Sealed power storage device and method for manufacturing the same

A resin sealing member with an annular joint to an annular roughened surface addresses sealing issues in sealed power storage devices, enhancing airtightness and serving as a safety valve to manage pressure without additional components.

JP7591535B2Active Publication Date: 2024-11-28PRIME PLANET ENERGY & SOLUTIONS INC +2
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2022086255
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-05-26
Publication Date
2024-11-28
Estimated Expiration
2042-05-26

AI Technical Summary

Technical Problem

Existing sealed power storage devices face issues with improper sealing of liquid injection holes due to poor welding of metal sealing members, leading to potential leaks and compromised airtightness.

Method used

The use of a resin sealing member with an annular joint that is airtightly joined to an annular roughened surface on the metal wall, enhancing the sealing integrity by utilizing the anchor effect of the resin's uneven shape to ensure a secure fit.

Benefits of technology

This approach improves the airtightness of the sealed power storage device by ensuring the liquid injection hole is properly sealed, while also acting as a safety valve to prevent excessive internal pressure buildup without the need for additional components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007591535000001
    Figure 0007591535000001
  • Figure 0007591535000002
    Figure 0007591535000002
  • Figure 0007591535000003
    Figure 0007591535000003
Patent Text Reader

Abstract

To provide a sealed power storage device in which a liquid injection hole formed at a metallic wall part of a device case is properly sealed by a resin sealing member formed of a resin, and to provide a manufacturing method of the sealed power storage device.SOLUTION: A sealed power storage device 1 includes: a device case 30 having a metallic wall part 15 formed with a liquid injection hole 12; and a sealing member 18 which seals the liquid injection hole 12 in a manner that the sealing member 18 covers the liquid injection hole 12 from the outer surface 15b side of the metallic wall part 15. The sealing member 18 is a resin sealing member 18 formed of a resin. The outer surface 15b of the metallic wall part 15 includes an annular seal surface 13 which surrounds an opening 12b of the liquid injection hole 12. The resin sealing member 18 has an annular joint part 18b which is joined to the annular seal surface 13 in an airtight manner.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sealed electricity storage device and a manufacturing method thereof. [Background technology]

[0002] Patent Document 1 discloses a sealed electricity storage device including a device case having a metal wall portion in which a liquid injection hole is formed, and a sealing member that seals the liquid injection hole. The sealing member is a metal sealing member made of metal. Therefore, in the sealed electricity storage device of Patent Document 1, the liquid injection hole formed in the metal wall portion is sealed by the metal sealing member. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2007-66600 A

[0004] As in Patent Document 1, a sealed electricity storage device having a structure in which an inlet hole formed in a metal wall portion is sealed by a metal sealing member is manufactured, for example, as follows. Specifically, in a liquid inlet process, an electrolyte is injected into the inside of the device case through the liquid inlet hole. Then, in a sealing process, the liquid inlet hole is sealed by the metal sealing member in a manner that covers the liquid inlet hole from the outer surface side of the metal wall portion. More specifically, in the sealing process, in a state in which the liquid inlet hole is blocked by the metal sealing member, the metal sealing member is welded to the entire circumference of the metal wall portion by laser welding in a manner in which a laser beam is irradiated from the outer surface side of the metal wall portion to the boundary between the periphery of the liquid inlet hole and the metal sealing member and its vicinity. As a result, the liquid inlet hole is sealed by the metal sealing member. Summary of the Invention [Problem to be solved by the invention]

[0005] However, in a structure in which the liquid inlet hole is sealed by welding a metal sealing member to a metal wall portion of a device case, the liquid inlet hole may not be properly sealed due to poor welding, and therefore a structure in which the liquid inlet hole formed in the metal wall portion of the device case is sealed by a resin sealing member made of resin has been considered.

[0006] The present invention has been made in consideration of the current situation, and aims to provide a sealed electricity storage device in which a liquid injection hole formed in a metal wall portion of a device case is properly sealed by a resin sealing member made of resin, and a manufacturing method thereof. [Means for solving the problem]

[0007] (1) One aspect of the present invention is a sealed electricity storage device including a device case having a metal wall portion with a liquid injection hole formed therein, and a sealing member that seals the liquid injection hole in a manner that covers the liquid injection hole from an outer surface side of the metal wall portion. The sealing member is a resin sealing member made of resin, the outer surface of the metal wall portion includes an annular sealing surface that surrounds an opening of the liquid injection hole, and the resin sealing member has an annular joint that is airtightly joined to the annular sealing surface. The annular seal surface is an annular roughened surface having projections and recesses on the order of nm, and the resin sealing member is hermetically joined to the annular roughened surface in such a manner that the resin forming the annular joint enters into the recesses of the annular roughened surface. It is a sealed electricity storage device.

[0008] In the above-mentioned sealed electricity storage device, the liquid inlet formed in the metal wall of the device case is sealed by a resin sealing member made of resin in a manner that covers the liquid inlet from the outer surface side of the metal wall. This resin sealing member has an annular joint that is airtightly joined to "annular seal surface on the outer surface of the metal wall that surrounds the opening of the liquid inlet". By having such an annular joint, the resin sealing member is airtightly joined to the metal wall, and the liquid inlet is sealed by the resin sealing member. Therefore, the above-mentioned sealed electricity storage device is a sealed electricity storage device in which the liquid inlet formed in the metal wall of the device case is appropriately sealed by the resin sealing member.

