Battery pulse heating durability test method and system, and data table generation method
The battery pulse heating durability test method addresses the issue of long test durations in traditional testing by using continuous pulse heating and temperature adjustments to efficiently evaluate battery durability.
Patent Information
- Application Number
- JP2022509665
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-08-29
- Filing Date
- 2020-08-27
- Publication Date
- 2024-11-28
- Estimated Expiration
- 2040-08-27
AI Technical Summary
Traditional power battery durability testing requires long periods at low temperatures between charging and discharging processes, leading to prolonged test durations.
A battery pulse heating durability test method involving continuous pulse heating until a stable temperature is reached, followed by adjusting the temperature chamber to obtain a capacity reduction value, and generating a data table reflecting battery durability under different pulse heating parameters.
This method significantly shortens test time and test cycles by eliminating the need for long periods at low temperatures, allowing for efficient evaluation of battery durability through multiple experiments.
Smart Images

Figure 0007591559000002 
Figure 0007591559000003 
Figure 0007591559000004
Abstract
Description
[Technical field]
[0001] The present application relates to the technical field of battery management, and in particular to a battery pulse heating durability test method and system and a data table generation method. [Background technology]
[0002] With the development of the automobile industry, China has grown into the largest country in terms of automobile growth. Under the trend of global warming and rising oil prices, new energy vehicles have become the focus of research and development in the current automobile industry. Today, electric vehicles are the focus of new energy vehicle development, but the performance of electric vehicles closely depends on the performance of lithium-ion batteries. The durability of lithium-ion batteries is an important indicator for judging the overall performance of electric vehicles. The durability of lithium-ion batteries is generally judged by the number of charge and discharge cycles required when the capacity of the battery has decreased to a certain percentage of its initial capacity.
[0003] The conventional durability test of a power battery detects the decrease in battery capacity after the battery is charged and discharged multiple times, thereby reflecting the durability of the battery. However, the conventional durability test of a power battery requires a long time at low temperature between two charging and discharging processes, which results in a long test period. Summary of the Invention [Problem to be solved by the invention]
[0004] In order to address the problem of conventional power battery durability testing, which requires a long period of standing at low temperature between the two processes of charging and discharging, causing the problem of a long test period, it is necessary to provide a method and system for battery pulse heating durability testing and a data table generation method. [Means for solving the problem]
[0005] A battery pulse heating durability test method, comprising: S10, providing a battery to be tested, placing the battery to be tested in a temperature chamber, and setting a temperature of the temperature chamber to a first temperature value; S20, performing pulse heating of the battery to be tested under first pulse parameters until the pulse heating time reaches a preset pulse duration, and obtaining a stable temperature; S30, adjusting the temperature of the temperature chamber to a second temperature value and obtaining a capacity fade value of the battery being tested at the second temperature value; S40, obtaining the durability of the tested battery at a stable temperature after pulse heating under a first pulse parameter according to a preset pulse duration and capacity degradation value.
[0006] In one embodiment, the step S20 of performing pulse heating of the battery to be tested under first pulse parameters until the pulse heating time reaches a preset pulse duration and obtaining a stable temperature includes: S210, charging at a first amplitude value in a constant current mode for a second time value; S220, discharging at a first amplitude value in a constant current mode for a second time value, where a sum of two second time values is a pulse period value, and the first pulse parameters include the first amplitude value and the pulse period value; S230, repeating steps S210 to S220, and stopping the pulse heating when the pulse heating time reaches the preset pulse duration.
[0007] In one embodiment, the step S40 of obtaining the durability of the tested battery at a stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and capacity fade value includes: Obtaining a pulse heating time according to a preset pulse duration and pulse period value; Obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity fade value.
[0008] In one embodiment, the step S30 of adjusting the temperature of the temperature chamber to a second temperature value and obtaining a capacity fade value of the battery being tested at the second temperature value includes: S310, adjusting the temperature of the temperature chamber to a second temperature value and allowing the temperature chamber to stand for a first time value; S320, discharging the battery to be tested at a lower cut-off voltage in a constant current mode at a second amplitude value and leaving the battery for a fourth time value; S330, charging the battery to be tested at a second amplitude value in a constant current mode to an upper cutoff voltage of the battery to be tested, then charging the battery to be tested at a constant voltage mode until the current of the battery to be tested decreases to a third amplitude value, allowing to stand for a fourth time value, and obtaining a current battery discharge capacity value of the battery to be tested; S340, repeating steps S320 to S330 for a preset time, and obtaining an average battery discharge capacity value to obtain a capacity degradation value of the tested battery.
