Hydroquinone flakes

Hydroquinone flakes with controlled dimensions and low fine powder content address dissolution and handling issues, offering rapid water solubility and reduced blocking, suitable for use in polymerization inhibitors and antioxidants.

JP7581666B2Active Publication Date: 2024-11-13UBE CORPORATION
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2020107925
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-23
Publication Date
2024-11-13
Estimated Expiration
2040-06-23

AI Technical Summary

Technical Problem

Existing hydroquinone forms, such as beads and fine powders, face issues with high dissolution times, susceptibility to static electricity, equipment incompatibility, dust generation, and increased fine powder ratios during transportation and storage, leading to handling difficulties and blocking problems.

Method used

Hydroquinone flakes with defined dimensions (2.0 mm to 45.0 mm length, 2.0 mm to 30.0 mm width, 1.6 mm to 3.5 mm thickness) and low fine powder content (<1% by mass) are produced using common flaking equipment, ensuring low agglomeration and easy dissolution in water.

Benefits of technology

The hydroquinone flakes exhibit rapid dissolution in water, reduced fine powder generation, and improved handling characteristics, minimizing blocking and enhancing transportation efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007581666000002
    Figure 0007581666000002
  • Figure 0007581666000003
    Figure 0007581666000003
  • Figure 0007581666000004
    Figure 0007581666000004
Patent Text Reader

Abstract

To obtain a hydroquinone flake group that has a practical range of time of dissolution in water, has a low ratio of powderization, and resists blocking.SOLUTION: The inventive hydroquinone flake group is characterized by that: an average length of hydroquinone flakes in the flake group is in a range of 2.0 mm-45.0 mm, an average width of the flakes in the flake group is in a range of 2.0 mm-30.0 mm, and an average thickness of the flakes in the flake group is in a range of 1.6 mm-3.5 mm.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to flakes of hydroquinone. [Background technology]

[0002] Hydroquinone is widely used as a polymerization inhibitor or antioxidant. Patent Document 1 describes a method in which hydroquinone is dissolved in hot water, the solution is broken down into droplets, and the droplets are brought into contact with cold gas to be processed into beads having a particle size of 100 μm to 3000 μm. Patent Document 2 describes that hydroquinone flakes having a specific length, width, thickness and a specific bulk density can be obtained by spraying molten hydroquinone, depositing it on a cylinder and solidifying it, and then rotating the cylinder to drop the solidified hydroquinone. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 4909515 [Patent Document 2] Patent No. 5676101 Summary of the Invention [Problem to be solved by the invention]

[0004] When hydroquinone is used as a polymerization inhibitor or an antioxidant, it is desired that it has a high dissolution rate in order to dissolve it in water or an organic solvent, which is a solvent. Furthermore, when hydroquinone is in the form of a fine powder, it becomes charged and is easily affected by static electricity, which makes it difficult to handle. The hydroquinone beads described in Patent Document 1 have a problem that they require special equipment in the manufacturing process and cannot use existing equipment. In addition, there is a problem that hydroquinone dust is generated when the droplets are broken down into small pieces. Furthermore, it takes time to dissolve in water or an organic solvent. The hydroquinone flakes described in Patent Document 2 have a low ratio of fine powder immediately after production, and because of their thin thickness, the ratio of fine powder increases due to collapse during transportation and storage, which causes significant dust problems. In addition, they have a problem of being easily blocked. An object of the present invention is to obtain hydroquinone flakes which have a low fine powder rate, a dissolution time in water within a practical range, and are less susceptible to blocking. [Means for solving the problem]

