Manufacturing method of pillar garnish
The multi-part injection mold method for pillar garnishes addresses sink marks by directing molten polymer away from the main body surface and trapping low-fluidity material, ensuring high-quality appearance.
Patent Information
- Application Number
- JP2021147278
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-09-10
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2041-09-10
AI Technical Summary
The existing method for manufacturing pillar garnishes results in sink marks on the surface due to the softening and contraction of the garnish main body edge during the molding process, leading to a deterioration in appearance quality.
A method involving a multi-part injection mold with a communication channel cavity that directs molten elastic polymer material away from the main body's contact surface, allowing it to fill the cushion portion indirectly, reducing injection pressure and heat impact, and incorporating a protrusion to minimize cushion part size and a mass cavity to trap low-fluidity material.
Prevents sink marks on the main body surface by reducing injection pressure and heat impact, and traps low-fluidity material, thereby maintaining the appearance quality of the pillar garnish.
Smart Images

Figure 0007554723000004 
Figure 0007554723000005 
Figure 0007554723000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a pillar garnish in which a long main body and a cushion portion provided along the edge of the main body are integrated together. In general, a pillar garnish is a long member that is attached to the gap between the outer periphery of a vehicle window panel and the pillar portion, and is interposed between them to ensure functions such as decoration and waterproofing. [Background technology]
[0002] Patent Document 1 relates to a composite molded product (pillar garnish as an example) and a manufacturing method thereof. According to the explanation in paragraph 0052 and figures 13 and 14 of the document, after the garnish main body 32 is positioned and held in the fixed mold 71 and the movable mold 91 is closed, the heated and molten elastic polymer material is injected from the injection gate 80 and flows into the molding cavity 125 through the injection passage 85. Then, "at this time, the flow pressure of the elastic polymer material flowing into the molding cavity 125 through the injection passage 85 presses the edge 55 of the garnish main body 32 against the concave mold surface 96a of the movable mold 91 to make them adhere to each other" (second sentence of paragraph 0052), and as a result, the effect of "the surface 33 of the garnish main body 32 adheres to the mold surface 96a of the main mold part 96, no gap is generated between them, and no burrs are generated" (second sentence of paragraph 0054) is obtained. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2007-069517 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the technology of Patent Document 1, when the flow pressure of the elastic polymer material presses the edge 55 of the garnish main body 32 against the concave surface 96a of the movable die 91, the heat of the molten elastic polymer material softens the edge 55 of the garnish main body 32. Then, after the cushion portion 65 is fused and integrated with the edge of the garnish main body 32, the softened edge 55 of the garnish main body 32 may be pulled toward the cushion portion 65 in the process of the cushion portion 65 solidifying and shrinking. As a result, sink marks (deformations) may occur on the surface 33 of the garnish main body 32, deteriorating the appearance quality.
[0005] An object of the present invention is to provide a method for manufacturing a pillar garnish which enables the manufacture of a pillar garnish while preventing a deterioration in the appearance quality of the main body portion when molding a cushion portion on the main body portion of the pillar garnish. [Means for solving the problem]
[0006] The invention of claim 1 is a method for manufacturing a pillar garnish having an elongated main body portion and a cushion portion made of an elastic polymer material having a lower hardness than the main body portion, the method comprising the steps of: a pillar garnish main body preparation step of preparing a long main body having a head portion and a leg portion protruding from a rear surface of the head portion; an injection molding die preparation step of preparing an injection molding die that can be opened and closed for molding a cushion portion, the injection molding die having at least a first molding die and a second molding die that are relatively movable, and a third molding die that can slide in a direction intersecting the direction of relative movement of the first and second molding dies, the third molding die having an abutment surface that abuts against a portion located on the back surface side of the head of the main body portion, and a cavity for a communication flow path that is located in an internal position away from the abutment surface and extends in a direction intersecting the sliding direction of the third molding die; placing the elongated body portion in an open injection mold; A mold closing process for closing the injection mold, in which the injection mold is closed, an injection cavity adjacent to the leg of the body; and A cavity for a cushion portion defined between a part of the main body portion and a molding surface of the injection molding die. and a mold closing step in which the cavity for the injection passage and the cavity for the cushion portion are connected by a cavity for a communication passage of the third molding die. an injection step of injecting a heated and molten elastic polymer material into the injection passage cavity after the mold closing step; Equipped with This is a manufacturing method for a pillar garnish, characterized in that in the injection process, an elastic polymer material is filled from the injection flow path cavity through the communicating flow path cavity into the cushion portion cavity, thereby forming a cushion portion that is integrally joined to the main body portion along the longitudinal direction.