[0010] In this sealed electricity storage device, The annular seal surface is an annular roughened surface having nanometer-order irregularities,The annular joint of the resin sealing member is hermetically joined to the annular roughened surface in such a manner that the resin forming the annular joint enters into the recess of the annular roughened surface. Of which, nm order The annular joint of the resin sealing member is airtightly joined to the annular roughened surface by the anchor effect caused by the protrusion biting into the annular joint of the resin sealing member, which increases the airtightness between the annular joint of the resin sealing member and the annular roughened surface of the metal wall portion, thereby improving the airtightness of the sealed electricity storage device.

[0011] ( 2 ) Furthermore, the above (1 )of It is preferable that the sealed electricity storage device is a sealed electricity storage device in which the resin sealing member also serves as a safety valve member, and when the internal pressure of the device case reaches a valve opening pressure, the resin sealing member is destroyed, thereby releasing the seal on the liquid injection hole by the resin sealing member.

[0012] In this sealed electricity storage device, the resin sealing member also functions as a safety valve member. Therefore, even if the device case is not provided with a separate gas exhaust hole and even if a separate safety valve member for sealing the gas exhaust hole is not provided, when the internal pressure of the device case reaches the valve opening pressure, the resin sealing member is destroyed (for example, the resin sealing member is cleaved), thereby discharging the gas inside the battery case to the outside through the liquid injection hole and preventing the internal pressure of the device case from rising too high.

[0013] ( 3) Another aspect of the present invention is a method for manufacturing a sealed electricity storage device, the sealed electricity storage device comprising: a device case having a metal wall portion in which a liquid injection hole is formed; and a sealing member that seals the liquid injection hole in a manner that covers the liquid injection hole from an outer surface side of the metal wall portion, the sealing member being a resin sealing member made of resin, the outer surface of the metal wall portion including an annular sealing surface that surrounds an opening of the liquid injection hole, the resin sealing member having an annular joint that is airtightly joined to the annular sealing surface, and the method for manufacturing the sealed electricity storage device further comprises: This method for manufacturing a sealed electricity storage device includes an injection step of injecting an electrolyte solution, and a sealing step of sealing the injection hole in a manner that covers the injection hole from the outer surface side of the metal wall portion with the resin sealing member, wherein the sealing step includes an application step of applying molten resin to the device case from the outer surface side of the metal wall portion so as to cover at least the annular sealing surface and the injection hole of the outer surface of the metal wall portion, and a solidification step of solidifying the molten resin to form the resin sealing member having the annular joint that is airtightly joined to the annular sealing surface.

[0014] In the above-mentioned manufacturing method, by carrying out the application step and the solidification step, a sealed electricity storage device can be manufactured in which the liquid injection hole formed in the metal wall part of the device case is properly sealed by the resin sealing member made of resin. More specifically, as the resin sealing member, a resin sealing member having an annular joint part that is airtightly joined to the "annular seal surface surrounding the opening of the liquid injection hole in the outer surface of the metal wall part" can be formed. By forming a resin sealing member having such an annular joint part, the resin sealing member is airtightly joined to the metal wall part, and the liquid injection hole is sealed by the resin sealing member. A sealed electricity storage device having such a sealing structure for the liquid injection hole is a sealed electricity storage device in which the liquid injection hole is properly sealed.

[0015] In addition, examples of the method of applying the molten resin in the application step include hot melt die and curtain coating. Here, the hot melt die is a method of applying the molten resin in a film shape using a die coater. Also, the curtain coating is a method of applying the molten resin in a film shape using a flow coater (curtain coater).

[0016] Furthermore, when the annular sealing surface is an annular roughened surface having an uneven shape, a portion of the molten resin applied to the annular roughened surface in the application process flows into the recesses of the annular roughened surface, and the molten resin is solidified in the solidification process, whereby the resin forming the annular joint penetrates into the recesses of the annular roughened surface to form a resin sealing member that is hermetically bonded to the annular roughened surface.

[0017] ( 4 ) Furthermore, the above ( 3 ), wherein the annular sealing surface is an annular roughened surface having an uneven shape, and in the applying step, when the molten resin is applied to the device case from the outer surface side of the metal wall portion so as to cover at least the annular roughened surface and the liquid injection hole of the outer surface of the metal wall portion, a part of the molten resin applied on the annular roughened surface flows into a recess of the annular roughened surface, and in the solidifying step, the molten resin is solidified to form the resin sealing member that is hermetically joined to the annular roughened surface in such a manner that the resin that forms the annular joint enters the recess of the annular roughened surface.

[0018] In the above-mentioned manufacturing method, a resin sealing member can be formed in which the resin forming the annular joint enters the recess of the annular roughened surface of the metal wall, and the annular joint of the resin sealing member is airtightly joined to the annular roughened surface. In other words, a resin sealing member can be formed in which the annular joint of the resin sealing member is airtightly joined to the annular roughened surface by the anchor effect caused by the convex portion of the annular roughened surface of the metal wall biting into the annular joint of the resin sealing member. Therefore, the airtightness between the annular joint of the resin sealing member and the annular roughened surface of the metal wall is increased, and the airtightness of the sealed type electricity storage device can be improved.

