METHOD FOR SEALING A MOLD FOR ALUMINOTHERMAL RAIL WELDING

DE502019012448D1Active Publication Date: 2024-11-28GOLDSCHMIDT GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502019012448
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-08-15
Filing Date
2019-07-31
Publication Date
2024-11-28
Estimated Expiration
2039-07-31

AI Technical Summary

Technical Problem

Current methods for sealing the casting space in aluminothermal rail connection and repair welds are time-consuming, labor-intensive, and prone to defects due to the use of lubricating sand, which can interact with molten steel and require manual application, leading to inconsistencies in sealing effectiveness.

Method used

Employing a thermally or chemically expandable fireproof sealing compound, such as expanded graphite, that fills gaps between mold halves and rail ends, providing a reliable seal through volume expansion initiated by heat or chemical reaction, reducing the need for large quantities of sealing material and minimizing dependence on welder expertise.

Benefits of technology

The method simplifies the sealing process, reduces time and effort, eliminates moisture-related defects, and ensures consistent sealing without the need for extensive manual application, enhancing the reliability and efficiency of the aluminothermal welding process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to methods for sealing the casting chamber of casting molds for carrying out aluminothermic rail joint welding and to methods for sealing the casting chamber of casting molds for carrying out aluminothermic repair welding.

[0002] An aluminothermic welded joint consists of an intermediate cast structure filling a weld joint between the end faces of the rail ends to be joined, which is produced as a reaction product of the aluminothermic fine-grained mixture of iron oxide and aluminum, to which certain alloying elements can be added to influence the hardness as well as other reactants to dampen the reaction.

[0003] The welding of the rail ends is regularly carried out under preheating to ensure homogeneous surface temperatures on the inner walls of the casting chamber and to expel any moisture present. The surface temperatures influence the cooling rate of the molten steel and thus the casting time and speed. However, temperature deviations are unavoidable depending on the different thermal conductivities of the inner walls of the casting mold and the end faces of the rail ends.

[0004] Such a casting mold is known, for example, from EP 0 925 866 B1 and consists of two mold halves positioned on either side of the rail joint to be produced, symmetrically overlapping the weld joint. The weld joint, together with the end faces of the rail ends to be joined and the inner walls of the mold halves, forms a casting chamber whose core area replicates the rail profile and into which the reaction product of the aluminothermic reaction, namely molten steel, is poured from the top.

[0005] The two mold halves form interfaces not only in the mold's parting plane, but also on the surfaces of the rail ends to be aluminothermically welded. Thus, gaps exist between them that require sealing to prevent uncontrolled escape of molten steel. This sealing must be designed to withstand the temperatures of the molten steel during the pouring process.

[0006] It is known to use so-called lubricating sand to seal these gaps. This sand must be carried in 25 kg bags when working on the laid track. This lubricating sand must be applied manually from the outside of the mold to each weld, thereby closing the gap, which is a considerable time-consuming process. This type of sealing is also not free from interactions with the molten steel, as sand burns can occur at the points where the lubricating sand comes into contact with the molten steel, which can be difficult to remove later by grinding. Furthermore, the lubricating sand regularly contains moisture, so that vapor bubbles can form under the influence of heat, which can lead to welding defects such as "worm holes."

[0007] From CH 658 817 A5 a method and a device for aluminothermic welding are known, in which a casting mold consists of two mold halves which are provided with sealing materials on their contact surfaces, wherein the mold halves are tightly closed by means of a pressing device which is firmly tightened.

[0008] The problem of sealing the casting chamber arises not only in rail joint welding but also in rail head repair or build-up welding and other welding operations that are carried out using aluminothermic methods.

[0009] From FR 2 323 488 A1, which forms the basis for the preamble of the independent claims, a method for sealing the casting chamber of a casting mold used in an aluminothermic rail welding process is known. The mold consists of two opposing mold halves. The mold halves are provided with grooves on their flat surfaces facing the respective rail ends, which grooves are designed to accommodate a thermally expandable sealing compound. Depending on the gaps existing between said surfaces and the rail ends in the region of the grooves, the sealing compound can expand both to the outside and into the actual casting chamber depending on the resulting pressure conditions, thereby disrupting the welding process.

[0010] EP 0 444 480 A1 discloses another comparable method for sealing a casting chamber of a casting mold used in an aluminothermic process. The mold halves are provided with recesses designed to receive a sealing compound that seals the gap between the surface of a rail end facing the mold half and the mold half. The sealing compound, which is in a malleable state, is introduced into the recess after the mold halves have been positioned and secured. However, due to the open design toward the outside, a reproducible pressure buildup is only possible to a limited extent.