[0007] The present invention has the following effects. That is, the molten elastic polymer material injected and supplied to the injection passage cavity is supplied to the cushion portion cavity through the communicating passage cavity located in an internal position away from the contact surface of the third mold. Therefore, compared to a case where the communicating passage cavity does not exist and the molten elastic polymer material is directly filled from the injection passage cavity to the cushion portion cavity, the injection pressure and heat of the elastic polymer material acting on the back surface of the head of the main body portion set in the injection mold are smaller, and as a result, it is possible to prevent or suppress the occurrence of sink marks on the front surface side of the head of the main body portion. Furthermore, according to the present invention, the size (particularly the thickness) of the cavity for the cushion portion can be designed to be smaller than when the cavity for the injection passage and the cavity for the cushion portion are continuous (directly connected), and the amount of shrinkage when the elastic polymer material solidifies and shrinks can be reduced, thereby preventing or suppressing the occurrence of sink marks on the surface side of the head of the main body portion. Therefore, according to the present invention, it is possible to prevent a decrease in the appearance quality of the pillar garnish main body portion.
[0008] The invention of claim 2 is a manufacturing method of the pillar garnish according to claim 1, The elongated main body further has a protruding portion that faces a back surface of the head portion and protrudes in a width direction of the head portion, In the mold closing process, the protrusion of the main body portion is positioned between the cavity for the injection flow path and the back surface of the head, thereby forming a cavity for the cushion portion between the protrusion and the back surface of the head.
[0009] According to the invention of claim 2, in addition to the effects of the invention of claim 1, the following effect is further achieved. That is, since the main body of the pillar garnish faces the back surface of the head and has a protruding portion that protrudes in the width direction of the head, the cavity for the cushion portion formed in the injection molding die when the die is closed is limited to the area between the protruding portion and the back surface of the head. As a result, the size (especially the thickness) of the cavity for the cushion portion is reduced, and it is possible to prevent or suppress the occurrence of sink marks on the front surface side of the head of the main body.
[0010] The invention of claim 3 is characterized in that, in the manufacturing method of a pillar garnish described in claim 1 or 2, in the mold closing process, a cavity for a block portion is further formed between the cavity for the injection flow path and the cavity for the cushion portion for capturing and sealing a relatively cooled portion of the elastic polymer material.
[0011] According to the invention of claim 3, in addition to the effects of the invention of claim 1 or 2, the following effect is further achieved. That is, the molten elastic polymer material is supplied from the injection passage cavity to the cushion portion cavity via the block portion cavity. This makes it possible to capture and seal in the block portion cavity a portion of the elastic polymer material that has cooled relatively and has reduced fluidity and that adheres or remains near the nozzle of the hot runner. This makes it possible to prevent the elastic polymer material with reduced fluidity from entering the cushion portion cavity, thereby avoiding poor appearance of the cushion portion.
[0012] The invention of claim 4 is a manufacturing method for a pillar garnish described in any one of claims 1 to 3, further comprising a mold opening process in which, after the injection process, the injection molding mold is opened and the pillar garnish molded product obtained by integrally joining the cushion portion to the main body portion is removed from the injection molding mold, and is characterized in that when the third molding mold is slid away from the first and second molding molds during the mold opening, the communicating portion formed by the elastic polymer material filled in the cavity for the communicating flow path of the third molding mold is broken.
[0013] According to the invention of claim 4, in addition to the effects of the inventions of claims 1 to 3, the following effect is further achieved: When the third mold slides during mold opening, the communicating portion formed by the elastic polymer material filled in the communicating flow passage cavity is broken, making it easier to remove the pillar garnish molded product from the injection molding mold.
[0014] The invention of claim 5 is characterized in that, in the manufacturing method of a pillar garnish described in claim 4, the cavity for the communicating flow passage has a narrowest portion where the cross-sectional area is smallest, and the communicating portion formed by the cavity for the communicating flow passage has a narrowest portion corresponding to the narrowest portion.
