An integrated in-situ magnetic field and optical observation dendrite monitoring device
By integrating magnetic field generation, electrochemical testing, and optical observation, the problem of the difficulty in studying the influence of magnetic fields on zinc dendrite growth in existing technologies has been solved. Real-time, in-situ recording and dynamic correlation of the zinc deposition process have been achieved, simplifying the operation process and improving research efficiency.
Patent Information
- Application Number
- CN202522736762.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-12-24
AI Technical Summary
Existing technologies lack an integrated device that can synchronously and conveniently apply a controllable magnetic field of direction and intensity within the same apparatus and achieve high-quality in-situ optical observation, making it difficult to systematically study the dynamic effects of magnetic fields on zinc dendrite growth.
Design an integrated dendrite monitoring device that combines in-situ magnetic field and optical observation, integrating magnetic field generation, electrochemical testing and in-situ optical observation functions, to realize dynamic and visual research on zinc deposition process and dendrite growth behavior under controllable direction and intensity magnetic field.
It enables real-time, in-situ recording of the zinc deposition process under magnetic field conditions, directly establishing a dynamic correlation between the magnetic field and deposition behavior, simplifying the operation process, lowering the technical threshold, and improving research efficiency and user-friendliness.
Smart Images

Figure CN224985386U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of aqueous zinc-ion batteries, and in particular to an integrated dendrite monitoring device that combines in-situ magnetic field and optical observation. Background Technology
[0002] Aqueous zinc-ion batteries have shown great promise for large-scale energy storage due to their high safety, low cost, and environmental friendliness. However, zinc anodes are prone to dendrite growth during cycling. Dendrites can puncture the separator, causing short circuits and severely impacting cycle life and safety performance. Therefore, in-depth research into the zinc deposition process, especially the growth and morphological evolution of dendrites, is crucial for developing high-performance zinc anodes and improving battery performance.
[0003] Currently, the main methods for studying zinc deposition behavior include electrochemical testing, offline morphology characterization (such as scanning electron microscopy), and in-situ observation techniques. Among these, in-situ optical observation techniques can record the dynamic changes on the electrode surface in real time and intuitively, and have become an important tool for studying metal deposition processes. On the other hand, research shows that external magnetic fields, as a non-contact physical field, can affect ion transport and electrochemical reaction processes through magnetohydrodynamic effects and magnetic forces, and may thus regulate the morphology of metal deposition and inhibit dendrite growth. However, existing techniques usually separate magnetic field studies and optical observations, lacking an integrated device that can synchronously and conveniently apply controllable magnetic fields of varying directions and intensities within the same apparatus, and achieve high-quality in-situ optical observations. This makes it difficult and cumbersome to systematically study the dynamic effects of different magnetic field conditions (especially magnetic field direction) on the entire zinc dendrite growth process.
[0004] Therefore, there is an urgent need to develop a device that integrates magnetic field control, electrochemical testing, and in-situ optical observation to facilitate and systematically study the influence mechanism of magnetic fields on zinc deposition behavior, thereby providing an effective experimental platform and technical support for optimizing the zinc deposition process and suppressing dendrite growth. Utility Model Content
[0005] In view of the shortcomings of the prior art, the purpose of this utility model is to provide an integrated in-situ magnetic field and optical observation dendrite monitoring device. This device integrates magnetic field generation, electrochemical control and in-situ optical observation functions, and can dynamically and visually study the zinc deposition process and dendrite growth behavior of the negative electrode of an aqueous zinc-ion battery under the condition of applying a magnetic field with controllable direction and intensity. It is easy to operate and has comprehensive functions.
