A low-pressure process for the synthesis of Pt(PF3)4 using soluble intermediates and storage of the resulting Pt(PF3)4
The synthesis of Pt(PF3)4 at low pressures using anhydrous solvents and specific metal powders addresses scalability and purity issues, enabling high-yield production for industrial applications in film-forming compositions.
Patent Information
- Application Number
- JP2024532230
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-09
- Filing Date
- 2022-12-07
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-12-07
AI Technical Summary
Existing methods for synthesizing Pt(PF3)4 are limited by low yields, scalability issues, and the lack of suitable precursors for industrial applications due to high-pressure requirements and impurities, making it difficult to produce high-purity Pt(PF3)4 for use in film-forming compositions.
A method involving the reaction of platinum compounds with PF3 in anhydrous solvents at low pressures using copper, zinc, or aluminum powders, followed by purification and storage in metal containers with passivated or electropolished surfaces to achieve high yields and purity.
Enables the scalable production of high-purity Pt(PF3)4, suitable for industrial use in film-forming compositions, by avoiding high-pressure equipment and maintaining purity during synthesis and storage.
Smart Images

Figure 2024543192000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of priority under 35 U.S.C. §119(a) and (b) to U.S. patent application Ser. No. 17 / 546,169, filed December 9, 2021, the entire contents of which are incorporated herein by reference.
[0002] The present invention relates to the synthesis and storage of Pt(PF3)4, which is used as a precursor for film-forming compositions. Pt(PF3)4 is a compound selected from the group consisting of Pt(Hal)2 (Hal=F, Cl, Br or I) and Pt(Hal)2(PF3). x (Hal = F, Cl, Br or I; x = 1, 2), metal powder and PF3 at low pressure in an anhydrous solvent capable of dissolving the reaction intermediate Pt(Hal)2(PF3), where Pt(Hal)2(PF3) x can be formed from Pt(Hal)2 and PF3. The resulting Pt(PF3)4 is then stored at room temperature under air- and moisture-free conditions in devices and ampoules made of metal, such as stainless steel, and preferably having passivated or electropolished inner surfaces. [Background technology]
[0003] Chemical vapor deposition (CVD) and atomic layer deposition (ALD) methods have attracted great interest in the fabrication of catalysts and batteries on an industrial scale. Precursors suitable for high-throughput industrial processes should ideally have high vapor pressure at room temperature, ensuring maximum application in the shortest time and at temperatures that do not compromise the stability of the precursor. Platinum is widely used as a catalyst, and a wide variety of materials containing platinum on a support are now available. Nevertheless, due to the lack of suitable platinum precursors, processes utilizing the deposition of platinum from the gas phase are rare.
[0004] For example, platinum hexafluoride (PtF6, CAS number 13693-05-5), which is solid at room temperature but volatile at room temperature, is rarely applied as a deposition precursor due to its very strong oxidizing and correspondingly strong etching properties. (MeCp)PtMe3 (CAS number 94442-22-5), widely cited for deposition processes, has a vapor pressure of 1 Torr at 69 °C but begins to decompose slowly at 50 °C (Journal of Vacuum Science & Technology, B: Microelectronics and Nanometer Structures (1990), 8 (6), 1826-9), which prevents the use of this compound in high-throughput processes.
[0005] The complex Pt(PF3)4 (CAS number 19529-53-4) is a volatile liquid at room temperature and has a vapor pressure of 36 Torr at room temperature (RD Sanner et al., Report (1989), (UCRL-53937; Order No. DE90000902)), making it a nearly ideal potential precursor for Pt deposition from the gas phase. However, this compound has very limited commercial availability. The reason for the lack of scalability may be the technical difficulties associated with the synthesis of Pt(PF3)4, a nearly ideal potential precursor for Pt deposition from the gas phase. However, this compound has very limited commercial availability (only one supplier in Japan [Japan Advanced Chemicals in grams]) and no suitable ALD process using this chemical has been reported so far. The reason for the lack of scalability may be the technical difficulties associated with the synthesis of Pt(PF3)4 in grams, which may be even more difficult in a manner that can be industrially scaled up with acceptable yields and realistic operating conditions.
[0006] The original synthesis of Pt(PF3)4, in grams and with a yield of 70-80%, was carried out by reaction (1) at 100-150 atm. PF3 and 100°C, applying "fine and oxide-free copper powder" (Angew. Chem. Int. Ed. 1965, 4, 521). The synthesis process is described in a single sentence in the literature and in a later reference that employs the same method, without any details regarding the reaction and the equipment. The reaction requires the application of PF3 gas under high pressure to a mixture of two solids (PtCl2 and Cu powder), and is hardly scalable even for a skilled chemist. PtCl2 + 2Cu + PF3 (excess amount) → Pt(PF3)4 + 2CuCl (1)
[0007] It is noteworthy that the reaction of PtCl2 with PF3 (2) at 60-80 °C and undisclosed pressure gives Pt(PF3)4 in only 1% yield (Inorg. Nucl. Chem. Letters, Vol. 4, pp. 275-278, 1968). Such low yields make this approach impossible to implement for industrial applications. PtCl2 + PF3 (excess) → Pt(PF3)4 + other products (2)
[0008] Flow reactions (3) from the same starting compounds under undisclosed pressures produced only donor-acceptor adducts (Inorg. Nucl. Chem. Letters, Vol. 4, pp. 275-278, 1968). 3PtCl2 + PF3 (excess amount) → PtCl2(PF3)2 + [PtCl2(PF3)]2 (3)
[0009] The compounds PtCl2(PF3)2 and [PtCl2(PF3)]2 were synthesized from solid PtCl2 and PF3 gas (J. Chatt, AA William, J. Chem. Soc. [London] 1951, 3061). According to a sentence on page 200 of Zeitschrift fur Anorganische und Allgemeine Chemie, Band 364, 1969, p192-208, the solid compound may react with PF3 under undisclosed "higher" pressure to form Pt(PF3)4. This "higher pressure" may be assumed to be 40-150 atm, since this is the range reported for the synthesis of Pt(PF3)4 in Zeitschrift fur Anorganische und Allgemeine Chemie, Band 364, 1969, p192-208. The compound PtCl2(PF3)2 is soluble in the polar solvent CDCl3, and its NMR was reported by J. Chem. Res., Syn., 1981, 2, 38. According to J. Chem. Soc. [London] 1951, 3061, the solubility of PtCl2(PF3)2 in benzene is reported to be "low", with molar concentrations ranging from 0.005 to 0.01 M, and the melting point of PtCl2(PF3)2 is 118.3 °C. The FTIR spectrum of PtCl2(PF3)2 is disclosed in the Journal of Chemical Research, Synopses (1981), (2), 37.
[0010] Alternatively, the preparation of Pt(PF3)4 has been achieved in gram quantities in a difficult to obtain rotary autoclave by reaction (4) under a PF3 atmosphere of 40 atm in 95% yield (Zeitschrift fur Anorganische und Allgemeine Chemie. Band 364. 1969, 192-208). PtCl4+4Cu+4PF3→Pt(PF3)4+4CuCl(4)
[0011] PtCl4+6PF3→Pt(PF3)4+2PF3Cl2(5) It should be noted that reaction (5) without copper produces PF3Cl2, but the purification of Pt(PF3)4 is complicated due to the comparable volatility (Zeitschrift fur Anorganische und Allgemeine Chemie.Band 364.1969,192-208). The addition of copper reduces the amount of PF3Cl2, suggesting that reactions (4) and (5) may result in Pt(PF3)4 containing impurities that do not meet the quality standards for CVD and ALD precursors. Of note, reaction (4) also requires mixing two solids and contacting them with PF3 gas, which adds to the scalability problems mentioned above. The reaction of PtCl4 with excess PF3 makes scalability even more impractical.
[0012] Russian Patent No. 2478576C2 discloses a two-step process under 2-6.3 MPa (19.7-62.2 atm) PF3 (6a and 6b) atmosphere, in which CuO is reduced in the same autoclave, and then K2PtCl6 and PF3 are introduced. CuO+H2→Cu+H2O(6a) K2PtCl6 + 4Cu + PF3 (excess amount) → Pt(PF3)4 + 4CuCl + 2KCl (6b)
[0013] Russian Patent No. 2201463С1, US Patent No. 7044995B2, Terekhov et al. (Terekhov et al., International Symposium on Recycling of Metals and Engineered Materials, Proceedings, 4th, October 22-25, 2000, pp. 487-491), and Kovtun et al. (Publications of the Australasian Institute of Mining and Metallurgy (2002), 2 / 2002, 367-372) disclose the extraction of platinum from ores by interaction of the "PGM matte" or "feedstock" with PF3 gas, resulting in the formation of volatile Pt(PF3)4. The feedstock was assumed to contain Pt metal and to interact with PF3 according to (7d). However, as first reported in 1891, Pt and PF3 gave the platinum compound F5PPt (H. Moissan, Bull. Soc. Chim. France 5, 454 (1891)), which was thought to be similar to (PCl3)PtCl2. 3Pt+4HNO3+18HCl→3H2PtCl6+4NO+8H2O(7a) H2PtCl6+2NH3→(NH4)2PtCl6(7b) (NH4)2PtCl6+H2=2NH4Cl+4HCl+Pt (under ultrasound irradiation) (7c) Pt+PF3(excess amount) → Pt(PF3)4(7d)
[0014] In addition, according to Chem. Ber. 101, 138-142 (1968), Pt metal does not react with PF3 under any conditions. US Patent No. 7,044,995 B2 discloses that finely dispersed Pt metal (platinum black, particle size <20 μm) does not react with PF3, and only "activated" Pt metal obtained by applying the multi-step procedure (7a-7c) and reduction with hydrogen under ultrasonic irradiation in step (7c) may react with PF3.
[0015] For reactions initiated from PtCl2, the solvent effect may be negative because, according to Zhurnal Neorganicheskoi Khimii (1970), 15(9), 2445-8, the reaction of these reagents in organic solvents gave various products but not PtCl2I2, in contrast to the solvent-free reaction of PtCl2+I2=PtCl2I2. Several classes of solvents react with PF3, PtCl2, and reduced Pt species and therefore cannot be used for the synthesis of Pt(PF3)4. These classes of solvents include primary amines, which react with PF3 to give RNHPF2, (RNH)2PF2H, and (RNH)2PF (see J. Chem. Soc. A (1970), (11), 1935-8). Tertiary amines, e.g., NMe3, NEt3, form adducts with PF3 (see Inorganic Chemistry (1963), 2, 384-8). Alcohols and PF3 form organic phosphites (see Transactions of the Illinois State Academy of Science (1936), 29(No.2), 89-91). The general pattern of reactivity of P(Hal)3 (Hal=Cl, Br) towards alcohols has been widely reported. Dienes, olefins, unsaturated aldehydes, and ketones react with PF3 to form adducts, as shown for PCl3 and PBr3 (see Uspekhi Khimii (1968), 37(5), 745-77). Acetone reacts with PF3 and Pt(II) compounds (see Zhurnal Obshchei Khimii (1975), 45(3), 512-18; Inorganica Chimica Acta (1997), 264(1-2), 297-303).Halocarbons can react with Pt compounds under reaction conditions via oxidative addition, as shown in selected examples in [Organometallics (2019), 38(10), 2273; Organometallics 2009, 28, 1358-1368; and Organometallics (1987), 6(12), 2548], where oxidative addition of alkyl and aryl halides to platinum complexes is a widely reported reaction.
[0016] In conclusion, existing synthetic approaches to Pt(PF3)4 are highly dependent on the reaction conditions, while changes in conditions can significantly reduce the yield of Pt(PF3)4 or lead to different products, indicating a lack of process robustness, and no synthetic process has been reported to date that requires a PF3 pressure lower than 3 MPa (29.6 atm, 420 psig), as claimed in Russian Patent No. 2478576C2. Most of the syntheses require special equipment or conditions that are not usually available for the scale-up of processes to large scale, such as high-pressure autoclaves. In particular, existing methods lack technical details, and the purity of Pt(PF3)4 is not reported in any of the literature. Moreover, all of the disclosed methods are essentially dry approaches, which also poses significant challenges for scale-up to industrial scale.
[0017] There are numerical standards for catalytic conversion of hydrocarbons by platinum compounds, such as Journal of the American Chemical Society (2002), 124(42), 12550-12556. In Jackson et al., J. Am. Chem. Soc. 1997, 119, 7567-7572, the catalytic activity of Pt compounds is shown for the model system Pt4(PF3)8-saturated and aromatic cyclic hydrocarbons. That is, small platinum clusters generated from Pt4(PF3)8 react with various saturated and aromatic cyclic hydrocarbons (cyclohexane, benzene, toluene). The catalytic and dehydrogenation behavior of platinum is revealed by Jackson et al. Therefore, it can be assumed that the introduction of a hydrocarbon solvent into the reaction system and subsequent heating can lead to a mixture of products by various catalytic reactions, and it can be considered to be an unfavorable idea for the selective synthesis of Pt(PF3)4. For these reasons, Pt(PF3)4 has never been synthesized and manipulated in organic solvents, and only anhydrous HF and SO2 have been applied as solvents to study Pt(PF3)4 chemistry (Drews et al., Chem. Eur. J. 2008, 14, 4280-4286).