[0015] According to the invention of claim 5, in addition to the effects of the invention of claim 4, the following effect is further achieved. That is, the communicating passage cavity of the third mold is provided with a narrowest part having a minimum cross-sectional area, so that the communicating passage cavity formed by the communicating passage cavity has a narrowest part corresponding to the narrowest part. In such a communicating passage, the narrowest part corresponding to the narrowest part is the weakest point in terms of mechanical strength, so that in the breaking process of the communicating passage, it is possible to cause a position-specific break at the narrowest part, and it is possible to improve the controllability or selectivity of the break position. Effect of the Invention
[0016] According to the pillar garnish manufacturing method of the present invention, when molding a cushion portion on the main body portion of the pillar garnish, the pillar garnish can be manufactured while preventing deterioration in the appearance quality of the main body portion. [Brief description of the drawings]
[0017] [Figure 1] FIG. 4 is a perspective view showing a state in which the pillar garnish is attached to the vehicle body. [Diagram 2] A diagram showing the back side of the pillar garnish. [Diagram 3] Schematic cross-sectional view of the pillar garnish taken along line AA in Figure 2. [Figure 4] 3 is an enlarged perspective view showing a portion surrounded by an imaginary circle B in FIG. 2. [Diagram 5] 5 is a schematic cross-sectional view taken at a position corresponding to cross section CC in FIG. 4, showing a state in which the pillar garnish body is set in an injection molding die and then the die is closed. [Figure 6] 5 is a schematic cross-sectional view taken at a position corresponding to cross section DD in FIG. 4, showing the pillar garnish body set in the injection molding die and then closed. FIG. [Figure 7] FIG. 5 is a schematic cross-sectional view taken at a position corresponding to cross section DD in FIG. 4, showing a state in which the injection mold is being opened after injection molding. [Figure 8] 3A and 3B show cross sections of a pillar garnish obtained by injection molding, in which (A) is a schematic cross-sectional view showing a state in which a communicating portion remains, and (B) is a schematic cross-sectional view showing a state in which the communicating portion has been removed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0019] FIG. 1 is a view of a part of a cabin (passenger compartment) of a general passenger vehicle, seen from an oblique front. As shown in FIG. 1, front pillars 4 (only the left front pillar is shown) are provided on both the left and right sides of the vehicle 1, which extend in an inclined manner from the front end of a roof panel 2 to the rear end edge of a bonnet 3. A front window glass 5 (hereinafter referred to as a "window plate") is provided between the left and right front pillars 4 on the front side of the cabin of the vehicle 1. A pillar garnish 6 is attached to fill any gap that may occur between the outer periphery of the window plate 5 and the front pillar 4. The pillar garnish 6 of this embodiment is a long resin member that is interposed between the front pillar 4 and the window plate 5 to ensure decorative functions, waterproof functions, and other functions.
[0020] As shown in Figures 1 and 2, the pillar garnish 6 comprises a long pillar garnish main body 10 (hereinafter simply referred to as the "main body") that extends roughly along the front pillar 4, and a plurality of cushion portions (31-34) integrated with the main body 10.
[0021] As shown in Figure 3, the main body 10 has a hollow portion 11 extending longitudinally of the main body at the center of the main body, a head 12 located on the exterior side of the main body and exposed to the exterior of the vehicle, and a leg portion 13 protruding from the back side of the head toward the interior side of the vehicle.
[0022] The main body 10 is molded, for example, by gas-assisted injection molding, in which a polymer material for molding the main body is injected into a cavity of an injection mold (not shown) to fill the cavity and a gas (e.g., nitrogen gas) for forming a hollow portion is injected, using a full shot method or a short shot method. In other words, the hollow portion 11 is a remnant of a gas channel in gas-assisted injection molding. In addition, a polymer material that is more rigid and hard than the cushion portion is suitable as a polymer material for molding the main body. Examples of polymer materials that can be used for the main body 10 include thermoplastic synthetic resins such as acrylonitrile-butadiene-styrene resin (ABS resin), acrylonitrile-ethylene-propylene-styrene resin (AES resin), rigid or semi-rigid polyvinyl chloride resin (rigid PVC resin), polycarbonate resin (PC resin), polypropylene resin (PP resin), polyethylene resin (PE resin), polystyrene resin (PS resin), polyamide resin (PA resin), and polymethylmethacrylate resin (PMMA resin).
[0023] The head portion 12 is the portion that is disposed on the outermost side of the vehicle when the pillar garnish 6 is attached to the vehicle body, and that covers the gap that inevitably occurs between the outer periphery of the window panel 5 and the front pillar 4. The surface 12a of the head portion 12 provides the decorative surface (design surface) of the pillar garnish 6 (see FIG. 3).
[0024] The leg portion 13 serves as a mounting portion when the main body portion 10 is mounted on the vehicle body, and as a reinforcing rib that enhances the mechanical strength of the main body portion 10. As shown in Fig. 2, the leg portion 13 as a reinforcing rib has a rib shape and extends intermittently generally along the longitudinal direction of the main body portion 10, but extends along a partially meandering path to avoid or detour around the chunks 15 (described later) provided in various places on the back surface of the main body portion 10. In this application, the meandering rib portion that avoids each of the chunks 15 on the back surface of the main body portion is referred to as an "avoidance rib 14."
