Manufacturing process for producing sealed disposable food containers using a sealing head with a specific profile having ribs

The sealing process with a ribbed sealing head effectively addresses wrinkles on paper/PLA laminate containers, ensuring a hermetic seal and maintaining content quality without additional materials, thus meeting consumer demands for eco-friendly packaging.

JP7568623B2Active Publication Date: 2024-10-16SOCIETE DES PRODUITS NESTLE SA
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021532476
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-12-19
Filing Date
2019-12-17
Publication Date
2024-10-16
Estimated Expiration
2039-12-17

AI Technical Summary

Technical Problem

Disposable containers made from paper/PLA laminates face issues with wrinkles on the rim during sealing, leading to gas and vapor leakage, which compromises the quality of the contents due to insufficient oxygen and vapor barrier properties.

Method used

A sealing process using a sealing head with a first die featuring a circumferentially continuous rib on its sealing surface to flatten wrinkles on the rim, creating a continuous sealing groove that ensures a hermetic seal without additional encapsulating materials.

Benefits of technology

The process achieves a hermetic seal on paper/PLA laminate containers, maintaining content quality by preventing gas and vapor ingress, while reducing manufacturing complexity and cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007568623000001
    Figure 0007568623000001
  • Figure 0007568623000002
    Figure 0007568623000002
  • Figure 0007568623000003
    Figure 0007568623000003
Patent Text Reader

Abstract

The present invention relates to a manufacturing process for producing a sealed disposable food container, comprising the steps of forming a container body (30) having a peripheral rim (31), placing the container body in a sealing head having a first die (2) and a second die (8), the first and second dies (2, 8) having cooperating annular sealing surfaces (4, 10) facing the peripheral rim (31), and sealing a closure lid (34) placed on the container body with the peripheral rim (31) by applying the first and second dies (2, 8) against each other. According to the present invention, the first die (2) is provided with a continuous annular rib (6) on its sealing surface (4), the rib having a height (h) at least equal to the maximum depth of wrinkles that may appear on the rim when forming the container body, whereby a sealing groove (12) is formed by the rib (6) on one side of the rim during sealing.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to containers, and more particularly to disposable containers sealed with a lidding film or other top designed to minimize air or vapor flow into the container. Such containers are used for food products, such as coffee pods used in beverage systems.

[0002] Disposable containers sealed by a lidding film are well known. Such containers usually have a container body having a sidewall or sidewalls and a rim extending outwardly from a top of the sidewall(s); a lid film or similar that closes the top of the container body by sealing with a rim; Includes. [Background technology]

[0003] Some known container bodies are manufactured from a laminated material that includes a plastic barrier.

[0004] On the other hand, single-use plastic barrier containers already on the market exhibit good sealing between the container body and the lid due to the stretchability of the plastic, which is about 600%. The rim of the plastic thermoformed / injected container body has a flat surface and a certain thickness. Therefore, the sealing of the lid onto the rim of such a container body is strong.

[0005] Meanwhile, consumers are demanding more ecological and environmentally friendly packaging materials that have a "natural" appealing aspect.

[0006] PLA laminates (such as PLA / PVOH / PLA) (PLA stands for polylactic acid and PVOH stands for polyvinyl alcohol) are compostable, while paper provides a "natural" feel. Thus, a disposable container body made from paper / PLA laminate would answer consumer concerns. Heat sealing is done by the PLA plastic material.

[0007] Unfortunately, the elasticity of paper is about 10%. Therefore, in a container body manufactured from such a paper material, wrinkles (up to 1 mm) appear on the surface of the container rim when the flat paper is formed into a three-dimensional shape. Thus, channels are formed between the container body and the closure lid or between the layers of the paper laminate material. Such channels allow gas and vapor (moisture) to enter the container, which is detrimental to the quality of the raw materials contained inside after the storage period. During heat sealing with a normal heat sealing head, the wrinkles remain to some extent and no seal is ensured at the wrinkles. Thus, even if a partially effective seal can be created, the contents of the container are still exposed to some amount of external air and moisture that penetrates through these wrinkles. This in turn promotes the spoilage of the contents of the container. The oxygen and vapor barrier properties at the rim are not fully obtained.

