Method for producing battery cells

The C-folding method addresses the challenge of precise stacking and air inclusion in battery cell production by folding a wide separator web around electrodes and using a smoothing roller to expel air, resulting in improved battery performance and reduced faulty cells.

WO2024240621A1PCT designated stage expired Publication Date: 2024-11-28ROBERT BOSCH GMBH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/063635
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-19
Filing Date
2024-05-17
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

Existing methods for producing battery cells, such as Z-folding, face challenges in achieving precise stacking and minimizing air inclusions, leading to lower battery performance and increased faulty cells due to imprecise positioning and trapped air pockets.

Method used

The C-folding method involves folding a wide separator web around an electrode, using a smoothing roller to expel air laterally and apply a second electrode externally, allowing for precise stacking and minimizing air inclusions, with the option to integrate lamination during the process for improved tolerance compliance.

Benefits of technology

This method enables precise and high-speed stacking of battery cells with reduced air inclusions, improving battery performance and eliminating the need for separate lamination steps, thus enhancing the quality and reliability of the battery cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024063635_28112024_PF_FP_ABST
    Figure EP2024063635_28112024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a method for producing battery cells in the form of layered components, comprising a first electrode (14), a second electrode (16), and at least one separator layer (12). The method has the following steps: a) arranging the first electrode (14) in a first orientation (76), b) folding one side or both sides of the separator layer (12) about the first electrode (14) oriented in step a), c) smoothing the assembly of the first electrode (14) and the separator layer (12), obtained in step b), in a pulling direction (54) using at least one smoothing element (50), d) applying the second electrode (16) onto the outer face (40, 68) of the separator layer (12) and producing a monocell (58), and e) stacking the monocells (58) obtained in step d) in a stacking direction (60). The invention additionally relates to the use of the method in order to produce battery cells which are provided in the form of monocells (58) and stack same in order to form a stack (72).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Process for producing battery cells

[0002] Technical area

[0003] The invention relates to a method for producing battery cells as layered components comprising a first electrode, a second electrode, and at least one separator layer. Furthermore, the invention relates to the use of the method for producing battery cells designed as monocells and stacking them into a stack.

[0004] State of the art

[0005] DE 10 2013 019 071 A1 relates to an electrode arrangement in a layered structure comprising a first and a second electrode and a separator disposed therebetween, as well as a method for its production. A folding process increases process reliability and the speed of production of the electrode arrangement through improved yield. The simultaneous routing of a conductive track together with an insulating separator track can significantly reduce sources of error in the electrode arrangement. Since the electrodes and separator are provided as tracks, the production and positioning of individual electrodes is unnecessary. The configuration in which the first and second electrodes are preferably arranged at right angles to one another can lead to improved fixation of the individual electrodes within the arrangement and reduce possible slippage of the individual components within the layered structure.Due to the orthogonal arrangement of the two folding directions to one another, complex adhesive bonds or laminations are not necessary. DE 10 2019 202 161 A1 relates to a method for producing battery electrodes. A first electrode sheet is folded along a first folding axis such that the active material region of this sheet covers a separator. Furthermore, a second electrode sheet and a separator are folded together along a second folding axis such that the folded active material region of the second electrode sheet and the co-folded separator cover the first electrode sheet. Within a folded section of a sheet, overlapping parts are connected to one another via a loop, which is also referred to as a C-fold. Such loops are also shown laterally in flat partial stacks, so that a stacking with at least partial C-folding is obtained.

[0006] DE 10 2014 101 051 A1 relates to a method for producing an electrode stack, in particular for an energy storage unit. A material web is folded into an electrode stack, and then at least one folded region of the stack is severed. Defects or joints in the material web are placed in the region to be severed, removing them and creating a high-quality energy storage cell. The material web comprises either an electrode web made of a film web with cathode or anode material, or a separator web made of non-conductive plastic material. Sheets of the other material are then inserted during folding. Severing the folded regions creates open folds similar to C-folds, with air pockets removed laterally. This applies particularly to folded regions on only one side of the electrode stack.

