Display panel and display device
By setting the non-electrically connected reflective metal film layer and appropriate spacing, the problem of shorting between the metal film layer and the test trace in the display panel is solved, improving product yield and display effect, and extending service life.
Patent Information
- Application Number
- CN202210280948.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-21
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-03-21
AI Technical Summary
In the display panel with narrow borders, the distance between the metal film layer and the box test trace is small, causing the metal to melt and overflow and short connection during laser sintering, causing the problem of abnormal signal.
The first reflective metal film layer and the second reflective metal film layer are not electrically connected, and are located between the test trace and the first reflective metal film layer in the horizontal distribution direction. The width of the second reflective metal film layer is greater than 50 microns. The minimum spacing between a reflective metal film layer and the test trace is greater than 100 microns to avoid overflow of the metal film layer and short-connection of the test trace.
It effectively avoids short-connection of the metal film layer with the test trace during laser sintering, improves product yield and display effect, and extends service life.
Smart Images

Figure CN114678406B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to a display panel and a display device. Background Art
[0002] OLED devices (such as AMOLED (Active-matrix organic light emitting diode) devices) are self-luminous devices that rely on driving their own organic light-emitting materials to emit light. They have the advantages of high brightness, low power consumption, and high resolution. With the iteration and update of new technologies and new products, new products currently have higher requirements for narrow borders. To achieve narrow borders, a basic rule in design is to continuously compress the spacing at each position while meeting the requirements of process equipment.
[0003] In the current product design, in order to meet the narrow bezel requirement of the product, the distance between the metal film layer that provides the VSS signal and the box test trace closest to the metal film layer is only about 7 microns. The distance is very small. During packaging, the Frit glue (packaging glue layer on the cover) printing offset and laser sintering energy fluctuation may occur. After the offset, metal melts and overflows at the edge of the metal film layer during the laser sintering process. Since the distance between the metal film layer and the box test trace closest to it is very small, the metal melts and overflows, which is easy to short-circuit with the box test trace, resulting in signal abnormality, thereby causing product display abnormality and other defects.
[0004] Therefore, current display panels and display devices still need to be further improved. Summary of the invention
[0005] The present invention aims to solve one of the technical problems in the related art at least to a certain extent.
[0006] In view of this, in one aspect of the present invention, the present invention provides a display panel, the display panel comprises: a cover plate, a glue layer is arranged around the peripheral area of the cover plate; a substrate, the substrate is arranged opposite to the cover plate, the substrate has a display area and a peripheral area, the substrate comprises: a substrate; a test line, the test line is located on at least one side of the peripheral area; a first reflective metal film layer, the first reflective metal film layer is located around the peripheral area, and is located on the side of the test line close to the display area; a second reflective metal film layer, in the horizontal distribution direction, the second reflective metal film layer is located between the test line and the first reflective metal film layer, and is not electrically connected to the first reflective metal film layer; wherein the test line, the first reflective metal film layer, and the second reflective metal film layer are all arranged on the side of the substrate close to the cover plate. Thus, the first reflective metal film layer and the second reflective metal film layer are not connected, and the first reflective metal film layer is arranged close to the test line, which can avoid the situation that the metal overflows from the edge of the reflective metal film layer after it melts during the laser sintering process and shorts the test line, thereby improving the product yield.
[0007] According to an embodiment of the present invention, the first reflective metal film layer and the second reflective metal film layer are provided in the same layer or in different layers.
[0008] According to an embodiment of the present invention, the substrate includes a thin film transistor, the first reflective metal film layer is disposed in the same layer as a source-drain electrode layer in the thin film transistor, and the second reflective metal film layer is disposed in the same layer as a gate electrode in the thin film transistor.
[0009] According to an embodiment of the present invention, the orthographic projection of the first reflective metal film layer on the substrate partially overlaps or does not overlap with the orthographic projection of the second reflective metal film layer on the substrate.
[0010] According to an embodiment of the present invention, the test line includes a first test line and a second test line, the length extension direction of the second test line is the same as the length extension direction of the second reflective metal film layer, and the length extension direction of the second test line and the length extension direction of the first test line have an included angle. This is conducive to further improving the overall performance of the display panel.
[0011] According to an embodiment of the present invention, the first test line is set at the same layer as the gate of the thin film transistor, and the second test line is set at the same layer as the source and drain electrode layer of the thin film transistor, or the first test line is set at the same layer as the source and drain electrode layer of the thin film transistor, and the second test line is set at the same layer as the gate of the thin film transistor.