[0019] ( 5 ) Also, (1) Or (2) a sealing step of sealing the liquid injection hole from an outer surface side of the metal wall portion with the resin sealing member, the sealing step preferably including: a coating step of coating the molten resin on the device case from the outer surface side of the metal wall portion so as to cover at least the annular sealing surface and the liquid injection hole of the outer surface of the metal wall portion; and a solidification step of solidifying the molten resin to form the resin sealing member having the annular joint that is airtightly joined to the annular sealing surface.

[0020] ( 6 )or, (1) or (2)a sealing step of sealing the liquid injection hole from an outer surface side of the metal wall portion with the resin sealing member, the sealing step including: a disposing step of disposing a resin film on the device case so as to cover at least the annular sealing surface and the liquid injection hole of the outer surface of the metal wall portion from the outer surface side of the metal wall portion; a melting step of melting at least a portion of the resin film located on the annular sealing surface to form a molten resin; and a solidifying step of solidifying the molten resin to form the resin sealing member having the annular joint that is airtightly joined to the annular sealing surface.

[0021] ( 5 ) and ( 6 According to the manufacturing method of ), a sealed electricity storage device can be manufactured in which the liquid injection hole formed in the metal wall portion of the device case is properly sealed by the resin sealing member. More specifically, as the resin sealing member, a resin sealing member having an annular joint portion that is airtightly joined to an annular seal surface that surrounds the opening of the liquid injection hole formed in the outer surface of the metal wall portion can be formed. By forming a resin sealing member having such an annular joint portion, the resin sealing member is airtightly joined to the metal wall portion and the liquid injection hole is sealed by the resin sealing member. A sealed electricity storage device having such a sealing structure for the liquid injection hole is a sealed electricity storage device in which the liquid injection hole is properly sealed. [Brief description of the drawings]

[0022] [Figure 1] 1 is a plan view (top view) of a sealed electricity storage device according to an embodiment. [Diagram 2] FIG. 2 is a front view of the sealed electricity storage device. [Diagram 3] FIG. 2 is a cross-sectional view of FIG. [Figure 4] FIG. 4 is an enlarged view of part C in FIG. [Diagram 5]4 is a flowchart showing a flow of a method for manufacturing a sealed electricity storage device according to an embodiment. [Figure 6] 1 is a flowchart showing a flow of a sealing process according to an embodiment. [Figure 7] FIG. 13 is an explanatory diagram of a liquid injection step according to the embodiment. [Figure 8] FIG. 4 is an explanatory diagram of a surface roughening step according to the embodiment. [Figure 9] FIG. 2 is an enlarged cross-sectional view of an annular roughened surface. [Figure 10] FIG. 4 is an explanatory diagram of a coating step according to the embodiment. [Figure 11] FIG. [Figure 12] 15A and 15B are enlarged views of a portion D in FIG. 10 and a portion F in FIG. [Figure 13] FIG. [Figure 14] 13A to 13C are explanatory diagrams of a coating step according to a modified embodiment. [Figure 15] 15 is another explanatory view of the coating step, and is a cross-sectional view of the GG portion of FIG. 14. [Figure 16] FIG. 13 is a plan view of an annular roughened surface according to a modified embodiment. [Figure 17] 13A to 13C are explanatory diagrams of a sealing step according to a modified embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] Next, an embodiment of the present invention will be described. The sealed electricity storage device 1 of this embodiment is a sealed battery, and more specifically, a lithium ion secondary battery. The sealed electricity storage device 1 includes a device case 30, an electrode body 50 housed inside the device case 30, a positive electrode terminal member 41, and a negative electrode terminal member 42 (see Figs. 1 to 3). The device case 30 is a hard case made of metal, and has a rectangular box shape. The device case 30 includes a metal case body 21 having a rectangular bottomed cylindrical shape, and a rectangular flat metal cover body 11 that closes an opening 21b of the case body 21 (see Figs. 1 to 3). The metal cover body 11 has a metal wall portion 15 in which a liquid injection hole 12 is formed. The metal wall portion 15 is a part of the metal cover body 11.

[0024] The metal lid 11 has two rectangular cylindrical through holes (first and second through holes, not shown). A positive electrode terminal member 41 is inserted into the first through hole, and a negative electrode terminal member 42 is inserted into the second through hole (see FIGS. 1 and 2). A cylindrical insulating member (not shown) is interposed between the inner peripheral surface of the first through hole of the metal lid 11 and the outer peripheral surface of the positive electrode terminal member 41, and between the inner peripheral surface of the second through hole of the metal lid 11 and the outer peripheral surface of the negative electrode terminal member 42. Furthermore, the metal lid 11 (more specifically, the metal wall portion 15) has a cylindrical liquid injection hole 12 penetrating the metal lid 11 in the thickness direction (see FIGS. 1 and 3).

