Isolation structure configured to reduce crosstalk in an image sensor

By increasing the height of the isolation structure to contact the metal grid structure, crosstalk between photodetectors in CMOS image sensors is minimized, enhancing quantum efficiency and performance.

JP7561222B2Active Publication Date: 2024-10-03TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023021220
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-07-11
Filing Date
2023-02-15
Publication Date
2024-10-03
Estimated Expiration
2043-02-15

AI Technical Summary

Technical Problem

Crosstalk between adjacent photodetectors in CMOS image sensors is high due to the relatively low height of the isolation structure, which reduces quantum efficiency and overall performance.

Method used

The isolation structure is designed with a higher height, protruding above the semiconductor substrate and contacting the metal grid structure, reducing the vertical path of obliquely incident light and minimizing crosstalk between photodetectors.

Benefits of technology

This design enhances optical isolation and reduces crosstalk, thereby improving the quantum efficiency and overall performance of the image sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007561222000001
    Figure 0007561222000001
  • Figure 0007561222000002
    Figure 0007561222000002
  • Figure 0007561222000003
    Figure 0007561222000003
Patent Text Reader

Abstract

To provide an image sensor and a method for forming the same that reduce crosstalk between adjacent light receiving elements due to the relatively low height of an isolation structure.SOLUTION: In an image sensor having a light receiving element 120 provided within a semiconductor substrate 104, an upper dielectric structure 132 is provided on the backside surface 104B of the semiconductor substrate. An isolation structure 122 includes an upper portion 122up that extends from the dielectric structure into the back surface of the semiconductor substrate, laterally envelops the light receiving element, and is provided above the back surface of the semiconductor substrate to directly contact the sidewall of the dielectric structure. The isolation structure includes a first material that is different from a second material of the dielectric structure.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Background technology]

[0001] Many modern electronic devices (e.g., digital cameras, optical imaging devices, etc.) contain image sensors. Image sensors convert optical images into digital data that can be represented as a digital image. Image sensors contain an array of pixel sensors, which are the unit elements for the conversion of optical images into digital data. Some types of pixel sensors include charge-coupled device (CCD) image sensors and complementary metal-oxide semiconductor (CMOS) image sensors (CIS). Compared to CCD pixel sensors, CIS are preferred due to their low power consumption, small size, high-speed data processing, direct output of data, and low manufacturing costs. Summary of the Invention [Problem to be solved by the invention]

[0002] One challenge with the CIS is crosstalk between adjacent light receiving elements due to the relatively low height of the isolation structure. For example, the top surface of the isolation structure is aligned with the backside surface of the semiconductor substrate and / or is disposed below the upper dielectric structure. This results in the isolation structure being separated from the metal grid structure by a relatively long distance. Incident light disposed at an angle to the backside surface of the semiconductor substrate may traverse a relatively long distance between the isolation structure and the metal grid structure from a first light receiving element to an adjacent second light receiving element. This increases the crosstalk between the light receiving elements and reduces the quantum efficiency (QE) of the first light receiving element. Thus, the relatively low height of the isolation structure reduces the optical isolation between the light receiving elements, thereby reducing the overall performance of the CIS. [Means for solving the problem]

[0003] The present disclosure provides, in some embodiments, an image sensor that includes a light receiving element disposed in a semiconductor substrate, a dielectric structure disposed on a first side of the semiconductor substrate, and an isolation structure extending from the dielectric structure into the first side of the semiconductor substrate. The semiconductor substrate includes a plurality of protrusions disposed on a first side of the semiconductor substrate above the light receiving elements.The isolation structure laterally encases the light receiving element, the isolation structure including a top portion disposed above the first side of the semiconductor substrate and in direct contact with a sidewall of the dielectric structure, the isolation structure including a first material different from a second material of the dielectric structure. The isolation structures are configured to direct incident light toward corresponding light receiving elements, and the height of the plurality of protrusions is less than the height of a top of the isolation structures.

[0004] The present disclosure also provides, in some embodiments, an image sensor including a photodetector disposed in a semiconductor substrate including a first side opposite a second side, an interconnect structure disposed on the first side of the semiconductor substrate, a dielectric structure disposed on the second side of the semiconductor substrate, a metal grid structure disposed in the dielectric structure and vertically offset from the second side of the semiconductor substrate by a first distance, and an isolation structure disposed in the semiconductor substrate. The semiconductor substrate includes a plurality of protrusions disposed on a first side of the semiconductor substrate above the light receiving elements. The light receiving element is spaced between opposing sidewalls of the metal grid structure. The isolation structure includes an upper portion that extends continuously along a first distance from the second side of the semiconductor substrate to a bottom surface of the metal grid structure. The isolation structures are configured to direct incident light toward corresponding light receiving elements, and the height of the plurality of protrusions is less than the height of a top of the isolation structures.

[0005] The present disclosure provides, in some embodiments, a method for forming an image sensor, the method including forming a photodetector in a semiconductor substrate including a front surface opposite a back surface, forming an interconnect structure on the front surface of the semiconductor substrate, patterning a backside surface of a semiconductor substrate to form a plurality of protrusions above the light receiving elements; depositing a first dielectric layer and a second dielectric layer on a backside surface of a semiconductor substrate; performing a patterning process on the backside surface of the semiconductor substrate to form isolation openings extending into the backside surface of the semiconductor substrate; and forming an isolation structure extending into the backside surface of the semiconductor substrate. The isolation structure is disposed vertically above the backside surface. A first dielectric layer and The isolation structure includes a top portion contacting a sidewall of the second dielectric layer. The isolation structure includes a first material that is different from a second material of the second dielectric layer. The isolation structures are configured to direct incident light toward corresponding light receiving elements, and the height of the plurality of protrusions is less than the height of a top of the isolation structures. Effect of the Invention

[0006] Due to the relatively high height of the isolation structure above the semiconductor substrate, the vertical path of incident light (e.g., obliquely incident light) crossing between the first light receiving element and the adjacent second light receiving element is reduced. This, in part, reduces crosstalk between adjacent light receiving elements and improves the overall performance of the image sensor. In addition, in an embodiment in which the image sensor includes a metal grid structure above the isolation structure, the top of the isolation structure protrudes from the backside surface of the semiconductor substrate to contact the bottom surface of the metal grid structure, so that incident light at an angle to the backside surface of the semiconductor substrate is mitigated from crossing the distance between the isolation structure and the metal grid structure, thereby further reducing crosstalk between the light receiving elements. [Brief description of the drawings]

[0007] Aspects of the present disclosure are best understood by reading the following detailed description in conjunction with the accompanying drawings, in which: It should be noted that, in accordance with standard practice in the industry, various features have not been drawn to scale, and in fact, the dimensions of various features illustrated in the accompanying drawings may be arbitrarily expanded or reduced for illustrative clarity. [Figure 1] FIG. 1 illustrates cross-sectional views of several embodiments of an image sensor that includes isolation structures that protrude upward from a semiconductor substrate into an overlying dielectric structure. [Diagram 2] FIG. 2 illustrates cross-sectional views of some alternative embodiments of the image sensor of FIG. [Diagram 3] FIG. 3 depicts a top view of some embodiments of the image sensor of FIG. 2 taken along line AA'. [Figure 4] 4A and 4B depict various cross-sectional views of several other embodiments of the image sensor of FIG. 1 in which the semiconductor substrate includes a plurality of protrusions. [Diagram 5] 5A-5D depict various cross-sectional views of several other embodiments of the image sensor of FIG. 1 in which a metal grid structure is provided above an isolation structure. [Figure 6] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 7] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 8] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 9] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 10] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 11] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 12] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 13] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 14] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 15] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 16] 6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 17]6-17 depict cross-sectional views of several embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 18] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 19] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 20] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 21] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 22] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 23] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 24] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 25] 18-25 depict cross-sectional views of various embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 26] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 27]26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 28] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 29] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 30] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 31] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 32] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 33] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 34] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 35] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Diagram 36] 26-36 depict cross-sectional views of several other embodiments of methods of forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. [Figure 37]37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Figure 38] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Figure 39] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 40] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 41] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 42] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 43] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 44] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Diagram 45] 37-45 depict cross-sectional views of further embodiments of methods of forming an image sensor that include isolation structures that protrude above a semiconductor substrate into an upper dielectric structure. [Figure 46] FIG. 46 depicts a flow diagram according to some embodiments of a method for forming an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The following embodiments provide many different embodiments or examples for implementing different features of the present disclosure. To simplify the present disclosure, specific examples of elements and arrangements are described below. Of course, these are illustrative and not intended to be limiting. For example, a configuration of a first feature above or on a second feature in the following description may include an embodiment in which the first and second features are formed in direct contact, and may also be an embodiment in which an additional feature is formed between the first and second features such that the first and second features are not in direct contact. In addition, the present disclosure may repeat reference signs and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself dictate a relationship between the various embodiments and / or configurations referred to.

[0009] Additionally, spatially relative terms such as "below," "lower," "bottom," "upper," "top," and the like may be used to facilitate the description to explain the relationship of one element or feature depicted in the figures to another element or feature. The spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation depicted. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein may be interpreted accordingly.

[0010] Additionally, "first," "second," "third," etc. may be used for ease of description to distinguish between different elements in a figure or series of figures. "First," "second," "third," etc. are not intended to describe corresponding elements, but are merely general identifiers. For example, a "first dielectric layer" described in connection with the first figure does not necessarily correspond to a "first dielectric layer" described in connection with some embodiments, but rather may correspond to a "second dielectric layer" in other embodiments.

