Method for manufacturing a liquid cosmetic impregnated foam and the foam
By using a mixing ratio of polyester polyol and polyether polyol of 3:7 or 4:6, combined with specific additives and testing methods, the problem of imbalance between water resistance and oil resistance of liquid cosmetic carrier foam was solved, achieving reliable monitoring and excellent impregnation performance.
Patent Information
- Application Number
- CN202511504699.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-11-21
- Filing Date
- 2025-10-21
- Publication Date
- 2026-05-22
AI Technical Summary
Existing liquid cosmetic composition carrier foams have an imbalance in water resistance and oil resistance, making the carriers prone to corrosion and unable to be used for a long time.
A foam was manufactured by mixing polyester polyol and polyether polyol in a ratio of 3:7 or 4:6, combined with specific foaming agents, catalysts and surfactants, through a series of process steps. The balance of its hydrolysis resistance, water resistance and oil resistance was monitored by FT-IR and solid NMR tests.
It provides measurement methods and standards that can reliably monitor the state of foam, producing foams with uniform pore size, excellent fluffiness, softness and elasticity, capable of uniformly impregnating and expelling liquid cosmetics for a long time, and maintaining excellent durability.
Smart Images

Figure CN122071567A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a method for manufacturing a foam for impregnating liquid cosmetics and the foam itself. The foam exhibits excellent oil and water resistance when used for impregnating liquid cosmetic compositions (such as solutions, emulsions, gels, creams, or suspensions), enabling prolonged use. More specifically, this invention relates to a method for manufacturing a foam for impregnating liquid cosmetics and the foam itself, the method comprising a test method for quantitatively quantifying the oil and water resistance of the foam for impregnating liquid cosmetics. Background Technology
[0002] Traditional liquid cosmetic compositions are primarily stored and distributed in vacuum containers, pump containers, or glass containers. However, these containers are inconvenient to carry. Recently, with the increasing demand for convenient makeup application or touch-ups while on the go, the need for portable liquid cosmetic compositions is growing.
[0003] As a container that can easily carry liquid cosmetic compositions, a powder-cartridge type container can be considered. In order to fill the liquid cosmetic composition into the powder-cartridge type container, it is necessary to consider whether the cosmetic composition carrier is suitable for the powder-cartridge type container, whether the cosmetic composition can be fully filled into the carrier, whether the carrier can hold the cosmetic composition evenly for a long time, and whether the cosmetic composition can be appropriately discharged from the carrier when it is used.
[0004] In view of these considerations, it has recently been found that foams made by foaming synthetic resins have excellent filling, impregnation and drainage capabilities, thus satisfying the above considerations. Therefore, synthetic resin foams (e.g., ester-based foams and ether-based foams) are used as carriers for liquid cosmetic compositions.
[0005] However, for foams used as carriers of traditional liquid cosmetic compositions, ether-based foams are water-resistant but not oil-resistant, thus they corrode and their oil resistance weakens. Ester-based foams are oil-resistant but not water-resistant, thus they corrode and their water resistance weakens. For these reasons, prolonged use of the carrier can lead to breakage and loss of function, rendering it unusable.
[0006] [Prior Technology Documents] (Patent Document 0001) Korean Patent Publication No. 10-2013-0116205 (Patent Document 0002) Korean Patent Publication No. 10-0725240 The applicant's patent No. 1574493, entitled "Method for manufacturing foam for liquid cosmetic impregnation and the foam", discloses a foam for liquid cosmetic impregnation in order to improve the hydrolysis resistance of polyester sponge and ensure the balance between water resistance and oil resistance. The foam is made by mixing polyester polyol and polyether polyol in a ratio of 3:7 or 4:6.
[0007] With the widespread application of foams for liquid cosmetic impregnation both domestically and internationally, the scale of equipment in production sites is expanding day by day. This places high demands on the reliability of the manufactured foams for liquid cosmetic impregnation, including their resistance to hydrolysis and the balance between water resistance and oil resistance.
[0008] In particular, corrosion of foam used for impregnating liquid cosmetics can lead to deterioration of the liquid cosmetics, which can cause skin problems for customers. Therefore, it is very important to evaluate the balance of hydrolysis resistance, water resistance and oil resistance of foam used for impregnating liquid cosmetics.