[0006] The technical solution of this utility model is as follows: An integrated dendrite monitoring device combining in-situ magnetic field and optical observation includes: an electrochemical testing module, a magnetic field generating module, and an optical observation recording module; The electrochemical testing module includes: an electrolytic cell with at least one optically transparent window as the observation surface, a zinc negative electrode and a copper positive electrode disposed on opposite sides of the electrolytic cell, and a charge-discharge tester connected to the zinc negative electrode and the copper positive electrode; the electrolytic cell is used to contain electrolyte. The magnetic field generating module is used to generate a static magnetic field with controllable direction and intensity in the electrolytic cell area; The optical observation and recording module includes: an optical microscope and a camera unit; the lens of the optical microscope is aimed at the zinc sheet negative electrode deposition surface in the electrolytic cell; The static magnetic field generated by the magnetic field generating module acts on the electrolytic cell area, and the charge-discharge tester controls the deposition process and is triggered synchronously with the optical observation and recording module to realize dynamic in-situ recording of the deposition morphology under static magnetic field environment.
[0007] Preferably, the in-situ magnetic field and optical observation coupled dendrite monitoring device further includes: a computer control module; The computer control module is connected to the charge-discharge tester and is used to set the deposition parameters controlled by the charge-discharge tester and synchronously send trigger signals to the camera unit.
[0008] Preferably, the zinc negative electrode and the copper positive electrode are fixed in the electrolytic cell by a fixing device, and the two are kept in parallel relative positions with adjustable spacing.
[0009] Preferably, the magnetic field generating module includes: a magnetic field generator and a magnetic field generating power supply for controlling the magnetic field strength of the magnetic field generator.
[0010] More preferably, the magnetic field generator is an electromagnet or permanent magnet system with adjustable pole spacing.
[0011] More preferably, the magnetic field generator is arranged around the outside of the electrolytic cell.
[0012] More preferably, the magnetic field strength of the magnetic field generator is in the range of 0 ~ 5 T.
[0013] Preferably, the direction of the static magnetic field is either perpendicular or parallel. Wherein, the vertical direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode, and the parallel direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode.
[0014] Preferably, the camera unit is a high-speed or high-resolution camera.
[0015] Preferably, the optical observation and recording module further includes a light source for illumination.
[0016] The technical solution of this utility model has the following advantages: 1. The device provided by this utility model deeply integrates three major functions: magnetic field control, electrochemical deposition, and in-situ optical observation. It has a compact structure, avoids the complexity of using multiple devices and the problem of signal synchronization, and provides a dedicated platform for studying the influence of magnetic fields on electrodeposition.
[0017] 2. This invention enables independent and precise control of magnetic field strength (0-5 T) and direction (vertical / parallel), facilitating systematic research on the regulation of zinc deposition morphology and dendrite growth kinetics by different magnetic field parameters.
[0018] 3. This invention can capture and record the entire process of micromorphological evolution of zinc deposition interface in real time and in situ under the condition of applying a magnetic field, and directly establish the dynamic correlation between magnetic field conditions and deposition behavior, making mechanism research intuitive and efficient.
[0019] 4. The operation process of this utility model is clear, and the modules have good synergy, which reduces the technical threshold for conducting magnetic field experiments and in-situ observations simultaneously. It has good user-friendliness, repeatability and practical value. Attached Figure Description
[0020] Figure 1 This is a schematic diagram of the structure of an integrated dendrite monitoring device that combines in-situ magnetic field and optical observation.
[0021] Figure 2 This is a schematic diagram of a further improved in-situ magnetic field and optical observation coupled dendrite monitoring device.
[0022] Figure 3 These are the chronocurrent curves for zinc electrodeposition under vertical magnetic fields of different intensities.
[0023] Figure 4 The images show the planar SEM morphology of zinc deposits under vertical magnetic fields of different intensities; where (a) represents no magnetic field; (b) represents a vertical magnetic field of 0.2 T; (c) represents a vertical magnetic field of 0.4 T; and (d) represents a vertical magnetic field of 0.6 T.
[0024] Figure 5 These are in-situ characterizations of the zinc electrodeposition process; (a) is the time-voltage curve of zinc electrodeposition without a magnetic field and (b) is the in-situ optical image; (c) is the time-voltage curve of zinc electrodeposition under a 0.4 T parallel magnetic field and (d) is the in-situ optical image.
