Stainless steel composite panels and batteries

Through the design of stainless steel composite panels, including multi-layer bonding and insulation structures, the problem of poor sealing of button batteries is solved, the processing efficiency and the stability of the battery casing are improved, and a more efficient battery manufacturing process is achieved.

CN113131050BActive Publication Date: 2024-10-11HEFEI GUOYAN NEW ENERGY IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110485344.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-04-30
Publication Date
2024-10-11
Estimated Expiration
2041-04-30

AI Technical Summary

Technical Problem

The sealing effect of existing button batteries is poor, resulting in leakage problems, and the installation of the insulating film is difficult, which reduces processing efficiency.

Method used

A stainless steel composite plate is used, including a first stainless steel layer, a first adhesive layer, an anti-conduction layer, a second adhesive layer and a second stainless steel layer. The sealing and insulation of the battery case are achieved through these layers of adhesive and insulating materials. connection to improve processing efficiency.

Benefits of technology

It improves the sealing and processing efficiency of the battery case, reduces the processing difficulty of the battery case, prevents electrolyte leakage and external moisture penetration, and enhances the structural stability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113131050B_ABST
    Figure CN113131050B_ABST
Patent Text Reader

Abstract

The invention discloses a stainless steel composite plate and a battery. The stainless steel composite plate at least comprises a first stainless steel layer, a first bonding layer, an anti-conduction layer, a second bonding layer and a second stainless steel layer in sequence; the thickness d1 of the first stainless steel layer is 0.1 mm-5 mm; the thickness d2 of the first bonding layer is 0.05 mm-10 mm; the thickness d3 of the anti-conduction layer is 0.05 mm-5 mm; the thickness d4 of the second bonding layer is 0.05 mm-10 mm; the thickness d5 of the second stainless steel layer is 0.1 mm-5 mm; the melting temperature of the first bonding layer is lower than the melting temperature of the anti-conduction layer, and the melting temperature of the second bonding layer is lower than the melting temperature of the anti-conduction layer; before the battery shell is sealed, the first bonding layer and the second bonding layer are melted at a temperature greater than or equal to 100° C. and lower than the melting temperature of the anti-conduction layer, respectively, and the bonding strengths between the first bonding layer and the second stainless steel layer at cooling room temperature are both greater than or equal to 1.0 N per square millimeter.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of batteries, and in particular to a stainless steel composite plate and a battery. Background Art

[0002] In the existing button battery, the battery shell is formed by splicing the positive electrode shell, the negative electrode shell and the insulating plastic sleeve. The positive electrode shell and the negative electrode shell need to be insulated to avoid short circuit of the button battery. The related technology achieves insulation by setting an insulating film between the positive electrode shell and the negative electrode shell. In the related production process, the insulating plastic sleeve is squeezed between the positive electrode shell and the negative electrode shell to complete the sealing of the entire shell, and the positive electrode shell and the negative electrode shell are welded and fixed. During the processing, since the existing shell packaging only relies on the squeezing of the positive electrode shell and the negative electrode shell, this leads to poor sealing effect, resulting in leakage of a large number of button batteries. The setting of the insulating film is difficult, which makes the processing of the button battery difficult and reduces the processing efficiency. Summary of the invention

[0003] The main purpose of the present invention is to propose a stainless steel composite plate for a battery housing, aiming to solve the technical problems of how to improve battery processing efficiency and poor sealing.

[0004] To achieve the above-mentioned purpose, the stainless steel composite plate proposed by the present invention comprises at least a first stainless steel layer, a first bonding layer, an anti-conduction layer, a second bonding layer and a second stainless steel layer in sequence;

[0005] The thickness d1 of the first stainless steel layer is 0.1 mm to 5 mm, and is used for electrically conducting with one of the electrodes of the battery cell inside the battery housing, and for preventing moisture outside the battery housing from penetrating into the housing;

[0006] The thickness d2 of the first bonding layer is 0.05 mm-10 mm, and is used to bond the first stainless steel layer and the anti-conduction layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing;

[0007] The thickness d3 of the anti-conduction layer is 0.05 mm-5 mm, which is used to prevent the first stainless steel layer from being electrically conductive with the second stainless steel layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing;

[0008] The thickness d4 of the second bonding layer is 0.05 mm to 10 mm, and is used to bond the second stainless steel layer and the anti-conduction layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing;

[0009] The thickness d5 of the second stainless steel layer is 0.1 mm to 5 mm, and is used for electrically conducting with the other electrode of the battery cell inside the battery housing, and for preventing moisture outside the battery housing from penetrating into the housing;

[0010] The melting temperature of the first adhesive layer is lower than the melting temperature of the conduction prevention layer, and the melting temperature of the second adhesive layer is lower than the melting temperature of the conduction prevention layer;

[0011] Before the battery shell is sealed, the first adhesive layer and the second adhesive layer are seamlessly bonded to the first stainless steel layer and the second stainless steel layer respectively when they melt at a temperature greater than or equal to 100°C and lower than the melting temperature of the anti-conduction layer, and the bonding strength between the first stainless steel layer and the second stainless steel layer at cooling room temperature is greater than or equal to 1.0N per square millimeter.