[0011] Some complementary metal oxide semiconductor image sensors (CIS) include a plurality of light receiving elements disposed on a semiconductor substrate. A plurality of pixel elements (e.g., transfer transistors, reset transistors, etc.) and an interconnect structure are disposed on a front surface of the semiconductor substrate. The light receiving elements are configured to record incident light disposed on a back surface of the substrate, and the pixel elements facilitate readout of the recording. An isolation structure (e.g., a deep trench isolation (DTI) structure) extends into the back surface of the semiconductor substrate and is disposed laterally between adjacent light receiving elements in the plurality of light receiving elements. The isolation structure is configured to enhance optical and electrical isolation between adjacent light receiving elements. A passivation layer covers the back surface of the semiconductor substrate, and an upper dielectric structure covers the isolation structure. Additionally, a metal grid structure on the upper dielectric structure is disposed around a plurality of grid openings directly above the plurality of light receiving elements. The metal grid structure is configured to guide incident light to the light receiving elements and reduce crosstalk between the light receiving elements, thereby further enhancing optical isolation between the light receiving elements.

[0012] One challenge with the CIS is crosstalk between adjacent light receiving elements due to the relatively low height of the isolation structure. For example, the top surface of the isolation structure is aligned with the backside surface of the semiconductor substrate and / or is disposed below the upper dielectric layer. This results in the isolation structure being separated from the metal grid structure by a relatively long distance (e.g., in the range of about 1000 angstroms (Å) to about 1600 Å). Incident light disposed at an angle to the backside surface of the semiconductor substrate may traverse a relatively long distance between the isolation structure and the metal grid structure from a first light receiving element to an adjacent second light receiving element. This increases the crosstalk between the light receiving elements and reduces the quantum efficiency (QE) of the first light receiving element. Thus, the relatively low height of the isolation structure reduces the optical isolation between the light receiving elements, thereby reducing the overall performance of the CIS.

[0013] In some embodiments, the present disclosure is directed to an image sensor configured to include an isolation structure protruding above a semiconductor substrate to enhance optical isolation of the image sensor. The image sensor includes a plurality of light receiving elements disposed in a semiconductor substrate. The isolation structure extends into a backside surface of the semiconductor substrate and is disposed laterally between adjacent light receiving elements. An upper dielectric structure covers the backside surface of the semiconductor substrate. The isolation structure includes an upper portion protruding from the backside surface of the semiconductor substrate into the upper dielectric structure such that a height of the isolation structure above the backside surface of the semiconductor substrate is relatively high (e.g., in a range of about 800 Å to about 1300 Å). Due to the relatively high height of the isolation structure above the semiconductor substrate, a vertical path that incident light (e.g., obliquely incident light) traverses between a first light receiving element and an adjacent second light receiving element is reduced. This, in part, reduces crosstalk between adjacent light receiving elements and improves overall performance of the image sensor.

[0014] In addition, the image sensor includes a grid structure above the isolation structure, the top of which protrudes from the backside surface of the semiconductor substrate to contact the bottom surface of the grid structure, which mitigates incident light that is angled relative to the backside surface of the semiconductor substrate from traversing the distance between the isolation structure and the grid structure, thereby further reducing crosstalk between the light receiving elements.

[0015] FIG. 1 illustrates a cross-sectional view 100 of several embodiments of an image sensor that includes an isolation structure that protrudes above a semiconductor substrate into an overlying dielectric structure.

[0016] The image sensor includes a plurality of light receiving elements 120 disposed in a semiconductor substrate 104 and an interconnect structure 102 disposed along a front surface 104f of the semiconductor substrate 104. In some embodiments, the semiconductor substrate 104 includes any semiconductor body (e.g., bulk silicon) and / or has a first doping type (e.g., p-type). The interconnect structure 102 includes an interconnect dielectric structure 106, a plurality of conductive lines 108, and a plurality of conductive vias 110. A plurality of pixel elements 112 are disposed on the front surface 104f of the semiconductor substrate 104. The pixel elements 112 are electrically coupled to each other and / or to other semiconductor devices (not shown) by the plurality of conductive lines 108 and the plurality of conductive vias 110. The plurality of pixel elements 112 may include a gate electrode 116 and a gate dielectric layer 114 disposed between the gate electrode 116 and the front surface 104f of the semiconductor substrate 104.

[0017] The plurality of light receiving elements 120 are disposed laterally within the pixel region 103 of the semiconductor substrate 104. Each of the light receiving elements 120 has a second doping type (e.g., n-type) opposite to a first doping type (e.g., p-type). In some embodiments, the first doping type is p-type and the second doping type is n-type, or vice versa. The light receiving elements 120 are configured to absorb incident light (e.g., photons) and generate respective electrical signals corresponding to the incident light. In some embodiments, the light receiving elements 120 may generate electron-hole pairs from the incident light. The pixel elements 112 are configured to read out the electrical signals generated from the plurality of light receiving elements 120. For example, the pixel elements 112 may be or include one or more transfer transistors configured to selectively form conductive channels in the semiconductor substrate 104 to transfer accumulated charge (e.g., due to absorption of incident radiation) from the light receiving elements 120.

[0018] A shallow trench isolation (STI) structure 118 is provided in the semiconductor substrate 104 along the front surface 104f of the semiconductor substrate 104. The isolation structure 122 extends into the back surface 104b of the semiconductor substrate 104. A passivation layer 130 covers the back surface 104b, and an upper dielectric structure 132 covers the passivation layer 130. A plurality of microlenses 136 are above the back surface 104b of the semiconductor substrate 104 and configured to focus incident light toward the light receiving element 120. Furthermore, a conductive pad 134 is provided on the back surface 104b of the semiconductor substrate 104 and laterally in a peripheral region 105 of the semiconductor substrate 104 adjacent to the pixel region 103. In various embodiments, the peripheral region 105 laterally wraps around the pixel region 103 in a continuous manner. In yet further embodiments, the conductive pad 134 laterally continuously encapsulates the plurality of light receiving elements 120 along an uninterrupted path. In some embodiments, the conductive pad 134 may be configured as and / or referred to as a conductive shielding structure configured to block incident light from crossing from the backside surface 104b of the semiconductor substrate 104 to the peripheral region 105 of the semiconductor substrate 104. In further embodiments, the conductive pad 134 directly contacts the semiconductor substrate 104, such that the conductive pad 134 and the semiconductor substrate 104 are directly electrically coupled together.

[0019] The isolation structure 122 is disposed in the semiconductor substrate 104 and includes a first liner layer 124, a second liner layer 126, and a trench fill layer 128. In various embodiments, the first liner layer 124 includes a first dielectric material (e.g., a high-k dielectric), and the second liner layer 126 includes a second dielectric material (e.g., an oxide such as silicon dioxide) different from the first dielectric material. Furthermore, the trench fill layer 128 may include polysilicon, doped polysilicon, or a metal (e.g., tungsten, aluminum, etc.). The isolation structure 122 is configured to guide incident light toward a corresponding light receiving element 120. For example, incident light disposed at an angle above a first light receiving element can be redirected toward the first light receiving element by hitting a sidewall of the isolation structure 122, rather than crossing the isolation structure 122 to an adjacent second light receiving element. Thus, the isolation structures 122 improve the QE of each photodetector 120 and increase optical isolation.

[0020] Additionally, the isolation structure 122 includes an upper portion 122up that protrudes through the backside surface 104b and the passivation layer 130 into the upper dielectric structure 132. The upper portion 122up of the isolation structure 122 has a relatively high height h1 (e.g., in the range of about 800 Å to about 1300 Å) above the backside surface 104b. Due to the relatively high height h1 of the upper portion 122up, incident light at an angle to the backside surface 104b has a shorter vertical path across the region between adjacent light receiving elements 12. This reduces crosstalk between the light receiving elements and improves the overall performance of the image sensor.

[0021] In various embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is in the range of about 800 Å to about 1300 Å, in the range of about 800 Å to about 1050 Å, in the range of about 1050 Å to about 1300 Å, or other suitable value. In some embodiments, the height h1 is relatively high (e.g., about 800 Å or more), such that the upper portion 122up of the isolation structure 122 is sufficiently high to reduce crosstalk between adjacent light receiving elements 120 while maintaining structural integrity. In further embodiments, the height h1 is less than about 1300 Å, such that the upper portion 122up of the isolation structure 122 enhances optical isolation of the image sensor while reducing costs associated with manufacturing the image sensor and facilitating device scaling.

[0022] FIG. 2 illustrates a cross-sectional view 200 of some embodiments of an image sensor that includes isolation structures that protrude above a semiconductor substrate into an overlying dielectric structure.

[0023] The image sensor of FIG. 2 includes a plurality of light receiving elements 120 disposed in a semiconductor substrate 104 having a backside surface 104b and an opposing frontside surface 104f. An isolation structure 122 extends into the backside surface 104b, and the isolation structure 122 includes an upper portion 122up that protrudes from the semiconductor substrate 104 into an upper dielectric structure 132. The isolation structure 122 laterally surrounds the plurality of light receiving elements 120 and provides a space between adjacent light receiving elements of the plurality of light receiving elements 120. The semiconductor substrate 104 may be or include, for example, single crystal silicon, epitaxial silicon, germanium, silicon germanium, a silicon-on-insulator (SOI) substrate, other semiconductor materials, any combination of the foregoing, and the like. In some embodiments, the semiconductor substrate 104 has a first doping type (e.g., p-type). The interconnect structure 102 is disposed on a front surface 104f of a semiconductor substrate 104 and includes an interconnect dielectric structure 106, a plurality of conductive lines 108, and a plurality of conductive vias 110. The interconnect dielectric structure 106 includes one or more dielectric layers, each of which may be or include, for example, silicon dioxide, a low-k dielectric material, an ultra-low-k dielectric material, other suitable dielectric materials, or any combination thereof. As used herein, a low-k dielectric material is a dielectric material having a dielectric constant less than 3.9. The conductive lines 108 and conductive vias 110 may be or include, for example, aluminum, copper, ruthenium, tungsten, titanium nitride, tantalum nitride, other conductive materials, or any combination thereof.