[0025] Figure reference numerals: Electrochemical testing module 10, electrolytic cell 101, zinc negative electrode 102, copper positive electrode 103, charge / discharge tester 104, electrolyte 105; magnetic field generating module 20, magnetic field generator 201, magnetic field generating power supply 202; optical observation and recording module 30, optical microscope 301, camera unit 302, light source 303; computer control module 40. Detailed Implementation
[0026] This utility model provides an integrated dendrite monitoring device that combines in-situ magnetic field and optical observation. To make the purpose, technical solution and effects of this utility model clearer and more explicit, the following is a more detailed description of this utility model.
[0027] like Figure 1 As shown, this utility model embodiment provides an in-situ magnetic field and optical observation coupled dendrite monitoring device, including: an electrochemical testing module 10, a magnetic field generating module 20, and an optical observation recording module 30; The electrochemical testing module 10 includes: an electrolytic cell 101 with at least one optically transparent window as the observation surface; a zinc negative electrode 102 and a copper positive electrode 103 disposed on opposite sides of the electrolytic cell 101; and a charge / discharge tester 104 connected to the zinc negative electrode 102 and the copper positive electrode 103; the electrolytic cell is used to contain an electrolyte 105. The magnetic field generating module 20 is used to generate a static magnetic field with controllable direction and intensity in the electrolytic cell area; The optical observation and recording module 30 includes: an optical microscope 301 and a camera unit 302; the lens of the optical microscope 301 is aimed at the deposition surface of the zinc sheet negative electrode 102 in the electrolytic cell 101; The static magnetic field generated by the magnetic field generating module 20 acts on the region of the electrolytic cell 101. The charge and discharge tester 104 controls the deposition process and is triggered synchronously with the optical observation and recording module 30, so as to realize dynamic in-situ recording of the deposition morphology under static magnetic field environment.
[0028] In this embodiment, the device combines a magnetic field generation module with an optical observation and recording module to achieve real-time and dynamic monitoring of the zinc dendrite growth process on the electrode surface under an externally controlled magnetic field environment. It is particularly suitable for studying the influence of magnetic fields in different directions on dendrite growth behavior during zinc deposition.
[0029] In the electrochemical testing module, the electrolytic cell is used to contain the electrolyte and electrodes; the charge-discharge tester is electrically connected to the zinc negative electrode and the copper positive electrode to control the potential / current conditions of zinc deposition and to simultaneously collect voltage and current data.
[0030] In the optical observation and recording module, the optical microscope lens is aimed at the surface of the zinc sheet negative electrode in the electrolytic cell, and the electrodeposition process is carried out simultaneously with image / video recording, so as to realize the morphological comparison and analysis at different deposition time points.
[0031] In some implementations, such as Figure 2 As shown, the in-situ magnetic field and optical observation coupled dendrite monitoring device further includes: a computer control module 40; The computer control module 40 is connected to the charge-discharge tester 104 and is used to set the deposition parameters controlled by the charge-discharge tester and synchronously send trigger signals to the camera unit.
[0032] In some embodiments, the zinc negative electrode 102 and the copper positive electrode 103 are fixed in the electrolytic cell 101 by a fixing device, and the zinc negative electrode 102 and the copper positive electrode 103 are kept in parallel relative positions with adjustable spacing.
[0033] In some embodiments, the electrolyte is a zinc salt electrolyte, but it is not limited thereto.
[0034] In some embodiments, the magnetic field generating module 20 includes: a magnetic field generator 201 and a magnetic field generating power supply 202 for controlling the magnetic field strength of the magnetic field generator 201.
[0035] In some more specific embodiments, the magnetic field generator 201 is an electromagnet or permanent magnet system with adjustable pole spacing. Specifically, the magnetic field generator is capable of generating a relatively uniform and stable static magnetic field; the magnetic field strength is controlled by adjusting the current or the pole spacing, and is calibrated and measured using a high-precision gaussmeter.