[0012] Optionally, the first stainless steel layer is made of SUS304, and / or the second stainless steel layer is made of SUS304.

[0013] Optionally, the first adhesive layer, the anti-conduction layer and the second adhesive layer are made of one or more of PP, PFA, PVDF, PTFE, ETFE and PVC.

[0014] Optionally, the bonding strength between the first bonding layer and the second bonding layer and the first stainless steel layer and the second stainless steel layer respectively at cooling room temperature is less than or equal to 5.0 N / mm.

[0015] Optionally, the first adhesive layer and the second adhesive layer melt at a temperature of 350° C. or less to be seamlessly bonded to the first stainless steel layer and the second stainless steel layer respectively.

[0016] Optionally, a first bonding enhancement layer is provided on the first surface of the first stainless steel layer close to the first bonding layer to strengthen the bonding strength between the first bonding layer and the first bonding layer; and / or a second bonding enhancement layer is provided on the second surface of the second stainless steel layer close to the second bonding layer to strengthen the bonding strength between the second bonding layer and the second bonding layer.

[0017] Optionally, the first bonding enhancement layer is a first surface layer of the first stainless steel layer close to the first bonding layer that is treated by sand blasting to form a uniform first rough surface layer; and / or the second bonding enhancement layer is a second surface layer of the second stainless steel layer close to the second bonding layer that is treated by sand blasting to form a uniform second rough surface layer.

[0018] Optionally, the first bonding enhancement layer is a first inclined sheet protruding from the first surface layer and having a certain inclination angle with the first surface layer, and the height h1 of the first inclined sheet is less than the thickness d2 of the first bonding layer; the second bonding enhancement layer is a second inclined sheet protruding from the second surface layer and having a certain inclination angle with the second surface layer, and the height h2 of the second inclined sheet is less than the thickness d4 of the second bonding layer.

[0019] Optionally, the first bonding enhancement layer is a first groove sunken into the first surface layer, and the sunken direction of the first groove is away from the direction of the first bonding layer; and / or the second bonding enhancement layer is a second groove sunken into the second surface layer, and the sunken direction of the second groove is away from the direction of the second bonding layer.

[0020] The present invention also proposes a battery, which includes a battery shell, wherein the battery shell is at least partially a stainless steel composite plate, and the stainless steel composite plate at least has a first stainless steel layer, a first bonding layer, an anti-conduction layer, a second bonding layer and a second stainless steel layer in sequence; the thickness d1 of the first stainless steel layer is 0.1mm-5mm, which is used for electrically conducting with one of the electrodes of the battery core inside the battery shell, and for preventing moisture outside the battery shell from penetrating into the shell; the thickness d2 of the first bonding layer is 0.05mm-10mm, which is used for bonding the first stainless steel layer and the anti-conduction layer, resisting electrolyte corrosion and preventing moisture outside the battery shell from penetrating into the shell; the thickness d3 of the anti-conduction layer is 0.05mm-5mm, which is used for preventing the first stainless steel layer from being electrically conductive with the second stainless steel layer, resisting electrolyte corrosion and preventing moisture outside the battery shell from penetrating into the shell; the thickness d4 of the second bonding layer is 0.05mm-10mm, which is used for bonding the second stainless steel layer and the anti-conduction layer The conductive layer is resistant to electrolyte corrosion and prevents moisture from outside the battery shell from penetrating into the shell; the thickness d5 of the second stainless steel layer is 0.1mm-5mm, which is used for electrical conduction with another electrode of the battery core inside the battery shell, and for preventing moisture from outside the battery shell from penetrating into the shell; the melting temperature of the first adhesive layer is lower than the melting temperature of the anti-conduction layer, and the melting temperature of the second adhesive layer is lower than the melting temperature of the anti-conduction layer; before the battery shell is sealed, the first adhesive layer and the second adhesive layer are seamlessly bonded to the first stainless steel layer and the second stainless steel layer respectively at a melting temperature greater than or equal to 100°C and lower than the melting temperature of the anti-conduction layer, and the bonding strength between the first stainless steel layer and the second stainless steel layer at cooling room temperature is greater than or equal to 1.0N per square millimeter; the battery shell contains at least a positive electrode, a negative electrode and an electrolyte battery element, the positive electrode is electrically conductive with the first stainless steel layer, and the negative electrode is electrically conductive with the second stainless steel layer;

[0021] The battery housing contains at least a battery element including a positive electrode, a negative electrode and an electrolyte. The positive electrode is electrically connected to the first stainless steel layer, and the negative electrode is electrically connected to the second stainless steel layer.

