Manufacturing method, cylinder, circuit breaker and distribution board
The described manufacturing method for cylinders, using extrusion processing with specific punches, maintains cylindricity during forging, ensuring smooth plunger movement and improved circuit breaker performance.
Patent Information
- Application Number
- JP2020204222
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-09
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-12-09
AI Technical Summary
The use of forging methods in manufacturing cylinders for circuit breakers can lead to a decrease in cylindricity, which is crucial for smooth plunger movement and proper operation.
A manufacturing method involving extrusion processing with specific punches forms a first and second recess in the forged material, maintaining the inner diameters of these recesses in a specific relationship to stabilize the cylindricity of the cylinder.
The method effectively suppresses the decrease in cylindricity, ensuring the plunger moves smoothly within the cylinder, enhancing the operational accuracy and reliability of the circuit breaker.
Smart Images

Figure 0007578478000001 
Figure 0007578478000002 
Figure 0007578478000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a manufacturing method, a cylinder, a circuit breaker and a distribution board. [Background technology]
[0002] Conventionally, a circuit breaker is known that includes a dashpot having a bottomed cylindrical cylinder, an electromagnetic coil wound around the cylinder, a damping spring and a plunger (movable iron core) inside the cylinder, and a pole head (fixed iron core) at the opening of the cylinder. In such a circuit breaker, the plunger is attracted to the pole head by a magnetic flux formed by an overcurrent flowing through the electromagnetic coil, which reduces the magnetic resistance and attracts the armature (operating iron piece) outside the cylinder to the pole head. This activates the trip mechanism and breaks the circuit. For the circuit breaker to operate accurately, it is important that the plunger moves smoothly inside the cylinder.
[0003] A known method for producing such cylinders is drawing, in which a metal plate is sandwiched between dies and pressed (see Patent Document 1). By using drawing, it is possible to produce a cylinder with high cylindricity, that is, a cylinder in which the plunger can move smoothly. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2019-206962 A Summary of the Invention [Problem to be solved by the invention]
[0005] In addition to drawing, forging is also known as a method for processing metal formed products. Forging has the advantages of improving the mechanical properties of the metal formed products and reducing the amount of material to be cut.
[0006] However, when the above cylinder is formed by forging, there is a concern that the cylindricity of the cylinder may decrease.
[0007] Therefore, the present invention provides a cylinder manufacturing method that can suppress a decrease in cylindricity even when forging is used. [Means for solving the problem]
[0008] One embodiment of the manufacturing method of the present invention is a method for manufacturing a bottomed cylindrical cylinder for use in a dashpot, comprising the steps of: extruding a predetermined length of material to be forged with a first punch to form a first recess in the material to be forged; and extruding a bottom surface of the first recess with a second punch to form a second recess that is spatially continuous with the first recess, and the inner diameter of the first recess is larger than the inner diameter of the second recess.
[0009] A cylinder according to one aspect of the present invention is a cylinder produced by the above-mentioned manufacturing method.
[0010] A circuit breaker according to one embodiment of the present invention comprises the above-mentioned cylinder, a pole head provided at an opening of the cylinder for sealing the cylinder, and a plunger housed in the cylinder and movable in a direction toward the pole head when an overcurrent flows, wherein the length of the second recess in the direction is longer than the distance between the plunger and the pole head when no overcurrent is occurring.
[0011] A distribution board according to one aspect of the present invention includes one or more of the above-described circuit breakers. Effect of the Invention
[0012] According to the manufacturing method etc. according to one aspect of the present invention, even when a forging process is used, it is possible to suppress a decrease in the cylindricity of the cylinder. [Brief description of the drawings]
[0013] [Figure 1] FIG. 1 is a schematic cross-sectional view of a circuit breaker including a cylinder according to an embodiment. [Diagram 2] FIG. 2 is a configuration diagram of a dashpot having a cylinder according to an embodiment. [Diagram 3] FIG. 3 is a cross-sectional view of a cylinder according to the embodiment. [Figure 4] FIG. 4 is a schematic diagram showing the configuration of a forging device for producing a cylinder according to the embodiment. [Diagram 5] FIG. 5 is a flow chart for producing a cylinder according to an embodiment. [Figure 6] FIG. 6 is a schematic cross-sectional view showing the shape of the cylinder in each process according to the embodiment. [Figure 7] FIG. 7 is an external view of the distribution board according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, the embodiments will be described in detail with reference to the drawings. Note that the embodiments described below are all comprehensive or specific examples. The numerical values, shapes, materials, components, arrangement and connection forms of the components, steps, and order of steps shown in the following embodiments are merely examples and are not intended to limit the present invention.
[0015] In addition, each drawing is a schematic diagram and is not necessarily a precise illustration. In addition, in each drawing, the same reference numerals are used for substantially the same configuration, and duplicated explanations may be omitted or simplified.
[0016] In addition, in this specification, terms indicating the relationship between elements, such as coincidence and orthogonal, terms indicating the shape of elements, such as cylinder, rectangle, trapezoid, etc., as well as numerical values and numerical ranges, are not expressions that only express the strict meaning, but are expressions that include a substantially equivalent range, for example, a difference of about a few percent.
[0017] In the present specification and drawings, the X-axis, Y-axis, and Z-axis refer to the three axes of a three-dimensional Cartesian coordinate system. In the embodiment, the Z-axis direction is the longitudinal direction of the cylinder. The X-axis direction and the Y-axis direction are perpendicular to each other on a plane perpendicular to the Z-axis direction. In the following embodiments, a "planar view" refers to a view from the Z-axis direction, and a "cross-sectional view" refers to a view of a cut surface cut by a plane including the X-axis and Y-axis from a direction perpendicular to the plane.
[0018] (Embodiment) [1. Circuit breaker configuration] Fig. 1 is a schematic cross-sectional view of a circuit breaker 1 equipped with an electromagnetic tripping device 100 having a cylinder 10 according to the present embodiment. Fig. 2 is a configuration diagram of a dashpot 100a having a cylinder 10 according to the present embodiment. Fig. 2 shows the configuration of the dashpot 100a when no overcurrent is flowing. Fig. 2 also shows a state in which the cylinder 10 and the pole head 40 are cut in the XZ plane, but the braking spring 30 is not shown in the portion where the protrusion 22 of the plunger 20 and the braking spring 30 overlap.
