A crystal growth device

By using a liftable heating hood mechanism and a gas source box in the crystal growth apparatus, the instability and dissociation problems in the crystal growth process of volatile elements were solved, thereby improving the stability of crystal growth and the yield.

CN112695376BActive Publication Date: 2024-11-01THE 13TH RES INST OF CHINA ELECTRONICS TECH GRP CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110145355.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-02-03
Publication Date
2024-11-01
Estimated Expiration
2041-02-03

AI Technical Summary

Technical Problem

Existing Czochralski crystal growth equipment suffers from problems such as unstable crystal growth, polycrystalline formation, severe dissociation, and inaccurate temperature gradient control when growing crystals of volatile elements. In particular, instability is prone to occur during the crystal pulling and shoulder formation stages, resulting in low crystal yield.

Method used

A liftable heating hood mechanism is adopted to cover the crystal but not the melt. The heating hood keeps the crystal warm, and the gas source box provides an atmosphere of volatile elements to suppress crystal dissociation, maintain a stable temperature gradient in the melt, and reduce internal stress and defects in the crystal.

Benefits of technology

This approach achieves improved stability and yield in the crystal growth process, avoids crystal polymorphism and dissociation, and ensures high-quality crystal growth.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112695376B_ABST
    Figure CN112695376B_ABST
Patent Text Reader

Abstract

A crystal growth device relates to the field of crystal preparation, and in particular to a device for preparing low-stress, low-defect crystals using a Czochralski method. The device comprises a furnace body, a crucible and a heating and heat-insulating system placed at the bottom of the furnace body, a crystal pulling mechanism, and a quartz observation window. The device also comprises a liftable heating cover mechanism, including a heating cover body, a heating cover support component, heating wires arranged around the heating cover body, and a heating cover lifting mechanism. The device can reduce the stress in the crystal during the crystal growth process and during the cooling process after the crystal is lifted, reduce defects, and avoid crystal cracking. At the same time, the temperature gradient in the melt is maintained to ensure the stability of the crystal growth process, thereby ensuring the crystal yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of crystal preparation, and in particular to a device for preparing low-stress and low-defect crystals by using a Czochralski method. Background Art

[0002] The Czochralski method is a method of growing crystals from a melt. It is a common growth method for semiconductor crystals, optical crystals, etc. This method has the characteristics of high yield, fast growth rate, and easy observation.

[0003] The Czochralski method often uses a single heater growth method. Because the Czochralski method requires pulling the crystal out of the melt, especially when pulling it to a higher position, the first part of the crystal pulled out will cool down to a lower temperature due to the lower ambient temperature. The temperature at the solid-liquid interface of the crystal growth is always maintained near the melting point of the crystal. Therefore, assuming that the longitudinal temperature distribution in the crystal is linear, the gradient in the crystal is approximately equal to (Tjunction-Ttable) / L, L is the distance from the solid-liquid interface of the crystal growth to the crystal surface, Ttable is the crystal surface temperature, and Tjunction is the temperature at the solid-liquid interface of the crystal growth (approximately the melting point temperature of the crystal). In the steady-state growth process, Tjunction is approximately equal to the melting point temperature of the crystal, which is approximately a fixed value. The main way to reduce the crystal temperature gradient is to increase the crystal surface temperature Ttable. It is a common method to keep and heat the pulled crystal to increase the crystal surface temperature gradient.

[0004] At present, the mainstream method is to add a heat preservation cover and a post-heater above the crucible and the crystal. For example, Chinese patent application 201810509188.0 discloses a Czochralski CeAlO3 crystal growth device and its control method. Its technical solution is to set up two sets of fixed heating mechanisms, and heat the crucible and the pulled crystal respectively, and the heater and the upper cover cover the entire melt. However, although this method has a heat preservation effect on the crystal to a certain extent, it has major defects in practical applications. First, the overall coverage of the crucible body by the heater and the upper cover reduces the temperature gradient of the melt, which makes the crystal growth process easy to become unstable, the crystal has twins, and even polycrystallization. Especially in the early stages of crystal growth (seeding and shouldering stages), the crystal is in the central area of ​​the melt with a low temperature gradient, the growth is not stable, and the crystal is very easy to polycrystallize. Moreover, when this method is used to grow compound crystals containing volatile elements (such as indium phosphide, gallium arsenide, gallium phosphide, indium arsenide, indium antimonide, gallium antimonide, phosphorus germanium zinc, etc.), the post-heater heats the crystal, which will cause the crystal to dissociate, that is, the volatile elements evaporate into the atmosphere. If the degree of crystal dissociation is serious, the crystal will be unusable. Therefore, when using this thermal field to grow compound crystals of volatile elements, the power of the post-heater is limited.

