Insulated gate bipolar transistor device and preparation process thereof

By adopting circular or annular trench gates and honeycomb arrangements in IGBT devices, the channel density is improved, and the problems of current density and on-state loss are solved, and high-power and low-cost IGBT devices are realized.

CN120417412AInactive Publication Date: 2025-08-01JIANGSU CHANGJING ELECTRONICS TECH CO LTD

Patent Information

Application Number
CN202510927336.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-07
Publication Date
2025-08-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The current density and power density of existing trench IGBT devices are limited, and the on-state loss is high, making it difficult to meet the needs of high power and low cost.

Method used

The trench gate with a circular or annular closed structure is adopted, combined with a honeycomb arrangement, and the channel density is increased, and the design of the doped layer and the dielectric layer is formed to form an IGBT structure with high current density and low pass-state loss.

Benefits of technology

Achieve higher current density and lower on-state loss while reducing chip area and cost, suitable for IGBT and MOS devices of various voltages.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120417412A_ABST
    Figure CN120417412A_ABST
Patent Text Reader

Abstract

The invention discloses an insulated gate bipolar transistor device and a preparation process thereof, and the device comprises a substrate, a drain electrode which is formed below the substrate, a dielectric layer which is formed above the substrate, a source electrode which is formed above the dielectric layer, and a plurality of grooves which are formed in the substrate in a downward etching and sinking manner and are independently arranged, independent trench gates are deposited in the trenches, the cross section of the plurality of trenches is of a circular or annular or polygonal closed structure, and the trench gates are insulated and isolated from the side walls of the trenches and the source electrodes through dielectric layers. The novel groove type IGBT structure is achieved through the groove gates arranged in a circular layout mode, the structure has the advantages of being high in channel density, large in current density, simple in process and the like, and the chip area and the cost can be reduced while the current capacity is kept; or the current density and the power density of the device are improved while the chip area is maintained, and the on-state loss is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductors, and particularly relates to an insulated gate bipolar transistor device and a manufacturing process thereof. Background Art

[0002] Insulated gate bipolar transistors (IGBTs) are widely used in AC motors, inverters, switching power supplies, lighting circuits, motor drives, etc. due to their high power and low loss characteristics. With the increasing requirements for improving the current and power output capabilities of IGBTs and reducing the chip cost and area at the application end, it is necessary to further improve the current density and power density of IGBT devices, reduce their on-state losses, and achieve a better compromise between power capabilities and chip costs.

[0003] Conventional trench IGBTs have a strip gate topology structure, and the channel density of this structure is restricted by the topology, which restricts the further improvement of the current and power capabilities of IGBT devices. Summary of the Invention

[0004] The object of the present invention is to provide an insulated gate bipolar transistor device and a manufacturing process thereof that can achieve higher current density and lower on-state losses.

[0005] The present invention provides an insulated gate bipolar transistor device, including a substrate, an epitaxial layer formed above the substrate, a drain formed below the substrate, a dielectric layer formed above the epitaxial layer, a source formed above the dielectric layer, and a plurality of independently arranged trenches etched downward in the epitaxial layer. A separate trench gate is deposited in the trenches, wherein the cross-sections of the plurality of trenches are circular or annular or polygonal closed structures, and the trench gate is insulated and isolated from the trench sidewalls and the source through the dielectric layer.

[0006] As a further improvement of the present invention, the plurality of trenches are evenly divided into a plurality of rows of parallel trench rows for arrangement.

[0007] As a further improvement of the present invention, the trenches in the odd-numbered trench rows and the trenches in the even-numbered trench rows are alternately complementary to each other and arranged in a honeycomb shape.

[0008] As a further improvement of the present invention, the device further includes a first doped layer doped in the peripheral area near the upper part of the trench in the substrate and a second doped layer doped below the first doped layer.

[0009] As a further improvement of the present invention, the first doped layers doped in the peripheral areas of the upper part of each trench are not physically connected, and the second doped layers are connected to form an entire area. The source includes a source electrode that is buried downward from the hole area to connect the first doped layers in the peripheral areas of the upper part of each trench and is buried into the second doped layer.

