Delayed disintegration-type capsule and method for producing same

By integrating an amphoteric surfactant and specific melting point fats into the capsule core, the disintegration of seamless capsules is delayed and pH-independent, addressing design limitations and ensuring targeted delivery.

CA3139731CActive Publication Date: 2026-07-07MORISHITA JINTAN CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CA3139731
Authority / Receiving Office
CA · CA
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-06-14
Filing Date
2020-06-12
Publication Date
2026-07-07
Estimated Expiration
2040-06-12

AI Technical Summary

Technical Problem

Existing seamless capsules lack the ability to effectively delay disintegration and offer limited design freedom due to the reliance on film layers that are sensitive to pH changes in the gastrointestinal tract.

Method used

Incorporating an amphoteric surfactant, such as lecithin, into the core of the capsule, combined with fats having specific melting points and a water-soluble natural polymer outermost layer, allows for controlled disintegration independent of pH changes.

Benefits of technology

This approach enables delayed disintegration and enhanced design flexibility, allowing the capsule to maintain integrity through the stomach and small intestine before disintegrating in the large intestine, thus ensuring targeted delivery of active substances.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

An object of the present invention is to provide a technique for delaying disintegration of a capsule by blending a certain component in a core of the capsule, and to increase the degree of freedom in capsule design. The present invention relates to a delayed disintegration-type seamless capsule that is a seamless capsule including a core, one or more intermediate layers formed on the core, and an outermost layer formed on the intermediate layers, wherein the core contains an active substance, an amphoteric surfactant, and a fat having a melting point of 40C or more, at least one layer of the intermediate layers contains a fat having a melting point of 45C or more, and the outermost layer contains a water-soluble natural polymer. The present invention also relates to a method for producing the same.
Need to check novelty before this filing date? Find Prior Art