[0024] A plurality of pixel elements 112 are disposed in and / or on the front surface 104f of the semiconductor substrate 104. In some embodiments, the pixel elements 112 are configured as transfer transistors and each includes a gate electrode 116 and a gate dielectric layer 114 disposed between the gate electrode 116 and the semiconductor substrate 104. The gate electrode 116 may be or include, for example, polysilicon, a metallic material such as aluminum, titanium, tantalum, tungsten, other metallic materials, or any combination thereof. The gate dielectric layer 114 may be or include, for example, a high-k dielectric material such as silicon dioxide, tantalum oxide, hafnium oxide, aluminum oxide, other dielectric materials, or any combination thereof. As used herein, a high-k dielectric material is a dielectric material having a dielectric constant greater than 3.9.

[0025] Additionally, a shallow trench isolation (STI) structure 118 is provided on the front surface 104f of the semiconductor substrate 104. In various embodiments, the STI structure 118 may laterally surround the pixel element 112 and define a device area for, for example, the pixel region 103 of the semiconductor substrate 104. The STI structure 118 may be or include, for example, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, silicon dioxide, other suitable dielectric material, or any combination thereof. In some embodiments, the top surface of the STI structure 118 directly contacts the bottom surface of the isolation structure 122. In yet further embodiments, the STI structure 118 may be part of the isolation structure 122 (e.g., the STI structure 118 has the same layout as the isolation structure 122 in a top view and is in direct contact with the isolation structure 122), such that the isolation structure 122 extends continuously and vertically from the third dielectric layer 206 to the backside surface 104b of the semiconductor substrate 104. In such embodiments, the STI structure 118 may be referred to as and / or configured as a lower portion of the isolation structure 122.

[0026] The light receiving element 120 is disposed on the semiconductor substrate 104 and has a second doping type (e.g., n-type) opposite to the first doping type. In some embodiments, the doping concentration of the light receiving element 120 is about 10 13 ~10 16 atoms / cm 3 or other suitable value. The passivation layer 130 is disposed on the backside surface 104b of the semiconductor substrate 104. The passivation layer 130 may be or include a high-k dielectric material, such as, for example, titanium oxide, tantalum oxide, aluminum oxide, other suitable dielectric material, or any combination thereof. Further, an upper dielectric structure 132 covers the passivation layer 130. In some embodiments, the upper dielectric structure 132 includes a first dielectric layer 202, a second dielectric layer 204, a third dielectric layer 206, and a fourth dielectric layer 208. In various embodiments, the dielectric layers 202-208 of the upper dielectric structure 132 may be or include an oxide, such as, for example, silicon dioxide, other suitable dielectric material, or any combination thereof. In some embodiments, the passivation layer 130, the first dielectric layer 202, and the second dielectric layer 204 directly contact opposing sidewalls of the upper portion 122up of the isolation structure 122, respectively. In a further embodiment, the third dielectric layer 206 directly contacts the top surface of the isolation structure 122. In yet a further embodiment, the top surface of the second dielectric layer 204 is flush with the top surface of the isolation structure 122.

[0027] A plurality of microlenses 136 are on the upper dielectric structure 132. The microlenses 136 are configured to focus incident light toward the light receiving elements 120. Conductive pads 134 are disposed above the backside surface 104b of the semiconductor substrate 104 and are laterally spaced apart in the peripheral region 105 of the semiconductor substrate 104 adjacent the pixel region 103. In various embodiments, the conductive pads 134 are disposed on the upper dielectric structure 132 and extend through the passivation layer 130 to contact the backside surface 104b of the semiconductor substrate. In further embodiments, the conductive pads 134 include an upper surface 134us disposed along the top surface of the third dielectric layer 206 and a lower surface 134ls vertically below the upper surface 134us. In yet further embodiments, the conductive pads 134 are configured as conductive shielding structures that block incident light from crossing the backside surface 104b of the semiconductor substrate 104 to the peripheral region 105 of the semiconductor substrate 104. The conductive pads 134 may be or include a metallic material, such as aluminum, copper, titanium, tungsten, other conductive materials, or any combination thereof. In some embodiments, the top surface of the isolation structure 122 is vertically between the lower surface 134ls of the conductive pad 134 and the upper surface 134us of the conductive pad 134.

[0028] The isolation structure 122 extends continuously from the upper dielectric structure 132 into the semiconductor substrate 104. In some embodiments, the bottom surface of the isolation structure 122 is disposed between the front surface 104f and the back surface 104b. In various embodiments, the isolation structure 122 includes a first liner layer 124, a second liner layer 126, and a trench fill layer 128. The trench fill layer 128 extends into the semiconductor substrate 104, and the first liner layer 124 is disposed between the trench fill layer 128 and the semiconductor substrate 104. The second liner layer 126 is disposed between the first liner layer 124 and the trench fill layer 128. In various embodiments, the top surface of the first liner layer 124, the top surface of the second liner layer 126, and the top surface of the trench fill layer 128 are coplanar with one another. The second liner layer 126 extends along opposing sidewalls of the trench fill layer 128 and overlies a bottom surface of the trench fill layer 128. Additionally, the first liner layer 124 extends along opposing sidewalls of the second liner layer 126 and overlies a bottom surface of the second liner layer 126. In various embodiments, the thickness of the trench fill layer 128 is greater than the thickness of the first liner layer 124 and the thickness of the second liner layer 126. In further embodiments, the height ht of the isolation structure 122 is greater than the height hs of the semiconductor substrate 104.

[0029] The first liner layer 124 may be or include, for example, a high-k dielectric material, such as aluminum oxide, hafnium oxide, titanium oxide, other high-k dielectric materials, other dielectric materials, or any combination thereof. The second liner layer 126 may be or include, for example, silicon dioxide, other suitable dielectric materials, or the like. In some embodiments, the dielectric constant of the first liner layer 124 is higher than the dielectric constant of the second liner layer 126. The trench fill layer 128 may be or include, for example, polysilicon, doped polysilicon, metals such as tungsten or aluminum, other metallic materials, or any combination thereof. Additionally, a height h1 of the top portion 122up of the isolation structure 122 above the backside surface 104b of the semiconductor substrate 104 is within a range of about 800 Å to about 1300 Å, or other suitable value. Due to the relatively high height h1 of the upper portion 122up, incident light at an angle to the backside surface 104b has a shorter path to cross the area between adjacent light receiving elements 120. This reduces crosstalk in the multiple light receiving elements 120 and increases the overall optical isolation of the image sensor. Furthermore, because the trench fill layer 128 includes a metal (e.g., tungsten, aluminum, etc.), incident light is more likely to reflect off the sidewalls of the trench fill layer 128 toward the corresponding light receiving element 120 and is less likely to cross the isolation structure 122 between the adjacent light receiving elements 120. Thus, the material and the relatively high height h1 of the upper portion 122up improve the performance of the image sensor.

[0030] Figure 3 illustrates a top view 300 of some embodiments of the image sensor of Figure 2 taken along line A-A' of Figure 2. As illustrated in the top view 300 of Figure 3, the isolation structures 122 laterally surround the plurality of light receiving elements 120. The isolation structures 122 have a grid structure and extend continuously between adjacent light receiving elements of the plurality of light receiving elements 120.

[0031] FIG. 4A illustrates a cross-sectional view 400a of some alternative embodiments of the image sensor of FIG. 1, in which the semiconductor substrate 104 includes a plurality of protrusions 402 disposed on the backside surface 104b of the semiconductor substrate 104. In various embodiments, the plurality of protrusions 402 are configured to provide a non-flat pattern (e.g., a jigsaw pattern) on the semiconductor substrate 104 above the light receiving elements 120 to increase the light receiving surface area for incident light disposed on the backside surface 104b of the semiconductor substrate 104. Thus, the protrusions 402 improve the sensitivity and / or QE of the light receiving elements 120, thereby improving the overall performance of the image sensor. The passivation layer 130 and the first dielectric layer 202 conform to the shape of the protrusions 402, and the passivation layer 130 is in direct contact with the protrusions 402. In various embodiments, the second dielectric layer 204 includes a plurality of upward protrusions extending below the top surface of the semiconductor substrate 104 and adjacent to the protrusions 402. In some embodiments, the upward protrusion of the second dielectric layer 204 has the same shape (e.g., triangular) as the protrusion 402 of the semiconductor substrate 104. In yet further embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is greater than the height hp of the protrusion 402. This, in part, facilitates the isolation structure 122 to reduce crosstalk between adjacent light receiving elements 120. In yet further embodiments, the height ht of the isolation structure 122 is less than the height hs of the semiconductor substrate 104.

[0032] 4B illustrates a cross-sectional view 400b of several alternative embodiments of the image sensor of FIG. 4A in which the isolation structures 122 extend continuously from the third dielectric layer 206 to the STI structures 118. In various embodiments, the bottom surfaces of the isolation structures 122 directly contact the top surfaces of the STI structures 118.

[0033] FIG. 5A illustrates a cross-sectional view 500 a of some alternative embodiments of the image sensor of FIG. 4A in which a metal grid structure 502 is provided on the upper dielectric structure 132 and overlies the isolation structure 122 .

[0034] The metal grid structure 502 includes sidewalls that define a number of openings that are directly over the corresponding ones of the plurality of light receiving elements 120. In some embodiments, the metal grid structure 502 includes one or more metal layers configured to reduce crosstalk between adjacent ones of the plurality of light receiving elements 120, thereby increasing optical isolation of the image sensor. For example, due to the material and layout of the metal grid structure 502, incident light (e.g., obliquely incident light) provided on the backside surface 104b of the semiconductor substrate 104 can be reflected from the metal grid structure 502 toward the corresponding light receiving element 120 (e.g., reflected from the sidewalls of the metal grid structure 502). The metal grid structure 502 may be or include, for example, tungsten, aluminum, other metallic materials, or any combination thereof. In yet further embodiments, the metal grid structure 502 and the trench fill layer 128 include the same material (e.g., tungsten, aluminum, etc.). In further embodiments, the metal grid structure 502 includes a different material than the conductive pad 134. In some embodiments, the height of the metal grid structure 502 is less than the height h1 of the top portion 122up of the isolation structure 122.