[0012] According to an embodiment of the present invention, the first reflective metal film layer has a plurality of first openings disposed at intervals, and / or the second reflective metal film layer has a plurality of second openings disposed at intervals, thereby further improving the overall performance of the display panel.
[0013] According to an embodiment of the present invention, the width of the second reflective metal film layer is greater than 50 micrometers. Therefore, the second reflective metal film layer is wider, which is more conducive to avoiding the short circuit between the first reflective metal film layer and the test wiring, thereby improving the yield of the product.
[0014] According to an embodiment of the present invention, the minimum spacing between the first reflective metal film layer and the test line is greater than 100 microns. Thus, the distance between the first reflective metal film layer and the test line is large, which can more effectively avoid short circuit between the first reflective metal film layer and the test line.
[0015] In another aspect of the present invention, the present invention provides a display device, the display device comprising the display panel described above. Thus, the display device has all the features and advantages of the display panel described above, which will not be described in detail here. In general, the display device is not prone to short circuit problems, has a good display effect, and has a long service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A partial structural schematic diagram of a display panel according to an embodiment of the present invention is shown;
[0017] Figure 2 A partial structural schematic diagram of a display panel in the prior art is shown;
[0018] Figure 3 A partial structural schematic diagram of a display panel according to another embodiment of the present invention is shown;
[0019] Figure 4 A partial structural schematic diagram of a display panel according to another embodiment of the present invention is shown;
[0020] Figure 5 A partial structural schematic diagram of a display panel according to another embodiment of the present invention is shown;
[0021] Figure 6 A partial structural schematic diagram of a display panel according to yet another embodiment of the present invention is shown. DETAILED DESCRIPTION
[0022] The embodiments of the present invention are described in detail below. The embodiments described below are exemplary and are only used to explain the present invention, and should not be construed as limiting the present invention. If no specific techniques or conditions are specified in the embodiments, the techniques or conditions described in the literature in the art or the product specifications are used.
[0023] In one aspect of the present invention, the present invention provides a display panel, referring to Figure 1 , the display panel includes a cover plate 100, a glue layer 200 and a substrate 300. According to an embodiment of the present invention, Figure 1 , a glue layer 200 is arranged around the peripheral area of the cover plate 100; the substrate 300 is arranged opposite to the cover plate 100, the substrate 300 has a display area 10 and a peripheral area 20, the peripheral area 20 is arranged around the display area 10 (not shown in the figure), the substrate 300 includes a substrate 310, a test wiring 320, a first reflective metal film layer 330 and a second reflective metal film layer 340, wherein the test wiring 320, the first reflective metal film layer 330, and the second reflective metal film layer 340 are all arranged on a side of the substrate 310 close to the cover plate 100, the test wiring 320 is located on at least one side of the peripheral area 20, the first reflective metal film layer 330 is located around the peripheral area 20, and the first reflective metal film layer 330 is located on a side of the test wiring 320 close to the display area 10, in the horizontal distribution direction, the horizontal distribution direction can be referred to Figure 1 In the X direction shown in FIG. 1 , the second reflective metal film layer 340 is located between the test trace 320 and the first reflective metal film layer 330, and the second reflective metal film layer 340 is not electrically connected to the first reflective metal film layer 330. That is, in the horizontal distribution direction ( Figure 1 In the X direction shown in FIG. 1 , the first reflective metal film layer 330, the second reflective metal film layer 340 and the test wiring 320 are sequentially arranged away from the display area 10. It should be noted that: Figure 1 Only a partial structural schematic diagram of the display panel is shown, and the entire surrounding area of the cover plate and the entire peripheral area of the substrate are not shown. In the present invention, the first reflective metal film layer 330 can be used to provide a VSS signal, that is, the first reflective metal film layer 330 can be used as a VSS signal line, and the second reflective metal film layer 340 is not electrically connected to the first reflective metal film layer 330, and in the horizontal distribution direction, the second reflective metal film layer 340 is located between the first reflective metal film layer 330 and the test line 320, which can effectively avoid the VSS signal line (first reflective metal film layer 330) and the test line 320 from being short-circuited, thereby improving the display effect of the display panel and improving the overall performance of the display panel.