[0007] Disclosure of the invention

[0008] According to the invention, a method for producing battery cells as layered components is proposed, comprising a first electrode, a second electrode and at least one separator layer, wherein the following method steps are carried out: a) arranging the first electrode in a first orientation, b) folding the separator layer on one or both sides around the first electrode oriented according to method step a), c) smoothing the arrangement of first electrode and separator layer obtained according to method step b) with at least one smoothing element in a drawing direction, d) applying the second electrode to an outer side of the separator layer and producing a monocell and e) stacking the monocells obtained according to d) on top of one another in the stacking direction.

[0009] On the one hand, the method proposed according to the invention allows a folded edge to be used as a reference, which results in better tolerances for subsequent processes. Furthermore, the method proposed according to the invention can minimize air inclusions, since the air is rolled outwards during the folding process.

[0010] In an advantageous further development of the method proposed according to the invention, the separator layer is folded in one-sided folding direction according to method step b).

[0011] In an advantageous embodiment of the method proposed according to the invention, according to method step b), the separator layer is folded on one side from its first orientation before folding.

[0012] In the method proposed according to the invention, the separator layer is designed as a separator track or as a separator track segment.

[0013] In the procedure proposed by the invention, the width of the separator track segment corresponds to at least twice the width of the first electrode. This ensures that the electrode is overlapped on both sides by the length of the separator track segment during folding.

[0014] Alternatively, in the method proposed by the invention, according to method step b), the separator layer can be folded in both directions. This allows the first electrode to be covered simultaneously on both sides by folding the separator layer in one operation.

[0015] In an advantageous embodiment of this process variant, according to process step b), the folding of the separator layer on both sides is carried out essentially from a second orientation before the folding process is carried out.

[0016] In this embodiment of the method proposed according to the invention, the separator layer is designed as a separator track or as a separator track segment.

[0017] In the method proposed according to the invention, according to method step c), the smoothing of a layered arrangement of separator layer and first electrode is carried out by means of at least one smoothing element designed as a temperature-controlled smoothing roller.

[0018] In the method proposed according to the invention, air inclusions within the arrangement of the folded separator layers and the first electrode are expelled laterally in a laterally oriented drawing direction before the second electrode is applied to the already formed material composite according to method step d).

[0019] In the method proposed according to the invention, the monocell obtained according to method step d) is advantageously smoothed starting from a reference edge formed by a back of the monocell.

[0020] In an advantageous development of the method proposed according to the invention, the monocells obtained are built up into a stack in the stacking direction according to method step e).

[0021] In the solution proposed according to the invention, it can also be provided that air inclusions, in particular air bubbles, on an upper side and / or a lower side of the monocell are expelled by smoothing elements arranged opposite one another in a horizontal or vertical direction, depending on which direction is more favorable with regard to the production orientation.

[0022] Furthermore, the invention relates to the use of the method for producing battery cells designed as monocells and stacking them into a stack. Advantages of the invention

[0023] The method proposed according to the invention creates the possibility of stacking battery assemblies made up of individual layers precisely and without air inclusions, even at high speeds. The method proposed according to the invention, which is also referred to as C-folding, advantageously enables the lateral expulsion of any air inclusions that may occur. For this purpose, a relatively wide separator film is folded as a web material around one of the electrodes and smoothed in the lateral drawing direction by at least one roller, which can also be heated. A second electrode of the battery assembly is subsequently placed on the outside of the separator film, creating a monocell.

[0024] In this process, the electrode material used can advantageously be provided in the form of a single sheet, but can also be provided in the form of cut segments. The stacked sheet material can then be cut and laminated, requiring fewer cutting processes to assemble the separator film, as only one separator sheet is present instead of the duplicate separator film that would otherwise be required. The transportation resources otherwise required for the elimination of the second separator film can be advantageously saved.

[0025] Furthermore, the method proposed by the invention advantageously offers the possibility of using the folded edge as a reference, thus enabling better tolerance compliance in subsequent processes. A particular advantage of C-folding is the minimization of air inclusions, as already mentioned above, since the air can be rolled outward from the sides of the composite material during folding. Furthermore, a lamination process can be integrated into the stacking or folding process by appropriately controlling the temperature of the at least one smoothing roller, thus eliminating the need for a separate processing step in this regard. Brief Description of the Drawings

[0026] Embodiments of the invention are explained in more detail with reference to the drawings and the following description.