[0025] As shown in Fig. 6, the main body 10 further has a protrusion 20. This protrusion 20 is located near the base of the avoidance rib 14 that is part of the leg 13 at a specific position along the longitudinal direction of the main body 10, and is provided so as to face the back surface of the head 12 and protrude in the width direction of the head (to the left in the width direction in Fig. 6).
[0026] As shown in FIG. 2, in the pillar garnish 6, the cushion portion integrated with the main body portion 10 is composed of a first cushion portion 31 and a second cushion portion 32, which are approximately the same length as the main body portion and located on both the left and right sides of the main body portion, an upper end cushion portion 33 located at the upper end of the main body portion, and a lower end cushion portion 34 located at the lower end of the main body portion. When the pillar garnish 6 is attached to the vehicle body, the first cushion portion 31 contacts especially the window plate 5 and functions as a waterproof seal portion, and the second cushion portion 32 contacts especially the front pillar 4 and functions as a waterproof seal portion. In the main body portion 10, the portion to which the first cushion portion 31 is integrally joined is referred to as the "first portion 21" (see FIG. 3), and the portion to which the second cushion portion 32 is integrally joined is referred to as the "second portion 22" (see FIG. 3).
[0027] As the polymer material for molding the cushion portion, an elastic polymer material that has lower hardness and flexibility than the polymer material for molding the main body portion is suitable. Examples of the elastic polymer material that can be used for the cushion portion (31-34) include thermoplastic synthetic resins such as olefin-based thermoplastic elastomer (TPO), styrene-based thermoplastic elastomer (SBC), and soft PVC resin, and rubber. Note that the elastic polymer material for the cushion portion (31-34) is preferably compatible with the polymer material for the main body portion 10.
[0028] FIG. 4 is an enlarged perspective view of the area surrounded by the imaginary circle B in FIG. 2, that is, the block 15 and the vicinity of the meandering avoidance rib 14 to avoid it. As shown in FIG. 4, the block 15 is a substantially rectangular parallelepiped part extending along the longitudinal direction of the main body 10 on the back surface of the main body 10. Near one end of the block 15, an injection flow path 16 is provided, which stands substantially vertically. The injection flow path 16 refers to a fleshy part formed by a polymer material filling the injection flow path cavity 50 (see FIG. 5) connected to the injection gate 41a (see FIG. 5). In addition, at the other end opposite to the one end of the block 15 connected to the injection flow path 16, a main trap part 15a is provided, which is located at the innermost part of the block 15 and has a shape that bulges slightly upward.
[0029] Generally, elastic polymer material that has cooled and become less fluid tends to adhere or remain near the nozzle tip of the hot runner 45 (see FIG. 5), and the elastic polymer material with low fluidity may unintentionally enter the target cavity during the next injection, causing molding defects. The lump portion 15 is provided to avoid such inconvenience, and the lump portion 15 (especially the main trap portion 15a located at the innermost part of the lump portion 15) functions as a "cold slug well" for receiving, capturing, and sealing the elastic polymer material that has cooled relatively and become less fluid. The presence of the lump portion 15 and the main trap portion 15a as cold slug wells makes it possible to prevent the elastic polymer material with low fluidity from flowing into the cavities (described later) for molding the first cushion portion 31 and the second cushion portion 32.
[0030] As shown in Fig. 4, the injection flow path 16 is connected to the second cushion portion 32 via a curved, generally columnar communication portion 18. The communication portion 18 refers to a solid portion formed by a polymer material filling a communication flow path cavity 43b (see Fig. 6, explained later) that communicates between the injection flow path cavity 50 (see Fig. 5) and the second cushion portion molding cavity 52 (see Figs. 5 and 6). The tip of the communication portion 18 on the injection flow path 16 side is positioned so as to be connected to the remaining portion of the block portion 15 avoiding the main trap portion 15a. Although not shown, a connecting portion (not shown) is provided between the avoidance rib 14 and the first cushion portion 31 to connect them. This connecting portion refers to a solid portion molded from a polymer material that fills holes or cavities (not shown) that connect the block portion cavity 53 (see Figure 6) and the first cushion portion cavity 51 (see Figures 5 and 6) (for example, holes or cavities set to penetrate the avoidance rib 14 or the fixed mold 41 described later).
[0031] [Manufacturing method of pillar garnish] The pillar garnish 6 as shown in Figures 2 to 4 is manufactured by integrally joining the cushion parts (particularly the first and second cushion parts 31, 32) to the main body part 10 as described above by injection molding. The method for manufacturing the pillar garnish according to this embodiment generally includes a pillar garnish main body part preparation step, an injection mold preparation step, a step of setting the main body part 10 in the injection mold, a mold closing step of closing the injection mold, an injection step after the mold closing step, and a mold opening step of opening the injection mold after the injection step. Each step will be described in order below.