[0035] The bottom surface of the metal grid structure 502 directly contacts the top surface of the trench fill layer 128. In various embodiments, no dielectric material (e.g., from the upper dielectric structure 132) is provided between the metal grid structure 502 and the trench fill layer 128. The direct contact of the metal grid structure 502 with the trench fill layer 128 mitigates incident light at an angle to the backside surface 104b of the semiconductor substrate 104 from passing through the space between the metal grid structure 502 and the trench fill layer 128. Instead, the incident light can be reflected from the sidewalls of the upper portion 122up of the isolation structure 122 and / or from the sidewalls of the metal grid structure 502 toward the corresponding light receiving element 120. This, in part, further enhances the optical isolation between the light receiving elements 120, further enhancing the overall performance of the image sensor. In yet a further embodiment, the metal grid structure 502 is directly above the isolation structures 122 and has a grid-shaped layout that corresponds to the grid layout of the isolation structures 122 (e.g., as shown in FIG. 3 ). In yet a further embodiment, the center of the metal grid structure 502 is aligned with the center of the isolation structures 122.

[0036] FIG. 5B illustrates a cross-sectional view 500b of some alternative embodiments of the image sensor of FIG. 5A in which the metal grid structure 502 is laterally shifted toward the peripheral region 105. The metal grid structure 502 includes a first grid segment 502a directly above a first isolation structure segment 128a of the trench fill layer 128. In some embodiments, a center 504 of the first isolation structure segment 128a is laterally offset from a center 506 of the first grid segment 502a by a non-zero distance d1. In various embodiments, the center of the metal grid structure 502 is laterally shifted by a distance d1 from the center of the isolation structure 122 toward the peripheral region 105. Laterally shifting the metal grid structure 502 toward the peripheral region 105 blocks incident light from entering the peripheral region 105 while increasing the incident light provided on the pixel region 103 of the semiconductor substrate 104.

[0037] Figure 5C illustrates a cross-sectional view 500c of some alternative embodiments of the image sensor of Figure 5A in which the metal grid structure 502 and the trench fill layer 128 are a single continuous structure comprising the same material (e.g., a metallic material such as tungsten, aluminum, etc.) In some embodiments, the metal grid structure 502 and the trench fill layer 128 are formed by a single deposition process.

[0038] FIG. 5D illustrates a cross-sectional view 500d of some alternative embodiments of the image sensor of FIG. 5A, in which the height ht of the isolation structures 122 is less than the height hs of the semiconductor substrate 104.

[0039] 6-17 depict cross-sectional views 600-1700 of several embodiments of a method for forming an image sensor including an isolation structure protruding into an upper dielectric structure above a semiconductor substrate. Although the cross-sectional views 600-1700 shown in FIGS. 6-17 are described with reference to a method, it should be understood that the structures shown in FIGS. 6-17 are not limited to the method, but rather may stand alone apart from the method. Furthermore, although FIGS. 6-17 are described as a sequence of operations, it should be understood that the operations are not limiting, and the order of operations may be changed in other embodiments, and the disclosed method may be applicable to other structures. In other embodiments, some operations shown and / or described may be omitted in whole or in part.

[0040] As shown in the cross-sectional view 600 of FIG. 6, a semiconductor substrate 104 is provided and a plurality of photodetectors 120 are formed in a pixel region 103 of the semiconductor substrate 104. The semiconductor substrate 104 may be or include, for example, single crystal silicon, epitaxial silicon, germanium, silicon germanium, silicon-on-insulator (SOI) substrate, other semiconductor materials, any combination of the above, etc. In some embodiments, the semiconductor substrate 104 has a first doping type (e.g., p-type). In various embodiments, each photodetector 120 includes a region of the semiconductor substrate 104 having a second doping type (e.g., n-type) opposite to the first doping type (e.g., p-type). In some embodiments, the photodetector 120 may be formed by a selective ion implantation process utilizing a masking layer (not shown) on the front surface 104f of the semiconductor substrate 104 to selectively implant ions into the semiconductor substrate 104.

[0041] As shown in cross-sectional view 700 of FIG. 7, a shallow trench isolation (STI) structure 118 is formed in a front surface 104f of a semiconductor substrate 104. The STI structure 118 may be or include, for example, silicon oxide, silicon nitride, silicon carbide, silicon oxynitride, silicon oxycarbide, other suitable dielectric material, or any combination thereof. In various embodiments, a method for forming the STI structure 118 includes patterning the front surface 104f of the semiconductor substrate 104 to form a trench extending into the front surface 104f, depositing a dielectric material in the trench (e.g., by chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), thermal oxidation, etc.), and performing a planarization process (e.g., an etch process, a chemical mechanical planarization (CMP) process, etc.) on the dielectric layer.

[0042] 8, a plurality of pixel elements 112 and interconnect structures 102 are formed on a front surface 104f of a semiconductor substrate 104. In some embodiments, each pixel element 112 includes a gate electrode 116 and a gate dielectric layer 114 disposed between the gate electrode 116 and the semiconductor substrate 104. In some embodiments, a process for forming the pixel elements 112 includes depositing a gate dielectric material (e.g., by CVD, PVD, ALD, etc.) above the semiconductor substrate 104, depositing a gate electrode material (e.g., by CVD, PVD, ALD, electrolytic plating, electroless plating, etc.) above the gate dielectric material, and patterning the gate electrode material and the gate dielectric material.

[0043] Further, the interconnect structure includes an interconnect dielectric structure 106, a plurality of conductive lines 108, and a plurality of conductive vias 110. In various embodiments, the interconnect dielectric structure 106 may be formed by one or more deposition processes, such as a PVD process, a CVD process, an ALD process, or other suitable growth or deposition process. In some embodiments, the plurality of conductive lines 108 and / or the plurality of conductive vias 110 may be formed by one or more deposition processes, one or more patterning processes, one or more planarization processes, other suitable processes, or any combination of the above. For example, the plurality of conductive lines 108 and the plurality of conductive vias 110 may be formed by one or more single damascene processes, one or more dual damascene processes, other manufacturing processes, or any combination of the above.

[0044] 9, the passivation layer 130 is deposited on the backside surface 104b of the semiconductor substrate 104, and the first dielectric layer 202 is deposited on the passivation layer 130. In some embodiments, the passivation layer 130 and the first dielectric layer 202 are deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In some embodiments, the passivation layer 130 comprises a high-k dielectric material and the first dielectric layer 202 comprises an oxide (e.g., silicon dioxide) having a lower dielectric constant than the passivation layer 130.

[0045] As shown in cross-sectional view 1000 of FIG. 10, the second dielectric layer 204 is deposited on the first dielectric layer 202. In some embodiments, the second dielectric layer 204 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In further embodiments, a planarization process (e.g., a CMP process) is performed on the second dielectric layer 204 such that a top surface of the second dielectric layer 204 is substantially flat. In yet further embodiments, the thickness of the second dielectric layer 204 is greater than the thickness of the first dielectric layer 202 and greater than the thickness of the passivation layer 130.

[0046] 11, a patterning process is performed on the backside surface 104b of the semiconductor substrate 104 to form isolation openings 1102 extending into the backside surface 104b. In some embodiments, the patterning process includes forming a masking layer (not shown) over the second dielectric layer 204, etching the semiconductor substrate 104 according to the masking layer (e.g., by a dry etching process, a wet etching process, etc.), and removing the masking layer.

[0047] As shown in cross-sectional view 1200 of FIG. 12, a first liner layer 124 is deposited over the semiconductor substrate 104 to line the isolation opening 1102, and a second liner layer 126 is deposited on the first liner layer 124. In some embodiments, the first liner layer 124 and the second liner layer 126 are each deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. The first liner layer 124 may be or include a high-k dielectric material, such as, for example, aluminum oxide, hafnium oxide, titanium oxide, other high-k dielectric materials, other dielectric materials, or any combination of the above. The second liner layer 126 may be or include, for example, silicon dioxide, other suitable dielectric materials, etc.

[0048] As shown in cross-sectional view 1300 of FIG. 13, a trench fill layer 128 is deposited above the second liner layer 126 and in the isolation opening (1102 of FIG. 12). In various embodiments, the trench fill layer 128 is deposited above the second liner layer 126 by a CVD process, a PVD process, an ALD process, electrolytic plating, electroless plating, or other suitable growth or deposition process. The trench fill layer 128 may be or include, for example, polysilicon, doped polysilicon, metals such as tungsten or aluminum, other metallic materials, or any combination of the above. In some embodiments, prior to depositing the trench fill layer 128, a blanket etch process may be performed (not shown) to remove portions of the second liner layer 126 and / or the first liner layer 124 that are deposited on the top surface of the second dielectric layer 204. In various embodiments, after the blanket etch process, the top surfaces of the first and second liner layers 124, 126 are aligned with the top surface of the second dielectric layer 204 (eg, as depicted in FIG. 2).

[0049] As shown in cross-sectional view 1400 of FIG. 14, a removal process is performed to remove excess material from above the second dielectric layer 204, thereby forming isolation structures 122 extending into the semiconductor substrate 104. In some embodiments, the removal process includes performing an etching process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 to remove excess material from above the second dielectric layer 204. In various embodiments, the etching process includes a dry etch, a blanket etch, and / or the like. The etching process may overetch to remove at least a portion of the second dielectric layer 204. In still further embodiments, the removal process includes performing a CMP process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 until a top surface of the second dielectric layer 204 is reached. In various embodiments, the top surface of the isolation structures 122 is coplanar with the top surface of the second dielectric layer 204. The removal process is further performed such that the isolation structure 122 includes an upper portion 122up that extends above the semiconductor substrate 104 and has a height h1. In various embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is in a range between about 800 Å and about 1300 Å, in a range between about 800 Å and about 1050 Å, in a range between about 1050 Å and about 1300 Å, or other suitable value. In still further embodiments, the height ht of the isolation structure 122 is less than the height hs of the semiconductor substrate 104.