[0005] The present invention relates to, for example, the following [1] to

[15] . [1] A group of hydroquinone flakes, A group of hydroquinone flakes having an average flake length in the range of 2.0 mm to 45.0 mm, an average flake width in the range of 2.0 mm to 30.0 mm, and an average flake thickness in the range of 1.6 mm to 3.5 mm. [2] A flake group of hydroquinone according to [1], in which the fine powder content in the flake group is less than 1 mass%. [3] A group of hydroquinone flakes according to [2], in which the fine powder content in the group of flakes immediately after production is less than 0.5 mass%. [4] A flake group of hydroquinone [1] to [3], in which the average flake length in the group is in the range of 5.0 mm to 30.0 mm. [5] A flake group of hydroquinone [1] to [4], in which the average flake width in the group is in the range of 2.0 mm to 16.0 mm. [6] A hydroquinone flake group of any of [1] to [5], in which the average flake thickness in the flake group is in the range of 1.6 mm to 3.0 mm. [7] A flake group of hydroquinone selected from [1] to [6], in which the maximum thickness in the flake group is in the range of 2.0 mm to 4.0 mm. [8] The cumulative specific surface area of ​​the flake group is 10 m 2A flake group of hydroquinone, any of [1] to [7], having a molecular weight of 1.0 or more per 1000 g / g or more. [9] The cumulative specific surface area of ​​the flakes is 13 m 2 / g~15m 2 / g range, [8] hydroquinone flake group.

[10] A group of hydroquinone flakes according to any one of [1] to [9], wherein the cumulative pore volume of the flake group is 0.04 ml / g or more.

[11] The cumulative pore volume of the flake group is in the range of 0.05 ml / g to 0.20 ml / g for the hydroquinone flake group in

[10] .

[12] A hydroquinone flake group of any of [1] to

[11] , in which the Hausner ratio of the flake group is 1.5 or less.

[13] A hydroquinone flake group of any of [1] to

[12] , wherein the degree of compression of the flake group is 33% or less.

[14] A hydroquinone flake group of any of [1] to

[13] , wherein the crushing strength of the flake group is 15 N or less or the flake group does not aggregate.

[15] [1]~

[14] A polymerization inhibitor using any of the hydroquinone flakes. Effect of the Invention

[0006] The hydroquinone flakes of the present invention have a low fine powder ratio, a dissolution time in water within a practical range, and are less prone to blocking. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a schematic diagram showing an example of a steel belt flaker. [Diagram 2] FIG. 1 is a schematic diagram illustrating an example of a drum flaker. [Diagram 3] FIG. 1 is a schematic diagram illustrating an example of a drum flaker. [Figure 4] 1 is an optical microscope photograph of an example flake. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] In this specification, The term "flake" refers to a particle having a ratio of thickness to length (thickness / length) defined below in the range of 0.030 to 1.000. The shape of the "flakes" is not particularly limited and includes various shapes such as a sphere, an ellipse, a rectangular parallelepiped, and a polygon. "Hydroquinone flakes" refers to an aggregate of hydroquinone flakes. Hereinafter, this will also be referred to as "flakes".

[0009] The "length," "width," and "thickness" of a flake are defined as follows: When one flake is placed in a parallelepiped so that each of the inner faces of the parallelepiped is in contact with one or more points, the longest side of the three mutually orthogonal directions of the parallelepiped is called the "length," the second longest side is called the "width," and the shortest side is called the "thickness." The side values ​​are measured with a vernier caliper scale of 0.01 mm and rounded to one decimal place.

[0010] The hydroquinone flakes are obtained with a distribution of flake length, width and thickness. The average flake length in a group of flakes, the average flake width in a group of flakes, and the average flake thickness in a group of flakes refer to the average length, the average width, and the average thickness of any 10 flakes in a group of flakes, respectively. In this specification, one or more of the average length, average width, average thickness, and maximum thickness of a single flake in a group of flakes may also be referred to as a flake dimension.

[0011] "Maximum thickness" refers to the maximum thickness among the thicknesses of any 10 flakes in a group of flakes. In this specification, the term "fine powder" refers to disintegrated flakes that pass through a sieve with 105 μm openings.

[0012] Figure 4 shows an example of a single flake. The average length of a single flake in the group of flakes is in the range of 2.0 mm to 45.0 mm, preferably in the range of 5.0 mm to 30.0 mm, and more preferably in the range of 5.0 mm to 25.0 mm. The average width of a single flake in the group of flakes is in the range of 2.0 mm to 30.0 mm, preferably in the range of 2.0 mm to 16.0 mm, and more preferably in the range of 5.0 mm to 13.0 mm. The average thickness of a single flake in the group of flakes is in the range of 1.6 mm to 3.5 mm, preferably in the range of 1.6 mm to 3.0 mm, and more preferably in the range of 1.6 mm to 2.5 mm. The maximum thickness of the flakes in the flake group is in the range of 2.0 mm to 4.0 mm, preferably in the range of 2.0 mm to 3.5 mm, and more preferably in the range of 2.0 mm to 3.0 mm. It is preferable that the average length, average width, average thickness, and maximum thickness of a single flake in a flake group are within the ranges described above, since this can suppress both an increase in the dissolution time in water and an increase in the fine powder rate.

