magnetic sensor

The magnetic sensor design with magnetostatically coupled magnetic layers in a TMR element effectively reduces noise by suppressing domain formation, improving sensitivity and dynamic range.

JP7809275B2Active Publication Date: 2026-02-02ROTARY INDUCTION MFG CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2022033515
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-03-04
Publication Date
2026-02-02
Estimated Expiration
2042-03-04

AI Technical Summary

Technical Problem

Existing magnetic sensors using TMR elements suffer from low-frequency noise due to magnetic domain formation and fluctuations in domain walls, which need to be further reduced.

Method used

A magnetic sensor design with a free layer having multiple magnetic layers and non-magnetic insertion layers, where adjacent magnetic layers are magnetostatically coupled to suppress domain formation, using materials like NiFe, CoFeSiB, Ru, and Ta for enhanced noise reduction.

Benefits of technology

The design effectively suppresses multiple magnetic domains, leading to reduced noise levels in the magnetic sensor, enhancing its performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007809275000001
    Figure 0007809275000001
  • Figure 0007809275000002
    Figure 0007809275000002
  • Figure 0007809275000003
    Figure 0007809275000003
Patent Text Reader

Abstract

To provide a magnetic sensor which can further reduce noise by an element alone.SOLUTION: A magneto-resistance effect element comprises a reference layer 15 whose magnetization direction is fixed, a free layer 13 whose magnetization direction is changeable, and a barrier layer 14 that is disposed between the reference layer 15 and the free layer 13. The free layer 13 includes a first magnetism divided layer 21 which is composed of a non-magnetic substance, and a pair of fragmentation layers 22 which are disposed by being laminated on both sides of the first magnetism divided layer 21. Each of the fragmentation layers 22 includes: two magnetic layers 22a whose magnetization directions are changeable and are parallel to each other; and a second fragmentation layer 22b which is composed of a non-magnetic substance and is disposed between the magnetic layers 22a so that the magnetic layers 22a are magnetostatically coupled. The first magnetism divided layer 21 is provided so that the two magnetic layers 22a disposed on both sides thereof are magnetostatically coupled.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a magnetic sensor. [Background technology]

[0002] Conventionally, as a magnetic sensor using a magnetoresistive effect element, there is an MR sensor (magnetoresistive sensor) that uses the TMR effect of a tunnel magnetoresistive (TMR) element. The sensitivity of a magnetic sensor using a TMR element is TMR ratio / 2H k To increase the sensitivity, it is necessary to improve the TMR ratio and k It is effective to reduce H k is the anisotropy magnetic field of the free layer of the TMR element, and when the TMR element is used as a magnetic sensor, it becomes the dynamic range of the magnetic sensor.

[0003] The present inventors have developed a highly sensitive magnetic sensor using a TMR element (see, for example, Non-Patent Documents 1 and 2). However, in a magnetoresistive element, in order to reduce the magnetostatic energy in the free layer made of a magnetic material, multiple magnetic domains with different magnetization directions are formed in the free layer, and the boundary regions (domain walls) between these magnetic domains fluctuate due to heat, causing noise such as 1 / f noise in the low frequency range.

[0004] Therefore, the present inventors have developed a magnetic sensor capable of reducing noise with a single element, in which the free layer has multiple magnetic layers with variable magnetization directions and one or more insertion layers made of a non-magnetic material, the magnetization directions of some of the magnetic layers being the same direction and the magnetization directions of the remaining magnetic layers being antiparallel to each other, and the magnetic layers and insertion layers are alternately stacked with the insertion layers sandwiched between the magnetic layers so that adjacent magnetic layers are magnetostatically coupled (see, for example, Patent Document 1). In this magnetic sensor, because the magnetic layers are magnetostatically coupled with the insertion layer sandwiched between them, the formation of multiple magnetic domains within each magnetic layer is suppressed, suppressing the generation of low-frequency noise due to magnetic domain formation, and noise can be reduced with a single element. [Prior art documents] [Non-patent literature]

[0005] [Non-Patent Document 1] K. Fujiwara, M. Oogane, S. Yokota, T. Nishikawa, H. Naganuma, and Y. Ando, ​​“Fabrication of magnetic tunnel junctions with a bottom synthetic antiferro-coupled free layers for high sensitive magnetic field sensor device”, J. Appl. Phys., 2012, 111, 07C710. [Non-patent document 2] D. Kato, M. Oogane, K. Fujiwara, T. Nishikawa, H. Naganuma, and Y. Ando, ​​“Fabrication of Magnetic Tunnel Junctions with Amorphous CoFeSiB Ferromagnetic Electrode for Magnetic Field Sensor Devices”, Appl. Phys. Express, 2013, 6, 103004 [Patent documents]

