SUBSTRATE FOR A TEMPERATURE-COMPENSATED DEVICE WITH ACOUSTIC SURFACE OR VOLUME WAVES

DE602016096316T2Active Publication Date: 2026-09-30SOITEC SA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602016096316
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2015-12-22
Filing Date
2016-12-21
Publication Date
2026-09-30
Estimated Expiration
2036-12-21

AI Technical Summary

Technical Problem

SAW and BAW devices are sensitive to temperature variations due to differing thermal expansion coefficients of piezoelectric and metallic materials, leading to instability and spurious resonances, especially when exposed to high temperatures during manufacturing processes.

Method used

A substrate is designed with a semiconducting layer between a piezoelectric layer and a stiffening substrate, where the stiffening substrate has a thermal expansion coefficient closer to the piezoelectric material, minimizing thermal stress and allowing integration of electronic components, using materials like sapphire, glass, or spinel, and semiconductor layers such as silicon, germanium, or SiGe, with a dielectric layer for improved bonding.

Benefits of technology

The substrate provides enhanced thermal stability up to 300°C, reducing mechanical stress and enabling easy integration of electronic components, thus stabilizing the device performance and preventing spurious resonances.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

DOMAINE DE L'INVENTION

[0001] The present invention relates to a substrate for a temperature-compensated surface acoustic wave or body acoustic wave device, as well as a method for manufacturing such a substrate and a surface acoustic wave or body acoustic wave device comprising such a substrate. ARRIERE PLAN DE L'INVENTION

[0002] Surface acoustic wave devices, generally referred to by the acronym SAW, from the English term "Surface Acoustic Wave", find applications in the field of radio frequency (RF) communications, particularly for filter applications.

[0003] A SAW device typically comprises a piezoelectric layer and two electrodes in the form of two interdigitated metal combs deposited on the surface of said piezoelectric layer.

[0004] An electrical signal, such as a change in voltage, applied to one electrode is converted into an elastic wave that propagates across the surface of the piezoelectric layer. This wave is then converted back into an electrical signal upon reaching the other electrode.

[0005] The choice of piezoelectric material takes into account the electromechanical coupling coefficient which reflects the rate of electromechanical conversion by said material, and the temperature stability of the oscillation frequency of the piezoelectric material.

[0006] However, SAW devices are very sensitive to temperature variations, which induce different expansions of the piezoelectric layer and metallic electrodes due to the different coefficients of thermal expansion of these materials.

[0007] More precisely, the temperature frequency coefficient, denoted TCF, an acronym for the Anglo-Saxon term "Temperature Coefficient of Frequency", which is defined as the frequency variation for a given frequency f as a function of temperature T, is given by the formula: TCF = 1 f ∂ f ∂ T = TCV − CTE Or : TCV = 1 V ∂ V ∂ T V is the speed of surface acoustic waves and CTE is the coefficient of thermal expansion of the piezoelectric material in the direction of propagation of surface acoustic waves.

[0008] Measures already exist to compensate for the effects of temperature on SAW devices.

[0009] In particular, the article by Hashimoto et al [1] presents a review of the different temperature compensation techniques for SAW devices.

[0010] Among these different techniques, the main ones are: (1) an overlay technique consisting of covering the surface of the piezoelectric layer and the electrodes with a dielectric material (typically silicon dioxide (SiO₂)), which has a coefficient of thermal expansion opposite to that of the piezoelectric layer; (2) a wafer bonding technique consisting of bonding the piezoelectric layer to a substrate with the lowest possible coefficient of thermal expansion so as to block the thermal expansion of the piezoelectric layer. This substrate, which may be, for example, silicon, sapphire, glass, or spinel (MgAl₂O₄), thus provides rigidity to the piezoelectric layer. Given its thickness, the piezoelectric layer is considered to extend infinitely in a direction opposite to the electrodes, so that the presence of the substrate does not disrupt the propagation of surface acoustic waves.However, the bonding of the support substrate seems to create spurious resonances at frequencies higher than the main frequency of the device (cf. [1]. Fig. 5 ).

