A method of mechanical welding
The mechanical welding method employing an oscillating pin and shoulder tool enables efficient, low-temperature welding without preheating, achieving strong and symmetrical welds with reduced energy consumption and avoiding heat treatment issues.
Patent Information
- Application Number
- GB2022002710
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-02-26
- Filing Date
- 2022-02-28
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2042-02-28
AI Technical Summary
Existing mechanical welding methods, such as friction stir welding, face high energy consumption due to the need for preheating and often result in weaker welds at the trailing edge, with potential issues like uncontrolled heat treatment leading to decreased strength properties and grain growth.
A mechanical welding method using a tool with a pin and shoulder, where the pin oscillates between ±2° to ±15° during contact with the workpieces, allowing for visco-plastic flow without heating, using a split or profiled tool with enhanced surface roughness and cooling, significantly reducing energy consumption and avoiding material deformation.
This method achieves a strong, narrow weld with properties matching the joined materials, eliminating heat treatment issues and reducing tool pressure requirements by over 50%, while maintaining material symmetry and avoiding oxidation.
Smart Images

Figure 00000001_0000 
Figure 00000001_0001 
Figure 00000002_0000
Abstract
Description
The object of the invention is a method of mechanical welding applicable particularly for joining metal parts such as sheet metal. A method of friction stir welding is well known, which consists in inducing a relative motion, preferably rotational, of a tool between a pair of materials pressed against each other, in order to plasticise them within the contact zone due to the frictional heat generated and to stir the plasticised materials. When the relative motion stops and the temperature drops, a permanent bonding of the materials takes place. A method of friction bonding process of materials is known from the U.S. Application Description US 4144110, in which heat is generated by friction between these materials and a rotating hard circular member, neither the member nor any part thereof being part of the weld produced. As the place where the materials are bonded is not the same as the place where heat is generated, a protective atmosphere must be used during the welding process to protect the materials from oxidation. A method of friction welding is known from the U.S. patent description US 5460317 B1, in which a one-sidedly rotating high-strength working tool comprising a probe and contact face of suitably selected shapes, is pressed against and moved along the contact line of the materials to be joined, and the material plasticized and stirred in this zone, forms a good quality durable weld without passing to the liquid state. This method does not require a protective atmosphere and the weld is characterised by a favourable fine-grained structure. It is recommended that the material in the contact zone is heated to about 80% of its melting temperature, as it then has very high plasticity and can be deformed under low stress, and just as importantly, the material is then guaranteed to remain in the solid state. Approximately 80% of the heat generated in the friction stir welding process is believed to be generated by the friction between the material and the rotating tool. On the other hand, the primary role of the rotating probe is to properly stir the material. A friction stir welding process is known from the U.S. patent description US 8205785 B2, wherein a pin tool of the friction welding spindle rotates at a first speed in a one direction and a shoulder rim rotates in the opposite direction, with the rotation movement continuing after the spindle is pressed against the material of the workpieces and the direction of rotation of the spindle is changed before the spindle is retracted from the material of the workpieces. Under the trade name Re-stir™ a friction welding process is known, which involves angular reciprocating / reversal motion of the working tool, whereby the change of the direction may occur during or after one or more revolutions. The main objective of this solution is a better stirring of the material. The effectiveness of the Re-stir™ method has been experimentally confirmed for repeated several revolutions of the working tool in one direction and several revolutions of the working tool in the reverse direction. The solution allows for an improvement in the quality of the material joint due to obtaining better symmetry of the weld, which is worse at the trailing edge when the working tool rotates only in one direction. However, this does not change the fact that, from an energy point of view, an angular reciprocating / reversal motion of the working tool is a much less effective way of frictional heating, and thus of welding the material, than that induced by a unidirectional rotation motion at constant speed. The known solutions are characterised by high energy consumption related, among other things, to the frequent need for preheating of the material; in addition, in solutions using unidirectional rotation motion of the welding tool, a weaker weld is obtained at the trailing edge of the tool. A method of mechanical welding using a mechanical welding tool, which includes a shoulder and a spindle with a pin as its working part, wherein the pin of the spindle is inserted