[0022] In the technical solution of the present invention, the first stainless steel layer is fixedly connected to one side of the anti-conduction layer by the first adhesive layer, and the second stainless steel layer is fixedly connected to the other side of the anti-conduction layer by the second adhesive layer, so that the first stainless steel layer and the second stainless steel layer can be connected and insulated from each other; after the stainless steel composite plate is manufactured, the first stainless steel layer and the second stainless steel layer can be further processed to form the shape of a battery shell, wherein the first stainless steel layer can form a positive electrode shell, and the second stainless steel layer can form a negative electrode shell, and the positive electrode shell and the negative electrode shell can be sealed and insulated by the first adhesive layer, the anti-conduction layer and the second adhesive layer, thereby reducing the processing difficulty of the battery shell and improving the processing efficiency of the battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0024] Figure 1 This is a schematic structural diagram of an embodiment of a stainless steel composite plate of the present invention;

[0025] Figure 2 It is a cross-sectional schematic diagram of an embodiment of a stainless steel composite plate of the present invention;

[0026] Figure 3 It is a cross-sectional schematic diagram of another embodiment of the stainless steel composite plate of the present invention;

[0027] Figure 4 It is a cross-sectional schematic diagram of another embodiment of the stainless steel composite plate of the present invention;

[0028] Figure 5 It is a cross-sectional schematic diagram of another embodiment of the stainless steel composite plate of the present invention;

[0029] Figure 6 FIG. 1 is a cross-sectional schematic diagram of an embodiment of a battery of the present invention.

[0030] Description of Figure Numbers:

[0031] Label name Label name Label name 10 First stainless steel layer 20 First bonding layer 30 Anti-conduction layer 40 Second adhesive layer 50 Second stainless steel layer 11 First bonding enhancement layer 51 Second bonding enhancement layer 111 First tilted piece 511 Second inclined piece 112 First groove 512 Second groove 60 positive electrode 70 negative electrode

[0032] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0035] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the meaning of "and / or" appearing in the full text is to include three parallel solutions, taking "A and / or B as an example", including solution A, or solution B, or solutions that satisfy both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in the field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0036] The invention provides a stainless steel composite plate for a battery casing.

[0037] In the embodiment of the present invention, Figures 1 to 5As shown, the stainless steel composite plate has at least a first stainless steel layer 10, a first adhesive layer 20, an anti-conduction layer 30, a second adhesive layer 40 and a second stainless steel layer 50 in sequence; the thickness d1 of the first stainless steel layer 10 is 0.1mm-5mm, which is used for electrically conducting with one of the electrodes of the battery cell inside the battery shell, and for preventing moisture outside the battery shell from penetrating into the shell; for specific examples, d1 can be 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.5mm, 1.0mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, 4.0mm, 4.5mm, 5.0mm. It should be understood that the specific stainless steel thickness can be specifically designed according to the specific product. For small button batteries, the preferred thickness d1 is 0.1mm-0.25mm, and for power batteries, electric vehicle batteries, etc., in order to ensure safety, the preferred thickness d1 is 1mm-3mm.

[0038] The thickness d2 of the first adhesive layer 20 is 0.05mm-10mm, which is used to bond the first stainless steel layer 10 and the anti-conduction layer 30, resist electrolyte corrosion and prevent moisture outside the battery shell from penetrating into the shell; for example, d2 can be 0.05mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.5mm, 1.0mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, 4.0mm, 4.5mm, 3.0mm, 4mm, 5.0mm, 6.0mm, 7.0mm, 8.0mm, 9.0mm, 10.0mm, it should be understood that the specific thickness of the first bonding layer can be specifically designed according to the specific product. For small button batteries, the preferred thickness d2 is 0.15mm-0.25mm, and for power batteries, electric vehicle batteries, etc., in order to ensure safety, the preferred thickness d2 is 1mm-5mm. In order to ensure that the first stainless steel layer 10 and the second stainless steel layer 50 can be firmly bonded and avoid contact short circuits between them, a relatively thick thickness is better. However, there is a certain amount of permeability in the first bonding layer, and it is also necessary to minimize the leakage.