[0009] A data table generation method used to reflect the durability of a battery under different pulse heating parameters, comprising: providing a plurality of groups of cells to be tested, each group having a plurality of cells; Placing each battery to be tested in each group into a temperature chamber, performing pulse heating of the battery to be tested in each group until a pulse heating time reaches a preset pulse duration, and obtaining a stable temperature of the battery to be tested; adjusting the temperature of each temperature chamber to a second temperature value and obtaining a capacity fade value for each battery being tested at the second temperature value; generating a data table according to the corresponding pulse heating parameters of each battery being tested and the capacity fade value of each battery being tested; wherein the corresponding pulse heating parameters of the tested batteries of the same group are the same, while the corresponding pulse heating parameters of the tested batteries of different groups are different, and the pulse heating parameters include: stable temperature of the battery, state of charge of the battery, pulse period, pulse amplitude value, and pulse duration.
[0010] A battery pulse heating durability test system, comprising: a pulse heating device electrically connected to the battery to be tested and used for performing pulse heating of the battery to be tested under first pulse parameters until a pulse heating time reaches a preset pulse duration and for obtaining a stable temperature; a capacity fade acquisition device electrically connected to the battery under test and used to acquire a capacity fade value of the battery under test at a second temperature value after the pulse heating is stopped when the pulse heating time reaches a preset pulse duration; and a processing device electrically connected to the pulse heating device and the capacity decline acquisition device, respectively, and used to acquire the durability of the tested battery at a stable temperature after pulse heating under first pulse parameters according to a preset pulse duration and capacity decline value.
[0011] In one embodiment, the pulse heating device comprises: a temperature chamber used to place the battery to be tested and to provide stable temperature conditions for the battery to be tested; and a pulse heating element electrically connected to the battery to be tested and used to provide a charge-discharge pulse heating cycle under first pulse parameters until the pulse heating time reaches a preset pulse duration.
[0012] In one embodiment, the pulse heating element comprises: a charging unit electrically connected to the battery under test and used to charge the battery under test at the first amplitude value for the second time value; a discharge unit electrically connected to the battery to be tested and used to discharge the battery to be tested at a first amplitude value in a constant current mode for a second time value, the sum of the two second time values being a pulse period value of the pulse heating.
[0013] In one embodiment, the processing device comprises: A first acquisition module is electrically connected to the charging unit and the discharging unit, respectively, and is used to acquire a pulse heating time according to a preset pulse duration and period value; and a first data processing module electrically connected to the first acquisition module and used to acquire the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity fade value.
[0014] In one embodiment, a capacity degradation acquisition device includes: a first test module electrically connected to the battery to be tested, used for charging in a constant current mode at a second amplitude value to an upper cutoff voltage, then charging in a constant voltage mode until the current in the battery decreases to a third amplitude value, and allowing to stand for a fourth time value, and further used for discharging in a constant current mode at the second amplitude value to a lower cutoff voltage, and allowing to stand for a fourth time value; and a second data processing module electrically connected to the first testing module and used to obtain a battery capacity value of the battery being tested multiple times to obtain a capacity degradation value of the battery being tested.
[0015] In one embodiment, the second data processing module comprises: A second acquisition unit is electrically connected to the first test module, and is used for acquiring battery discharge capacity values of the batteries to be tested multiple times and calculating an average battery discharge capacity value; and a second processing unit electrically connected to the second acquisition unit, used for acquiring a capacity degradation value of the battery to be tested according to the battery discharge capacity value of the battery to be tested and the preset battery discharge capacity value.