[0008] A known solution is to add a plastic rim to ensure a smooth and uniform rim surface. Such a container with an encapsulated rim feature is disclosed in EP 1485178. In fact, EP 1485178 proposes various container bodies with fully or partially encapsulated rims or flanges. The encapsulating material is generally made of a plastic such as polyolefin, nylon, polyethylene terephthalate, polycarbonate, or other engineering thermoplastics. This encapsulating material covers at least a portion of the rim or flange and can extend a distance from the outer edge of the rim. The outside of the encapsulating material is substantially smooth even if those portions fill or cover the irregularities of the rim. Furthermore, the encapsulated rim presents a hermetic barrier against gases and moisture and may be sealed with a film or other material to completely isolate the inside of the container.

[0009] However, the polymers used for encapsulation are expensive and the amount used increases the cycle time required to form a useful container body, further complicating the manufacturing process.

[0010] To reduce the impact of encapsulation of the rim on manufacturing costs and time, EP 1485178 proposes reducing the amount of polymer by encapsulating only a portion of the rim or flange. For example, only the underside of the rim is covered with encapsulation material. By injecting resin only on the underside or backside of the rim during the injection molding process, the paperboard pleats exposed on the top surface of the rim are pressed upwards against the surface of the metal mold by the hot and high pressure injected material, thereby compressing or "ironing" the pleats on the top surface of the flange. This creates an improved sealing surface on the top side, which helps ensure that a hermetic seal is obtained across the now flattened pleats. Furthermore, the smooth surface of the encapsulated underside of the rim can also be bonded to the lid while the lid is bent downwards.

[0011] Nevertheless, this solution still uses an encapsulating material and the injection of this material into a mold, so the manufacturing costs and time are reduced, but only very slightly, and furthermore, this solution falls short of consumer expectations for more natural and renewable products.

[0012] In another solution disclosed in WO 2015 / 082268 to Billerud, wrinkles created by three-dimensional deformation of the paper layer of the container body are reclosed by spraying or otherwise coating with a material to "fill" the wrinkles before the top lid is sealed thereto. This solution has the disadvantage of requiring an additional component to the pod's structure (i.e., the rim coating material) and also additional spraying steps and equipment that add cost and complexity to the process.

[0013] Therefore, there is a need to develop a method to ensure proper sealing of the paper / PLA laminate using current manufacturing techniques and without adding any additional container elements. Summary of the Invention

[0014] It is an object of the present invention to provide a simpler and less costly manufacturing process for producing sealed disposable food containers such as coffee pods, in particular to avoid the need to even partially encapsulate the rim of the pod.

[0015] The manufacturing method of the present invention also aims to obtain an efficient seal on the rim of the disposable food container, even with a container body made from a paper / PLA laminate, to ensure in-cup quality and adequate shelf life due to efficient oxygen and vapor barrier properties.

[0016] In other words, the objective of the present invention is to provide a new environmentally friendly pod that does not have an encapsulated rim feature, but is at least as sealed as conventional pods that have an encapsulated rim feature.

[0017] For this purpose, the manufacturing process for producing the sealed disposable food container according to the invention comprises the steps of: forming a container body having a peripheral upper rim; placing the container body in a sealing head having a first die and a second die, at least one of the first die and the second die being movable, the first die and the second die having cooperating annular sealing surfaces facing the rim; applying a closure lid, such as a lidding film, onto the container body disposed on the sealing head; sealing the closure lid with the rim of the container body by applying a first die and a second die against each other; Includes.