[0039] The thickness d3 of the anti-conduction layer 30 is 0.05mm-5mm, which is used to prevent the first stainless steel layer 10 and the second stainless steel layer 50 from being electrically conductive, resisting corrosion by the electrolyte, and preventing moisture outside the battery shell from penetrating into the shell; the thickness d4 of the second adhesive layer 40 is 0.05mm-10mm, which is used to bond the second stainless steel layer 50 and the anti-conduction layer 30, resisting corrosion by the electrolyte, and preventing moisture outside the battery shell from penetrating into the shell; for specific examples, d4 can be 0.05mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.5mm, 1.0mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, 4.0mm, 4. 5mm, 3.0mm, 4mm, 5.0mm, 6.0mm, 7.0mm, 8.0mm, 9.0mm, 10.0mm. It should be understood that the specific thickness of the second bonding layer 40 can be specifically designed according to the specific product. For small button batteries, the preferred thickness d4 is 0.15mm-0.25mm. For power batteries, electric vehicle batteries, etc., in order to ensure safety, the preferred thickness d4 is 1mm-5mm. In order to ensure that the first stainless steel layer 10 and the second stainless steel layer 50 can be firmly bonded and avoid contact short circuits between them, a relatively thick thickness is better. However, there is a certain amount of permeability in the second bonding layer 40, and it is also necessary to minimize the leakage.

[0040] The thickness d5 of the second stainless steel layer 50 is 0.1mm-5mm, which is used for electrically conducting with the other electrode of the battery cell inside the battery shell and for preventing moisture from outside the battery shell from penetrating into the shell. To give a specific example, d5 can be 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.5mm, 1.0mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, 4.0mm, 4.5mm, 5.0mm. It should be understood that the specific thickness of the stainless steel can be specifically designed according to the specific product. For small button batteries, the preferred thickness d5 is 0.1mm-0.25mm. For power batteries, electric vehicle batteries, etc., in order to ensure safety, the preferred thickness d5 is 1mm-3mm.

[0041] The melting temperature of the first adhesive layer 20 is lower than the melting temperature of the anti-conduction layer 30, and the melting temperature of the second adhesive layer 40 is lower than the melting temperature of the anti-conduction layer 30; before the battery shell is sealed, the first adhesive layer 20 and the second adhesive layer 40 are melted at a temperature greater than or equal to 100°C and lower than the melting temperature of the anti-conduction layer 30, respectively, and are seamlessly bonded to the first stainless steel layer 10 and the second stainless steel layer 50, and the bonding strength between the first stainless steel layer 10 and the second stainless steel layer 50 at cooling room temperature is greater than or equal to 1.0N per square millimeter, and the temperature is greater than or equal to 100°C. The first is to melt the first adhesive layer 20 and the second adhesive layer 40, and the temperature is greater than or equal to the first stainless steel layer 10 and the second stainless steel layer 20. The water, grease, etc. on the surface of the first stainless steel layer 10 and the second stainless steel layer 20 can be volatilized to ensure the bonding strength between the first adhesive layer 20, the second adhesive layer 40 and the first stainless steel layer 10 and the second stainless steel layer 20.

[0042] The first stainless steel layer 10 and the second stainless steel layer 50 are provided as stainless steel plates, and the first adhesive layer 20, the anti-conduction layer 30 and the second adhesive layer 40 form an interlayer between the first stainless steel layer 10 and the second stainless steel layer 50. The specific material of the anti-conduction layer 30 is not limited, and only needs to have insulating properties, such as rubber. The specific material of the first adhesive layer 20 and the second adhesive layer 40 is not limited, and only needs to be able to adhere the first stainless steel layer 10 and the second stainless steel layer 50 to the anti-conduction layer 30 and prevent corrosion from the electrolyte.

[0043] For example, the material of the first adhesive layer 20, the second adhesive layer 40 and the anti-conduction layer 30 may be one or more of PP (polypropylene), PFA (a copolymer of a small amount of perfluoropropyl perfluorovinyl ether and polytetrafluoroethylene), PVDF (polyvinylidene fluoride), PTFE (polytetrafluoroethylene), ETFE (ethylene-tetrafluoroethylene copolymer), and PVC (polyvinyl chloride). The raw material of the first adhesive layer 20 will melt at a melting temperature, such as 100°C, to flow and adhere to the first stainless steel layer 10 and the anti-conduction layer 30. The melting temperature of the first adhesive layer 20 is lower than that of the anti-conduction layer 30, which can prevent the anti-conduction layer 30 and the first adhesive layer 20 from melting at the same temperature and blending with each other, thereby ensuring that the performance of the anti-conduction layer 30 will not be destroyed in the process of connecting the anti-conduction layer 30 and the first stainless steel layer 10. The function and melting temperature of the second adhesive layer 40 can refer to the first adhesive layer 20.