[0019] 1, the circuit breaker 1 includes an electromagnetic tripping device 100, a latch 110, a mechanism 120, a handle 130 for receiving operations from a person, and a contact 140. The electromagnetic tripping device 100 also includes a dashpot 100a, an electromagnetic coil 50 provided to wind around the cylinder 10, a yoke 60, and an armature 70 capable of rotating toward the pole head 40. The electromagnetic tripping device 100 is, for example, a fully electromagnetic type tripping device.
[0020] The circuit breaker 1 is configured to be able to switch between a closed-circuit state in which the contacts 140 are closed and an open-circuit state in which the contacts 140 are open, by operating the handle 130. When an overcurrent flows through the electromagnetic coil 50, the armature 70 moves (for example, rotates) and presses the latch 110, which causes the mechanism 120 to operate and open the contacts 140. In other words, the circuit breaker 1 trips. As a result, the circuit breaker 1 cuts off the power supply to the load when an overcurrent occurs. The latch 110, the mechanism 120, and the contacts 140 are an example of a trip mechanism.
[0021] As shown in FIG. 2, the dashpot 100a includes a cylinder 10, a plunger 20 accommodated inside the cylinder 10, a damping spring 30 for pushing the plunger 20 toward the bottom side (Z-axis minus side) of the cylinder 10, and a pole head 40 for sealing the cylinder 10. In this embodiment, the dashpot 100a has a structure in which the plunger 20 and damping spring 30 are enclosed in the cylinder 10 filled with a liquid such as oil (e.g., damping oil such as silicon oil), and the cylinder 10 is sealed with the pole head 40. The viscosity of the oil can impart a self-extending characteristic to the movement of the plunger 20. Note that, although an example of the dashpot 100a is an oil dashpot in which the cylinder 10 is filled with a liquid such as oil, it is not essential that the cylinder 10 is filled with a liquid such as oil.
[0022] The cylinder 10 is cylindrical with a bottom, and accommodates the plunger 20, oil, and the brake spring 30. A pole head 40 is provided on the opposite side to the bottom of the cylinder 10 (the positive side of the Z axis, the opening side of the cylinder 10). The plunger 20 and the brake spring 30 are accommodated in a space surrounded by the cylinder 10 and the pole head 40.
[0023] Since the cylinder 10 according to the present embodiment is formed by forging, it is preferable that the cylinder 10 is made of a non-magnetic material that is easily deformed by forging (by hammering). The cylinder 10 is preferably made of brass, which is easy to process and can be resistance welded. Note that the cylinder 10 is not limited to being made of brass, and may be made of any material that can be processed by forging and can be resistance welded.
[0024] The plunger 20 is a movable iron core that overcomes the braking spring 30 and moves toward the pole head 40 when an overcurrent flows through the electromagnetic coil 50. The plunger 20 has an axially symmetric shape with a circular cross section, and has a large diameter portion 21 with which one end of the braking spring 30 comes into contact, and a protruding portion 22 whose diameter is smaller than the inner diameter of the braking spring 30. The protruding portion 22 is configured to enter inside the braking spring 30. The plunger 20 is made of a magnetic material.
[0025] The large diameter portion 21 and the protruding portion 22 are each cylindrical and integrally formed. In a plan view, the center of the large diameter portion 21 and the center of the protruding portion 22 coincide with each other.
[0026] The damping spring 30 is an elastic member that restricts the movement of the plunger 20. The damping spring 30 fixes the plunger 20 by pressing it toward the bottom side of the cylinder 10, and separates the plunger 20 from the pole head 40. In other words, in normal times when no overcurrent is flowing, a gap (a space filled with oil in this embodiment) is formed between the protruding portion 22 of the plunger 20 and the pole head 40.
[0027] The pole head 40 is provided at the opening of the cylinder 10 and seals the cylinder 10. The pole head 40 is press-fitted into the opening of the cylinder 10, and then fixed to the cylinder 10 by resistance welding or the like.
[0028] The yoke 60 forms a magnetic path of magnetic flux that is formed when a current flows through the electromagnetic coil 50. The yoke 60 is made of an L-shaped magnetic material, and has a parallel piece arranged parallel to the axis (Z-axis) of the cylinder 10 and a right-angled piece extending perpendicular to the axis of the cylinder 10. The right-angled piece extends to the plunger 20 and is connected to the cylinder 10. Note that, as long as a magnetic path can be formed by the yoke 60 and the plunger 20, the yoke 60 does not need to be fixed to the cylinder 10.
[0029] The electromagnetic coil 50 is sandwiched between the plunger 20 and the yoke 60 and is provided so as to wind around the cylinder 10. The electromagnetic coil 50 is also connected to a main electric circuit. In this embodiment, the electromagnetic coil 50 and the main electric circuit are integrally formed from the same member. Note that the electromagnetic coil 50 and the main electric circuit may be separate members and electrically connected to each other.
[0030] The armature 70 is made of a magnetic material and is connected to the parallel piece of the yoke 60 in such a manner that it can rotate toward the pole head 40 .
[0031] In such an electromagnetic tripping device 100, when an overcurrent flows through the electromagnetic coil 50, a magnetic flux is generated. The magnetic flux passes through a magnetic path formed by the pole head 40, the armature 70, the yoke 60, and the plunger 20. Since a gap is normally formed between the pole head 40 and the protruding portion 22 of the plunger 20, a magnetic attraction force acts between the pole head 40 and the plunger 20. In other words, when an overcurrent flows through the electromagnetic coil 50, a force acts on the plunger 20 in a direction moving it toward the pole head 40.
[0032] When the magnetic attraction force acting on the plunger 20 becomes greater than the force of the brake spring 30 pushing the plunger 20, the plunger 20 starts to move toward the pole head 40. As the plunger 20 moves, the gap between the pole head 40 and the plunger 20 (the protrusion 22) becomes smaller. When the gap becomes smaller, the resistance of the magnetic circuit formed by the pole head 40, the armature 70, the yoke 60, and the plunger 20 becomes smaller, and the magnetic flux becomes larger.