[0018] To date, the potentially ideal Pt(PF3)4 precursor has not been applied solely due to the lack of scalable methods, and therefore it would be a major advance to provide a scalable method for the production of Pt(PF3)4 in high yield. Summary of the Invention [Means for solving the problem]
[0019] A method for synthesizing Pt(PF3)4 (CAS number 19529-53-4): General formula Pt(Hal)2(PF3) x The platinum compound having the formula Pt(Hal)2(PF3) was dissolved in anhydrous solvent. x forming a solution where Hal=F, Cl, Br or I, x=1, 2; Metal powder and excess PF3 were mixed with Pt(Hal)2(PF3) x adding to the solution; and Pt(Hal)2(PF3) under reaction conditions x A method is disclosed that includes forming Pt(PF3)4 via a reaction of PF3 and a metal powder. The method of the present disclosure may include one or more of the following aspects: · reaction conditions including a reaction temperature in the range of approximately -120 to 200 °C; · reaction conditions including a reaction temperature in the range of approximately 30-200°C; Reaction conditions including reaction temperatures ranging from room temperature to approximately 180°C; Reaction conditions including a reaction temperature ranging from room temperature to approximately 130°C; · reaction conditions including a reaction temperature in the range of approximately 80-130°C; Reaction conditions including reaction pressures ranging from approximately 10 psig to approximately 3000 psig; Reaction conditions including reaction pressures ranging from approximately 20 psig to approximately 1000 psig; Reaction conditions including reaction pressures ranging from about 20 to about 300 psig; Reaction conditions including a reaction pressure of less than approximately 300 psig; · Anhydrous solvents with a boiling point above 150 °C; · Anhydrous solvents with a boiling point above 200 °C; Metal powders, which are copper, zinc or aluminium powders; Metal powder, which is copper powder; Metal powder, which is zinc powder; Metal powder, which is aluminum powder; Metal powders with a lower electrode potential than Pt; Metal powders that do not interact with PF3 and do not form complexes with PF3 under the reaction conditions; Metal powders with an appropriate particle size range that allows them to maintain their powder form during the reaction process; Metal powders with a particle size ranging from 200 to 900 microns; Metal powders with a particle size in the range of 300-500 microns; ·Platinum compound Pt(Hal)2(PF3)x (Hal=F, Cl, Br or I; x=1, 2), Dispersing a platinum precursor having the general formula Pt(Hal)2 in an anhydrous solvent to form a suspension of Pt(Hal)2, where Hal = F, Cl, Br or I; introducing PF3 into the suspension of Pt(Hal)2; The reaction of PF3 and Pt(Hal)2 produces the platinum compound Pt(Hal)2(PF3) x forming a solution of (Hal=F, Cl, Br or I; x=1, 2) in an anhydrous solvent; The further step includes the steps of: · Anhydrous platinum precursor Pt(Hal)2; ·PtCl2, the platinum precursor Pt(Hal)2; ·Platinum precursor Pt(Hal)2, which is anhydrous PtCl2; ·Anhydrous platinum compound Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I, x=1, 2); ·PtCl2(PF3)2, the platinum compound Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I, x=1, 2); ·Pt(Hal)2(PF3), the platinum compound anhydrous PtCl2(PF3)2 x (Hal=F, Cl, Br or I, x=1, 2); ·moreover: Purifying Pt(PF3)4 under air- and moisture-free conditions in a metallic trap; and Storing the purified Pt(PF3)4 in a metal container under air- and moisture-free conditions. Here, the steps to save are removing moisture from the interior surface of the container; and Electropolishing the interior surface of the container; or Passivating the container with PF3 before introducing purified Pt(PF3)4 Contains; a metal for the trap selected from carbon steel, stainless steel, or stainless steel alloy 316, respectively; a metal for the container selected from carbon steel, stainless steel, or stainless steel 316 alloy, respectively; · Anhydrous solvents that are hydrocarbon solvents; ·General formula (C n H 2n+1 )2O(n≧1) and H3C(O(CH2)2) n a hydrocarbon solvent selected from oxyhydrocarbon solvents having OCH3 (n≧1); ·General formula (C n H 2n+1 ) x C6H 6-x (x≧1, n≧1); ·General formula C n H 2n+2 (n≧1); anhydrous solvents, which are dry alkane solvents selected from decane, di-, tri-, tetra-, penta- and hexadecane, etc.; Anhydrous solvents, which are dry arene solvents selected from xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene, etc.; Anhydrous solvents, which are dry ether solvents selected from dibutyl ether, dihexyl ether, dioctyl ether, diethylene glycol dimethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, etc.; Anhydrous solvents, which are arene solvents selected from xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene, etc.; Dry ether solvents, preferably dibutyl ether, dihexyl ether, dioctyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether; Dry arene solvents, preferably xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene; a dry alkane solvent, preferably di-, tri-, tetra-, penta- and hexadecane, as well as a mixture of alkanes known as mineral oil; Anhydrous solvents capable of dissolving the reaction intermediates; ·Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I, x=1, 2) ·Anhydrous solvent capable of dissolving PtCl2(PF3)2); ·Anhydrous solvent that does not react with Pt(PF3)4; Anhydrous solvents that do not react with Pt(Hal)2 (Hal = F, Cl, Br or I); ·Anhydrous solvent that does not react with PtCl2; Xylene is an anhydrous solvent; Hexadecane is an anhydrous solvent; Yield of Pt(PF3)4 in the range of approximately 70-99.9%; Yield of Pt(PF3)4 in the range of approximately 70-95%; Yield of Pt(PF3)4 in the range of approximately 70-93%; The purity of Pt(PF3)4 is greater than 99% by weight; The purity of Pt(PF3)4 is greater than 99.5% by weight; The purity of Pt(PF3)4 is approximately 90-99.9% by weight; The purity of Pt(PF3)4 being approximately 99.0-99.9% by weight; A purity of Pt(PF3)4 of approximately 99.5-99.9% by weight; and · Formed Pt(PF3)4 with scalability to large industrial scale.
[0020] Also disclosed is a method for producing and storing Pt(PF3)4 (CAS number 19529-53-4), which comprises: a) forming a suspension of a platinum precursor Pt(Hal)2 (wherein Hal = F, Cl, Br or I) and metal powder in an anhydrous solvent; b) introducing an excess of PF3 into a suspension of Pt(Hal)2 and metal powders; c) The reaction of PF3 and Pt(Hal)2 (where Hal = F, Cl, Br or I; x = 1, 2) under low pressure conditions to give the soluble intermediate Pt(Hal)2(PF3) in anhydrous solvents. x forming a d) Pt(Hal)2(PF3) in anhydrous solvent x reacting the metal powder and PF to form Pt(PF); e) purifying Pt(PF3)4 under air- and moisture-free conditions in a metallic trap; and f) storing the purified Pt(PF3)4 in a metal container under air- and moisture-free conditions. The method of the present disclosure may include one or more of the following aspects: ·PtCl2, the platinum precursor Pt(Hal)2; · Anhydrous solvents with a boiling point above 150 °C; · Anhydrous solvents with a boiling point above 200 °C; ·General formula (C n H 2n+1 )2O(n≧1) and H3C(O(CH2)2) n Oxyhydrocarbon solvents having the general formula (C n H 2n+1 ) x C6H 6-x (x≧1, n≧1) or an arene solvent having the general formula C n H 2n+2 (n≧1); an anhydrous solvent which is a hydrocarbon solvent selected from alkane solvents having Anhydrous solvents such as xylene or hexadecane; ·Anhydrous solvent capable of dissolving reaction intermediates; ·Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I, x=1, 2) ·Anhydrous solvent capable of dissolving PtCl2(PF3)2); ·Anhydrous solvent that does not react with Pt(PF3)4; Anhydrous solvents that do not react with Pt(Hal)2 (Hal = F, Cl, Br or I); ·Anhydrous solvent that does not react with PtCl2; Reaction temperature in the range of approximately 30-200°C; Reaction temperature in the range of approximately 80-130°C; · Low pressure conditions, which are pressures below approximately 300 psig; Low pressure conditions, which are pressures in the range of approximately 20~300psig; Metal powders, which are copper, zinc or aluminium powders; Metal powder, which is copper powder; Metal powders with a lower electrode potential than Pt; Metal powders that do not interact with PF3 and do not form complexes with PF3 under the reaction conditions; Metal powders with an appropriate particle size range that allows them to maintain their powder form during the reaction process; Metal powders with a particle size ranging from 200 to 900 microns; Metal powders with a particle size in the range of 300-500 microns; Yield of Pt(PF3)4 in the range of approximately 70-99.9%; Yield of Pt(PF3)4 in the range of approximately 70-95%; Yield of Pt(PF3)4 in the range of approximately 70-93%; The purity of Pt(PF3)4 after purification is approximately 90-99.9 wt%; The purity of Pt(PF3)4 after purification is 99.0-99.9 wt%; a metal for the trap and a metal for the container, respectively, selected from carbon steel, stainless steel, or stainless steel alloy 316; and ·moreover: Electropolishing the interior surface of the container; or Passivating the container with PF3 before introducing purified Pt(PF3)4 The steps include:
[0021] Also disclosed is a method for producing and storing Pt(PF3)4 (CAS number 19529-53-4), which comprises: a) forming a suspension of a platinum precursor, Pt(Cl)2, in an anhydrous solvent selected from xylene or hexadecane; b) An excess of PF3 is introduced into a suspension of Pt(Cl)2 to form Pt(Cl)2(PF3) by the reaction of PF3 and Pt(Cl)2. x forming a solution of (x=1, 2) in an anhydrous solvent; c) Copper powder in Pt(Cl)2(PF3) x (x=1, 2) to a solution; d) Copper powder, PF3 and Pt(Cl)2(PF3) x forming Pt(PF3)4 from the reaction in an anhydrous solvent at a reaction temperature ranging from 30 to 200° C. and a low PF3 pressure ranging from 20 to 300 psig; e) purifying Pt(PF3)4 under air- and moisture-free conditions in a stainless steel trap; and f) storing the purified Pt(PF3)4 under air- and moisture-free conditions in a stainless steel container, the interior surface of which is electropolished or passivated with PF3. The disclosed method may include one or more of the following aspects: Copper powder having a particle size in the range of 200 to 900 microns; and Copper powder with particle size ranging from 300 to 500 microns.
[0022] Notation and Nomenclature In the following detailed description and claims, a number of abbreviations, symbols and terms that are generally well known in the art are used. While a definition is typically provided at the first occurrence of each acronym, such as Stainless Steel (SS). Certain abbreviations, symbols and terms are used throughout the following specification and claims, including the following:
[0023] In the following detailed description and claims, a number of abbreviations, symbols and terms that are commonly known in the art are used.
[0024] As used herein, the indefinite article "a" or "an" means one or more.
[0025] As used herein, the terms "about" or "around" or "approximately" in the text or claims mean ±10% of the stated value.
[0026] As used herein, "room temperature" in the text and claims means approximately 18°C to approximately 25°C.
[0027] As used herein, "atmospheric pressure" in the text or claims means approximately 1 atm.
[0028] Standard abbreviations of elements from the periodic table are used herein. It should be understood that elements can be referred to by these abbreviations (e.g., Si refers to silicon, N refers to nitrogen, O refers to oxygen, C refers to carbon, H refers to hydrogen, and Hal refers to halogens, which are F, Cl, Br, and I).
[0029] Unique CAS Registry Numbers assigned by the Chemical Abstract Service (ie, "CAS") are provided to identify the particular molecules disclosed.
[0030] As used herein, the term "hydrocarbon" refers to saturated or unsaturated functional groups containing only carbon and hydrogen atoms.
[0031] As used herein, the terms "low pressure", "low reaction pressure" or "low PF3 pressure" refer to pressures below 300 psig or below 20 atm. The same applies to "reduced pressure", which refers to pressures reduced or lowered to below 300 psig or 20 atm. In some cases, "low pressure", "low reaction pressure" or "low PF3 pressure" may refer to a pressure range ranging from 20 psig to 300 psig.
[0032] Ranges may be expressed herein as from one about a particular value and / or to another about a particular value. When such a range is expressed, it is to be understood that other embodiments are from the one particular value and / or to the other particular value, with all combinations within said ranges. Any and all ranges described herein include their endpoints (i.e., x=1-4 or x ranges from 1-4 includes x=1, x=4, and x=any number therebetween), regardless of whether the term "inclusive" is provided.
[0033] In this specification, reference to "one embodiment" or "embodiment" means that a particular feature, structure, or characteristic described in connection with the embodiment may be included in at least one embodiment of the invention. The appearances of the phrase "in one embodiment" in various places in this specification do not necessarily all refer to the same embodiment, nor are separate or alternative embodiments necessarily mutually exclusive. The same applies to the term "implementation."
[0034] As used in this application, the word "exemplary" is used herein to mean serving as an example, instance, or illustration. Any aspect or design described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other aspects or designs. Rather, use of the word exemplary is intended to present concepts in a concrete manner.
[0035] In addition, the term "or" is intended to mean an inclusive "or" rather than an exclusive "or." That is, unless otherwise specified or clear from the context, "X employs A or B" is intended to mean any of the natural inclusive permutations. That is, "X employs A or B" is satisfied if X employs A; if X employs B; or if X employs both A and B. In addition, as used in this application and the appended claims, the articles "a" and "an" should be construed generally to mean "one or more" unless otherwise specified or clear from the context to refer to the singular form.