[0011] Substrates for acoustic wave devices having a semiconducting layer in their structure are presented for example in EP 2 738 939 A1 or US 4 019 200.

[0012] Among the materials considered for the support substrate in this second technique, silicon seems the most promising because it allows the implementation of processes for integrating electronic components at the substrate level ("wafer level", according to Anglo-Saxon terminology).

[0013] However, there is a significant difference in the coefficient of thermal expansion between the piezoelectric material and silicon (for an anisotropic LiTaO3 crystal, the CTEs are approximately 4 x 10⁻⁶ / °C and 14 x 10⁻⁶ / °C, while the CTE of silicon is on the order of 2.3 x 10⁻⁶ / °C). This difference affects the stability of the substrate / piezoelectric layer stack if it is exposed to high temperatures during subsequent stages of the surface acoustic wave device manufacturing process. For such stages, it is necessary to ensure the thermal stability of the piezoelectric layer / substrate stack up to a temperature of approximately 250°C.

[0014] A similar problem arises for bulk acoustic wave filters and resonators, known by the acronym BAW (from the Anglo-Saxon term "Bulk Acoustic Wave").

[0015] Volume acoustic wave filters and resonators typically comprise a thin piezoelectric layer (i.e., generally less than 1 µm thick) and two electrodes arranged on each main face of said thin layer. An electrical signal, such as a change in voltage, applied to one electrode is converted into an elastic wave that propagates through the piezoelectric layer. This wave is converted back into an electrical signal upon reaching the electrode on the opposite face. BREVE DESCRIPTION DE L'INVENTION

[0016] One aim of the invention is to design a substrate for a surface acoustic wave device or for a temperature-compensated body acoustic wave device that overcomes the drawbacks mentioned above. In particular, such a substrate must be more stable than the silicon support substrate / piezoelectric layer stack mentioned above up to a temperature of approximately 300°C, while also allowing for easy integration of electronic components.

[0017] According to the invention, a substrate is proposed for a surface acoustic wave or body acoustic wave device, comprising a support substrate and a piezoelectric layer on said support substrate, characterized in that the support substrate comprises a semiconducting layer on a stiffening substrate having a coefficient of thermal expansion closer to the coefficient of thermal expansion of the material of the piezoelectric layer than that of silicon, the semiconducting layer comprising at least one electronic component and being arranged between the piezoelectric layer and the stiffening substrate.

[0018] The electronic component in question is chosen from: a CMOS transistor, a switch, and a power amplifier.

[0019] The stiffening substrate advantageously comprises sapphire, glass and / or spinel (MgAl 2 O 4 ).

[0020] Preferably, the semiconductor layer is formed from one of the following materials: silicon, germanium, SiGe, SiC, III-V material.

[0021] According to one embodiment, the ratio between the thickness of the piezoelectric layer and the thickness of the stiffening substrate is less than or equal to 0.125.

[0022] For example, the thickness of the piezoelectric layer is less than 50 µm, preferably less than 20 µm, even more preferably less than 1 µm, and the thickness of the stiffening substrate is between 400 and 800 µm.

[0023] According to one embodiment, the substrate comprises a dielectric layer between the piezoelectric layer and the semiconductor layer and a charge-trapping layer at the interface between said dielectric layer and the semiconductor layer and / or at the interface between the dielectric layer and the piezoelectric layer.

[0024] The charge-trapping layer may include a layer of polycrystalline silicon.

[0025] In the case where the piezoelectric layer is anisotropic and therefore has at least two different coefficients of thermal expansion in a plane parallel to a main face of the substrate, we consider the coefficient of thermal expansion providing the greatest difference with respect to the coefficient of thermal expansion of the stiffening substrate.

[0026] The invention also relates to a surface acoustic wave device comprising a substrate as described above and two electrodes formed of two metal combs interdigitated on the surface of the piezoelectric layer.

[0027] The invention also relates to a volume acoustic wave device comprising a substrate as described above and two electrodes arranged on either side of the piezoelectric layer.