[0013] The cumulative specific surface area of ​​the flakes measured by mercury intrusion porosimetry is 10 m 2 / g or more, and 2 / g~15m 2 More preferably, the range is 13m / g. 2 / g~14m 2 It is more preferable that the molecular weight is in the range of / g. The cumulative pore volume of the flakes measured by mercury intrusion porosimetry is preferably 0.04 ml / g or more, more preferably in the range of 0.05 ml / g to 0.20 ml / g, and even more preferably in the range of 0.06 ml / g to 0.15 ml / g. If the cumulative specific surface area and cumulative pore volume are within the above ranges, it is assumed that nano-order pores that can be impregnated with a solvent such as water can be formed while suppressing an increase in the fine powder ratio, thereby increasing the contact area with the solvent, which is preferable from the viewpoint of shortening the dissolution time. The cumulative specific surface area and cumulative pore volume are measured by the methods described in the Examples.

[0014] The bulk density of the flakes is preferably 0.3 g / ml to 0.7 g / ml, and more preferably 0.4 g / ml to 0.6 g / ml. The tap density of the flakes is preferably 0.5 g / ml to 0.8 g / ml, and more preferably 0.6 g / ml to 0.7 g / ml. If the bulk density and tap density are within the above ranges, the powder has good flowability. That is, if the Hausner ratio (tap density / bulk density) is 1.5 or less, the transport efficiency in piping or the like can be improved, and it is preferably 1.3 or less, and more preferably 1.27 or less. Furthermore, when the bulk density and tap density are within the above ranges, the compressibility, which is an index of powder compressibility {(tap density-bulk density) / tap density x 100}, is preferably 33% or less from the viewpoint of improving the filling efficiency into containers such as silos and hoppers, more preferably 25% or less, and even more preferably 22% or less. The bulk density and tap density are values ​​measured by the measurement methods described in the Examples.

[0015] The fine powder ratio in 100% by mass of the flake group is preferably less than 1% by mass, more preferably less than 0.5% by mass, and even more preferably less than 0.2% by mass. The fine powder ratio refers to the ratio (% by mass) of the mass of fine powder that passed through a sieve with a mesh size of 105 μm to the mass of the entire flake group. If the flakes are subjected to impact during transportation or storage, they may break down and generate fine powder. The fine powder rate is the percentage of fine powder contained in the flakes before such fine powder is newly generated. Specifically, it is measured immediately after the flakes are produced by the production method described below.

[0016] When dissolving hydroquinone flakes in water, the time required to completely dissolve 1.44g of hydroquinone flakes in 28.56g of pure water at 25°C and a rotation speed of 600 rpm, that is, the dissolution time required to prepare an aqueous solution with a hydroquinone concentration of 4.8% by mass, is preferably 30 minutes or less, more preferably 5 to 20 minutes, and even more preferably 5 to 15 minutes.Thus, the flakes of the present invention have a suitable dissolution time in water, despite the flakes being larger in size than conventional hydroquinone flakes.

[0017] From the viewpoint of suppressing blocking, the crushing strength is preferably 15N or less or no aggregation, more preferably 10N or less or no aggregation, even more preferably 5N or less or no aggregation, and particularly preferably no aggregation. However, if three or more flakes are not aggregated, it is determined that there is no aggregation. The crushing strength is a value measured by the measurement method described in the examples.

[0018] <Method of producing hydroquinone> Hydroquinone is usually obtained by oxidizing phenol or a hydroxyl-protected compound thereof with a peroxide or the like. Specifically, it can be obtained by the production method described in, for example, International Publication No. 2019 / 182035.

[0019] <Flake manufacturing method> As a method for producing hydroquinone flakes, a general flake device such as a drum flaker, a table flaker, a steel belt flaker, a double steel belt flaker, etc. is selected. There is no particular limitation. Thus, the hydroquinone flakes of the present invention can be produced using known devices described in JP2012-82158A, JP5837755A, etc.