[0006] [Patent Document 1] Patent Publication No. 2021-52050 Summary of the Invention [Problem to be solved by the invention]

[0007] The magnetic sensor described in Patent Document 1 can suppress the formation of multiple magnetic domains inside each magnetic layer and reduce noise, but there is a need for the development of a magnetic sensor with even less noise.

[0008] The present invention has been made in view of these problems, and has an object to provide a magnetic sensor that can further reduce noise in a single element. [Means for solving the problem]

[0009] In order to achieve the above object, the magnetic sensor of the present invention is a magnetic sensor that uses a magnetoresistive effect element, and the magnetoresistive effect element has a reference layer whose magnetization direction is fixed, a free layer whose magnetization direction is changeable, and a barrier layer arranged between the reference layer and the free layer, and the free layer has a first magnetic decoupling layer made of a non-magnetic material and a pair of subdivided layers stacked on both sides of the first magnetic decoupling layer, and each subdivided layer has two magnetic layers whose magnetization direction is changeable and which are antiparallel to each other, and a second magnetic decoupling layer made of a non-magnetic material and arranged between the magnetic layers so that the magnetic layers are magnetostatically coupled, and the first magnetic decoupling layer is arranged so that the two magnetic layers arranged on both sides are magnetostatically coupled.

[0010] In the magnetic sensor according to the present invention, a pair of subdivision layers is disposed on both sides of a first magnetic decoupling layer made of a non-magnetic material, and not only the two magnetic layers sandwiching the first magnetic decoupling layer but also the two magnetic layers sandwiching the second magnetic decoupling layer in each subdivision layer are magnetostatically coupled, which prevents the formation of multiple magnetic domains within each magnetic layer and enables noise reduction within the element itself. In particular, because the subdivision layers are disposed symmetrically on both sides of the first magnetic decoupling layer, noise can be reduced even more effectively.

[0011] The magnetic sensor according to the present invention is not limited to a case in which a pair of subdivided layers is arranged on both sides of the first magnetic splitting layer, but may have multiple pairs of subdivided layers arranged on both sides of the first magnetic splitting layer. In this case, it is preferable that multiple third magnetic splitting layers are arranged between each of the subdivided layers on both sides of the first magnetic splitting layer, and that the third magnetic splitting layer is arranged so that the two magnetic layers arranged on both sides are magnetostatically coupled. As a result, the two magnetic layers sandwiching the third magnetic splitting layer are also magnetostatically coupled, which prevents multiple magnetic domains from forming inside each magnetic layer and reduces noise. Also, in this case, since each subdivided layer is arranged symmetrically on both sides of the first magnetic splitting layer, noise can be reduced even more effectively with just the element itself.

[0012] In the magnetic sensor according to the present invention, the first, second, and third magnetic splitting layers preferably have a thickness of 2 nm or more because the magnetic layers sandwiching them must be magnetostatically coupled, rather than coupled via RKKY interaction. Furthermore, the first, second, and third magnetic splitting layers preferably have a thickness that can split the magnetic order of the magnetic layers sandwiching them. In particular, to more effectively reduce noise, it is preferable that the first magnetic splitting layer reliably splits the magnetic order of the magnetic layers sandwiching it, and the second and third magnetic splitting layers reliably magnetostatically couple the magnetic layers sandwiching them. Therefore, when there is one pair of subdivided layers, it is preferable that the thickness of the first magnetic splitting layer be greater than the thickness of the second magnetic splitting layer. When there are multiple pairs of subdivided layers, it is preferable that the thickness of the first magnetic splitting layer be greater than the thickness of the second and third magnetic splitting layers. The first magnetic decoupling layer preferably has a thickness of 2 nm to 50 nm, and particularly preferably 8 nm or more, in order to magnetostatically couple the magnetic layers sandwiching it while reliably decoupling the magnetic order of the magnetic layers sandwiching it.