[0009] However, there are currently no reliable measurement methods or standards to monitor the condition of the manufactured foam for impregnation in liquid cosmetics. Summary of the Invention
[0010] Technical issues The present invention is proposed to solve the above-mentioned problems. The purpose of the present invention is to provide a method for manufacturing a foam and the foam, wherein the manufacturing method includes a test method for a foam for impregnating liquid cosmetics that can reliably monitor the balance of hydrolysis resistance, water resistance and oil resistance.
[0011] Technical solution To solve the above problems, the method for manufacturing a liquid cosmetic impregnation foam of the present invention may include: step a: placing polyester polyols into a chamber, venting at a temperature of 55 to 65°C, and letting it stand for 60 minutes under a pressure of 0.1 to 0.2 kPa, then lowering the temperature to 25 to 35°C, supplying nitrogen, and letting it stand for 48 hours under a pressure of 2 to 3 kPa to prepare polyester polyols; Step b: Place the polyether polyols into the chamber and let it stand for 60 minutes at a temperature of 15-25°C and a pressure of 0.1-0.2 kPa. Then supply nitrogen and let it stand for 48 hours at a pressure of 2-3 kPa to prepare the polyether polyols. Step c: According to the required dosage, inject the foaming agent, catalyst and surfactant into the tank for later use; Step d: The polyester polyol, polyether polyol, foaming agent, catalyst and surfactant are added to the mixing tank in sequence according to the ratio, and the mixture is stirred at 5000 rpm / min under the conditions of 22-24℃ and 3kPa pressure, while continuous foaming is carried out. Step e: Aging the foam formed after the foaming step for 48 hours; Step f: Cut the foam body for productization. The method further includes a testing step for the foam, which may include the following steps: manufacturing a foam for impregnating liquid cosmetics that can be used to impregnate liquid or solid cosmetic compositions; performing an FT-IR test on the manufactured foam for impregnating liquid cosmetics; determining whether the FT-IR test result value is within a specific proportional range that provides a balance between the hydrolysis resistance, water resistance, and oil resistance of the foam for impregnating liquid cosmetics; and if the FT-IR test result value is within the specific proportional range, performing a solid-state NMR test.
[0012] Wherein, the mixing in step d is characterized in that, relative to 100 parts by weight of the mixture formed by mixing the polyester polyol and the polyether polyol in a weight ratio of 3:7 to 4:6, it is mixed to form a mixture comprising 0.2 to 0.4 parts by weight of foaming agent, 0.2 to 0.4 parts by weight of catalyst, and 2 to 4 parts by weight of surfactant.
[0013] The foaming agent is characterized in that it is selected from any one of HCFC-141b, HCFC-142b, and HCF-22 sold by Soo Kyung Chemical Co., Ltd.
[0014] The catalyst is characterized in that it is selected from any one of TEDA, DETDA, 33lv, A-1, A-99, and TEOA sold by Soo Kyung Chemical Co., Ltd.
[0015] The surfactant is characterized in that it is selected from any one of AK8818, AK8803, and AK8806 sold by Soo Kyung Chemical Co., Ltd.
[0016] Furthermore, the present invention provides a foam for impregnation in liquid cosmetics, characterized in that it is manufactured by the above-described manufacturing method, wherein the mixing ratio of polyester polyol and polyether polyol is either 3:7 or 4:6.
[0017] This invention provides a foam for impregnation in liquid cosmetics, the foam having an average pore size of 900–1100 μm, a pore number of 60–80 ppi (pores / inch), and a density of 40–45 kg / m³. 3 Physical properties include a resilient modulus of 40%–45%, a compressive strain rate of 30%–40%, a hardness of 75–80°, a tensile strength of 220–230 kPa, and an absorption rate of 300%–400%.
[0018] Beneficial effects According to one embodiment of the present invention, a test method for a foam for liquid cosmetic impregnation that can reliably monitor the balance of hydrolysis resistance, water resistance and oil resistance of the foam for liquid cosmetic impregnation, and a foam for liquid cosmetic impregnation that passes the test method and a method for manufacturing the same are provided.