[0033] As the magnetic flux increases, the magnetic attraction force acting on the plunger 20 increases, and the gap between the pole head 40 and the plunger 20 becomes smaller. By repeating the above, the gap gradually becomes smaller and the magnetic flux gradually increases. In the case of a low overcurrent region, when the protruding portion 22 of the plunger 20 reaches a position where it contacts or is close to the pole head 40, a large attraction force also acts on the armature 70 toward the pole head 40, and the armature 70 rotates. The armature 70 is then attracted to the pole head 40. When the latch 110 of the trip mechanism of the circuit breaker 1 is pressed by the armature 70, the circuit breaker 1 operates. In other words, the circuit breaker 1 cuts off the overcurrent.
[0034] [2. Cylinder configuration] The configuration of the cylinder 10 used in the dashpot 100a of the circuit breaker 1 as described above will be described with reference to Fig. 3. Fig. 3 is a cross-sectional view of the cylinder 10 according to the present embodiment. The cylinder 10 according to the present embodiment is formed by forging and therefore has a shape specific to forging.
[0035] As shown in Fig. 3, the cylinder 10 is an elongated member having a bottomed tubular shape (a bottomed cylindrical shape in this embodiment). The longitudinal direction of the cylinder 10 is parallel to the Z-axis direction. The cylinder 10 has a first tubular portion 11, a second tubular portion 12, and a third tubular portion 13. The first tubular portion 11, the second tubular portion 12, and the third tubular portion 13 are, for example, integrally formed.
[0036] The first cylindrical portion 11 includes the bottom of the cylinder 10 and is a portion with an inner diameter D1. The inner diameter D1 is, for example, a size corresponding to the large diameter portion 21 of the plunger 20, and is a size capable of accommodating the large diameter portion 21 and allowing the plunger 20 to move toward the pole head 40 when an overcurrent occurs. The first cylindrical portion 11 is a portion configured to include a second recess (see the second recess 310e1 in FIG. 6).
[0037] The first cylindrical portion 11 has a side surface portion 11a, a bottom surface portion 11b, and an inclined portion 11c. The side surface portion 11a constitutes the cylindrical portion of the first cylindrical portion 11, and the bottom surface portion 11b and the inclined portion 11c constitute a bottom portion that closes one opening of the cylindrical portion of the first cylindrical portion 11.
[0038] The side surface portion 11a has a constant thickness (length in the X-axis direction) and extends in the Z-axis direction.
[0039] The bottom surface portion 11b is provided near the center of the opening of the side surface portion 11a and closes a part of the opening. The cross-sectional shape of the bottom surface portion 11b is, for example, rectangular, and the planar shape is, for example, circular. For example, the bottom surface portion 11b is cylindrical. For example, the inner surface (inner surface 11b1) of the cylinder 10 of the bottom surface portion 11b is perpendicular to the inner surface (inner surface 11a1) of the cylinder 10 of the side surface portion 11a in the cross-sectional view.
[0040] The inclined portion 11c is provided between the bottom surface portion 11b and the side surface portion 11a in a cross-sectional view, and closes the remaining part of the opening. The cross-sectional shape of the inclined portion 11c is, for example, trapezoidal, and the planar shape is annular (for example, annular). The inner surface (inclined surface 11c1) of the cylinder 10 of the inclined portion 11c has a relationship in which it intersects with both the inner surface 11a1 of the side surface portion 11a and the inner surface 11b1 of the bottom surface portion 11b in a cross-sectional view. The inclined surface 11c1 is formed so that the distance from the opening of the cylinder 10 (the opening on the positive side of the Z axis) increases as it moves toward the bottom surface portion 11b side (the negative side of the Z axis) in a cross-sectional view. In other words, the inclined portion 11c becomes thicker from the bottom surface portion 11b toward the side surface portion 11a. The angle a between the inner surface 11b1 of the bottom portion 11b and the inclined surface 11c1 of the inclined portion 11c may be, for example, 45 degrees or less in terms of ease of forming in a forging device (see FIG. 4), and may be further 40 degrees or less, for example, 30 degrees. Note that the angle in this specification means an acute angle.
[0041] The second cylindrical portion 12 is provided between the first cylindrical portion 11 and the third cylindrical portion 13, and is a cylindrical portion with an inner diameter D2. In plan view, the inner diameter D2 is larger than the large diameter portion 21 of the plunger 20. In addition, the inner diameter D2 is larger than the inner diameter D1 in plan view. Therefore, a step 14 is formed at the boundary between the first cylindrical portion 11 and the second cylindrical portion 12 inside the cylinder 10. The second cylindrical portion 12 can also be said to be a wide portion of the cylinder 10 with a large recess (hole).
[0042] The step 14 may be inclined. For example, the step 14 may be formed so that the thickness (length in the X-axis direction) increases from the second tube portion 12 toward the first tube portion 11 in a cross-sectional view.
[0043] The third cylindrical portion 13 has a flange portion 13a of the cylinder 10 and a cylindrical portion with an inner diameter D3. The flange portion 13a is provided so as to expand from the opening of the cylinder 10 toward the outside (X-axis direction) in a plan view. The flange portion 13a is a portion that abuts against the pole head 40. The inner diameter D3 is a size that allows the pole head 40 to be press-fitted, and is smaller than the inner diameter D2, for example. Therefore, a step 15 is formed at the boundary between the second cylindrical portion 12 and the third cylindrical portion 13 inside the cylinder 10. The pole head 40 has a size that allows the pole head 40 to be press-fitted when the inner diameter is D1, that is, a size that corresponds to the size of the large diameter portion 21 of the plunger 20. In the following, a case where the pole head 40 is a size that allows the pole head 40 to be press-fitted when the inner diameter is D1 will be described as an example, but is not limited thereto.
[0044] The outer circumferential surfaces of the cylindrical parts of the first cylindrical part 11, the second cylindrical part 12, and the third cylindrical part 13 are formed to be flush. In other words, no step is formed on the outer circumferential surfaces of the cylindrical parts of the first cylindrical part 11, the second cylindrical part 12, and the third cylindrical part 13. In addition, it can be said that the first cylindrical part 11 and the second cylindrical part 12 have different thicknesses in a cross-sectional view, and the second cylindrical part 12 and the third cylindrical part 13 have different thicknesses. In this embodiment, the first cylindrical part 11 and the third cylindrical part 13 have the same thickness. That is, the inner diameters D1 and D3 are equal. In addition, the thickness (thickness in the Z-axis direction) of the bottom part 11b and the thickness (thickness in the Z-axis direction) of the inclined part 11c are each thicker than the thickness (thickness in the X-axis direction) of the side part 11a, for example.