[0027] They show:

[0028] Figure 1 shows the Z-folding in a schematic way,

[0029] Figure 2 shows the C-folding method proposed according to the invention with one-sided folding direction and

[0030] Figure 3 shows the C-folding process proposed according to the invention with double-sided folding direction.

[0031] The illustration in Figure 1 shows a schematic representation of a folding method that has been commonly used to date, namely the Z-folding method.

[0032] A separator layer 12 is continuously conveyed from a web supply 10 for a separator. By stacking using the Z-folding process 22 as part of a stacking process 18, first electrodes 14, corresponding to the anode, and second electrodes 16, corresponding to a cathode, are inserted from each open side at the open ends of the Z-shaped stack structure, resulting in a stacking process 18 taking place in the building direction 20 for building a stack. The individual layers are thin films which are cut to size and alternately stacked on top of one another. The stacking process 18 takes place either by placing the individual sheets on top of one another or by the Z-folding process. The first electrode 14 (anode) and the second electrode 16 (cathode) are alternately folded into the separator layer 12 from the right and left.The layers are bonded together in the lamination process by pressure from above and the application of heat, with the individual sheets being glued together via the separator layer 12. Due to high stacking speeds, the Z-folding method 22 shown in Figure 1 reaches its limits. During normal stacking of the blanks, the positioning of the individual segments of the separator layer 12, first electrode 14 (anode), and second electrode 16 (cathode) relative to one another becomes less precise, and air can become trapped between the layers. These inaccuracies or the resulting air pockets result in reduced battery performance, which is why the defective cells are defined as rejects and cannot be used again.

[0033] Embodiments of the invention

[0034] In the following description of the embodiments of the invention, identical or similar elements are designated by the same reference numerals, whereby a repeated description of these elements is omitted in individual cases. The figures only schematically illustrate the subject matter of the invention.

[0035] Figure 2 shows a first embodiment of the C-folding method 30 proposed according to the invention with a one-sidedly oriented folding direction 36.

[0036] Figure 2 shows that a separator web 32 or a separator web segment 34 is essentially oriented in a first orientation 76. The first orientation 76 as shown in Figure 2 corresponds to a horizontal orientation. The separator web segment 34 or the separator web 32 considered for the C-folding method 30 is folded in a one-sided folding direction 36—in this case, counterclockwise—around the first electrode 14, which is also essentially in a first orientation 76 and serves here, for example, as an anode. The first electrode 14 can alternatively also be the cathode.

[0037] In the folding process illustrated in Figure 2, a second part 46 of the separator web segment 34 is folded counterclockwise in the one-sided folding direction 36 onto the top side of the first electrode 14, which here serves, for example, as an anode. The first part 44 and the second part 46 of the separator web segment 34 together have a width 38. This width is dimensioned such that after the first part 44 of the separator web segment 34 is folded toward the second part 46 of the separator web segment, a ridge 42 is formed on the resulting layer layer.

[0038] The illustration in Figure 2 further shows that the second part 46 of the separator web segment 34 is parallel to the first part 44 of the separator web segment 34, which has remained in its horizontal orientation. The first electrode 14, here in the form of the anode, which has remained in its original horizontal orientation, is enclosed between these. Its outer side 40 points upwards. According to the illustration in Figure 2, a smoothing element 50 in the form of a roller is pulled over the arrangement in a drawing direction 54, which can also be referred to as the drawing direction, in order to expel any remaining air inclusions from the resulting material composite between the resulting layer structure consisting of the first part 44 of the separator web segment 34, the second part 46 of the separator web segment 34, and the first electrode 14 in the direction of the open end, i.e. to smooth and press the resulting material composite starting from a reference edge 48.The tempering 52 of the preferably roller-shaped at least one smoothing element 50 can be selected depending on the materials used for the separator track segment 34 or the separator track 32.

