Photosensitive chip components, camera modules and terminal equipment

By arranging a stress layer on the back side of the photosensitive chip and adjusting its bending direction to be consistent with the imaging surface of the lens, the field curvature problem caused by the deformation of the photosensitive chip during the manufacturing process is solved and the imaging quality of the camera is improved.

CN115336245BActive Publication Date: 2024-10-15NINGBO SUNNY OPOTECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080093815.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-01-10
Filing Date
2020-12-18
Publication Date
2024-10-15
Estimated Expiration
2040-12-18

AI Technical Summary

Technical Problem

The deformation of the photosensitive chip due to thickness limitations during the manufacturing process causes its field curvature to be in the opposite direction to the curvature of the imaging surface of the lens, affecting the camera's photo quality.

Method used

By setting a stress layer on the back side of the photosensitive chip, the bending direction is controlled to be consistent with the bending direction of the lens imaging surface, and a compensation film or stress film is used to adjust the bending degree of the photosensitive chip to ensure that the field curvature matches the field curvature of the lens.

Benefits of technology

It effectively improves the imaging clarity of the camera, reduces the blurring around the middle, improves the photo quality, and reduces the processing difficulty and batch molding challenges.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115336245B_ABST
    Figure CN115336245B_ABST
Patent Text Reader

Abstract

The present application discloses a photosensitive chip assembly, a camera module and a terminal device. The chip assembly includes: a photosensitive chip, including a substrate, an active area located on the substrate and a microlens array located on the active area; a stress layer, which is arranged on the back side of the photosensitive chip, so that the photosensitive chip is deformed toward the substrate of the photosensitive chip. By arranging a stress layer on the back side of a traditional photosensitive chip, the bending direction and degree of the photosensitive chip are controlled to control the field curvature of the photosensitive chip, so that the bending direction of the photosensitive chip is consistent with the field curvature direction of the lens, thereby improving the clarity of the imaging.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of camera technology, and specifically to a photosensitive chip component, a camera module and a terminal device. Background Art

[0002] Cameras are essential input devices for electronic products such as mobile phones and tablet computers. As users' requirements for camera imaging quality continue to improve, the pixels of cameras are getting larger and larger, requiring the area of ​​the photosensitive chip inside to be larger and larger.

[0003] The imaging process of the camera is mainly the process of digitizing the light signal, which is mainly completed by the camera module. The camera module mainly includes the lens, photosensitive chip and circuit board. The photosensitive chip is the main component of the camera module. Its working principle is: the external light passes through the lens and shines on the surface of the photosensitive chip. The photosensitive chip converts the light uploaded from the lens into an electrical signal, and then converts it into a digital signal through analog-to-digital conversion.

[0004] Among them, the quality of the photosensitive chip is an important factor affecting the image quality. However, as the camera pixels become larger and larger, the area of ​​the photosensitive chip is also getting larger and larger. However, due to the market demand for increasingly thinner electronic products such as mobile phones, the thickness of the photosensitive chip cannot be increased accordingly. As a result, the ratio of the area to the thickness of the photosensitive chip is gradually increasing.

[0005] The ratio of the area to the thickness of the photosensitive chip is gradually increasing, which makes the photosensitive chip more likely to deform during manufacturing, especially during the heating and curing process of the photosensitive chip. Figure 1 shown.

[0006] Since the center area of ​​the photosensitive chip protrudes upward, the photosensitive area forms a curved surface, which leads to an increase in the field curvature of the photosensitive chip. The direction of the increase in field curvature is opposite to the direction of the image plane curvature of the lens (i.e., the field curvature of the lens). Figure 2 The deformation direction of the photosensitive chip is opposite to the image plane of the lens, which results in poor photo quality with the center being clear and the surroundings being blurred when the camera takes photos.

[0007] In order to solve the above problems, the commonly used method is to bend the photosensitive chip itself into a cylindrical, spherical or curved shape required by the lens group. However, in the method of bending the photosensitive chip, the commonly used method is to extrude the mold. For example, Figure 3 As shown, for the spherical photosensitive chip 1100, a lower mold 002 with a spherical curved surface is provided, and the thin-film photosensitive chip 1100 is pressed onto the lower mold curved surface by an upper mold 001 with a spherical curved surface, thereby bending the entire photosensitive chip 1100 into a sphere. In addition, there is also a method of making the chip into a curved shape during molding. However, this method is difficult to process and is not conducive to mass molding. Summary of the invention

[0008] Based on this, the present application aims to provide a photosensitive chip assembly, so that the photosensitive chip remains bent during the assembly process and is consistent with the bending direction of the actual imaging surface of the lens. By controlling the degree of bending of the photosensitive chip, the field curvature of the photosensitive chip can be controlled to improve the photo quality of the photosensitive chip assembly.

[0009] According to a first aspect of the present application, a photosensitive chip assembly is provided, comprising:

[0010] A photosensitive chip, comprising a substrate, an active area located on the substrate, and a microlens array located on the active area;

[0011] The stress layer is arranged on the back side of the photosensitive chip, so that the photosensitive chip is deformed toward the substrate of the photosensitive chip.