[0045] The length L1 (length in the Z-axis direction) from the bottom surface of the first cylindrical portion 11 to the boundary between the first cylindrical portion 11 and the second cylindrical portion 12 (to the position of the step 14) is determined based on, for example, the sliding range of the plunger 20 (for example, the sliding range of the large diameter portion 21). The length L1 is longer than the sliding range of the plunger 20. For example, the length L1 may be longer than the distance L3 between the protruding portion 22 of the plunger 20 and the pole head 40. Note that the length L1 may be, for example, half or more of the length of the recess (hole) of the cylinder 10 (length L1+L2 shown in FIG. 3), but is not limited to being half or more.
[0046] Further, the outer surface of the side portion 11a and the outer bottom surface of the bottom portion (bottom portion 11b and inclined portion 11c) are perpendicular to each other in a cross-sectional view.
[0047] [3. Cylinder manufacturing method] Next, a method for manufacturing the cylinder 10 will be described with reference to Figs. 4 to 6. First, a forging device for manufacturing the cylinder 10 will be described with reference to Fig. 4. Fig. 4 is a schematic diagram showing a configuration of a forging device 200 for manufacturing the cylinder 10 according to the present embodiment. The shapes (diameter, length, etc.) of the forging dies provided in the forging device 200 are illustrated as being the same or similar, but are not limited to this. The shapes of the dies may be different from each other and are not limited to the shapes shown in Fig. 4. In the forging device (also called a parts former) shown in Fig. 4, the view from the Y-axis direction is generally referred to as a plan view, but in this specification, the view from the Z-axis direction is referred to as a plan view.
[0048] As shown in FIG. 4, the forging apparatus 200 includes a cutting machine 210, a ram 220, a plurality of punch side dies (a first punch side die 231 to a sixth punch side die 236), a die block 240, and a plurality of die side dies (a first die side die 251 to a sixth die side die 256).
[0049] The cutter 210 is a cutting device that cuts the wire rod 300 made of a metal material to a predetermined length. The forged material 310 cut to a predetermined length by the cutter 210 has, for example, a cylindrical shape. The wire rod 300 may be made of, for example, brass or steel. Note that FIG. 4 shows a state in which the forged material 310 is held by a conveyor.
[0050] The ram 220 holds a number of punch side dies and strikes the material to be forged 310 by reciprocating (moving up and down on the paper) toward the die block 240. The ram 220 is connected to a drive unit (not shown) such as a motor and moves reciprocatingly in the Z-axis direction. The ram 220 is moved by the drive unit in the direction of the arrow in the figure (Z-axis minus direction) to perform forming (forging). Note that the direction in which the ram 220 moves to apply a load to the material to be forged 310, that is, the Z-axis minus direction, is an example of a pressing direction. Furthermore, when forming is completed, the ram 220 is moved by the drive unit in the opposite direction to the pressing direction (Z-axis minus direction).
[0051] Each of the multiple punch side dies is a die for pressing the material to be forged 310 against the die side die. The multiple punch side dies include six punch side dies, the first punch side die 231 to the sixth punch side die 236, but the number of punch side dies is not limited to this. Also, each of the first punch side die 231 to the sixth punch side die 236 has a first protruding portion 231a to a sixth protruding portion 236a protruding toward the die block 240 side. Each of the first protruding portion 231a to the sixth protruding portion 236a is a columnar (for example, cylindrical) protrusion. Each of the first protruding portion 231a to the sixth protruding portion 236a processes the material to be forged 310 by directly contacting the material to be forged 310.
[0052] The die block 240 holds a plurality of die side dies. The die block 240 is not connected to a driving unit (not shown) such as a motor, and does not move. In other words, the die side dies are stationary dies.
[0053] Each of the multiple die side dies is a die in which the material to be forged 310 is placed and receives a load by the movement of the punch side die in the pressing direction. The multiple die side dies include six die side dies, the first die side die 251 to the sixth die side die 256, but the number of die side dies is not limited to this. Each of the first die side die 251 to the sixth die side die 256 has a first concave portion 251a to a sixth concave portion 256a. Each of the first concave portion 251a to the sixth concave portion 256a is a recess for forming the material to be forged 310 into a predetermined shape. Note that the forged material 310 being placed in the die side die includes that at least a part of the material to be forged 310 is accommodated in the recess, and that the material to be forged 310 is larger than the recess and is placed on the die side die so as to cover the recess. For example, when viewed from the pressing direction, the material to be forged 310 is positioned so that at least a portion of the material to be forged overlaps the recess.
[0054] The punch side dies and the die side dies are provided in a one-to-one correspondence. For example, the first punch side die 231 corresponds to the first die side die 251, and the second punch side die 232 corresponds to the second die side die 252. The same applies to the third punch side die 233 and onwards. The material to be forged 310 is formed into a predetermined shape by the shape of the punch (specifically, the shape of the end of the punch in the pressing direction) and the shape of the recess of the die side die.
[0055] Here, the shapes of the tip portions (end portions on the negative Z-axis side) of the fourth protrusion 234a and the fifth protrusion 235a will be described. The tip portions of the fourth protrusion 234a and the fifth protrusion 235a may each be frustum-shaped. In other words, the fourth protrusion 234a and the fifth protrusion 235a may each have a tapered shape.
[0056] The inclination angle b2 between the tip surface 235a1 and the inclined surface 235a2 of the fifth protrusion 235a is larger than the inclination angle b1 between the tip surface 234a1 and the inclined surface 234a2 of the fourth protrusion 234a. The inclination angle b2 is, for example, less than 45 degrees, more preferably less than 40 degrees, and is, for example, 30 degrees. If the inclination angle b2 is 45 degrees or more, the pressure of the fifth punch side die 235 is not applied to the end of the cylinder 10 (for example, near the inclined portion 11c), and it may not be possible to form a clean shape. If the inclination angle b2 is 45 degrees or more, there is a concern that the material will not enter the end of the cylinder 10 (for example, near the inclined portion 11c) during processing (punching) in the forging device 200, resulting in poor molding. Therefore, the inclination angle b2 is set to be less than 45 degrees.
[0057] The tip portion is an example of a processed portion. The fourth protruding portion 234a is an example of a first punch, and the fifth protruding portion 235a is an example of a second punch. The first punch and the second punch are different dies.