[0016] The above-mentioned battery pulse heating durability test method includes: putting the battery to be tested into a temperature chamber, and setting the temperature of the temperature chamber to a first temperature value; performing pulse heating of the lithium ion battery under the first pulse parameters until the pulse heating time reaches a preset duration; adjusting the temperature of the temperature chamber to a second temperature value; obtaining the capacity drop value of the battery to be tested at the second temperature value; and obtaining the durability of the battery to be tested after pulse heating under the first pulse parameters according to the preset pulse duration and capacity drop value. In the battery pulse heating durability test method provided by the present application, continuous pulse heating is performed before testing the capacity drop value of the battery to be tested. After the battery is heated for a certain period of time, the temperature rise and heat dissipation of the battery will reach a stable value and the temperature will no longer rise. Such pulse heating does not need to be left at a low temperature for a long time. This can greatly shorten the test time, shorten the test period, and verify the effect of battery temperature on the durability of the battery through a large number of experiments. [Brief description of the drawings]
[0017] [Figure 1] 2 is a flow chart of a battery pulse heating durability test method provided by an embodiment of the present application. [Diagram 2] FIG. 2 is a result diagram of a battery pulse heating durability test method provided by an embodiment of the present application. [Diagram 3] FIG. 2 is a structural connection diagram of a battery pulse heating durability test system provided by an embodiment of the present application. [Figure 4] FIG. 2 is a structural connection diagram of a battery pulse heating durability test system provided by an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] In order to make the above-mentioned objects, features and advantages of the present application more clear and easily understood, a specific implementation method of the present application will be described in detail by referring to the following attached drawings. In the following description, many details are provided to fully understand the present application. However, the present application is not limited to the specific implementation disclosed below, since the present application can be implemented in many ways different from this description, and those skilled in the art can make similar modifications without departing from the spirit of the present application.
[0019] It should be noted that when an element is said to be "disposed on" another element, the element may be directly on the other element, or there may be intermediate elements present. When an element is considered to be "connected" to another element, the element may be directly connected to the other element, or there may be intermediate elements present as well.
[0020] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this application pertains. The terms used in the specification of this application herein are intended only to describe certain embodiments and are not intended to limit this application. The term "and / or" used herein includes any one or more of the associated listed items, and all combinations thereof.
[0021] See Figure 1. The present application provides a battery pulse heating durability test method. The method includes:
[0022] S10, providing a battery to be tested, placing the battery to be tested in a temperature chamber, and setting the temperature of the temperature chamber to a first temperature value. The battery to be tested can be a lithium ion battery and can be in multiple forms, such as soft package, square and cylinder. The temperature chamber can be a high and low temperature explosion-proof temperature chamber. In an optional embodiment, the temperature chamber is a Bell high and low temperature explosion-proof temperature chamber. The Bell high and low temperature explosion-proof temperature chamber can provide a charging and discharging environment of the temperature of the battery in the chamber. The inside of the temperature chamber may have a temperature sensor and a cold air outlet. The temperature chamber can also adjust the humidity inside the chamber. The first temperature value can be -20°C, -10°C, 10°C, 30°C, etc.
[0023] S20, performing pulse heating of the battery to be tested under first pulse parameters until the pulse heating time reaches a preset pulse duration, and obtaining a stable temperature of the battery to be tested. The first pulse parameters include a pulse period and a pulse amplitude value. The preset pulse duration can be 100 hours. The stable temperature is the temperature when the temperature rise and heat dissipation of the battery are stable.
[0024] S30, adjusting the temperature of the temperature chamber to a second temperature value, and obtaining a capacity fade value of the battery being tested at the second temperature value. The second temperature value can be room temperature. The capacity fade value is a ratio of the current actual discharge capacity to the initial discharge capacity.
[0025] S40, obtaining a durability of the tested battery at a stable temperature after pulse heating under the first pulse parameters according to a preset pulse duration and a capacity fade value. The durability reflects a capacity fade value of the battery at the first temperature value after a preset period of pulse heating under the first pulse parameters. In an optional embodiment, obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the preset pulse duration and capacity fade value can be obtaining a pulse heating time according to a preset pulse duration and pulse period value, and obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity fade value.
[0026] In an optional embodiment, after the step of obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the preset pulse duration and capacity degradation value, steps S10 to S40 can be repeated to obtain the durability of the tested battery after pulse heating under the first pulse parameters for two preset pulse durations.
[0027] In this embodiment, in the above-mentioned battery pulse heating durability test method, before testing the capacity drop value of the battery to be tested, continuous pulse heating is performed. After the battery is heated for a certain period of time, the temperature rise and heat dissipation of the battery will reach a stable value and the temperature will no longer rise. Such pulse heating does not need to be left at a low temperature for a long time. This can greatly shorten the test time, shorten the test period, and verify the effect of battery temperature on the durability of the battery through a large number of experiments.