[0044] The stainless steel composite plate can be processed into a battery shell, and then combined with a battery cell and an electrolyte to form a button battery. The first stainless steel layer 10 can form a positive electrode shell, and the second stainless steel layer 50 can form a negative electrode shell. The positive electrode shell is connected to the positive electrode 60 of the battery cell, and the negative electrode shell is connected to the negative electrode 70 of the battery cell. The positive electrode shell and the negative electrode shell are insulated and sealed by the first adhesive layer 20, the second adhesive layer 40 and the anti-conduction layer 30, thereby preventing electrolyte leakage and preventing external moisture from penetrating into the battery shell.

[0045] The first adhesive layer 20, the second adhesive layer 40 and the anti-conduction layer 30 are corrosion-resistant to avoid being damaged by electrolyte corrosion. Compared with the existing battery shell, the first adhesive layer 20, the second adhesive layer 40 and the first stainless steel layer 10 and the second stainless steel layer 20 are seamlessly bonded and are completed before the battery shell is packaged, which is convenient for production and processing, and improves the sealing of the battery shell. At the same time, when the insulating layer exceeds the bonding strength, it can also crack, which protects the battery and avoids the explosion of a large amount of gas inside the battery due to some circumstances.

[0046] The thickness d1 of the first stainless steel layer 10 and the thickness d5 of the second stainless steel layer 50 are set to 0.1mm-5mm, which can not only make the first stainless steel layer 10 and the second stainless steel layer 50 have sufficient structural strength, but also reasonably control the overall size of the battery shell made of the stainless steel composite plate. The thickness d2 of the first adhesive layer 20 and the thickness d4 of the second adhesive layer 40 are set to 0.05mm-10mm, so that in the subsequent processing of the stainless steel composite plate, the first adhesive layer 20 and the second adhesive layer 40 can stably withstand the changes in temperature or external force, so as to improve the bonding stability of the first adhesive layer 20 and the second adhesive layer 40, and at the same time reasonably control the overall size of the battery shell made of the stainless steel composite plate. The thickness d3 of the anti-conduction layer 30 is set to 0.05mm-5mm, which can prevent the anti-conduction layer 30 from being squeezed and damaged during the subsequent processing or the use of the battery, so as to improve the insulation stability; at the same time, the overall size of the battery shell made of the stainless steel composite plate can be reasonably controlled.

[0047] The bonding strength between the first adhesive layer 20 and the second adhesive layer 40 and the first stainless steel layer 10 and the second stainless steel layer 50 at a cooling room temperature is set to be greater than or equal to 1.0N per square millimeter, which can prevent the first stainless steel layer 10 and the second stainless steel layer 50 from easily falling off from the first adhesive layer 20 and the second adhesive layer 40 during the subsequent processing of the stainless steel composite plate or the use of the battery made of the stainless steel composite plate, so as to ensure the structural stability of the stainless steel composite plate. Specifically, the bonding strength between the first adhesive layer 20 and the second adhesive layer 40 and the first stainless steel layer 10 and the second stainless steel layer 50 at a cooling room temperature is less than or equal to 5.0N / mm, so as to prevent the internal stress of the stainless steel composite plate from being too high, thereby avoiding the first stainless steel layer 10 or the second stainless steel layer 50 from being damaged due to internal forces when processing the stainless steel composite plate, and protecting the battery at the same time.

[0048] The material of the first stainless steel layer 10 is SUS304, and / or the material of the second stainless steel layer 50 is SUS304. SUS304 is 304 stainless steel, which contains a high nickel content and is an austenite single-phase structure at room temperature, has high corrosion resistance, good cold forming and weldability, and has high plasticity and toughness at low temperature, room temperature and high temperature. Setting the first stainless steel layer 10 and the second stainless steel layer 50 to SUS304 can ensure the structural stability of the stainless steel composite plate during processing, as well as the chemical stability when used as a battery shell.

[0049] Since the stainless steel composite plate itself has achieved the insulation connection between the first stainless steel layer 10 and the second stainless steel layer 50 before being processed into the battery shell, after the first stainless steel layer 10 and the second stainless steel layer 50 are processed to form the positive electrode shell and the negative electrode shell, the positive electrode shell and the negative electrode shell no longer need to be connected or insulated through other processes, thereby reducing the processing difficulty of the battery shell and improving the processing efficiency of the battery.

