Method for producing release oil composition
A mold release oil and fat composition is produced by refining crude oil without deoxidation, using degumming, decolorization, and deodorization, addressing the need for additive-free products and improving food release and manufacturing efficiency.
Patent Information
- Application Number
- JP2021536966
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-07-30
- Filing Date
- 2020-07-20
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-07-20
AI Technical Summary
Existing mold release oils and fats often contain synthetic additives like emulsifiers and lecithin, which can impart unpleasant tastes and odors, and there is a growing demand for additive-free food products due to health consciousness, while existing technologies do not effectively address mold release during cooking and noodle peeling without these additives.
A method for producing a mold release oil and fat composition by omitting the deoxidation step in the refining process of crude oil, followed by degumming, decolorization, and deodorization, using oils from soybean, rapeseed, or palm pulp, to achieve excellent mold release effects without additives.
The method results in a mold release oil and fat composition that effectively prevents food adhesion to cooking utensils, improves noodle peeling, and enhances workability in food manufacturing, reducing labor and time required during production.
Smart Images

Figure 0007595399000001 
Figure 0007595399000002 
Figure 0007595399000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a release oil composition. [Background technology]
[0002] Conventionally, release oils have been used for the purpose of preventing food ingredients from adhering to cooking utensils, baking molds, baking trays, etc. Another aspect of release oils is to improve the peeling of boiled noodles from buckets or net conveyors and the loosening of noodle strings. As release oils, synthetic additives such as emulsifiers (Patent Document 1) and edible fats and oils to which lecithin, a natural additive, has been added (Patent Document 2) are generally used. However, due to the recent increase in health consciousness, there is an increasing need for additive-free products, not only for release oils but also for food in general. Furthermore, depending on the amount of emulsifiers and lecithin added, they may have an undesirable, unique, unpleasant taste or odor.
[0003] Furthermore, the following prior art uses intermediate oils and fats obtained by subjecting the refining process to specific conditions: Patent Document 3 claims that adding compressed oil and / or extracted oil, or degummed oil to refined edible oils and fats can suppress coloring and cooked odors that occur when an oil and fat composition for deep frying is heated for a long period of time.
[0004] However, the invention of Patent Document 3 relates to the heat resistance of an oil composition containing intermediate oils and fats for deep-frying, and does not disclose or suggest the release effect of the intermediate oils and fats. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 7-170910 [Patent Document 2] JP 2007-306840 A [Patent Document 3] JP 2009-050234 A Summary of the Invention [Problem to be solved by the invention]
[0006] An object of the present invention is to provide a method for producing a mold release oil composition having excellent mold release effect. [Means for solving the problem]
[0007] Therefore, the inventors conducted extensive research and discovered that an oil and fat composition containing a prepared oil obtained by omitting the deacidification process in the refining process of crude oil obtained from oil-based raw materials and going through a specified refining process has a release effect, thereby completing the present invention.
[0008] That is, according to the present invention, there are provided a method for producing an oil-and-fat composition for release, a method for producing a food product using the oil-and-fat composition for release, and a method for improving workability during the production of a food product using the oil-and-fat composition for release. [1] A method for producing an oil composition for release containing 0.5% by mass or more and 100% by mass or less of the following preparation oil, The prepared oil is obtained by omitting the deacidification step in the refining process of crude oil obtained from an oil feedstock, and by (1) degumming process, (2) a bleaching step that may or may not have been performed; and (3) Deodorization process The method for producing the release oil composition, [2] The method for producing an oil composition for release according to the above item [1], wherein the phosphorus content of the prepared oil is 30 ppm by mass or more and 300 ppm by mass or less. [3] The method for producing an oil composition for release according to the above [1] or [2], wherein the phosphatidylcholine content of the prepared oil is 0 ppm by mass or more and 5 ppm by mass or less. [4] The method for producing the release oil composition according to any one of [1] to [3] above, characterized in that the absorbance difference, obtained by subtracting the absorbance at a wavelength of 750 nm from the absorbance at a wavelength of 660 nm using isooctane as a control, after the step (2) of the prepared oil is 0.005 or more and 1.5 or less. [5] The method for producing an oil composition for release according to any one of [1] to [4], wherein the oil raw material is at least one selected from soybeans, rapeseed, and palm pulp. [6] A method for producing a food product, comprising using the release oil composition obtained by the method for producing a release oil composition according to any one of [1] to [5] as a release agent for the food product. [7] The method for producing a food product described in [6] above, wherein the food product is rice, noodles, omelette or bread. [8] A method for improving workability in food production, comprising using the oil-and-fat composition for release obtained by the production method described in any one of [1] to [5] as a release agent for food.
[0009] Any combination of these configurations and conversion of the present invention between methods, devices, etc. are also valid aspects of the present invention. Effect of the Invention
[0010] According to the method for producing a release oil composition of the present invention, a release oil composition having an excellent release effect can be obtained.
[0011] In addition, when producing food products, the oil and fat composition for release obtained by the production method of the present invention is used as a release agent for food products to improve workability, which can reduce the labor and time required for food production, thereby improving workability. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Specific embodiments of the method for producing the release oil composition of the present invention, the method for producing a food product using the release oil composition, and the method for improving workability using the release oil composition will be described below.