[0032] First, a main body 10 made of a hard polymer material is prepared in advance as described with reference to Figures 2 to 4. The long main body 10 has at least a head 12, a leg 13 (including an avoidance rib 14), and a first portion 21 and a second portion 22 extending along the longitudinal direction of the main body, and is positioned as an insert material in injection molding.
[0033] In this embodiment, an injection mold 40 consisting of at least four molds (i.e., a fixed mold 41, a movable mold 42, a left slide mold 43, and a right slide mold 44) is used as an injection mold (or an injection molding device) that can be opened and closed for molding a cushion part. As shown in Figs. 5 and 6, the fixed mold 41 as a first mold and the movable mold 42 as a second mold are arranged vertically, and the movable mold 42 can approach and move away from the fixed mold 41 (i.e., can move vertically). The left slide mold 43 as a third mold and the right slide mold 44 as a fourth mold are arranged on the left and right of the fixed mold 41 and the movable mold 42 between the fixed mold 41 and the movable mold 42, and each of them can move (slide) in the horizontal direction. Note that Figs. 5 and 6 show a so-called mold closed state (a state in which the four molds 41 to 44 are closest to each other), but in a mold open state (not shown), the four molds 41 to 44 are kept apart from each other.
[0034] 5, the fixed mold 41 has an injection gate 41a extending vertically. The injection gate 41a is connected to a nozzle of a hot runner 45, which is a device for supplying an elastic polymer material in a heated and molten state.
[0035] As shown in FIG. 6, the left sliding die 43 as the third molding die has an abutment surface 43a that can abut against a portion (specifically, the protruding portion 20) located on the back side of the head 12 of the main body 10 when the main body 10 is set in the fixed die 41. Furthermore, the left sliding die 43 has a communication passage cavity 43b that exists in an internal position away from the abutment surface 43a (to the left in the paper surface of FIG. 6). The communication passage cavity 43b extends in a substantially vertical direction (i.e., in a direction intersecting with the sliding direction of the left sliding die 43). Note that the cross-sectional area of the communication passage cavity 43b at each position along its length is not uniform, and the cross-sectional area gradually decreases as it approaches the tip position of the communication passage cavity 43b (the lower end position in FIG. 6, i.e., the end position connected to the second cushion part cavity 52), and the narrowest part where the cross-sectional area is the smallest is set at the tip position.
[0036] After preparation of the main body 10 and the injection mold 40 is completed, the main body 10 is set as an insert material in the injection mold 40 in the mold open state. That is, as shown in Figures 5 and 6, the main body 10 is set (or positioned) in the fixed mold 41 so that the back surface of the main body 10 abuts against the lower surface side of the fixed mold 41.
[0037] Once the setting of the main body 10 in the fixed die 41 is completed, the injection molding die 40 is closed. Specifically, the movable die 42 approaches (moves upward) toward the fixed die 41, and the main body 10 is sandwiched and held from above and below by the fixed die 41 and the movable die 42. At the same time, the left slide die 43 and the right slide die 44 approach (slide horizontally) toward the fixed die 41 and the movable die 42, respectively, and the main body 10 is sandwiched and held from the left and right by these slide dies 43, 44. Then, various cavities are defined and formed inside the closed injection molding die 40, as shown in Figures 5 and 6. Specifically, inside the injection molding die 40, a) An injection passage cavity 50 (FIG. 5) adjacent to a part of the leg portion of the main body 10 (avoidance rib 14); (b) a first cushion portion cavity 51 (FIGS. 5 and 6) defined between the first portion 21 of the main body 10 and the molding die surfaces (41c, 44c) of the fixed die 41 and the right sliding die 44; c) a cavity 52 for a second cushion portion defined between the second portion 22 of the main body portion 10 and the molding surfaces (42c, 43c) of the movable mold 42 and the left slide mold 43 (FIGS. 5 and 6); d) A cavity 53 for a block portion (FIG. 6) which is located between the cavity 50 for the injection passage and the cavity 52 for the second cushion portion and is defined in the middle of the path connecting the two. is formed.
[0038] Incidentally, with the completion of the mold closing, the injection flow path cavity 50 is connected to the second cushion part cavity 52 via the block part cavity 53 and the communicating flow path cavity 43b of the left slide die 43 (see Figs. 5 and 6). Also, when the mold is closed, the protruding part 20 of the main body part 10 is disposed between the injection flow path cavity 50 and the back surface of the head part 12 (see Fig. 5), and the second cushion part cavity 52 is partitioned and formed between the protruding part 20 and the back surface of the head part 12 (see Figs. 5 and 6).