[0020] For example, when a steel belt flaker is used, the hydroquinone melt is continuously extruded from a nozzle at the tip of the extruder to form a plate-shaped or string-shaped hydroquinone melt (hereinafter also referred to as "melt"). The amount of liquid sent is, for example, the amount described in the Examples, etc., for reference. The nozzle may have a single hole or may have multiple holes. The shape of the nozzle hole is appropriately selected according to the cross-sectional shape of the desired melt, and may be any shape, such as a circle, an ellipse, a diamond, or a rectangle.

[0021] The molten liquid extruded from the nozzle is supplied onto a metal belt functioning as a metal belt cooler, and is cooled and solidified by the metal belt. The material, belt length, belt width, etc. of the metal belt are referred to, for example, in the contents described in the Examples. The metal belt cooler is a device having a metallic endless conveyor belt (metal belt), and this endless conveyor belt is cooled by a cooling mechanism provided on the inner periphery side, and the material to be cooled is supplied to the outer periphery side of this endless conveyor belt to cool the material to be cooled. The cooling temperature is preferably 5 to 50°C, more preferably 10 to 30°C. The cooling temperature is the temperature of a cooling medium such as cooling water or the temperature of the endless conveyor belt.

[0022] There is no particular limitation on the type of metal belt cooler, and for example, as shown in Fig. 1, the molten liquid 2 extruded from the nozzle 1 of the melt extruder is sandwiched between two metal belts 3, 4 and transported to the end of the belts. The two metal belts 3, 4 are cooled by spraying cooling water from cooling mechanisms 5, 6. In the metal belt cooler, the cooling water does not come into contact with the molten liquid 2, and the molten liquid 2 is cooled via the metal belts 3, 4, so there is no risk of the molten liquid 2 absorbing moisture when it is cooled. As shown in FIG. 1, the metal belt cooler may be provided with a press roller 11 for rolling the molten liquid 2 or the like.

[0023] The metal belt cooler is not limited to the one shown in Fig. 1, and it is also possible to use, for example, a single belt cooler that cools the molten liquid with one metal belt. However, a double cooler system that sandwiches and cools the molten liquid from two directions is preferable in terms of cooling efficiency, etc.

[0024] The plate-like or string-like solidified product of hydroquinone (hereinafter also referred to as "solidified product") obtained by the above-mentioned molten liquid solidification step is cut to the desired length of hydroquinone flakes, or the solidified product is crushed and fragmented by a crusher 21. Note that Fig. 1 shows an example in which the solidified product is crushed by a crusher 21 to form hydroquinone flakes 22.

[0025] When cutting the solidified material, the cutting is usually performed perpendicular to the longitudinal direction of the solidified material.

[0026] The device used to cut the solidified material may be any device equipped with a cutter for cutting the solidified material, such as a scraper blade that scrapes off plate-like or string-like solidified material by grounding the blade against the end of a belt, or a pelletizer that cuts with a rotating blade and a fixed blade.

[0027] A drum flaker is shown in Figures 2 and 3. Molten hydroquinone is provided in the supply tanks 35 and 42. The supply tanks 35 and 42 are equipped with temperature control devices to keep the hydroquinone in a molten state. The temperature of the molten hydroquinone is usually 172°C to 220°C. In FIG. 2, a part of the cooling drum 30 is immersed in the supply tank 35 as shown in FIG. 2. The immersion depth of the cooling drum 30 in the supply tank 35 is usually 1 mm to 5 mm. The cooling drum 30 rotates, and the molten hydroquinone is attached to its surface by the rotation to form a thin film 36. Alternatively, as shown in FIG. 3, the molten hydroquinone is transferred from the supply tank 42 to the liquid supply nozzle 45 using a pump 43, and is supplied from the liquid supply nozzle 45 to the outer surface of the cooling drum 40, and the molten hydroquinone is attached to the outer surface of the cooling drum, and the thin film 46 is formed by the rotation. The cooling drum may be, for example, a vertical or horizontal metal pressure vessel, as well as a general-purpose metal drum or a resin drum. The cooling drum is preferably made of a heat conductive material or is coated with a heat conductive material. The dimensions of the cooling drum are not particularly limited, but are generally about 0.5 m to 1.0 m.