[0036] The foregoing and various other aspects, features, and advantages of the present invention, as well as the invention itself, may be more fully understood by reference to the following detailed description of the invention when considered in conjunction with the following drawings, which are presented for illustrative purposes only and are not intended to limit the invention. [Brief description of the drawings]
[0037] [Figure 1] FIG. 1 is a block diagram of an exemplary disclosed system for synthesizing Pt(PF3)4. [Figure 2a] FIG. 2a is a flow chart of an exemplary disclosed process for the synthesis of Pt(PF3)4 starting from Pt(Hal)2 (Hal=F, Cl, Br, or I). [Figure 2b] FIG. 2b is a flow chart of an exemplary disclosed process for the synthesis of Pt(PF) starting from Pt(Hal)(PF) (x=1, 2; Hal=F, Cl, Br, or I). [Diagram 3] FIG. 3 shows the 19F NMR spectra of the PtCl2(PF3)2 crystals and the supernatant solution of hexadecane from the reaction mixture stopped at the PtCl2(PF3)2 stage. [Figure 4]FIG. 4 is a graph of the Pt(PF3)4 assay and relative amounts of impurities over time in electropolished stainless steel small canisters at room temperature. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0038] Methods for synthesizing, preparing, producing and storing Pt(PF3)4 (CAS number 19529-53-4) are disclosed. The disclosed methods are scalable to produce Pt(PF3)4 in high yields, which can be used as a precursor for Pt-containing film deposition in microelectronic devices or catalytic industries.
[0039] The disclosed synthesis method involves the synthesis of an insoluble platinum compound, Pt(Hal)2 (Hal = F, Cl, Br or I), and a soluble reaction intermediate, the platinum compound Pt(Hal)2(PF3). x (Hal = F, Cl, Br or I; x = 1, 2), which involves the formation of a soluble reactive intermediate from an insoluble Pt(Hal)2 (Hal = F, Cl, Br or I) suspension at low pressure conditions, and the reaction of the soluble intermediate with a coreactant such as metal powder and PF3 to form Pt(PF3)4.
[0040] Alternatively, the soluble intermediate Pt(Hal)2(PF3) x Since (Hal = F, Cl, Br or I; x = 1, 2) can be isolated and purified, the disclosed synthesis method can be used to obtain soluble Pt(Hal)2(PF3) under certain reaction conditions. x It can be a one-step wet synthesis of Pt(PF3)4 using (Hal=F, Cl, Br or I; x=1, 2) reacted with metal powder and a co-reactant such as PF3 to form Pt(PF3)4. Preferably, Hal=Cl. Preferably, the metal powder is copper powder.
[0041] Furthermore, a robust, high-yielding and scalable synthesis of Pt(PF3)4 is disclosed that can proceed at low pressure and can be carried out in a conventional reactor or equipment. More specifically, Pt(PF3)4 can be prepared from Pt(Hal)2 (Hal = F, Cl, Br or I) or Pt(Hal)2(PF3). x (Hal=F, Cl, Br or I; x=1, 2) with PF3 and a metal powder such as copper powder, in an anhydrous solvent under low PF3 pressure. The metal powder may have a particle size ranging from approximately 200 to 900 microns, preferably approximately 300 to 500 microns. The anhydrous solvent is used to synthesize the reaction intermediate Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I; x=1, 2), where Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2) can be formed from Pt(Hal)2 and PF3 under certain reaction conditions, such as under low pressure conditions. Herein, the platinum compound Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I; x=1, 2) can be isolated and purified for use as reactants or starting materials for the synthesis of Pt(PF3)4. The yield of Pt(PF3)4 using the disclosed synthesis method can range from approximately 70 to 99.9%. The disclosure also includes a purification process of the product Pt(PF3)4 by metal trapping, and storage conditions of the purified Pt(PF3)4 in a container. Pt(PF3)4 can be stored in devices and ampoules made of stainless steel and preferably having passivated or electropolished inner surfaces under air- and moisture-free conditions. Pt(PF3)4 can be stored in metal containers, such as stainless steel containers and stainless steel containers with passivated or electropolished inner surfaces, at room temperature without changing its purity.
[0042] As mentioned above, the lack of scalable methods in the art may be due to the fact that commonly available reactors for pilot plant synthesis and bulk production are not designed for operation under high pressure and for efficient stirring (mixing) of air-sensitive solids. That is, commercially available reactors (e.g., from High Pressure Equipment Company) that can operate under high pressure of about 100 atm do not have the stirring function required for the reaction to proceed. In addition, commercially available reactors (e.g., from Buchiglas USA) have difficulty even cooling to the dry ice temperature required to condense PF3 in the reactor. Although the stirring of solids can be improved to some extent by using specially designed stirring shafts, parasitic reactions such as PtCl2 / Cu, which result in platinum metal and reduce the yield of Pt(PF3)4, are not resolved. In addition, the removal of impurities is difficult, requiring additional purification steps that are expensive and uncertain.
[0043] The disclosed method for robust, high-yield and scalable synthesis of Pt(PF3)4 can proceed under low PF3 pressure, e.g., less than 20 atm, and can be carried out in commonly used commercial reactors. The potentially ideal Pt(PF3)4 precursor has not been applied so far solely due to the lack of scalable synthesis methods, and therefore the disclosed method provides a method that can lead to scaled-scale production of Pt(PF3)4 in high yields, which is an important advance in the art. The reason for the lack of scalable synthesis methods is that commonly used commercial reactors for pilot plant synthesis and bulk production are not designed for operation under high pressure (e.g., 30 atm or higher), as mentioned above, and are not designed for efficient agitation (mixing) of air-sensitive solids.
[0044] The disclosed method may demonstrate, for the first time, that the reaction aimed at synthesizing Pt(PF3)4 by PtCl2+PF3+Cu in a solvent proceeds through a sufficiently soluble intermediate PtCl2(PF3)2 under reaction conditions (e.g., low pressure of 20-300 psig and temperature of 80-130°C) when the starting material Pt(Hal)2 (Hal=F, Cl, Br or I) is PtCl2 and the metal powder is Cu powder. It is common knowledge that the solubility of inorganic compounds such as PtCl2(PF3)2 is lower in saturated hydrocarbon solvents than in benzene, an arene solvent, and therefore it is counterintuitive to rely on the solubility in hexadecane, a hydrocarbon solvent, and also counterintuitive to rely on such low solubility reactions even in arene solvents.
[0045] According to the prior art, Pt(PF3)4 was usually prepared from PtCl2, K2PtCl6 and K2PtCl6, while K2PtCl6 is necessary to reduce the PF3 pressure. Both PtCl2 and K2PtCl6 are insoluble in the disclosed solvents (e.g. arenes, saturated hydrocarbons). As shown in the following examples and comparative examples, the solvent effect is not the same for platinum starting compounds, such as PtCl2 (Example 1, Table 1, Comparative Example 1) and K2PtCl6 (Example 7, Table 5). The addition of the disclosed solvents (e.g. xylene, hexadecane) is beneficial for reactions initiated from PtCl2, but the reaction without solvent from the starting compound K2PtCl6 without solvent: K2PtCl6 + Cu (excess amount) + PF3 (excess amount) → Pt(PF3)4 + 4CuCl + 2KCl The yield of Pt(PF3)4 is higher than that of the reaction starting from K2PtCl6 in hexadecane solvent, indicating that the solvent benefit is beneficial for certain Pt precursors such as PtCl2, PtF2, PtI2, PtBr2, etc. Therefore, the use of solvents in the synthesis of Pt(PF3)4 from Pt(Hal)2 (Hal = F, Cl, Br or I) is novel.
[0046] FIG. 1 is a block diagram of an exemplary disclosed solid-gas PtCl2+PF3+Cu system for the synthesis of Pt(PF3)4. As shown, first, a metal powder, such as Cu powder 11, is added to a reactor 16 via line 101. In the disclosed process, an anhydrous solvent is used as the solvent 14. The solvent applied as the solvent 14 may have a moisture content of 0-50 ppm, preferably 0-10 ppm, more preferably 0-1 ppm. The solvent 14 may be dried by contacting with a desiccant selected from 3 Å or 4 Å molecular sieves or activated alumina through a drying process 104. The drying process 104 may be carried out at a temperature range of 10-50° C., preferably at room temperature, for a period of 0.5 hours to 20 hours. In some embodiments, the drying process 104 may be accomplished by keeping the solvent in a container 15 with molecular sieves or by passing the solvent through a column (not shown) containing a desiccant in the drying process 104. The moisture content in the container 15 after drying may be measured by Karl Fischer titration or any other suitable analysis. The solvent 14 may be a commercially available solvent and may be degassed by applying a vacuum-inert gas cycle or by bubbling with an inert gas containing less than 0.5 ppm O2 and moisture before contacting with the desiccant. The solvent or anhydrous solvent 14 may be stored in the container 15 or sent to the reactor 16 via line 105 immediately after the drying process 104. The container 15 with the dried anhydrous solvent 14 may be stored before the next step or may be transported to another location where the reactor 16 is located.
[0047] The reactor 16 is then charged with PtCl2 12 under an inert atmosphere (e.g., nitrogen, argon, helium) by any suitable means, for example by applying a solid dropping funnel 102. The PtCl2 12 can be anhydrous PtCl2. In the following, PF3 13 is charged to the reactor 16 via the addition line 103 by pressure difference, but the reactor 16 may be pre-evacuated and heated, or at room temperature and pre-evacuated, or contain PF3 at constant pressure and temperature. The reactor 16 may be depressurized to 0.1-50 Torr, preferably 0.1-2 Torr, before the addition of PF3, to remove an inert gas selected from nitrogen, argon, helium. The absence of non-condensable gases (nitrogen, argon, helium) in the reactor 16 makes the distillation of the product Pt(PF3)4 more efficient. Alternatively, the PF3 added to the reactor 16 may contain 1 atm of nitrogen, argon or helium at room temperature. Adding PF3 13 to reactor 16 creates a PF3 pressure of 20 psig to 300 psig in reactor 16. PF3 can be added in portions or continuously during the process. The value of the PF3 pressure depends on the pressure rating of the applied reactor, and can be added in portions or continuously during the process and recycled after the process.
[0048] The reactor 16 may be a typical vessel with stirring, temperature and pressure control, and reaction monitoring means applied to the synthesis and purification of Pt(PF3)4. The reactor 16 has cooling and heating equipment maintained at a temperature ranging from about -120°C to about 200°C, preferably from room temperature to 180°C, more preferably from room temperature to 130°C, and a corresponding pressure ranging from about 10 psig to about 3000 psig, preferably from about 20 psig to about 1000 psig, more preferably from about 20 psig to about 300 psig. The reactor 16 is connected to an empty vessel that acts as a ballast, and has a vent to vent the reaction contents if overpressurized. The reactor 16 is connected to nitrogen and vacuum lines (not shown), and a PF3 scrubber (not shown), and is connected to traps 18 and 20 for recovering the product Pt(PF3)4 via line 107 and recycling unreacted PF3 via line 110.
[0049] The solvent 14 may include various organic solvents. In some embodiments, the solvent 14 may be a dry alkane solvent selected from decane, di-, tri-, tetra-, penta-, or hexadecane. In this case, the Cu powder 11, anhydrous PtCl2 12, and dry alkane solvent 14 are charged into the reactor 16 to form a suspension. The starting amount of PtCl2 solids in the solvent 14 is 1% to 50%, preferably 5% to 40%, and more preferably 20% to 30%. The molar ratio of PtCl2 12 to Cu powder 11 is 1:2 to 1:20, preferably 1:6 to 1:10. That is, the molar ratio of Pt to Cu is 1:2 to 1:20, preferably 1:6 to 1:10. The reactor 16 is depressurized to 0.1 to 50 Torr, preferably 0.2 to 5 Torr, before introducing the PF3 13.
[0050] Alternatively, the solvent 14 can be a dry arene solvent selected from xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene or diisobutylbenzene. In this case, Cu powder 11, anhydrous PtCl2 12 and dry arene solvent 14 are charged into the reactor 16. The starting amount of PtCl2 solids in the solvent is 1%-50%, preferably 10-40%, more preferably 20%-30%. The molar ratio of PtCl2 to Cu is 1:2-1:20, preferably 1:6-1:10. That is, the molar ratio of Pt to Cu is 1:2-1:20, preferably 1:6-1:10. The reactor 16 is depressurized to 0.1-50 Torr, preferably 0.2-5 Torr, before the introduction of PF3 13.
[0051] Alternatively, the solvent 14 can be a dry ether solvent selected from dibutyl ether, dihexyl ether, dioctyl ether, dimethyl ether of diethylene glycol, triethylene glycol dimethyl ether, and tetraethylene glycol dimethyl ether. In this case, Cu powder 11, anhydrous PtCl2 12, and dry ether solvent 14 are charged into the reactor 16. The starting amount of PtCl2 solids in the solvent is 1% to 50%, preferably 10% to 40%, and more preferably 20% to 30%. The molar ratio of PtCl2 to Cu is 1:2 to 1:20, preferably 1:6 to 1:10. That is, the molar ratio of Pt to Cu is 1:2 to 1:20, preferably 1:6 to 1:10. The reactor 16 is depressurized to 0.1 to 50 Torr, preferably 0.2 to 5 Torr, before the introduction of PF3 13.