[0050] As shown in cross-sectional view 1500 of FIG. 15, the third dielectric layer 206 is deposited over the isolation structures 122, and a patterning process is performed to form an opening 1502 in the peripheral region 105 of the semiconductor substrate 104. In some embodiments, the third dielectric layer 206 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In various embodiments, the patterning process includes forming a masking layer (not shown) over the third dielectric layer 206, performing an etching process (e.g., dry etching, wet etching, etc.) according to the masking layer, and removing the masking layer. The opening 1502 exposes a portion of the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105.

[0051] As shown in cross-sectional view 1600 of FIG. 16, a conductive pad 134 is formed on the backside surface 104b of the semiconductor substrate 104 in the opening (1502 of FIG. 15) and in the peripheral region 105. In some embodiments, a process for forming the conductive pad 134 includes depositing (e.g., by CVD, PVD, ALD, electrolytic plating, electroless plating, etc.) a conductive material over the semiconductor substrate 104 and in the opening (1502 of FIG. 15) and patterning the conductive material. The conductive pad 134 may be or include, for example, aluminum, copper, titanium, tungsten, other conductive materials, or any combination thereof. In various embodiments, the trench fill layer 128 includes a first metal material and the conductive pad 134 includes a second metal material that is different from the first metal material.

[0052] As shown in the cross-sectional view 1700 of FIG. 17, a fourth dielectric layer 208 is formed over the third dielectric layer 206 and the conductive pad 134, thereby forming an upper dielectric structure 132. Further, a plurality of microlenses 136 are formed on the fourth dielectric layer 208. The upper dielectric structure 132 includes the first dielectric layer 202, the second dielectric layer 204, the third dielectric layer 206, and the fourth dielectric layer 208. In some embodiments, a planarization process (e.g., a CMP process) is performed on the fourth dielectric layer 208 such that the upper dielectric structure 132 has a thickness t1. In some embodiments, the thickness t1 is about 4700 Å, in a range between about 3000 Å and about 6000 Å, or other suitable value.

[0053] 18-25 depict cross-sectional views 1800-2500 of several embodiments of a method for forming an image sensor including an isolation structure protruding into an upper dielectric structure above a semiconductor substrate. Although the cross-sectional views 1800-2500 shown in FIGS. 18-25 are described with reference to a method, it should be understood that the structures shown in FIGS. 18-25 are not limited to the method, but rather may stand alone apart from the method. Furthermore, although FIGS. 18-25 are described as a sequence of operations, it should be understood that the operations are not limiting, and the order of operations may be changed in other embodiments, and the disclosed method may be applicable to other structures. In other embodiments, some operations shown and / or described may be omitted in whole or in part.

[0054] As shown in cross-sectional view 1800 of Figure 18, a passivation layer 130, a first dielectric layer 202, and a second dielectric layer 204 are formed on the backside surface 104b of the semiconductor substrate 104. In some embodiments, the structure of Figure 18 is formed as shown and / or described in Figures 6-10.

[0055] As shown in cross-sectional view 1900 of Figure 19, a patterning process is performed on the backside surface 104b of the semiconductor substrate 104 to form isolation openings 1902 extending into the backside surface 104b. In some embodiments, the patterning process includes forming a masking layer (not shown) over the second dielectric layer 204, etching the semiconductor substrate 104 according to the masking layer (e.g., by a dry etching process, a wet etching process, etc.), and removing the masking layer. In various embodiments, the patterning process is performed until the top surface of the STI structure 118 is reached.

[0056] As shown in cross-sectional view 2000 of FIG. 20, a first liner layer 124 is deposited over the semiconductor substrate 104 to line the isolation opening 1902, and a second liner layer 126 is deposited on the first liner layer 124. In some embodiments, the first liner layer 124 and the second liner layer 126 are each deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. The first liner layer 124 may be or include a high-k dielectric material, such as, for example, aluminum oxide, hafnium oxide, titanium oxide, other high-k dielectric materials, other dielectric materials, or any combination of the above. The second liner layer 126 may be or include, for example, silicon dioxide, other suitable dielectric materials, etc.

[0057] As shown in cross-sectional view 2100 of FIG. 21, a trench fill layer 128 is deposited over the second liner layer 126 and in the isolation opening (1902 of FIG. 20). In various embodiments, the trench fill layer 128 is deposited over the second liner layer 126 by a CVD process, a PVD process, an ALD process, electrolytic plating, electroless plating, or other suitable growth or deposition process. The trench fill layer 128 may be or include, for example, polysilicon, doped polysilicon, metals such as tungsten or aluminum, other metallic materials, or any combination of the above. In some embodiments, prior to depositing the trench fill layer 128, a blanket etch process may be performed (not shown) to remove portions of the second liner layer 126 and / or the first liner layer 124 that are deposited on the top surface of the second dielectric layer 204. In various embodiments, after the blanket etch process, the top surfaces of the first and second liner layers 124, 126 are aligned with the top surface of the second dielectric layer 204 (eg, as depicted in FIG. 2).

[0058] As shown in cross-sectional view 2200 of FIG. 22, a removal process is performed to remove excess material from above the second dielectric layer 204, thereby forming isolation structures 122 extending into the semiconductor substrate 104. In some embodiments, the removal process includes performing an etching process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 to remove excess material from above the second dielectric layer 204. In various embodiments, the etching process includes a dry etch, a blanket etch, and / or the like. The etching process may overetch to remove at least a portion of the second dielectric layer 204. In still further embodiments, the removal process includes performing a CMP process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 until a top surface of the second dielectric layer 204 is reached. In various embodiments, the top surface of the isolation structures 122 is coplanar with the top surface of the second dielectric layer 204. The removal process is further performed such that the isolation structure 122 includes an upper portion 122up that extends above the semiconductor substrate 104 and has a height h1. In various embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is in a range between about 800 Å and about 1300 Å, in a range between about 800 Å and about 1050 Å, in a range between about 1050 Å and about 1300 Å, or other suitable value. In still further embodiments, the height ht of the isolation structure 122 is less than the height hs of the semiconductor substrate 104.

[0059] As shown in cross-sectional view 2300 of FIG. 23, the third dielectric layer 206 is deposited over the isolation structures 122, and a patterning process is performed to form an opening 2302 in the peripheral region 105 of the semiconductor substrate 104. In some embodiments, the third dielectric layer 206 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In various embodiments, the patterning process includes forming a masking layer (not shown) over the third dielectric layer 206, performing an etching process (e.g., dry etching, wet etching, etc.) according to the masking layer, and removing the masking layer. The opening 2302 exposes a portion of the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105.

[0060] As shown in cross-sectional view 2400 of FIG. 24, a conductive pad 134 is formed in the opening (2302 of FIG. 23) and on the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105. In some embodiments, a process for forming the conductive pad 134 includes depositing (e.g., by CVD, PVD, ALD, electrolytic plating, electroless plating, etc.) a conductive material over the semiconductor substrate 104 and in the opening (2302 of FIG. 23) and patterning the conductive material. The conductive pad 134 may be or include, for example, aluminum, copper, titanium, tungsten, other conductive materials, or any combination thereof. In various embodiments, the trench fill layer 128 includes a first metal material and the conductive pad 134 includes a second metal material that is different from the first metal material.

[0061] As shown in the cross-sectional view 2500 of FIG. 25, a fourth dielectric layer 208 is formed over the third dielectric layer 206 and the conductive pad 134, thereby forming an upper dielectric structure 132. Further, a plurality of microlenses 136 are formed on the fourth dielectric layer 208. The upper dielectric structure 132 includes the first dielectric layer 202, the second dielectric layer 204, the third dielectric layer 206, and the fourth dielectric layer 208. In some embodiments, a planarization process (e.g., a CMP process) is performed on the fourth dielectric layer 208 such that the upper dielectric structure 132 has a thickness t1. In some embodiments, the thickness t1 is about 4700 Å, in a range between about 3000 Å and about 6000 Å, or other suitable value.

[0062] 26-36 depict cross-sectional views 2600-3600 of several embodiments of a method for forming an image sensor including an isolation structure protruding into an upper dielectric structure above a semiconductor substrate. Although the cross-sectional views 2600-3600 shown in FIGS. 26-36 are described with reference to a method, it should be understood that the structures shown in FIGS. 26-36 are not limited to the method, but rather may stand alone apart from the method. Furthermore, although FIGS. 26-36 are described as a sequence of operations, it should be understood that the operations are not limiting, and the order of operations may be changed in other embodiments, and the disclosed method may be applicable to other structures. In other embodiments, some operations shown and / or described may be omitted in whole or in part.

[0063] As shown in cross-sectional view 2600 of Figure 26, a plurality of photodetector elements 120 are formed in a semiconductor substrate 104, and a plurality of pixel elements 112 and interconnect structures 102 are formed on a front surface 104f of the semiconductor substrate 104. In some embodiments, the structure of Figure 26 is formed as shown and / or described in Figures 6-8.

[0064] 27, an etching process is performed on the backside surface 104b of the semiconductor substrate 104 to form a plurality of protrusions 402 above the light receiving elements 120. In some embodiments, the etching process includes wet etching, dry etching, other suitable etching, or any combination thereof. In various embodiments, the etching process includes forming a masking layer (not shown) above the backside surface 104b, etching the semiconductor substrate 104 according to the masking layer (e.g., by a dry etching process, a wet etching process), and removing the masking layer.