[0058] Moreover, the diameter D4 of the fourth protrusion 234a is larger than the diameter D5 of the fifth protrusion 235a. Moreover, the diameter D6 of the sixth protrusion 236a is smaller than the diameter D5 of the fifth protrusion 235a. Moreover, the diameter D6 of the sixth protrusion 236a may be the same as the diameter D4 of the fourth protrusion 234a, or may be smaller than the diameter D4 of the fourth protrusion 234a. In this embodiment, the diameter D6 of the sixth protrusion 236a is the same as the diameter D4 of the fourth protrusion 234a. The sixth protrusion 236a is an example of a third punch.
[0059] In addition, the tip of one of the fourth protrusion 234a and the fifth protrusion 235a is not limited to be in a truncated cone shape. In other words, the tip of one of the fourth protrusion 234a and the fifth protrusion 235a does not have to have a tapered shape, and may be flat (at least one of the inclination angle b1=0 degrees and the inclination angle b2=0 degrees).
[0060] Next, a manufacturing method for manufacturing the cylinder 10 using the forging device 200 will be described. FIG. 5 is a flow chart for manufacturing the cylinder 10 according to this embodiment. FIG. 5 shows a manufacturing method for the bottomed cylindrical cylinder 10 used in the dashpot 100a. FIG. 6 is a schematic cross-sectional view showing the shape of the cylinder 10 according to this embodiment in each process. In each of (a) to (f) of FIG. 6, the outer bottom surface 310a1 (the surface on the negative side of the Z axis) is formed in a state supported by the die-side metal mold. Note that FIG. 6 is merely a conceptual diagram showing the shape of the cylinder 10 in each process, and does not disclose the exact shape, thickness, etc. Also, in FIG. 6, the steps 14 and 15 and the shapes of the bottom surface, etc. are emphasized.
[0061] 5, first, a cutting step is performed (S10) in which the wire rod 300 is cut to a predetermined length by the cutting machine 210 to prepare the forged material 310. In step S10, the wire rod 300 is cut to a length according to the product to be produced. The forged material 310 is transported from the cutting machine 210 to the first die side mold 251 by a transport machine (not shown).
[0062] Next, a first processing step is performed on the predetermined length of the material to be forged 310 by the first punch side tool 231 and the first die side tool 251 (S20). The first processing step is a step for adjusting the shape of the cut surface of the material to be forged 310. The cut surface is smoothed by the first processing step.
[0063] 6(a) shows the material 310a to be forged, the cut surfaces of which (the upper and lower surfaces, i.e., the outer bottom surface 310a1 and the surface facing away from the outer bottom surface 310a1) have been smoothed by the first processing step. The material 310a to be forged is, for example, cylindrical. The material 310a to be forged is transported from the first die side mold 251 to the second die side mold 252 by a transport machine (not shown).
[0064] Next, the second processing step is performed on the shaped forged material 310a by the second punch side tool 232 and the second die side tool 252 (S30). The second processing step is a step for forming a flange portion at one tip portion of the cylindrical forged material 310a.
[0065] 6(b) shows the forged material 310b having a flange portion 310b1 formed at its tip by the second processing step. The flange portion 310b1 is formed around the circumference. The forged material 310b is transported from the second die side mold 252 to the third die side mold 253 by a transport machine (not shown).
[0066] Next, the forging material 310b with the flange portion 310b1 formed thereon is subjected to a third machining step by the third punch side tool 233 and the third die side tool 253 (S40). The third machining step is a step for forming a shallow hole in the flange portion 310b1.
[0067] FIG. 6(c) shows a forged material 310c in which a hole 310c1 is formed in a flange portion 310b1 by the third processing step. The inner diameter of the hole 310c1 is, for example, equal to or larger than the inner diameter D2 shown in FIG. 6(d). The hole 310c1 is provided to facilitate the insertion of the fourth protruding portion 234a in the next processing step. The formation of the hole 310c1 is expected to improve the accuracy of the processing position (punch position) of the fourth protruding portion 234a in the fourth processing step. In other words, the formation of the hole 310c1 is expected to improve the cylindricity of the cylinder 10 after molding. The forged material 310c is transported from the third die side mold 253 to the fourth die side mold 254 by a transport machine (not shown).
[0068] Next, the fourth machining step is performed on the forging material 310c in which the hole 310c1 is formed by the fourth punch side tool 234 and the fourth die side tool 254 (S50). The fourth machining step can also be said to be a first extrusion step in which the forging material 310c in which the hole 310c1 is formed is extruded by the fourth protrusion 234a (an example of a first punch). The fourth machining step is a step for forming the second tubular portion 12. In other words, the fourth machining step is a step for forming a space with an inner diameter D2 inside.
[0069] In the fourth processing step, the fourth protrusion 234a is pressed in to a position in the Z-axis direction corresponding to the step 14 shown in Fig. 3. That is, in the fourth processing step, the fourth protrusion 234a is pressed in only to a position on the positive side of the Z-axis by a length L1 from a position in the Z-axis direction corresponding to the inner surface 11b1 shown in Fig. 3.
[0070] 6(d) shows the forged material 310d in which the first recess 310d1 is formed by the fourth processing step. The inner diameter of the first recess 310d1 is the inner diameter D2. The inner bottom surface 310d2 formed by the fourth processing step is, for example, a surface facing away from the outer bottom surface 310a1. The forged material 310d is transported from the fourth die side mold 254 to the fifth die side mold 255 by a transport machine (not shown).
[0071] Next, a fifth machining step is performed on the inner bottom surface 310d2 (an example of a bottom surface) of the material to be forged 310d in which the first recess 310d1 is formed, by the fifth punch side metal mold 235 and the fifth die side metal mold 255 (S60). The fifth machining step can also be said to be a second extrusion step in which the material to be forged 310d in which the first recess 310d1 is formed is extruded by the fifth protrusion 235a (an example of a second punch). The fifth machining step is a step for forming the first tubular portion 11. In other words, the fifth machining step is a step for forming a space with an inner diameter D1 inside.
[0072] 6(e) shows the forging material 310e in which the second recess 310e1, which is spatially continuous with the first recess 310d1, is formed by the fifth processing step. The inner diameter of the second recess 310e1 is an inner diameter D1. The fifth processing step forms an annular step 14. The direction in which the first recess 310d1 and the second recess 310e1 continue is the Z-axis direction, which is also the longitudinal direction of the cylinder 10.