[0013] In the magnetic sensor according to the present invention, the magnetic layers of the reference layer, barrier layer, and free layer, as well as the first, second, and third magnetic decoupling layers, are preferably made of materials that increase sensitivity. For example, the magnetic layers of the free layer are preferably made of soft magnetic materials such as NiFe, CoFeSiB, or FeCuNbSiB, the first, second, and third magnetic decoupling layers are preferably made of Ru, Ta, or TaB, and the barrier layer is preferably made of MgO, Mg-Al-O, or AlOx.

[0014] The magnetic sensor according to the present invention is preferably configured so that the sum of the magnetization intensities of the magnetic layers is approximately zero. The magnetic sensor according to the present invention may have one or more magnetoresistive effect elements. When the magnetic sensor has more than one magnetoresistive effect element, the magnetoresistive effect elements may be configured as an array. [Effects of the Invention]

[0015] According to the present invention, it is possible to provide a magnetic sensor that can further reduce noise with a single element. [Brief explanation of the drawings]

[0016] [Figure 1] 1 is a longitudinal sectional view of a magnetic sensor according to an embodiment of the present invention; [Figure 2] 10 is a longitudinal sectional view showing a modified example of the free layer other than the insertion coupling layer and the coupling magnetic layer of the magnetic sensor according to the embodiment of the present invention. FIG. [Figure 3] FIG. 1A is a longitudinal cross-sectional view of a magnetic sensor that is a comparative example (Comparative Example 1) of a magnetic sensor according to an embodiment of the present invention, showing a free layer other than the insertion coupling layer and the coupling magnetic layer; and FIG. 1B is a micrograph showing the magneto-optical Kerr effect on the surface of the coupling magnetic layer in zero magnetic field (the arrows in the figure indicate the expected magnetization direction). [Figure 4] FIG. 10A is a longitudinal cross-sectional view of a magnetic sensor of another comparative example (Comparative Example 2) to the magnetic sensor of the embodiment of the present invention, showing the free layer other than the insertion coupling layer and the coupling magnetic layer, and FIG. 10B is a micrograph showing the magneto-optical Kerr effect on the surface of the coupling magnetic layer in zero magnetic field (the arrows in the figure indicate the expected magnetization direction). [Figure 5](a) A longitudinal cross-section of the free layer excluding the insertion coupling layer and the coupling magnetic layer of the magnetic sensor shown in Figure 1, and (b) a micrograph showing the magneto-optical Kerr effect on the surface of the coupling magnetic layer in zero magnetic field (the arrows in the figure indicate the expected magnetization direction). DETAILED DESCRIPTION OF THE INVENTION

[0017] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. 1 to 5 show a magnetic sensor according to an embodiment of the present invention. As shown in FIG. 1, the magnetic sensor 10 is made up of a magnetoresistive element, and includes a substrate 11 , a buffer layer 12 , a free layer 13 , a barrier layer 14 , a reference layer 15 , and a cap layer 16 .

[0018] The magnetic sensor 10 is formed by stacking a buffer layer 12, a free layer 13, a barrier layer 14, a reference layer 15, and a cap layer 16 in this order on a substrate 11. The substrate 11 is made of a Si wafer or an SOI wafer. The buffer layer 12 is disposed on the substrate 11 to reduce the lattice mismatch between the substrate 11 and the free layer 13. The buffer layer 12 is made of, for example, Ta, Ru, Cr, TaB, etc., or a stacked structure thereof.

[0019] The free layer 13 is disposed on the buffer layer 12 and includes a first magnetic decoupling layer 21 made of a nonmagnetic material, a pair of subdivision layers 22, an insertion coupling layer 23 made of a nonmagnetic material, and a coupling magnetic layer 24. Each subdivision layer 22 is disposed on both sides of the first magnetic decoupling layer 21 and includes two magnetic layers 22a and a second magnetic decoupling layer 22b made of a nonmagnetic material. Each magnetic layer 22a is made of a soft magnetic material and has a variable magnetization direction. The magnetization directions of the two magnetic layers 22a of each subdivision layer 22 are antiparallel to each other and can be changed in a direction parallel to the surface of the layer under the influence of external magnetic flux. Each magnetic layer 22a has a thickness of 20 nm or more and is made of a soft magnetic material such as CoFeSiB amorphous or NiFe. The second magnetic decoupling layer 22b is disposed between the magnetic layers 22a.