[0039] After the injection mold 40 is closed, the heated elastic polymer material in a molten state is injected from the hot runner 45 through the injection gate 41a into the injection passage cavity 50. Then, after the leading edge of the flowing elastic polymer material reaches and fills the cavity forming the main trap portion 15a of the block cavity 53, the following elastic polymer material is supplied to the first and second cushion portion cavities 51, 52 through the injection passage cavity 50 and the block cavity 53. Specifically, the molten elastic polymer material supplied to the second cushion portion cavity 52 adjacent to the left slide mold 43 reaches the second cushion portion cavity 52 from the hot runner 45 through the injection passage cavity 50, the block cavity 53, and the communicating passage cavity 43b, and fills the cavity 52. In addition, the molten elastic polymer material supplied to the cavity 51 for the first cushion portion adjacent to the right slide mold 44 travels from the hot runner 45 through the cavity 50 for the injection flow path, the cavity 53 for the block portion, and holes and cavities not shown to reach the cavity 51 for the first cushion portion and fill the cavity 51.
[0040] In this embodiment, the elastic polymer material from the hot runner 45 is designed to pass through the block cavity 53 regardless of whether it is heading for the first or second cushion cavity 51, 52. This block cavity 53 is a cavity involved in molding the block 15 and the main trap portion 15a at its innermost position, but is directly connected to the injection passage cavity 50 through a significantly large communication cross-sectional area. For this reason, the elastic polymer material passing through the injection passage cavity 50 tends to fill the block cavity 53 first, and cannot head for the communicating passage cavity 43b or other cavities until after that. Therefore, as described above, most of the elastic polymer material that has cooled relatively and has reduced fluidity (i.e., the elastic polymer material that has adhered or stayed near the nozzle tip of the hot runner) is captured in the lump cavity 53, and as a result, is enclosed in the lump 15 molded in the lump cavity 53 (particularly the main trap portion 15a molded in the innermost region of the lump cavity 53). Such a cold slug trapping action by the lump cavity 53 prevents the low-fluidity elastic polymer material from flowing into the first cushion cavity 51 and the second cushion cavity 52. In other words, only the high-fluidity elastic polymer material following the low-fluidity elastic polymer material is supplied to the first and second cushion cavity 51, 52, so that molding defects in each cushion cavity 51, 52 (and thus poor appearance of each cushion portion) can be avoided.
[0041] As a result of supplying the elastic polymer material to each cavity from the injection gate 41a, each part made of the elastic polymer material is molded in a state in which it is directly or indirectly integrated with the main body 10, as described below. That is, the first cushion part 31 integrally joined to the first part 21 of the main body 10 is molded by the elastic polymer material filled in the first cushion part cavity 51. The second cushion part 32 integrally joined to the second part 22 of the main body 10 is molded by the elastic polymer material filled in the second cushion part cavity 52. The mass part 15 including the main trap part 15a is molded on the back side of the main body 10 by the elastic polymer material filled in the mass part cavity 53. The injection flow path 16 standing upward from the mass part 15 is molded by the elastic polymer material filled in the injection flow path cavity 50. The elastic polymer material filled in the communication passage cavity 43b forms the injection passage 16 and the communication portion 18 that connects the block portion 15 with the second cushion portion 32 (see FIG. 7).
[0042] After the elastic polymer material is injected through the injection gate 41a and filled into each cavity, the injection mold 40 is opened. That is, the movable mold 42 is moved downward and separated from the fixed mold 41, and the left and right slide molds 43, 44 are horizontally slid away from the fixed mold 41.
[0043] Fig. 7 shows a state in the middle of mold opening where only the movable mold 42 is separated from the fixed mold 41. As shown in Fig. 7, by opening the mold, a pillar garnish molded product 6A is obtained as an intermediate product in which the cushion portions (31, 32, 15, 16, 18) are integrally joined to the main body portion 10 in a state where it hangs down from the fixed mold 41.