[0073] When processing the recess, if the remaining plate thickness (plate thickness on the bottom side) becomes thin, the plate may break due to contact between the fifth punch side plate 235 and the fifth die side plate 255 before the material reaches the end of the fifth die side plate 255, or the material at the end may be torn off (so-called dead metal). In this embodiment, since the tip of the fifth protruding portion 235a is in a truncated cone shape, the plate thickness at the end (the thickness of the portion corresponding to the inclined portion 11c (see FIG. 3)) can be made thick, so that the plate may be prevented from breaking or the material may be prevented from being torn off. In other words, the cylinder 10 can be stably produced. In addition, since the inclination angle b2 of the tip of the fifth protruding portion 235a is less than 45 degrees, the pressure of the fifth punch side plate 235 can be applied to the material at the end, so that the cylinder 10 can be finished into a neater shape.
[0074] The material to be forged 310e is transported from the fifth die side mold 255 to the sixth die side mold 256 by a transport machine (not shown).
[0075] In the fifth processing step, the fifth protrusion 235a passes through the first recess 310d1 formed in the fourth processing step, and then comes into contact with the inner bottom surface 310d2, thereby performing the extrusion processing. In the fifth processing step, the fifth protrusion 235a is pushed into the inner bottom surface 310d2 shown in FIG. 6(d), forming a space with an inner diameter D1. In the fifth processing step, the fifth protrusion 235a is pushed into a position in the Z-axis direction corresponding to the inner surface 11b1 shown in FIG.
[0076] Since the inner diameter D2 of the first recess 310d1 is larger than the diameter D5 of the fifth protrusion 235a, the fifth protrusion 235a can smoothly pass through the first recess 310d1. In other words, the manufacturing method according to this embodiment can prevent the fifth protrusion 235a from touching an unintended part when passing through the first recess 310d1, thereby preventing the shape of the cylinder 10 from being deformed. This leads to an improvement in the cylindricity of the cylinder 10.
[0077] In addition, it is preferable that the center of the inner diameter D1 and the center of the inner diameter D2 coincide with each other in a plan view. In other words, it is preferable that the circle of the inner diameter D1 and the circle of the inner diameter D2 are concentric circles in a plan view.
[0078] Here, since the diameter D4 of the fourth protrusion 234a is larger than the diameter D5 of the fifth protrusion 235a, the inner diameter D1 of the first recess 310d1 is larger than the inner diameter D2 of the second recess 310e1. The difference between the inner diameters D1 and D2 is preferably small, for example, in consideration of the strength of the second cylindrical portion 12. The difference between the inner diameters D1 and D2 is preferably constant regardless of the size of the inner diameters D1 and D2. For example, when the inner diameter D1 has a diameter of D mm, the inner diameter D2 may be D+0.03 mm. In other words, the difference between the inner diameters D1 and D2 is preferably 0.03 mm or less. The difference between the inner diameters D1 and D2 is not limited to 0.03 mm or less, and may be determined, for example, according to the size of the inner diameter D1 (for example, 1% or less of the inner diameter D1), or may be determined according to the dimensional tolerance of the inner diameter D1. Furthermore, the difference between the inner diameters D1 and D2 may be determined to be large enough so as not to affect the operation of the dashpot 100a.
[0079] Next, the sixth machining step is performed on the forging material 310e in which the second recess 310e1 is formed, by the sixth punch side die 236 and the sixth die side die 256 (S70). The sixth machining step is a step for machining the opening of the cylinder 10 into a shape into which the pole head 40 can be pressed, specifically, a step for changing the inner diameter around the opening of the cylinder 10 to an inner diameter into which the pole head 40 can be pressed. In this embodiment, in the sixth machining step, the inner diameter around the opening of the cylinder 10 is changed from the inner diameter D2 to an inner diameter D3 smaller than the inner diameter D2 (for example, the same size as the inner diameter D1). The periphery of the opening of the cylinder 10 is an example of the opening side of the cylinder 10 of the first recess 310d1. The periphery of the opening of the cylinder 10 is a region of the opening side of the cylinder 10 of the first recess 310d1 (a region corresponding to the third cylindrical portion 13) including the opening of the cylinder 10.
[0080] In the sixth processing step, the sixth protrusion 236a is inserted to a position required for pressing in the pole head 40 (for example, a position corresponding to the step 15), and the flange portion 13a is struck. This allows the material to be concentrated inward (toward the center of the first recess 310d1 in plan view) around the opening of the cylinder 10, forming a region with an inner diameter smaller than that of the first recess 310d1. This region is the portion into which the pole head 40 is pressed in.
[0081] In this manner, in the sixth processing step, the sixth protrusion 236a having a smaller diameter than the fourth protrusion 234a is used for the forging material 310e in which the second recess 310e1 is formed, and a region having a smaller inner diameter than the first recess 310d1 is formed by moving the material inward on the opening side of the cylinder 10 of the first recess 310d1. Note that in the sixth punch side die 236, the sixth protrusion 236a and the portion for striking the flange portion 13a may be integrally formed, for example.
[0082] 6(f) shows a forging material 310f in which the opening side portion of the first recess 310d1 has an inner diameter D3 as a result of the sixth processing step. The inner diameter of the second recess 310e1 is, for example, the inner diameter D1. The sixth processing step forms a step 15 in an annular shape.
[0083] In addition, in a plan view, the center of the inner diameter D1, the center of the inner diameter D2, and the center of the inner diameter D3 may coincide. In other words, in a plan view, the circle of the inner diameter D1, the circle of the inner diameter D2, and the circle of the inner diameter D3 may be concentric circles. In addition, in a plan view, the circle of the step 14 and the circle of the step 15 may be concentric circles.
[0084] In this manner, in the present embodiment, two extrusion processes (a fourth process step and a fifth process step) are performed to form the cylinder 10 by forging. This improves the cylindricity compared to a case where a cylinder is formed by a single extrusion process. For example, the cylindricity of the cylinder 10 can be about the same as that of a cylinder formed by drawing.
[0085] [4. Distribution Board Configuration] Next, a distribution board including a circuit breaker 1 having a cylinder 10 according to the present embodiment will be described with reference to Fig. 7. Fig. 7 is an external view of a distribution board 400 according to the present embodiment.