[0052] After PF3 13 is introduced into the reactor 16, the reaction mixture is initially a suspension of PtCl2 12 and Cu powder 11 in the solvent 14 under PF3 13 pressure. The reaction mixture is then stirred while the reactor 16 is heated to form PtCl2(PF3) x(x=1, 2) is formed. The reaction can be stopped after heating for 20-80 minutes with stirring in the preferred temperature range above, and PtCl2(PF3)2 can be isolated from the solvent, reaction by-products, residual PF3, etc. The compound PtCl2(PF3) x (x=1, 2) are soluble in the solvent 14, which can be verified by NMR spectroscopy, as shown in FIG. 3. The reaction continues under PF3 pressure in the reactor 16, where PF3 and PtCl2 (PF3) x (x=1, 2) is dissolved in a solvent and reacted with copper powder 11. In the course of the reaction, PF313 is consumed. PF313 can be added in portions to reactor 16 or can be added continuously to maintain a constant selected pressure. Once all starting and intermediate platinum compounds have been consumed, the pressure in reactor 16 becomes constant at a given temperature.
[0053] The reaction time may be in the range of 1 hour to 24 hours, preferably 4 hours to 8 hours. The conversion rate may be monitored by the consumption rate of PF3 and the pressure change in the reactor 16, by in situ Raman spectroscopy or any other suitable technique.
[0054] In some embodiments, the reaction in reactor 16 occurs in hexadecane, under 20-50 psig PF3, at a temperature of 100-125° C., and is completed in 6 hours. Alternatively, in some embodiments, the reaction in reactor 16 occurs in xylene, under 20-40 psig PF3, at a temperature of 100-125° C., and is completed in 5 hours.
[0055] After the reaction is completed, the reaction mixture is cooled to 20-65°C, preferably 30-45°C. The gas consisting of the remaining PF3, Pt(PF3)4 and solvent is sent to the pre-evacuated trap 17, which is maintained at a temperature in the range of -196°C to -160°C. PF3 (melting point -151.5°C, boiling point -101.9°C) and Pt(PF3)4 (melting point -15°C) and the solvent are condensed in the pre-evacuated trap 17. After the condensation of Pt(PF3)4 in the pre-evacuated trap 17 is completed, the pressure can be intermittently reduced to remove the remaining gases such as nitrogen, argon, helium, etc., to form a reduced pressure in the range of 0.1-50 Torr, preferably 0.2-2 Torr, to facilitate the distillation of the remaining Pt(PF3)4 from the reactor 16 in the pre-evacuated trap 17. Before condensing the reaction products containing Pt(PF3)4 and PF3, the pre-depressurized trap 17, the Pt(PF3)4 trap 18 and the PF3 trap 20 are pre-depressurized to 0.01 to 10 Torr, preferably 0.1 to 1 Torr.
[0056] Alternatively to the above procedure, after the reaction is completed, the reaction mixture is cooled to 20-65°C, preferably 30-45°C, and a part of the gas containing PF3, Pt(PF3)4 and the solvent is sent to the pre-depressurized trap 17 through the line 106, which is maintained at a temperature in the range of -60--80°C. PF3 is not condensed, and Pt(PF3)4 and the solvent are condensed in the pre-depressurized trap 17. After Pt(PF3)4 and the solvent are condensed in the pre-depressurized trap 17, the uncondensed PF3 is sent from the pre-depressurized trap 17 by the pressure difference to the PF3 trap 20, which is maintained at a temperature in the range of -160--196°C, and then the next part of the gas containing PF3, Pt(PF3)4 and the solvent is sent from the reactor 16 to the pre-depressurized trap 17, and this cycle continues until all PF3 is condensed in the PF3 trap 20 and all Pt(PF3)4 is condensed in the pre-depressurized trap 17.
[0057] Condensation of the gaseous products is preferably performed by the steps disclosed above for a continuous process, because even with efficient engineering and cooling of the pre-depressurized trap 17 with dry ice-isopropanol (-79°C), the continuous flow of gas from the reactor 16 would result in 20-60% of the Pt(PF3)4 in the PF3 trap 20 being bypassed 108, necessitating an additional step (not shown) to recover all of the Pt(PF3)4 from the PF3 trap 20. The additional step may include warming the trap 20 to a temperature higher than the boiling point of PF3 (-102°C), typically -79°C (dry ice cooling), and trapping all of the PF3 in a first separate trap (not shown) cooled with liquid nitrogen. After trapping all of the PF3, the trap 20 is warmed to room temperature and the Pt(PF3)4 is trapped in a second separate trap (not shown). The PF3 captured in the first individual trap can be recycled to PF3 13 through line 110 for synthesis in reactor 16. The pre-depressurized trap 17, the Pt(PF3)4 trap 18 and the PF3 trap 20 and all the connecting lines are made of metal or are made of metal, where the metal materials are preferably carbon steel, stainless steel and stainless steel alloy. In some embodiments, the pre-depressurized trap 17, the Pt(PF3)4 trap 18 and the PF3 trap 20 and all the connecting lines are made of stainless steel. All the traps can have passivated or electropolished inner surfaces.
[0058] Pt(PF3)4 is separated from PF3 by fractional distillation under air- and moisture-free conditions. After recovery of volatile species, the pre-evacuated trap 17 is warmed to a temperature in the range of −20 to −90° C., preferably −60 to −80° C., and PF3 is distilled in PF3 trap 20, which is maintained at a temperature in the range of −160 to −196° C. The PF3 in PF3 trap 20 can be stored, transferred to a different location, or recycled as PF3 13 for further synthesis.
[0059] Pt(PF3)4 contaminated with reaction by-products such as solvent, solid copper chloride, etc. remains in the pre-evacuated trap 17 after consumption of PF3. The Pt(PF3)4 in the pre-evacuated trap 17 has a purity of 90-99% and contains 0.1-5% PF3, 0.1-10% solvent, and 0.1-1% other impurities, preferably phosphorus oxofluoride and solid copper chloride. Pt(PF3)4 and the solvent and solids are separated when the mixture is maintained at a temperature in the range of 10-40°C, preferably at room temperature, and the receiver is maintained at a temperature in the range of -50-196°C, where the apparatus and receiver can be pre-evacuated before distillation, and the pressure during distillation is 0.01 Torr-760 Torr, preferably 0.1 Torr-5 Torr. More specifically, the Pt(PF3)4 recovered in the pre-evacuated trap 17 is purified by distillation in the Pt(PF3)4 trap 18. In one embodiment, the pre-evacuated trap 17 containing Pt(PF3)4 after consumption of PF3 is warmed to 0-40°C, preferably room temperature, and Pt(PF3)4 is distilled in the pre-evacuated trap 17 at a pressure of 0.01-50 Torr, preferably 0.1-2 Torr, while the Pt(PF3)4 trap 18 is maintained at a temperature in the range of -15 to -196°C.
[0060] The Pt(PF3)4 recovered in the Pt(PF3)4 trap 18 has a purity of 70 to 99.9% w / w, preferably 80 to 99.9% w / w, more preferably 90 to 99.9% w / w, even more preferably 95 to 99.9% w / w, and even more preferably 99.0 to 99.99% w / w after purification. Preferably, the recovered Pt(PF3)4 has a purity of 99.50 to 99.99% w / w, and contains 0 to 0.5% PF3, 0.01 to 0.5% other impurities (such as phosphorus oxofluorides and thermal decomposition products of Pt4(PF3)8), and 0 to 0.5% remaining solvent. The purity of Pt(PF3)4 is 1 H, 19 F, 31 P, 195 The Pt NMR, FTIR and Raman spectroscopy were used.
[0061] The purified Pt(PF3)4 may have about 0% to about 0.1% by weight of PF3, preferably about 0% to about 0.05% by weight of PF3 impurities. The purified Pt(PF3)4 may have about 0% to about 1% by weight, preferably about 0% to about 0.05% by weight of phosphorus fluorides and oxofluorides including PF3, POF3, (HO)POF2, and (HO)2POF. The purified Pt(PF3)4 may have 0% to about 0.1% by weight, preferably about 0% to about 0.05% by weight of platinum compounds other than Pt(PF3)4. Pt(Hal)2, Pt4(PF3)8, and Pt(Hal)2(PF3) in Pt(PF3)4 x The total concentration of (Hal=F, Cl, Br or I, x=1, 2) after purification can be about 0% by weight to about 0.1% by weight, preferably about 0% by weight to about 0.05% by weight. Furthermore, the purified Pt(PF3)4 can have 0.1 ppmw to 1000 ppmw of the solvent used in the synthesis, preferably about 0 ppmw to 200 ppmw of the solvent, more preferably 0 ppmw to 50 ppmw of the solvent, and even more preferably 0 ppmw to 20 ppmw of the solvent. Moreover, the purified Pt(PF3)4 can have about 0 ppmw to about 100 ppmw of hydrogen fluoride and 0 ppmw to about 50 ppmw of hydrogen chloride. In addition, the purified Pt(PF3)4 can have about 0 ppb to 10 ppm of trace metals such as iron, nickel, manganese, cobalt, copper, etc. The remaining PF3 is recycled to the synthesis of Pt(PF3)4.
[0062] In some embodiments, an internal standard such as Me4Si may be used to measure the amount of organic compounds in Pt(PF3)4. In some embodiments, sample preparation may include adsorption of the organic solvent with a suitable adsorbent such as C8 derivatized silica gel.
[0063] In some embodiments, the Pt(PF3)4 trap 18 may include two subsequent traps, such as trap 18a and trap 18b (not shown), for distillation to obtain Pt(PF3)4 of a desired purity. After purification, the Pt(PF3)4 may be stored in the Pt(PF3)4 trap 18 before packaging into a metal ampoule 19 for shipping, deposition, or storage. Alternatively, the Pt(PF3)4 may be stored in the metal ampoule 19 after packaging 109. The metal ampoule 19 may be a metallic container / vessel made from metals such as stainless steel, carbon steel, and stainless steel 316 alloy. The inner surface of the metal ampoule 19 may be passivated with PF3 or electropolished.
[0064] Moisture derived from the surfaces of the metal Pt(PF3)4 trap 18 and the metal ampoule 19 can be removed by heating Pt(PF3)4 at approximately 100 to 170° C. under reduced pressure before introducing Pt(PF3)4 into the metal Pt(PF3)4 trap 18 and the metal ampoule 19. Alternatively, moisture derived from the surfaces of the metal Pt(PF3)4 trap 18 and the metal ampoule 19 can be removed by passivating the trap container with PF3 before introducing Pt(PF3)4 into the metal Pt(PF3)4 trap 18 and the metal ampoule 19.
[0065] The purified Pt(PF3)4 may be stored in the metal Pt(PF3)4 trap 18 or metal ampoule 19 at a temperature range of -80 to 60°C, preferably 10 to 40°C, more preferably 20 to 25°C. The method of the present disclosure includes storing Pt(PF3)4 in a metal container, such as a stainless steel, carbon steel, or stainless steel 316 alloy container. The inner surface of the metal container may be passivated with PF3 or electropolished. Here, the stainless steel container may be a small stainless steel open-ended sample cylinder or a small electropolished stainless steel canister. In an exemplary embodiment, the purified Pt(PF3)4 was stored in a small stainless steel open-ended sample cylinder at room temperature for 2 months without any change in the purity of Pt(PF3)4. Alternatively, the purified Pt(PF3)4 was stored in a small electropolished stainless steel canister at room temperature for 2 months without any change in the purity of Pt(PF3)4.
[0066] The disclosed method involves the synthesis of a soluble intermediate, Pt(Hal)2(PF3), shown in FIG. x(x=1, 2; Hal=F, Cl, Br or I) through step process, so-called solid-gas Pt(Hal)2-M-PF3 synthesis process in solution. Here, HAL is F, Cl, Br or I, preferably Hal is Cl; M is metal (such as Cu), then Pt(Hal)2-M-PF3 synthesis process becomes PtCl2-Cu-PF3 synthesis process. The method of the present disclosure produces Pt(PF3)4 with high yield (i.e., 70-99.9%) and high purity (i.e., more than 99%, preferably more than 99.99%), as well as storage and delivery of high purity Pt(PF3)4 without loss of purity. The use of a hydrocarbon solvent is advantageous for the disclosed solid-gas PtCl2-Cu-PF3 reaction process, where the solvent is capable of dissolving the reaction intermediate (e.g., platinum complex PtCl2(PF3)2) formed under suitable reaction conditions from the insoluble starting materials, solid platinum compound PtCl2 and PF3 gas, and does not react with Pt(PF3)4. The use of such a solvent allows Pt(PF3)4 to be obtained in high yield, in a shorter time, and at low PF3 pressure. The low pressure of PF3 in the disclosed synthesis method of Pt(PF3)4 eliminates the need for reactor cooling to condense PF3, and allows the use of reactors with low pressure ratings. As a result, commonly available equipment and reactors can be utilized in the disclosed synthesis method of Pt(PF3)4. This results in a Pt(PF3)4 synthesis process that is scalable to large industrial scales and requires limited equipment complexity due to the low pressure requirements. Here, the reaction conditions include reaction temperature, reaction pressure, etc.