[0024] According to an embodiment of the present invention, the test trace 320 may be located only on one side of the peripheral area 20 , for example, the test trace 320 may be disposed only on one side of the peripheral area where a COF (chip on flexible circuit board) is formed.
[0025] The principle that the present invention can effectively avoid short circuit between the VSS signal line and the test line is described below: Figure 2FIG. 1 shows a schematic diagram of a partial structure of a display panel in the prior art, wherein the test wiring includes a first test line 321 and a second test line 322, the first test line 321 and the second test line 322 can be arranged in different layers, the metal film layer 30 is arranged in the same layer as the first test line 321, and the metal film layer is used to provide a VSS signal. In order to meet the requirements of a narrow frame, the distance d between the metal film layer 30 and the first test line 321 closest to it is only about 7 microns, as shown in FIG. Figure 2 As shown, when edge packaging is performed, due to the offset of Frit glue printing and the fluctuation of laser sintering energy, the metal at the edge of the metal film layer 30 may melt and overflow during the sintering process, and the overflowed metal is easy to short-circuit with the first test line 321, resulting in abnormal signals, thereby causing panel display abnormalities and other defects. In the present invention, by setting the first reflective metal film layer 330 and the second reflective metal film layer 340 not to be electrically connected, and the second reflective metal film layer 340 is located between the first reflective metal film layer 330 and the test line 320 in the horizontal distribution direction, the VSS signal can be provided only by the first reflective metal film layer 340, and the second reflective metal film layer 330 does not provide a signal, thereby significantly increasing the minimum spacing between the first reflective metal film layer 330 and the test line 320, and effectively preventing the first reflective metal film layer 330 from overflowing metal and short-circuiting with the test line during laser sintering.
[0026] According to an embodiment of the present invention, referring to Figure 3 The test line 300 includes a first test line 321 and a second test line 322. The length extension direction of the second test line 322 is the same as the length extension direction of the second reflective metal film layer 340. Figure 3 In the Y direction shown in FIG, the length extension direction of the first test line 321 is Figure 3 In the Z direction shown in , the length extension direction Y direction of the second test line 322 and the length extension direction Z direction of the first test line 321 have an included angle, that is, the length extension direction of the first test line 321 is different from the length extension direction of the second test line 322.
[0027] It should be noted that, in order to facilitate the explanation of the technical solution of the present invention, Figure 2 and Figure 3 Only a partial structure of the display panel is shown, and not all structural features of the display panel are shown.
[0028] According to some embodiments of the present invention, reference Figures 4 to 6The substrate 300 further includes a thin film transistor 350, which includes a source-drain electrode layer 351, a gate 352, an active layer 353 and other structures, wherein the source-drain electrode layer 351 is electrically connected to the active layer 353 through a via, and the source-drain electrode layer 351, the gate 352 and the active layer 353 are all arranged in different layers. It can be understood by those skilled in the art that the display panel can also include multiple pixel structures, Figures 4 to 6 In addition, the display panel may include multiple thin film transistors to adjust and control multiple pixel structures. Figures 4 to 6 Only the structure of a thin film transistor is shown in the figure, which is used to illustrate the structural features of some structures arranged in the same layer or different layers in the substrate.
[0029] According to an embodiment of the present invention, referring to Figures 4 to 6 , the first test line 321 can be arranged in the same layer as the source-drain electrode layer 351 of the thin film transistor 350, the second test line 322 can be arranged in the same layer as the gate 352 of the thin film transistor 350, and the first test line 321 can be electrically connected to the second test line 322 through a via. According to some embodiments of the present invention, the first test line 321 and the second test line 322 are used to detect whether the pixel can emit light normally. The first test line 321 can be connected to the signal input terminal, and the signal is given to the pixel structure in the display panel through the second test line 322 to test whether the pixel is displayed normally.
[0030] It should be noted that the reference Figure 3 A plurality of first test lines 321 and second test lines 322 may be provided in the display panel, and each first test line 321 may be connected to a via hole (see Figures 4 to 6 ) is electrically connected to a second test line 322 to facilitate input of a signal to a corresponding pixel structure.
[0031] According to other embodiments of the present invention, the first test line can also be set in the same layer as the gate electrode layer of the thin film transistor, and the second test line can be set in the same layer as the source and drain electrode layer of the thin film transistor, as long as the signal can be transmitted to the corresponding pixel structure through the first test line and the second test line to detect whether the pixel structure can emit light normally. It should be noted that in this case, the spacing between the first reflective metal film layer 330 and the test line set in the same layer can also be made larger to avoid short circuit between the first reflective metal film layer 330 and the test line set in the same layer during laser sintering.