[0065] As shown in cross-sectional view 2800 of FIG. 28, the passivation layer 130 is deposited on the backside surface 104b of the semiconductor substrate 104, and the first dielectric layer 202 is deposited on the passivation layer 130. The passivation layer 130 and the first dielectric layer 202 are deposited by a conformal deposition process and conform to the shape of the protrusion. In some embodiments, the passivation layer 130 and the first dielectric layer 202 are deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In some embodiments, the passivation layer 130 includes a high-k dielectric material and the first dielectric layer 202 includes an oxide (e.g., silicon dioxide) having a lower dielectric constant than the passivation layer 130.

[0066] As shown in cross-sectional view 2900 of FIG. 29, the second dielectric layer 204 is deposited on the first dielectric layer 202. In some embodiments, the second dielectric layer 204 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In further embodiments, a planarization process (e.g., a CMP process) is performed on the second dielectric layer 204 such that the top surface of the second dielectric layer 204 is substantially flat. In still further embodiments, the thickness of the second dielectric layer 204 is greater than the thickness of the first dielectric layer 202 and greater than the thickness of the passivation layer 130.

[0067] 30, a patterning process is performed on the backside surface 104b of the semiconductor substrate 104 to form isolation openings 3002 extending into the backside surface 104b. In some embodiments, the patterning process includes forming a masking layer (not shown) over the second dielectric layer 204, etching the semiconductor substrate 104 according to the masking layer (e.g., by a dry etching process, a wet etching process, etc.), and removing the masking layer.

[0068] As shown in cross-sectional view 3100 of FIG. 31, a first liner layer 124 is deposited over the semiconductor substrate 104 to line the isolation opening 3002, and a second liner layer 126 is deposited on the first liner layer 124. In some embodiments, the first liner layer 124 and the second liner layer 126 are each deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. The first liner layer 124 may be or include a high-k dielectric material, such as, for example, aluminum oxide, hafnium oxide, titanium oxide, other high-k dielectric materials, other dielectric materials, or any combination of the above. The second liner layer 126 may be or include, for example, silicon dioxide, other suitable dielectric materials, etc.

[0069] As shown in cross-sectional view 3200 of FIG. 32, a trench fill layer 128 is deposited on the second liner layer 126 and in the isolation opening (3002 of FIG. 31). In various embodiments, the trench fill layer 128 is deposited on the second liner layer 126 by a CVD process, a PVD process, an ALD process, electrolytic plating, electroless plating, or other suitable growth or deposition process. The trench fill layer 128 may be or include, for example, polysilicon, doped polysilicon, metals such as tungsten or aluminum, other metallic materials, or any combination of the above. In some embodiments, prior to depositing the trench fill layer 128, a blanket etch process may be performed (not shown) to remove portions of the second liner layer 126 and / or the first liner layer 124 that are deposited on the top surface of the second dielectric layer 204. In various embodiments, after the blanket etch process, the top surfaces of the first and second liner layers 124, 126 are aligned with the top surface of the second dielectric layer 204 (eg, as depicted in FIG. 2).

[0070] As shown in cross-sectional view 3300 of FIG. 33, a removal process is performed to remove excess material from above the second dielectric layer 204, thereby forming isolation structures 122 extending into the semiconductor substrate 104. In some embodiments, the removal process includes performing an etching process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 to remove excess material from above the second dielectric layer 204. In various embodiments, the etching process includes a dry etch, a blanket etch, and / or the like. The etching process may overetch to remove at least a portion of the second dielectric layer 204. In still further embodiments, the removal process includes performing a CMP process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 until a top surface of the second dielectric layer 204 is reached. In various embodiments, the top surface of the isolation structures 122 is coplanar with the top surface of the second dielectric layer 204. The removal process is further performed such that the isolation structure 122 includes an upper portion 122up that extends above the semiconductor substrate 104 and has a height h1. In various embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is in a range between about 800 Å and about 1300 Å, in a range between about 800 Å and about 1050 Å, in a range between about 1050 Å and about 1300 Å, or other suitable value. In still further embodiments, the height ht of the isolation structure 122 is less than the height hs of the semiconductor substrate 104.

[0071] As shown in cross-sectional view 3400 of FIG. 34, the third dielectric layer 206 is deposited over the isolation structures 122, and a patterning process is performed to form an opening 3402 in the peripheral region 105 of the semiconductor substrate 104. In some embodiments, the third dielectric layer 206 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In various embodiments, the patterning process includes forming a masking layer (not shown) over the third dielectric layer 206, performing an etching process (e.g., dry etching, wet etching, etc.) according to the masking layer, and removing the masking layer. The opening 3402 exposes a portion of the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105.

[0072] As shown in cross-sectional view 3500 of FIG. 35, a conductive pad 134 is formed in the opening (3402 in FIG. 34) and on the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105. In some embodiments, a process for forming the conductive pad 134 includes depositing (e.g., by CVD, PVD, ALD, electrolytic plating, electroless plating, etc.) a conductive material over the semiconductor substrate 104 and in the opening (3402 in FIG. 34) and patterning the conductive material. The conductive pad 134 may be or include, for example, aluminum, copper, titanium, tungsten, other conductive materials, or any combination thereof. In various embodiments, the trench fill layer 128 includes a first metal material and the conductive pad 134 includes a second metal material that is different from the first metal material.

[0073] As shown in cross-sectional view 3600 of FIG. 36, a fourth dielectric layer 208 is formed over the third dielectric layer 206 and the conductive pad 134, thereby forming an upper dielectric structure 132. Further, a plurality of microlenses 136 are formed on the fourth dielectric layer 208. The upper dielectric structure 132 includes the first dielectric layer 202, the second dielectric layer 204, the third dielectric layer 206, and the fourth dielectric layer 208. In some embodiments, a planarization process (e.g., a CMP process) is performed on the fourth dielectric layer 208 such that the upper dielectric structure 132 has a thickness t1. In some embodiments, the thickness t1 is about 4700 Å, in a range between about 3000 Å and about 6000 Å, or other suitable value.

[0074] 37-45 depict cross-sectional views 3700-4500 of several embodiments of a method for forming an image sensor including an isolation structure protruding into an upper dielectric structure above a semiconductor substrate. Although the cross-sectional views 3700-4500 shown in FIGS. 37-45 are described with reference to a method, it should be understood that the structures shown in FIGS. 37-45 are not limited to the method, but rather may stand alone apart from the method. Furthermore, although FIGS. 37-45 are described as a sequence of operations, it should be understood that the operations are not limiting, and the order of operations may be changed in other embodiments, and the disclosed method may be applicable to other structures. In other embodiments, some operations shown and / or described may be omitted in whole or in part.

[0075] As shown in cross-sectional view 3700 of Figure 37, a plurality of protrusions 402 are formed on the backside surface 104b of the semiconductor substrate 104, and a passivation layer 130, a first dielectric layer 202, and a second dielectric layer 204 are formed over the plurality of protrusions 402. In some embodiments, the structure of Figure 37 is formed as shown and / or described in Figures 26-29.

[0076] As shown in cross-sectional view 3800 of FIG. 38, a patterning process is performed on the backside surface 104b of the semiconductor substrate 104 to form an isolation opening 3802 extending into the backside surface 104b. In some embodiments, the patterning process includes forming a masking layer (not shown) over the second dielectric layer 204, etching the semiconductor substrate 104 according to the masking layer (e.g., by a dry etching process, a wet etching process, etc.), and removing the masking layer. In various embodiments, the patterning process is performed until the top surface of the STI structure 118 is reached. In yet further embodiments, the patterning process is performed (not shown) such that the bottom of the isolation opening 3802 is disposed vertically above the top surface of the STI structure 118 (e.g., as depicted in FIG. 11).

[0077] As shown in cross-sectional view 3900 of FIG. 39, a first liner layer 124 is deposited over the semiconductor substrate 104 to line the isolation opening 3802, and a second liner layer 126 is deposited on the first liner layer 124. In some embodiments, the first liner layer 124 and the second liner layer 126 are each deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. The first liner layer 124 may be or include a high-k dielectric material, such as, for example, aluminum oxide, hafnium oxide, titanium oxide, other high-k dielectric materials, other dielectric materials, or any combination of the above. The second liner layer 126 may be or include, for example, silicon dioxide, other suitable dielectric materials, etc.

[0078] As shown in cross-sectional view 4000 of FIG. 40, trench fill layer 128 is deposited on second liner layer 126 and in isolation opening (3802 in FIG. 39). In various embodiments, trench fill layer 128 is deposited above second liner layer 126 by a CVD process, a PVD process, an ALD process, electrolytic plating, electroless plating, or other suitable growth or deposition process. Trench fill layer 128 may be or include, for example, polysilicon, doped polysilicon, metal such as tungsten or aluminum, other metallic materials, or any combination of the above. In some embodiments, prior to depositing trench fill layer 128, a blanket etch process may be performed (not shown) to remove portions of second liner layer 126 and / or first liner layer 124 deposited on the top surface of second dielectric layer 204. In various embodiments, after the blanket etch process, the top surfaces of the first and second liner layers 124, 126 are aligned with the top surface of the second dielectric layer 204 (eg, as depicted in FIG. 2).

[0079] As shown in cross-sectional view 4100 of FIG. 41 , a removal process is performed to remove excess material from above the second dielectric layer 204, thereby forming isolation structures 122 extending into the semiconductor substrate 104. In some embodiments, the removal process includes performing an etching process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 to remove excess material from above the second dielectric layer 204. In various embodiments, the etching process includes a dry etch, a blanket etch, and / or the like. The etching process may overetch to remove at least a portion of the second dielectric layer 204. In still further embodiments, the removal process includes performing a CMP process in the first liner layer 124, the second liner layer 126, and / or the trench fill layer 128 until a top surface of the second dielectric layer 204 is reached. In various embodiments, the top surface of the isolation structures 122 is coplanar with the top surface of the second dielectric layer 204. The removal process is further performed such that the isolation structure 122 includes an upper portion 122up that extends above the semiconductor substrate 104 and has a height h1. In various embodiments, the height h1 of the upper portion 122up of the isolation structure 122 is in a range between about 800 Å and about 1300 Å, in a range between about 800 Å and about 1050 Å, in a range between about 1050 Å and about 1300 Å, or other suitable value. In some embodiments, the height h1 of the isolation structure 122 is greater than the height hs of the semiconductor substrate 104. In still further embodiments, the isolation structure 122 is formed such that the height ht of the isolation structure 122 is less than the height hs of the semiconductor substrate 104 (e.g., as depicted in FIG. 5D ).

