PREPARATION OF GRAPHITIC-CARBON-NITRIDE (g-C3N4) / RUST / PVDF NANOCOMPOSITE FOAM AND THEIR APPLICATIONS THEREOF FOR OIL / WATER SEPARATION

IN595811BActive Publication Date: 2026-07-17NAT INST OF TECH CALICUT AN INDIAN INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202541059302
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-06-20
Publication Date
2026-07-17
Estimated Expiration
2045-06-20

AI Technical Summary

Technical Problem

Existing methods for oil/water separation in wastewater treatment, such as skimming and chemical dispersants, are costly, complex, and pose environmental threats, while traditional adsorbents are inefficient for comprehensive remediation of oily contaminants and water-soluble pollutants.

Method used

A graphitic-carbon-nitride (g-C3N4)/Rust/PVDF nanocomposite foam is prepared via a solvent-free thermal decomposition method, exhibiting high hydrophobicity and oleophilicity for efficient oil/water separation.

Benefits of technology

The g-C3N4/Rust/PVDF foam achieves effective, cost-effective, and scalable oil/water separation with high absorption capacity and environmental friendliness, suitable for industrial applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

ABSTRACT PREPARATION OF GRAPHITIC-CARBON-NITRIDE (g-C3N4) / RUST / PVDF NANOCOMPOSITE FOAM AND THEIR APPLICATIONS THEREOF FOR OIL / WATER SEPARATION The present invention provides a method for the preparation of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam comprising the following steps: (a) transferring a melamine precursor to a receiver and calcinating said precursor, (b) cooling down the product to ambient temperature, collecting the same, and grinding it to a fine powder, (c) sieving the rust so obtained from step b) to remove debris, washing the same suitably and drying it, (d) subjecting the product obtained from step (c) to further calcination to obtain α-Fe2O3, (e) mixing calcinated rust, g-C3N4, PVDF powder, and table salt and heating the mixture, (f) subjecting the heated mixture to hot water for a prolonged period till obtaining template-free graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam. A graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam with enhanced traits is also disclosed. FIG. 3
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTIONThe present invention relates to a novel method for the preparation of graphitic-carbon-nitride (g-C3N4) / Rust / Poly (vinylidene fluoride) nanocomposite foam. Hereinafter Poly (vinylidene fluoride) is referred to as PVDF for the sake of brevity.More particularly, the present invention relates to the preparation of graphitic-carbon-nitride (hereinafter referred to as g-C3N4, at places for the sake of brevity) / Rust / PVDF nanocomposite foam with enhanced traits which can be effectively applied for controlling water pollution. It is a cost-effective and environmental and user-friendly tool for controlling water pollution.TECHNICAL BACKGROUND OF THE INVENTIONIt is known that in the field of wastewater treatment, traditional techniques such as in situ burning, bioremediation, sorption, skimming, and chemical dispersants are employed for the remediation of oil spills. Among these, skimming is the most widely utilized method for oil / water separation. However, its practical application is hindered by limitations such as high operational costs, complex procedures, extended processing times, and limited efficiency, which hinder their scalability for industrial applications. Similarly, chemical dispersants are the second most commonly adopted approach; yet, the combined toxicity of oil-dispersant mixtures poses severe threats to marine ecosystems. These challenges underscore the need for the development of cost-effective and highly efficient absorbent materials for oil / water separation. Moreover, the complex composition of wastewater, comprising not only oily contaminants but also water-soluble organic pollutants, necessitates further treatment to achieve comprehensive remediation.To address these challenges, there is an urgent need to develop an innovative, environmentally friendly, cost-effective, and user-friendly material for its effective application for water pollution control. In that view of the matter, the present invention provides a g-C3N4 / Rust / PVDF nanocomposite foam, which as an adsorbent, is suitable for industrial oil / water separation applications. The present invention provides a method for preparing such a nanocomposite foam by a simple thermal decomposition technique, that being a solvent-free methodology. The g-C3N4 / Rust / PVDF nanocomposite foam obtained by the method is found to be effective in industrial oil / water separation applications for wastewater pollution control.OBJECTIVES OF THE INVENTIONThe principal objective of the present invention is to provide a method for the preparation of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam which is an environmentally friendly, cost-effective, and user-friendly material for its effective application for oily wastewater treatment and water pollution control.Another important objective of the present invention is to provide a graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam, which as an adsorbent is suitable for industrial oil / water separation applications ensuring water pollution control.It is yet another objective of the present invention to improve the oil / water separation efficiencies of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam as an adsorbent, through optimization. It is a further objective of the present invention to provide a method for the preparation of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam, which has enhanced traits and the methodology involves a simple thermal decomposition