[0032] According to an embodiment of the present invention, referring to Figure 4The first reflective metal film layer 330 and the second reflective metal film layer 340 can be arranged in the same layer, the first reflective metal film layer 330 is used to input the VSS signal, the second reflective metal film layer 340 is arranged close to the first test line 321, and the second reflective metal film layer 340 is not electrically connected to the first reflective metal film layer 330. When laser sintering is performed, there is a certain distance between the second reflective metal film layer 340 and the first metal film layer 330. Even if metal melts and overflows at the edge of the second reflective metal film layer 340 close to the first test line 321 during laser sintering, or even the second reflective metal film layer 340 is connected to the edge of the first test line 321, the second reflective metal film layer 340 will not be short-circuited with the first test line 321, and the display panel can still maintain a good display function.
[0033] According to an embodiment of the present invention, referring to Figure 5 and Figure 6 , the first reflective metal film layer 330 and the second reflective metal film layer 340 can be arranged in different layers, the first reflective metal film layer 330 and the source-drain electrode layer 351 in the thin film transistor 350 are arranged in the same layer, and the second reflective metal film layer 340 and the gate electrode 352 in the thin film transistor 350 are arranged in the same layer. Thus, the first reflective metal film layer 330 and the first test line 321 are arranged in the same layer as the source-drain electrode layer 351 in the thin film transistor 350, and the second reflective metal film layer 340 and the second test line 322 are arranged in the same layer as the gate electrode 352 in the thin film transistor 350, which is more conducive to avoiding the first reflective metal film layer 330 and the first test line 321 from being short-circuited during laser sintering.
[0034] According to an embodiment of the present invention, referring to Figure 3 The width L of the second reflective metal film layer 340 can be greater than 50 microns, for example, 55 microns, 60 microns, 65 microns, 80 microns, 100 microns, etc., which is beneficial to increase the minimum spacing between the first reflective metal film layer and the test line (such as the first test line 321), and further helps to avoid the short circuit between the first reflective metal film layer and the test line during laser sintering. It should be noted that, if Figure 3 As shown, the spacings between the plurality of first test lines 321 and the first reflective metal film layer 330 are different, and the minimum spacing refers to the spacing between the first test line 321 closest to the first reflective metal film layer and the first reflective metal film layer 330 .
[0035] According to an embodiment of the present invention, referring to Figure 3The minimum spacing D between the first reflective metal film layer 330 and the test trace 320 (such as the first test trace 321) can be greater than 100 microns, for example, it can be 110 microns, 120 microns, 130 microns, etc. Therefore, the minimum spacing between the first reflective metal film layer 330 and the test trace 320 is larger, which is more conducive to avoiding the short circuit between the first reflective metal film layer and the test trace during laser sintering.
[0036] According to an embodiment of the present invention, the orthographic projection of the first reflective metal film layer 330 on the substrate 310 partially overlaps or does not overlap with the orthographic projection of the second reflective metal film layer 340 on the substrate 310. Figure 4 , the first reflective metal film layer 330 and the second reflective metal film layer 340 are arranged in the same layer and there is a certain distance between them, and the orthographic projection of the first reflective metal film layer 330 on the substrate 310 and the orthographic projection of the second reflective metal film layer 340 on the substrate 310 have no overlapping area; according to some other embodiments of the present invention, reference Figure 5 , the first reflective metal film layer 330 and the second reflective metal film layer 340 are arranged in different layers, and the orthographic projection of the first reflective metal film layer 330 on the substrate 310 and the orthographic projection of the second reflective metal film layer 340 on the substrate 310 may not overlap, that is, there is no overlapping area; according to some other embodiments of the present invention, reference Figure 6 , the first reflective metal film layer 330 and the second reflective metal film layer 340 are arranged in different layers, and the orthographic projection of the first reflective metal film layer 330 on the substrate 310 and the orthographic projection of the second reflective metal film layer 340 on the substrate 310 can partially overlap. In the above-mentioned arrangement, the requirement of having a large spacing between the first reflective metal film layer 330 and the first test line 321 can be met, thereby avoiding the problem of short circuit between the first reflective metal film layer and the test line during laser sintering.