[0011] WO 2014 / 106646 A1 discloses a process for producing core and / or molding sand for foundry purposes, using a mineral molding base material with a binder consisting of water glass and expanded graphite. This binder mixture is intended to facilitate core removal and simultaneously improve the surface quality of the resulting casting.

[0012] This well-known technique for producing a seal for the casting mold is therefore technically suboptimal, time-consuming and labor-intensive, and difficult to handle in practice when working on laid track, as heavy tools must be carried along. The achievable result also depends on the experience and diligence of the welder.

[0013] The object of the invention is to develop methods of the type mentioned above with a view to simplifying the sealing of the casting chamber. This object is achieved in such methods by the features of claims 1 and 2.

[0014] The key is to use a mineral or carbon-based, refractory sealant that expands through thermal or chemical initiation instead of the previously used smear sand. The idea is to position this compound in a gap defined on one side by the surfaces of the rail body or other two workpieces to be welded, and on the other side by wall sections of the mold halves. Through thermally or chemically initiated expansion of the sealant, it will fill the gap, be pressurized within it, and thus form a seal that reliably seals the gap. During thermally initiated expansion, an embedded or chemically bound liquid evaporates due to the heat input, and the resulting increase in volume causes the compound to expand.For example, hydrates, carbonates, or nitrates can be used in this context, which release hydrogen, carbon dioxide, or nitrogen. In chemically initiated expansion, a chemical reaction leads to the release of a gas or vapor, which causes the compound to expand. Because the sealing compound is therefore expandable, this has the advantage that significantly less mass needs to be carried when working on the laid track compared to the conventional use of smear sand. Since these sealing compounds develop their actual sealing effect as a result of expansion after proper application, the care required to seal the casting mold is reduced, as is the associated time and effort.Since the process of applying the sealant is simplified, there is less dependence on the care and experience of the welder performing this work. A further advantage is that the risk of moisture ingress into the casting chamber of the mold, which cannot otherwise be ruled out when using smear sand, is eliminated.

[0015] An expandable sealing compound can be used, similar to the use of lubricating sand previously used for this purpose, also on the outside of the casting mold, i.e., next to an actual weld bead, without contacting it. In this case, too, a gap between the rail body and the surfaces of the casting mold facing it is sealed. The advantages associated with using such a compound as a sealing compound are also present in this case.

[0016] The areas of application of a casting mold equipped according to the invention relate to rail joint welding or repair welding. The latter typically involves repairing wear-related defects of the rail head, particularly rail defects such as squats, burrs, indentations, chipping, and spin marks. In such repair welding, the damaged part of the rail head is first removed, and then the resulting recess is filled with a build-up weld. The aim is to achieve a consistent progression of the essential properties of the rail body across the weld. In addition to rail joint welding, the invention can also be used for welding other workpieces wherever aluminothermic welding is used.

[0017] The sealant can be inserted directly into the grooves of the mold halves and then placed in this state at the welding site. This means that the mold halves and the sealant can be brought to their place of use as a single piece. However, the sealant can also be introduced into the grooves of the mold halves at the respective place of use. This means that the mold halves and the sealant are brought to their place of use separately.

[0018] To initiate the expansion of the sealant, materials capable of exothermic reaction can be used. Such a reaction can be triggered by an ignition rod, which initiates the expansion process. However, expansion can also be triggered directly by preheating the mold. In any case, this requires sufficient heat to be introduced into the sealant, so other techniques familiar to the expert are also available.

[0019] The casting mold is adapted to the expansion process of the sealing compound. The aim here is to prevent the compound, which is held in a groove, from expanding toward the casting chamber. At the same time, the expansion process must generate sufficient pressure in the groove, which is machined into a wall section of the casting mold, to create a reliable sealing effect in a gap between the rail body and the opposing wall sections of the casting mold. This can be achieved, for example, by different inside and outside gap widths, so that correspondingly different outflow resistances are presented for the expanding sealing compound and outflow to the inside is at least severely impeded.

[0020] According to the features of claim 4, the sealing compound, e.g., expandable graphite, is used as a shaped body, wherein production by an extrusion process is suitable.

[0021] According to the features of claims 5 to 7, the sealing compound is used in the form of a tape, in particular a self-adhesive tape. This offers the advantage of flexible installation on the contours of the mold halves or the rail body. With appropriate structural provisions on the mold halves, for example, in the form of grooves, it is possible to fix the tape in these grooves with a positive fit.