[0013] Here, the oil and fat composition for release of the present invention is an oil and fat composition used as a food release agent for the purpose of preventing adhesion between food materials and cooking utensils such as frying pans, iron plates, baking trays, and baking molds during cooking, and for the purpose of preventing adhesion between foods and cooking utensils such as trays and packaging containers during cooking other than cooking. Another aspect of the oil and fat composition for release of the present invention is to improve the peeling of boiled noodles from buckets and net conveyers, the loosening properties of noodles, and the like.
[0014] [1. Release oil composition] The oil and fat composition for release of the present invention contains the following prepared oils in an amount of 0.5% by mass or more and 100% by mass or less. The prepared oils are prepared by omitting the deacidification step in the refining process of crude oil obtained from an oil-based raw material, and are, in order: (1) degumming process, (2) a bleaching step that may or may not have been performed; and (3) Deodorization process The prepared oil will be described in more detail below.
[0015] [1-1. Prepared oil] Examples of oil feedstocks for crude oil when producing prepared oils include soybeans, rapeseed, palm pulp, corn, olives, sesame, safflower, sunflower, cottonseed, rice, peanuts, palm kernels, coconut, linseed, etc. The oil feedstock is preferably one or more selected from soybeans, rapeseed, and palm pulp, more preferably one or two selected from rapeseed and soybeans, and even more preferably rapeseed.
[0016] The crude oil is obtained by subjecting the oil feedstock to compression extraction and / or solvent extraction. Compression extraction is performed by applying high pressure to the oil feedstock to squeeze out the oil in the cells. Compression extraction is suitable for oil feedstocks with a relatively high oil content, such as sesame. Solvent extraction is performed by contacting the residue after compression or compression extraction of the oil feedstock with a solvent, extracting the oil as a solvent solution, and distilling off the solvent from the resulting solution to obtain the oil. Solvent extraction is suitable for oil feedstocks with a low oil content, such as soybeans. An organic solvent, such as hexane, is used as the solvent.
[0017] The degumming step (1) is a step of hydrating and removing gums, the main component of which is phospholipids, contained in the oil. Specifically, steam or water is added to the crude oil and stirred, the gums are hydrated and transferred to the water layer, and the water layer is then separated and removed to obtain the degummed oil. It is essential that the prepared oil in this embodiment undergoes a degumming step. The processing conditions for the degumming step for the prepared oil can be the same as those used in the manufacturing process for general refined oils and fats, but it is preferable to employ processing conditions that satisfy, for example, the following (i) to (iv). (i) Amount of water used: 1% by mass or more and 5% by mass or less, preferably 1.5% by mass or more and 3% by mass or less, based on the crude oil (ii) Degumming aid: This can be used as necessary, and is preferably an aqueous solution of one or more acids selected from oxalic acid, citric acid, and phosphoric acid. (iii) Degumming temperature: 30°C to 95°C, preferably 35°C to 60°C (iv) Stirring time: preferably more than 0 seconds and not exceeding 60 minutes. When a line mixer is used, preferably from 1 to 10 seconds. When stirring in a tank, preferably from 10 to 60 minutes.
[0018] The decolorization step (2) is a step of removing the pigment contained in the oil by adsorbing it to activated clay, activated carbon, or the like under reduced pressure. Specifically, the degummed oil is contacted with activated clay or activated carbon, and then the activated clay or activated carbon adsorbing the pigment is removed by vacuum filtration or the like to obtain a decolorized oil. The prepared oil in this embodiment may or may not be subjected to a decolorization step, but it is preferable to perform the decolorization step. When the decolorization step is performed, the treatment conditions for the decolorization step for the prepared oil can be the conditions used in the manufacturing process of general refined oils and fats, but it is preferable to adopt treatment conditions that satisfy, for example, the following (v) to (vii). (v) Amount of activated clay used: 0.05% by mass or more and 5% by mass or less, preferably 0.05% by mass or more and 4% by mass or less, more preferably 0.05% by mass or more and 3% by mass or less, and even more preferably 0.1% by mass or more and 2.5% by mass or less, based on the degummed oil. (vi) Bleaching temperature: 60° C. or higher and 120° C. or lower, preferably 65° C. or higher and 120° C. or lower, more preferably 70° C. or higher and 115° C. or lower, and even more preferably 70° C. or higher and 110° C. or lower (vii) Bleaching time: 5 minutes or more and 120 minutes or less, preferably 5 minutes or more and 80 minutes or less, more preferably 5 minutes or more and 60 minutes or less, and even more preferably 10 minutes or more and 50 minutes or less.