[0086] 7, the distribution board 400 includes a housing 410, a main breaker 420, and a plurality of branch breakers 430 provided on each power line (branch circuit) connected to the distribution board 400. Power (system power) from a power system which is a facility of a power company or the like is supplied to the distribution board 400, and the distribution board 400 branches the system power into a plurality of branch circuits. The distribution board 400 is installed inside a facility that uses power, such as a house, a hospital, a factory, or a building.
[0087] The housing 410 has a main body 411 that houses a main breaker 420 and a plurality of branch breakers 430, and a door 412 that is attached to the main body 411 in an openable and closable manner. The main body 411 and the door 412 are electrically insulating. The main body 411 and the door 412 are made of, for example, an electrically insulating resin material. The housing 410 also has holes and openings (not shown) through which each power line passes.
[0088] The main breaker 420 is a breaker that stops the supply of power from the power grid when a current exceeding a predetermined current (for example, a current based on the power specified in a contract with the power company) flows from the power grid.
[0089] Branch breaker 430 is a breaker that, when an overcurrent flows through a power line connected to the branch breaker, stops the supply of power to the power line.
[0090] The circuit breaker 1 according to the present embodiment may be used as either the main breaker 420 or the branch breaker 430 of the distribution board 400. In other words, the distribution board 400 may include one or more circuit breakers 1.
[0091] [5. Effects, etc.] As described above, the manufacturing method according to the present embodiment is a method for manufacturing the bottomed cylindrical cylinder 10 used for the dashpot 100a, in which the forging material 310 having a predetermined length is extruded with the fourth protrusion 234a (an example of a first punch) to form the first recess 310d1 in the forging material 310 (S40), and the inner bottom surface 310d2 (an example of a bottom surface) of the first recess 310d1 is extruded with the fifth protrusion 235a (an example of a second punch) to form the second recess 310e1 spatially continuous with the first recess 310d1 (S50). The inner diameter D2 of the first recess 310d1 is larger than the inner diameter D1 of the second recess 310e1.
[0092] As a result, two extrusion processes (S40 and S50) are performed to form the cylinder 10 by forging, so the processing length in each extrusion process (the length struck by the punch) can be made shorter than when the first recess 310d1 and the second recess 310e1 are formed by one extrusion process. By shortening the processing length in the extrusion process, distortion of the shape of the recesses to be formed can be reduced. In other words, the shape of the cylinder 10 can be stabilized. Therefore, the manufacturing method according to this embodiment can suppress a decrease in the cylindricity of the cylinder 10 even when a forging process is used.
[0093] Moreover, the tip of the fifth protrusion 235a is shaped like a truncated cone.
[0094] This allows the plate thickness of the end of the cylinder 10 (the thickness of the portion corresponding to the inclined portion 11c (see FIG. 3)) to be increased, thereby suppressing the effect on the shape of the cylinder 10 caused by the plate thickness being reduced at the end. In other words, it is possible to further suppress a decrease in the cylindricity of the cylinder 10. In addition, it is possible to suppress the mold from breaking or the material from tearing, thereby enabling stable production.
[0095] The inclination angle b2 of the truncated cone shape of the tip of the fifth protrusion 235a is less than 45 degrees.
[0096] This allows the pressure of the fifth punch side die 235 to be applied to the end of the cylinder 10 (near the inclined portion 11c (see FIG. 3)), so that the cylinder 10 can be finished into a neater shape. This further prevents the cylindricity of the cylinder 10 from decreasing.
[0097] Furthermore, the tip of the fourth protrusion 234a is shaped like a truncated cone, and the inclination angle b2 of the truncated cone shape of the tip of the fifth protrusion 235a is greater than the inclination angle b1 of the truncated cone shape of the tip of the fourth protrusion 234a.
[0098] This makes it possible to effectively prevent the die from breaking or the material from tearing during extrusion processing at the fifth protrusion portion 235a, which is prone to cause the die to break or the material to tear.
[0099] Furthermore, a sixth protruding portion 236a (an example of a third punch) having a smaller diameter than the fourth protruding portion 234a is used for the forging material 310e in which the second recess 310e1 is formed, and a region having a smaller inner diameter than the first recess 310d1 is formed by drawing material inward on the opening side of the cylinder 10 of the first recess 310d1. This process corresponds to step S70.
[0100] As a result, for example, when a pole head 40 having a size corresponding to the size of the second recess 310e1 is attached to the cylinder 10, the pole head 40 can be press-fitted into the cylinder 10. This makes it possible to prevent the pole head 40 from coming off the cylinder 10 due to transportation, etc., from when the pole head 40 is attached to the cylinder 10 until the pole head 40 is joined to the cylinder 10 by resistance welding, etc. This makes it possible to prevent a decrease in productivity when manufacturing the dashpot 100a using the cylinder 10 formed by forging.
[0101] Furthermore, the wire rod 300 is cut to a predetermined length to produce the material to be forged 310 (S10).
[0102] This makes it possible to integrally perform the process from forming the wire material 300 to forming the cylinder 10. That is, according to the manufacturing method of the present embodiment, the cylinder 10 can be produced by simply preparing the wire material 300.
[0103] As described above, the cylinder 10 according to the present embodiment is a cylinder 10 manufactured using the manufacturing method described above.
[0104] This provides the same effects as the above-mentioned manufacturing method, specifically, the cylinder 10 in which the decrease in cylindricity is suppressed can be realized by forging.
[0105] As described above, the circuit breaker 1 according to this embodiment includes the cylinder 10, the pole head 40 that is provided at the opening of the cylinder 10 and seals the cylinder 10, and the plunger 20 that is housed in the cylinder 10 and is movable in a direction toward the pole head 40 (Z-axis direction) when an overcurrent flows. The length L1 of the cylinder 10 in the longitudinal direction at the second recess 310e1 is longer than the distance L3 between the plunger 20 and the pole head 40 when no overcurrent is generated.
[0106] As a result, the circuit breaker 1 has a high degree of cylindricity of the cylinder 10, and the plunger 20 can move smoothly inside the cylinder 10, so that the circuit breaker 1 can perform an accurate breaking operation. In addition, since the length L1 is longer than the distance L3, the plunger 20 can move smoothly from the pole head 40 due to an overcurrent to the normal position (the position shown in FIG. 2) when the overcurrent is eliminated. For example, it is possible to prevent the large diameter portion 21 of the plunger 20 from getting caught on the step 14.