[0025] The electrode body 50 has a positive electrode plate 60, a negative electrode plate 70, and a separator 80 interposed between the positive electrode plate 60 and the negative electrode plate 70. More specifically, the electrode body 50 is a laminated electrode body including a plurality of positive electrode plates 60, a plurality of negative electrode plates 70, and a plurality of separators 80, in which the positive electrode plates 60 and the negative electrode plates 70 are alternately laminated in the lamination direction DL with the separators 80 interposed therebetween (see FIG. 3). An electrolyte 90 is contained inside the electrode body 50. The electrolyte 90 is also contained on the bottom side inside the device case 30. The positive electrode plate 60 of the electrode body 50 is connected to the positive electrode terminal member 41 through a positive electrode current collector tab (not shown). The negative electrode plate 70 is connected to the negative electrode terminal member 42 through a negative electrode current collector tab (not shown).

[0026] Furthermore, the sealed electricity storage device 1 includes a resin sealing member 18 that seals the liquid injection hole 12 (see Figs. 1 to 3). This resin sealing member 18 seals the liquid injection hole 12 in such a manner that it covers (in other words, blocks) the liquid injection hole 12 from the outer surface 11b (specifically, the outer surface 15b of the metal wall portion 15) side of the metal lid body 11. The resin sealing member 18 is made of resin and has a disk shape. The resin sealing member 18 is preferably formed of a resin that has low permeability to the electrolyte 90 and high resistance to the electrolyte (resistance to the electrolyte 90), and is preferably formed of, for example, PPS (polyphenylene sulfide), PAS (polyarylene sulfide), olefin resin, or fluororesin.

[0027] The outer surface 11b of the metal cover 11 (specifically, the outer surface 15b of the metal wall portion 15) includes a circular annular seal surface 13 surrounding the opening 12b of the liquid injection hole 12 (see FIGS. 3 and 8). The resin sealing member 18 has an annular joint portion 18b that is airtightly joined to the annular seal surface 13 (see FIGS. 3 and 4). The annular joint portion 18b has a circular ring shape in a plan view. By having such an annular joint portion 18b, the resin sealing member 18 is airtightly joined to the metal cover 11 (specifically, the metal wall portion 15), and the liquid injection hole 12 is sealed by the resin sealing member 18. Therefore, it can be said that the sealed electricity storage device 1 is a sealed electricity storage device 1 in which the liquid injection hole 12 formed in the metal wall portion 15 of the device case 30 is appropriately sealed by the resin sealing member 18.

[0028] Particularly, in this embodiment, the annular seal surface 13 of the metal cover 11 (more specifically, the metal wall portion 15) is an annular roughened surface 14 having an uneven shape (see FIG. 4). This annular roughened surface 14 has a circular ring shape in a plan view (see FIG. 8). The resin sealing member 18 is hermetically joined to the annular roughened surface 14 in such a manner that the resin forming the annular joint portion 18b enters the recessed portion 14b of the annular roughened surface 14 (see FIG. 4). In other words, the annular joint portion 18b of the resin sealing member 18 is hermetically joined to the annular roughened surface 14 by an anchor effect caused by the protruding portion 14c of the annular roughened surface 14 of the metal wall portion 15 biting into the annular joint portion 18b of the resin sealing member 18. Therefore, the airtightness between the annular joint portion 18b of the resin sealing member 18 and the annular roughened surface 14 of the metal wall portion 15 is increased, and the airtightness of the sealed type electricity storage device 1 can be improved.

[0029] The annular roughened surface 14 can be formed by performing a known surface roughening treatment on the hole peripheral surface 16 of the outer surface 11b of the metal lid body 11. The hole peripheral surface 16 is a portion of the outer surface 11b of the metal lid body 11 (specifically, the outer surface 15b of the metal wall portion 15) located around the opening 12b of the liquid injection hole 12. Examples of the surface roughening treatment include laser surface treatment, sandblasting treatment, and anodizing treatment. Among these, examples of the laser surface treatment include the laser surface treatment disclosed in JP 2022-28587 A. In this embodiment, as described later, the hole peripheral surface 16 of the metal lid body 11 is made into the annular roughened surface 14 by laser surface treatment.

[0030] Moreover, in the sealed electricity storage device 1 of this embodiment, the resin sealing member 18 also functions as a safety valve member. That is, the resin sealing member 18 also functions as a safety valve member that prevents the internal pressure of the device case 30 from rising too high. For this reason, when the internal pressure of the device case 30 reaches a valve-opening pressure (release pressure), the resin sealing member 18 is broken, and the sealing of the liquid injection hole 12 by the resin sealing member 18 is released. This allows gas inside the device case 30 to be discharged to the outside of the device case 30 through the liquid injection hole 12, making it possible to prevent the internal pressure of the device case 30 from rising too high.

[0031] More specifically, when the internal pressure of the device case 30 increases due to the generation of gas inside the device case 30, the pressing force against the lower surface 18g of the resin sealing member 18 increases, and the stress generated in the resin sealing member 18 increases. Then, when the internal pressure of the device case 30 reaches the valve-opening pressure (releasing pressure), the stress generated in the resin sealing member 18 reaches the breaking strength of the resin sealing member 18, which causes the resin sealing member 18 to break (e.g., split open), forming an air hole in the resin sealing member 18, and releasing the seal of the liquid injection hole 12. As a result, the gas inside the device case 30 is discharged to the outside of the device case 30 through the liquid injection hole 12 (more specifically, the air hole formed in the resin sealing member 18), so that the internal pressure of the device case 30 can be prevented from rising too much.

[0032] In this way, by using the resin sealing member 18 also as a safety valve member, there is no need to provide a separate gas exhaust port in the device case 30, and further, there is no need to provide a separate safety valve member for sealing this gas exhaust port.