[0028] Another object relates to a process for manufacturing a substrate as described above, characterized in that it comprises: the transfer of the semiconductor layer onto the stiffening substrate from a first donor substrate, the transfer of the piezoelectric layer onto the semiconductor layer from a second donor substrate.

[0029] According to one embodiment, at least one of the transfer steps includes the following substeps: formation of a weakening zone in the first, respectively the second donor substrate by implantation of atomic species; bonding of the first, respectively the second donor substrate on the stiffening substrate, respectively on the semiconducting layer; detachment of said first, respectively second, substrate along the weakening zone. BREVE DESCRIPTION DES DESSINS

[0030] Other features and advantages of the invention will become apparent from the detailed description that follows, with reference to the accompanying drawings in which: there figure 1 is a schematic cross-sectional view of a temperature-compensated surface acoustic wave filter, the figure 2 is a schematic cross-sectional view of a temperature-compensated volume acoustic wave resonator, the figure 3 is a cross-sectional diagram of a substrate according to one embodiment of the invention, the figure 4 is a cross-sectional diagram of a temperature-compensated surface acoustic wave filter according to an embodiment of the invention, the figure 5 is a cross-sectional diagram of a temperature-compensated surface acoustic wave filter according to an embodiment of the invention, the figures 6A à 6E illustrate successive stages in the manufacture of a substrate according to an embodiment of the invention.

[0031] For the sake of clarity, the illustrated elements are not necessarily drawn to scale. Furthermore, elements designated by the same reference symbols in different figures are identical. DESCRIPTION DETAILLEE DE MODES DE REALISATION DE L'INVENTION

[0032] There figure 1 is a schematic view of a surface acoustic wave filter.

[0033] The filter comprises a piezoelectric layer 10 and two electrodes 12, 13 in the form of two interlocking metal combs deposited on the surface of the piezoelectric layer. On the side opposite the electrodes 12, 13, the piezoelectric layer rests on a support substrate 11 designed to provide temperature compensation, the structure of which will be described in detail below. The piezoelectric layer 10 preferably has excellent crystalline quality to avoid attenuation of the surface wave. The layer is therefore single-crystal. Currently, suitable materials for industrial use are quartz, LiNbO3, or LiTaO3. The piezoelectric layer 10 is generally obtained by cutting an ingot of one of these materials; the required precision for the thickness of the layer is not critical since the waves must propagate primarily on its surface.

[0034] There figure 2 is a schematic view of a volume acoustic wave resonator.

[0035] The resonator comprises a thin piezoelectric layer (i.e., generally less than 20 nm thick) and two electrodes 12, 13 arranged on either side of said piezoelectric layer 10. The piezoelectric layer 10 rests on a support substrate 11, the structure of which will be described in detail below. To isolate the resonator from the substrate and thus prevent wave propagation within the substrate, a Bragg mirror 14 is interposed between the electrode 13 and the substrate 11. Alternatively (not illustrated), this isolation could be achieved by creating a cavity between the substrate and the piezoelectric layer. These different arrangements are known to those skilled in the art and will therefore not be described in detail in this text.

[0036] For a bulk acoustic wave device, the piezoelectric layer 10 has a fixed and uniform thickness throughout. However, since crystalline quality is not particularly important for the resonator's performance, a polycrystalline piezoelectric material is acceptable. The piezoelectric layer 10 is therefore generally formed by deposition onto a support (for example, a silicon substrate). Currently, the materials used industrially for such deposition are AIN, ZnO, and PZT.

[0037] There figure 3 is a cross-sectional diagram of a substrate for manufacturing a surface acoustic wave or temperature-compensated body acoustic wave device according to one embodiment of the invention.

[0038] The substrate 1 includes a piezoelectric layer 10 intended to receive electrodes to form a surface or volume acoustic wave device.

[0039] The material, crystalline quality, and thickness of the piezoelectric layer 10 are chosen by a person skilled in the art according to the intended application. The selection criteria are known in themselves and do not need to be described in detail in this text.