[0107] As described above, the distribution board 400 according to this embodiment includes one or more circuit breakers 1 described above.
[0108] As a result, even when the distribution board 400 includes the circuit breaker 1 having the cylinder 10 formed by forging, the distribution board 400 can perform an accurate breaking operation.
[0109] (Other embodiments) Although the embodiment has been described above, the present invention is not limited to the above embodiment.
[0110] For example, in the above embodiment, the manufacturing method of the cylinder 10 used for the dashpot 100a has been described, but the cylinder 10 manufactured by the above manufacturing method is not limited to the cylinder 10 used for the dashpot 100a. The above manufacturing method of the cylinder 10 may be applied as a manufacturing method of the cylinder 10 used for any purpose other than the dashpot 100a. It is particularly effective for manufacturing a cylinder that requires high cylindricity.
[0111] In the above embodiment, the cutting step (S10), the third processing step (S40), and the sixth processing step (S70) are not essential steps. At least one of the cutting step, the third processing step, and the sixth processing step may not be performed. For example, when a forged material 310 of a predetermined length is prepared in advance, the cutting step may not be performed. Also, for example, when a pole head 40 is placed in the opening of the inner diameter D2 and immediately joined by resistance welding, or when a pole head 40 of a size that can be pressed in at the inner diameter D2 is prepared, the sixth processing step may not be performed. Note that, if the sixth processing step is not performed, the step 15 is not formed.
[0112] In the above embodiment, an example in which the extrusion process is performed twice (the fourth processing step (S50) and the fifth processing step (S60)) has been described, but the extrusion process may be performed three or more times. In other words, it is sufficient that the extrusion process is performed two or more times.
[0113] In addition, in the above embodiment, an example has been described in which the fourth processing step (S50) is followed by the fifth processing step (S60), but other processing steps may be performed between the fourth processing step and the fifth processing step.
[0114] In the above embodiment, the steps 14 and 15 are formed in an annular shape, but the annular shape here also includes a case where the steps are interrupted at least in a part in the circumferential direction. In other words, the steps 14 and 15 are not limited to being complete annular.
[0115] In the above embodiment, the tip of the fourth protrusion 234a and the fifth protrusion 235a is in a truncated cone shape, but the present invention is not limited to this. The tip of at least one of the fourth protrusion 234a and the fifth protrusion 235a does not have to be in a truncated cone shape. For example, the tip may be flat. Furthermore, the tip of at least one of the first protrusion 231a, the second protrusion 232a, the third protrusion 233a, and the sixth protrusion 236a may be in a truncated cone shape. Even in this case, the inclination angle b2 of the fifth protrusion 235a is the largest.
[0116] In the above embodiment, the forging device 200 is described as being equipped with the cutter 210, but the present invention is not limited thereto and may not be equipped with the cutter 210. The forging device 200 may be capable of, for example, using a die to shape a forged material 310 having a predetermined length that is prepared in advance.
[0117] The order of the processes described in the flowcharts of the above embodiments is merely an example. The order of the processes may be changed, and the processes may be executed in parallel.
[0118] Furthermore, each step in the manufacturing method described in the above embodiment may be performed in one step or in separate steps. Performing in one step includes performing each step using one device, performing each step consecutively, or performing each step at the same location. Separate steps includes performing each step using separate devices, performing each step at different times (e.g., different days), or performing each step at different locations.
[0119] In addition, the present invention also includes forms obtained by applying various modifications to the embodiments that a person skilled in the art may conceive, or forms realized by arbitrarily combining the components and functions of each embodiment within the scope that does not deviate from the spirit of the present invention. [Explanation of symbols]
[0120] 1 Circuit Breaker 10 Cylinders 20 Plunger 40 Pole Head 100a dashpot 234a Fourth protrusion (first punch) 235a Fifth protrusion (second punch) 236a 6th protrusion (3rd punch) 300 wire rod 310, 310a, 310b, 310c, 310d, 310e, 310f Forged material 310d1 First recess 310d2 Inner bottom surface 310e1 Second recess 400 Distribution Board b1, b2 Tilt angle D1, D2 inner diameter L1 Length L3 Distance
Claims
1. A method for manufacturing a bottomed cylindrical cylinder used in a dashpot, comprising the steps of: A first recess is formed in a forged material having a predetermined length by performing an extrusion process with a first punch; performing an extrusion process on a bottom surface of the first recess with a second punch to form a second recess that is spatially continuous with the first recess; an inner diameter of the first recess is larger than an inner diameter of the second recess; The tip of the second punch is frusto-conical, In forming the second recess, the second punch having a truncated cone shape is used to form the cylinder having a cylindrical side portion, a bottom portion and an inclined portion that closes one opening of the side portion, the inclined portion being thicker from the bottom portion toward the side portion, The tip of the first punch is flat. Manufacturing method.
2. The inclination angle of the truncated cone shape of the tip of the second punch is less than 45 degrees. The method of claim 1 .
3. Furthermore, a third punch having a diameter smaller than that of the first punch is used to push material inward on the opening side of the cylinder of the first recess, thereby forming a region having an inner diameter smaller than that of the first recess, for the forging material in which the second recess is formed. The method according to claim 1 or 2.
4. Furthermore, the wire is cut to the predetermined length to prepare the forging material. The method according to any one of claims 1 to 3.
5. A cylinder produced by the manufacturing method according to any one of claims 1 to 4.
6. A cylinder according to claim 5; a pole head provided at an opening of the cylinder for sealing the cylinder; a plunger that is housed in the cylinder and that is movable in a direction toward the pole head when an overcurrent flows; The length of the second recess in the direction is longer than the distance between the plunger and the pole head when no overcurrent is generated. Circuit breaker.
7. A distribution board comprising one or more circuit breakers according to claim 6.
Citation Information
Patent Citations
Working method for end part of steel pipe
JP1988115643A
Cold and warm forging method for cylindrical body
JP1992089153A
Distribution board
JP2005124307A
Dash pot, electromagnetic trip device of circuit breaker using the same
JP2013145643A
Electromagnetic trip device and circuit breaker
JP2016167390A