[0080] As shown in cross-sectional view 4200 of FIG. 42, a metal grid structure 502 is formed on the isolation structure 122. In some embodiments, a method for forming the metal grid structure 502 includes depositing a metal material above the backside surface 104b of the semiconductor substrate 104 (e.g., by a CVD process, a PVD process, an ALD process, electrolytic plating, electroless plating, etc.) and patterning the metal material. In further embodiments, the metal grid structure 502 is formed simultaneously with the isolation structure 122, the metal grid structure 502 is defined from the removal process of FIG. 41, and the metal grid structure 502 and the trench fill layer 128 are a single continuous structure (e.g., as shown and / or described in FIG. 5C). In yet further embodiments, the patterning process is performed such that the center of the metal grid structure 502 is shifted from the center of the isolation structure 122 in a direction toward the peripheral region 105 of the semiconductor substrate 104 (e.g., as shown and / or described in FIG. 5B). In various embodiments, the metal grid structure 502 comprises the same metal material as the trench fill layer 128 .

[0081] As shown in cross-sectional view 4300 of FIG. 43, the third dielectric layer 206 is deposited over the isolation structures 122, and a patterning process is performed to form an opening 4302 in the peripheral region 105 of the semiconductor substrate 104. In some embodiments, the third dielectric layer 206 is deposited by a CVD process, a PVD process, an ALD process, or other suitable growth or deposition process. In various embodiments, the patterning process includes forming a masking layer (not shown) on the third dielectric layer 206, performing an etching process (e.g., dry etching, wet etching, etc.) according to the masking layer, and removing the masking layer. The opening 4302 exposes a portion of the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105.

[0082] As shown in cross-sectional view 4400 of FIG. 44, a conductive pad 134 is formed in the opening (4302 in FIG. 43) and on the backside surface 104b of the semiconductor substrate 104 in the peripheral region 105. In some embodiments, a process for forming the conductive pad 134 includes depositing (e.g., by CVD, PVD, ALD, electrolytic plating, electroless plating, etc.) a conductive material over the semiconductor substrate 104 and in the opening (4302 in FIG. 43) and patterning the conductive material. The conductive pad 134 may be or include, for example, aluminum, copper, titanium, tungsten, other conductive materials, or any combination thereof. In various embodiments, the trench fill layer 128 and / or the metal grid structure 502 include a first metal material and the conductive pad 134 includes a second metal material different from the first metal material.

[0083] As shown in cross-sectional view 4500 of FIG. 45, a fourth dielectric layer 208 is formed over the third dielectric layer 206 and the conductive pad 134, thereby forming an upper dielectric structure 132. Further, a plurality of microlenses 136 are formed on the fourth dielectric layer 208. The upper dielectric structure 132 includes the first dielectric layer 202, the second dielectric layer 204, the third dielectric layer 206, and the fourth dielectric layer 208. In some embodiments, a planarization process (e.g., a CMP process) is performed on the fourth dielectric layer 208 such that the upper dielectric structure 132 has a thickness t1. In some embodiments, the thickness t1 is about 4700 Å, in a range between about 3000 Å and about 6000 Å, or other suitable value.

[0084] FIG. 46 illustrates a method 4600 of forming an image sensor including an isolation structure that protrudes into an upper dielectric structure above a semiconductor substrate. Although the method 4600 is described as a series of acts or events, it should be understood that the method is not limited to the order or acts shown. Thus, in some embodiments, acts may occur in a different order than that shown and / or may occur simultaneously. Furthermore, in some embodiments, an act or event shown may be divided into multiple acts or events that may occur at different times or simultaneously with other acts or sub-acts. In some embodiments, some acts or events shown may be omitted and acts or events not shown may be included.

[0085] In an operation 4602, a plurality of photodetectors are formed in a semiconductor substrate. Figure 6 illustrates a cross-sectional view 600 corresponding to some embodiments of operation 4602.

[0086] A plurality of pixel elements and interconnect structures are formed on a front surface of a semiconductor substrate in operation 4604. Figure 8 illustrates a cross-sectional view 800 corresponding to some embodiments of operation 4604.

[0087] An etching process is performed on the backside surface of the semiconductor substrate to form a plurality of protrusions in the semiconductor substrate above the light receiving elements in operation 4606. Figure 27 depicts a cross-sectional view 2700 corresponding to some embodiments of operation 4606.

[0088] At operation 4608, a first dielectric layer and a second dielectric layer are deposited on the backside surface of the semiconductor substrate. Figures 9 and 10 depict cross-sectional views 900 and 1000 corresponding to various embodiments of operation 4608. Figures 28 and 29 depict cross-sectional views 2800 and 2900 corresponding to some embodiments of operation 4608.

[0089] In operation 4610, the first dielectric layer, the second dielectric layer, and the backside surface are patterned to form isolation openings in the semiconductor substrate. Figure 11 illustrates a cross-sectional view 1100 corresponding to various embodiments of operation 4610. Figure 19 illustrates a cross-sectional view 1900 corresponding to some embodiments of operation 4610. Figure 30 illustrates a cross-sectional view 3000 corresponding to another embodiment of operation 4610. Figure 38 illustrates a cross-sectional view 3800 corresponding to a further embodiment of operation 4610.

[0090] At operation 4612, a first liner layer, a second liner layer, and a trench fill layer are formed in the isolation opening. Figures 12 and 13 depict cross-sectional views 1200 and 1300 corresponding to various embodiments of operation 4612. Figures 20 and 21 depict cross-sectional views 2000 and 2100 corresponding to some embodiments of operation 4612. Figures 31 and 32 depict cross-sectional views 3100 and 3200 corresponding to other embodiments of operation 4612. Figures 39 and 40 depict cross-sectional views 3900 and 4000 corresponding to further embodiments of operation 4612.

[0091] At operation 4614, a removal process is performed on the first liner layer, the second liner layer, and the trench fill layer to form an isolation structure having an upper portion extending above the backside surface of the semiconductor substrate. Figure 14 illustrates a cross-sectional view 1400 corresponding to various embodiments of operation 4614. Figure 22 illustrates a cross-sectional view 2200 corresponding to some embodiments of operation 4614. Figure 33 illustrates a cross-sectional view 3300 corresponding to another embodiment of operation 4614. Figure 41 illustrates a cross-sectional view 4100 corresponding to a further embodiment of operation 4614.

[0092] In operation 4616, a metal grid structure is formed on the isolation structure, where the metal grid structure directly contacts the trench fill layer. FIG. 42 depicts a cross-sectional view 4200 corresponding to various embodiments of operation 4616.

[0093] At operation 4618, a third dielectric layer is formed over the isolation structure. Figure 15 illustrates a cross-sectional view 1500 corresponding to various embodiments of operation 4618. Figure 23 illustrates a cross-sectional view 2300 corresponding to some embodiments of operation 4618. Figure 34 illustrates a cross-sectional view 3400 corresponding to another embodiment of operation 4618. Figure 43 illustrates a cross-sectional view 4300 corresponding to a further embodiment of operation 4618.

[0094] At operation 4620, conductive pads are formed on the backside surface of the semiconductor substrate in a peripheral region laterally adjacent the plurality of light receiving elements. Figure 16 illustrates a cross-sectional view 1600 corresponding to various embodiments of operation 4620. Figure 24 illustrates a cross-sectional view 2400 corresponding to some embodiments of operation 4620. Figure 35 illustrates a cross-sectional view 3500 corresponding to another embodiment of operation 4620. Figure 44 illustrates a cross-sectional view 4400 corresponding to a further embodiment of operation 4620.

[0095] At operation 4622, a fourth dielectric layer is formed over the isolation structures and the conductive pads. Figure 17 illustrates cross-sectional views 1700 corresponding to various embodiments of operation 4622. Figure 25 illustrates cross-sectional view 2500 corresponding to some embodiments of operation 4622. Figure 36 illustrates cross-sectional view 3600 corresponding to another embodiment of operation 4622. Figure 45 illustrates cross-sectional view 4500 corresponding to a further embodiment of operation 4622.

[0096] Accordingly, in some embodiments, the present disclosure relates to an image sensor that includes a plurality of light receiving elements disposed in a semiconductor substrate, and an isolation structure disposed in the semiconductor substrate and having an upper portion protruding above a backside surface of the semiconductor substrate.

[0097] In some embodiments, the present disclosure provides an image sensor including a light receiving element disposed in a semiconductor substrate, a dielectric structure disposed on a first side of the semiconductor substrate, and an isolation structure extending from the dielectric structure into the first side of the semiconductor substrate, the isolation structure laterally encapsulating the light receiving element and including an upper portion disposed above the first side of the semiconductor substrate and directly contacting a sidewall of the dielectric structure, the isolation structure including a first material different from a second material of the dielectric structure. In one embodiment, the isolation structure includes a trench fill layer and a first liner layer disposed between the semiconductor substrate and the trench fill layer, the trench fill layer including a first material, the first liner layer including a third material different from the first material, the first material including a metal. In one embodiment, the third material is different from the second material. In one embodiment, the isolation structure further comprises a second liner layer disposed between the trench fill layer and the first liner layer, the second liner layer comprising a second material. In one embodiment, the image sensor further comprises a metal grid structure overlying the isolation structure and directly contacting a top surface of the isolation structure. In one embodiment, a height of a top of the isolation structure is greater than a height of the metal grid structure. In one embodiment, a height of the isolation structure is greater than a height of the semiconductor substrate. In one embodiment, the image sensor further comprises a passivation layer disposed between the dielectric structure and the first side of the semiconductor substrate, the top surface of the isolation structure being vertically above the top surface of the passivation layer. In one embodiment, the image sensor comprises a dielectric structure disposed within the dielectric structure above the first side of the semiconductor substrate. Conductive shielding structure and a top surface of the isolation structure is Conductive shielding structure is provided between the upper and lower surfaces.