[0019] Furthermore, according to one embodiment of the present invention, a reliable means and standard for monitoring the state of foam for impregnation with liquid cosmetics can be provided, thereby enabling the reliable production of foams with uniform pore size and excellent fluffiness, softness, flexibility and elasticity, as well as excellent filling ability for liquid cosmetics, excellent impregnation ability for long-term uniform impregnation with liquid cosmetics, high discharge ability for discharging an appropriate amount of liquid cosmetics when taking out liquid cosmetics, and excellent durability even after impregnation with liquid cosmetics. Attached Figure Description
[0020] Figure 1 This is an exploded perspective view of a traditional cosmetic box with foam material for impregnating liquid cosmetics.
[0021] Figure 2 This is a flowchart describing the test method used in the manufacturing method of the liquid cosmetic impregnation foam of the present invention.
[0022] Figure 3 This is a graph showing the spectral analysis information of foam used for impregnation in liquid cosmetics.
[0023] Figure 4 This is a graph showing the solid NMR test results of a foam for liquid cosmetic impregnation according to an embodiment of the present invention.
[0024] Explanation of reference numerals in the attached figures 1: Foam for impregnating liquid cosmetics 2: Powder puff 3: Powder puff container 4: Cosmetic containers 5: Foam containment section Detailed Implementation
[0025] The invention will be described in further detail below with reference to the accompanying drawings.
[0026] Unless otherwise defined, all terms (including technical or scientific terms) used in this specification have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains.
[0027] The present invention aims to provide a method for manufacturing a foam for impregnating liquid cosmetics, which can be used to impregnate liquid or solid cosmetic compositions (such as solutions, emulsions, gels, creams, or suspensions). The method for manufacturing a foam for impregnating liquid cosmetics according to the present invention is characterized by comprising the following steps.
[0028] Step a: Place the polyester polyol into the chamber, exhaust the gas at a temperature of 55-65°C, and let it stand for 60 minutes under a pressure of 0.1-0.2 kPa. Then lower the temperature to 25-35°C, supply nitrogen, and let it stand for 48 hours under a pressure of 2-3 kPa to prepare the polyester polyol. Step b: Place the polyether polyol into the chamber and let it stand for 60 minutes at a temperature of 15-25°C and a pressure of 0.1-0.2 kPa. Then supply nitrogen and let it stand for 48 hours at a pressure of 2-3 kPa to prepare the polyether polyol. Step c: According to the required dosage, inject the foaming agent, catalyst and surfactant into the tank for later use; Step d: The polyester polyol, polyether polyol, foaming agent, catalyst and surfactant are added to the mixing tank in the specified proportions. The mixture is stirred at 5000 rpm / min under the conditions of 22-24℃ and 3kPa pressure. The mixture is then placed in a mold for continuous foaming. Step e: Aging the foam formed after the foaming step for 48 hours; and Step f: Cut the foam body into products.
[0029] According to the present invention, for the mixing in step d, the mixture is characterized in that, relative to 100 parts by weight of the mixture formed by mixing the polyester polyol and the polyether polyol in a weight ratio of 3:7 to 4:6, it is mixed to form a mixture comprising 0.2 to 0.4 parts by weight of foaming agent, 0.2 to 0.4 parts by weight of catalyst, and 2 to 4 parts by weight of surfactant.
[0030] At this point, if the mixing ratio of the polyester polyol and the polyether polyol exceeds the critical value, there is a disadvantage that the pore size of the final foam cannot be uniformly formed, and the density cannot be fully guaranteed, resulting in a decrease in absorption rate.
[0031] Furthermore, due to the low resilience modulus, there may be issues such as reduced usability after impregnation with liquid cosmetics and uneven drainage of the liquid cosmetics after impregnation. The pore size is one of the important factors in impregnating liquid cosmetics. Preferably, when the appropriate pore size for processing into impregnating liquid cosmetics has an average pore size of 900–1100 μm, and the number of pores formed meets the requirement of 60–80 ppi, it tends to exhibit excellent impregnation capacity, filling capacity, and drainage capacity of the liquid cosmetic.
[0032] Furthermore, preferably, the elastic modulus of the foam is 40% to 45%, because it makes the foam easy to return to its initial state after being compressed.