[0037] According to an embodiment of the present invention, referring to Figures 4 to 6 , the substrate 300 may further include a buffer layer 360, a planarization layer 370 and other structures, wherein the buffer layer 360 is arranged between the substrate 310 and the active layer 353 of the thin film transistor 350, the planarization layer 370 is arranged close to the cover plate 100, and the planarization layer 370 covers the surface of the source and drain electrode layer 351 away from the substrate 310, and the glue layer 200 covers part of the surface of the planarization layer 370. The buffer layer 360 and the planarization layer 370 are both formed of insulating materials, such as silicon oxide, silicon nitride, silicon oxynitride, etc. It should be noted that in the display panel, the parts that need to be insulated between the metal materials are also provided with insulating materials, and in order to facilitate the explanation of the technical solution of the present invention, the present invention does not show all the structures.
[0038] According to an embodiment of the present invention, referring to Figure 3The first reflective metal film layer 330 may have a plurality of first openings 331 spaced apart from each other. A through hole may be correspondingly provided at a position of the planarizing layer 370 corresponding to the first opening 331 of the first reflective metal film layer 330. The aperture of the through hole may be smaller than the size of the first opening 331. During laser sintering, on the one hand, the first reflective metal film layer 330 may reflect the laser so that the heat generated by the laser is concentrated on the adhesive layer, which is more conducive to the packaging of the cover plate 100 and the substrate 300. On the other hand, part of the adhesive layer 200 may penetrate into the first opening 331, and a stronger bond between the cover plate 100 and the substrate 300 may be achieved through the partially penetrated adhesive layer.
[0039] According to some embodiments of the present invention, Figure 3 As shown, the shape of the first opening 331 can be rectangular; according to other embodiments of the present invention, the shape of the first opening 331 can also be rhombus, circular, triangular, etc. Therefore, the first opening 331 is set to the above shape, which is conducive to achieving a firm connection between the cover plate 100 and the substrate 300.
[0040] According to an embodiment of the present invention, referring to Figure 3 , the second reflective metal film layer 340 may also have a plurality of second openings 341 arranged at intervals, and a through hole may also be correspondingly arranged at a position corresponding to the second opening 341 of the planarization layer 370 and the second reflective metal film layer 340, and the aperture of the through hole may be smaller than the size of the second opening 341. Similarly, during laser sintering, on the one hand, the second reflective metal film layer 340 may reflect the laser so that the heat generated by the laser is concentrated in the adhesive layer, which is more conducive to the packaging of the cover plate 100 and the substrate 300, and on the other hand, part of the adhesive layer 200 may penetrate into the second opening 341, and the part of the adhesive layer that penetrates may further achieve a firm bond between the cover plate 100 and the substrate 300.
[0041] According to some embodiments of the present invention, Figure 3 As shown, the shape of the second opening 341 can be rectangular; according to an embodiment of the present invention, the shape of the second opening 341 can also be rhombus, circular, triangular, etc. Therefore, the second opening 341 is set to the above shape, which is conducive to achieving a firm connection between the cover plate 100 and the substrate 300.
[0042] It should be noted that the shape of the through hole is not particularly limited. For example, the through hole can be a circular through hole, a triangular through hole, a rectangular through hole, etc., as long as part of the adhesive layer can penetrate into the first opening 331 and / or the second opening 341 through the through hole to achieve a firm connection between the cover plate 100 and the substrate 300. It should also be noted that the aperture of the through hole can be smaller than the size of the first opening 331, which means that the setting of the through hole corresponding to the first opening 331 can expose a part of the first opening 331 so that a part of the adhesive layer can be filled in the first opening 331. Similarly, the aperture of the through hole can be smaller than the size of the second opening 341, which means that the setting of the through hole corresponding to the second opening 341 can expose a part of the second opening 341 so that a part of the adhesive layer can be filled in the second opening 341.
[0043] According to an embodiment of the present invention, the material of the first reflective metal film layer 330 and the second reflective metal film layer 340 may include at least one of aluminum and molybdenum, and the materials of the first reflective metal film layer 330 and the second reflective metal film layer 340 may be the same or different.
[0044] According to some specific embodiments of the present invention, Figure 5 and Figure 6 The first reflective metal film layer 330 is arranged on the same layer as the source-drain electrode layer 351 of the thin film transistor 350. The material of the first reflective metal film layer 330 and the material of the source-drain electrode layer 351 can both be aluminum. At this time, the first reflective metal film layer 330 can be formed in the same step as the source-drain electrode layer 351, that is, the same set of mask templates can be used to form the first reflective metal film layer 330 and the source-drain electrode layer 351 at the same time using the same process steps. Therefore, the manufacturing process can be simplified, while saving manufacturing costs and improving product yield.