[0022] According to the features of claims 8 to 10, the sealing compound is used in the form of a pasty mass, which is applied at its application site in a bead-like manner by spraying or injected into a groove of the respective mold half. In this case, the sealing compound can be delivered to the application site in a cartridge.

[0023] According to the features of claim 11, expandable graphite is used in the form of a free-flowing granulate, which is then mixed with other mineral refractory materials to modify their properties. A mixture of materials composed in this way can then be used as an expandable sealing compound.

[0024] According to the features of claim 12, an intumescent mass or a mass containing at least intumescent components is used as the expandable sealing compound. This intumescent mass is expandable graphite. The expansion of expandable graphite, which can be triggered by increasing the temperature, is known but has so far only been used as a flame retardant, namely to prevent the spread of fire, in metallurgy as oxidation protection, and in the chemical industry in conjunction with varnishes and paints. Expandable graphite meets all the requirements that must be met by a sealing compound in a casting mold for aluminothermal welding processes. Another mineral mass that can be used in this context is vermiculite, a mineral, particularly silicate, material from which water vapor is released when heat is applied, leading to expansion.In this context, expanded graphite can be used alone or in combination with other mineral substances.

[0025] The features of claim 13 are directed to a particular type of use of the expandable sealing compound. This compound develops a sealing effect by directly contacting a weld bead.

[0026] It can be seen that the method according to the invention makes it possible to provide a seal for the casting chamber of a casting mold to be used in an aluminothermic process in a simple and rapid manner, with less work than with the method presented at the beginning, which is to be assigned to the state of the art, and in a reproducible manner independent of the experience and care of the respective welder.

[0027] The invention will be explained in more detail below with reference to the accompanying drawings. They show: Fig. 1 is a perspective view of a casting mold according to the invention in partial section; Fig. 2 is a planar sectional view of a casting mold half according to Fig. 1 in the initial state; Fig. 3 a planar sectional view of a casting mold half according to Fig. 2 at the time of the beginning of an expandable graphite expansion; Fig. 4 a planar sectional view of a casting mold half according to Fig. 2 at the time of the beginning of an expandable graphite expansion during the initiation of the expansion process by preheating; Fig. 5 a planar sectional view of a casting mold half according to Fig. 2 at the time of completed expandable graphite expansion; Fig. 6 a planar sectional view of a casting mold prepared for overlay repair welding in the rail head area; Fig. 7 a planar partial sectional view of a band-shaped insert of expandable graphite as a sealant in a casting mold.

[0028] Fig. 1shows two rail ends 1, 2 to be welded by means of an aluminothermic process, between whose mutually facing end faces a weld joint 3 exists. 4, 5 denote two identical mold halves of a casting mold 6, which are made of the usual refractory material and are partially enclosed on the outside in a metallic casing 7, a retaining plate.

[0029] The mold halves 4, 5, of which the last-mentioned is only shown incompletely, lie in the assembled state of the casting mold 6 in a vertical parting plane against one another and - seen in the longitudinal direction of the rail ends 1, 2 - surround the welding joint 3 on both sides, forming a casting space 8 which is delimited by the end faces of the rail ends 1, 2 and furthermore laterally and underside by wall sections of the mold halves 4, 5.

[0030] The two mold halves 4, 5 are secured together for welding by means not shown in the drawing. The aluminothermic reaction takes place in a crucible (also not shown in the drawing) placed on the casting mold 6. One of the reaction products is molten steel, which is then introduced into the open-topped casting mold.

[0031] Both mold halves 4, 5 have grooves 11, 12 on their wall sections 9, 10 adjacent to the rail ends 1, 2, into each of which a band 13, 14 is inserted, which consists of a thermally expandable substance, e.g., expandable graphite. Fig. 1shows the respective band 13, 14 after expansion, which takes place towards the outside, thus away from the casting chamber 8. To ensure this, the gaps between the wall sections 9, 10 and the rail ends 1, 2 on the inside, i.e. the sides facing the casting chamber 8, are smaller than those on the outside, so that there is a significantly greater flow resistance towards the inside than towards the outside. The expansion of the bands 13, 14 leads to the formation of beads 15, 16 on the outside of the wall sections 9, 10, whereby in the space between the rail ends 1, 2 and the grooves 11, 12, as a result of the expansion, promoted by a throttling effect during the flow of the expandable substance, there is compaction and the formation of a reliable sealing effect by this substance.