[0033] In addition, foams used for impregnation in liquid cosmetics need to ensure an appropriate compressive strain rate, preferably 30% to 40%, because they can provide a soft touch when used.
[0034] On the other hand, in order to impregnate liquid cosmetics, it is necessary to ensure appropriate density and hardness, tensile strength and absorption rate, preferably ensuring a density of 40-45 kg / m³. 3 It has physical properties such as a hardness of 75-80°, a tensile strength of 220-230 kPa, and an absorption rate of 300%-400%, which is because it is easy to impregnate large amounts of cosmetics.
[0035] According to the present invention, the foaming agent can be any commonly used foaming agent, as long as it is used for foaming synthetic resins. However, more preferably, it is preferable to use any one selected from HCFC-141b, HCFC-142b, and HCF-22, so that the foam of the final product ensures excellent physical properties for impregnating liquid cosmetics and for uniformly dispersing the raw materials without tangling. HCFC-141b is preferred.
[0036] According to the present invention, the catalyst functions to uniformly form pores in the foam by generating bubbles. It is selected from any one of TEDA, DETDA, 33lv, A-1, A-99, and TEOA, with TEDA being the most preferred. Furthermore, the surfactant is added to prevent the formation of large and defective bubbles; it is preferably selected from any one of AK8818, AK8803, and AK8806. AK8818 is even more preferred.
[0037] According to the manufacturing method of the present invention as described above, a foam for liquid cosmetic impregnation can be provided, which has an average pore size of 900-1100 μm, a pore number of 60-80 ppi (pores / inch), and a density of 40-45 kg / m³. 3Physical properties include a resilient modulus of 40%–45%, a compressive strain rate of 30%–40%, a hardness of 75–80°, a tensile strength of 220–230 kPa, and an absorption rate of 300%–400%.
[0038] [Examples 1 and 2] 1) Preparation of polyester polyol: Place the polyester polyol in the chamber, exhaust it at a temperature of 55-65°C, and let it stand for 60 minutes under a pressure of 0.1-0.2 kPa. Then lower the temperature to 25-35°C, supply nitrogen, and let it stand for 48 hours under an internal pressure of 2-3 kPa to prepare the polyester polyol.
[0039] 2) Preparation of polyether polyol: Place the polyether polyol in the chamber and let it stand for 60 minutes at a temperature of 15-25°C and a pressure of 0.1-0.2 kPa. Then supply nitrogen and let it stand for 48 hours at a pressure of 2-3 kPa to prepare the polyether polyol.
[0040] 3) Prepare other additives: According to the required dosage, inject the foaming agent, catalyst and surfactant into the tank for later use.
[0041] 4) Foaming and molding: The prepared polyester polyol and polyether polyol, foaming agent, catalyst and surfactant are added to the mixing tank in sequence according to appropriate mixing conditions. The mixture is stirred at 5000 rpm / min under the conditions of 22-24℃ and 3kPa pressure in the tank, and continuous foaming is carried out at the same time. The resulting foam is then aged for 48 hours, and the foam is cut into a size that can be used to impregnate liquid cosmetics for productization.
[0042] At this time, the polyester polyol and polyether polyol are added to a weight ratio of 3:7 (Example 1) and 4:6 (Example 2). For the foaming agent, catalyst and surfactant, relative to 100 parts by weight of the mixture of polyester polyol and polyether polyol, 0.3 parts by weight of foaming agent, 0.3 parts by weight of catalyst and 3 parts by weight of surfactant are added and mixed before the foaming process is carried out. D19 is used as the foaming agent, A230 is used as the catalyst and SL9205 is used as the surfactant.
[0043] [Compare Examples 1 and 2] Foams made using polyester polyol alone (Comparative Example 1) and foams made using polyether polyol alone (Comparative Example 2) were prepared.
[0044] The physical properties of the foams prepared according to the disclosed embodiments and comparative examples were compared, and the results are shown in Table 1 below.