technique, that being a solvent-free methodology.How the foregoing objects are achieved will be clear from the following description. In this context, it is clarified that the description provided is non-limiting and is only by way of explanation.SUMMARY OF THE INVENTIONAccordingly, the present invention provides a method for the preparation of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam comprising the following steps: (a) transferring a melamine precursor to a receiver and calcinating said precursor, (b) cooling down the product to ambient temperature, collecting the same, and grinding it to a fine powder,(c) sieving the rust so obtained from step (b) to remove debris, washing the same suitably and drying it,(d) subjecting the product obtained from step (c) to further calcination to obtain α-Fe2O3,(e) mixing calcinated rust, g-C3N4, PVDF powder, and table salt and heating the mixture,(f) subjecting the heated mixture to hot water for a prolonged period till obtaining template-free graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam.In accordance with preferred embodiments: Step a) involves at first, transferring the melamine precursor to a crucible and calcinating at 550 °C for 4 hours in a muffle furnace at the rate of 2 °C / min.Step b) involves cooling down the product to ambient temperature, collecting the same, and grinding it into fine powder using agate mortar.Step c) involves washing the sieved product twice with deionised (DI) water by ultrasonication for 15 minutes and with ethanol for another 15 minutes and drying in an oven at 80 °C.Step d) involves calcinating the product at 600 °C to obtain α-Fe2O3 and steps e) and f) involves mixing calcinated rust, g-C3N4, PVDF powder and table salt in a mass ratio of x: 0.5: 1: 7, thoroughly grinding the same and pouring into a crucible followed by heating at 250 °C for 3hours in a muffle furnace and putting the obtained material into 80 °C hot water, updating every 2 hours for a continuous period of 24 hours, thereby obtaining graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam.The present invention also provides a graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam with enhanced traits prepared by the method as described hereinbefore.BRIEF DESCRIPTION OF THE ACCOMPANYING DRAWINGSThe nature and scope of the present invention will be better understood from the accompanying drawing, which are by way of illustration of a preferred embodiment and not by way of any sort of limitation. In the accompanying drawing: -Figure 1 is a schematic representation of the preparation of g-C3N4 according to the present invention. Figure 2 is a schematic representation of the cleaning of rust according to the present invention.Figure 3 is a schematic diagram of the synthesis of g-C3N4 / Rust / PVDF foam.Figure 4 represents photographs of (a) pure PVDF foam, (b) g-C3N4-PVDF foam, (c) rust-PVDF foam, and (d) g-C3N4 / Rust-PVDF foam.Figure 5 represents photographs (a) water droplet and engine oil (red) droplet on the surface of g-C3N4 / rust- PVDF foam, (b) water contact angle of g-C3N4 / rust- PVDF foam, (c) and (d) photographs of the g-C3N4 / rust- PVDF foam immersed in water while (e), (f) and (g) represent sequential photographs demonstrating the oil removal process from water using the g-C3N4 / rust- PVDF foam.DETAILED DESCRIPTION OF THE INVENTIONHaving described the main features of the invention above, a more detailed and non-limiting description of a preferred embodiment will be given in the following paragraphs with reference to the accompanying drawings.The present invention provides a novel g-C3N4 / Rust / PVDF nanocomposite foam for oil / water separation with a motive to effectively control water pollution. It involves cost-effective synthesis, high-yield production, and effective separation of oil and organic solvents from water. The g-C3N4 / Rust / PVDF nanocomposite foam is prepared by solvent-free method. The prepared g-C3N4 / Rust / PVDF foam shows a water contact angle of around 123.9° (hydrophobic) and an oleophilic nature. Hence, the preparation of g-C3N4 / Rust / PVDF foam presents an effective solution for oily wastewater treatment. The present was utilized abundant and inexpensive raw materials. Overall, the g-C3N4 / Rust / PVDF foam is a promising material for oily wastewater treatment, with several advantages such as efficient oil / water separation, reusability, low-energy consumption, scalability, and cost-effectiveness.The developed adsorbent material does not require any expensive chemicals or equipment for the preparation, making it an affordable solution for large-scale applications.Advantages: cost-effective synthesis, high-yield production, reusability, scalability, environmentally friendly, and effective separation of oil and organic solvents from water.The working principle of oil / water separation foam is based on the selective wettability and absorption properties of the foam material, which allows it to preferentially absorb oil while repelling water. This is achieved through the foam surface energy characteristics and porous 3D structure.So, briefly, the present invention teaches a simple, low-cost, environmentally friendly, highly hydrophobic, and oleophilic g-C3N4 / Rust / PVDF nanocomposite foam for oil / water separation. The g-C3N4 is synthesized by thermal decomposition method and the g-C3N4 / Rust / PVDF nanocomposite foam is prepared by the solvent-free method. Compared with pure rust nanocomposite foam, the g-C3N4 / rust-PVDF nanocomposite foam shows a water contact angle of around 123.9º (hydrophobic) and an oleophilic nature. Then the g-C3N4 / Rust-based PVDF foam is a good choice for oil / water separation. Hence, the developed g-C3N4 / Rust / PVDF nanocomposite foam absorbent has excellent