[0033] Next, a method for manufacturing the sealed electricity storage device 1 of the present embodiment will be described. Fig. 5 is a flowchart showing the flow of the method for manufacturing the sealed electricity storage device 1 according to the embodiment. First, in step S1 (assembly step), components of the sealed electricity storage device 1 are assembled to produce an assembly structure 1A (see Fig. 7).

[0034] Specifically, an electrode body 50 is produced using a plurality of positive electrode plates 60, a plurality of negative electrode plates 70, and a plurality of separators 80, in which the positive electrode plates 60 and the negative electrode plates 70 are alternately stacked in the stacking direction DL with the separators 80 interposed therebetween (see FIG. 3). In addition, a metal lid body 11 having a liquid injection hole 12 formed therein is prepared, and a positive electrode terminal member 41 and a negative electrode terminal member 42 are assembled to the metal lid body 11 (see FIGS. 1 and 3).

[0035] Thereafter, the positive electrode terminal member 41 assembled to the metal lid body 11 and the positive electrode plate 60 included in the electrode body 50 are connected via a positive electrode current collecting tab (not shown). Furthermore, the negative electrode terminal member 45 assembled to the metal lid body 11 and the negative electrode plate 70 included in the electrode body 50 are connected via a negative electrode current collecting tab (not shown). As a result, the metal lid body 11 and the electrode body 50 are integrated via the positive electrode terminal member 41 and the negative electrode terminal member 45.

[0036] Next, the electrode body 50 integrated with the metal lid 11 is housed inside the case body 21, and the opening 21b of the case body 21 is closed by the metal lid 11. In this state, the metal lid 11 and the case body 21 are welded all around. As a result, the case body 21 and the metal lid 11 are joined to form the device case 30, and the assembled structure 1A is produced (see FIG. 7). At this point, the liquid injection hole 12 is not sealed by the resin sealing member 18 and is open.

[0037] Next, in step S2 (pouring step), as shown in Fig. 7, the electrolyte 90 is poured into the inside of the device case 30 through the pouring hole 12 of the metal lid 11 of the assembled structure 1A. As a result, the inside of the electrode body 50 is impregnated with the electrolyte 90, and the electrolyte 90 is accommodated on the inside bottom side of the device case 30. In this embodiment, a non-aqueous electrolyte containing an organic solvent (e.g., ethylene carbonate, ethyl methyl carbonate, and dimethyl carbonate) and LiPF6 is used as the electrolyte 90.

[0038] Next, in step S3 (surface roughening step), the hole surrounding surface 16 of the metal lid body 11 is made into an annular roughened surface 14 by laser surface treatment (see FIG. 8). The hole surrounding surface 16 is a portion of the outer surface 11b of the metal lid body 11 (specifically, the outer surface 15b of the metal wall portion 15) located around the opening 12b of the liquid injection hole 12.

[0039] Specifically, as shown in Fig. 8, a laser beam LB is irradiated onto the hole peripheral surface 16 of the metal lid body 11 by a known laser device 110 to roughen the hole peripheral surface 16. The laser beam LB is irradiated in a circular manner along the outer periphery of the opening 12b of the liquid injection hole 12. More specifically, the laser beam LB is irradiated in a circular manner along the outer periphery of the opening 12b of the liquid injection hole 12, starting from a portion of the hole peripheral surface 16 of the metal lid body 11 that is closer to the opening 12b of the liquid injection hole 12, so as to draw a plurality of concentric circles. As a result, an annular roughened surface 14 having an uneven shape can be formed on the outer surface 11b of the metal lid body 11 (specifically, the outer surface 15b of the metal wall portion 15) as the annular sealing surface 13 surrounding the opening 12b of the liquid injection hole 12 (see Fig. 9).

[0040] Next, in step S4 (sealing step), the liquid injection hole 12 is sealed with a resin sealing member 18. In other words, the resin sealing member 18 that seals the liquid injection hole 12 is formed. Fig. 6 is a flowchart showing the flow of step S4 (sealing step) according to the embodiment. As shown in Fig. 6, step S4 (sealing step) includes step S41 (application step) and step S42 (solidification step).

[0041] Specifically, first, in step S41 (application step), molten resin MR is applied to the device case 30 from the outer surface 11b (specifically, the outer surface 15b of the metal wall portion 15) side of the metal cover body 11 so as to cover the annular roughened surface 14, which is the annular sealing surface 13, and the opening 12b of the liquid injection hole 12 (see Figs. 10 and 11). The molten resin MR is a melted resin for forming the resin sealing member 18. Fig. 10 is a plan view (top view) showing the state when the application step is being performed. Fig. 11 is a side view partial cross-sectional view showing the state when the application step is being performed, and corresponds to the E-E partial cross-sectional view of Fig. 10.

[0042] 10 and 11, step S41 (coating step) of this embodiment is performed using a heating device 130 (e.g., an infrared heater) having a heating part 131 and a die coater 120 having a nozzle 121. Specifically, while the annular roughened surface 14 is heated by the heating part 131 of the heating device 130, the molten resin MR is applied in the form of a film by the die coater 120 so as to cover the heated annular roughened surface 14 and the opening 12b of the liquid injection hole 12.