[0019] The deodorizing step (3) is a step of removing odorous components contained in the oil by steam distillation under reduced pressure. Specifically, steam is blown into the bleached oil under reduced pressure to remove odorous components and obtain a deodorized oil. It is essential that the prepared oil in this embodiment undergoes a deodorizing step. The processing conditions for the deodorizing step for the prepared oil can be the same as those used in the manufacturing process of general refined oils and fats, but it is preferable to adopt processing conditions that satisfy, for example, the following (viii) to (xi). (viii) Amount of water vapor used: 0.1% by mass or more and 10% by mass or less, preferably 0.3% by mass or more and 8% by mass or less, more preferably 0.3% by mass or more and 5% by mass or less, based on the bleached oil. (ix) Deodorization temperature: 180°C or higher and 300°C or lower, preferably 190°C or higher and 300°C or lower, more preferably 200°C or higher and 300°C or lower, even more preferably 220°C or higher and 290°C or lower, and even more preferably 240°C or higher and 280°C or lower (x) Deodorization time: 10 minutes or more and 240 minutes or less, preferably 20 minutes or more and 240 minutes or less, more preferably 50 minutes or more and 240 minutes or less (xi) Degree of reduced pressure: 150 Pa or more and 1000 Pa or less, preferably 200 Pa or more and 800 Pa or less In addition, when the decolorization step is not carried out, the decolorized oil is read as degummed oil.
[0020] The prepared oil in this embodiment is characterized in that it does not require a deacidification step, which is a step in which the oil is treated with an aqueous solution of an alkali such as sodium carbonate or caustic soda to remove free fatty acids contained in the oil as soap components.
[0021] In this embodiment, the refinement process for the prepared oil is carried out in the following order: a degumming process, a bleaching process which may or may not be carried out, and a deodorization process.
[0022] The phosphorus content in the prepared oil is preferably 30 ppm by mass or more and 300 ppm by mass or less, more preferably 50 ppm by mass or more and 250 ppm by mass or less, even more preferably 70 ppm by mass or more and 250 ppm by mass or less, and even more preferably 100 ppm by mass or more and 220 ppm by mass or less.
[0023] From the viewpoint of enhancing releasability, the phosphatidylcholine (PC) in the prepared oil is preferably 0 mass ppm or more and 5 mass ppm or less, more preferably 0 mass ppm or more and 3 mass ppm or less, even more preferably 0 mass ppm or more and 2 mass ppm or less, and even more preferably 0 mass ppm or more and 1 mass ppm or less. In addition, the phosphatidylethanolamine (PE) in the prepared oil is preferably 0 mass ppm or more and 1 mass ppm or less, and the phosphatidylinositol (PI) in the prepared oil is preferably 0 mass ppm or more and 1 mass ppm or less. Here, phosphatidylcholine, phosphatidylethanolamine, and phosphatidylinositol are all phospholipids and are major components of animal and vegetable lecithin.
[0024] After the process (2) of the prepared oil, the absorbance difference (hereinafter also simply referred to as the absorbance difference) obtained by subtracting the absorbance at a wavelength of 750 nm from the absorbance at a wavelength of 660 nm using isooctane as a control is preferably 0.005 or more, more preferably 0.020 or more, even more preferably 0.025 or more, and even more preferably 0.030 or more, from the viewpoint of improving releasability. From the same viewpoint, the upper limit of the absorbance difference is preferably 1.5 or less, more preferably 1.3 or less, even more preferably 1.0 or less, and even more preferably 0.5 or less. In addition, when the process (2) is not performed, the above "process (2)" is read as "process (1)".
[0025] Here, a method for determining the absorbance difference will be described. First, isooctane (a spectroscopic reagent, manufactured by Wako Pure Chemical Industries, Ltd.) is placed in a control and measurement quartz cell (1 cm), and baseline correction is performed in the range of 600 to 750 nm using an ultraviolet-visible spectrophotometer (product name: SHIMADZU UV-2450, manufactured by Shimadzu Corporation). Next, a sample is placed in the measurement quartz cell and the absorbance is measured. The absorbance at 660 nm when the absorbance at 750 nm is set to zero is obtained as the absorbance difference.
[0026] [1-2. Edible oils and fats] The release oil composition can contain edible oils other than the prepared oil. The edible oils referred to here are those that have been subjected to a degumming process, a deacidification process, a decolorization process, and a deodorization process for crude oil obtained from an oil-based raw material. The refining method and refining conditions of each refining process are not particularly limited, and generally used methods and conditions can be applied.
[0027] Examples of edible fats and oils include vegetable fats and oils such as soybean oil, rapeseed oil, palm oil, palm kernel oil, corn oil, sunflower oil, olive oil, cottonseed oil, safflower oil, linseed oil, sesame oil, rice oil, peanut oil, coconut oil, etc., animal fats and oils such as lard, beef tallow, chicken fat, milk fat, medium-chain fatty acid triglycerides, and processed fats and oils obtained by fractionation, hydrogenation, transesterification, etc., of these edible fats and oils may be used alone or in combination of two or more. The edible fats and oils are preferably at least one selected from soybean oil, rapeseed oil, palm-based fats and oils, corn oil, sunflower oil, olive oil, cottonseed oil, rice oil, and safflower oil, and more preferably at least one selected from soybean oil, rapeseed oil, and palm-based fats and oils. The edible fats and oils preferably contain soybean oil, rapeseed oil, palm-based fats and oils, corn oil, sunflower oil, olive oil, cottonseed oil, rice oil and safflower oil in a total content of 60% by mass or more and 100% by mass or less, more preferably 75% by mass or more and 100% by mass or less, even more preferably 90% by mass or more and 100% by mass or less, and particularly preferably 100% by mass. The palm-based fats and oils referred to here mean palm oil and processed palm oil.