[0010] As a further improvement of the present invention, the device further includes a charge storage layer formed by doping under the second doping layer, an FS buffer layer formed by doping on the lower surface of the substrate, and a collector layer formed by doping on the lower surface of the buffer layer.

[0011] As a further improvement of the present invention, the first doping layer is implanted with N-type ions, the second doping layer is implanted with P-type ions, the charge storage layer is implanted with N-type ions, the FS buffer layer is implanted with N-type ions, and the collector layer is implanted with P-type ions.

[0012] As a further improvement of the present invention, the distance between each trench and its adjacent trenches around is 0.2 - 4 um.

[0013] The present invention also provides a preparation process for an insulated gate bipolar transistor device, including the following steps: S1. Prepare a substrate, deposit a hard mask on the upper surface of the substrate, then perform photoresist patterning according to the designed trench arrangement scheme, and subsequently transfer the pattern to the hard mask for deep silicon etching. S2. Etch downward on the substrate to form a number of independent and non-connected trenches, then oxidize or deposit a dielectric layer on the sidewall surface of the trenches, and continue to precipitate polysilicon in the trenches to form trench gates. S3. Perform N-type ion implantation doping on the surface area of the substrate between the trenches to form a carrier storage layer, then perform P-type ion implantation doping to form a second doping layer on the carrier storage layer, and then continue to perform N-type ion implantation on the surface of the substrate near the upper region of the trenches to form a first doping layer. S4. Deposit a dielectric layer on the entire upper surface of the substrate, perform reverse etching pattern formation for the contact hole area based on the designed trench arrangement scheme, etch downward from the dielectric layer based on the contact hole area etching pattern to form a contact hole structure, and deposit metal into the contact hole structure to form a source electrode and a gate electrode. This step can be repeated to achieve a metal structure with two or more layers so as to properly lead out the relevant source and gate electrodes. S5. Passivation protection on the front side of the device, device thinning, backside implantation and metal sputtering, backside N-type ion implantation to form an FS buffer layer, backside P-type ion implantation to form a collector structure, and backside sputtering or evaporation of metal growth to form a drain electrode.

[0014] As a further improvement of the present invention, the cross-sectional area of the trench is circular, the diameter is 0.2 - 1.5 um, the trench depth is 0.5 - 7 um, the distance between adjacent trenches in the trench arrangement scheme is 0.2 - 4 um, and the maximum width of the contact hole structure in the contact hole area etching pattern is at least 0.1 um smaller than the distance between the trenches at the corresponding position in the trench arrangement scheme.

[0015] Advantages of the present invention The present invention realizes a novel trench IGBT structure through a trench gate with a circular layout. This structure has the characteristics of high channel density, large current density, and simple process. It can reduce the chip area while maintaining the current capacity, thereby reducing costs; or improve the current density and power density of the device while maintaining the chip area, and reduce the on-state loss. By using a channel gate pattern with a special structure, the perimeter of the emitter is increased, thereby increasing the channel density, enabling higher current density and lower on-state loss. This structure can be used in various devices with a trench gate structure, including IGBTs and MOSs of various voltages; at the same time, it can also be combined with short-circuiting part of the gate and the emitter to control the switching speed and saturation current capacity. Brief description of the drawings

[0016] Figure 1 It is a schematic vertical cross-sectional view of the channel of an insulated gate bipolar transistor device in the present invention; Figure 2 It is a schematic horizontal cross-sectional view of the channel of an insulated gate bipolar transistor device in the present invention; Figure 3 It is a schematic diagram of the manufacturing process flow of an insulated gate bipolar transistor device in the present invention. Detailed implementation manners

[0017] In order to enable those skilled in the art to better understand the technical solutions in the present invention, the following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. All other embodiments obtained by those of ordinary skill in the art without creative efforts in the embodiments of the present invention should fall within the protection scope of the present invention.

[0018] This embodiment provides an insulated gate bipolar transistor device 100, including a substrate 101, an epitaxial layer 102 formed above the substrate 101, and a drain 103 formed below the substrate. A dielectric layer 104 is formed above the epitaxial layer 102, and a source 105 is formed above the dielectric layer 104. A plurality of independently arranged trenches 106 are formed by etching depressions downward in the epitaxial layer 102. A separate trench gate 107 is deposited in the trenches 106. The cross-sections of the plurality of trenches 106 are in a circular or annular or polygonal closed structure, and the trench gate 107 is insulated from the trench sidewalls and the source 105 by the dielectric layer 104.