[0043] More specifically, the heating device 130 disposed above the outer surface 11b of the metal cover 11 (specifically, the outer surface 15b of the metal wall portion 15) is moved in the circumferential direction along the outer circumferential circle of the opening 12b of the liquid inlet 12 (in other words, the inner circumference of the annular roughened surface 14) with the central axis CL of the liquid inlet 12 as the rotation center axis (see FIGS. 10 and 11). As a result, the annular roughened surface 14 is heated sequentially in the circumferential direction by the heating portion 131 of the heating device 130. The heating by the movement of the heating device 130 ends when the heating portion 131 of the heating device 130 has made one revolution on the annular roughened surface 14 (i.e., when the heating device 130 has made one revolution with the central axis CL of the liquid inlet 12 as the rotation center axis). In addition, in the coating step of this embodiment, the temperature of the annular roughened surface 14 is made to be 100° C. or higher by heating by the heating device 130.

[0044] Further, the die coater 120 arranged above the outer surface 11b of the metal cover 11 (specifically, the outer surface 15b of the metal wall portion 15) is moved in the circumferential direction along the outer circumferential circle of the opening 12b of the liquid injection hole 12 (in other words, the inner circumference of the annular roughened surface 14) with the central axis CL of the liquid injection hole 12 as the rotation central axis while discharging the molten resin MR from the discharge port 122 of the nozzle 121 so as to follow the heating device 130 moving in this manner (see FIGS. 10 and 11). As a result, the molten resin MR can be applied in a film form by the die coater 120 so as to cover the annular roughened surface 14 heated by the heating device 130 and the opening 12b of the liquid injection hole 12. At this time, as shown in FIG. 12, a part of the molten resin MR applied onto the annular roughened surface 14 flows into the recess 14b of the annular roughened surface 14.

[0045] The width dimension W1 of the discharge port 122 of the nozzle 121 and the width dimension W2 of the molten resin MR discharged from the discharge port 122 of the nozzle 121 are equal to the radius of the disk-shaped molten resin film 18A (see FIG. 13) to be formed. As described later, the molten resin film 18A becomes the resin sealing member 18 by solidifying. Also, the die coater 120 rotates so that the discharge port 122 of the nozzle 121 rotates around the central axis CL of the liquid injection hole 12 while aligning one end 122b in the width direction with the position of the central axis CL of the liquid injection hole 12. Therefore, the film formed by the molten resin MR discharged from the discharge port 122 of the nozzle 121 has a fan shape centered on the position of the central axis CL of the liquid injection hole 12 in a plan view, and the central angle of the fan-shaped film becomes larger as the rotational movement of the die coater 120 progresses.

[0046] Therefore, the nozzle 121 of the die coater 120 rotates once along the inner circumference of the annular roughened surface 14 (i.e., the die coater 120 rotates once around the central axis CL of the liquid inlet 12 as the central axis of rotation), thereby forming a disk-shaped molten resin film 18A that covers the annular roughened surface 14 and the opening 12b of the liquid inlet 12 (see FIG. 13). Therefore, the application of the molten resin MR by the movement of the die coater 120 ends when the nozzle 121 of the die coater 120 rotates once along the inner circumference of the annular roughened surface 14 (i.e., when the die coater 120 rotates once around the central axis CL of the liquid inlet 12 as the central axis of rotation). Note that FIG. 13 is a plan view of the molten resin film 18A and the device case 30 from above the device case 30 at the time when the application process is completed.

[0047] Next, in step S42 (solidification step), the molten resin film 18A made of the molten resin MR is solidified to form the resin sealing member 18. In this embodiment, the molten resin film 18A is solidified by natural cooling. This forms a disk-shaped resin sealing member 18 having an annular joint portion 18b that is airtightly joined to the "annular seal surface 13 surrounding the opening 12b of the liquid injection hole 12 in the outer surface 15b of the metal wall portion 15" (see FIGS. 1 and 3). This manufactures a sealed electricity storage device 1 in which the liquid injection hole 12 formed in the metal wall portion 15 of the device case 30 is properly sealed by the resin sealing member 18 made of resin.

[0048] Particularly, in this embodiment, the annular seal surface 13 is an annular roughened surface 14 having an uneven shape. Therefore, in step S41 (application step), as shown in FIG. 12, a part of the molten resin MR applied onto the annular roughened surface 14 flows into the recessed portion 14b of the annular roughened surface 14. As a result, by solidifying the molten resin MR in step S42 (solidification step), as shown in FIG. 4, a resin sealing member 18 is formed in which the annular joint portion 18b is airtightly joined to the annular roughened surface 14 in a manner in which a part of the resin forming the annular joint portion 18b enters the recessed portion 14b of the annular roughened surface 14. Therefore, the airtightness between the annular joint portion 18b of the resin sealing member 18 and the annular roughened surface 14 of the metal wall portion 15 is increased, and the airtightness of the sealed type electricity storage device 1 can be improved.