[0028] Hydroquinone is solidified by cooling the cooling drums 30 and 40. The cooling method is not particularly limited, but examples thereof include a method of circulating water through a jacket and a method of spraying water, water vapor, or a refrigerant onto the inner surfaces of the cooling drums 30 and 40 from cooling water spray nozzles 34 and 44. The cooling temperature is preferably 5°C to 50°C.

[0029] The solidified hydroquinone is collected in flakes 38 and 48 by any known means, such as by gravity, using scraper blades 37 and 47 to peel the solidified films 36 and 46 from the cooling drums 30 and 40. The collected hydroquinone flakes 38 and 48 are removed from the chambers 31 and 41 by a conveyor 32 or the like. The thickness of the flakes is determined by controlling the thickness of the thin films 36 and 46, that is, by controlling the feed rate of hydroquinone to the cooling drums 30 and 40, the rotational speed of the cooling drums, and the cooling temperature.

[0030] <Application> The hydroquinone flakes of the present invention are useful as organic synthesis intermediates or manufacturing raw materials, and are used in the fields of reducing agents, rubber chemicals, dyes, medicines, agricultural chemicals, polymerization inhibitors, oxidation inhibitors, etc., and are preferably used as polymerization inhibitors. EXAMPLES

[0031] The present invention will be specifically described with reference to examples and comparative examples.

[0032] The dimensions and measurements shown in Table 1 for the flakes obtained in the Examples and Comparative Examples were measured by the following methods. <Measurement of flake dimensions> Ten flakes were randomly selected and their length, width, and thickness were measured using a caliper (with 0.01 mm scale). The average length, width, and thickness of the ten flakes were calculated (hereinafter also referred to as "average length," "average width," and "average thickness"). The maximum thickness among the thicknesses of the ten flakes was recorded as the maximum thickness.

[0033] <Measurement of fine powder ratio> The flakes were sieved through a sieve with 105 μm openings, and the ratio (mass %) of the mass of the fine powder that passed through the sieve to the total mass of the flakes was determined. If the flakes are subjected to an impact during transportation or storage, the flakes may break down and generate fine powder. The fine powder content in this specification refers to the content of fine powder contained in the flakes before such fine powder is newly generated. Specifically, it was measured immediately after the flakes were produced.

[0034] <Measurement of bulk density> 100 g of the flake group was gently placed into a 250 ml measuring cylinder, and the mass per volume was calculated by reading the scale.

[0035] <Measurement of tap density> 100 g of the flakes were gently placed into a 250 ml measuring cylinder, the measuring cylinder was raised about 5 cm, and then dropped under its own weight onto a workbench to give it vibration. This operation was repeated 100 times, and the scale was then read to calculate the mass per volume.

[0036] <Measurement of dissolution time> 1.44 g of flakes and 28.56 g of pure water were placed in a 50 ml glass container, stirred at 600 rpm with a magnetic stirrer at 25° C., and the time it took for the flakes to completely dissolve was measured. The measured time was the time required to prepare a 4.8% by mass aqueous solution of hydroquinone.

[0037] <Measurement of cumulative specific surface area and cumulative pore volume> The cumulative specific surface area and cumulative pore volume were measured using a mercury porosimeter by the mercury intrusion method (JIS R1655). The measurement device used was a fully automatic pore distribution measurement device PORE MASTER 60-GT manufactured by Quantachrome Instruments. Specifically, the flakes were placed in a sample container and degassed for 30 minutes at a pressure of 2.67 Pa or less. Mercury was then introduced into the sample container and gradually pressurized to inject mercury into the pores of the sample. Mercury was injected into the porous resin body from a pressure of 0.53 psia (approximately 3.68 kPa) corresponding to a pore diameter of 400 μm to a pressure of 60,000 psia (approximately 413 MPa) corresponding to a pore diameter of 3.6 nm, and the cumulative pore volume (mL / g) was calculated by dividing the total amount of mercury injected (mL) by the sample weight (g). The cumulative specific surface area was calculated by dividing the average pore diameter from the total amount of mercury injected, assuming that all pores are cylindrical.