[0019] In this embodiment, each groove is independent of each other and is not connected. The cross section of each groove is preferably circular. The plurality of grooves are evenly divided into a plurality of parallel rows of grooves for arrangement. The grooves of the odd-numbered rows of grooves and the grooves of the even-numbered rows of grooves are alternately complementary to each other and arranged in a honeycomb shape. In the arrangement method, it is preferred to arrange them in a honeycomb-like manner. Admittedly, in the actual process, it is difficult to ensure that the cross section of each groove is a standard circle. Therefore, designing the groove cross section into a ring or a polygon that is approximately circular is also within the optional solution of the present invention, and the spacing between each groove and its surrounding adjacent grooves is 0.2-4um, the groove diameter is between 0.2-1.5um, and the depth is between 0.5-7um.

[0020] The device also includes a first doped layer 108 formed by doping in the upper peripheral region of the substrate 101 near the trench 106, and a second doped layer 109 formed by doping below the first doped layer 108. The first doped layers 108 formed by doping in the upper peripheral region of each trench 106 are not physically connected, and the second doped layers 109 are interconnected to form a whole region. The source 105 includes a source electrode 111 buried downwardly through the hole region 110 and connected to the first doped layer 108 at the upper peripheral region of each trench 106, and buried in the second doped layer 109. The device also includes a charge storage layer 112 formed by doping below the second doped layer 109, a FS buffer layer 113 formed by doping on the lower surface of the substrate 101, and a collector layer 114 formed by doping on the lower surface of the buffer layer 113.

[0021] In this embodiment, the first doping layer is injected with N-type ions, the second doping layer is injected with P-type ions, the charge storage layer is injected with N-type ions, the FS buffer layer is injected with N-type ions, and the collector layer is injected with P-type ions.

[0022] The present invention also provides a process for preparing an insulated gate bipolar transistor device, comprising the following steps: S1. Prepare the substrate, deposit a hard mask on the upper surface of the substrate, then pattern the designed trench arrangement with photoresist, and then transfer the pattern to the hard mask for deep silicon etching.

[0023] In the process of preparing the substrate, the substrate needs to be N-type doped first. The substrate is first prepared by FZ, CZ, MCZ or Epi. The material resistivity is generally related to the breakdown voltage, and the resistivity is 0.1-300ohm. Then the active area is photolithography and etching, and then the N-type doping concentration is 1E14-1E19cm -3 , forming a charge storage layer to complete substrate preparation.

[0024] In this embodiment, in order to achieve a high degree of uniformity in the overall layout and spacing control of trenches and contact holes in the front and back etching processes, in this step, after patterning the designed trench arrangement with photoresist, the formed pattern scheme is saved for later use.

[0025] S2. Etch downward on the substrate to form a number of independent and non-connected trenches, then oxidize or deposit a dielectric layer on the sidewall surfaces of the trenches, and continue to precipitate polysilicon in the trenches to form trench gates.

[0026] In this embodiment, the top-view morphology of the trenches is preferably a circular structure. Therefore, during the formation of specific trenches, after removing the oxide layer and photoresist in the active region, sacrificial oxidation is required to repair the morphology inside the trenches and reduce the defect density. Of course, in other feasible implementation schemes, the top-view morphology of the trenches can also be designed as a general annular shape or a polygon-like approximate circular structure. On the other hand, in the arrangement of the trenches, it is preferred to arrange the trenches according to a certain rule. For example, they can be arranged in rows in an orderly manner horizontally or vertically. In this embodiment, the optimal arrangement is an alternating arrangement of upper and lower rows, presenting an overall honeycomb-like shape. This can achieve a higher current density. Parallel arrangement can also be used. In this embodiment, generally, the diameter of the trench circle is between 0.2 - 1.5 μm, and the depth is between 0.5 - 7 μm; the spacing between two circular trenches is generally 0.2 - 4 μm.