[0036] In some more specific embodiments, the magnetic field generator 201 is arranged around the outside of the electrolytic cell 101 to ensure that the zinc ion deposition process is within a uniform magnetic field area.
[0037] In some more specific embodiments, the magnetic field strength of the magnetic field generator 201 is in the range of 0 ~ 5 T, in order to meet the research needs of the influence of magnetic fields of different intensities on the deposition morphology.
[0038] In some embodiments, the magnetic field direction of the static magnetic field is either vertical or parallel. Wherein, the vertical direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode, and the parallel direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode.
[0039] In some embodiments, the camera unit 302 is a high-speed or high-resolution camera used to record the continuous dynamic process of zinc dendrite formation and growth.
[0040] In some implementations, such as Figure 2 As shown, the optical observation and recording module 30 also includes a light source 303 for illumination.
[0041] The present invention will be further described below through specific embodiments.
[0042] Example 1 At room temperature, the magnetic field generating module employs a neodymium iron boron permanent magnet magnetic field generator, which can generate a stable static magnetic field (vertical electric field) perpendicular to the bottom surface of the electrolytic cell in the electrolytic cell area. The magnetic field strength is controlled by adjusting the pole spacing, and the strength value is measured by a high-precision gaussmeter. In this embodiment, the working magnetic field strength is set to 0~0.6 T. The zinc negative electrode (both with dimensions of 6 mm × 10 mm × 0.1 mm) and the copper positive electrode (both with dimensions of 6 mm × 10 mm × 0.1 mm) are fixed parallel to each other inside the electrolytic cell (10 mm × 10 mm × 30 mm) using polytetrafluoroethylene (PTFE) insulating clamps, with the electrode spacing set to 10 mm. The electrode leads are led out from the sealed interface on the side wall of the electrolytic cell. The electrolyte is a mixed solution of 6 mol / L KOH and 0.2 mol / L ZnO, injected into the electrolytic cell using a micro-syringe, with the liquid level fully submerging the electrode working area.
[0043] The charge-discharge tester (Chenhua CHI760e) is reliably connected to the zinc negative electrode and copper positive electrode leads via alligator clips. The tester connects to a computer via a data cable to control the constant current / constant potential deposition process and record time-current / voltage curves. The external trigger port of the tester connects to the camera unit (camera) control terminal of the optical observation and recording module to achieve hardware synchronization of the electrochemical process and image acquisition.
[0044] The optical observation and recording module mainly consists of a 48-megapixel industrial camera, a 130x continuous zoom lens, and a four-dimensional adjustable support. During the experiment, the lens needs to be aimed at the deposition area on the surface of the copper cathode in the transparent electrolytic cell. The electrodeposition process and camera recording are started simultaneously, and fixed-point image acquisition is performed after the deposition begins.
[0045] The results showed that the potential during the test was -1.5 V vs Hg / HgO, as... Figure 3 As shown, the absolute value of the limiting current density at 0 T is 17.12 mA / cm². 2 At 0.2 T, it is 22.33 mA / cm. 2 At 0.4 T, it is 34.45 mA / cm. 2 At 0.6 T, it is 45.78 mA / cm. 2Under vertical magnetic fields of 0.2 T, 0.4 T, and 0.6 T, the limiting current density during zinc electrodeposition increased by 5.21 mA / cm² compared to the case without a magnetic field. 2 17.33 mA / cm 2 and 28.66 mA / cm 2 The rate of diffusion of zincate ions to the electrode surface under a magnetic field is significantly higher than that without a magnetic field, and the stronger the magnetic field, the faster the diffusion. This is likely due to the stronger magnetohydrodynamic effect generated by a larger magnetic field. The increase in limiting current density during zinc electrodeposition under a vertical magnetic field indicates that the electrolyte mass transfer during zinc electrodeposition is effectively enhanced after applying a magnetic field.