[0028] In one embodiment, the step of performing pulse heating of the battery to be tested under the first pulse parameters until the pulse heating time reaches the preset pulse duration, and the step of obtaining a stable temperature of the battery to be tested S20 can include the steps of charging at a first amplitude value in a constant current mode for a second time value, discharging at a first amplitude value in a constant current mode for a second time value, where the sum of the two second time values is a pulse period value, and the first pulse parameters include the first amplitude value and the pulse period value, repeating the pulse charging and discharging steps multiple times, and stopping the pulse heating when the pulse heating time reaches the preset pulse duration. After the temperature of the temperature chamber is set to the temperature value, the battery is subjected to continuous pulse operation under the parameters. Eventually, the temperature rise and heat dissipation of the battery will reach a stable value and the temperature will not increase significantly. The battery is continuously heated in this state until the pulse heating time reaches the preset pulse duration. Such a pulse heating method saves a lot of test time and shortens the test period. See Table 1. The table shows the specific parameters and stable test temperature values of the 10 tested batteries. All 10 batteries tested are at 50% SOC and are provided with various pulse parameters and environmental temperatures. [Table 1]
[0029] After the above ten tested batteries are continuously acted on for a certain period of time, the pulse is withdrawn and the capacity loss value of the tested batteries is measured respectively. The test results are shown in Figure 2. Without considering the temperature of the battery temporarily, the capacity loss is faster under the action of the high amplitude pulse with a large period. The loss value is analyzed. The battery with the highest capacity loss rate is battery F. Its capacity is reduced by 1% under the action of the pulse with an amplitude value of 4C and a period of 8 seconds. The action of the pulse current needs to continue for about 130 hours without stopping. At 500 hours, the capacity is reduced by only 2.5%.
[0030] Under the same pulse parameters, the lower the temperature, the faster the lifespan will decrease, but different batteries with the same parameters and different temperatures will not show significant differences in degradation. In contrast, the effects of amplitude and period on lifespan are more obvious.
[0031] In one embodiment, the step of adjusting the temperature of the temperature chamber to a second temperature value and obtaining a capacity fade value of the tested battery at the second temperature value S30 includes:
[0032] S310, adjusting the temperature of the temperature chamber to a second temperature value and allowing to stand for a first time value; S320, discharging to a lower cut-off voltage at a second amplitude value in a constant current mode and allowing to stand for a fourth time value; S330, charging to an upper cut-off voltage of the battery being tested at the second amplitude value in a constant current mode, then charging to an upper cut-off voltage of the battery being tested at a constant voltage mode until the current of the battery being tested decreases to a third amplitude value, allowing to stand for a fourth time value and obtaining a current battery discharge capacity value of the battery being tested; S340, repeating steps S320 to S330 for a preset time and obtaining an average battery discharge capacity value to obtain a capacity decay value of the battery being tested.
[0033] In an optional embodiment, to obtain the current battery discharge capacity value, after the pulse heating is stopped, the battery can be placed in a temperature chamber and the temperature of the temperature chamber can be adjusted to 25°C. After being left for a sufficient time, the battery is discharged in 1 / 3C constant current mode to the lower cut-off voltage, and then left for 3 hours. Then, the battery is discharged in 1 / 3C constant current mode to the upper cut-off voltage, and then charged in constant voltage mode until the current drops to 1 / 20C, and left for 3 hours. The discharge and charge process is repeated three times. The average of the capacity test data obtained in the three tests is used as the current actual discharge capacity of the battery. The initial capacity of the battery is obtained by the above method before the pulse heating to obtain the capacity degradation value from the ratio of the current actual discharge capacity to the initial discharge capacity.
[0034] One embodiment of the present application provides a method for generating a data table used to reflect the durability of a battery under different pulse heating parameters. The method for generating the data table includes:
[0035] providing a plurality of groups of batteries to be tested, each group having a plurality of batteries; placing each battery to be tested of each group into a temperature chamber; performing pulse heating of the batteries to be tested of each group until a pulse heating time reaches a preset pulse duration, and obtaining a stable temperature of the batteries to be tested; adjusting a temperature of each temperature chamber to a second temperature value, and obtaining a capacity fade value of each battery to be tested at the second temperature value; and generating a data table according to corresponding pulse heating parameters of each battery to be tested and the capacity fade value of each battery to be tested.
[0036] Here, the corresponding pulse heating parameters of the tested batteries of the same group are the same, while the corresponding pulse heating parameters of the tested batteries of different groups are different, and the pulse heating parameters include the stable temperature of the battery, the charge state of the battery, the pulse period, the pulse amplitude value, and the pulse duration.
