Reactive polyurethane modified asphalt drainage pavement structure

By using reactive polyurethane modified asphalt pavement structure in asphalt pavement, combined with cooling structure and porous cement concrete, the problem of poor road performance of asphalt pavement under large displacement is solved, and higher stability and durability are achieved. And reduces construction temperature and cost.

CN222119819UActive Publication Date: 2024-12-06CHINA METALLURGICAL ROAD & BRIDGE CONSTR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323234793.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-11-29
Publication Date
2024-12-06
Estimated Expiration
2033-11-29

AI Technical Summary

Technical Problem

Under the premise of large displacement, the existing asphalt pavement has poor water stability and durability, and has high construction temperature, high cost and unstable bonding performance.

Method used

Using reactive polyurethane modified asphalt pavement structure, the gravel layer, fine stone concrete, steel mesh, cooling structure and porous cement concrete are laid on the roadbed successively, and combined with polyurethane modified asphalt, the bonding performance and drainage permeability are increased, and the water-permeable performance is reduced. Construction temperature and improve thermal stability.

Benefits of technology

It improves the bonding performance stability, water stability and durability of the pavement structure, while reducing construction temperature and cost, and enhancing drainage permeability and thermal stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222119819U_ABST
    Figure CN222119819U_ABST
Patent Text Reader

Abstract

According to the reaction type polyurethane modified asphalt drainage pavement structure, a gravel layer, fine stone concrete, a reinforcing mesh and a cooling structure are sequentially laid on a roadbed from bottom to top, and porous cement concrete and modified asphalt concrete are embedded in the outer side of the cooling structure. And polyurethane modified asphalt is laid above the cooling structure and the modified asphalt concrete. The cooling structure comprises a bent pipeline and concrete columns arranged on the outer wall of the pipeline, through holes are formed in the concrete columns, the pipeline and the concrete columns are laid on a reinforcing mesh, and the concrete columns are arranged at equal intervals. According to the reaction type polyurethane modified asphalt drainage pavement structure provided by the utility model, on the premise that the pavement structure has a large drainage amount, the pavement structure also has higher pavement performance, and the comprehensive effect is improved by improving the pavement structure and the pavement mode of the surface layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of road structures, and in particular relates to a reactive polyurethane modified asphalt drainage pavement structure. Background Art

[0002] Asphalt pavement refers to various types of pavement paved with road asphalt materials mixed into mineral materials. The asphalt binder improves the ability of paving aggregate to resist damage to the road surface caused by traffic and natural factors, making the road surface smooth, dust-free, impermeable and durable. Therefore, asphalt pavement is the most widely used high-grade pavement in road construction.

[0003] The porosity of large-pore drainage mixture is between 18% and 25%, which can timely drain the surface water on the road and eliminate the adverse effects of road surface water film. It also has the advantages of high anti-skid performance, noise reduction, water mist suppression, and water drift prevention, which improves driving comfort on rainy days and at night. However, since the strength of drainage asphalt pavement comes from the interlocking effect between coarse aggregates, the porosity itself is relatively large, which easily leads to insufficient adhesion between the mixtures. In terms of road performance, the water stability and durability are relatively poor. The current high-viscosity asphalt can solve the above problems to a certain extent, but there are problems such as high construction temperature, high cost and unstable bonding performance.

[0004] Therefore, how to make the pavement structure have high road performance while having a large drainage volume has become the key technical problem to be solved in this plan. Utility Model Content

[0005] The purpose of the utility model is to provide a reactive polyurethane modified asphalt drainage pavement structure, which solves the technical problem of how to make the pavement structure have high road performance while having a large drainage volume, and achieves an improvement in the overall effect by improving the pavement structure and the surface layer paving method.

[0006] A reactive polyurethane modified asphalt drainage pavement structure, wherein a crushed stone layer, fine stone concrete, a steel mesh, and a cooling structure are laid on the roadbed in sequence from bottom to top, porous cement concrete and modified asphalt concrete are embedded on the outer side of the cooling structure, and polyurethane modified asphalt is laid above the cooling structure and the modified asphalt concrete.

[0007] The cooling structure comprises a bent pipe, a concrete column arranged against the outer wall of the pipe, the concrete column is provided with a through hole, the pipe and the concrete column are laid on the steel mesh, and a plurality of concrete columns are arranged at equal intervals.

[0008] The polyurethane modified asphalt comprises base asphalt, polyurethane material and limestone powder.

[0009] The polyurethane modified asphalt is mixed with composite fibers.

[0010] The polyurethane modified asphalt is mixed with clay.

[0011] The heights of the pipeline and the concrete column are consistent, and the upper end of the modified asphalt concrete is flush with the upper end of the concrete column.

[0012] The porous cement concrete is formed by mixing crushed stone with a particle size of 5 mm, silicate cement, mineral powder, water reducing agent, air entraining agent and water.

[0013] The pipe is made of concrete.