[0040] If the chosen piezoelectric material is anisotropic, it exhibits different coefficients of thermal expansion in different directions.

[0041] The piezoelectric layer 10 is arranged on a composite support substrate 11, that is to say formed from a stack of several layers of different materials.

[0042] The said support substrate 11 includes a substrate 110 called stiffener whose function, within the substrate 1, is to ensure the rigidity of the stack in particular during heat treatments.

[0043] The stiffening substrate 110 advantageously comprises sapphire, glass and / or spinel (MgAl 2 O 4 ).

[0044] These materials have the advantage of having a coefficient of thermal expansion closer to the coefficient of thermal expansion of the piezoelectric material than silicon, which allows better temperature stability (up to about 300°C) of the stack, although this greater proximity of the coefficients of thermal expansion slightly penalizes the temperature compensation effect.

[0045] Furthermore, the stiffening substrate 110 has a significant thickness, typically on the order of 400 to 800 µm, which is considerably greater than the thickness of the other layers of substrate 1 and, in particular, much greater than the thickness of the piezoelectric layer, which is generally less than 50 µm, preferably less than 20 µm, and even more preferably less than 1 µm. Thus, the temperature behavior of the stiffening substrate is predominant compared to that of the other layers.

[0046] Due to the relative proximity between the coefficient of thermal expansion of the stiffening substrate 110 and the piezoelectric layer 10, the stresses due to the difference in coefficients of thermal expansion during heat treatments undergone by the substrate 1 are minimized.

[0047] A semiconductor layer 111 is interposed between the stiffening substrate 110 and the piezoelectric layer 10. This semiconductor layer may comprise silicon, germanium, SiGe, SiC, or a type III-V material such as GaAs, GaN, or InGaN (this list is not exhaustive). Germanium and GaAs are less preferred among these materials due to their brittleness. In a preferred embodiment of the invention, the semiconductor layer is a silicon layer.

[0048] Advantageously, the semiconductor layer 111 includes at least one electronic component 112. This component is manufactured using techniques known in microelectronics. It may be a CMOS transistor, a switch, or a power amplifier (this list is not exhaustive). Furthermore, vias 113 may be provided within the semiconductor layer 111 to allow the electrical connection of various components. These components and vias are formed using conventional microelectronic techniques, which will not be described in detail herein.

[0049] The semiconductor layer 111 is significantly thinner than the stiffening substrate 110. Thus, the semiconductor layer 111 typically has a thickness between 10 nm and 2 µm. Consequently, even if the semiconductor layer material has a greater difference in coefficient of thermal expansion compared to the piezoelectric material than the difference in coefficient of thermal expansion between the stiffening substrate material 110 and the piezoelectric material 10, the semiconductor layer 111 is sufficiently thin not to generate mechanical stress in the piezoelectric layer 10 during heat treatment.

[0050] In addition, compared to a solid sapphire substrate, the composite substrate 11 formed from the stiffening sapphire substrate 110 and the semiconducting layer 111 allows the integration of electronic components on the back side of the piezoelectric layer 10.

[0051] According to an advantageous but not mandatory embodiment, a dielectric layer 114 is arranged at the interface between the semiconducting layer 111 and the piezoelectric layer 10. Such a dielectric layer is generally used to promote the bonding of the piezoelectric layer 10 to the semiconducting layer 111. The dielectric layer can be formed, prior to the bonding of the piezoelectric layer 10 to the semiconducting layer 111, either on one of these layers or on each of them (an oxide-on-oxide bonding being carried out in the latter case).In this case, a charge-trapping layer 115 is made beneath the piezoelectric layer, advantageously interposed between the dielectric layer 114 and the piezoelectric layer 10, or between the semiconductor layer 111 and the dielectric layer 114, in order to trap any electrical charges present that might disrupt the operation of the electronic components arranged in the semiconductor layer 111. This trapping layer 115 may, for example, comprise a layer of polycrystalline or amorphous silicon. However, any other layer (or stack of layers) fulfilling the function of electrical charge trapping may be used.