[0067] In the disclosed synthesis method, the problems of low, moderate and non-reproducible yields in solid-gas reactions, as well as the problem of high pressure PF3 required for the synthesis of Pt(PF3)4, are solved by adding the disclosed solvent to the PtCl2-Cu-PF3 reaction system. The addition of the solvent achieves the synthesis of Pt(PF3)4 under low PF3 pressure in a shorter time with reproducible high yields (Table 1, Examples 1-4). The reason for the improvement of the synthesis process is the solubility of PtCl2(PF3)2, which is obtained in situ under low pressure reaction conditions from PtCl2 and PF3. It is a common finding that solution-solid reactions are much more efficient than reactions between two different solids and gases. The addition of the solvent changes the solid-gas PtCl2-Cu-PF3 reaction system into a much more efficient solution-solid reaction. Although the use of solvents in synthesis is a common practice, it is not an obvious solution for a given reaction system and may even be subject to challenge due to the reaction conditions applied, the high reactivity of PF3, and the diverse platinum coordination and catalytic chemistry in organic solvents.
[0068] The addition of a solvent in the solid-gas Pt(Hal)2-M-PF3 synthesis system solves the problems of low, moderate and non-reproducible yields in solid-gas reactions (see Comparative Example 1 below) and the high PF3 pressure (50-150 Atm) required for the synthesis of Pt(PF3)4. The addition of a solvent allows the synthesis of Pt(PF3)4 at low PF3 pressure, in a shorter time and with a reproducible high yield (see Examples 2-4 below). The reason for the improved yield is the solubility of the reaction intermediate PtCl2(PF3)2, which is obtained in situ under certain reaction conditions from PtCl2 and PF3 (Figure 3). Again, it is known that solution-solid reactions are much more efficient than reactions between two different solids and gases. In the following Examples 2 to 4, the addition of a solvent in the PtCl2-Cu-PF3 synthesis system enables the synthesis of Pt(PF3)4 with a reproducible high yield at a PF3 pressure of 10 to 50 psig for 5 to 6 hours (see also Example 1), because the solid-gas PtCl2-Cu-PF3 synthesis system becomes a solution-solid reaction. As a result, commonly available equipment and reactors can be used for the disclosed Pt(PF3)4 synthesis process.
[0069] A suitable solvent should be "inert" to the starting compounds and intermediates and products Pt(PF3)4 and should not react with the starting compounds and intermediates and products Pt(PF3)4 under the reaction conditions. In other words, a suitable solvent should not catalytically convert the starting compounds, intermediates and products Pt(PF3)4 under the reaction conditions, and the solvent should not convert the starting compounds and products to other compounds. A suitable solvent should dissolve only at least one intermediate in the reaction to achieve a solution-solid reaction that is fairly efficient, reproducible, and therefore more scalable than the reaction between two different solids and gases. A suitable solvent should be able to dissolve Pt(Hal)2(PF3) obtained in situ from Pt(Hal)2 and PF3 under the reaction conditions. x The catalyst should be capable of dissolving at least one platinum-containing reaction intermediate such as (wherein Hal=F, Cl, Br or I; x=1, 2).
[0070] Platinum precursors may form soluble intermediates in solvents under certain reaction conditions, and in other cases, the addition of a solvent results in a lower yield of Pt(PF3)4 compared to the reaction without a solvent (see Comparative Example 1(b)), where the yield of Pt(PF3)4 is 60% in the solid-gas reaction and Example 7 (No. 9), and the yield of Pt(PF3)4 is 26% in the reaction in hexadecane under the same pressure and temperature. The disclosed platinum precursors Pt(Hal)2 (Hal=F, Cl, Br, or I) form soluble intermediates, and therefore are suitable for the disclosed synthesis process.
[0071] Suitable solvents used herein may be selected from ether, arene or alkane solvents. The preferred boiling point (BP) of the solvent may be greater than 150° C., preferably greater than 200° C. This is necessary for efficient separation of the solvent and the product Pt(PF3)4, since the calculated boiling point of Pt(PF3)4 is about 77° C., calculated by the equation logP=10.34-2610 / T (P is Torr and T is Kelvin) from “Vapor Pressure Measurements of Volatile Transition-Metal Complexes”, RD Scanner, JH Schatcher, Jr., Report (1989), UCRL-53937. For example, hexadecane (BP: 285° C., melting point (MP): 18° C., and vapor pressure (VP): 0.07 Torr at 20° C.), p-cymene (BP: 177° C., MP: −68° C., and VP: 1 Torr at 20° C.), and dihexyl ether (BP: 223° C., MP: −43° C., and VP: 0.05 Torr at 20° C.), triethylene glycol dimethyl ether (BP: 216° C., MP: −45° C., and VP: 0.025 Torr at 20° C.), tetraethylene glycol dimethyl ether (BP: 275° C., MP: −30° C., and VP: 0.001 Torr at 20° C.) may be suitable for use as a solvent in the disclosed Pt(Hal)2-M-PF3 synthesis system.
[0072] In one embodiment, intermediate PtCl2(PF3)2 was isolated from the reaction of PtCl2 and PF3 in hexadecane and its identity was confirmed by analysis. PtCl2(PF3)2 was further reacted with copper and PF3 under conditions disclosed in item 5 of Table 1 to produce Pt(PF3)4.
[0073] PF3, PtCl2, PtCl2(PF3) x Anhydrous solvents must be used in the synthesis of Pt(PF3)4 because (x=1, 2) and Pt(PF3)4 react with moisture. The reaction with moisture results in by-products such as HCl, HF, and / or phosphorus oxofluorides, fluorophosphoric acids, which contaminate the product Pt(PF3)4. For example, when Pt(PF3)4 is placed in any glass container, HF can form SiF4. To prevent the formation of contaminants, commercially available solvents can be dried by contact with a desiccant.
[0074] FIG. 2a is a flow chart of the disclosed Pt(Hal)2-M-PF3 synthesis process for the synthesis of Pt(PF3)4, starting with Pt(Hal)2 (Hal=F, Cl, Br or I). The starting materials include Pt(Hal)2 (Hal=F, Cl, Br or I) and metal powder (M) and PF3. At reaction temperatures ranging from 20 to 180° C., Pt(Hal)2 (Hal=F, Cl, Br or I) and metal powder may not be soluble. For example, PtCl2 is not soluble at reaction temperatures ranging from 20 to 180° C. First, in step 202, a suspension of starting materials Pt(Hal)2 (Hal=F, Cl, Br or I) and metal powder is formed in an anhydrous solvent by dispersing Pt(Hal)2 (Hal=F, Cl, Br or I) and metal powder in the anhydrous solvent. Then, an excess of PF3 gas is introduced into the suspension of Pt(Hal)2 (Hal=F, Cl, Br or I) and a metal powder, where preferably Hal=Cl and then Pt(Hal)2 is PtCl2. Preferably, the metal powder is a Cu powder.
[0075] Pt(Hal)2 (Hal=F, Cl, Br or I) is anhydrous and suspended in an anhydrous solvent. The solvent is dried with a desiccant to form an anhydrous solvent, which is used to mix with the starting materials, anhydrous Pt(Hal)2 and metal powders. The solvent or anhydrous solvent has the general formula (C n H 2n+1 )2O and H3C(O(CH2)2) n Oxyhydrocarbon solvents having the general formula (C n H 2n+1 ) x C6H 6-x (x≧1, n≧1), or an arene solvent having the general formula C n H 2n+2 The anhydrous solvent may be a hydrocarbon solvent such as an alkane solvent having n≧1. The anhydrous solvent suitable for use in the method of the present disclosure may be a dry alkane solvent selected from decane, di-, tri-, tetra, penta- and hexadecane, etc.; a dry arene solvent selected from xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene, etc.; a dry ether solvent selected from dibutyl ether, dihexyl ether, dioctyl ether, dimethyl ether of diethylene glycol, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, etc.; or an arene solvent selected from xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene, etc.; or a combination thereof. The ether solvent is preferably dibutyl ether, dihexyl ether, dioctyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether. The arene solvent is preferably xylene, mesitylene, cymene, pentylbenzene, diisopropylbenzene, diisobutylbenzene. The alkane solvent is preferably di-, tri-, tetra-, penta-, and hexadecane, as well as mixtures of alkanes known as mineral oils. The anhydrous solvent used in the process of the present disclosure may be xylene or hexadecane.
[0076] In some embodiments, the solvent or anhydrous solvent can be xylene or hexadecane. The drying agent can be 3 Å or 4 Å molecular sieves. With Pt(Hal)2 (Hal=F, Cl, Br or I) in anhydrous solvent, metal powder and excess PF3, the soluble reaction intermediate Pt(Hal)2(PF3) x (x=1, 2; Hal=F, Cl, Br or I) can be formed in step 204. As used herein, the solvent or anhydrous solvent is a soluble reaction intermediate Pt(Hal)2(PF3) x (x=1, 2; Hal=F, Cl, Br or I) must be soluble in PF3. Here, an excess of PF3 can be added to a suspension of Pt(Hal)2 (Hal=F, Cl, Br or I) and metal powders. Thus, the soluble reaction intermediate Pt(Hal)2(PF3) x (x=1, 2; Hal=F, Cl, Br or I) can be formed from Pt(Hal)2 (Hal=F, Cl, Br or I) and excess PF3 at temperatures, for example, 80° C. to 130° C. and low pressures, for example, 20 psig to 300 psig. The solvent is the intermediate Pt(Hal)2(PF3) x (x=1, 2; Hal=F, Cl, Br or I) is selected to be capable of dissolving Pt(Hal)2 (Hal=F, Cl, Br or I) so that Pt(Hal)2 (Hal=F, Cl, Br or I) reacts with an excess of PF3 to form the reaction intermediate Pt(Hal)2(PF3) x (x=1, 2; Hal=F, Cl, Br or I) in an anhydrous solvent. In step 206, the reaction intermediate Pt(Hal)2(PF3) xThe solution of (x=1, 2; Hal=F, Cl, Br or I) can react with metal powder and PF3 gas (e.g., when Hal=Cl, the metal powder is Cu powder, PtCl2(PF3)2+2Cu+3PF3=2CuCl+Pt(PF3)4) to form Pt(PF3)4. In this step, an excess of PF3 is used. Then, in step 208, the produced Pt(PF3)4 is separated and purified from unreacted starting materials, solvents, and reaction by-products such as copper halides (e.g., CuCl, CuCl2) and their complexes with PF3. As shown in FIG. 1, the separation and purification steps can be performed in a pre-evacuated trap and / or a metal trap to remove the remaining PF3 and solvents and reaction by-products. The remaining PF3 can be recycled for use as starting material. The metal trap can be made of metal, such as stainless steel, carbon steel, and stainless steel 316 alloy. The purified product Pt(PF3)4 is then stored in a metal ampoule or vessel or container in step 210. The storage metal ampoule or vessel or container can be made of metal, such as stainless steel, carbon steel, and stainless steel alloy 316. Alternatively, the storage ampoule or vessel or container can be made of plastic. The inner surface of the ampoule or vessel or container can be passivated with PF3 or electropolished.
[0077] In the method of the present disclosure, PF3, PtCl2, PtCl2(PF3) xSince (x=1, 2) and Pt(PF3)4 react with moisture, anhydrous solvents must be used for the synthesis of Pt(PF3)4. To prevent the formation of contaminants, the commercially available solvents can be dried by contact with a desiccant selected from 3 Å or 4 Å molecular sieves or activated alumina. The solvent drying process can be achieved by contacting the solvent and the desiccant, which can be achieved in a static or flow process. Prior to the drying step, the commercially available solvents may be degassed by passing an inert gas through them or by applying a vacuum-inert gas cycle, where the vacuum is in the range of 0.1 Torr to 100 Torr, preferably 0.5 to 10 Torr, and the inert gas is selected from N2, Ar or He, which contain less than 1 ppm oxygen and moisture. Alternatively, the commercially available solvents are dried with a desiccant without degassing.
[0078] The disclosed synthesis method provides a practical / scalable synthesis method of Pt(PF3)4 by adjusting and optimizing the reaction conditions to favor the product Pt(PF3)4 in high yield and with minimal impact from side reactions. The disclosed synthesis method can be carried out in standard high pressure reactors, such as Parr Instrument Company reactors Series 4520, 4530, 4540, 4540 (rated at 1900-5000 psig); pressure rated glass reactors, such as Parr Instrument Company Series 5100 glass reactors (rated at 150 psig); or Buechiglas laboratory and test pressure reactors equipped with standard agitators and heaters.
[0079] In some embodiments, the disclosed synthetic methods for the synthesis, purification and storage of Pt(PF3)4 may include the following steps: a) drying the solvent; b) dispersing a platinum compound having the general formula Pt(Hal)2 (Hal=Cl, Br, I), such as PtCl2, and a metal powder having a defined particle size, such as copper metal powder, in a dry or anhydrous solvent in a flow reactor to form a mixture or suspension of Pt(Hal)2 (Hal=Cl, Br, I) and copper metal powder; c) adding an excess amount of PF3 to the mixture or suspension; d) stirring the reaction mixture formed in step c) at the required temperature and required PF3 pressure (i.e., low PF3 pressure) that results in the following reaction and products: a. PtCl2(PF3) x Formation of (x=1, 2); b. PtCl2(PF3) x in a dry solvent; and c. PtCl2(PF3) x and reaction of PF3 with metallic copper powder to form the product Pt(PF3)4; e) purifying the product Pt(PF3)4 by distilling volatile species from the reaction mixture into a separate trap to achieve: i. Separation of unreacted starting materials, by-products, and solvents; and ii. Separation of the product Pt(PF3)4 from unreacted PF3. f) purifying the crude Pt(PF3)4 by distillation; g) recycling unreacted PF3 to step c); and h) storing the purified product Pt(PF3)4 in a metal ampoule or container made of metal such as stainless steel, carbon steel, and stainless steel 316 alloy, and the inner surface of the metal ampoule or container is passivated or electropolished with PF3.
