based on the expected operating temperature profile of the power battery sealing system, the preset full life cycle, and the preset electrolyte permeation loss model. The liquid injection volume calculation module is used to determine the target liquid injection volume of the power battery based on the basic liquid injection volume, the expected permeation loss, and the preset safety factor.
9. A device for determining the amount of electrolyte injected, characterized in that, The electrolyte injection volume determination device includes: a memory, a processor, and an electrolyte injection volume determination program stored in the memory and executable on the processor, the electrolyte injection volume determination program being configured to implement the steps of the electrolyte injection volume determination method as described in any one of claims 1 to 7.
10. A storage medium, characterized in that, The storage medium is a computer-readable storage medium, and the computer-readable storage medium stores an electrolyte injection volume determination program, which, when executed by a processor, implements the steps of the electrolyte injection volume determination method as described in any one of claims 1 to 7.