[0032] In the Figures 2 to 5 are functional elements that are compatible with those of the Fig. 1correspond, are quantified accordingly, so that a repeated description in this regard can be dispensed with.

[0033] Figure 2 shows the casting mold 6 in a state shortly before the pouring of molten steel, with 17 denoting the inlet of a side riser not otherwise shown in the drawing. It can be seen that the gap widths 18 between the wall sections 9, 10 and the rail ends 1, 2 on the inside, namely on the side facing the casting chamber 8, are significantly smaller than the gap widths 19 on the respective outside. In this way, a clearly preferred expansion direction of the strips 13, 14 is structurally predetermined. Fig. 2 shows bands 13, 14 in a not yet expanded state.

[0034] Fig. 3shows the casting mold 6 in a state in which the expansion of the strips 13, 14 has been initiated manually by means of a pyrotechnic mass 32 or an exothermically reactive mass with an ignition rod 20. The beads 15, 16 are formed, and a seal is established across the gap widths 18, 19. After completion of this process, the molten steel can be poured.

[0035] Fig. 4 shows the casting mold 6 in a state in which the expansion of the strips 13, 14 is just beginning. This expansion is thermally initiated by the preheating of the casting chamber 8, which is effected in a conventional manner, with the heat introduced thereby acting on the strips from the inside of the casting chamber 8.

[0036] Fig. 5shows the casting mold in a state in which the expansion of the bands 13, 14 is completed, so that beads 15, 16 have been formed on the outer sides of the casting mold 6 and a sufficient sealing profile has been created in the area of ​​the gap widths 18, 19.

[0037] Fig. 6 shows a casting mold 21 configured for repair welding on the rail head 22 of a rail profile 23. The casting mold 21 in turn consists of two mold halves 24, 25, which are fixed on both sides of the rail profile 23 in a manner not shown in the drawing, for example by means of a retaining plate, and which lie sealingly against one another along a vertical parting plane 26, thereby forming a casting chamber 27 open at the top.

[0038] The dividing plane 26 extends in a vertical center plane of the rail profile 23, with both mold halves 24, 25 engaging below the rail head 22. 28, 29 denote grooves in the mold halves, which extend below the rail head 22 parallel to a longitudinal direction of the rail and each accommodate a strip 30, 31, which is made of the same material as the strips 13, 14.

[0039] In preparation for a build-up repair welding, the damaged area of ​​the rail head profile is removed by grinding and / or other abrasive processing, e.g., by means of a cutting torch, and the casting mold 21 is positioned and fixed around the exposed area of ​​the rail profile 23.

[0040] The belts 13, 14 are intended to create a seal on the underside of the casting chamber 27. In preparation for a steel pour, an expansion of the belts 30, 31 is initiated, which can be carried out in the same way as with the casting mold 6. It is essential that, after the expansion is complete, the underside of the casting chamber 27 is sealed. If necessary, a comparable sealing system can also be provided in the vertical direction between the wall sections of the casting mold 21 and the rail profile.

[0041] In a reaction crucible placed on the casting mold 21, a steel melt is prepared in a conventional manner by aluminothermic means, to which alloying elements are optionally added depending on the material of the rails to be treated. The cast steel poured into the casting chamber fills, in particular, the recess in the rail head 22 created by material removal, with the proviso that in this area treated by build-up welding, particularly in a running surface, metallurgical properties, for example with regard to hardness and strength, are presented that correspond as closely as possible to those of the remaining running surface profile, so that no discontinuity in the property profile arises as a result of the build-up welding.

[0042] The application of the method according to the invention was presented above with reference to a two-part casting mold 6 composed of two mold halves 4, 5. However, the application of the method is not limited to such casting molds and can equally be used with three-part casting molds, e.g., composed of a base plate supporting the rail foot and two side mold parts, or with any other multi-part casting mold. Fig. 7 shows an application of the expandable sealing compound 33, e.g., expandable graphite or another substance, in a gap 36 to be sealed between an underside of the rail end 1 and a surface section 35 of the casting mold 21 facing this.

[0043] The sealing compound 33 is incorporated into a tubular casing 34, which may be bonded to the surface section 35 in its initial or as-delivered state. The casing 34 consists of a fire-resistant material, e.g., a fabric, which may be elastic or inelastic.

[0044] Figure 7 shows the sealing compound 33 in an expanded state, in which the enveloping body 34, under the pressure of the sealing compound 33, firmly adheres to the aforementioned underside of the rail end 1 and the surface section 35, thereby sealing the gap 36. In the initial state, in which the sealing compound has not yet expanded, the enveloping body is accordingly in a relaxed state.