[0049] Incidentally, in step S2 (pouring step), when the electrolyte solution 90 is injected into the device case 30 through the injection hole 12 of the metal lid 11, the electrolyte solution 90 may adhere to a portion of the outer surface 11b of the metal lid 11 that is located around the opening 12b of the injection hole 12 (i.e., the hole peripheral surface 16). Therefore, if the injection step is performed after the surface roughening step, the electrolyte solution 90 may adhere to the annular roughened surface 14 when the injection step is performed, and then the sealing step may be performed with the electrolyte solution 90 adhered to the annular roughened surface 14. In this case, the components of the electrolyte solution 90 may be present between the annular roughened surface 14 of the metal lid 11 and the annular joint portion 18b of the resin sealing member 18. Such an embodiment is not considered to be a preferable embodiment.

[0050] In contrast, in this embodiment, a surface roughening step (step S3) using laser surface treatment is performed before the sealing step (step S4) and after the liquid injection step (step S2). As a result, even if the electrolytic solution 90 adheres to the hole peripheral surface 16 of the metal lid body 11 in step S2 (liquid injection step), the electrolytic solution 90 adhering to the hole peripheral surface 16 can be evaporated and removed by irradiating the hole peripheral surface 16 (the portion to be made into the annular roughened surface 14) of the metal lid body 11 with a laser beam LB in step S3 (surface roughening step). As a result, the annular roughened surface 14 to which the electrolytic solution 90 does not adhere can be formed. Therefore, in this embodiment, the sealing step can be performed in a state in which the electrolytic solution 90 does not adhere to the annular roughened surface 14, so that the electrolytic solution 90 can be prevented from being interposed between the annular roughened surface 14 of the metal lid body 11 and the annular joint portion 18b of the resin sealing member 18.

[0051] Although the present invention has been described above with reference to an embodiment, it goes without saying that the present invention is not limited to the above embodiment and can be modified as appropriate without departing from the spirit of the present invention.

[0052] For example, in the coating process of the embodiment, a die coater 120 positioned above the outer surface 11b of the metal lid body 11 is moved circumferentially along the outer circumferential circle of the opening 12b of the liquid injection hole 12, with the central axis CL of the liquid injection hole 12 as the rotation center axis, while ejecting molten resin MR from the outlet 122 of the nozzle 121, to form a disk-shaped molten resin film 18A.

[0053] However, a rectangular plate-shaped molten resin film 218A may be formed using a die coater 320 in which a width dimension W3 of a discharge port 322 of a nozzle 321 is larger than the diameter of the liquid injection hole 12. Then, the molten resin film 218A may be solidified to form a rectangular plate-shaped resin sealing member 218 (see FIGS. 14 to 17). This manufacturing method will be specifically described below as a manufacturing method according to a modified embodiment.

[0054] First, the coating step will be described. Specifically, first, the die coater 320 is disposed above the outer surface 11b of the metal cover body 11 in such a position that the width direction DW of the discharge port 322 of the die coater 320 is perpendicular to the stacking direction DL of the electrode body 50 and the discharge port 322 faces downward (see FIGS. 14 and 15). However, the die coater 320 is disposed so that the discharge port 322 of the die coater 320 is adjacent to one side (left side in FIGS. 14 and 15) of the opening 12b of the liquid injection hole 12 in the stacking direction DL in a plan view, and the center of the width direction of the discharge port 322 and the central axis CL of the liquid injection hole 12 are spaced apart in the stacking direction DL in a plan view. At this time, the discharge port 322 of the die coater 320 is disposed above the annular roughened surface 214 and in a position facing the annular roughened surface 214. As shown in FIG. 16, the annular roughened surface 214 in this modified embodiment is annular and surrounds the opening 12b of the liquid inlet 12, and in plan view has a circular inner circumference (specifically, a circle that follows the outer circumference of the opening 12b of the liquid inlet 12) and a rectangular outer circumference.

[0055] Next, while discharging the molten resin MR from the discharge port 322 of the nozzle 321, the die coater 320 is moved to the other side of the stacking direction DL (the right side in FIGS. 14 and 15). Then, after the discharge port 322 of the nozzle 321 passes above the opening 12b of the liquid injection hole 12, the discharge of the molten resin MR from the discharge port 322 is stopped. As a result, the molten resin MR is applied to the annular roughened surface 214 of the outer surface 15b of the metal wall portion 15, and the molten resin MR can be applied in a film shape so as to bridge over the liquid injection hole 12 and cover the liquid injection hole 12. That is, the molten resin MR is applied in a film shape by the die coater 120 so as to cover the annular roughened surface 214 and the opening 12b of the liquid injection hole 12, thereby forming a rectangular plate-shaped molten resin film 218A (see FIG. 17). 12, a portion of the molten resin MR applied onto annular rough surface 214 flows into recesses 214b of annular rough surface 214. Prior to application of the molten resin MR by die coater 320, it is preferable to heat annular rough surface 214 by a heating device (not shown).

[0056] Next, in a solidification process, the molten resin film 218A made of the molten resin MR is solidified to form a rectangular plate-shaped resin sealing member 218 (see FIG. 17). This forms a rectangular plate-shaped resin sealing member 218 having an annular joint portion 218b that is airtightly joined to the "annular roughened surface 214 surrounding the opening 12b of the liquid injection hole 12 on the outer surface 15b of the metal wall portion 15."

[0057] In the embodiment, the molten resin MR is applied to the device case 30 from the outer surface 11b side of the metal lid body 11 so as to cover the annular roughened surface 14 and the opening 12b of the liquid injection hole 12, and the applied molten resin MR is solidified to form the resin sealing member 18 that seals the liquid injection hole 12. However, as described below, a resin film prepared in advance may be welded to the outer surface 11b of the metal lid body 11 to form a resin sealing member made of a resin film.