[0080] Alternatively, the disclosed method for synthesizing Pt(PF3)4 with platinum compound Pt(Hal)2 (wherein Hal = F, Cl, Br or I) comprises the following steps: Dispersing a platinum compound Pt(Hal)2, where Hal = F, Cl, Br or I, in an anhydrous solvent to form a suspension of Pt(Hal)2; introducing an excess of PF3 into a suspension of Pt(Hal)2; The reaction of PF3 and Pt(Hal)2 produces the platinum compound Pt(Hal)2(PF3) x forming a solution of in an anhydrous solvent; Metal powder with a certain particle size and an additional excess amount of PF3 were mixed together to form Pt(Hal)2(PF3). x adding to the solution; and Pt(Hal)2(PF3) under reaction conditions x forming Pt(PF3)4 via reaction of PF3 and metal powder.
[0081] In this case, Pt(Hal)2(PF3) x is a reaction intermediate synthesized by suspending excess PF3 and Pt(Hal)2 in an anhydrous solvent. Again, the use of a solvent for the synthesis of Pt(PF3)4 is believed to be novel. To the best of the inventors' knowledge, no other method has been used to synthesize Pt(PF3)4 by suspending Pt(Hal)2(PF3) in a solvent. x It has never been synthesized from any platinum compound containing (Hal=F, Cl, Br or I; x=1, 2).
[0082] Alternatively, the disclosed method for synthesizing Pt(PF) with platinum compound Pt(Hal) (wherein Hal=F, Cl, Br or I) comprises the following steps: providing a metal powder having a particle size; providing PF3 gas; At least one platinum-containing reaction intermediate P(Hal)2(PF3) formed from platinum precursors Pt(Hal)2 and PF3 under reaction conditions such as low pressures of 20 psig to 300 psig and temperatures ranging from 80°C to 130°C. x (Hal=F, Cl, Br or I; x=1, 2) in an anhydrous solvent capable of dissolving Pt(PF3)4 from metal powder, PF3 and a platinum compound Pt(Hal)2 (wherein Hal=F, Cl, Br or I); and Purifying and storing Pt(PF3)4 in devices and ampoules made from metal or plastic under air- and moisture-free conditions.
[0083] Alternatively, the disclosed method for synthesizing Pt(PF) with platinum compound Pt(Hal) (wherein Hal=F, Cl, Br or I) comprises the following steps: a) drying the solvent with a desiccant to form an anhydrous solvent; b) Adding a metal powder having a certain particle size, a platinum compound having the general formula Pt(Hal)2 (where Hal = F, Cl, Br or I) and an excess of PF3 to an anhydrous solvent to obtain Pt(Hal)2(PF3) x where x=1, 2, and the anhydrous solvent is Pt(Hal)2(PF3) x A dissolvable step; c) Metal powder, PF3 and Pt(Hal)2(PF3) x in an anhydrous solvent to synthesize Pt(PF3)4; and d) purifying the synthesized Pt(PF3)4 and storing the purified Pt(PF3)4 in devices and ampoules made from metal or plastic, such as stainless steel or plastic, under air- and moisture-free conditions.
[0084] Here, the plastic may be selected from polyethylene, polypropylene, styrene, Teflon, polytetrafluoroethylene (PTFE), perfluoroalkoxyalkane (PFA).
[0085] As mentioned above, the reaction intermediate Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2) is soluble in hydrocarbon solvents and can be isolated and purified. The synthesis of Pt(PF3)4 is carried out by the platinum compound Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2). Figure 2b shows Pt(Hal)2(PF3) x3 is a flow chart of an exemplary process for synthesizing Pt(PF3)4 starting from (x=1, 2; Hal=F, Cl, Br, or I). As shown, in step 302, Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2) solution is Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2) in an anhydrous solvent. Preferably, Hal is Cl and Pt(Hal)2(PF3) x is PtCl2(PF) x Then, in step 304, a metal powder having a certain particle size is mixed with Pt(Hal)2(PF3) x (Hal=F, Cl, Br or I; x=1, 2) is introduced into the solution to form a suspension. Preferably, the metal powder is Cu powder having a certain particle size. Then, an excess of PF3 gas is introduced into the suspension in step 306. Then, Pt(Hal)2(PF3) xPt(PF3)4 is formed by reacting (x=1, 2; Hal=F, Cl, Br or I) with metal powder and PF3 under low pressure in step 308. Excess PF3 is used in this step. Then, in step 310, the produced Pt(PF3)4 is separated and purified from unreacted starting materials, solvents, and reaction by-products such as copper halides (e.g., CuCl, CuCl2) and their complexes with PF3. As shown in FIG. 1, the separation and purification steps can be performed in a pre-evacuated trap and / or a metal trap to remove the remaining PF3 and solvents and reaction by-products. The remaining PF3 can be recycled for use as starting material. The metal trap can be made of metal such as stainless steel, carbon steel, and stainless steel 316 alloy. The purified product Pt(PF3)4 is then stored in a metal ampoule or vessel or container in step 312. The storage metal ampoules or vessels or containers may be made of metals such as stainless steel, carbon steel, and stainless steel alloy 316. Alternatively, the storage ampoules or vessels or containers may be made of plastic. The interior surfaces of the ampoules or vessels or containers may be passivated with PF3 or electropolished.
[0086] Platinum compound Pt(Hal)2(PF3) x The disclosed method for synthesizing Pt(PF3)4 with Hal=F, Cl, Br or I; x=1, 2 comprises the following steps: Pt(Hal)2(PF3) x (Hal = F, Cl, Br or I; x = 1, 2) was dissolved in anhydrous solvent to obtain Pt(Hal)2(PF3). x forming a solution; Metal powder with a certain particle size and an excess amount of PF3 were mixed with Pt(Hal)2(PF3). x adding to the solution; and Pt(Hal)2(PF3) under reaction conditions of low pressure ranging from 20 psig to 300 psig and temperature ranging from 80°C to 130°C x , forming Pt(PF3)4 by reaction of PF3 and metal powder.
[0087] Or the platinum compound Pt(Hal)2(PF3) x The disclosed method for synthesizing Pt(PF3)4 with Hal=F, Cl, Br or I; x=1, 2 comprises the following steps: a) drying the solvent with a desiccant to form an anhydrous solvent; b) Platinum compound Pt(Hal)2(PF3) x (wherein Hal=F, Cl, Br or I; x=1, 2), a metal powder having a certain particle size and an excess amount of PF3 are added to an anhydrous solvent to synthesize Pt(PF3)4, and the anhydrous solvent is Pt(Hal)2(PF3) x and c) purifying the synthesized Pt(PF3)4 and storing the purified Pt(PF3)4 in devices and ampoules made from metals such as stainless steel or plastics under air- and moisture-free conditions.
[0088] Here, the plastic may be selected from polyethylene, polypropylene, styrene, Teflon, polytetrafluoroethylene (PTFE), perfluoroalkoxyalkane (PFA). The metal may be selected from carbon steel, stainless steel, or stainless steel alloy 316. The metal powder may be Cu, Zn, or Al powder, etc.
[0089] The present disclosure also includes the purity of the product Pt(PF3)4 and a storage container for the product Pt(PF3)4. The product Pt(PF3)4 can be stored in a stainless steel and electropolished stainless steel container at room temperature without any change in purity. The disclosed method for the synthesis of Pt(PF3)4 further includes a step of purifying the synthesized Pt(PF3)4: distilling the synthesized Pt(PF3)4 with a metal trap to remove the solvent and by-products to form by-product-free Pt(PF3)4; distilling the by-product-removed Pt(PF3)4 in a metal vessel to remove the solvent and residual PF3 to form purified Pt(PF3)4; and Optionally, recycling the remaining PF3 to the synthesis of Pt(PF3)4. Includes.
[0090] The disclosed method for synthesizing Pt(PF3)4 further includes the step of storing the purified Pt(PF3)4: Storing the purified Pt(PF3)4 in a metal (e.g., stainless steel) container or in a passivated or electropolished metal (e.g., stainless steel) container at room temperature. Includes.
[0091] Here, the purity of purified Pt(PF3)4 stored in a metal container or an inner surface passivated or electropolished metal container can remain constant without change. The containers are made of carbon steel, stainless steel, and stainless steel 316 alloy. The metal container can have an inner surface that is electropolished. Alternatively, Pt(PF3)4 can be stored in a plastic container. The plastic material can be polyethylene, polypropylene, styrene, Teflon, polytetrafluoroethylene (PTFE), perfluoroalkoxyalkane (PFA).
[0092] The metal powders used in the methods of the present disclosure are composed of metals that have a lower electrode potential than platinum, do not interact with or form complexes with PF3 under the reaction conditions, and have an appropriate particle size range that allows them to maintain a powder form during the reaction process.
[0093] Preferably, the metal powder is copper, zinc, aluminum powder, etc. Any metal and its halide that does not interact with and does not form a complex with PF3 under reaction conditions and has an electrode potential lower than platinum (+1.2) can be used herein. For example, Cu (+0.34), Pb (-0.13), Sn (-0.14), Cd (-0.40), Zn (-0.76) and their halides do not interact with and do not form a complex with PF3 under reaction conditions and can be used as the metal powder.
[0094] The following non-limiting examples are provided to further illustrate embodiments of the present invention, however, the examples are not intended to be all inclusive and are not intended to limit the scope of the invention described herein. EXAMPLES
[0095] Experimental Method Reaction mixtures, starting materials, solvents and products may be analyzed by any suitable means, such as gas chromatography, NMR, Raman, FTIR spectroscopy, using portions of the stream or aliquots. All measurements were performed with samples in sealed containers, suitable test tubes or ampoules, completely preventing contact with oxygen and moisture containing atmosphere. High purity liquid nitrogen, nitrogen gas with O2 and water less than 0.1 ppm.
[0096] Reagents: Potassium hexachloroplatinate(IV) (K2PtCl6, Pt assay 40.1±0.7%, CAS: 16921-30-5) was from Colonial Metals, Inc.; platinum(II) chloride (PtCl2, Pt assay 73.3±1.0%, CAS: 10025-65-7) was from Colonial Metals, Inc. Three copper powders were obtained: one from Strem Chemicals Inc. (99.999%) 100 mesh (100 mesh=149 μm); another from Sigma-Aldrich <425 μm, 99.5%; another from Sigma-Aldrich <45 μm, 99.99%. Phosphorus(III) fluoride (PF3, CAS: 7783-55-3) was from Advance Research Chemicals, Inc. Molecular sieves, 3 Å, beads, 4-8 mesh (Sigma-Aldrich) were regenerated at temperatures of 300-350°C in a dry nitrogen stream or at 300-350°C under reduced pressure and operated after regeneration under a nitrogen atmosphere with O2 and water less than 0.5 ppm. The solvents xylene and hexadecane were from Sigma-Aldrich and were degassed and dried over 3 Å molecular sieves. The reactor was filled with platinum compounds and copper powder under a nitrogen atmosphere with O2 and water less than 0.5 ppm.
[0097] Example 1. Synthesis of Pt(PF3)4 with hexadecane solvent in a high pressure reactor. Referring to Table 1 below, the amounts of PtCl2, Cu, and hexadecane used are charged to a Parr Instrument Company reactor (Series 4540, 600 mL, 5000 psig rated) in a glove box. The reactor is removed, connected to a vacuum line, and depressurized to less than 0.3 Torr, and the required amount of PF3 is introduced into the reactor at less than -79°C (Nos. 1-3) or at room temperature (No. 6). The reactor is then warmed to room temperature, stirring is started, and the temperature in the reactor is then increased to 105°C and the reaction mixture is stirred under PF3 pressure. In reaction No. 6, PF3 is added to the reactor in several portions during the reaction to maintain the pressure within the range of 100-200 psig. In all reactions, a drop in pressure is observed at 105°C during the first 6 hours, and then the pressure stabilizes, indicating that the reaction may take approximately 6 hours. The pressure in the reactor was monitored for a few more hours, then the reactor contents were cooled to 35-45°C and a portion of the gas (about 25-35%) was sent to a pre-evacuated trap (0.44 L, stainless steel material) cooled with a dry ice-isopropanol mixture. In reaction number 6, all pressure in the trap was released. The reactor was closed and the trap was maintained for about 10 minutes, then the non-condensable gas was sent to a second trap (6 L, aluminum material) cooled with liquid nitrogen. The transfer lines and valves were warmed by the passing gas if they were cooled below 0°C. After condensing the PF3 portion in the 6L Al trap, a vacuum was applied to the 6L Al trap to bring the pressure in the trap to less than 1 Torr. The operation was repeated until all PF3 and Pt(PF3)4 were cleared from the reactor and collected in two different traps. The trap containing Pt(PF3)4 was then reconnected to another pre-evacuated vessel (0.4 L, electropolished stainless steel). The parent trap containing Pt(PF3)4 was warmed to room temperature while the receiving vessel was cooled with liquid nitrogen and all the Pt(PF3)4 was distilled in the receiving vessel under static vacuum. After distillation, the receiving vessel was warmed to room temperature and the remaining PF3 was released from the scrubber. The yields of Pt(PF3)4 are shown in Table 1 below.