[0046] like Figure 4 As shown in Figure (a), the current density used in the test was 20 mA / cm². 2 Under a constant current and without a magnetic field, severe zinc dendrite growth occurs on the electrode surface. The zinc deposition layer consists of numerous sharp and large zinc dendrites, with dendrite widths reaching up to 391 µm. In the magnified image, the zinc crystals are vertically stacked, forming a pyramid structure with sharp apexes. This structure has strong penetrating power and, in severe cases, may pierce the separator, causing direct contact between the positive and negative electrodes and ultimately leading to a short circuit. When a vertical magnetic field of 0.2 T is applied, as... Figure 4 As shown in (b), the entire zinc deposition layer does not exhibit vigorous dendrite growth, but is instead covered with small, granular zinc crystals. Figure 4 As shown in (c), when the magnetic field strength increases to 0.4 T, the zinc deposition layer becomes more uniform, and the zinc deposition particles become further refined. When the magnetic field strength increases to 0.6 T, as... Figure 4 As shown in (d), the zinc electrodeposited layer is more compact and smooth at this time compared to 0.2 T and 0.4 T. As can be seen from the magnified view, the zinc crystal stacking becomes more compact.
[0047] Example 2 At room temperature, the magnetic field generating module uses a neodymium iron boron permanent magnet magnetic field generator, which can generate a stable static magnetic field (parallel electric field) parallel to the bottom surface of the electrolytic cell in the electrolytic cell area. The magnetic field strength is controlled by adjusting the pole spacing, and the strength value is measured by a high-precision gaussmeter. In this embodiment, the working magnetic field strength is set to 0~0.6 T. The zinc negative electrode (both with dimensions of 6 mm × 10 mm × 0.1 mm) and the copper positive electrode (both with dimensions of 6 mm × 10 mm × 0.1 mm) are fixed parallel to each other inside the electrolytic cell (10 mm × 10 mm × 30 mm) using polytetrafluoroethylene (PTFE) insulating clamps, and the electrode spacing is set to 10 mm. The electrode leads are led out from the sealed interface on the side wall of the electrolytic cell. The electrolyte is a mixed solution of 6 mol / L KOH and 0.2 mol / L ZnO, which is injected into the electrolytic cell using a micro-syringe, and the liquid level completely submerges the electrode working area.
[0048] The charge-discharge tester (Chenhua CHI760e) is reliably connected to the zinc negative electrode and copper positive electrode leads via alligator clips. The tester connects to a computer via a data cable to control the constant current / constant potential deposition process and record time-current / voltage curves. The external trigger port of the tester connects to the camera unit (camera) control terminal of the optical observation and recording module to achieve hardware synchronization of the electrochemical process and image acquisition.
[0049] The optical observation and recording module mainly consists of a 48-megapixel industrial camera, a 130x continuous zoom lens, and a four-dimensional adjustable support. During the experiment, the lens needs to be aimed at the deposition area on the surface of the copper cathode in the transparent electrolytic cell. The electrodeposition process and camera recording are started simultaneously, and fixed-point image acquisition is performed after the deposition begins.