[0014] The positive effects of the utility model are as follows:

[0015] (1) In this scheme, a cooling structure is provided. During construction, water is passed into the pipe, which helps to solve the problem of high temperature during asphalt construction. After the construction is completed, it can also serve as a road reinforcement. At the same time, the hollow structure in the pipe can also help to drain water;

[0016] (2) The structures from top to bottom are polyurethane modified asphalt, modified asphalt concrete, and porous cement concrete. The upper and lower adjacent surface structures have common components, which helps to increase the connection strength of adjacent surface layers, thereby helping to increase the overall bonding performance stability of the mixture, thereby improving water stability and durability;

[0017] (3) The height of the pipe and the concrete column is consistent, and the upper end of the modified asphalt concrete is flush with the upper end of the concrete column, so the top layer is polyurethane modified asphalt, that is, there is only one layer of polyurethane modified asphalt above the pipe and the concrete column, which greatly reduces the absorption of light energy and helps to improve the thermal stability of the drainage pavement structure;

[0018] (4) The cooling structure in this scheme, combined with the various surface layers laid up and down, has good drainage and water permeability, and has great bonding strength, good heat dissipation and thermal stability. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the structure of the pipeline and concrete column in the utility model.

[0020] Figure 2 It is a structural schematic diagram of the drainage pavement structure in the utility model.

[0021] Among them, the figures are marked as: 1. pipeline; 2. concrete column; 3. through hole; 4. gravel layer; 5. fine stone concrete; 6. porous cement concrete; 7. modified asphalt concrete; 8. polyurethane modified asphalt. DETAILED DESCRIPTION

[0022] In order to more clearly illustrate the technical features of this solution, this solution is described below through specific implementation methods.

[0023] See also Figure 1-Figure 2 A reactive polyurethane modified asphalt drainage pavement structure, on which a crushed stone layer 4, fine stone concrete 5, a steel mesh, and a cooling structure are laid in sequence from bottom to top on the roadbed, porous cement concrete 6 and modified asphalt concrete 7 are embedded on the outside of the cooling structure, and polyurethane modified asphalt 8 is laid above the cooling structure and the modified asphalt concrete 7.

[0024] The cooling structure comprises a bent pipe 1, a concrete column 2 arranged against the outer wall of the pipe 1, a through hole 3 arranged on the concrete column 2, the pipe 1 and the concrete column 2 are laid on a steel mesh, and a plurality of concrete columns 2 are arranged at equal intervals.

[0025] The polyurethane modified asphalt 8 comprises base asphalt, polyurethane material and limestone powder.

[0026] The polyurethane modified asphalt 8 is mixed with composite fibers.

[0027] Polyurethane modified asphalt 8 is mixed with clay.

[0028] The heights of the pipeline 1 and the concrete column 2 are consistent, and the upper end of the modified asphalt concrete 7 is flush with the upper end of the concrete column 2.

[0029] The porous cement concrete 6 is a mixture of crushed stone with a particle size of 5 mm, silicate cement, mineral powder, water reducing agent, air entraining agent and water.

[0030] Pipe 1 is made of concrete.

[0031] The specific working process of this utility model:

[0032] First, a crushed stone layer 4, fine stone concrete 5, and a steel mesh are laid on the roadbed from bottom to top, and the pipeline 1 and the concrete column 2 are laid on the steel mesh, and the steel mesh is pressed down. There can be several pipelines 1 and several concrete columns 2, and they are arranged close to the outer wall of the pipeline 1 at equal intervals;

[0033] Porous cement concrete 6 and modified asphalt concrete 7 are laid in sequence in the space between the pipe 1 and the concrete column 2, so that the upper end surface of the modified asphalt concrete 7 is flush with the upper ends of the pipe 1 and the concrete column 2, and the last layer of polyurethane modified asphalt 8 is laid on it and compacted.

[0034] Technical features not described in the present invention can be achieved through or by adopting existing technologies, and will not be elaborated here. Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by ordinary technicians in this technical field within the essential scope of the present invention should also fall within the scope of protection of the present invention.

Claims

1. A reactive polyurethane modified asphalt drainage pavement structure, characterized in that: A crushed stone layer (4), fine stone concrete (5), a steel mesh, and a cooling structure are sequentially laid on the roadbed from bottom to top, and porous cement concrete (6) and modified asphalt concrete (7) are embedded on the outer side of the cooling structure, and polyurethane modified asphalt (8) is laid on the top of the cooling structure and the modified asphalt concrete (7); The cooling structure comprises a bent pipe (1), a concrete column (2) arranged against the outer wall of the pipe (1), a through hole (3) being arranged on the concrete column (2), the pipe (1) and the concrete column (2) being laid on the steel mesh, and a plurality of concrete columns (2) being arranged at equal intervals.

2. The reactive polyurethane modified asphalt drainage pavement structure according to claim 1, characterized in that: The pipe (1) and the concrete column (2) have the same height, and the upper end of the modified asphalt concrete (7) is flush with the upper end of the concrete column (2).