[0098] [Table 1]
[0099] 1 H, 19 The purity of Pt(PF3)4 is >99% in all experiments by F NMR. For example, in reaction 1, 19 F NMR (σCFCl3, ppm): -11.5 (m, J(PF) = 1302 Hz, 99.63%, Pt(PF3)4), -34.4 (d, J(PF) = 1402 Hz, 0.05%, PF3), -81.58 (0.19%, fluorophosphate, unassigned), -92.4 (d, J(PF) = 2035 Hz, 0.12%, POF3). 1 H NMR (σSiMe4, ppm): 0.90 and 1.32 (hexadecane), 13.1 (s, fluorophosphate). 1 H NMR analysis of hexadecane. 0.18 g of purified product was taken from reaction #1 and mixed with 0.77 g of C6D6 containing 0.03% (0.23 mg, 0.0026 mmol) of SiMe4. The solution 1 H NMR (σSiMe4, ppm): 0.00 (s, 97.7 mol.%, SiMe4), 1.32 (2.3 mol.%, hexadecane), 7.16 (s, fluorophosphoric acid, relative intensity not measured for C6D6 as water was not dried). To recalculate mol% to weight%, taking into account that the solution contains 0.23 mg of TMS, the total amount of hexadecane in the Pt(PF3)4 sample is 0.014 mg, which corresponds to 79 ppm in the Pt(PF3)4 from reaction #1.
[0100] Additional trap-to-trap distillation affords Pt(PF3)4 at 99.79% purity. 19 F NMR was measured in a glass ampoule (σCFCl3, ppm): -11.5 (m, J(PF) = 1302 Hz, 99.79%, Pt(PF3)4), -88.20 (d, J(PF) = 975 Hz, 0.19%, (HO)POF2), -92.4 (d, J(PF) = 2035 Hz, 0.01%, POF3) -166.1 (s, 0.02%, SiF4).1 H NMR (σSiMe4, ppm): 0.90 and 1.32 (hexadecane, 28% relative intensity), 12.94 (s, (HO)POF2, 72% relative intensity). The hexadecane resonances were below the detection limit for a solution of 0.07 g sample in 0.78 g C6D6 containing 0.03% SiMe4. The total amount of hexadecane is therefore less than 80 ppm. FTIR. [Liquid Pt(PF3)4 in Golden Gate™ probe, 4 cm resolution. -1 ]:882, 827, 496cm -1 .
[0101] Example 2. Synthesis of Pt(PF3)4 with isolation of PtCl2(PF3)2 and hexadecane solvent. a) PtCl2(PF3) in hexadecane x The composition of (x=1, 2). PtCl2 (1.9 g, 7.1 mmol), hexadecane (15.8 g, 20.4 mL) were charged into a 150 mL pressure glass ampoule (Chemglass Life Sciences, part number CG-1880-31) equipped with a stir bar, thermocouple, and pressure gauge. The ampoule was connected to a vacuum line and a cylinder containing PF3. The ampoule containing the starting material was evacuated to approximately 0.2 Torr to remove the nitrogen, then 35 psig of PF3 was added, and the suspension was heated under stirring. The contents were stirred for 4 hours at a temperature range of 100-120 °C under 20-35 psig of PF3, where PF3 was added in portions when the pressure approached 20 psig. During the reaction, PtCl2, which was initially insoluble in hexadecane, reacted completely with PF3, forming a compound soluble in hexadecane, some of which sublimed as colorless crystals in the cold part of the apparatus. After 4 hours, the heating was stopped, the reaction mixture was cooled to room temperature, the PF3 was condensed back into the cylinder, and a portion of the crystals was separated from the solution and analyzed; a portion of the supernatant solution of hexadecane was also 19 The crystals were analyzed by F NMR. 19F NMR (σCFCl3, ppm): -36.4 (m, J(Pt-F) = 628 Hz, J(PF) = 1320 Hz, PtCl2(PF3)2). 19 F NMR (σCFCl3, ppm): -32.5 (d, J(PF) = 1405 Hz, PF3), -36.4 (m, J(Pt-F) = 622 Hz, J(PF) = 1318 Hz, PtCl2(PF3)2). FTIR of the crystal (pure solid on a Golden Gate™ probe, 4 cm resolution). -1 ):417(sh,w),447(sh,w),461(m),483(s),507(s),518(s),531(m),551(s),901(vs),907(sh),933(vs),961(s),969(w),974(m),985(w) DSC of crystals: 19.0℃ (phase transition), 72.5℃ (phase transition), 118.3℃ (melting point).
[0102] b) PtCl2(PF3) in hexadecane x Synthesis of Pt(PF3)4 from (x=1, 2). The colorless crystals from a) were placed in a supernatant solution of hexane, copper was added (2.22 g, 34.9 mmol), and an ampoule (150 mL HW pressure glass vessel) was connected to a vacuum line and a cylinder containing PF3. The ampoule containing the starting material was briefly evacuated to about 2 Torr to remove the nitrogen, then 40 psig of PF3 was added, and the suspension was heated with stirring at a temperature range of 100-130 °C for 4 hours. The reaction was under 20-40 psig of PF3, where PF3 was added in portions when the pressure approached 20 psig. After 4 hours, heating was stopped, the reaction mixture was cooled to 35 °C, and Pt(PF3)4, PF3, and some of the solvent were condensed in a liquid nitrogen-cooled trap (made of stainless steel) under static vacuum. Pt(PF3)4 was purified from PF3 and remaining hexadecane by trap-to-trap distillation. The yield of Pt(PF3)4 was 1.25 g (32%, low yield due to the use of PtCl2(PF3)2 and a portion of the supernatant solution for analysis in a). 19F NMR (σCFCl3, ppm): -11.5 (m, J(PF) = 1301 Hz, Pt(PF3)4). 1 H NMR (σSiMe4, ppm): 0.23 (t, J=6.1Hz, 71.7mol.%, Me2SiF2), 0.90 and 1.32 (28.3mol.%, hexadecane).
[0103] Example 3. Synthesis of Pt(PF3)4 with hexadecane solvent in a glass ampoule. PtCl2 (8.75 g, 32.9 mmol), Cu (18.25 g, 287.2 mmol), and hexadecane (30.95 g, 40 mL) were charged into an ampoule (150 mL HW pressure glass vessel from Chemglass Life Sciences, part number CG-1880-31) equipped with a stir bar, thermocouple, and pressure gauge. The ampoule was connected to a vacuum line and a cylinder containing PF3. The ampoule containing the starting material was evacuated to approximately 0.2 Torr to remove the nitrogen, then 40 psig of PF3 was added and the contents were heated with stirring. The contents were stirred at a temperature range of 110-120°C under 20-50 psig of PF3 for 5.5 hours, where PF3 was added in portions when the pressure approached 20 psig. During the reaction, crystals of PtCl2(PF3)2 formed and were then consumed, and at the end of the reaction the reaction mixture contained two immiscible liquids. After 5 hours and 30 minutes, the heating was stopped, the reaction mixture was cooled to 41°C, and Pt(PF3)4, PF3, and some of the solvent were condensed in a liquid nitrogen-cooled trap (made of stainless steel) under static vacuum. Pt(PF3)4 was purified from PF3 and remaining hexadecane by trap-to-trap distillation. The yield of Pt(PF3)4 is 79% (14.2 g). The neat sample 19 F NMR (σCFCl3, ppm): -11.5 (m, J(PF) = 1301 Hz, 99.40%, Pt(PF3)4), -34.4 (d, J(PF) = 1402 Hz, 0.36%, PF3), -92.4 (d, J(PF) = 2035 Hz, 0.23%, POF3), -166.0 (s, 0.007%, SiF4). 1H NMR(σSiMe4,ppm):0.23(t,J=6.1Hz,67.4mol.%,Me2SiF2),0.90 and 1.32(6.9mol.%,hexadecane),1.45(d,J=6.1Hz,25.8mol.%,P(O i Pr)3). 1 Determination of organic content by H NMR. The resonance intensities of organic compounds were below the detection limit for a solution of 0.09 g of Pt(PF3)4 sample dissolved in 0.76 g of C6D6 containing 0.03% (0.228 mg, 0.0026 mmol) of SiMe4. Thus, the total amount of organic compounds is less than 80 ppm in Pt(PF3)4.
[0104] Example 4. Synthesis of Pt(PF3)4 in a glass ampoule applying xylene solvent. PtCl2 (2.19 g, 8.2 mmol), Cu (4.69 g, 73.8 mmol), and xylene (16.1 g) were charged into a 150 mL pressure glass ampoule (Chemglass Life Sciences, part number CG-1880-31) equipped with a stir bar, thermocouple, and pressure gauge. The ampoule was connected to a vacuum line and a cylinder containing PF3. The ampoule containing the starting material was briefly evacuated to approximately 3 Torr to remove the nitrogen, then 40 psig of PF3 was added and the contents were heated with stirring. The contents were stirred for 4.5 hours at a temperature range of 100-120°C under 20-40 psig of PF3, where PF3 was added in portions when the pressure approached 20 psig. During the reaction, crystals of PtCl2(PF3)2 formed and were then consumed, and at the end of the reaction, the reaction mixture contained two immiscible liquids. After 4 hours and 30 minutes, the heating was stopped, the reaction mixture was cooled to 38°C, and Pt(PF3)4, PF3, and some of the solvent were condensed in a liquid nitrogen-cooled trap (stainless steel) under static vacuum. Pt(PF3)4 was purified from PF3 and the remaining solvent xylene by trap-to-trap distillation. The yield of Pt(PF3)4 is 95% (4.3 g). 19F NMR (σCFCl3, ppm): -11.5 (m, J(PF) = 1301 Hz, 99.58%, Pt(PF3)4), -34.4 (d, J(PF) = 1402 Hz, 0.39%, PF3), -92.4 (d, J(PF) = 2035 Hz, 0.03%, POF3), -166.0 (s, 0.01%, SiF4). % is based on integration. 1 H NMR (σSiMe4, ppm): 0.12 (t, J = 6.1 Hz, 0.7 mol.%, Me2SiF2), 1.11 (t) and 2.56 (q) (18.8 mol.%, Et-C6H5), 2.05 (s) and 2.14 (s) (79.4 mol.%, xylene), 6.97 (m, aromatic protons), 12.46 (br, 1.0 mol.%, fluorophosphate). 1 Determination of remaining solvent by H NMR: A 0.088 g sample of Pt(PF3)4 was taken and dissolved in 0.80 g of C6D6 containing 0.03% (0.24 mg, 0.0027 mmol) of SiMe4. 1 H NMR (σSiMe4, ppm): 0.00 (s, 6.28 mol.%, SiMe4), 1.07 (t) and 2.39 (q) (18.64 mol.%, Et-C6H5), 2.02 (s, 11.41 mol.%, xylene), 2.14 (s, 63.67 mol.%, xylene), 6.97 (m, aromatic protons). Recalculating mol% to wt%, taking into account that the solution contains 0.24 mg of TMS, the total amount of organic compounds is 4.27 mg, which corresponds to 4.85 wt.% in the 88 mg Pt(PF3)4 sample.
[0105] Example 5. Pt(PF3)4 storage life The shelf life test was carried out at room temperature for 12 weeks. Pt(PF3)4 was obtained by the synthesis described in Examples 3 and 4 and was dissolved in 50 cm 3 The samples were collected in a small sample cylinder made of 316 alloy with a blind cap and an open end, and in a small canister made of electropolished stainless steel with a blind cap (V = 400 cm). 3 ) at room temperature. Before the introduction of Pt(PF3)4, both containers were baked at approximately 150 °C and 30–50 mTorr. 19 F and1 H NMR spectra were taken every two weeks on the original Pt(PF3)4 to determine the Pt(PF3)4 assay and the relative amounts of impurities. 19 F and 1 The shelf life was monitored from H NMR spectra. The results of the shelf life tests are shown in Table 2.
[0106] [Table 2]
[0107] The Pt(PF3)4 assay and relative amount of impurities are similar in all experiments over the 12 week period. The deviation is higher for the 316SS steel ampoules. These results show the stability of Pt(PF3)4 over time. Figure 4 is a graph of Pt(PF3)4 assay and relative amount of impurities over time at room temperature in a 400 mL electropolished stainless steel mini canister. The disclosed Pt(PF3)4 is intended for use as a precursor for Pt-containing films in microelectronic devices or the catalytic industry.