[0027] In this step, after repairing the trench morphology, gate oxide is grown on the inner wall of the trenches to form a dielectric layer. Generally, the gate oxide temperature is 900 - 1200 °C. The traditional process can use dry oxidation process or wet oxidation process. Generally, DCE gas is added to improve the quality of the gate oxide, and the thickness is generally 100 - 2000 Å; after the dielectric layer is formed, polysilicon is deposited in the trenches and the trenches are filled, and then the polysilicon is lithographed and etched to form trench gates.

[0028] S3. Perform N-type ion implantation doping on the surface area of the substrate between the trenches to form a carrier storage layer, then perform P-type ion implantation doping to form a second doping layer on the carrier storage layer, and then continue to perform N-type ion implantation on the surface of the substrate near the upper region of the trenches to form a first doping layer.

[0029] In this embodiment, after the doping of the first doping layer is completed, it forms an entire interconnected area. The top-view morphology of this area is the surface area of the substrate outside the trenches. After the second doping layer is completed, it is only formed in the area around the upper part of the trench sidewalls. The top-view morphology of this area is an annular area surrounding the periphery of the trenches. The annular areas formed around each trench are physically isolated from each other and not connected.

[0030] S4. Deposit a dielectric layer on the entire upper surface of the substrate, reverse-etch to form an etching pattern for the contact hole region based on the designed trench arrangement scheme, etch downward from the dielectric layer based on the etching pattern for the contact hole region to form a contact hole structure, and deposit metal into the contact hole structure to form a source electrode and a gate electrode.

[0031] In this step, it is necessary to reverse-design an etching pattern for the contact hole region that is complementary to the trench position, shape, and size based on the pattern scheme formed according to the trench arrangement scheme designed in step S1. And in the etching pattern for the contact hole region, it is necessary to ensure that the maximum width of the contact hole is 0.1 um smaller than the distance between adjacent trenches in the corresponding position of the trench arrangement scheme. Such a design can ensure that there is a certain thickness of the doped layer between the metal electrode buried in the contact hole and the trench dielectric layer, rather than directly contacting the dielectric layer or even damaging the dielectric layer and directly contacting the trench gate to form leakage. In the specific implementation process, this step can be repeated to achieve a metal structure with two or more layers in order to properly lead out the relevant source and gate electrodes.

[0032] S5. Passivation protection of the front side of the device, device thinning, backside implantation and metal sputtering, N-type ion implantation on the backside to form an FS buffer layer, P-type ion implantation on the backside to form a collector structure, and metal growth by sputtering or evaporation on the backside to form a drain electrode.

[0033] The present invention realizes a novel trench-type IGBT structure through a trench gate with a circular layout. This structure has the characteristics of high channel density, large current density, and simple process. It can reduce the chip area and cost while maintaining the current-carrying capacity; it can also increase the current density and power density of the device while maintaining the chip area, and reduce the on-state loss. By using a channel gate pattern with a special structure, the perimeter of the emitter is increased, thereby increasing the channel density, enabling a higher current density and a lower on-state loss. This structure can be used in various devices with a trench gate structure, including IGBTs and MOSs of various voltages; at the same time, it can also be combined with short-circuiting part of the gate and the emitter to control the switching speed and saturation current capacity.

[0034] For those skilled in the art, it is obvious that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic characteristics of the present invention. Therefore, from any point of view, the embodiments should be regarded as exemplary and non-limiting. The scope of the present invention is defined by the appended claims rather than the above description. Therefore, all changes falling within the meaning and scope of the equivalent elements of the claims are intended to be included in the present invention. Any reference signs in the claims should not be regarded as limiting the claimed rights.

[0035] In addition, it should be understood that although this specification is described according to embodiments, not every embodiment only contains an independent technical solution. This narrative way of the specification is only for clarity. Those skilled in the art should regard the specification as a whole, and the technical solutions in each embodiment can also be appropriately combined to form other embodiments that can be understood by those skilled in the art.

Claims

1. An insulated gate bipolar transistor device, characterized in that: It includes a substrate, an epitaxial layer formed above the substrate, a drain formed below the substrate, a dielectric layer formed above the epitaxial layer, and a source formed above the dielectric layer. A number of independently arranged trenches are etched downward in the epitaxial layer, and individual trench gates are formed by deposition within the trenches. Among them, the cross-sections of the number of trenches are circular or annular or polygonal closed structures, and the trench gates are insulated from the trench sidewalls and the source by the dielectric layer.