[0018] The process according to the invention is characterized in that the first die of the sealing head is provided with an annular rib on its sealing surface, the rib extending continuously in a circumferential direction substantially all around the sealing surface and having a height at least equal to the maximum depth of wrinkles that may appear on the rim when the container body is formed, so that when the closure lid is sealed to the container body, a continuous sealing groove is recessed by the rib on one side of the rim (all around the rim) and the closure lid is joined to the peripheral rim in front of this sealing groove.

[0019] It should be noted that the sealing step in the process according to the invention can use heat sealing or ultrasonic sealing techniques, whereby the sealing head can be equipped with a heating element or means for generating ultrasonic vibrations. Other types of sealing are also possible, for example induction sealing.

[0020] Furthermore, in all descriptions, the "sealing surface" of the die refers to the surface of the die that contacts, or more generally acts on, the lid or container body during sealing. This surface may have the same dimensions as the rim, or it may be smaller. Furthermore, the sealing surfaces of the two dies may have different widths.

[0021] During sealing, the ribs of the first die flatten the wrinkles and erase the channels between the two membranes, creating one continuous sealing line.

[0022] Preferably, the height of the rib is less than the thickness of the container body.

[0023] The ribs of the first die of the sealing head according to the invention allow the container body to be manufactured from a sheet of paper / PLA laminate using a very simple manufacturing process, which can be summarized as a seal stamping step with a very basic sealing head, which is just a heating or ultrasonic press without any injection element. The only peculiarity of the sealing head is the design of its seal, which includes ribs, the height of which is higher than the wrinkle depth at the rim.

[0024] Please note that in all descriptions, the term "a" means "at least one" (but not "one and only one") unless otherwise specified. Thus, the first die may have two or more concentric ribs on its sealing surface.

[0025] Preferably, the sealing head is a vertical press head, i.e., the sealing head is arranged so that the movable die translates vertically (so that the sealing line lies in a horizontal plane), and the sealing head has an upper die and a lower die.

[0026] In such a configuration, the first die (having the ribs) may be the upper die and the second die may be the lower die, whereby the sealing groove recessed by the ribs is formed in the upper surface of the rim, or the first die may be the lower die and the second die may be the upper die, whereby the sealing groove is formed in the lower surface of the rim.

[0027] The sealing surface of the second die may be flat, more particularly flat and rigid, or may comprise a sealing groove or a rubber sheet in front of the ribs of the first die.

[0028] In a preferred embodiment, the first die is the lower die of a vertical press (the second die is the upper die), and the sealing surface of the second die is flat and rigid. Thus, the sealing groove is formed by the rib on the underside of the rim, and the upper surface of the closing lid remains flat in front of the rim. Thus, if a reference code is printed on the upper surface of the closing lid at the rim, this reference code will not be deformed by the sealing process, and the sealing groove on the underside of the rim will not prevent the reading of this reference code.

[0029] Preferably, the container body, the rim and the sealing surface of the sealing head have circular portions, in which case the ribs of the first die are also advantageously circular.

[0030] The invention also relates to an apparatus used to carry out the manufacturing process according to the invention. In particular, the invention relates to a sealing head for sealing a closure lid onto a rim of a container body of a disposable food container, the sealing head comprising a first die and a second die, one of which is movable, the first die and the second die having cooperating annular sealing surfaces facing the rim when the container body is placed on the sealing head, the sealing head being characterized in that the first die is provided on its sealing surface with an annular rib, the rib having a height at least equal to the maximum depth of wrinkles that may appear in the rim when forming the container body.

[0031] In a preferred embodiment adapted for producing pods such as coffee pods, the annular sealing surface of the die and the ribs of the first die are all circular.

[0032] In a preferred embodiment, particularly suitable for producing coffee pods made from sheets of paper / PLA laminate, the height of the ribs is at least equal to 0.7 mm, preferably at least equal to 1 mm.