[0050] The results show that, Figure 5 As shown, a current density of 20 mA / cm² is used. 2 A constant current was applied, and a parallel magnetic field with a strength of 0.4 T was used for constant current electrodeposition for 30 min. During the test, images were captured at four different time points: 0 min, 10 min, 20 min, and 30 min, which were marked with colored numerical boxes 1, 2, 3, and 4, respectively. The corresponding overpotential values were marked in the corresponding time-voltage curves. Figure 5 (a) and Figure 5 (b) shows the time-voltage curve and in-situ optical image of zinc electrodeposition without a magnetic field. Figure 5 (a) and Figure 5 In (b), red box 1 shows the initial state before zinc electrodeposition. Subsequently, electrodeposition was performed for 10 minutes without a magnetic field, from... Figure 5In Figure (a), at point 2 (red box), an overpotential value as high as 0.31 V can be observed, accompanied by fluctuations. This is caused by severe concentration polarization resulting from the high current density. During this stage, a thick and loose zinc deposition layer appears. Figure 5 In the image corresponding to red box 2 in (b), a large number of small zinc dendrites are clearly visible in the deposited layer, accompanied by a large hydrogen bubble. As the deposition time increases to 20 min ( Figure 5 In (b), red box 3), the voltage fluctuation amplitude increased, and zinc dendrite growth became more intense, with a further increase in the number and length of dendrites. Electrodeposition ended at 30 min. Figure 5 In (b), red box 4), the entire zinc deposition layer exhibits a very rough, forest-like morphology, with large and sharp zinc dendrites reaching lengths of up to 500 µm. Conversely, zinc electrodeposition under a parallel magnetic field exhibits drastically different behavior. Figure 5 As shown in (c), the time-voltage curve for zinc electrodeposition under a parallel magnetic field is flat and without fluctuations, and the overpotential is stably maintained at 0.1 V, which is much smaller than 0.31 V without a magnetic field. Figure 5 As shown in (d), no obvious dendrite growth was observed throughout the zinc electrodeposition process. Zinc was uniformly covered on the substrate, with only a small bubble on the surface caused by hydrogen evolution. The in-situ optical microscopy characterization results clearly and powerfully demonstrate that applying a parallel magnetic field can also effectively suppress zinc dendrite growth.
[0051] It should be understood that the application of this utility model is not limited to the examples above. Those skilled in the art can make improvements or modifications based on the above description, and all such improvements and modifications should fall within the protection scope of the appended claims.
Claims
1. A dendrite monitoring device integrating in-situ magnetic field and optical observation coupling, characterized in that, include: Electrochemical testing module, magnetic field generation module, and optical observation and recording module; The electrochemical testing module includes: an electrolytic cell with at least one optically transparent window as the observation surface, a zinc negative electrode and a copper positive electrode disposed on opposite sides of the electrolytic cell, and a charge-discharge tester connected to the zinc negative electrode and the copper positive electrode; the electrolytic cell is used to contain electrolyte. The magnetic field generating module is used to generate a static magnetic field with controllable direction and intensity in the electrolytic cell area; The optical observation and recording module includes: an optical microscope and a camera unit; the lens of the optical microscope is aimed at the zinc sheet negative electrode deposition surface in the electrolytic cell; The static magnetic field generated by the magnetic field generating module acts on the electrolytic cell area, and the charge-discharge tester controls the deposition process and is triggered synchronously with the optical observation and recording module to realize dynamic in-situ recording of the deposition morphology under static magnetic field environment.
2. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 1, characterized in that, Also includes: Computer control module; The computer control module is connected to the charge-discharge tester and is used to set the deposition parameters controlled by the charge-discharge tester and synchronously send trigger signals to the camera unit.
3. The in-situ magnetic field and optical observation coupled dendrite monitoring device according to claim 1, characterized in that, The zinc negative electrode and the copper positive electrode are fixed in the electrolytic cell by a fixing device, and the two are kept in parallel relative positions with adjustable spacing.
4. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 1, characterized in that, The magnetic field generating module includes: a magnetic field generator and a magnetic field generating power supply for controlling the magnetic field strength of the magnetic field generator.
5. The in-situ magnetic field and optical observation coupled dendrite monitoring device according to claim 4, characterized in that, The magnetic field generator is an electromagnet or permanent magnet system with adjustable pole spacing.
6. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 4, characterized in that, The magnetic field generator is arranged around the outside of the electrolytic cell.
7. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 4, characterized in that, The magnetic field strength range of the magnetic field generator is 0 ~ 5 T.
8. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 1, characterized in that, The direction of the static magnetic field is either perpendicular or parallel. Wherein, the vertical direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode, and the parallel direction is parallel to the current direction between the zinc negative electrode and the copper positive electrode.
9. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 1, characterized in that, The optical observation and recording module also includes a light source for illumination.
10. The in-situ magnetic field and optical observation coupled integrated dendrite monitoring device according to claim 1, characterized in that, The camera unit is a high-speed or high-resolution camera.