[0005] Chinese patent application 200910112711.7 discloses a method and device for growing large-sized sodium yttrium tungstate crystals by a two-stage heating and pulling method. Two sets of fixed heating mechanisms are also provided to heat the crucible and the pulled crystals respectively. However, in this device, the upper part of the crystal is in an open state, the heat dissipation will be more serious, the heat preservation effect on the crystal is not strong, and the stress reduction effect is not obvious. Especially for crystals containing volatile elements, the dissociation phenomenon of the heated crystals will be very serious in a relatively open environment. For some materials with higher growth environment pressure, the high-pressure airflow will have a strong heat dissipation effect on the unsealed crystals, thereby reducing the heating effect of the post-heater.

[0006] Chinese patent application 201910631648.1 discloses a coil-movable temperature field structure and single crystal growth method suitable for the Czochralski method. The technical solution adopted is to set a post-heating cylinder above the crucible, and heat the crucible and the post-heating cylinder separately by moving the heating coil. This device uses an external mobile coil to heat the crucible and the post-heating cylinder at the same time. There is power interference between the two, and the control accuracy is not high. Crystal growth requires very high stability of the temperature in the crucible. The movement of the coil that heats the crucible will have a greater impact on the thermal field. Moreover, the heating cylinder is sensed at the same time and the coil power is shunted, which can easily cause large-scale fluctuations in the melt temperature gradient and lead to crystal growth failure. The relative position of the insulation cylinder and the crystal is far away, and the post-heating barrel heats the entire environment, which will reduce the temperature gradient of the entire environment, including the melt, and will also cause the crystal growth to have lower stability. Moreover, this coil device heats the melt and the crystal in the cooling process at the end of crystal growth, but has no obvious effect on the insulation and heating of the crystal during crystal growth, and has no obvious effect on the stress and dislocation defects caused by the temperature difference between the upper and lower ends of the crystal during crystal growth. Summary of the invention

[0007] The purpose of the present invention is to solve the problems existing in the prior art.

[0008] To this end, the present invention adopts the following technical means to achieve: a crystal growth device, including a furnace body, a crucible and a heating and heat preservation system placed at the bottom of the furnace body, a crystal pulling mechanism facing the center of the crucible, and a quartz observation window placed on the side of the furnace body, the heating and heat preservation system includes a crucible, a heater, a crucible rod, and an insulation sleeve, the crystal pulling mechanism includes a seed crystal rod and a seed crystal chuck, and the key is that the device also includes a liftable heating cover mechanism, the liftable heating cover mechanism includes a heating cover body, a heating cover support component, heating wires arranged around the heating cover body, and a heating cover lifting mechanism, and a thermocouple is arranged inside the heating cover body.

[0009] Furthermore, the heating cover is conical at the top and cylindrical at the bottom, and is made of transparent material, and the outer diameter of the cylinder is smaller than the inner diameter of the crucible.

[0010] Furthermore, the seed crystal rod passes through the heating cover body, and the heating cover lifting mechanism drives the liftable heating cover mechanism to move up and down along the seed crystal rod.

[0011] Furthermore, an air source box is also arranged inside the liftable heating cover mechanism.

[0012] With the above device, during the crystal growth stage, the heating cover descends to cover the growing crystal, forming a consistent temperature field around the crystal. Compared with the traditional two-stage temperature field, it has the following characteristics:

[0013] The coverage area varies.