[0033] More generally, the height of the rib is preferably 0.1 mm to 4 mm, and the width of the rib is preferably 0.15 mm to 6 mm, and further, the width of the rib is preferably less than three times the height of the rib.

[0034] The present invention also relates to a sealed disposable food container obtained by the manufacturing process according to the invention. In particular, the sealed disposable food container comprises a container body having a peripheral rim and a closure lid closing the container body. The sealed disposable food container comprises: a container body made of a paper laminate material and having at least a rim with substantially radially extending creases; A sealed disposable container exhibits an annular sealing groove recessed into one side of the rim, the annular sealing groove extending continuously in a circumferential direction substantially all around the rim and having a depth at least equal to the maximum depth of the wrinkles, whereby the wrinkles are flattened by the sealing groove and the closure lid is joined to the peripheral rim of the container body at least in the area of ​​the sealing groove. It is characterized by:

[0035] With respect to the first feature above, the term "paper laminate material" means that the material constituting the container body includes several layers, one of which is a paper sheet, and furthermore, the wrinkles are a result of forming the (3D (three-dimensional)) container body from a 2D (two-dimensional) blank of the paper laminate material.

[0036] With regard to the second feature, a direct result of the sealing groove (by flattening the wrinkles) is that the upper surface of the rim of the container body is flat in front of the groove and therefore can sealingly join to the closure lid in that area.

[0037] In a preferred embodiment, the closure lid has a flat upper surface at least at the rim.

[0038] In a preferred embodiment, the sealing groove is recessed into the underside of the rim.

[0039] Preferably, the container body is manufactured from a sheet of paper / PLA laminate.

[0040] In a more preferred embodiment, the container body has a weight of 130 g / m 2 The closure lid is made from a sheet of 50μm PLA-PVOH-PLA laminated with 30g / m formable paper. 2 It is made from a sheet containing a PLA barrier laminated with paper.

[0041] The sealing groove recessed into one surface of the rim may have a height of 0.05 mm to 3 mm and a width of 0.15 mm to 5 mm. Furthermore, the width of the sealing groove is preferably less than three times the height of the rib, and more preferably the width and height of the sealing groove are equal.

[0042] Additional features and advantages of the present invention will be described in, or will be apparent from, the description of the presently preferred embodiments presented below with reference to the drawings. [Brief description of the drawings]

[0043] [Figure 1] FIG. 1 is a schematic perspective view of a container body according to the present invention or the prior art. [Diagram 2] 1 is a schematic cross-sectional view of a disposable food container according to the present invention. [Diagram 3] 1 is a schematic cross-sectional view of a forming apparatus that can be used in a manufacturing process according to the present invention; [Figure 4] 1 is a schematic cross-sectional view of a portion of one embodiment of a sealing head according to the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0044] The first step of the manufacturing process according to the invention aims to produce a 3D container body, such as the container body 100 shown in Figures 1 and 2, from a 2D blank 10 shown in Figure 3. The forming process used in the manufacturing process according to the invention can be selected from known sliding blank processes, such as stamping processes or deep drawing processes (sliding of the blank into the mold and lateral contraction of the blank causes microfolding of the blank), or from known fixed blank processes, such as air forming / vacuum forming processes and heat pressing processes (the container is substantially formed by distortion of the blank), depending on the desired shape of the container body (specifically the desired depth), the material of the blank, etc.

[0045] For example, the shaping of the container body may be performed by deep drawing using a press as shown in FIG. 3, with a male die 20, the female moulding die being absent and may be present as a counterholder 21, as shown or used to emboss the underside of the shape. The 2D blank 10 is placed in the moulding machine, where it is clamped by a blank holder 24 with a given force F, and then the male die 20 starts its downward movement towards the counterholder 21 along the moulding cavity 22, where the actual shaping takes place. Finally, the shape is released from the moulding device. The moulding cavity is preferably surrounded by a heating element 23. A heating element 23' may also be provided in the male die 20.