potential in oil / water separation applications.Now the present invention is described in greater detail.Preparation of graphitic-carbon-nitride (g-C3N4): The g-C3N4 is prepared via a simple thermal decomposition method. Referring to figure 1 at first, the melamine precursor is transferred to a crucible and calcinated at 550 °C for 4 hours in a muffle furnace at the rate of 2 °C / min. After cooling down to ambient temperature, the product is collected and ground into a fine powder (using agate mortar) as shown in figure 1.Cleaning of Rust: Referring to figure 2, the collected rust is sieved to remove debris and washed twice with deionised (DI) water by ultrasonication for 15 minutes and with ethanol for another 15 minutes, and dried in an oven at 80 °C. Then the product is calcinated at 600 °C to obtain α-Fe2O3 as shown in Figure 2.Fabrication of Porous g-C3N4 / Rust / PVDF Foam: This entire process is now described with reference to figure 3. Calcinated rust, g-C3N4, PVDF powder, and table salt in a mass ratio of x: 0.5: 1: 7 are mixed, thoroughly ground, and poured into a crucible, heated at 250 °C for 3 h in a muffle furnace. Then the obtained sample is put into 80 °Chot water, that is updated every 2 hours for a continuous 24 hours, to obtain a template-free porous foam.The graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam is subjected to various experiments results whereof are discussed below: The absorption capacity of oils and solvents like olive oil, engine oil, pump oil, methanol, ethanol, acetone, toluene, etc., are used for oil / water separation studies. Maximum absorption capacity is observed for engine oil, ~70 times the original weight of g-C3N4 / Rust / PVDF -composite foam.The wettability of the composite foam is evaluated by measuring the contact angles of water and oil using 6 μL droplets deposited on g-C3N4 / rust-PVDF nanocomposite foam surface. Upon immersion in water, a silver-colored appearance was observed on the g-C3N4 / rust-PVDF nanocomposite foam surface, indicating a highly hydrophobic nature. This effect arises from the presence of a trapped air layer between the foam surface and water. Furthermore, when the g-C3N4 / rust-PVDF nanocomposite foam is placed on an oil film floating on water, it rapidly absorbed the oil, demonstrating its strong oleophilic behavior.Absorption StudyReferring to figure 4, water and red-coloured engine oil droplets are dropped onto the foam surface, oil is immediately absorbed into the foam; water droplet maintained a spherical shape on the surface. These results indicate that foam is oleophilic and hydrophobic in nature.Referring to figure 5, upon immersion in water, a silver-colored appearance is observed on the g-C3N4 / rust-PVDF nanocomposite foam surface (Fig. 5 (c-d)), indicating a highly hydrophobic nature. This effect arises from the presence of a trapped air layer between the foam surface and water.Absorption Capacity of g-C3N4 / RUST / PVDF nanocomposite foamThe absorption capacity of the g-C3N4 / RUST / PVDF nanocomposite foam are evaluated using the manual squeezing method. The manual squeezing method involves simply immersing and squeezing the foam in the oil or organic solvent to collect the absorbed liquid, making it an eco-friendly and time-saving alternative to heating methods or burn-off techniques.Absorption Capacity=(W2-w1) / W1where W1 and W2 denote the weights of the g-C3N4 / RUST / PVDF nanocomposite foam before and after the absorption of oils or organic solvents, respectively.The results are provided in the Table 1 below:Table 1From the foregoing description including the experimental results, it would be clear that the present invention provides the following technical advantages:a) It is a simple, low-cost, environmentally friendly, highly hydrophobic, and super oleophilic g-C3N4 / Rust / PVDF nanocomposite foam. Hence it is suitable for oily wastewater treatment. b) The g-C3N4 / Rust / PVDF composite foam shows excellent absorption capacity, and it can separate different oils and solvents from water. c) Hence, the developed g-C3N4 / Rust / PVDF -composite foam-absorbent has excellent potential in oil / water separation applications.d) The g-C3N4 / rust-PVDF nanocomposite foam shows a water contact angle of around 123.9º (hydrophobic) and an oleophilic nature. e) The g-C3N4 / Rust / PVDF foam is an inexpensive adsorber for oily wastewater treatment.f) g-C3N4 / Rust / PVDF foam has a porous structure that enables it to absorb oil and organic solvents from water efficiently. This high absorption capacity ensures the effective removal of contaminants from the wastewater.g) The precursors required for synthesizing g-C3N4 / Rust / PVDF foams are low-cost and easily available in bulk quantities. h) Utilizing rust for oily wastewater treatment is an efficient and economical waste management [waste to wealth] approach. i) The synthesizing process of g-C3N4 / Rust / PVDF foam is simple and ensures good reproducibility. It involves a simple thermal decomposition method which is a solvent-free method.j) The synthesis process of g-C3N4 / Rust / PVDF foam does not require any sophisticated equipment.k) Oily wastewater treatment using the hydrophobic g-C3N4 / Rust / PVDF foam absorbent material is technically a good economical waste management approach for the oily wastewater treatment industry. From the foregoing it would be clear that all objectives of the present invention have been met.The present invention has been described with reference to some drawings and a preferred embodiment purely for the sake of understanding and not by way of any limitation and the present invention includes all legitimate developments within the scope of what has been described herein before and claimed in the appended claims.