[0028] The melting point of the edible oil or fat is preferably 10° C. or lower, more preferably 0° C. or lower. In this specification, the melting point means the slip melting point. The slip melting point can be measured in accordance with the Standard Method for Analysis of Fats, Oils and Related Materials 2.2.4.2-1996.
[0029] The oil and fat composition for mold release of the present invention suppresses adhesion between food and cooking utensils, containers, etc., and improves peeling. Examples of such effects include suppressing adhesion between food ingredients and frying pans, iron plates, etc., during heat cooking such as stir-frying, and removing breads and baked goods from baking molds after heat cooking. On the other hand, the oil and fat composition for mold release of the present invention can also suppress undesirable adhesion between foods. An example of such a case is the use of the composition for loosening noodle strings after cooking noodles.
[0030] When used for stir-frying, the content of the prepared oil in the release oil composition of the present invention is 0.5% by mass or more and 100% by mass or less, preferably 3% by mass or more and 90% by mass or less, more preferably 5% by mass or more and 80% by mass or less, even more preferably 8% by mass or more and 60% by mass or less, and even more preferably 10% by mass or more and 55% by mass or less.
[0031] When used for the purpose of removing breads or baked goods from baking molds, the content of the modified oil in the oil composition for release of the present invention is 0.5% by mass or more and 100% by mass or less, preferably 1% by mass or more and 60% by mass or less, more preferably 1.5% by mass or more and 30% by mass or less, even more preferably 1.5% by mass or more and 15% by mass or less, and even more preferably 4% by mass or more and 13% by mass or less.
[0032] In addition, when used for loosening noodles, the content of the prepared oil in the oil and fat composition for release of the present invention is 0.5% by mass or more and 100% by mass or less, preferably 10% by mass or more and 90% by mass or less, more preferably 20% by mass or more and 80% by mass or less, even more preferably 35% by mass or more and 65% by mass or less, and even more preferably 40% by mass or more and 60% by mass or less.
[0033] When the oil-and-fat composition for release of the present invention contains an edible oil-and-fat, the total amount of the edible oil-and-fat and the prepared oil in the oil-and-fat composition for release is preferably 80% by mass or more and 100% by mass or less, more preferably 85% by mass or more and 100% by mass or less, and even more preferably 90% by mass or more and 100% by mass or less.
[0034] The oil and fat composition for release of the present invention may contain, in addition to the edible oil and fat and the prepared oil, for example, silicone, antioxidant, fragrance, colorant, etc., within the range that does not impair the effects of the present invention. In addition, although the oil and fat composition for release of the present invention has a mold-releasing effect even without using an emulsifier, an emulsifier may be used in combination as necessary.
[0035] The food in which the release oil composition of the present invention is used is not particularly limited. Examples of the food in which the release oil composition is used include (1) cooked rice such as fried rice, rice with sauce, ketchup rice, etc., (2) noodles such as yakisoba and pasta, (3) stir-fried and baked dishes using meat, vegetables, seafood, and eggs, (4) flour-based foods such as takoyaki and okonomiyaki, (5) breads such as bread and koppepan, and baked goods such as sponge cake, pound cake, and cookies, and (3) includes hamburger steak, gyoza, and tamagoyaki. The food in which the release oil composition is used is preferably cooked rice, noodles, stir-fried and baked dishes, and breads, and more preferably cooked rice, noodles, tamagoyaki, and breads. Here, the release oil composition can be used for removing breads and baked goods from the baking mold during baking, and for loosening the noodle strings in noodles such as yakisoba and pasta.
[0036] By using the release oil composition of the present invention as described above, an excellent release effect can be obtained even without adding an emulsifier.
[0037] [2. Food manufacturing methods] In the food manufacturing method of the present invention, when preventing adhesion between food and cooking utensils or containers, it is important to apply a release oil composition containing a predetermined amount of the prepared oil as a food release agent to either or both of the surface of the cooking utensil or container and the surface of the food. When preventing undesirable adhesion between food products, it is preferable to apply the oil composition to the entire food product, as in the case of noodle loosening oil. The explanation of the prepared oil and food product is omitted here, as it is the same as that described in [1. Release oil composition] above.
[0038] In the method for producing food of the present invention, the method for attaching the oil and fat composition for release to the surface of a cooking utensil or a container, or to the surface of a food, is not particularly limited, and can be appropriately selected from, for example, dropping, spraying, immersion, coating, etc. When the release oil-and-fat composition is used to suppress adhesion between food and cooking utensils or containers, for example, when used for stir-fry or bread, it is preferable to apply the release oil-and-fat composition to cooking utensils or containers, since it is possible to use the release oil-and-fat composition repeatedly by applying it once. Also, when preventing adhesion between foods, for example, when used to loosen noodles, it is preferable to apply the release oil-and-fat composition to the surface of the food. When the oil and fat composition for release is applied to the surfaces of cooking utensils or containers and to the surfaces of foods, it may be applied entirely or partially to these surfaces. From the viewpoint of more effectively exerting the release effect, it is preferable to apply it to the entire surfaces where the food comes into contact with the cooking utensil or container, or the entire surfaces where the food comes into contact with each other.