[0046] The entire forming sequence can be several seconds long. The selection of forming parameters such as die force, blank holding force F, forming gap or clearance (the lateral distance between the edge of the forming cavity and the edge of the male die) is performed experimentally.

[0047] Concerning the forming gap, it can be noted that this distance varies, among other things, according to the thickness of the material from which the blank is produced. If the forming gap is too small, out-of-plane and in-plane shear and forces increase. This can lead to the formation of cracks and eventual failure of the material in the formed shape. Typically, the gap is about 0.7 times the thickness of the paperboard (it can be noted that dimensions and ratios are not taken into account in FIG. 3, which is very schematic). On the other hand, if the forming gap is too large, it leads to significant wrinkling that creates voids that lead to poor appearance of the shape and limit the possibility of gas-tight sealing of such shapes.

[0048] As a negative result of the molding process, the container body 100 exhibits wrinkles 103 (see FIG. 1) substantially at the rim 102 as well as at the junction between the rim 102 and the sidewall 101 and in most of the sidewall 101 .

[0049] To close the container body thus obtained, a closure lid (not shown in FIG. 1) is later sealed onto the top surface of the rim 102 after the container body 100 is filled with food. The wrinkles 103 impair the complete sealing between the closure lid and the rim, and a hermetic seal cannot be obtained. Specifically, the wrinkles formed on the surface of the rim are oriented in the radial direction of the container body 100, impairing the precise flatness of the rim. Thus, when the top lid is sealed onto the rim, radial channels are generated along the wrinkles, through which oxygen and moisture can circulate from outside the container into the internal compartment of the container, thus rapidly deteriorating the quality of the food contained therein.

[0050] To solve this problem, the invention proposes to use a sealing head, one of whose dies has a sealing surface with a particular profile. An embodiment of a sealing head according to the invention is partially represented in figure 4, with a container body 30 and a closing lid 34 inside. The sealing head comprises a fixed lower die (first die) 2 with an annular upper sealing surface 4 and a movable upper die (second die) 8 with a bottom sealing surface 10, the cooperating sealing surfaces 4 and 10 being circular and having a width corresponding to the width of the rim 31 of the container body 30.

[0051] The sealing surface 4 of the first die 2 comprises a circular rib 6, whereas the sealing surface 10 of the second die 8 is flat (planar). The rib 6 gives rise to a sealing groove 12 on the underside of the rim, which eliminates the wrinkles (such wrinkles are not represented in FIG. 4). More precisely, the formation of the grooves 12 in a direction perpendicular to the wrinkle direction causes the wrinkles to be "flattened" by forcing the material of the rim back into the empty space of each wrinkle, and thus reclosed. As a result, all wrinkles on the rim's periphery are removed by deformation of the material, at least in the area of ​​the grooves. In a highly preferred embodiment of the invention, the grooves are formed on the underside of the rim (as shown in FIG. 4), but wrinkle removal grooves may also be formed on the upper surface of the container's rim. By forming the grooves on the underside of the rim as shown in FIG. 4, the upper surface of the rim is preserved, and not only that, but the entire surface of the rim is kept in principle perfectly flat. As a result, it is much easier to later seal the top lid and maintain the integrity of the resulting container seal.

[0052] The rib 6 has dimensions h (height) and w (width) which are selected so that the sealing groove 12 recessed in the rim has a height of 0.1 mm to 3 mm and a width of 0.15 mm to 5 mm. The dimensions of the rib 6 may be slightly larger than the desired dimensions of the sealing groove 12, depending on the elasticity of the material from which the container body is made. Furthermore, the width of the rib 6 is preferably less than three times its height. In any case, according to the invention, the height of the rib 6 and the height of the sealing groove 12 must be higher than the maximum depth of the wrinkles in the container body 30, the depth of the wrinkles depending, inter alia, on the dimensions, material and molding conditions of the container body.