[0045] According to some other specific embodiments of the present invention, Figure 5 and Figure 6 The second reflective metal film layer 340 is arranged on the same layer as the gate electrode 352 of the thin film transistor 350. The material of the second reflective metal film layer 340 and the material of the gate electrode 352 can both be molybdenum. At this time, the second reflective metal film layer 340 can be formed in the same step as the gate electrode 352, that is, the second reflective metal film layer 340 and the gate electrode 352 can be formed simultaneously using the same set of mask templates and the same process steps. Therefore, the production steps can be further simplified, while saving production costs and further improving product yield.
[0046] In another aspect of the present invention, the present invention provides a display device, which includes the display panel described above. Therefore, the display device has all the features and advantages of the display panel described above, which will not be described in detail here. In general, the display device has a good display effect, is not prone to short circuit, and has a long service life.
[0047] According to the embodiments of the present invention, there are no special requirements for the specific type of the above-mentioned display device, and those skilled in the art can flexibly select it according to actual needs. For example, it can be a mobile phone, iPad, notebook or other display device.
[0048] Those skilled in the art will appreciate that, in addition to the display panel described above, the display device also has the necessary structures and components of a conventional display device. Taking a mobile phone as an example, in addition to the display panel described above, it may also include necessary structures and components such as a battery back cover, a middle frame, a touch panel, an audio module, and a motherboard.
[0049] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0050] In the description of this specification, the description with reference to the terms "one embodiment", "another embodiment", "yet another embodiment", "some embodiments", "some specific embodiments" or "some other specific embodiments" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.
[0051] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A display panel, characterized in that: include: A cover plate, wherein a glue layer is arranged around the peripheral area of the cover plate; A substrate, the substrate is arranged opposite to the cover plate, the substrate has a display area and a peripheral area, and the substrate includes: substrate; A test line, the test line is located at at least one side of the peripheral area, and the test line is used to detect whether the pixel can emit light normally; A first reflective metal film layer, wherein the first reflective metal film layer is located around the peripheral area and is located on a side of the test line close to the display area; a second reflective metal film layer, wherein in a horizontal distribution direction, the second reflective metal film layer is located between the test trace and the first reflective metal film layer, is not electrically connected to the first reflective metal film layer, and does not provide a signal; The test wiring, the first reflective metal film layer, and the second reflective metal film layer are all arranged on a side of the substrate close to the cover plate.
2. The display panel according to claim 1, characterized in that: The first reflective metal film layer and the second reflective metal film layer are arranged in the same layer or in different layers.
3. The display panel according to claim 2, characterized in that: The substrate includes a thin film transistor, the first reflective metal film layer is arranged in the same layer as a source-drain electrode layer in the thin film transistor, and the second reflective metal film layer is arranged in the same layer as a gate electrode in the thin film transistor.
4. The display panel according to claim 3, characterized in that: The orthographic projection of the first reflective metal film layer on the substrate partially overlaps or does not overlap with the orthographic projection of the second reflective metal film layer on the substrate.
5. The display panel according to claim 3, characterized in that: The test line includes a first test line and a second test line. The length extension direction of the second test line is the same as the length extension direction of the second reflective metal film layer. The length extension direction of the second test line and the length extension direction of the first test line have an included angle.
6. The display panel according to claim 5, characterized in that: The first test line is set at the same layer as the gate of the thin film transistor, and the second test line is set at the same layer as the source and drain electrode layer of the thin film transistor, or the first test line is set at the same layer as the source and drain electrode layer of the thin film transistor, and the second test line is set at the same layer as the gate of the thin film transistor.
7. The display panel according to any one of claims 1 to 6, characterized in that: The first reflective metal film layer has a plurality of first openings disposed at intervals, and / or the second reflective metal film layer has a plurality of second openings disposed at intervals.
8. The display panel according to any one of claims 1 to 6, characterized in that: The width of the second reflective metal film layer is greater than 50 micrometers.
9. The display panel according to any one of claims 1 to 6, characterized in that: The minimum spacing between the first reflective metal film layer and the test trace is greater than 100 microns.
10. A display device, characterized in that: A display panel comprising any one of claims 1 to 9.