[0037] In this embodiment, multiple groups of tests were conducted by the aforementioned durability test method for the same model of battery under different pulse parameters and different temperatures. Finally, a durability scatter diagram with at least six dimensions (i.e., a data table) can be established. The six variables include five independent variables and one dependent variable. The five independent variables are battery temperature, battery state of charge, pulse period, pulse amplitude value, and pulse duration. The dependent variable is the capacity degradation value. Using the data table, the sensitivity of each factor can be analyzed, and in combination with the actual needs, the pulse heating rate and the aforementioned durability results can be compared and examined to perform joint optimization to complete the creation of a pulse heating solution.
[0038] See Fig. 3. One embodiment of the present application provides a battery pulse-heating durability test system 10. The battery pulse-heating durability test system 10 includes a pulse heating device 100, a capacity fade acquisition device 200, and a processing device 300.
[0039] The pulse heating device 100 is electrically connected to the battery to be tested. The pulse heating device 100 is used for performing pulse heating of the battery to be tested under a first pulse parameter until the pulse heating time reaches a preset pulse duration, and for acquiring a stable temperature of the battery to be tested. The capacity loss acquisition device 200 is electrically connected to the battery to be tested. The capacity loss acquisition device 200 is used for acquiring a capacity loss value of the battery to be tested at a second temperature value after the pulse heating is stopped when the pulse heating time reaches a preset pulse duration. The processing device 300 is electrically connected to the pulse heating device 100 and the capacity loss acquisition device 200, respectively. The processing device 300 is used for acquiring the durability of the battery to be tested at a stable temperature after pulse heating under the first pulse parameter according to the preset pulse duration and capacity loss value. The pulse heating device may include a charger capable of providing positive and negative pulses. The capacity loss acquisition device 200 may include a current flow sensor. The processing device 300 may be a microprocessor, a single chip microcomputer (SCM), etc.
[0040] In one embodiment, the pulse heating apparatus 100 includes a temperature chamber 110 and a pulse heating element 120 .
[0041] The temperature chamber 110 is used to place the battery to be tested and provide a stable temperature condition for the battery to be tested. The pulse heating element 120 is electrically connected to the battery to be tested and is used to provide a charge-discharge pulse heating cycle under a first pulse parameter until the pulse heating time reaches a preset pulse duration. The temperature chamber is a Bell high and low temperature explosion-proof temperature chamber. The Bell high and low temperature explosion-proof temperature chamber can provide a temperature charging and discharging environment for the battery in the chamber. The inside of the temperature chamber may have a temperature sensor and a cold air outlet. The temperature chamber can also adjust the humidity inside the chamber. The first temperature value can be -20°C, -10°C, 10°C, 30°C, etc.
[0042] The pulse heating element 120 includes a charging unit 121 and a discharging unit 122. The charging unit 121 is electrically connected to the battery to be tested and is used to charge the battery to be tested at a first amplitude value for a second time value. The discharging unit 122 is electrically connected to the battery to be tested and is used to discharge the battery to be tested at a first amplitude value in a constant current mode for a second time value, where the sum of the two second time values is a pulse period value of the pulse heating.
[0043] The processing device 300 includes a first acquisition module 310 and a first data processing module 320. The first acquisition module 310 is electrically connected to the charging unit 121 and the discharging unit 122, respectively, and is used to acquire a pulse heating time according to a preset pulse duration and period value. The first data processing module 320 is electrically connected to the first acquisition module 310, and is used to acquire the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity degradation value.
[0044] The capacity degradation acquisition device 200 includes a first test module 210 and a second data processing module 220. The first test module 210 is electrically connected to the battery to be tested and is used for charging in a constant current mode with a second amplitude value to an upper cut-off voltage, then charging in a constant voltage mode until the current of the battery decreases to a third amplitude value, leaving for a fourth time value, and further used for discharging in a constant current mode with the second amplitude value to a lower cut-off voltage, and leaving for a fourth time value. The second data processing module 220 is electrically connected to the first test module 210 and is used to acquire the battery capacity value of the battery to be tested multiple times to acquire the capacity degradation value of the battery to be tested.
[0045] The second data processing module 220 includes a second acquisition unit 221 and a second processing unit 222. The second acquisition unit 221 is electrically connected to the first test module 210 and is used for acquiring the battery discharge capacity value of the battery to be tested multiple times and calculating the average battery discharge capacity value. The second processing unit 222 is electrically connected to the second acquisition unit 221 and is used for acquiring the capacity degradation value of the battery to be tested according to the battery discharge capacity value of the battery to be tested and the preset battery discharge capacity value.