[0014] In principle, the greater the melt temperature gradient, the higher the stability of crystal growth. Therefore, it is desirable to strengthen the melt temperature gradient to ensure smooth crystallization. The greater the temperature gradient inside the crystal, the greater the thermal stress inside the crystal. Therefore, it is desirable to have a small temperature gradient inside the crystal. The traditional two-stage temperature field often covers the entire crucible body, which reduces both the crystal temperature gradient and the melt temperature gradient. Although it can play a certain role in reducing stress, it also causes the crystal growth process to become unstable, and the crystals may become twinned or even polycrystalline. The present invention utilizes a heating hood that matches the crystal diameter to insulate the crystal without covering the melt. Therefore, the temperature gradient inside the melt will not be significantly reduced, and smooth crystal growth can be ensured.

[0015] The time periods covered vary.

[0016] During the seeding and shouldering stage, the crystal is in the center of the melt, and the radial temperature gradient of the melt surface in the center area of ​​the crucible is small. Therefore, during the seeding and shouldering process, the smaller crystal is more likely to become unstable, resulting in polycrystallization. The traditional non-movable two-stage thermal field covers the crucible throughout the entire process, and the melt temperature gradient is small, which leads to polycrystallization during the seeding and shouldering process.

[0017] By adopting this device, the temperature gradient inside the crystal can be reduced during the crystal growth process and the cooling process after the crystal is lifted, thereby reducing the stress inside the crystal, reducing defects, and avoiding crystal cracking. At the same time, the temperature gradient in the melt is maintained to ensure the stability of the crystal growth process, thereby ensuring the crystal yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a structural schematic diagram of the present invention,

[0019] Figure 2 It is a working state diagram.

[0020] Figure 3 is another working state diagram,

[0021] Figure 4 It is the depth mark on the heating hood.

[0022] Figure 5 Another example of a depth mark on a heating hood.

[0023] Among them, there are seed crystal 1, seed crystal chuck 2, seed crystal rod 3, crystal 4, covering agent 5, melt 6, heater 7, heating hood 8, heating hood support component 9, heating hood lifting mechanism 10, quartz observation window 11, crucible rod 12, insulation sleeve 13, heating wire 14, gas source box fixing pin 15, gas source material 16, gas source box 17, crucible 18, furnace body 19, heating wire package 20, and thermocouple 21. DETAILED DESCRIPTION

[0024] The present invention will be further described below in conjunction with the accompanying drawings.

[0025] A crystal growth device, see Figure 1 , including a furnace body 19 , a crucible 18 and a heating and heat preservation system placed at the bottom of the furnace body 19 , a crystal pulling mechanism facing the center of the crucible, and a quartz observation window 11 placed on the side of the furnace body 19 .

[0026] The heating and heat preservation system comprises a heater 7 placed around the crucible 18 , a crucible rod 12 supporting the crucible 18 at the bottom, and a heat preservation sleeve 13 outside the heater 7 .

[0027] The crystal pulling mechanism comprises a seed crystal rod 3 and a seed crystal chuck 2 .

[0028] The device also includes a liftable heating cover mechanism, including a heating cover body 8, a heating cover support component 9, heating wires 14 arranged around the heating cover body 8, and a heating cover lifting mechanism 10. The heating cover lifting mechanism 10 completes the lifting and lowering of the heating cover body 8 through the heating cover support component 9. A thermocouple 21 is arranged inside the heating cover body 8 for obtaining the internal temperature thereof.

[0029] The heating cover 8 is conical at the top and cylindrical at the bottom, and is made of transparent materials such as quartz, glass or sapphire. The heat of the heating wire 14 can be radiated into the interior of the heating cover to heat the crystal. The outer part of the heating wire 14 is covered with a heating wire wrap 20, so that after the heating cover 8 is lowered, the crystal growth can still be observed through the cover.

[0030] The inner diameter of the heating hood 8 is 5-10 mm larger than the diameter of the desired pulled crystal, and its cylindrical outer diameter is smaller than the inner diameter of the crucible 18 , so it cannot have an overall covering effect on the crucible 18 .