[0039] The amount of the release oil composition applied to food, cooking utensils, containers, etc. may be adjusted depending on the application. For example, in the case of stir-frying, the amount of the release oil composition applied to the bottom of a frying pan or a 100 cm iron plate may be adjusted depending on the application. 2 The amount of the oil and fat composition for release is preferably 0.02 g or more and 5 g or less, more preferably 0.05 g or more and 3 g or less, and even more preferably 0.1 g or more and 2 g or less, per 100 cm2 of the inner area of the baking mold. 2The amount is preferably 0.02 g or more and 5 g or less, more preferably 0.04 g or more and 2 g or less, and even more preferably 0.09 g or more and 1.5 g or less. Furthermore, when preventing food from sticking to itself, for example when used to loosen noodles, the amount of the oil and fat composition for release to be applied is 0.3 g or more and 6 g or less, preferably 0.5 g or more and 4 g or less, more preferably 0.8 g or more and 3 g or less per 100 g of food.
[0040] In the food manufacturing method of the present invention, when the adhesion between food and cooking utensils, containers, etc. is suppressed, the cooking utensils, containers, etc. to which the release oil composition is applied are not particularly limited, but examples of cooking utensils include frying pans, iron plates, baking sheets, bread molds, etc. In addition, it can also be applied to continuous baking machines using conveyers. Examples of containers include trays, packaging containers, storage containers, etc. The cooking utensils, containers, etc. to which the release oil composition of the present invention is applied are preferably cooking utensils, and more preferably frying pans, iron plates, baking sheets, bread molds.
[0041] In the food manufacturing method of the present invention, the timing of applying the release oil and fat composition to the surface of cooking utensils or containers and the surface of food is not particularly limited, but in the case of use for the purpose of suppressing adhesion between food and cooking utensils or containers, for example, in the case of stir-fried foods or bread, it is preferable to apply the release oil and fat composition before cooking. However, after applying the release oil and fat composition to cooking utensils once, it is not necessarily required to apply it every time cooking while the effect is still maintained. Furthermore, when used for the purpose of preventing or inhibiting adhesion between foods, for example when using it to loosen noodles, it is preferable to allow the adhesion to occur after boiling or steaming.
[0042] [3. Methods for improving workability] The method for improving workability of the present invention is characterized by using a release oil composition containing a predetermined amount of the prepared oil when producing food. The prepared oil and the type of food are the same as those described above in [1. Release oil composition], and the method and timing of application to food and cooking utensils are the same as those described above in [2. Food production method], so they are omitted here.
[0043] In the present invention, specific examples of workability include suppression of adhesion of food to cooking utensils during stir-frying; ease of removing food such as bread from baking molds; reduction in the number of times the release oil is applied (the release oil composition can be repeatedly used after being applied once to cooking utensils or containers); and improvement of the loosening property by adhering to food.
[0044] In the method for improving workability of the present invention, the release property is improved by using the oil and fat composition for release as a release agent for food, and therefore, loss or burning of food due to sticking to cooking utensils or containers during food production can be suppressed, and the time required for post-processing can be shortened, improving workability. For example, in the case of bread, loss due to food sticking to the mold can be suppressed, and further, the food can be quickly released from the mold, so that the work time can be shortened. EXAMPLES
[0045] The present invention will be described in more detail below by showing examples of the present invention, but the present invention is not limited to the following examples. [Preparation Example 1 of Prepared Oil] A prepared oil was prepared using rapeseed crude oil according to the refining process shown in Table 1. The detailed conditions for the degumming, bleaching and deodorizing processes are as follows. However, the bleaching and deodorizing processes were carried out under two different conditions: normal conditions and mild conditions. In addition, the refined rapeseed oil used was a commercially available product that had undergone a normal refining process (product name: smooth canola oil, manufactured by J-Oil Mills Co., Ltd., with a melting point of 0°C or less). (Degumming process conditions) Amount of water used: 2% by mass based on crude oil Degumming aid: None added Degumming temperature: 40℃ Mixing time: 3 seconds (Decolorization process conditions) 1. Normal conditions Amount of activated clay used: 2% by weight based on degummed oil Decolorization temperature: 100℃ Bleaching time: 20 minutes 2. Mild conditions Amount of activated clay used: 0.3% by weight based on degummed oil Decolorization temperature: 100℃ Bleaching time: 20 minutes (Deodorization process conditions) 1. Normal conditions Amount of steam used: 4% by mass of bleached oil (degummed oil if not bleached) Deodorization temperature: 255℃ Deodorization time: 120 minutes Degree of vacuum: 4 Torr (533 Pa) 2. Mild conditions Amount of steam used: 2% by mass of bleached oil (degummed oil if not bleached) Deodorization temperature: 200℃ Deodorization time: 45 minutes Degree of vacuum: 4 Torr (533 Pa)
[0046] [Table 1]
[0047] [Preparation Example 2 of Prepared Oil] The degummed soybean oil was not subjected to a deacidification step, but was subjected to a decolorization step and a deodorization step under normal refining conditions to obtain prepared oil 4 (phosphorus content: 198 ppm by mass, no PE, PC or PI was detected).