[0098] In some embodiments, the present disclosure provides an image sensor including a light receiving element disposed in a semiconductor substrate including a first side opposite a second side, an interconnect structure disposed on the first side of the semiconductor substrate, a dielectric structure disposed on the second side of the semiconductor substrate, a metal grid structure disposed in the dielectric structure, and an isolation structure disposed in the semiconductor substrate, the metal grid structure being vertically offset from the second side of the semiconductor substrate by a first distance, the light receiving element being spaced between opposing sidewalls of the metal grid structure, and the isolation structure including a top portion extending continuously along the first distance from the second side of the semiconductor substrate to a bottom surface of the metal grid structure. In one embodiment, the height of the top portion of the isolation structure is in the range of about 800 Å to about 1300 Å. In one embodiment, the isolation structure includes a trench fill layer, the trench fill layer and the metal grid structure including a first metal material. In one embodiment, the isolation structure further includes a first liner layer disposed between the trench fill layer and the semiconductor substrate, and a second liner layer disposed between the first liner layer and the trench fill layer, where a top surface of the first liner layer and a top surface of the second liner layer directly contact a bottom surface of the metal grid structure. In one embodiment, the image sensor further includes a conductive pad disposed on the second side of the semiconductor substrate, where a top surface of the isolation structure is disposed between a top surface and a bottom surface of the conductive pad, and the conductive pad includes a second metal material different from the first metal material. In one embodiment, there is no dielectric material between the top surface of the trench fill layer and the bottom surface of the metal grid structure. In one embodiment, the image sensor further includes a shallow trench isolation (STI) structure disposed on the first side of the semiconductor substrate, where a top surface of the STI structure directly contacts a bottom surface of the isolation structure.

[0099] In some embodiments, the present disclosure provides a method for forming an image sensor, the method including forming a light receiving element in a semiconductor substrate, the semiconductor substrate including a front surface opposite a back surface, forming an interconnect structure on the front surface of the semiconductor substrate, depositing a first dielectric layer and a second dielectric layer on the back surface of the semiconductor substrate, and forming an isolation structure extending into the back surface of the semiconductor substrate, the isolation structure including a top portion disposed vertically above the back surface and directly contacting a sidewall of the second dielectric layer, the isolation structure including a first material different from a second material of the second dielectric layer. In one embodiment, the method further includes forming a metal grid structure above the back surface of the semiconductor substrate, the metal grid structure directly contacting a top surface of the isolation structure, the metal grid structure including a first material. In one embodiment, the method further includes patterning the back surface of the semiconductor substrate to form a plurality of protrusions above the light receiving element before depositing the first dielectric layer. In one embodiment, the height of the plurality of protrusions is less than the height of the top portion of the isolation structure.

[0100] The foregoing outlines features of some embodiments so that those skilled in the art may more easily understand aspects of the present disclosure. Those skilled in the art should appreciate that this disclosure may be readily used as a basis for designing or modifying other processes and structures to carry out the same purposes and / or achieve the same advantages as the embodiments presented herein. Those skilled in the art should also appreciate that such equivalent structures do not depart from the spirit and scope of the present disclosure, and that various modifications, substitutions, and alterations may be made without departing from the spirit and scope of the present disclosure. [Industrial Applicability]

[0101] The image sensors and methods of forming the image sensors of the present disclosure may be applied to a variety of electronic devices, including CMOS image sensors. [Explanation of symbols]

[0102] 100, 200, 300, 400a, 400b, 500a, 500b, 500c, 500d, 600, 700, 800, 900, 1000, 1100, 1200, 1300, 1400, 1500, 1600, 1700, 1800, 1900, 2000, 2100, 2200, 2300, 2400, 2500, 2600, 2700, 2800, 2900, 3000, 3100, 3200, 3300, 3400, 3500, 3600, 3700, 3800, 3900, 4000, 4100, 4200, 4300, 4400, 4500: Cross-section 102: Interconnect structure 103: Pixel area 104: Semiconductor substrate 104b: Back surface of 104 104f: Front surface of 104 105: Surrounding area 106: Interconnect dielectric structure 108: Conductive wire 110: Conductive via 112: Pixel element 114: Gate dielectric layer 116: Gate electrode 118:STI structure 120: Light receiving element 122: Isolation structure 122up: Top of 122 124: First liner layer 126: Second liner layer 128: Trench filling layer 128a: First isolation structure segment 130: Passivation layer 132: Upper dielectric structure 134: Conductive pad 134ls: The underside of 134 134us:Top of 134 136: Microlens 202: First dielectric layer 204: second dielectric layer 206: Third dielectric layer 208: Fourth dielectric layer 402: Protrusion 502: Metal grid structure 502a: First grid segment Center of 504:128a Center of 506:502a 1102, 1902, 3002, 3802: Isolation opening 1502, 2302, 3402, 4302: Opening 4600: Method 4602, 4604, 4606, 4608, 4610, 4612, 4614, 4616, 4618, 4620, 4622: Operation A-A': Section line d1: distance h1, hp, hs, ht: height t1: thickness

Claims

1. A light receiving element provided in a semiconductor substrate; a dielectric structure disposed on a first side of the semiconductor substrate; an isolation structure extending from the dielectric structure into the first side of the semiconductor substrate; Including, the semiconductor substrate includes a plurality of protrusions disposed on the first side of the semiconductor substrate above the light receiving elements; the isolation structure laterally envelops the light receiving element, the isolation structure including an upper portion disposed above the first side of the semiconductor substrate and in direct contact with a sidewall of the dielectric structure; the isolation structure includes a first material that is different from a second material of the dielectric structure; the isolation structures are configured to direct incident light toward the corresponding light receiving elements; a height of the plurality of protrusions is less than a height of the top of the isolation structure; Image sensor.

2. the isolation structure includes a trench fill layer and a first liner layer disposed between the semiconductor substrate and the trench fill layer; the trench fill layer comprises the first material, and the first liner layer comprises a third material different from the first material; the first material comprises a metal; 2. The image sensor of claim 1.

3. 10. The image sensor of claim 1, further comprising a metal grid structure overlying and directly contacting a top surface of said isolation structure.

4. a passivation layer disposed between the dielectric structure and the first side of the semiconductor substrate; a top surface of the isolation structure is vertically above a top surface of the passivation layer; 2. The image sensor of claim 1.

5. a conductive shielding structure disposed within the dielectric structure above the first side of the semiconductor substrate; a top surface of the isolation structure is disposed between the upper surface and the lower surface of the conductive shielding structure; 2. The image sensor of claim 1.

6. a light receiving element disposed in a semiconductor substrate including a first side opposite a second side; an interconnect structure disposed on the first side of the semiconductor substrate; a dielectric structure disposed on the second side of the semiconductor substrate; a metal grid structure disposed within the dielectric structure; an isolation structure provided on the semiconductor substrate; Including, the semiconductor substrate includes a plurality of protrusions disposed on the first side of the semiconductor substrate above the light receiving elements; the metal grid structure is vertically offset from the second side of the semiconductor substrate by a first distance, the light receiving elements being spaced between opposing sidewalls of the metal grid structure; the isolation structure includes a top portion extending continuously along a first distance from the second side of the semiconductor substrate to a bottom surface of the metal grid structure; the isolation structures are configured to direct incident light toward the corresponding light receiving elements; a height of the plurality of protrusions is less than a height of the top of the isolation structure; Image sensor.

7. 7. The image sensor of claim 6, wherein the height of the top of the isolation structure is within a range of about 800 Å to about 1300 Å.

8. the isolation structure includes a trench fill layer; the trench fill layer and the metal grid structure comprise a first metal material; 7. The image sensor according to claim 6.

9. 1. A method for forming an image sensor, comprising: forming a light receiving element on a semiconductor substrate, the semiconductor substrate including a front surface opposite a back surface; forming an interconnect structure on the front surface of the semiconductor substrate; patterning the backside surface of the semiconductor substrate to form a plurality of protrusions above the light receiving elements; depositing a first dielectric layer and a second dielectric layer on the backside surface of the semiconductor substrate; performing a patterning process on the backside surface of the semiconductor substrate to form isolation openings extending into the backside surface of the semiconductor substrate; forming an isolation structure in the isolation opening extending into the backside surface of the semiconductor substrate, the isolation structure including an upper portion disposed vertically above the backside surface and directly contacting sidewalls of the first dielectric layer and the second dielectric layer, the isolation structure including a first material different from a second material of the second dielectric layer; Including, the isolation structures are configured to direct incident light toward the corresponding light receiving elements; a height of the plurality of protrusions is less than a height of the top of the isolation structure; A method for forming an image sensor.

10. forming a metal grid structure above the backside surface of the semiconductor substrate; the metal grid structure directly contacts a top surface of the isolation structure; the metal grid structure comprises the first material; A method for forming the image sensor of claim 9.

Citation Information

Patent Citations

  • Image sensor adopting deep groove isolation and manufacturing method thereof

    CN104637968A

  • Solid-state imaging device

    JP2014022448A

  • Solid-state imaging device, method of manufacturing the same, and electronic apparatus

    JP2016100347A

  • Image sensor and method of manufacturing the same

    KR1020170071184A

  • CMOS image sensor structure with crosstalk improvement

    US20170077157A1