[0050] In the technical solution of the present invention, the first stainless steel layer 10 is fixedly connected to one side of the anti-conduction layer 30 through the first adhesive layer 20, and the second stainless steel layer 50 is fixedly connected to the other side of the anti-conduction layer 30 through the second adhesive layer 40, so that the first stainless steel layer 10 and the second stainless steel layer 50 can be connected and insulated from each other; after the stainless steel composite plate is made, the first stainless steel layer 10 and the second stainless steel layer 50 can be further processed to form the shape of a battery shell, wherein the first stainless steel layer 10 can form a positive electrode shell, and the second stainless steel layer 50 can form a negative electrode shell, and the positive electrode shell and the negative electrode shell can be sealed and insulated by the first adhesive layer 20, the anti-conduction layer 30 and the second adhesive layer 40, thereby reducing the processing difficulty of the battery shell and improving the processing efficiency of the battery.

[0051] In one embodiment, the first adhesive layer 20 and the second adhesive layer 40 melt at a temperature less than or equal to 350°C to be seamlessly bonded to the first stainless steel layer 10 and the second stainless steel layer 50, respectively. That is to say, the first adhesive layer 20 and the second adhesive layer 40 melt at 100°C-350°C to be seamlessly bonded to the first stainless steel layer 10 and the second stainless steel layer 50, so that the first adhesive layer 20 and the second adhesive layer 40 can be fully melted to be in full contact with the first stainless steel layer 10 and the second stainless steel layer 50, thereby ensuring the bonding strength of the first adhesive layer 20 and the second adhesive layer 40; and the temperature of the first adhesive layer 20 and the second adhesive layer 40 can be prevented from being too high to affect the molecular structure of the anti-conduction layer 30, and the anti-conduction layer 30 can be prevented from losing its insulation performance, so as to ensure the structural stability of the anti-conduction layer 30. For example, the specific The temperature can be 100°C, 105°C, 110°C, 120°C, 130°C, 140°C, 150°C, 180°C, 200°C, 250°C, 300°C, 500°C, 600°C, 700°C, 800°C, 850°C. It should be understood that the specific temperature depends on the specific first adhesive layer 20 and the second adhesive layer 40 and is not restrictive. The first adhesive layer 20, the second adhesive layer 40 can be seamlessly bonded to the first stainless steel layer 10 and the second stainless steel layer 20 within a temperature range in which the first adhesive layer 20 and the second adhesive layer 40 are melted without destroying the properties of the materials themselves.

[0052] In one embodiment, if Figures 3 to 5 As shown, the first surface layer of the first stainless steel layer 10 close to the first adhesive layer 20 is provided with a first adhesive reinforcement layer 11 for strengthening the bonding strength with the first adhesive layer; and / or the second surface layer of the second stainless steel layer 50 close to the second adhesive layer 40 is provided with a second adhesive reinforcement layer 51 for strengthening the bonding strength with the second adhesive layer. The specific forms of the first adhesive reinforcement layer 11 and the second adhesive reinforcement layer 51 are not limited, as long as the connection area with the first adhesive layer 20 and the second adhesive layer 40 can be increased to strengthen the bonding strength. For example, the first adhesive reinforcement layer 11 and the second adhesive reinforcement layer 51 can be set as a protrusion. The forms of the first adhesive reinforcement layer 11 and the second adhesive reinforcement layer 51 can be the same or different. It should be noted that the first adhesive reinforcement layer 11 and the second adhesive reinforcement layer 51 should avoid passing through the first adhesive layer 20 and the second adhesive layer 40 to avoid affecting the connection stability between the first adhesive layer 20 and the anti-conduction layer 30, and the second adhesive layer 40 and the anti-conduction layer 30.