[0031] The top of the heating cover 8 is a multi-layer hollow structure, forming multiple cavities, which has a certain heat preservation effect.

[0032] The heating cover mechanism is attached to the seed crystal rod 3 , and the seed crystal rod 3 passes through the heating cover body 8 . The heating cover lifting mechanism 10 drives the lifting heating cover mechanism to move up and down along the seed crystal rod 3 .

[0033] The top of the heating cover 8 holds the seed crystal rod 3 tightly, and a gap is left between the heating cover 8 and the seed crystal rod 3. The gap does not exceed 2 mm, connecting the inside of the heating cover 8 and the inside of the furnace body 19 to maintain basically the same pressure.

[0034] The liftable heating cover mechanism is also provided with an air source box 17, which is positioned at the inner upper end of the heating cover body 8 using an air source box fixing pin 15. The air source box fixing pins 15 are distributed radially along the heating cover body 8 in no less than 4 numbers to ensure that the air source box is firmly positioned.

[0035] In order to prevent the heating wire 14 from dipping into the covering agent 5 and the melt 6 , no heating wire is arranged at the bottom of the heating cover 8 . The starting position of the heating wire 14 is arranged upward from the bottom of the heating cover 8 , which is greater than 1 / 6 of the length of the heating cover 8 .

[0036] In order to facilitate observation, a depth marking line is set on the periphery of the heating cover 8 from the bottom, and the depth marking line adopts an inverted triangle shape, such as Figure 4 As shown, the depth of the heating cover 8 immersed in the covering agent 5 is intuitively represented, and the depth can also be represented by interval lines, such as Figure 5 shown.

[0037] The observation window 11 is made of transparent materials such as quartz, glass or sapphire, and is used to observe the crystal growth. After the liftable heating cover mechanism descends, the quartz observation window 11 is aligned with the set mark line.

[0038] The heating cover lifting mechanism 10 can fine-tune the heating cover body 8 up and down to ensure that when the liquid level of the covering agent 5 drops, the lower part of the heating cover body 8 is in continuous contact with the covering agent 5.

[0039] Working process:

[0040] The gas source material 16 is a volatile element material in the compound crystal. Phosphorus is used as the gas source material 16 for growing indium phosphide, gallium phosphide crystals, etc.; arsenic is used as the gas source material 16 for growing gallium arsenide crystals. The gas source material 16 is placed in a gas source box 17 and placed inside a heating cover 8. The covering agent 5 uses boron oxide.

[0041] Step 1: Place the raw material and the covering agent in the crucible 18, turn on the heater 7 for a period of time, and wait for the raw material and the covering agent 5 in the crucible 18 to melt. The covering agent 5 covers the raw material melt 6 because of its lower density than the raw material.

[0042] Step 2: Set the seed crystal 1 on the seed crystal chuck 2, and the crystal pulling mechanism descends until the seed crystal 1 contacts the surface of the melt 6. If the melt temperature is suitable for crystal growth, then after contact, the contact position between the seed crystal 1 and the melt 6 will gradually grow and become a crystal 4.

[0043] Step 3: Observe the growth of the crystal 4 at the contact position between the seed crystal 1 and the melt 6 through the quartz observation window 11, and adjust the power of the heater 7 according to the expansion / contraction of the crystal 4, so that the crystal 4 gradually grows. In the process of gradual growth of the crystal, gradually change the pulling speed of the pulling mechanism.

[0044] Step 4: When the crystal 4 grows to the required diameter, turn on the power of the heating wire 14 and lower the heating cover mechanism so that the bottom of the heating cover body 8 contacts the covering agent 5. The outer part of the heating wire 14 is covered with the heating wire wrap 20, and the position near the observation window 11 is not covered, leaving the observation window, such as Figure 2 shown.

[0045] The above "required diameter" is the standard wafer size + about 5mm. For example, if the target diameter is 2 inches, the required diameter is 55.8mm; if the target diameter is 3 inches, the required diameter is 81.2mm; if the target diameter is 4 inches, the required diameter is 105mm; if the target diameter is 6 inches, the required diameter is 155mm.