[0046] In this embodiment, in the above-mentioned battery pulse heating durability test system 10, before the capacity drop acquisition device 200 tests the capacity drop value of the battery to be tested, continuous pulse heating is performed via the pulse heating device 100. After the battery is heated for a certain period of time, the temperature rise and heat dissipation of the battery will reach a stable value and the temperature will no longer rise. Such pulse heating does not need to be left at a low temperature for a long time. This can greatly shorten the test time, shorten the test period, and verify the effect of battery temperature on the durability of the battery through a large number of experiments.
[0047] The technical features of the above-mentioned embodiments can be freely combined. For the sake of brevity, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combinations of these technical features, they should be considered to be within the scope of this specification.
[0048] The above embodiments merely represent some implementation methods of the present application. Although the descriptions are specific and detailed, they should not be understood as limitations on the scope of the pending patent. It should be noted that those skilled in the art can make various changes and modifications to the embodiments without departing from the concept of the present application. All of these are included in the scope of protection of the present application. Therefore, the scope of protection of the patent based on the present application shall be subject to the scope of the attached claims. This specification includes the disclosure of the following inventions. [Item 1] A battery pulse heating durability test method, S10, providing a battery to be tested, placing the battery to be tested in a temperature chamber, and setting a temperature of the temperature chamber to a first temperature value; S20, performing pulse heating of the battery under test under first pulse parameters until a pulse heating time reaches a preset pulse duration, and obtaining a stable temperature; S30, adjusting the temperature of the temperature chamber to a second temperature value and obtaining a capacity fade value of the tested battery at the second temperature value; S40. obtaining a durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity degradation value. [Item 2] The step S20 of performing pulse heating of the battery under test under first pulse parameters until the pulse heating time reaches the preset pulse duration, and obtaining a stable temperature, S210, charging at a first amplitude value in a constant current mode for a second time value; S220, discharging at the first amplitude value in a constant current mode for the second time value, where a sum of two second time values is a pulse period value, and the first pulse parameters include the first amplitude value and the pulse period value; 2. The battery pulse heating durability test method according to claim 1, further comprising: S230, repeating steps S210 to S220, and stopping pulse heating when the pulse heating time reaches the preset pulse duration. [Item 3] The step S40 of acquiring the durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity degradation value, Obtaining a pulse heating time according to the preset pulse duration and the pulse period value; and obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity degradation value. [Item 4] The step S30 of adjusting the temperature of the temperature chamber to a second temperature value and obtaining the capacity degradation value of the battery under test at the second temperature value, S310, adjusting the temperature of the temperature chamber to a second temperature value and allowing time for a first time value; S320, discharging the battery under test at a second amplitude value in a constant current mode to a lower cut-off voltage of the battery under test, and leaving the battery for a fourth time value; S330, charging the battery under test at the second amplitude value in a constant current mode to an upper cutoff voltage of the battery under test, then charging the battery under test at a constant voltage mode until the current of the battery under test decreases to a third amplitude value, allowing to stand for the fourth time value, and obtaining a current battery discharge capacity value of the battery under test; 2. The battery pulse heating durability test method according to claim 1, further comprising: S340, repeating steps S320 to S330 for a preset time; and obtaining an average battery discharge capacity value to obtain the capacity degradation value of the tested battery. [Item 5] A data table generation method, the method being used to reflect the durability of a battery under different pulse heating parameters, providing a plurality of groups of cells to be tested, each group having a plurality of cells; placing each battery to be tested in each group into a temperature chamber; performing pulse heating of the battery to be tested in each group until a pulse heating time reaches a preset pulse duration; and obtaining a stable temperature of the battery to be tested; adjusting the temperature of each temperature chamber to a second temperature value and obtaining a capacity fade value for each battery being tested at the second temperature value; generating the data table according to corresponding pulse heating parameters of each battery being tested and the capacity fade value of each battery being tested; A data table generating method, wherein the corresponding pulse heating parameters of the tested batteries of the same group are the same, while the corresponding pulse heating parameters of the tested batteries of different groups are different, and the pulse heating parameters include a stable temperature of the battery, a state of charge of the battery, a pulse period, a pulse amplitude value, and a pulse duration. [Item 6] A battery pulse heating durability test system, a pulse heating device (100) electrically connected to a battery to be tested and used for performing pulse heating of the battery to be tested under first pulse parameters until a pulse heating time reaches a preset pulse duration, and for obtaining a stable temperature of the battery to be tested; a capacity degradation acquisition device (200) electrically connected to the battery under test and used to acquire a capacity degradation value of the battery under test at the second temperature value after the pulsed heating is stopped when the pulsed heating time reaches the preset