[0045] Table 1 In Table 1 above, pore size and pore number are measured using the WI-QA-14 (ASTM standard) method, while the absorption rate is calculated as follows: For the manufactured foam, a sample of 3 cm × 3 cm is prepared and dried in a 70°C oven for 24 hours, at which point the initial weight (A) is measured. After immersion in distilled water at 25°C for 48 hours, the sample is removed, the surface moisture is wiped off with a lint-free paper towel, and the weight is measured again (B). Finally, the calculation is performed using Equation 1 below.
[0046] (Equation 1) Absorption rate (%) = (BA) / A × 100 Furthermore, hydrolysis resistance was measured using the so-called Jungle Test (ASTM D-6860), and the results are shown in Table 2 below. Oil resistance was measured using the Jungle Test (ASTM D-6860), and the results are shown in Table 3 below.
[0047] <Experimental Methods> T: 60℃ R / H: 98% Exposure time (days): 15 days Table 2 ×: No deformation △: Deformation begins ○: Deformation ends Table 3 ×: No deformation △: Deformation begins ○: Deformation ends As shown in Tables 1 to 3 above, the results of hydrolysis resistance and oil resistance indicate that traditional ether-based foams composed of a single component are water-resistant but not oil-resistant, while ester-based foams are oil-resistant but not water-resistant. Therefore, they cannot be used for a long time and have the disadvantage of short lifespan. However, the present invention improves both water resistance and oil resistance.
[0048] As shown in Table 1 above, the method for manufacturing foam for liquid cosmetic impregnation provided in this invention can provide foam with excellent physical properties. Specifically, the foam provided according to this invention has uniform pore size and excellent fluffiness, softness, flexibility, and elasticity. Furthermore, it exhibits excellent filling capacity for liquid cosmetics, outstanding impregnation ability for long-term uniform impregnation of liquid cosmetics, high discharge capacity for discharging an appropriate amount of liquid cosmetics when dispensing, and maintains excellent durability even after impregnation with liquid cosmetics.
[0049] In particular, due to its high absorption rate, it can soak a large amount of cosmetics and has the advantage of easily soaking cosmetics.
[0050] The following reference Figure 1 Briefly describe how to use foam for impregnating liquid cosmetics.
[0051] Figure 1 This is an exploded perspective view of a traditional cosmetic box with foam material for impregnating liquid cosmetics.
[0052] like Figure 1 As shown, the cosmetic box includes: a cosmetic container 4 having a liquid cosmetic impregnation foam body receiving portion 5; a liquid cosmetic impregnation foam body 1 placed and received in the liquid cosmetic impregnation foam body receiving portion 5 and impregnated with cosmetics; a powder puff receiving portion 3 hinged to the cosmetic container 4; and a powder puff 2 received in the powder puff receiving portion 3. When the user takes out the powder puff 2 received in the powder puff receiving portion 3 and wears it on their hand, the powder puff receiving portion 3 is opened to expose the liquid cosmetic impregnation foam body 1 to the outside. Then, the powder puff 2 is pressed against the surface of the liquid cosmetic impregnation foam body 1, causing the cosmetics impregnated in the liquid cosmetic impregnation foam body 1 to be squeezed out and adhered to the powder puff 2, and then makeup is applied.
[0053] Figure 2 This is a flowchart describing the test method used in the manufacturing method of the liquid cosmetic impregnation foam of the present invention.
[0054] like Figure 2 As shown, a testing method for a foam for impregnating liquid cosmetics according to an embodiment of the present invention may include: step S110: manufacturing a foam for impregnating liquid cosmetics capable of being used to impregnate liquid or solid cosmetic compositions; step S120: performing an FT-IR test on the manufactured foam for impregnating liquid cosmetics; step S130: determining whether the FT-IR test result value is within a specific proportional range that provides a balance between the hydrolysis resistance, water resistance, and oil resistance of the foam for impregnating liquid cosmetics; and step S140: if the FT-IR test result value is within the specific proportional range, performing a solid-state NMR test.