[0048] The absorbance, phosphorus content, and phospholipids of the above refined rapeseed oil and prepared oil were measured by the following methods. The results are shown in Table 1.
[0049] (absorbance difference) Isooctane (spectroscopic reagent, manufactured by Wako Pure Chemical Industries, Ltd.) was placed in a control quartz cell (1 cm) and a measurement quartz cell (1 cm), and baseline correction was performed in the range of 600 to 750 nm using an ultraviolet-visible spectrophotometer (product name "SHIMAZU UV-2450", manufactured by Shimadzu Corporation). Next, the oil to be measured was placed in the measurement quartz cell and the absorbance was measured. The absorbance at 660 nm was recorded when the absorbance at 750 nm was set to zero, and this was used as the absorbance difference obtained by subtracting the absorbance at a wavelength of 750 nm from the absorbance at a wavelength of 660 nm using isooctane as a control.
[0050] (phosphorus content) The oil to be measured was diluted with xylene and analyzed using an ICP emission spectrometer (Hitachi High-Tech Science Corp.). For quantification, CONOSTAN (registered trademark) Oil Analysis Standard (SCP Science) was used.
[0051] (Phospholipids) Each test oil was diluted with chloroform:methanol = 2:1 and analyzed under the following conditions. Equipment: HPLC (product name: manufactured by Thermo SCIENTIFIC) Detector: Charged particle detector Corona Veo Mobile phase: A n-hexane:2-propanol:acetic acid:triethylamine = 814.2:170:15:0.8 (volume ratio) B 2-propanol:water:acetic acid:triethylamine = 844.2:140:15:0.8 (volume ratio) Column: LiChrospher 100 Diol (5 μm) inner diameter 4.0 × 125 mm [Merck] Column temperature: 55℃ Sample temperature: 20℃ Gradient (flow rate = 1 ml / min) *Linear gradient (see Table 2)
[0052] [Table 2]
[0053] The standard was prepared by appropriately mixing crude lecithin (product name: Lecithin CL, manufactured by J-Oil Mills, Inc.) and PA lecithin (product name: Benecoat, manufactured by Kao Corporation), and the phospholipids were quantified at the Japan Food Research Center. This was used as the true value for the standard.
[0054] Example 1 In this example, rice with sauce was cooked and the releasability of the food from the frying pan was tested.
[0055] (How to make sauce rice) 1. A mixture was prepared by mixing 60 g of rice (product name: Sato no Gohan, manufactured by Sato Foods Co., Ltd.) that had been heated in a microwave oven for 2 minutes with 6 g of sauce (Bull-Dog Chuno Sauce, manufactured by Bull-Dog Co., Ltd.). 2. 1.5 g of each test oil or control oil with the composition shown in Table 3 was placed in a stainless steel frying pan (diameter 22 cm), the oil was spread evenly, and the pan was heated in an induction cooker (product name: National KZ-PH8) on high heat until the center reached 200°C. 3. Add the mixture prepared in step 1 above to the frying pan in step 2 above and spread it over the surface of the frying pan for 1 minute and 30 seconds. 4. One minute and 30 seconds after adding the mixture, the heating was stopped and sauced rice was obtained.
[0056] (Mold release and sensory evaluation) Immediately after heating, the frying pan was turned over, the unburned sauced rice was removed, and the mass of the rice on the surface was measured. In addition, two panelists evaluated the odor rising from the frying pan during cooking and the flavor of the resulting sauced rice. The results are shown in Table 3.
[0057] [Table 3]
[0058] From the above results, all of the examples using Test Oil 1 to Test Oil 5, which are the release oil compositions of the present invention, showed excellent release effects and good workability. Comparing Examples 1-1 to 1-3 using test oils 1 to 3, when the phosphorus content in the prepared oil was 133 mass ppm or more and 198 mass ppm or less, the release property was good with less burning. In addition, when the absorbance difference was 0.033 to 1.314 or less, the release property was good, and when it was 0.033 to 0.173 or less, it was even better. In addition, in Examples 1-1, 1-2, 1-4, and 1-5 in which the content of PC (phosphatidylcholine) in the prepared oil was less than 1.4 mass ppm, the release property was better in terms of less burning. With respect to the odor during cooking compared to the control example, in Example 1-3, test oil 3 had a faint grassy odor, but in Examples 1-1 and 1-2, test oils 1 and 2 had almost no noticeable odor. Furthermore, when test oils 4 and 5 in Examples 1-4 to 1-5 contained 20% by mass or more and 40% by mass or less of prepared oil 2, the odor was not noticeable at all. In addition, when each sauce-based rice was eaten and evaluated, the sauce-based rice in Control Example 1, cooked with Control Oil 1, had a weaker flavor, while the sauce-based rice in Example 1-2, cooked with Test Oil 2, was preferable in that the aroma of the sauce was better.