pulse duration; a processing device (300) electrically connected to each of the pulse heating device (100) and the capacity fade acquisition device (200), and used to acquire the durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity fade value. [Item 7] The pulse heating device (100), a temperature chamber (110) used for placing the battery to be tested and for providing stable temperature conditions for the battery to be tested; and a pulse heating element (120) electrically connected to the battery to be tested and used to provide a charge-discharge pulse heating cycle under the first pulse parameters until the pulse heating time reaches the preset pulse duration. [Item 8] The pulse heating element (120) a charging unit (121) electrically connected to the battery under test and used to charge the battery under test with a first amplitude value for a second time value; 8. The battery pulse heating durability test system according to item 7, comprising: a discharge unit (122) electrically connected to the battery to be tested and used to discharge the battery to be tested at the first amplitude value in a constant current mode for the second time value, wherein a sum of two second time values is a pulse period value of the pulse heating. [Item 9] The processing device (300) a first acquisition module (310) electrically connected to the charging unit (121) and the discharging unit (122), respectively, and used to acquire a pulse heating time according to the preset pulse duration and the period value; and a first data processing module (320) electrically connected to the first acquisition module (310) and used to acquire the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity degradation value. [Item 10] The capacity reduction acquisition device (200), a first test module (210) electrically connected to the battery to be tested and used for charging in a constant current mode at a second amplitude value to an upper cut-off voltage, then charging in a constant voltage mode until the current in the battery decreases to a third amplitude value, leaving for a fourth time value, and further used for discharging in a constant current mode at the second amplitude value to a lower cut-off voltage, and leaving for the fourth time value; and a second data processing module (220) electrically connected to the first testing module (210) and used to obtain a battery capacity value of the battery being tested multiple times to obtain the capacity degradation value of the battery being tested. [Item 11] The second data processing module (220): a second acquisition unit (221) electrically connected to the first test module (210), used for acquiring battery discharge capacity values of the tested batteries multiple times and calculating an average battery discharge capacity value; and a second processing unit (222) electrically connected to the second acquisition unit (221) and used for acquiring the capacity degradation value of the battery to be tested according to the battery discharge capacity value of the battery to be tested and the preset battery discharge capacity value. [Explanation of symbols]
[0049] Description of reference numbers of main elements in the accompanying drawings Battery Pulse Heating Durability Test System 10 Pulse Heating Device 100 Temperature Chamber 110 Pulse Heating Element 120 Charging unit 121 Discharge unit 122 Capacity drop acquisition device 200 First Test Module 210 Second Data Processing Module 220 Second Acquisition Unit 221 Second Processing Unit 222 Processing device 300 First Acquisition Module 310 First Data Processing Module 320
Claims
1. A battery pulse heating durability test method, comprising: S10. Providing a battery to be tested, placing the battery to be tested in a temperature chamber, and setting the temperature of the temperature chamber to a first temperature value; S20, performing pulse heating of the battery under test under first pulse parameters until the pulse heating time reaches a preset pulse duration, and obtaining a stable temperature; S30, adjusting the temperature of the temperature chamber to a second temperature value and obtaining a capacity fade value of the tested battery at the second temperature value; S40. obtaining a durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity fade value.
2. The step S20 of performing pulse heating of the battery under test under first pulse parameters until the pulse heating time reaches the preset pulse duration and obtaining a stable temperature includes: S210, charging at a first amplitude value in a constant current mode for a second time value; S220, discharging at the first amplitude value in a constant current mode for the second time value, where the sum of two second time values is a pulse period value, and the first pulse parameters include the first amplitude value and the pulse period value; 2. The battery pulse heating durability test method of claim 1, further comprising: S230, repeating steps S210 to S220, and stopping pulse heating when the pulse heating time reaches the preset pulse duration.
3. The step S40 of obtaining the durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity fade value, Obtaining a pulse heating time according to the preset pulse duration and the pulse period value; and obtaining the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity fade value.
4. The step S30 of adjusting the temperature of the temperature chamber to a second temperature value and obtaining the capacity fade value of the battery under test at the second temperature value includes: S310, adjusting the temperature of the temperature chamber to a second temperature value and allowing time for a first time value; S320, discharging the battery under test at a second amplitude value in a constant current mode to a lower cut-off voltage of the battery under test, and leaving the battery under test for a fourth time value; S330, charging the battery under test at the second amplitude value in a constant current mode to an upper cutoff voltage of the battery under test, then charging the battery under test at a constant voltage mode until the current of the battery under test decreases to a third amplitude value, allowing to stand for the fourth time value, and obtaining a current battery discharge capacity value of the battery under test; 2. The battery pulse heating durability testing method of claim 1, further comprising: S340, repeating steps S320 to S330 for a preset time; and obtaining an average battery discharge capacity value to obtain the capacity fade value of the tested battery.