[0055] More specifically, a testing method for a liquid cosmetic impregnation foam according to an embodiment of the present invention may include: step S110: manufacturing a liquid cosmetic impregnation foam capable of impregnating liquid or solid cosmetic compositions (such as solutions, emulsions, gels, creams, or suspensions); step S120: measuring the ratio of ester to ether in the manufactured liquid cosmetic impregnation foam using an FT-IR testing device with absorbance as a reference via an infrared spectrometer; step S130: determining whether the ratio of ester to ether is a specific ratio that provides a balance of hydrolysis resistance, water resistance, and oil resistance for the liquid cosmetic impregnation foam; step S140: if the ratio of ester to ether is not a specific ratio, then it is deemed unqualified; if the ratio of ester to ether is a specific ratio, then a solid-state NMR test is performed; step S150: determining, through the solid-state NMR test, whether there is a tendency based on PPM in a specific segment.
[0056] In step S150, if the solid-state NMR test determines whether there is a tendency based on the PPM of a specific segment, and the solid-state NMR test determines that there is no tendency based on the PPM of the specific segment, then the product is deemed unqualified. Only if there is a tendency is the product deemed qualified and the product is released. This ensures a reliable balance between the hydrolysis resistance, water resistance, and oil resistance of the foam for liquid cosmetic impregnation.
[0057] In the test method of the liquid cosmetic impregnation foam of the present invention, step S110 of manufacturing the liquid cosmetic impregnation foam may include: step a: placing polyester polyol in a chamber, venting at a temperature of 55-65°C, and standing for 60 minutes under a pressure of 0.1-0.2 kPa, then lowering the temperature to 25-35°C, supplying nitrogen, and standing for 48 hours under a pressure of 2-3 kPa to prepare polyester polyol; step b: placing polyether polyol in a chamber, standing for 60 minutes at a temperature of 15-25°C and a pressure of 0.1-0.2 kPa, then supplying nitrogen, and standing for 48 hours under a pressure of 2-3 kPa. a) Let it stand for 48 hours under atmospheric pressure to prepare polyether polyol; c) According to the required amount, inject the foaming agent, catalyst and surfactant into the tank for later use; d) Add the polyester polyol and polyether polyol, foaming agent, catalyst and surfactant into the mixing tank in the specified ratio, stir at 5000 rpm / min under the conditions of 22-24℃ and 3kPa pressure, and then put it into the mold for continuous foaming; e) Aging the foam formed after the foaming step for 48 hours; and f) Cut the foam for productization, which may include the step of preparing samples.
[0058] For the test method of the liquid cosmetic impregnation foam of the present invention, it is very important to verify whether the polyester polyol and polyether polyol in the liquid cosmetic impregnation foam have a weight ratio of 3:7 to 4:6.
[0059] The weight ratio of polyester polyol to polyether polyol of 3:7 to 4:6 was verified to be related to the chemical composition of the main components of the polymer chain and the physical properties of the polymer chain, such as crystallinity, melting point, and charge.
[0060] Therefore, the testing method for the liquid cosmetic impregnation foam of the present invention includes step S120, which involves measuring the ratio of ester to ether using an infrared spectrometer with absorbance as a reference on an FT-IR testing device for the liquid cosmetic impregnation foam manufactured as described above.
[0061] In other words, the FT-IR test step S120 uses a spectrophotometer to measure the spectral information of the manufactured liquid cosmetic impregnation foam sample. The spectrophotometer can be a Fourier transform infrared spectrophotometer (product name: TENSOR27, Bruker).
[0062] Using wavenumbers of 4000 to 400 cm and a resolution of 4 cm. -1 The analysis was performed using analysis software (product name: OPUS 7.0). In the specific ratio A / B, A represents the C=O stretching vibration of the ester, and B represents the bending vibration of NH.
[0063] In the spectrophotometer, as shown in Tables 4 and 5, when the ether is 100%, the specific ratio is ~0.45; when the ether to ester ratio is 7:3, the specific ratio is 0.90 to 0.94; and when the ether to ester ratio is 5:5, the specific ratio is 0.96 to 1.07.
[0064] Table 4 Table 5 Figure 3 This is a graph showing the spectral analysis information of foam used for impregnation in liquid cosmetics.
[0065] like Figure 3 As shown, for spectral information, wavenumber information is represented by the x-axis, and the spectral intensity corresponding to the absorption rate is represented by the y-axis. A peak is observed at a specific wavenumber, and the characteristics of the polymer corresponding to that peak can be analyzed.
[0066] In the data measurement method, a liquid cosmetic impregnation foam with an ether to ester ratio of 7:3 was used.