[0053] It should be understood that various changes and modifications to the presently preferred embodiments described herein will be apparent to those skilled in the art. Such changes and modifications can be made without departing from the spirit and scope of the present invention and without diminishing its attendant advantages. It is therefore intended that such changes and modifications be covered by the appended claims.

Claims

1. A manufacturing process for producing a sealed disposable food container that is a coffee pod for use in a beverage system, comprising: forming a container body (30) having a peripheral rim (31), said container body and said peripheral rim having a circular portion; placing the container body in a sealing head having a first die (2) and a second die (8), at least one of which is movable, the first die (2) and the second die (8) having cooperating annular sealing surfaces (4, 10) facing the peripheral rim (31); applying a closure lid (34) onto said container body (30); sealing the closure lid (34) to the peripheral rim (31) of the container body by applying the first die (2) and the second die (8) against each other; In the manufacturing process, the first die (2) is provided with an annular rib (6) on the sealing surface (4) of the first die (2), the rib having a height (h) at least equal to the maximum depth of wrinkles that may appear on the peripheral rim when the container body is formed, so that when the closure lid (34) is sealed to the container body (30), a sealing groove (12) is formed in the face of the peripheral rim by the rib (6) and the closure lid is joined to the peripheral rim in front of the sealing groove, said container body (30) being manufactured from a sheet of paper / PLA laminate; the first die (2) is the lower die of a vertical press and the second die (8) is the upper die, whereby the sealing groove (12) is recessed into the underside of the peripheral rim (31); A manufacturing process comprising:

2. The container body (30) has a weight of 130 g / m 2 The closure lid (34) is made from a sheet of 50 μm PLA-PVOH-PLA laminated with a 30 g / m formable paper. 22. The manufacturing process of claim 1, wherein the sheet is made from a sheet comprising PLA laminated with paper.

3. The manufacturing process according to claim 1 or 2, wherein the sealing surface (10) of the second die (8) is flat and rigid.

4. A sealed disposable food container which is a coffee pod for use in a beverage system, comprising a container body (30) having a peripheral rim (31) and a closure lid (34) for closing said container body, said container body and said peripheral rim having a circular portion, the container body being made of a paper laminate material and having radially extending creases at least at the peripheral rim; said sealed disposable food container presents an annular sealing groove (12) recessed into the face of said peripheral rim, said sealing groove (12) extending circumferentially and continuously all around said peripheral rim and having a depth at least equal to the maximum depth of said wrinkles, whereby said wrinkles are flattened by said sealing groove, said closure lid (34) being joined to said peripheral rim of said container body at least in the area of ​​said sealing groove (12); The sealing groove (12) recessed in the peripheral rim is formed in the underside of the peripheral rim, The container body is manufactured from a sheet of paper / PLA laminate. A sealed disposable food container.

5. 5. The sealed disposable food container of claim 4, wherein said closure lid has an upper surface that is flat at least at said peripheral rim.

6. A sealed disposable food container according to claim 4 or 5, wherein the sealing groove (12) recessed in the peripheral rim has a width of between 0.15 mm and 5 mm and a height of between 0.05 mm and 3 mm.

7. The container body (30) has a weight of 130 g / m 2 The closure lid (34) is made from a sheet of 50 μm PLA-PVOH-PLA laminated with a 30 g / m formable paper. 26. The sealed disposable food container of claim 4 or 5, made from a sheet comprising PLA laminated with paper.

8. A coffee pod, characterized in that it comprises a sealed disposable food container according to any one of claims 4 to 7.

Citation Information

Patent Citations

  • Welding method for the leaktight closure of thermoplastic containers, particularly containers intended to contain foodstuffs

    CH652965A5

  • FR01544071A

  • Paper-made laminate and paper-made container comprising the laminate

    JP2004106369A

  • Heat seal carrier assembly

    US4991375A

  • Cellulose materials and methods of making and using same

    WO2017144009A1