[0045] With regard to preheating and initiation of the expansion process of the sealing compound 33, the above statements apply analogously. List of reference symbols: 1. end of rail 10. Wall section 2 end of rail 11. Nut 3. Weld joint 12. Nut 4 mold half 13. edge 5 mold half 14. band 6 Casting mold 15. bead 7. Wrapping 16. bead 8. Casting room 17. Side climber 9. Wall section 18. Gap width 19. Gap width 20. ignition rod 21. Casting mold 22. Rail head 23. Rail profile 24. mold half 25. mold half 26. Division level 27. Casting room 28. Nut 29. Nut 30. band 31. band 32. pyrotechnic mass 33. Sealant 34. Envelope 35. Area section 36. gap

Claims

1. Method for sealing the casting space (8) of a casting mould (6) in order to carry out aluminothermic rail-joint welding between two rail ends (1, 2) comprising two mould halves (4, 5) producing a casting mould which is open at the top and reproducing the rail profile in the region of the welding, gaps present between the facing surfaces of the rail ends (1, 2) and the wall portions (9, 10) adjacent thereto of the casting mould (6) being sealed with a refractory sealing compound, in a reaction crucible, a molten steel being provided and introduced into the casting space (8) in order to carry out the welding set up as rail-joint welding, an expandable intumescent substance being used as the sealing compound, the expansion of which is thermally initiated by a pyrotechnic substance, an exothermically reactive substance, or by preheating the casting mould (6) before pouring in the molten steel, and the sealing compound being received in grooves (11, 12) in the mould halves (4, 5), characterized in that gaps between the wall portions 9, 10 and the rail ends 1, 2 on the inner sides, that is to say the sides facing the casting space (8), are formed so as to be smaller than those on the outer sides so that there is much greater flow resistance towards the inside than towards the outside.

2. Method for sealing the casting space (27) of a casting mould (21) in order to carry out aluminothermic repair welding comprising two mould halves (24, 25) producing a casting mould which is open at the top and reproducing a rail profile (23) in the region of the welding, gaps present between the facing surfaces of the rail profile (23) and the wall portions adjacent thereto of the casting mould being sealed with a refractory sealing compound, in a reaction crucible, a molten steel being provided and introduced into the casting space (27) in order to carry out the welding set up as repair welding, an expandable intumescent substance being used as the sealing compound, the expansion of which is thermally initiated by a pyrotechnic substance, an exothermically reactive substance, or by preheating the casting mould (21) before pouring in the molten steel, and the sealing compound being received in grooves (28, 29) in the mould halves (24, 25), characterized in that gaps between the wall portions of the casting mould (21) and the rail profile (23) on the inner sides, that is to say the sides facing the casting space (27), are formed so as to be smaller than those on the outer sides so that there is much greater flow resistance towards the inside than towards the outside.

3. Method according to either Claim 1 or Claim 2, characterized in that, in conjunction with an assembly of the mould halves (4, 5; 24, 25) at each welding point, the sealing compound is introduced into grooves (11, 12; 28, 19) in the mould halves.

4. Method according to Claim 1, Claim 2 or Claim 3, characterized in that the expandable sealing compound is used in the form of a shaped body.

5. Method according to Claim 1, Claim 2 or Claim 3, characterized in that the expandable sealing compound is used in the form of a strip.

6. Method according to Claim 5, characterized in that the strip is used in the form of an adhesive, in particular self-adhesive strip.

7. Method according to either Claim 5 or Claim 6, <b>characterized in that, in the location of the welding point, the strip is fixed in an interlocking manner in grooves (11, 12; 28, 29) in the mould halves (4, 5; 24, 25).

8. Method according to either Claim 1 or Claim 2, characterized in that the expandable sealing compound is used in the form of a pasty substance.

9. Method according to Claim 8, characterized in that the pasty substance is applied to the point of application thereof in the form of a bead.

10. Method according to Claim 9, <b>characterized in that, in the location of the welding point, the pasty substance is injected into grooves (11, 12; 28, 29) in the mould halves (4, 5; 24, 25).

11. Method according to either Claim 1 or Claim 2, characterized in that the expandable sealing compound is used in the form of free-flowing granules.

12. Method according to any of Claims 1 to 11, characterized in that a substance consisting of a combination of exfoliated graphite and other mineral refractory materials is used as an expandable sealing compound.

13. Method according to any of Claims 1, 3 to 6, 8, 9, 10 and 11, characterized in that the expandable sealing compound is used reproducing a weld bead geometry.