[0039] Figure 2 shows the application of the second electrode 16, which here serves as a cathode, for example, to the outer side 40 of the second part 46 of the separator track segment 34. Alternatively, the second electrode 16 can also serve as an anode. Arrows 56 indicate the escape of air pockets, which are expelled laterally from the material composite by the at least one smoothing element 50 moved in the drawing direction 54 (drawing direction) in order to extend its performance and service life. The layered material composite thus obtained, comprising the first part 44 of the separator track segment 34, the first electrode 14, which here serves as an anode, for example, the second part 46 of the separator track segment 34, and the second electrode 16 applied to its outer side 40, now form a monocell 58.According to the method proposed by the invention, after the respective completion of a monocell 58 in the C-folding process 30, a stack 72 is constructed in the stacking direction 60. This stack comprises a number of monocells 58 stacked one on top of the other in the stacking direction 60, which are open at one end and closed at the other end by the spine 42. The individual, stacked monocells 58 result in a finished stack 72 consisting of a corresponding number of monocells 58, depending on the stack height.

[0040] Figure 3 shows an embodiment of the C-folding method 30 according to the invention, in which a separator web segment 34 or a separator web 32 is arranged essentially in a second orientation 78, in particular vertically, at the beginning of the method. Figure 3 shows that, analogously to the illustration in Figure 1, the separator web segment 34 is divided into a first part 44 and a second part 46. The spine 42 is located between these. Starting from the second orientation 78 shown in Figure 3, the two parts 44, 46 of the separator web segment 34 are moved in the folding direction 62 on both sides. This means that the first part 44 of the separator web segment 34 is folded clockwise and is brought to the essentially horizontally oriented first electrode 14, which here, for example, forms the anode.At the same time, the second part 46 of the separator track segment 34 is folded counterclockwise in the direction of the top side of the first electrode 14, which serves as the anode here. As a result, a material composite is obtained within which the first electrode 14, which serves as the anode in this example, is covered on both sides, ie on the underside by the first part 44 and on its top side by the second part 46 of the separator track segment 34.

[0041] With a first inner side 64, the second part 46 of the separator web segment 34 covers the first electrode 14, which serves as the anode here, while a second inner side 66 of the first part 44 of the separator web segment 34 lies opposite the underside of the first electrode 14. Opposite the resulting back 42, which forms the reference edge 48, the resulting material composite is open. When the at least one smoothing element 50 shown in Figure 1, which is designed as a smoothing roller, is engaged, air inclusions 56 can be expelled laterally from the opening opposite the back 42 of the arrangement, so that no air inclusions remain in the resulting layered composite consisting of the first part 44 and second part 46 of the separator web segment 34 and the first electrode 14, which serves as the anode in this example, but rather they are expelled from the material composite.

[0042] The second electrode 16, which serves as a cathode here, is then applied to a first outer side 68 of the separator track segment 34 or the second part 46 of the separator track segment 34, which covers the electrode 14 on its upper side. The resulting layered composite forms the aforementioned monocell 58. The composite of the second electrode 16 of the second part 46 of the separator track segment 34, the first electrode 14, which serves as an anode here, for example, and the first part 44 of the separator track segment 34 forms the monocell 58.If this is passed over in the drawing direction 54 by a smoothing element 50 (not shown here but visible in Figure 1), which is designed in particular as at least one smoothing roller, then on the one hand air inclusions emerge 56 from the layer composite and on the other hand lamination can be achieved with appropriate temperature control 52 of the at least one smoothing element 50, which is preferably designed as a roller.

[0043] Depending on the number of monocells 58 stacked one above the other in the stacking direction 60, a stack 72 is formed. This stack 72 can be designed in different stack heights depending on the number of monocells 58 arranged one above the other, which can depend on the power to be delivered and the installation conditions for such stacks.

[0044] Both embodiments of the C-folding process 30 according to Figures 2 and 3 have in common that the electrode materials of the first electrode 14 and the second electrode 16 are pre-cut segments or web material. It should be noted that the first electrode 14 and the second electrode 16 can form both the anode and the cathode. Depending on the embodiment of the electrode materials, a corresponding separating cut is made before or after the C-folding process 30. The monocells 58 obtained by the C-folding process 30 with a one-sided folding direction 36 or with a two-sided folding direction 62 are laminated and then stacked with further monocells 58 in the stacking direction 60 to form a stack 72.When applying the double-sided folding direction 62, in the use of which the C-folding method 30 is shown in the embodiment according to Figure 3, the material of the separator web segment 34 can be subjected to less stress and possibly have improved performance.