[0052] There figure 4 schematically illustrates a surface acoustic wave filter formed on substrate 1 of the figure 3 . For this purpose, metallic electrodes 12, 13 were deposited in the form of two interdigitated combs on the free surface of the piezoelectric layer 10.

[0053] According to an illustrated variant of the execution in the figure 5 The substrate, after the formation of electrodes 12 and 13 on the piezoelectric layer 10, can be coated with a dielectric layer 15 (typically silicon dioxide (SiO2)), according to the "overlay" technique mentioned above. The thickness of the dielectric layer 15 is typically on the order of 100 to 10,000 nm.

[0054] In relation to the method of implementation of the figure 4 The dielectric layer 15, which has a coefficient of thermal expansion in the opposite direction to that of the piezoelectric layer 10, allows for improved temperature compensation.

[0055] We will now describe, with reference to figures 6A à 6E A method for manufacturing a substrate for a surface acoustic wave or body acoustic wave device according to a non-limiting embodiment of the invention. The method described below involves bonding and then thinning a donor substrate, but other techniques, such as a "removable substrate" approach as described in document FR 2 816 445, could be used. Such a "removable" substrate is produced before the manufacture of the components and contains a weakening zone or interface allowing the donor substrate to fracture after assembly onto a stiffening substrate.

[0056] With reference to the figure 6A , a donor substrate 116 is provided comprising the semiconductor layer 111 in which electronic components 112 and / or vias 113 are advantageously integrated, according to techniques commonly used in microelectronics.

[0057] With reference to the figure 6B , the donor substrate 116 is glued onto the stiffening substrate 110, so that the semiconducting layer 111 is at the bonding interface.

[0058] With reference to the figure 6C The donor substrate is thinned on the side opposite the semiconductor layer 111 so as to transfer the layer containing layer 111 onto the stiffening substrate 110. This thinning can be mechanical (such as polishing), chemical (etching), or otherwise. If necessary, electronic components and / or vias are then integrated into this layer.

[0059] With reference to the figure 6D , a donor substrate 118 of a piezoelectric material is provided and a weakening zone 119 is formed by implanting atomic species in said substrate, delimiting a piezoelectric layer to be transferred, namely the piezoelectric layer 10 of the final substrate illustrated on the figure 3 The implantation conditions are known in the state of the art, namely a dose of the order of 5 to 15E16 and an energy between 20 and 200 keV.

[0060] With reference to the figure 6E The donor substrate 118 is bonded to the stack formed by the stiffening substrate 110 and the semiconductor layer 111, such that the semiconductor layer 111 and the piezoelectric layer 10 are at the bonding interface. As mentioned above, a dielectric layer (not shown in the diagram) figure 6E ) can be formed beforehand on one or both of these layers to promote adhesion. If necessary, a filler trapping layer (not shown in the figure 6E A trapping layer can be formed between the dielectric layer and the piezoelectric layer. This trapping layer is advantageously formed after implantation in the piezoelectric substrate 118. Under these conditions, a low-temperature process is required. For example, an amorphous silicon layer is deposited on the piezoelectric substrate, or a polycrystalline silicon layer is deposited on a dielectric layer formed on the semiconductor layer 111.

[0061] In the case where it is desired to form a volume acoustic wave device, the bonding can be achieved by means of a metallic layer, said layer then fulfilling the function of an electrode buried in the device.

[0062] Next, the piezoelectric donor substrate 118 is fractured along the embrittlement zone 119 so as to transfer the piezoelectric layer 10 onto the semiconducting layer 111. Thinning of the piezoelectric layer may optionally be implemented to eliminate defects related to implantation.