[0044] Then, in the process of moving the left slide die 43 away from the fixed die 41 from the state shown in FIG. 7, the end position of the communication part 18 is broken (see FIG. 8(A)). Specifically, an end edge 43e (see FIG. 7) of the left slide die surface (molding die surface) at the boundary position between the communication flow path cavity 43b of the left slide die 43 and the second cushion part cavity 52 and adjacent to the boundary acts as a cutter (cutting blade). Therefore, as the left slide die 43 moves leftward (moves in a direction away from the fixed die 41 and the main body part 10), the end edge 43e cuts the connection between the communication part 18 molded in the communication flow path cavity 43b and the second cushion part 32 molded in the second cushion part cavity 52, and the communication part 18 comes out of the communication flow path cavity 43b. By breaking the end portion of the communication portion 18 in this manner, the pillar garnish molded product 6A can be easily removed from the injection molding die 40.
[0045] As already explained, the narrowest part with the smallest cross-sectional area is set at the tip position of the communicating passage cavity 43b (the lower end position in Figs. 6 and 7, i.e., the end position connected to the second cushion portion cavity 52), so that the communicating portion 18 formed by the communicating passage cavity 43b also has the thinnest part at the tip position. This thinnest part is the weakest point of mechanical strength. In this respect, in the breaking process of the communicating portion 18 accompanying the left sliding mold 43 moving to the left, the tip position (the thinnest part which is the weakest point) of the communicating portion 18 is cut by the end edge 43e of the left sliding mold 43, so that the communicating portion 18 is very easy to cut or break, and position-specific breaking at the thinnest part can be realized, so that the controllability or selectivity of the breaking position can be improved. Furthermore, since the communicating portion 18 has the thinnest part at the tip position, it is also possible to easily remove the communicating portion 18 from the communicating passage cavity 43b when the left sliding mold 43 is moved to the left.
[0046] After the left and right slide dies 43, 44 have been completely opened, the pillar garnish molding 6A is merely held to the underside of the fixed die 41 based on the adhesion force of the back surface of the main body 10 against the underside of the fixed die 41 and the holding force of a removable holding structure (not shown). Therefore, by pulling the pillar garnish molding 6A downward using manual or automatic force, the molding 6A can be removed from the fixed die 41 and the final product (see Figure 8) can be obtained.
[0047] There is no problem in using the pillar garnish 6 as shown in Figure 8(A) as the final product, but since the communicating portion 18 does not have any particular function in itself after injection molding, the pillar garnish 6 with the communicating portion 18 removed, as shown in Figure 8(B), may also be used as the final product.
[0048] [Effects of the embodiment] In this embodiment, the molten elastic polymer material injected and supplied to the injection flow path cavity 50 is supplied to the second cushion portion cavity 52 through the communication flow path cavity 43b located in an internal position away from the contact surface 43a of the left slide die 43. Therefore, compared to a case where the communication flow path cavity 43b does not exist and the molten elastic polymer material is directly filled from the injection flow path cavity 50 to the second cushion portion cavity 52, the injection pressure and heat of the elastic polymer material acting on the back surface of the head 12 of the main body portion 10 set in the injection molding die 40 are smaller, and as a result, the occurrence of sink marks on the front surface side of the head 12 of the main body portion 10 can be prevented or suppressed.
[0049] In addition, since the tip of the communication flow passage cavity 43b is narrow (the cross-sectional area at the tip position is narrow), the injection pressure of the elastic polymer material acting on the main body 10 is small. This contributes to preventing or suppressing sink marks on the surface side of the head 12 of the main body 10.
[0050] According to this embodiment, the size (particularly the thickness) of the cavity 52 for the second cushion portion can be designed to be smaller than when the cavity 50 for the injection flow path and the cavity 52 for the second cushion portion are continuous (directly connected). This in turn reduces the amount of shrinkage that occurs when the elastic polymer material solidifies and shrinks, making it possible to prevent or suppress the occurrence of sink marks on the surface side of the head 12 of the main body portion 10.
[0051] In addition, since the main body 10 of the pillar garnish has the protruding portion 20 that faces the back surface of the head 12 and protrudes in the width direction of the head 12, the cavity 52 for the second cushion portion formed in the injection molding die 40 when the die is closed is limited to the region between the protruding portion 20 and the back surface of the head 12. As a result, the size (especially the thickness) of the cavity 52 for the second cushion portion is reduced, and the occurrence of sink marks on the front surface side of the head 12 of the main body 10 can be prevented or suppressed.
[0052] As described above, from various perspectives, the occurrence of sink marks on the surface side of the head 12 of the main body 10 can be prevented or suppressed, and therefore, according to this embodiment, a decrease in the appearance quality of the pillar garnish main body can be prevented.