Claims

1. A method for preparation of graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam comprising the following steps: (a) transferring a melamine precursor to a receiver and calcinating said precursor, (b) cooling down the product to ambient temperature, collecting the same, and grinding it to a fine powder, (c) sieving the rust so obtained from step (b) to remove debris, washing the same suitably and drying it, (d) subjecting the product obtained from step (c) to further calcination to obtain α-Fe2O3, (e) mixing calcinated rust, g-C3N4, PVDF powder, and table salt and heating the mixture, (f) subjecting the heated mixture to hot water for a prolonged period till obtaining template-free graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam.

2. The method as claimed in claim 1, wherein step (a) involves at first, transferring the melamine precursor to a crucible and calcinating at 550 °C for 4 hours in a muffle furnace at the rate of 2 °C / min.

3. The method as claimed in claim 1, wherein step b) involves cooling down the product to ambient temperature, collecting the same, and grinding it into fine powder using agate mortar.

4. The method as claimed in claim 1, wherein step c) involves washing the sieved product twice with deionised (DI) water by ultrasonication for 15 minutes and with ethanol for another 15 minutes and drying in an oven at 80 °C.

5. The method as claimed in claim 1, wherein step d) involves calcinating the product at 600 °C to obtain α-Fe2O3 and steps e) and f) involves mixing calcinated rust, g-C3N4, PVDF powder, and table salt in a mass ratio of x: 0.5: 1: 7, thoroughly grinding the same and pouring into a crucible followed by heating at 250 °C for 3hours in a muffle furnace and putting the obtained material into 80 °C hot water, updating every 2 hours for a continuous period of 24 hours, thereby obtaining graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam.

6. A graphitic-carbon-nitride (g-C3N4) / Rust / PVDF nanocomposite foam prepared by any one of the preceding claims.