[0053] Specifically, Figure 3As shown, the first bonding enhancement layer 11 is the first surface layer of the first stainless steel layer 10 close to the first bonding layer, which is processed by sandblasting to form a uniform first rough surface layer; and / or the second bonding enhancement layer 51 is the second surface layer of the second stainless steel layer 50 close to the second bonding layer, which is processed by sandblasting to form a uniform second rough surface layer. Sandblasting uses compressed air as a power to form a high-speed jet beam to spray the material (copper ore sand, quartz sand, corundum, iron sand, Hainan sand) at high speed onto the surface of the workpiece to be processed, so that the appearance or shape of the outer surface of the workpiece surface changes. Due to the impact and cutting action of the abrasive on the workpiece surface, the surface of the workpiece obtains a certain degree of cleanliness and different roughness. It can be understood that the uniformity in this embodiment does not mean absolute uniformity, but the natural roughness formed by the first surface layer and the second surface layer after sandblasting. The first matte layer and the second matte layer can increase the adhesion to the first adhesive layer 20 and the second adhesive layer 40, and make the adhesion between the first surface layer and the second surface layer and the first adhesive layer 20 and the second adhesive layer 40 more uniform, thereby avoiding stress concentration. The first adhesive enhancement layer 11 and the second adhesive enhancement layer 51 are formed by sandblasting, which can simplify the processing method of the first adhesive enhancement layer 11 and the second adhesive enhancement layer 51 to improve the processing efficiency.

[0054] like Figure 4 As shown, the first adhesive reinforcement layer 11 is a first inclined sheet 111 protruding from the first surface layer and having a certain inclination angle with the first surface layer, and the height h1 of the first inclined sheet 111 is less than the thickness d2 of the first adhesive layer 20, and the second adhesive reinforcement layer 51 is a second inclined sheet 511 protruding from the second surface layer and having a certain inclination angle with the second surface layer, and the height h2 of the second inclined sheet 511 is less than the thickness d4 of the second adhesive layer 40. There are multiple first inclined sheets 111 distributed on the first surface layer, and the melted first adhesive layer 20 can fill the space between two adjacent first inclined sheets 111 to adhere to and connect with the side surfaces of each first inclined sheet 111. The height of the first inclined sheet 111 is the vertical distance between the end of the first inclined sheet 111 and the first surface layer. The height of the first inclined sheet 111 is less than the height of the first adhesive layer 20, which can prevent the first inclined sheet 111 from passing through the first adhesive layer 20. There are multiple second inclined sheets 511 distributed on the second surface layer, and the melted second adhesive layer 40 can fill the space between two adjacent second inclined sheets 511 to be adhered and connected to the side surfaces of each second inclined sheet 511. The height of the second inclined sheet 511 is the vertical distance between the end of the second inclined sheet 511 and the second surface layer. The height of the second inclined sheet 511 is less than the height of the second adhesive layer 40, so that the second inclined sheet 511 can be prevented from passing through the second adhesive layer 40.

[0055] like Figure 5As shown, the first bonding enhancement layer 11 is a first groove 112 that is recessed into the first surface layer, and the recessed direction of the first groove 112 is away from the direction of the first bonding layer; and / or the second bonding enhancement layer 51 is a second groove 512 that is recessed into the second surface layer, and the recessed direction of the second groove 512 is away from the direction of the second bonding layer. There are multiple first grooves 112, and multiple first grooves 112 are distributed in the first surface layer. The melted first bonding layer 20 can be filled in the first grooves 112 to increase the connection area with the first surface layer, thereby strengthening the bonding strength between the first stainless steel layer 10 and the first bonding layer 20. There are multiple second grooves 512, and multiple second grooves 512 are distributed in the second surface layer. The melted second bonding layer 40 can be filled in the second grooves 512 to increase the connection area with the second surface layer, thereby strengthening the bonding strength between the second stainless steel layer 50 and the second bonding layer 40.

[0056] like Figure 6 As shown, the present invention also proposes a battery, which includes a battery shell, and the battery shell is at least partially a stainless steel composite plate. The specific structure of the stainless steel composite plate refers to the above embodiment. Since the present battery adopts all the technical solutions of all the above embodiments, it has at least all the beneficial effects brought by the technical solutions of the above embodiments, which will not be repeated here. Among them, the battery shell contains at least a battery element including a positive electrode 60, a negative electrode 70 and an electrolyte, the positive electrode 60 is electrically conductive with the first stainless steel layer 10, and the negative electrode 70 is electrically conductive with the second stainless steel layer 50. It can be understood that the first stainless steel layer 10 and the second stainless steel layer 50 can form a battery shell by bending, or by connecting stainless steel plates.

[0057] The above descriptions are only optional embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings, or directly / indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.