[0053] [Modifications] The present invention is not limited to the above-described embodiment, and can be modified and implemented in the following aspects. In the above embodiment, the tip position of the communication part 18 (or the cavity for communication flow path 43b) is the thinnest part, but the base end position (the root on the block part 15 side) of the communication part 18 may be set as the thinnest part. Alternatively, the communication part 18 may be set to have a uniform thickness (or thinness) over its entire length direction. The injection molding die in the above embodiment is of a vertical type in which the injection molding die opens and closes vertically, but it may also be of a horizontal type in which the injection molding die opens and closes horizontally. In addition, in the above embodiment, an injection gate is provided and a configuration surrounded by imaginary circle B is applied, but injection gates may also be provided in other locations to form avoidance ribs 14, and the configuration surrounded by imaginary circle B may be applied to one location or multiple locations in the longitudinal direction. [Explanation of symbols]
[0054] 6 Pillar garnish (final product) 6A Pillar garnish molding (intermediate product) 10 Pillar garnish main body (main body) 12 Head 13 Legs 14 Avoidance rib (part of leg) 18 Communication section 20 Protruding part (part located on the back side of the head of the main body) 21 First part of the main body 22 Second part of the main body 31 First cushion section 32 Second cushion section (cushion section) 40 injection mold 41 Fixed mold (1st mold) 41a Ejection gate 41c mold surface 42 Movable mold (second mold) 42c mold surface 43 Left slide type (third mold) 43a Contact surface 43b Cavity for communicating flow path 44c mold surface 44 Right slide type 44c mold surface 50 Injection passage cavity 51 Cavity for first cushion part 52 Cavity for second cushion part (cavity for cushion part) 53 Cavity for lump
Claims
1. A method for manufacturing a pillar garnish having an elongated main body portion and a cushion portion made of an elastic polymer material having a lower hardness than the main body portion, the method comprising the steps of: a pillar garnish main body preparation step of preparing a long main body having a head portion and a leg portion protruding from a rear surface of the head portion; an injection molding die preparation step of preparing an injection molding die that can be opened and closed for molding a cushion portion, the injection molding die having at least a first molding die and a second molding die that are relatively movable, and a third molding die that can slide in a direction intersecting a direction of relative movement of the first and second molding dies, the third molding die having an abutment surface that abuts against a portion located on the back surface side of the head of the main body portion, and a cavity for a communication flow path that is located in an internal position away from the abutment surface and extends in a direction intersecting a sliding direction of the third molding die; placing the elongated body portion in an open injection mold; A mold closing process for closing the injection mold, in which the injection mold is closed, - an ejection cavity adjacent to the legs of the body; and A cavity for a cushion portion defined between a part of the main body portion and a molding surface of the injection mold. a mold closing step in which the cavity for the injection passage and the cavity for the cushion portion are connected by a cavity for a communication passage of the third molding die; an injection step of injecting a heated and molten elastic polymer material into the injection passage cavity after the mold closing step; Equipped with The method for manufacturing a pillar garnish is characterized in that, in the injection process, an elastic polymer material is filled from the injection flow path cavity through the communicating flow path cavity into the cushion portion cavity, thereby forming a cushion portion that is integrally joined to the main body portion along the longitudinal direction.
2. The elongated main body further has a protruding portion that faces a back surface of the head portion and protrudes in a width direction of the head portion, The method for manufacturing a pillar garnish as described in claim 1, characterized in that in the mold closing process, the protrusion of the main body portion is positioned between the cavity for the injection flow path and the back surface of the head, thereby defining and forming a cavity for the cushion portion between the protrusion and the back surface of the head.
3. The method for manufacturing a pillar garnish as described in claim 1 or 2, characterized in that in the mold closing process, a cavity for a block portion is further formed between the cavity for the injection flow path and the cavity for the cushion portion for capturing and sealing a relatively cooled portion of the elastic polymer material.
4. The method further includes a mold opening step of opening the injection mold after the injection step, and removing the pillar garnish molded product obtained by integrally joining the main body portion and the cushion portion from the injection mold, The method for manufacturing a pillar garnish according to any one of claims 1 to 3, characterized in that when the third molding die is slid away from the first and second molding dies during mold opening, a communicating portion formed by an elastic polymer material filled in a cavity for a communicating flow path of the third molding die is broken.
5. The method for manufacturing a pillar garnish as described in claim 4, characterized in that the cavity for the communicating flow passage has a narrowest portion where the cross-sectional area is smallest, and the communicating portion formed by the cavity for the communicating flow passage has a narrowest portion corresponding to the narrowest portion.
Citation Information
Patent Citations
Insert molding method of transmission member
JP1993004255A
Mold for molding resin
JP2003181892A
Method for manufacturing composite molded object and manufacturing device
JP2007069517A
Method and device for manufacturing composite molded product
JP2007076317A
Vehicle pillar garnish and manufacturing method of the same
JP2018062225A