[0063] In cases where the semiconductor layer does not contain electronic components, the Smart Cut™ process can also be used to transfer the semiconductor layer 111 onto the stiffening substrate 110. This process is well known to those skilled in the art. Specifically, a weakened zone is created in the donor substrate 116 by implanting atomic species, thus defining a transfer layer that includes the layer 111. This implantation generally involves hydrogen and / or helium atoms, and those skilled in the art can determine the dose and implantation energy based on the donor substrate material and the required depth. After bonding the donor substrate to the stiffening substrate 110, the donor substrate is detached along the weakened zone. This detachment can be initiated mechanically, thermally, chemically, or otherwise.

[0064] In the case where it is desired to manufacture a surface acoustic wave device, metallic electrodes in the form of two interdigitated combs are then deposited on the surface of the piezoelectric layer 10.

[0065] If one wishes to manufacture a volume acoustic wave device, an adaptation of the steps described above must be made. Firstly, before the gluing step illustrated on the... figure 6E A first electrode is placed on the free surface of the piezoelectric layer 10, which forms part of the piezoelectric donor substrate. This first electrode is embedded within the final stack. After the transfer of the piezoelectric layer 10 onto the semiconductor layer 111, a second electrode is deposited on the free surface of the piezoelectric layer, opposite the first electrode. Furthermore, to prevent the propagation of acoustic waves in the semiconductor layer 111 and in the stiffening substrate 110, an insulating means is integrated into the semiconductor layer 111. This means could be, for example, a Bragg mirror (as illustrated in the figure). figure 2 ) or a cavity etched into the semiconductor layer 111. REFERENCES

[0066] [1] Hashimoto et al, Recent Development of Temperature Compensated SAW Devices, Ultrasonics Symposium (IUS), Oct. 18-21, 2011, pp. 79-86, 2011 IEEE International FR 2 816 445

Claims

1. Substrate (1) for a surface acoustic wave or bulk acoustic wave device, comprising a support substrate (11) and a piezoelectric layer (10) on said support substrate, characterized in that the support substrate (11) comprises a semiconductor layer (111) on a stiffening substrate (110) having a coefficient of thermal expansion closer to the coefficient of thermal expansion of the material of the piezoelectric layer (10) than that of silicon, the semiconductor layer (111) comprising at least one electronic component (112) and being arranged between the piezoelectric layer (10) and the stiffening substrate (110), said electronic component (112) is selected from: a CMOS transistor, a switch, and a power amplifier.

2. Substrate according to claim 1, characterized in that the stiffening substrate (110) comprises sapphire, glass, and / or spinel, MgAl2O4.

3. Substrate according to either of claims 1 or 2, characterized in that the semiconductor layer (111) is formed from one of the following materials: silicon, germanium, SiGe, SiC, III-V material.

4. Substrate according to any of claims 1 to 3, characterized in that the ratio between the thickness of the piezoelectric layer (10) and the thickness of the stiffening substrate (110) is less than or equal to 0.125.

5. Substrate according to any of claims 1 to 4, characterized in that the thickness of the piezoelectric layer (10) is less than 50 µm, preferably less than 20 µm, even more preferably less than 1 µm, and the thickness of the stiffening substrate (110) is between 400 and 800 µm.

6. Surface acoustic wave device comprising a substrate (1) according to any of claims 1 to 5 and two electrodes (12, 13) formed by two interdigitated metal combs on the surface of the piezoelectric layer (10).

7. Bulk acoustic wave device comprising a substrate (1) according to any of claims 1 to 5 and two electrodes (12, 13) arranged on either side of the piezoelectric layer (10).

8. Method for manufacturing a substrate (1) according to any of claims 1 to 5, characterized in that it comprises: - transferring the semiconductor layer (111) onto the stiffening substrate (110) from a first donor substrate (116), said semiconductor layer (111) comprising said electronic component (112), - transferring the piezoelectric layer onto the semiconductor layer (111) from a second donor substrate (118).

9. Method according to claim 8, wherein at least one of the transferring steps comprises the following substeps: - forming an embrittlement zone in the first or the second donor substrate, respectively, by implantation of atomic species; - bonding the first or the second donor substrate, respectively, to the stiffening substrate or to the semiconductor layer, respectively; - detaching said first or second substrate, respectively, along the embrittlement zone.