into the area of a joint between workpieces to be joined and, by plasticizing the material of the workpieces, a weld is made and the tool is retracted from the material of the workpieces, according to the invention is characterized in that, when the pin of the spindle is in contact with the material of the workpieces, an oscillating motion of the pin of the spindle is carried out, with an angle of oscillating rotation ranging from ±2° to ±15°. Advantageously, an oscillation frequency of not less than 1 Hz is used. Further advantages are obtained if a split tool is used that allows a relative motion of the pin of the spindle and a part of the shoulder. Further advantages are obtained if, together with the pin of the spindle, a part of the rim of the shoulder on the side of the pin of the spindle is put into oscillating motion. Further advantages are obtained if a tool is used where the pin of the spindle has, at least on part of its surface, a roughness higher than the surface roughness of the workpieces. Further advantages are obtained if a tool is used where the pin of the spindle is at least partially profiled. Further advantages are obtained if while the pin of the spindle is in contact with the material of the workpieces, this material is cooled. Further advantages are obtained if the pin of the spindle is cooled while the tool is running. Further advantages are obtained if the cooling is carried out with a liquid stream, preferably having a room temperature. Further advantages are obtained if the cooling is carried out with a gas stream, preferably air. Further advantages are obtained if the oscillating motion is induced by means of a crank system. By using the method according to the invention, it is possible to carry out mechanical welding without heating the contact zone of the materials to be joined, in particular without using the friction heat, whereby possible heating is not an obstacle to its implementation. Moreover, in order to obtain a permanent connection, it is not required to stir the materials to be joined, whereby possible stirring does not constitute an obstacle to the implementation of the method. The invention makes it possible to activate a visco-plastic flow mechanism in the contact zone without heating the material and to form a strong metallurgical joint without achieving a large deformation. The solution makes it possible to significantly reduce the energy consumption of the welding process. In addition, the weld obtained by the method according to the invention is relatively narrow and has the appearance of a fine zigzag tailor's stitch and strength properties similar to those of the materials being joined, while when joining identical materials there is no heterogeneity of the materials on both sides of the weld. The dominance of visco-flow of the material significantly reduces the energy of deformation compared to other deformation mechanisms, which translates into the ability to apply less tool pressures even by more than 50%. Due to the fact that mechanical welding according to the invention is a low-temperature process, the negative effect of uncontrolled heat treatment of the materials inside and around the weld is eliminated, in particular the supersaturation of alloys, which poses serious problems in friction stir welding, as it leads to a decrease in the strength properties of the weld, as well as grain growth. The oscillating motion of the pin of the spindle, with an angle of oscillation ranging from ± 2° to ± 15°, allows the material of the workpieces adjacent to the pin of the spindle, together with this pin, to move against the remaining part of the material. The angle of oscillating rotations of the pin of the spindle > ± 2°, ensures that the sheared layer of material transits from elastic state to plastic state. On the other hand, the oscillating rotation angle of > ± 15° does not significantly improve the plastification of the sheared material layer, while it causes an increase in the energy consumption of the process, excessive tool wear and unnecessary heating of the material. Adequate adhesion of the material to the pin of the spindle is achieved by the roughness of the pin of the spindle being greater than the surface roughness of the workpieces or by using a tool with a profiled pin of the spindle, for example made by special cuts or bulges on its surface. The mechanical welding method according to the invention in the example of implementation is explained in more detail in the drawings, where Fig. 1 shows an illustrative realization of the method for making the weld of an overlap joint, Fig. 2 -detail A of fig. 1 in magnification, showing the pin of the tool spindle used in the first embodiment, Fig. 3 - detail A of fig. 1 in magnification, showing the pin of the tool spindle used in the second embodiment. In the first embodiment, the method of mechanical welding according to the invention is carried out using a split tool 1 for mechanical welding, which includes a shoulder 2 and a spindle 3 loosely mounted therein with a cylindrical pin 4 for plunging into the material of workpieces 5. The tool 1 used has a surface of the pin 4 of the spindle 3 with a roughness higher than the roughness of the surface of the workpieces 5. A lap joint is made. The workpieces 5 are sheets of hard, high-strength aluminium alloy with zinc and magnesium as the main alloying additives, grade 7075. The workpieces 5 are clamped on a support plate. Then the pin 4 of the spindle 3 is introduced in an oscillating motion