[0067] Analysis was performed using OPUS software, as shown in Table 6. The measured values were recorded at the C=O stretching vibration peak of the ester (i.e., 1710 to 1730 cm⁻¹). -1 It exhibits the highest wavenumber and intensity near NH bending vibration peak (i.e., 1530 to 1540 cm⁻¹), and records the peak intensity at NH bending vibration peak (i.e., 1530 to 1540 cm⁻¹). -1 The wave number and intensity (B) exhibit maximum intensity near the vicinity of ).
[0068] Table 6 Calculate the proportion of the confirmed C=O stretching vibration peak and NH bending vibration peak in each data point. After calculating the proportion for each data point, list the minimum and maximum values. Then exclude the minimum value of 10% and the maximum value of 10% to calculate the average value. When the results of the confirmed range rounded to three decimal places are shown, the value in Table 6 is 0.928.
[0069] Therefore, in step S130, which determines whether the ratio of ester to ether is a specific ratio that provides a balance of hydrolysis resistance, water resistance and oil resistance for foam used in liquid cosmetic impregnation, the numerical range is 0.90 to 0.94 when the ratio of ether to ester in the FT-IR test in Table 4 is 7:3, and the result value in Table 6 is 0.928, indicating that the numerical range is met.
[0070] The FR-IR analysis results are shown in Table 7.
[0071] Table 7 If the ratio of the ester to the ether is not a specific ratio, it is considered unqualified; if the ratio of the ester to the ether meets the specific ratio, the solid NMR test step S140 is performed.
[0072] Generally, nuclear magnetic resonance (NMR) spectroscopy offers atomic-level resolution, revealing structural and dynamic details of polymers, and has therefore played a crucial role in polymer research for a long time. The most significant advantage of NMR spectroscopy is its ability to perform quantitative analysis with minimal pretreatment; however, the equipment is expensive, increasing costs. Nevertheless, for liquid cosmetic impregnation foams that pass FT-IR tests in a single run, solid-state NMR testing can reduce costs.
[0073] The solid-state NMR test (S140) was designed to analyze tropism by confirming the ester polyol-derived peaks.
[0074] The solid-state NMR test (S140) was performed using an instrument called AVANCE Ⅲ HD (Bruker GmbH, Germany) and software TopSpin3X.
[0075] Figure 4 This is a view showing the solid NMR test results of a foam for liquid cosmetic impregnation according to an embodiment of the present invention.
[0076] like Figure 4 As shown, for the C peak of ester polyol, depending on the polyol, it can be observed at 12 ppm to 20 ppm or 60 to 80 ppm. Although other situations may exist, repeated experimental results show that when the weight ratio of polyester polyol to polyether polyol is 3:7 to 4:6, there is an almost certain tendency in the 60 to 80 ppm range. Therefore, the 60 to 80 ppm range is set as the directional analysis range, and the directionality of this range is determined.
[0077] Therefore, step S150, which uses the solid-state NMR test to determine whether there is a tendency based on PPM in a specific range, is to determine whether there is a tendency in the 60 to 80 ppm range within the error range. If there is a similar tendency within the error range, it is accepted; if there is a tendency outside the error range, it is rejected or unsuitable.
[0078] As described above, the present invention has been described in detail with reference to specific constituent elements, embodiments, and accompanying drawings. However, these descriptions are only intended to help to understand the present invention more fully. The present invention is not limited to the embodiments described above, and those skilled in the art can make various modifications and variations based on these descriptions.
[0079] Therefore, the ideas of this invention should not be limited to the described embodiments, and all the claims and their equivalents or variations fall within the scope of this invention.