[0020] The first magnetic decoupling layer 21 is provided so that two magnetic layers 22a of each of the subdivided layers 22 arranged on both sides of the first magnetic decoupling layer 21 are magnetostatically coupled. The second magnetic decoupling layer 22b is provided so that the magnetic layers 22a on both sides are magnetostatically coupled. The first magnetic decoupling layer 21 and the second magnetic decoupling layer 22b preferably have thicknesses that allow the magnetic layers 22a sandwiching them to not exhibit RKKY interaction and to be magnetostatically coupled. Furthermore, the first magnetic decoupling layer 21 and the second magnetic decoupling layer 22b preferably have thicknesses that allow the magnetic order of the magnetic layers 22a sandwiching them to be decoupled. In particular, it is preferable that the first magnetic decoupling layer 21 reliably decoupling the magnetic order of the two magnetic layers 22a sandwiching it, and that the second magnetic decoupling layer 22b reliably magnetostatically coupling the two magnetic layers 22a sandwiching it. Therefore, the thickness of the first magnetic decoupling layer 21 may be greater than the thickness of the second magnetic decoupling layer 22b.

[0021] The first magnetic decoupling layer 21 and the second magnetic decoupling layer 22b are made of, for example, Ru, Ta, or TaB. The first magnetic decoupling layer 21 and the second magnetic decoupling layer 22b have a thickness of, for example, 2 nm to 50 nm, and it is particularly preferable that the thickness of the first magnetic decoupling layer 21 be 8 nm to 12 nm and the thickness of the second magnetic decoupling layer 22b be 2 nm to 5 nm.

[0022] The insertion coupling layer 23 is disposed on the opposite side of one refinement layer 22 from the first magnetic decoupling layer. The coupling magnetic layer 24 is disposed on the opposite side of the insertion coupling layer 23 from one refinement layer 22. The coupling magnetic layer 24 is made of a ferromagnetic material and is configured so that its magnetization direction can change in a direction parallel to the surface of the layer. The coupling magnetic layer 24 is configured so that its magnetization direction can change following a change in the magnetization direction of the magnetic layer 22a of each magnetic layer 22a of one refinement layer 22 that is closer to the insertion coupling layer 23, so as to maintain a state antiparallel to the magnetization direction of that magnetic layer 22a.

[0023] The insertion coupling layer 23 is made of, for example, Ru or Ta, and has a thickness that allows the magnetization direction of the coupling magnetic layer 24 to change in accordance with the change in the magnetization direction of the magnetic layer 22a on the opposite side of the coupling magnetic layer 24. The thickness of the insertion coupling layer 23 is, for example, 1.5 nm or less. The coupling magnetic layer 24 is made of, for example, CoFeB, and has a thickness that makes its volume sufficiently smaller than the combined volume of the magnetic layers 22a of the free layer 13.

[0024] The free layer 13 is formed on the buffer layer 12 by laminating the other subdivided layer 22, the first magnetic decoupling layer 21, the one subdivided layer 22, the insertion coupling layer 23, and the coupling magnetic layer 24 in this order.

[0025] The barrier layer 14 is made of an insulating material and is disposed on the free layer 13 on the opposite side to the buffer layer 12, that is, on the opposite side of the coupling magnetic layer 24 to the insertion coupling layer 23. The barrier layer 14 is made of, for example, MgO, Mg—Al—O, AlOx, etc., and has a thickness of about 1 nm to 5 nm.

[0026] The reference layer 15 is made of a ferromagnetic material and is disposed on the barrier layer 14 on the opposite side of the free layer 13. The magnetization direction of the reference layer 15 is fixed parallel to the surface of the layer. The magnetization direction of each magnetic layer 22a of the free layer 13 can be changed between a direction perpendicular to the magnetization direction of the reference layer 15 and a perpendicular direction opposite to the magnetization direction of the reference layer 15. The reference layer 15 is made of, for example, CoFeB.

[0027] The cap layer 16 is disposed on the reference layer 15 on the side opposite to the barrier layer 14 in order to fix the magnetization of the reference layer 15. The cap layer 16 is made of an antiferromagnetic material such as IrMn, PtMn, or FeMn. Alternatively, the cap layer 16 may have a structure in which a coupling layer made of Ru or the like is disposed on top of the reference layer 15, a reference magnetic layer made of CoFe or the like is disposed on top of that, and an antiferromagnetic material such as IrMn, PtMn, or FeMn is further disposed on top of that.