[0108] Comparative Example 1. Synthesis of Pt(PF3)4 starting from K2PtCl6 using recipes from Angew. Chem. Int. Ed. 1965, 4,521 and Russian Patent No. 2478576C2 The synthesis of Pt(PF3)4 according to the recipe from Angew.Chem.Int.Ed.1965,4,521 and Russian Patent No. 2478576C2 is shown in Table 3 below. The experiments are carried out in a commercial high-pressure reactor (Series 4540, 600 mL, 5000 psig rating, with standard impeller in experiments no. 10 and no. 12, and with a U-shaped anchor stirrer designed for efficient stirring of the solids in b) manufactured by Parr Instrument Company. The process according to Russian Patent No. 2478576C2 utilizes pure hydrogen and a drying step after reduction, which requires expensive and highly safe equipment and long time, even if the water can be removed from the system by scaling up. As shown in Table 3, no. 10 was carried out with copper powder Cu of 149 μm size (copper powder was packaged in argon atmosphere by the supplier and used as is). Nos. 11 and 12 were prepared from 425 μm sized copper powder Cu (99.5%, Sigma-Aldrich). The synthesis of Pt(PF3)4 starting from PtCl2 (No. 12, Table 3) according to [Angew. Chem. Int. Ed. 1965, 4, 521] was carried out with Cu (99.5%, Sigma-Aldrich) prepared from 425 μm sized copper powder. Pt(PF3)4 (Nos. 10-12) are formed in low to moderate yields.
[0109] With reference to Table 3, the comparative examples were carried out in a standard commercial equipment, and the starting materials K2PtCl6, PtCl2, Cu were charged in the reactor in a glove box with oxygen and moisture <0.5 ppm. The reactor was sealed, connected to a vacuum line, depressurized to less than 0.2 Torr, cooled to less than -79°C, and the required amount of PF3 was introduced into reactions 10-12 with stirring at low temperature. The reactor was then warmed to room temperature, heated to 105-130°C, and the contents were stirred under PF3 pressure for 24 hours. The reactor contents were then cooled to 35-45°C, and a portion of the gas (about 25-35%) was sent to a pre-depressurized trap (0.44 L, stainless steel material) cooled with a dry ice-isopropanol mixture. The reactor was closed, the trap was maintained for about 10 minutes, and then the non-condensable gas was sent to a second trap (6 L, aluminum material) cooled with liquid nitrogen. The transfer lines and valves were warmed by the passing gas if cooled below 0°C. After condensing the PF3 portion in the 6L Al trap, a vacuum was applied to the 6L Al trap to bring the pressure in the trap to less than 1 Torr. The operation was repeated until all PF3 and Pt(PF3)4 were cleared from the reactor and collected in two different traps. The trap containing Pt(PF3)4 was then reconnected to another pre-vacuumed vessel (50 mL, stainless steel). The parent trap containing Pt(PF3)4 was warmed to room temperature while the receiving vessel was cooled with liquid nitrogen and all Pt(PF3)4 was distilled in the receiving vessel under static vacuum. After distillation, the receiving vessel was warmed to room temperature and the remaining PF3 was released from the scrubber. The yields of Pt(PF3)4 for each experiment showed low to moderate yields, but Russian Patent No. 2478576C2 claimed a yield of 60-95%. The low to moderate yield of Pt(PF3)4 obtained from the recipe of Russian Patent No. 2478576C2 may be due to the lack of solvent. The purity of Pt(PF3)4 is 1 H, 19 F NMR shows >97.9% in all experiments. 19F NMR(σCFCl3,ppm): -11.5(m,J(PF)=1302Hz,97.9%,Pt(PF3)4), -34.4(d,J(PF)=1402Hz,0.2%,PF3), -92.4(d,J(PF)=2035Hz,2.0%,POF3).
[0110] [Table 3]
[0111] Example 6. Synthesis of Pt(PF3)4 starting from K2PtCl6 with hexadecane solvent in a high pressure reactor. K2PtCl6 (79.5 g, 0.16 mol), Cu (120.6 g, 1.9 mol), and hexadecane (100 g) were charged into a reactor (Parr Instrument Company, Series 4540, 600 mL 5000 psig rated) in a glove box. The reactor was removed, connected to a vacuum line, depressurized to 0.3 Torr, cooled to below -79 °C, and 387 g (4.4 mol) of PF3 was introduced into the reactor. The reactor was then warmed to room temperature, stirring was started, the reactor was further warmed to 120 °C, and the contents were stirred under PF3 pressure for 22 h. The reactor contents were then cooled to 35-45 °C, and a portion of the gas (approximately 25-35%) was sent to a pre-depressurized trap (0.44 L, stainless steel material) cooled with a dry ice-isopropanol mixture. The reactor was closed and the trap was maintained for about 10 minutes, then the non-condensable gases were sent to a second trap (6 L, aluminum material) cooled with liquid nitrogen. The transfer lines and valves were warmed by the passing gas if they were cooled below 0°C. After condensing the PF3 portion in the 6L Al trap, a vacuum was applied to the 6L Al trap to bring the pressure in the trap to less than 1 Torr. The operation was repeated until all PF3 and Pt(PF3)4 had disappeared from the reactor and were collected in two different traps. The trap containing Pt(PF3)4 was then reconnected to another pre-evacuated vessel (50 mL, stainless steel). The parent trap containing Pt(PF3)4 was warmed to room temperature, while the receiving vessel was cooled with liquid nitrogen and all the Pt(PF3)4 was distilled in the receiving vessel under static vacuum. After distillation, the receiving vessel was warmed to room temperature and the remaining PF3 was released from the scrubber. The yield of Pt(PF3)4 is 23.2 g, 25.9% from K2PtCl6. See Table 4, which lists the yields of Pt(PF3)4 starting from K2PtCl6 in two reactions, this example and Comparative Example 1 above. Number 13 is from Comparative Example 1 above, and numbers 11 and 14 were the results of this example. Both reactions are at the same temperature and PF3 pressure. 19 Assay of Pt(PF3)4 by integration of the F NMR spectrum is 99.48%. 19F NMR(σCFCl3,ppm): -11.5(m,J(PF)=1302Hz,99.48%,Pt(PF3)4), -34.4(d,J(PF)=1402Hz,0.3%,PF3), -92.4(d,J(PF)=2035Hz,0.2%,POF3).
[0112] [Table 4]
[0113] The reason for the low yields for the use of PtCl2 in Table 3 may be due to inefficient mixing of the components, coverage of the metal by the metal chloride during the reaction, and other factors associated with a reaction starting from two different solids and gases. A solution may be to move from a solid-gas system to a solution-solid system to achieve better mixing of the components and more efficient interaction of the dissolved components in the liquid phase in which the metal powder is suspended. However, solution-solid systems have not been reported so far because it is expected that the solvent would undergo catalytic reactions with the Pt precursor or intermediate.
[0114] Although the subject matter described herein may be described in the context of example implementations for processing one or more computing application functions / operations for a computing application having a user-interactive component, the subject matter is not limited to these particular embodiments. Rather, the techniques described herein may be applied to any suitable type of user-interactive component execution management method, system, platform and / or apparatus.
[0115] It should be understood that many additional changes in the details, materials, steps and arrangements of parts described and illustrated herein to explain the nature of the invention may be made by those skilled in the art within the principles and scope of the invention as set forth in the appended claims. Therefore, the invention is not intended to be limited to the specific embodiments in the examples given above and / or the accompanying drawings.
[0116] Although embodiments of the present invention have been shown and described, modifications thereof may be made by one skilled in the art without departing from the spirit or teachings of the present invention. The embodiments described herein are merely illustrative and not limiting. Many variations and modifications of compositions and methods are possible and are within the scope of the present invention. Accordingly, the scope of protection is not limited to the embodiments described herein, but is limited only by the following claims, which scope is intended to include all equivalents of the subject matter of the claims. [Explanation of symbols]
[0117] 11 Cu powder 12 PtCl2 13 PF3 14 Solvents 15 Container 16 Reactor 17 Pre-depressurized trap 18 Pt(PF3)4 Trap 19 Metal ampoules 20 PF3 Trap 101 Line 102 Dripping funnel 103 Addition Line 104 Drying Process 105 Line 106 Line 107 Line 108 Bypass 109 Packaging 110 Line
Claims
1. Pt(PF 3 ) 4 (CAS No. 19529-53-4), comprising the steps of: General formula Pt(Hal) 2 (PF 3 ) x A platinum compound having the formula Pt(Hal) was dissolved in an anhydrous solvent to give 2 (PF 3 ) x forming a solution where Hal=F, Cl, Br or I, x=1, 2; Metal powder and excess PF 3 Pt(Hal) 2 (PF 3 ) x adding to the solution; and Pt(Hal) under reaction conditions 2 (PF 3 ) x , P.F. 3 and Pt(PF 3 ) 4 Step of forming A method comprising:
2. The method of claim 1, wherein the reaction conditions include a reaction temperature in the range of approximately 30 to 200°C.
3. 10. The method of claim 1, wherein the reaction conditions include a reaction pressure of less than about 300 psig.
4. 10. The method of claim 1, wherein the anhydrous solvent has a boiling point above 150°C.
5. The method of claim 1 , wherein the metal powder is copper, zinc or aluminum powder.
6. The method of claim 1, wherein the metal powder has a particle size in the range of 200 to 900 microns.
7. The platinum compound Pt(Hal) 2 (PF 3 ) x(Hal=F, Cl, Br or I; x=1, 2), said synthesizing step comprising: General formula Pt(Hal) 2 A platinum precursor having the formula: 2 forming a suspension of Hal = F, Cl, Br or I; P.F. 3 Pt(Hal) 2 into said suspension; and The platinum compound Pt(Hal) 2 (PF 3 ) x (Hal=F, Cl, Br or I; x=1, 2) in the anhydrous solvent, 3 and Pt(Hal) 2 2. The method of claim 1 , comprising forming via reaction of
8. The platinum precursor Pt(Hal) 2 The method of claim 7, wherein is anhydrous.
9. The platinum compound Pt(Hal) 2 (PF 3 ) x 9. The method of any one of claims 1 to 8, wherein (Hal = F, Cl, Br or I, x = 1, 2) is anhydrous.
10. The anhydrous solvent is represented by the general formula (C n H 2n+1 ) 2 O(n≧1) and H 3 C(O(CH 2 ) 2 ) n OCH 3 (n≧1), an oxyhydrocarbon solvent having the general formula (C n H 2n+1 ) x C 6 H 6-x (x≧1, n≧1) or an arene solvent having the general formula C n H 2n+2 The method according to any one of claims 1 to 8, wherein the hydrocarbon solvent is selected from alkane solvents having n > 1.
11. Pt(PF 3 ) 4 The method according to any one of claims 1 to 8, wherein the yield of is in the range of approximately 70 to 99.9%.
12. Pt(PF 3 ) 4 The method according to any one of claims 1 to 8, wherein the purity of is approximately 90 to 99.9% by weight after purification.
13. Pt(PF 3 ) 4 (CAS No. 19529-53-4), comprising the steps of: a) Platinum precursor Pt(Hal) 2 forming a suspension of Hal = F, Cl, Br or I and metal powder in an anhydrous solvent; b) Excessive amount of PF 3 Pt(Hal) 2 and introducing said metal powder into said suspension; c) PF under low pressure conditions 3 and Pt(Hal) 2 (wherein Hal=F, Cl, Br or I; x=1, 2), to produce a soluble reaction intermediate Pt(Hal) 2 (PF 3 ) x forming d) Pt(Hal) in said anhydrous solvent 2 (PF 3 ) x , the metal powder and PF 3 The reaction of Pt(PF 3 ) 4 forming e) In a metal trap, Pt(PF 3 ) 4 under air- and moisture-free conditions; and f) The purified Pt(PF 3 ) 4 storing the mixture in said metal container under said air and moisture free conditions. The method includes:
14. The platinum precursor Pt(Hal) 2 is anhydrous PtCl 2 The method of claim 13, wherein
15. 14. The method of claim 13, wherein the anhydrous solvent has a boiling point above 150°C.
16. The process according to any one of claims 13 to 15, wherein the reaction temperature is in the range of approximately 30 to 200°C.
17. The method of any one of claims 13 to 15, wherein the low pressure condition is a pressure of less than about 300 psig.
18. Pt(PF 3 ) 4 The method according to any one of claims 13 to 15, wherein the purity of is approximately 90 to 99.9% by weight after purification.
19. Pt(PF 3 ) 4 (CAS No. 19529-53-4), comprising the steps of: a) the platinum precursor Pt(Cl) in an anhydrous solvent selected from xylene or hexadecane 2 forming a suspension of b) Excessive amount of PF 3 Pt(Cl) 2 to the suspension to obtain PF 3 and Pt(Cl) 2 By the reaction of Pt(Cl) 2 (PF 3 ) x forming a solution of (x=1, 2) in said anhydrous solvent; c) Copper powder was dissolved in Pt(Cl) 2 (PF 3 ) x (x=1, 2) to said solution; d) The copper powder, PF 3 and Pt(Cl) 2 (PF 3 ) xThe reaction produces a low PF in the range of 20 to 300 psig in the anhydrous solvent. 3 Pt(PF) at pressure and reaction temperature in the range of 30 to 200°C. 3 ) 4 forming e) Pt(PF) in a stainless steel trap 3 ) 4 under air- and moisture-free conditions; and f) The purified Pt(PF 3 ) 4 storing the mixture in the stainless steel container under the air and moisture free conditions, the interior surface of the container being electropolished or having a PF 3 Steps passivated with A method comprising:
20. The method of claim 19, wherein the copper powder has a particle size in the range of 200 to 900 microns.
Citation Information
Patent Citations
Purification of metals from mixtures thereof
US20040093986A1
A method for depositing a ruthenium-containing film on a substrate by a cyclical deposition process