[0059] Example 2 In this example, a thin omelet (tamagoyaki) was cooked and the releasability of the food from the frying pan was tested.
[0060] (Production and evaluation of thin egg omelet) 1. Beat 10 eggs in a bowl to prepare beaten eggs. 2. 1.5 g of each test oil or control oil (product name: Rich and Umami Soybean Oil, manufactured by J-Oil Mills, Inc., with a melting point of 0°C or less) having the composition shown in Table 7 was placed into a stainless steel frying pan (diameter 22 cm), the oil was spread evenly, and the pan was heated in an induction cooker at high heat until the center reached 200°C. 3. 25 g of the beaten egg prepared in step 1 above was added to the frying pan and spread so as to cover the surface of the frying pan. 4. 20 seconds after adding the beaten eggs, the cooking was stopped and when the edges of the eggs had dried, the thin egg was removed from the frying pan. 5. Without adding any test oil, steps 2 to 4 above were repeated a maximum of 10 times to determine how many thin omelets were cooked before the frying pan started to burn. The results are shown in Table 4.
[0061] [Table 4]
[0062] From the above results, test oil 2 and test oil 6, which are the release oil compositions of the present invention, showed excellent releasability and good workability in cooking omelet. Surprisingly, when Control Oil 2 and Test Oil 2 were used alone in Control Example 2 and Example 2-1, respectively, burning occurred, but in Example 2-2, which used Test Oil 6, a 50:50 mixture of Control Oil 2 and Test Oil 2, no burning occurred even on the tenth omelet, demonstrating excellent release properties. Considering the results of Example 2-1 using the test oil 2 and Example 2-2 using the test oil 6, from the viewpoint of releasability, the content of the preparation oil in the release oil composition is good when it is 50% by mass or more and 100% by mass or less, and is even better when it is 50% by mass.
[0063] Example 3 In this example, bread dough was placed in a baking mold that had been coated with each test oil in advance, and after baking, the release properties of the bread were tested. (raw materials) In this example, the following raw materials were mainly used: (powder raw material) Strong flour: Product name "Eagle", manufactured by Nippon Flour Mills Co., Ltd. Powdered reduced maltose syrup: Product name: "Amalty", Mitsubishi Corporation Foodtech Co., Ltd. Bread improver: Product name: "Max Power", manufactured by J-Oil Mills Co., Ltd. Skim milk powder: Product name: "Skim milk powder", manufactured by Hokkaido Dairy Co., Ltd. Sugar: Product name: "White sugar", manufactured by Mitsui Sugar Co., Ltd. (Oil products) Processed oil 1: Product name "Atlanta SS", manufactured by J-Oil Mills Co., Ltd. Processed oils and fats 2: Product name "Meister Mybrot EZ200", manufactured by J-Oil Mills Co., Ltd. (others) Fresh yeast: Product name: "Oriental Yeast FD-1", Form: Paste-like, manufactured by Oriental Yeast Co., Ltd.
[0064] (Preparation of release oil composition and mold) 1. Each test oil was prepared by mixing the components according to the ratio shown in Table 5. However, test oil 9 was prepared by adding crude lecithin (product name: Lecithin CL, manufactured by J-Oil Mills Co., Ltd.) to refined rapeseed oil, mixing, and then heating to 60°C and stirring for 5 minutes. 2. Each test oil prepared in step 1 above was sprayed evenly onto the inside bottom and sides of an aluminum mold (27 cm length x 8 cm width x 4 cm height), then spread with a paper towel, and finally 1.5 g of test oil was applied to each mold.
[0065] [Table 5]
[0066] (How to make white bread) The dough was prepared as follows, according to the formulation shown in Table 6. 1. All ingredients except for fats and oils were placed in a mixer bowl and mixed under the following conditions using a bread mixer (product name: Kanto Mixer HP-20M, manufactured by Kanto Mixer Co., Ltd.). Mixing conditions: After mixing for 3 minutes at 1st speed and 4 minutes at 2nd speed using the hook, the oil was added and the dough was mixed for 1 minute at 3rd speed, then further mixed for 2 minutes at 1st speed, 3 minutes at 2nd speed, and 5 to 9 minutes at 3rd speed. 2. After mixing, the dough was removed from the mixer and allowed to rise at 28°C for 60 minutes. 3. The dough was divided into 50g portions, rolled into balls, and left to rest for 20 minutes, then passed through a molder to form into a loaf of bread. 4. Place the dough formed in step 3 above into the prepared aluminum mold and leave to ferment in a proofer at 38°C and 80% relative humidity for 50 minutes. 5. After fermentation, the dough was baked in an oven under the following conditions and for the following time. Firing conditions: upper 170℃ / lower 170℃ Baking time: 8 minutes 6. The baked bread was evaluated for releasability as follows.