[0028] Next, the operation will be described. In the magnetic sensor 10, a pair of subdivision layers 22 are arranged on both sides of a first magnetic decoupling layer 21 made of a non-magnetic material, and not only the two magnetic layers 22a sandwiching the first magnetic decoupling layer 21 but also the two magnetic layers 22a sandwiching the second magnetic decoupling layer 22b in each subdivision layer 22 are magnetostatically coupled, which prevents multiple magnetic domains from forming inside each magnetic layer 22a and enables noise reduction in the element itself. In particular, since the subdivision layers 22 are symmetrically arranged on both sides of the first magnetic decoupling layer 21, noise can be reduced even more effectively.

[0029] As shown in FIG. 2, the magnetic sensor 10 may have a free layer 13 with multiple pairs of refinement layers 22, each stacked in the same number on either side of the first magnetic decoupling layer 21. While FIG. 2 illustrates two pairs of refinement layers 22, the free layer 13 may have three or more pairs of refinement layers 22. In this case, multiple third magnetic decoupling layers 25 are provided between the refinement layers 22 on either side of the first magnetic decoupling layer 21. The third magnetic decoupling layers 25 are magnetostatically coupled to the two magnetic layers 22a of each of the refinement layers 22 on either side of the third magnetic decoupling layer 25. This magnetostatically couples the two magnetic layers 22a sandwiching the third magnetic decoupling layer 25, thereby preventing multiple magnetic domains from forming within each magnetic layer 22a and reducing noise. Furthermore, since the refinement layers 22 are symmetrically arranged on either side of the first magnetic decoupling layer 21, the element itself can more effectively reduce noise.

[0030] In this case, the third magnetic decoupling layer 25 preferably has a thickness that allows the magnetic layers 22a sandwiching it to be magnetostatically coupled without exhibiting RKKY interaction. Furthermore, the third magnetic decoupling layer 25 preferably has a thickness that can reliably decouple the magnetic order of the magnetic layers 22a sandwiching it. Therefore, the thickness of the third magnetic decoupling layer 25 is preferably smaller than that of the first magnetic decoupling layer 21 and approximately the same as that of the second magnetic decoupling layer 22b. The third magnetic decoupling layer 25 is made of, for example, Ru or Ta. The third magnetic decoupling layer 25 preferably has a thickness of, for example, 2 nm to 12 nm, and more preferably 2 nm to 5 nm. [Example]

[0031] The magnetic sensor 10 shown in Fig. 1 (hereinafter referred to as the magnetic sensor 10 of the present invention) was manufactured, and the magneto-optical Kerr effect was observed under a microscope. Furthermore, as comparative examples, the magneto-optical Kerr effect was similarly observed for a case in which the free layer 13 does not have one or more pairs of refinement layers 22, but is composed of only one ferromagnetic layer 31 in addition to the insertion coupling layer 23 and the coupling magnetic layer 24, as shown in Fig. 3(a) (hereinafter referred to as Comparative Example 1), and for a case in which the free layer 13 has a magnetic decoupling layer 32 and a pair of ferromagnetic layers 31 arranged on both sides of it, as shown in Fig. 4(a) (Comparative Example 2).

[0032] First, each layer was deposited on a substrate 11 by magnetron sputtering to manufacture the magnetic sensor 10 of the present invention and the magnetic sensors of Comparative Examples 1 and 2. As shown in FIG. 5(a), the magnetic sensor 10 of the present invention has a first magnetic decoupling layer 21 of the free layer 13 made of a Ru layer with a thickness of 10 nm, a second magnetic decoupling layer 22b of each subdivided layer 22 of the free layer 13 made of a Ru layer with a thickness of 2.5 nm, and a magnetic layer 22a of each subdivided layer 22 made of a Co layer with a thickness of 25 nm. 70.5 Fe 4.5 Si 15 B 10 In Comparative Example 1, as shown in FIG. 3(a), the ferromagnetic layer 31 of the free layer 13 is made of a Co amorphous layer having a thickness of 70 nm. 70.5 Fe 4.5 Si 15 B 10 In Comparative Example 2, as shown in FIG. 4(a), the magnetic decoupling layer 32 of the free layer 13 is made of a Ru layer having a thickness of 10 nm, and each ferromagnetic layer 31 of the free layer 13 is made of a Co layer having a thickness of 50 nm. 70.5 Fe 4.5 Si 15 B 10 It consists of an amorphous layer.