5. A data table generation method is used to reflect the durability of a battery under different pulse heating parameters; providing a plurality of groups of cells to be tested, each group having a plurality of cells; placing each battery to be tested in each group into a temperature chamber; performing pulse heating of the battery to be tested in each group until a pulse heating time reaches a preset pulse duration; and obtaining a stable temperature of the battery to be tested; adjusting the temperature of each temperature chamber to a second temperature value and obtaining a capacity fade value for each battery being tested at the second temperature value; generating a data table according to the corresponding pulse heating parameters of each battery being tested and the capacity fade value of each battery being tested; A data table generating method, wherein the corresponding pulse heating parameters of the tested batteries of the same group are the same, while the corresponding pulse heating parameters of the tested batteries of different groups are different, and the pulse heating parameters include a stable temperature of the battery, a state of charge of the battery, a pulse period, a pulse amplitude value, and a pulse duration.
6. A battery pulse heating durability test system, comprising: a pulse heating device (100) electrically connected to a battery to be tested and used for performing pulse heating of the battery to be tested under first pulse parameters until a pulse heating time reaches a preset pulse duration, and for obtaining a stable temperature of the battery to be tested; a capacity fade acquisition device (200) electrically connected to the battery under test and used to acquire a capacity fade value of the battery under test at a second temperature value after the pulse heating is stopped when the pulse heating time reaches the preset pulse duration; a processing device (300) electrically connected to each of the pulse heating device (100) and the capacity fade acquisition device (200), and used to acquire the durability of the tested battery at the stable temperature after pulse heating under the first pulse parameters according to the preset pulse duration and the capacity fade value.
7. The pulse heating device (100) a temperature chamber (110) used for placing the battery to be tested and for providing stable temperature conditions for the battery to be tested; and a pulse heating element (120) electrically connected to the battery to be tested and used to provide a charge-discharge pulse heating cycle under the first pulse parameters until the pulse heating time reaches the preset pulse duration.
8. The pulse heating element (120) a charging unit (121) electrically connected to the battery under test and used to charge the battery under test with a first amplitude value for a second time value; 8. The battery pulse heating durability testing system of claim 7, further comprising: a discharge unit (122) electrically connected to the battery to be tested and used to discharge the battery to be tested at the first amplitude value in a constant current mode for the second time value, wherein a sum of two second time values is a pulse period value of the pulse heating.
9. The processing device (300) a first acquisition module (310) electrically connected to the charging unit (121) and the discharging unit (122), respectively, and used to acquire a pulse heating time according to the preset pulse duration and pulse period value; and a first data processing module (320) electrically connected to the first acquisition module (310) and used to acquire the durability of the tested battery after pulse heating under the first pulse parameters according to the pulse heating time and the capacity fade value.
10. The capacity reduction acquisition device (200), a first test module (210) electrically connected to the battery to be tested, used for charging in a constant current mode at a second amplitude value to an upper cut-off voltage, then charging in a constant voltage mode until the current in the battery decreases to a third amplitude value, leaving for a fourth time value, and further used for discharging in a constant current mode at the second amplitude value to a lower cut-off voltage, and leaving for the fourth time value; and a second data processing module (220) electrically connected to the first testing module (210) and used to obtain a battery capacity value of the tested battery a plurality of times to obtain the capacity degradation value of the tested battery.
11. The second data processing module (220): a second acquisition unit (221) electrically connected to the first test module (210), used for acquiring battery discharge capacity values of the tested batteries multiple times and calculating an average battery discharge capacity value; and a second processing unit (222) electrically connected to the second acquisition unit (221) and used for acquiring the capacity degradation value of the tested battery according to the battery discharge capacity value of the tested battery and the preset battery discharge capacity value.
Citation Information
Patent Citations
Battery pack, and integrating method for use period of the same
JP2011233244A
Battery control system
JP2015070753A
Deterioration factor estimation method and remaining life estimation method
JP2016045149A
Device and method for estimating economy of storage battery
JP2019105565A
Method of charging battery and battery charging control system
US20120025773A1