[0038] <Measurement of crushing strength> Water was sprayed evenly onto the flakes to bring them to a 10% moisture content, at 0.18 kg / cm 2 A load of this magnitude was applied to the group of flakes, and a cycle of heating at 50°C for 9 hours and cooling at 25°C for 15 hours was carried out for a total of 5 days to create an aggregate (solidified material) of flakes. The maximum resistance value at the time of the aggregate's collapse was measured for the obtained aggregate of flakes using an Imada ZTS-500N, and this was taken as the crushing strength. However, if three or more flakes are not aggregated, it is determined that the aggregate is not aggregated. The higher the crushing strength, the more difficult it is to collapse the aggregate and the more likely it is to block. This is because it is affected by the dimensions and surface condition of the flakes.

[0039] [Example 1] Hydroquinone melted at 180 to 200°C was fed from a feed nozzle at 320 kg / hr, and the molten hydroquinone was extruded onto the lower belt of a pair of 1650SM belt coolers (upper belt: belt width 650 mm, belt length 3 m, lower belt: belt width 600 mm, belt length 6 m), and 15°C cooling water was sprayed onto the back of the belt, and the molten liquid was contact-solidified in the belt cooler. The solidified hydroquinone was cut with a scraper blade disposed at the end of the pair of belt coolers, and a group of hydroquinone flakes with an average length of 17.7 mm, an average width of 12.0 mm, and an average thickness of 1.6 mm was obtained.

[0040] [Example 2] Solidified hydroquinone was obtained in the same manner as in Example 1, except that the cooling water temperature was changed to 17° C. The solidified flakes were cut with a scraper blade in the same manner as in Example 1, and a group of hydroquinone flakes having an average length of 11.4 mm, an average width of 6.2 mm, and an average thickness of 2.0 mm were obtained.

[0041] [Example 3] Solidified hydroquinone was obtained in the same manner as in Example 1, except that the cooling water temperature was changed to 19° C. The solidified flakes were cut with a scraper blade in the same manner as in Example 1, and a group of hydroquinone flakes having an average length of 14.3 mm, an average width of 7.0 mm, and an average thickness of 2.2 mm were obtained.

[0042] [Example 4] Solidified hydroquinone was obtained in the same manner as in Example 1, except that the cooling water temperature was changed to 25° C. The solidified flakes were cut with a scraper blade in the same manner as in Example 1, and a group of hydroquinone flakes having an average length of 24.3 mm, an average width of 15.2 mm, and an average thickness of 2.4 mm were obtained.

[0043] [Example 5] Solidified hydroquinone was obtained in the same manner as in Example 1, except that the cooling water temperature was changed to 30° C. The solidified flakes were cut with a scraper blade in the same manner as in Example 1, and a group of hydroquinone flakes having an average length of 32.8 mm, an average width of 18.7 mm, and an average thickness of 2.7 mm were obtained.

[0044] [Comparative Example 1] Hydroquinone melted at 187℃ was immersed in the lower part of a cooling drum (drum diameter 0.63m, drum width 0.3m, drum circumference 1.98m, drum rotation speed 10.3rpm) to a depth of about 1mm, and the hydroquinone was solidified by applying saturated vapor refrigerant of 153℃ for 2 seconds, and then peeled off with a scraper blade to obtain flakes of hydroquinone. The flakes had an average length of 7.3mm, average width of 5.5mm, and average thickness of 0.5mm.

[0045] [Table 1]

[0046] The values ​​in Table 1 were determined as follows. The following values ​​are per one flake. Apparent volume (A): (A) = average length x average width x maximum thickness (ml) Apparent weight (B): (B) = (A) x 1.33 (g) (Density of hydroquinone is 1.33g / ml (20℃)) Actual volume (C): (C) = (A) - (B) x cumulative pore volume (ml) Actual weight (D): (D) = (C) x 1.33 (g) (Density of hydroquinone is 1.33g / ml (20℃)) Effective surface area (E): (E) = (D) × cumulative specific surface area (m 2 ) Apparent volume ratio (F): (F) = (A) / 0.04 (The value of (A) in each Example was divided by the value of (A) in Comparative Example 1.) Effective surface area ratio (G): (G) = (E) / 0.35 (The value of (E) in each Example was divided by the value of (E) in Comparative Example 1.) (G) / (F): This refers to the effect of increasing the contact area relative to the flake size. The larger (G) / (F) is, the greater the contact area with the solvent relative to the flake size is. Based on the comparative example, a ratio greater than 1.0 indicates a greater effect on shortening the dissolution time relative to the flake size.