[0033] In addition, in both the magnetic sensor 10 of the present invention and the magnetic sensors of Comparative Examples 1 and 2, the substrate 11 is made of a Si wafer with a thermal oxide film, the buffer layer 12 is made of a 5-nm-thick Ta layer, the insertion coupling layer 23 of the free layer 13 is made of a 0.4-nm-thick Ru layer, the coupling magnetic layer 24 of the free layer 13 is made of a 3-nm-thick CoFeB layer, the barrier layer 14 is made of a 2-nm-thick MgO layer, the reference layer 15 is made of a 3-nm-thick CoFeB layer, and the cap layer 16 is made of a 0.9-nm-thick Ru layer, a 2-nm-thick CoFe layer, and a 10-nm-thick IrMn layer.

[0034] Micrographs of the magneto-optical Kerr effect of the surface of the free layer 13 (the surface of the coupling magnetic layer 24) in zero magnetic field for Comparative Example 1 shown in Figure 3(a), Comparative Example 2 shown in Figure 4(a), and the magnetic sensor 10 of the present invention shown in Figure 5(a) are shown in Figures 3(b), 4(b), and 5(b), respectively. The arrows in each figure indicate the expected magnetization direction. The magnetic field in each figure indicates the magnitude of the external magnetic field applied in the horizontal direction (positive to the right) of each figure.

[0035] As shown in FIG. 3(b), in Comparative Example 1, in which the free layer 13 has one ferromagnetic layer 31, variations in density were observed in the coupling magnetic layer 24, confirming the formation of multiple magnetic domains with different magnetization directions. Also, as shown in FIG. 4(b), in Comparative Example 2, in which the free layer 13 has two ferromagnetic layers 31, most of the coupling magnetic layer 24 has the same density, but some thin areas were observed, confirming the formation of small magnetic domains with different magnetization directions. In contrast, as shown in FIG. 5(b), in the magnetic sensor 10 of the present invention, variations in density were not observed in the coupling magnetic layer 24, and the formation of multiple magnetic domains was not confirmed. Thus, in the magnetic sensor 10 of the present invention, the formation of multiple magnetic domains is suppressed, and it can be said that the element itself can reduce noise. [Explanation of symbols]

[0036] 10 Magnetic Sensor 11 Circuit Board 12 Buffer layer 13 Free layer 21 First magnetic fault 22 subdivision layer 22a Magnetic layer 22b Second magnetic fault 23 Insertion coupling layer 24 Coupling magnetic layer 14 Barrier Layer 15 Reference layer 16 Cap Layer 25 Third Magnetic Fault 31 Ferromagnetic layer 32 Magnetic Fault

Claims

1. A magnetic sensor using a magnetoresistive element, the magnetoresistive element includes a reference layer whose magnetization direction is fixed, a free layer whose magnetization direction is changeable, and a barrier layer disposed between the reference layer and the free layer; the free layer has a first magnetic splitting layer made of a non-magnetic material, a plurality of pairs of subdivided layers stacked in the same number on both sides of the first magnetic splitting layer, and a plurality of third magnetic splitting layers arranged between each subdivided layer on both sides of the first magnetic splitting layer, each subdivided layer having two magnetic layers whose magnetization directions are changeable and antiparallel to each other, and a second magnetic splitting layer made of a non-magnetic material arranged between each magnetic layer so that the magnetic layers are magnetostatically coupled, the first magnetic splitting layer is arranged so that the two magnetic layers arranged on both sides are magnetostatically coupled, and the third magnetic splitting layer is arranged so that the two magnetic layers arranged on both sides are magnetostatically coupled, and the thickness of the first magnetic splitting layer is greater than the thicknesses of the second magnetic splitting layer and the third magnetic splitting layer. A magnetic sensor characterized by:

2. 2. The magnetic sensor according to claim 1, wherein the first magnetic decoupling layer has a thickness of 2 nm to 12 nm.

Citation Information

Patent Citations

  • Magnetic head and magnetic recording reproducing device using it

    JP2005302131A

  • Magnetostatic coupling magnetic elements using spin transfer and magnetic elements MRAM devices

    JP2006516360A

  • Magnetic sensor

    JP2021052050A

  • MRAM free layer synthetic antiferromagnet structure and methods

    US20080205130A1

  • Magnetic memory element utilizing spin transfer switching