[0045] Furthermore, the invention relates to the use of the method for producing battery cells and stacking them into a stack 72.

[0046] A horizontal orientation of the first and second electrodes 14, 16 is not mandatory in the present context. Vertical processing of the first and second electrodes 14, 16 between rollers can provide manufacturing advantages. Furthermore, it should be noted that, in the above context, the smoothing out of air bubbles on the top and / or bottom of the resulting monocells 58 by two oppositely positioned smoothing elements 50, in the form of rollers or discs or the like, is also possible. The smoothing out of air inclusions can occur both vertically and horizontally and depends on the available manufacturing conditions.

[0047] The invention is not limited to the embodiments described here and the aspects highlighted therein. Rather, numerous modifications are possible within the scope of the claims, which are within the scope of one skilled in the art.

Claims

Claims 1. A method for producing battery cells as layered components, comprising a first electrode (14), a second electrode (16) and at least one separator layer (12), with the following method steps: a) arranging the first electrode (14) in a substantially first orientation (76), b) folding the separator layer (12) on one or both sides around the first electrode (14) oriented according to method step a), c) smoothing the arrangement of first electrode (14) and separator layer (12) obtained according to method step b) with at least one smoothing element (50) in a pulling direction (54), d) applying the second electrode (16) to an outer side (40, 68) of the separator layer (12) and producing a monocell (58) and e) stacking the monocells (58) obtained according to d) one above the other in the stacking direction (60).

2. Method according to claim 1, characterized in that according to method step b) the one-sided folding of the separator layer (12) takes place in a one-sided folding direction (36).

3. Method according to claims 1 and 2, characterized in that according to method step b) the one-sided folding of the separator layer (12) from its substantially horizontal first orientation (76) takes place before folding.

4. Method according to claims 1 to 3, characterized in that the separator layer (12) is designed as a separator web (32) or a separator web segment (34).

5. Method according to claims 1 to 4, characterized in that a width (38) of the separator track segment (34) corresponds to at least twice the width (74) of the first electrode (14).

6. Method according to claim 1, characterized in that according to method step b) a bilateral folding of the separator layer (12) in the bilateral folding direction (62) takes place 7. Method according to claims 1 and 6, characterized in that according to method step b) the folding of the separator layer (12) on both sides takes place essentially from a second orientation (78) before folding.

8. Method according to claims 1, 6 and 7, characterized in that the separator layer (12) is designed as a separator web (32) or a separator web segment (34).

9. Method according to claims 1 to 8, characterized in that the smoothing according to method step c) is carried out by means of a smoothing element (50) designed as at least one temperature-controlled smoothing roller.

10. Method according to claim 9, characterized in that air inclusions are expelled laterally in the drawing direction (54) before the second electrode (16) is applied according to method step d).

11. Method according to claims 1 to 8, characterized in that air inclusions, in particular air bubbles, on an upper side and / or a lower side of the monocell (58) are expelled in a horizontal or vertical direction by smoothing elements (50) arranged opposite one another.

12. Method according to claims 1 to 11, characterized in that the monocell (58) obtained according to method step d) is smoothed starting from a reference edge (48) which is formed by a back (42) of the monocell (58).

13. Method according to claims 1 to 12, characterized in that the monocells (58) obtained according to method step e) are built up in the stacking direction (60) to form a stack (72).

14. Use of the method according to one of claims 1 to 13 for producing battery cells designed as monocells (58) and stacking them to form a stack (72).

Citation Information

Patent Citations

  • Electrode arrangement, method for its manufacture and electrochemical cell

    DE102013019071A1

  • Method and apparatus for producing an electrode stack

    DE102014101051A1

  • Methods for manufacturing battery electrodes

    DE102019202161A1

  • Method and machine for producing a cell stack for the energy cell manufacturing industry

    DE102021212280A1

  • Device and method for producing electrode stacks

    US20150263375A1