Claims
1. A method for manufacturing a foam for impregnation in liquid cosmetics, characterized in that, include: Step a: Place the polyester polyol into the chamber, exhaust the gas at a temperature of 55-65°C, and let it stand for 60 minutes under a pressure of 0.1-0.2 kPa. Then lower the temperature to 25-35°C, supply nitrogen, and let it stand for 48 hours under a pressure of 2-3 kPa to prepare the polyester polyol. Step b: Place the polyether polyol into the chamber and let it stand for 60 minutes at a temperature of 15-25°C and a pressure of 0.1-0.2 kPa. Then supply nitrogen and let it stand for 48 hours at a pressure of 2-3 kPa to prepare the polyether polyol. Step c: According to the required dosage, inject the foaming agent, catalyst and surfactant into the tank for later use; Step d: The polyester polyol, polyether polyol, foaming agent, catalyst and surfactant are added to the mixing tank in sequence according to the ratio, and the mixture is stirred at 5000 rpm / min under the conditions of 22-24℃ and 3kPa pressure, while continuous foaming is carried out. Step e: Aging the foam formed after step d for 48 hours; as well as Step f: Cut the foam body for productization. In the method for manufacturing liquid cosmetic impregnation foam in a mixing ratio of polyester polyol and polyether polyol of either 3:7 or 4:6, Further, it includes a test step for the foam used for impregnating the liquid cosmetic. The testing steps for the foam for impregnation in liquid cosmetics include the following steps: preparing a sample of the foam for impregnation in liquid cosmetics that can be used to impregnate liquid or solid cosmetic compositions; performing an FT-IR test on the manufactured foam for impregnation in liquid cosmetics; determining whether the FT-IR test result value is within a specific proportional range that provides a balance between the hydrolysis resistance, water resistance, and oil resistance of the foam for impregnation in liquid cosmetics; and if the FT-IR test result value is within the specific proportional range, performing a solid-state NMR test.
2. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 1, characterized in that, The FT-IR testing procedure includes the following steps: preparing a sample of the manufactured liquid cosmetic impregnation foam; measuring the ester ratio using an infrared spectrometer based on the absorbance; and treating the ester ratio as non-compliant if it is not a specific ratio.
3. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 2, characterized in that, In the ester ratio, the specific ratio of 0.90 to 0.94 when the ether to ester ratio is 7:3 and the specific ratio of 0.96 to 1.07 when the ether to ester ratio is 5:5 are the reference values.
4. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 3, characterized in that, For the step of calculating the ester ratio, the measured values (A) are recorded at the C=O stretching vibration peak of the ester, i.e., from 1710 to 1730 cm⁻¹. -1 The wavenumber and intensity are highest in the vicinity, and are recorded at the NH bending vibration peak, i.e., 1530 to 1540 cm⁻¹. -1 The wavenumber and intensity (B) of the ester C=O stretching vibration peak and NH bending vibration peak (A / B) are then calculated. The minimum and maximum values are listed, and then the minimum and maximum values are excluded by 10% to calculate the average value, which is rounded to three decimal places.
5. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 1, characterized in that, For the solid NMR test procedure, it is determined whether there is a tendency based on PPM in a specific segment, so as to determine whether the foam for liquid cosmetic impregnation provides a balance of hydrolysis resistance, water resistance and oil resistance.
6. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 5, characterized in that, For the step of determining directionality based on PPM of a specific segment, when the weight ratio of polyester polyol and polyether polyol in the liquid cosmetic impregnation foam is 3:7 to 4:6, the 60 to 80 ppm segment is taken as the directionality analysis segment.
7. The method for manufacturing a foam for impregnation in liquid cosmetics according to claim 6, characterized in that, For the step of determining whether there is a tendency by using the solid-state NMR test as a reference for a specific range of PPM, if there is a tendency in the 60 to 80 ppm range within the error range, it is accepted; if it shows a tendency outside the error range, it is rejected or unsuitable.
8. A foam for impregnating liquid cosmetics, manufactured by the manufacturing method according to any one of claims 1 to 7, characterized in that: The mixing ratio of polyester polyol and polyether polyol is either 3:7 or 4:
6.
9. The foam body for impregnation in liquid cosmetics according to claim 8, characterized in that: The foam has an average pore size of 900–1100 μm, a pore number of 60–80 ppi (pores / inch), and a density of 40–45 kg / m³. 3 The elastic modulus is 40%–45%, the compressive strain rate is 30%–40%, the hardness is 75–80°, the tensile strength is 220–230 kPa, and the absorption rate is 300%–400%.
Citation Information
Patent Citations
The product method and foaming matter to absorb oil
KR100725240B1
Supporting material of cosmetic composition containing foamed material
KR1020130116205A