with an oscillating rotation angle of ± 2° and a frequency of not less than 1 Hz, after which the pin 4 of the spindle 3 is plunged into the material of the joined elements 5 and moved at a constant speed along the assumed weld line 6, continuing the oscillating motion of the spindle 3. Once the pin 4 of the spindle 3 has been plunged into the material of the workpieces 5, the cooling of this material in the contact zone and the cooling of the working tool 1 by means of a stream of air of a room temperature starts while the weld 6 is being made. The oscillating motion of the spindle 3 with the pin 4 is induced by a crank system. During the welding process, the shoulder 2, which has a smooth rim surface on the side of the pin 4 of the spindle 3, is not put into oscillating motion. The cyclic change of the deformation path of the pin 4 of the spindle 3 plunged in the material of the workpieces 5 leads to the generation of a strongly above-equilibrium concentration of point defects, which in aluminium is 10"7 for the interstitial atoms, so that, despite the low welding temperature, there is an increase of several orders of magnitude in the diffusion coefficient in the material compared to the equilibrium state, allowing its viscous flow. Furthermore, the cyclic change of the deformation path, from the very beginning of its activation in the material, allows for the initiation and domination, while making the weld 6, of the mechanism of localized plastic flow in the shear bands. The shear bands, by displacing in relation to each other the micro-layers of the material of the workpieces 5 which are in contact with each other, reveal “clean”, non-oxidized surfaces capable of metallurgical joining. Finally, the pin 4 of the spindle 3 is retracted from the material of the workpieces 5 to be joined. When the pin 4 is retracted and the material is cooled, a relatively narrow weld 6 with the appearance of a fine tailor's stitch and with strength properties similar to those of the material of the workpieces 5 is obtained along the entire length of the joint line, without heterogeneity of the materials on both sides of the weld 6. In the second embodiment, the method of mechanical welding according to the invention is carried out in order to make a joint of workpieces 5 which are sheets of low-strength aluminium of grade 1050. A split tool 1 is used with a profiled surface of the pin of the spindle 3 containing wedge-shaped cuts with a width and depth of 0.5 mm. The spindle 3 together with its pin 4 and a part of the rim of the shoulder 2 on the side of pin 4 of the spindle 3 are put into an oscillating motion with an oscillating rotation angle of 15°. The cooling of the material of the joined workpieces 5, in the contact zone, and the cooling of the tool 1 by means of a stream of cold liquid starts while the weld 6 is being made. During the welding process, the outer part of the shoulder 2 is not put into the oscillating motion. In the remainder of the embodiment, the method is realized as in the first embodiment. List of designation 1 - tool 2 - shoulder 3 - spindle 4 - pin 5 - workpiece 6 - weld
Claims
1. A method of mechanical welding using a mechanical welding tool which includes a shoulder and a spindle with a pin, the method comprising:inserting the pin of the spindle into the area of a joint between workpieces to be joined and,when the pin (4) of the spindle (3) is in contact with the material of the workpieces (5), carrying out an oscillating motion of the pin (4) of the spindle (4) with an angle of oscillating rotation ranging from ±2° to ±15°, thereby plasticizing the material of the workpieces such that a weld is made, andretracting the tool from the material of the workpieces.
2. The method as claimed in claim 1, wherein the oscillation frequency is not less than 1 Hz.
3. The method as claimed in claim 1 or 2, wherein the tool comprises a split tool (1) that allows a relative motion of the pin (4) of the spindle (3) and a part of the shoulder (2).
4. The method as claimed in claim 3, characterised in that a part of the rim of the shoulder (2) on the side of the pin (4) of the spindle (3), together with the pin (4) of the spindle (3), is put into oscillating motion.
5. The method as claimed in one of claims from 1 to 4, characterised in that the pin (4) of the spindle (3) has, at least on part of its surface, a roughness higher than the surface roughness of the workpieces (5).
6. The method as claimed in one of claims from 1 to 5, characterised in that the pin (4) of the spindle (3) is at least partially profiled.
7. The method as claimed in one of claims from 1 to 7, characterised in that the material of the workpieces (5) is cooled while the pin (4) of the spindle (3) is in contact with the material of the workpieces (5).
8. The method as claimed in one of claims from 1 to 6, characterised in that the pin(4) of the spindle (3) is cooled while the tool (1) is running.
9. The method as claimed in claim 7 or 8, characterised in that, the cooling is carried out with a liquid stream, preferably having a room temperature.
10. The method as claimed in claim 7 or 8, characterised in that, the cooling is carried out with a gas stream, preferably air.
11. The method as claimed in one of claims from 1 to 10, characterised in that, the oscillating motion is induced by means of a crank system.27 02 23
Citation Information
Patent Citations
Friction spot sealing of a defect area in a workpiece
US20180222000A1
Improvements relating to friction welding
WO1996038256A1