[0058] Specifically, first, in the arrangement step, a resin film is arranged on the device case 30 so as to cover at least the annular roughened surface 14, which is the annular seal surface 13 of the outer surface 15b of the metal wall portion 15, and the liquid inlet hole 12 from the outer surface 15b side of the metal wall portion 15. Next, in the melting step, the portion of the resin film located on the annular roughened surface 14 is melted to form a molten resin. At this time, a portion of the molten resin located on the annular roughened surface 14 flows into the recess 14b of the annular roughened surface 14. Next, in the solidification step, the molten resin is solidified to form an annular joint that is airtightly joined to the annular roughened surface 14, and a resin sealing member that seals the liquid inlet hole 12 is formed. More specifically, a resin sealing member in which the annular joint is airtightly joined to the annular roughened surface 14 is formed in such a manner that a portion of the resin forming the annular joint enters into the recess 14b of the annular roughened surface 14. In this manufacturing method, the sealing step includes an arrangement step, a melting step, and a solidification step.

[0059] In the embodiment, the sealed electricity storage device 1 is shown as having a liquid inlet 12 formed in the metal wall portion 15 of the metal lid 11 and a resin sealing member 18 that seals the liquid inlet 12. However, the present invention also includes a sealed electricity storage device in which a liquid inlet is formed in the metal wall portion of the case main body 21 and a resin sealing member that seals the liquid inlet. [Explanation of symbols]

[0060] 1. Sealed energy storage device 11 Metal cover 11b Outer surface of metal cover 12 Liquid injection hole 12b Inlet hole opening 13 Annular sealing surface 14,214 Annular roughened surface 14b,214b Recess 15 Metal wall 15b Outer surface of metal wall 18,218 Resin sealing member (sealing member) 18A, 218A Molten resin film 18b,218b Circular joint 21 Case body 30 Device Cases 50 Electrode body 90 Electrolyte MR Melt Resin S2 Liquid injection process S4 Sealing process S41 Coating process S42 Solidification process

Claims

1. a device case having a metal wall portion with a liquid injection hole formed therein; a sealing member that seals the liquid injection hole in a manner that covers the liquid injection hole from an outer surface side of the metal wall portion. In a sealed electricity storage device, the sealing member is a resin sealing member made of resin, the outer surface of the metal wall portion includes an annular seal surface surrounding an opening of the liquid injection hole, the resin sealing member has an annular joint portion that is airtightly joined to the annular seal surface, The annular sealing surface is an annular roughened surface having nanometer-order irregularities, The resin sealing member is hermetically joined to the annular roughened surface in such a manner that the resin forming the annular joint enters into a recess in the annular roughened surface. Sealed energy storage device.

2. The sealed electricity storage device according to claim 1 , The resin sealing member also serves as a safety valve member, When the internal pressure of the device case reaches a valve opening pressure, the resin sealing member is destroyed, and the sealing of the liquid injection hole by the resin sealing member is released. Sealed energy storage device.

3. A method for manufacturing a sealed electricity storage device, comprising: The sealed electricity storage device is a device case having a metal wall portion with a liquid injection hole formed therein; a sealing member that seals the liquid inlet hole in a manner that covers the liquid inlet hole from an outer surface side of the metal wall portion, the sealing member is a resin sealing member made of resin, the outer surface of the metal wall portion includes an annular seal surface surrounding an opening of the liquid injection hole, the resin sealing member has an annular joint portion that is airtightly joined to the annular seal surface, The method for producing the sealed electricity storage device includes the steps of: a liquid injection step of injecting an electrolyte into the inside of the device case through the liquid injection hole; a sealing step of sealing the liquid injection hole in a manner that covers the liquid injection hole from the outer surface side of the metal wall portion with the resin sealing member, The sealing step includes: a coating step of coating the device case with a molten resin from the outer surface side of the metal wall portion so as to cover at least the annular seal surface and the liquid injection hole of the outer surface of the metal wall portion; and a solidification process for solidifying the molten resin to form the resin sealing member having the annular joint portion that is airtightly joined to the annular seal surface. A method for manufacturing a sealed electricity storage device.

4. A method for producing the sealed electricity storage device according to claim 3, comprising the steps of: The annular sealing surface is an annular roughened surface having an uneven shape, In the coating step, when the molten resin is applied to the device case from the outer surface side of the metal wall portion so as to cover at least the annular roughened surface and the liquid injection hole of the outer surface of the metal wall portion, a portion of the molten resin applied to the annular roughened surface flows into a recess of the annular roughened surface, In the solidification step, The molten resin is solidified to form the resin sealing member that is airtightly joined to the annular roughened surface in such a manner that the resin that forms the annular joint portion enters the recess of the annular roughened surface. A method for manufacturing a sealed electricity storage device.

Citation Information

Patent Citations

  • Sealed battery

    JP2006172975A

  • Sealed battery

    JP2007066600A

  • Sealing plug and battery

    JP2008130273A

  • Manufacturing method of sealed battery

    JP2009181906A

  • Secondary battery having electrolyte injecting inlet, and method of manufacturing the same