[0047] The dissolution time is presumed to be a value corresponding to the flake size represented by the apparent volume, and although the apparent volumes of Examples 1 to 5 are 4.1 to 50.9 times larger than that of Comparative Example 1, the dissolution time is the same or at most 3 times longer. This is probably because the (G) / (F) values ​​of Examples 1 to 5 are 1.5 to 1.6 times larger, and therefore an appropriate dissolution time was achieved despite the flake size being larger than that of the Comparative Example. In comparison with Comparative Example 1, Examples 1 to 5 have lower Hausner ratios and compression degrees, and therefore have excellent fluidity and packing efficiency, making them suitable for transportation and storage. It is understood that Examples 1, 2, and 5 have lower crushing strength or do not aggregate compared to Comparative Example 1, and therefore are less susceptible to blocking than Comparative Example 1. It is understood that, compared with Comparative Example 1, Examples 1 to 5 have a lower fine powder ratio, and therefore the flakes are less likely to disintegrate. [Industrial Applicability]

[0048] The hydroquinone flakes of the present invention are useful as various organic synthesis intermediates or manufacturing raw materials, and are used in the fields of reducing agents, rubber chemicals, dyes, medicines, agricultural chemicals, polymerization inhibitors, oxidation inhibitors, etc. [Explanation of symbols]

[0049] 1 nozzle 2. Molten Liquid 3,4 Metal belt 5,6 Cooling mechanism 11 Press roller 21 Crusher 22 Hydroquinone Flakes 30 Cooling drum 31 Chamber 32 Nitrogen 33 Gas treatment equipment 34 Cooling water spray port 35 Supply Tank 36 Thin Film 37 Scraper Blade 38 Hydroquinone Flakes 39 Conveyor 40 Cooling drum 41 Chamber 42 Supply Tank 43 Pump 44 Cooling water spray nozzle 45 Liquid supply nozzle 46 Thin Film 47 Scraper Blade 48 Hydroquinone Flakes

Claims

1. Hydroquinone flakes, The average flake length in the flake group is in the range of 5.0 mm to 32.8 mm; The average flake width in the flake group is in the range of 2.0 mm to 18.7 mm; The average flake thickness in the group of flakes is in the range of 1.6 mm to 3.0 mm; The cumulative specific surface area of ​​the flakes is in the range of 13 m 2 / g to 15 m 2 / g; The cumulative pore volume of the flakes is 0.04 ml / g or more; The Hausner ratio of the flakes is 1.5 or less; Hydroquinone flakes.

2. 2. The hydroquinone flakes according to claim 1, wherein the fine powder ratio in the flakes is less than 1% by mass.

3. 3. The hydroquinone flakes according to claim 2, wherein the fine powder content in the flakes is less than 0.5% by weight.

4. 4. The flakes of hydroquinone according to any one of claims 1 to 3, wherein the maximum thickness of the flakes is in the range of 2.0 mm to 4.0 mm.

5. 5. The flakes of hydroquinone according to any one of claims 1 to 4, wherein the cumulative pore volume of the flakes is in the range of 0.05 ml / g to 0.20 ml / g.

6. 6. Flakes of hydroquinone according to any one of claims 1 to 5, wherein the degree of compression of the flakes is less than or equal to 33%.

7. 7. The flakes of hydroquinone according to any one of claims 1 to 6, wherein the flakes have a crushing strength of 15N or less, or do not aggregate.

Citation Information

Patent Citations

  • JP1974009515A

  • Headlight for vehicle

    JP1981076101A

  • Production of granular phenols

    JP2000302716A

  • Beads of phenolic compound and method for producing the same

    JP2006503900A

  • Novel forms of hydroquinone and methods for obtaining novel forms of hydroquinone

    JP2009541467A