[0046] Step 5: gradually increase the heating power of the heating wire 14 to significantly increase the temperature of the atmosphere in the heating cover. The temperature range is determined according to the gas source element. If the gas source element is phosphorus, it is raised to 500-600°C to allow the gas source to start evaporating gas to ensure the partial pressure of the gas source element atmosphere in the heating cover body 8. Continue heating to maintain the temperature in the heating cover body 8. The temperature is determined according to the thermocouple 21.

[0047] There is a small gap between the heating cover 8 and the seed crystal rod 3. The gas pressure inside and outside the heating cover 8 is the same, but the partial pressure of the gas source element inside the heating cover 8 is relatively high, which can play a role in inhibiting crystal dissociation.

[0048] The furnace body 19 contains an inert gas, such as nitrogen, argon, etc., but the inert gas has limited effect on crystal dissociation. Only the partial pressure of the corresponding gas element has the effect of inhibiting dissociation. Therefore, a gas source material 16 is used to provide the partial pressure of the element gas around the crystal to limit the escape of the element from the crystal surface.

[0049] Step 6. As the crystal 4 gradually grows and is pulled, the liquid levels of the melt 6 and the covering agent 5 gradually drop. Therefore, the heating cover mechanism also needs to be gradually lowered as the liquid level drops. Observe through the observation window 11 and adjust the position according to the marking line to ensure that the heating cover body 8 is in contact with the boron oxide of the covering agent 5, while avoiding the heating wire 14 from dipping into the covering agent 5.

[0050] Step 7: The crystal 4 is pulled to a position where the weight is sufficient, and the crystal pulling mechanism and the liftable heating cover mechanism are quickly pulled to lift the crystal 4 out of the melt 6 and the boron oxide 5. Figure 3 shown.

[0051] Step 8: The heater 7 is set to a cooling program, and the temperature will reach room temperature in 5-20 hours; the heating wire 14 is turned on to cool the temperature, and the temperature will reach room temperature in 5-20 hours.

[0052] Step 9: Dismantle the furnace and remove the crystal.

Claims

1. A crystal growth device, comprising a furnace body (19), a crucible (18) and a heating and heat preservation system arranged at the bottom of the furnace body (19), a crystal lifting mechanism facing the center of the crucible (18), and a quartz observation window (11) arranged on the side of the furnace body (19), the heating and heat preservation system comprising a heater (7), a crucible rod (12), and a heat preservation sleeve (13), the crystal lifting mechanism comprising a seed crystal rod (3), and a seed crystal chuck (2), characterized in that: The device further comprises a liftable heating cover mechanism, the liftable heating cover mechanism comprising a heating cover body (8), a heating cover support component (9), heating wires (14) arranged around the heating cover body (8), and a heating cover lifting mechanism (10), wherein a thermocouple (21) is arranged inside the heating cover body (8); an air source box (17) is also arranged inside the liftable heating cover mechanism, the air source box (17) is positioned at the upper end of the interior of the heating cover body (8) using an air source box fixing pin (15), and the air source box (17) has an air source material (16) built in. The heating cover (8) is conical at the top and cylindrical at the bottom, and is made of transparent material, and the outer diameter of the cylinder is smaller than the inner diameter of the crucible (18); The seed crystal rod (3) passes through the heating cover body (8), and the heating cover lifting mechanism (10) drives the liftable heating cover mechanism to move up and down along the seed crystal rod (3); The gap between the seed crystal rod (3) and the top of the heating cover (8) does not exceed 2 mm.

2. The crystal growth device according to claim 1, characterized in that: The top of the heating cover (8) is a multi-layer hollow structure.

3. The crystal growth device according to claim 1, characterized in that: The starting position of the heating wire (14) is set upward from the bottom of the heating cover (8) and is greater than 1 / 6 of the length of the heating cover (8).

4. The crystal growth device according to claim 1, characterized in that: The outer periphery of the heating hood (8) is provided with depth markings starting from the bottom.

5. The crystal growth device according to claim 4, characterized in that: After the liftable heating cover mechanism is lowered, the quartz observation window (11) is aligned with the set marking line.