[0067] [Table 6]
[0068] (Releasability evaluation) Two loaves of bread were baked with each test oil, and after allowing them to cool (after about 10 minutes at 25°C), the aluminum molds were turned upside down and the ease of removing the bread was evaluated according to the following criteria. After the first application of each test oil to the aluminum molds, they were used to bake bread a total of 15 times without any application, and the mold releasability was evaluated. The results are shown in Table 7. (standard) ○: Both pieces of bread fall off immediately when turned over. ×: For either of the two pieces, the bread was difficult to remove from the mold when turned over, and it took more than 2 seconds for the bread to fall off.
[0069] [Table 7]
[0070] From the above results, the aluminum molds coated with the release oil compositions of Test Oil 7 (Example 3-1) and Test Oil 8 (Example 3-2), which contain 2% by mass and 10% by mass of Preparation Oil 2, respectively, had good releasability of bread, i.e., good workability. In particular, when the content was 10% by mass, there was no difficulty in peeling even once, and the workability was very good. On the other hand, in Control Example 3 using Control Oil 1 and Comparative Example 3 using Test Oil 9, the bread became difficult to peel from the mold from the 12th baking.
[0071] Example 4 In this example, the loosening property of the oil and fat composition for release of the present invention as a yakisoba loosening oil was tested.
[0072] (Yakisoba sample preparation and evaluation) 1. Fresh Chinese noodles (product name: Hokkaido-Hatsubo Sapporo Nama Ramen, manufactured by Kikusui Co., Ltd.) were boiled in 800 g / 7 kg of boiling water for the time indicated on the product. 2. The boiled noodles obtained in step 1 were cooled under running water, drained in a colander and left to stand for 5 minutes. 3. Measure out 200g of the boiled noodles obtained in step 2 while mixing them up and down, add 1.8% (3.6g) of the test oil to the 200g of boiled noodles, and mix for 1 minute. 4. The boiled noodles obtained in step 3 above were placed in a tightly fitting container with a lid (product name: Tofu Making, size: 10 x 12.3 x 7.2 cm, manufactured by Skater Co., Ltd.) and the lid was placed on it. 5. A weight of 1.5 times the mass of the noodles (300 g) was placed on the lid. 6. Store in a refrigerator at 5℃ for one day.
[0073] (Evaluation of looseness) After storing for one day, the noodles were taken out of the container by turning it upside down, and the noodles that had solidified into a square shape were loosened by moving chopsticks back and forth, and the number of seconds it took for the noodles to loosen was recorded. The results are shown in Table 8.
[0074] [Table 8]
[0075] From the above results, the oil and fat composition for release of the present invention containing 50 mass% of Prepared Oil 2 (Example 4-1) had excellent releasability between noodles compared to Control Example 4 which used Control Oil 2.
[0076] As described above, the release oil composition of the present invention, which contains 2 to 100 mass% of the prepared oil obtained through a specified refining process, can suppress the adhesion of food to cooking utensils such as frying pans and baking molds, and has an excellent release effect. In addition, the oil and fat composition for release of the present invention, which contains 50 mass % of the prepared oil obtained through the specified refining process of the present invention, was excellent in the loosening properties of noodles.
Claims
1. A method for producing an oil-and-fat composition for release, comprising adding 0.5% by mass or more and 100% by mass or less of the following modified oil to edible oils and fats: The prepared oil is obtained by omitting the deacidification step in the refining process of crude oil obtained from an oil feedstock, and by (1) degumming step, (2) a bleaching step that may or may not have been performed; and (3) Deodorization process This is the result of The method for producing the oil composition for release, wherein the prepared oil has a phosphatidylcholine content of 0 ppm by mass or more and 5 ppm by mass or less.
2. 2. The method for producing an oil composition for release according to claim 1, wherein the phosphorus content of the prepared oil is 30 ppm by mass or more and 300 ppm by mass or less.
3. 3. The method for producing a mold release oil composition according to claim 1 or 2, characterized in that the absorbance difference, obtained by subtracting the absorbance at a wavelength of 750 nm from the absorbance at a wavelength of 660 nm using isooctane as a control, of the prepared oil after the step (2) is 0.005 or more and 3 or less.
4. The method for producing an oil composition for release according to any one of claims 1 to 3, wherein the oil raw material is one or more selected from soybean, rapeseed, and palm pulp.
5. A method for producing food, comprising using the oil and fat composition for mold release obtained by the method according to any one of claims 1 to 4 as a mold release agent for food.
6. The method for producing a food product according to claim 5 , wherein the food product is rice, noodles, rolled eggs or bread.
7. A method for improving workability in food production, comprising using the oil and fat composition for mold release obtained by the method according to any one of claims 1 to 4 as a mold release agent in the production of food.
Citation Information
Patent Citations
Mold-releasing oil
JP1995170910A
Lecithin-containing edible oil and its use
JP2000279092A
Functional releasing oil composition, method for producing the composition, and use of the composition
JP2007306840A
Method for producing oil and fat composition for deep-fried food, excellent in heating durability
JP2009050234A
Method of manufacturing fat composition containing lecithin and method of preventing precipitation of lecithin