2. The insulated gate bipolar transistor device according to claim 1, wherein: The number of trenches is evenly divided into a number of rows of parallel trench rows for arrangement.

3. The insulated gate bipolar transistor device according to claim 2, characterized in that: The trenches in the odd-numbered trench rows and the trenches in the even-numbered trench rows are alternately complementary to each other and arranged in a honeycomb shape.

4. The insulated gate bipolar transistor device according to claim 1, wherein: The device further includes a first doped layer formed by doping in the peripheral area near the upper part of the trench in the substrate and a second doped layer formed by doping below the first doped layer.

5. The insulated gate bipolar transistor device according to claim 4, characterized in that: The first doped layers formed by doping in the peripheral area near the upper part of each trench are not physically connected, and the second doped layers are connected to form an entire area. The source includes source electrodes that are buried downward from the hole area to connect the first doped layers in the peripheral area near the upper part of each trench and are buried into the second doped layer.

6. The insulated gate bipolar transistor device according to claim 5, characterized in that: The device further includes a charge storage layer formed by doping below the second doped layer, an FS buffer layer formed by doping on the lower surface of the substrate, and a collector layer formed by doping on the lower surface of the buffer layer.

7. The insulated gate bipolar transistor device according to claim 6, characterized in that: The first doped layer is implanted with N-type ions, the second doped layer is implanted with P-type ions, the charge storage layer is implanted with N-type ions, the FS buffer layer is implanted with N-type ions, and the collector layer is implanted with P-type ions.

8. The insulated gate bipolar transistor device according to claim 1, characterized in that: The distance between each trench and its adjacent trenches around it is 0.2 - 4 um.

9. A manufacturing process of an insulated gate bipolar transistor device as described in any one of claims 1-8, characterized in that: It includes the following steps S1. Prepare the substrate, deposit a hard mask on the upper surface of the substrate, then pattern the photoresist according to the designed trench arrangement scheme, and then transfer the pattern to the hard mask for deep silicon etching. S2. Etch downward on the substrate to form a number of independent and non-connected trenches, then oxidize or deposit a dielectric layer on the sidewall surface of the trenches, and continue to deposit polysilicon in the trenches to form trench gates. S3. Inject N-type ions into the surface area of the substrate between the trenches to form a carrier storage layer, then inject P-type ions to form a second doped layer on the carrier storage layer, and then continue to inject N-type ions into the surface of the substrate near the upper part of the trenches to form a first doped layer. S4. Deposit a dielectric layer on the entire upper surface of the substrate, etch and pattern to form a contact hole area in reverse according to the designed trench arrangement scheme, etch downward from the dielectric layer based on the contact hole area etching pattern to form a contact hole structure, and deposit metal into the contact hole structure to form source electrodes and gate electrodes. S5. Passivation protection of the front side of the device, device thinning, backside injection and metal sputtering, backside N-type ion injection to form an FS buffer layer, backside P-type ion injection to form a collector structure, and backside sputtering or evaporation of metal growth to form a drain electrode.

10. The manufacturing process of the insulated gate bipolar transistor device according to claim 9, characterized in that: The cross-sectional area of the groove is circular, with a diameter of 0.2 - 1.5 um, the groove depth is 0.5 - 7 um, the distance between adjacent grooves in the groove arrangement scheme is 0.2 - 4 um, and the maximum width of the contact hole structure in the contact hole area etching pattern is at least 0.1 um smaller than the distance between the grooves at the corresponding position in the groove arrangement scheme.

Citation Information

Patent Citations

  • Methods for fabricating transistors including circular trenches

    CN102683409A

  • Insulated gate bipolar transistor

    CN211150565U

  • Insulated gate bipolar transistor with multiple gate and method for menufacturing insulated gate bipolar transistor with multiple gate

    KR100744845B1

  • Vertical Transistor Device Structure with Cylindrically-Shaped Field Plates

    US20180069087A1

Cited By

  • Semiconductor structure

    CN121240476A