Claims

1. A stainless steel composite plate for a battery housing, characterized in that: The stainless steel composite plate at least comprises a first stainless steel layer, a first bonding layer, an anti-conduction layer, a second bonding layer and a second stainless steel layer in sequence; The thickness d1 of the first stainless steel layer is 0.1 mm to 5 mm, and is used for electrically conducting with one of the electrodes of the battery cell inside the battery housing, and for preventing moisture outside the battery housing from penetrating into the housing; The thickness d2 of the first bonding layer is 0.05 mm-10 mm, and is used to bond the first stainless steel layer and the anti-conduction layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing; The thickness d3 of the anti-conduction layer is 0.05 mm-5 mm, which is used to prevent the first stainless steel layer from being electrically conductive with the second stainless steel layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing; The thickness d4 of the second bonding layer is 0.05 mm to 10 mm, and is used to bond the second stainless steel layer and the anti-conduction layer, resist electrolyte corrosion, and prevent moisture outside the battery housing from penetrating into the housing; The thickness d5 of the second stainless steel layer is 0.1 mm to 5 mm, and is used for electrically conducting with the other electrode of the battery cell inside the battery housing, and for preventing moisture outside the battery housing from penetrating into the housing; The melting temperature of the first adhesive layer is lower than the melting temperature of the conduction prevention layer, and the melting temperature of the second adhesive layer is lower than the melting temperature of the conduction prevention layer; Before the battery case is sealed, the first adhesive layer and the second adhesive layer are seamlessly bonded to the first stainless steel layer and the second stainless steel layer respectively when they melt at a temperature greater than or equal to 100° C. and lower than the melting temperature of the anti-conduction layer, and the bonding strength between the first stainless steel layer and the second stainless steel layer at cooling room temperature is greater than or equal to 1.0 N per square millimeter; After the stainless steel composite plate is manufactured, the first stainless steel layer and the second stainless steel layer are further processed to form the shape of a battery shell, wherein the first stainless steel layer forms a positive electrode shell, the second stainless steel layer forms a negative electrode shell, and the positive electrode shell and the negative electrode shell are sealed and insulated by the first adhesive layer, the anti-conduction layer and the second adhesive layer.

2. The stainless steel composite plate according to claim 1, characterized in that: The material of the first stainless steel layer is SUS304, and / or the material of the second stainless steel layer is SUS304.

3. The stainless steel composite plate according to claim 1, characterized in that: The material of the first adhesive layer, the anti-conduction layer and the second adhesive layer is one or more of PP, PFA, PVDF, PTFE, ETFE and PVC.

4. The stainless steel composite plate according to claim 1, characterized in that: The bonding strength between the first bonding layer and the second bonding layer and the first stainless steel layer and the second stainless steel layer respectively at cooling room temperature is less than or equal to 5.0 N / mm.

5. The stainless steel composite plate according to claim 1, characterized in that: The first adhesive layer and the second adhesive layer melt at a temperature not higher than 350° C. to be seamlessly bonded to the first stainless steel layer and the second stainless steel layer respectively.

6. The stainless steel composite plate according to any one of claims 1 to 5, characterized in that: A first bonding enhancement layer is provided on the first surface of the first stainless steel layer close to the first bonding layer, for strengthening the bonding strength between the first bonding layer and the first bonding layer; and / or a second bonding enhancement layer is provided on the second surface of the second stainless steel layer close to the second bonding layer, for strengthening the bonding strength between the second bonding layer and the second bonding layer.

7. The stainless steel composite plate according to claim 6, characterized in that: The first bonding enhancement layer is a first surface layer of the first stainless steel layer close to the first bonding layer that is treated by sand blasting to form a uniform first rough surface layer; and / or the second bonding enhancement layer is a second surface layer of the second stainless steel layer close to the second bonding layer that is treated by sand blasting to form a uniform second rough surface layer.

8. The stainless steel composite plate according to claim 6, characterized in that: The first bonding enhancement layer is a first inclined sheet protruding from the first surface layer and having a certain inclination angle with the first surface layer, and the height h1 of the first inclined sheet is less than the thickness d2 of the first bonding layer. The second bonding enhancement layer is a second inclined sheet protruding from the second surface layer and having a certain inclination angle with the second surface layer, and the height h2 of the second inclined sheet is less than the thickness d4 of the second bonding layer.

9. The stainless steel composite plate according to claim 6, characterized in that: The first bonding enhancement layer is a first groove sunken into the first surface layer, and the sunken direction of the first groove is away from the first bonding layer; and / or the second bonding enhancement layer is a second groove sunken into the second surface layer, and the sunken direction of the second groove is away from the second bonding layer.

10. A battery, characterized in that: The battery comprises a battery shell, at least part of which is the stainless steel composite plate according to any one of claims 1 to 9, and the battery shell contains at least a battery element including a positive electrode, a negative electrode and an electrolyte, the positive electrode is electrically conductive with the first stainless steel layer, and the negative electrode is electrically conductive with the second stainless steel layer.