[0012] According to some embodiments of the present application, the thickness of the stress layer is 0.1 um to 10 um.

[0013] According to some embodiments of the present application, the thickness of the photosensitive chip is 100um to 200um.

[0014] According to some embodiments of the present application, the stress layer includes:

[0015] A compensation film, wherein the thermal expansion coefficient of the compensation film is greater than or equal to the thermal expansion coefficient of the microlens array.

[0016] According to some embodiments of the present application, the thickness of the compensation film is greater than or equal to the thickness of the microlens array.

[0017] According to some embodiments of the present application, a material of the compensation film includes at least one of silicon oxide, magnesium fluoride, aluminum oxide, and titanium oxide.

[0018] According to some embodiments of the present application, the compensation film includes a PVD film and / or a CVD film.

[0019] According to some embodiments of the present application, the PVD film includes at least one of a vacuum evaporated film, a magnetron sputtering film, and an atomic layer deposition film.

[0020] According to some embodiments of the present application, the active area further includes a photosensitive area, which is arranged below the microlens array and receives light from the outside that reaches the front of the photosensitive chip;

[0021] The stress layer includes a stress film having a predetermined thickness. The stress generated during the coating process causes the photosensitive area of ​​the photosensitive chip to deform toward the substrate of the photosensitive chip.

[0022] According to some embodiments of the present application, the stress film includes at least one of a silicon dioxide film, a magnesium fluoride film, a silicon nitride film, and an aluminum nitride film.

[0023] According to some embodiments of the present application, before the stress film is coated, the back side of the photosensitive chip is a flat surface.

[0024] According to some embodiments of the present application, the portion of the photosensitive chip corresponding to the photosensitive area is substantially flush with the back side of the photosensitive chip.

[0025] According to some embodiments of the present application, a portion of the photosensitive chip corresponding to the photosensitive area protrudes toward the stress film, and a distance of the protrusion ranges from 2 μm to 10 μm.

[0026] According to some embodiments of the present application, the stress film is attached to the entire back side of the photosensitive chip.

[0027] According to some embodiments of the present application, the area of ​​the photosensitive chip is 5mm2-40mm2.

[0028] According to some embodiments of the present application, the photosensitive chip assembly further includes:

[0029] The first intermediate layer is arranged between the photosensitive chip and the stress layer, and the bonding performance between the first intermediate layer and the substrate and the stress layer is better than the bonding performance between the substrate and the stress layer.

[0030] According to some embodiments of the present application, the photosensitive chip assembly further includes:

[0031] The second intermediate layer is arranged on the side of the stress layer opposite to the photosensitive chip, and the second intermediate layer bonds the photosensitive chip assembly to the carrier board on which the photosensitive chip assembly is mounted through an adhesive.

[0032] According to some embodiments of the present application, the photosensitive chip assembly further includes:

[0033] The second intermediate layer is arranged on the side of the stress layer opposite to the photosensitive chip, and the second intermediate layer bonds the photosensitive chip assembly to the carrier board on which the photosensitive chip assembly is mounted through an adhesive.

[0034] According to some embodiments of the present application, the bonding performance between the second intermediate layer and the stress layer and the adhesive is better than the bonding performance between the stress layer and the adhesive.

[0035] According to some embodiments of the present application, the material of the first intermediate layer includes one or more of silicon and silicon dioxide.

[0036] According to some embodiments of the present application, the material of the second intermediate layer includes one or more of porous silicon dioxide, titanium dioxide, and a hydrophilic silicon coating solution.

[0037] According to some embodiments of the present application, the thickness of the first intermediate layer or the second intermediate layer is 10-20 nm.

[0038] According to some embodiments of the present application, the first intermediate layer or the second intermediate layer includes a physical vapor deposition layer and / or a chemical vapor deposition layer.

[0039] According to a second aspect of the present application, a camera module is provided, including:

[0040] A lens assembly, including a lens;

[0041] The photosensitive chip assembly is connected to the lens assembly, and the field curvature of the photosensitive chip assembly is in the same direction as the field curvature of the lens and the difference is within ±10um.

[0042] According to some embodiments of the present application, the camera module further includes:

[0043] A carrier plate, on which the photosensitive chip assembly is arranged;

[0044] The electronic component is arranged on the carrying board.

[0045] According to some embodiments of the present application, the camera module further includes:

[0046] A packaging component is disposed on the carrier plate, wherein the packaging component and the carrier plate surround a cavity for accommodating the photosensitive chip assembly and the electronic element, and the packaging component has a window for exposing the microlens array of the photosensitive chip assembly;

[0047] or

[0048] A packaging component, covering the photosensitive chip assembly and the electronic component, and the packaging component has a window exposing the microlens array of the photosensitive chip assembly; and

[0049] The packaging component is integrally formed on the carrier plate by transfer molding, injection molding, or compression molding;

[0050] or

[0051] A packaging component, including a molding part, is disposed on the carrier board and covers the electronic component; and

[0052] The supporting part is arranged on the molding part. The molding part and the supporting part surround a cavity for accommodating the photosensitive chip component and the electronic element. The supporting part has a window for exposing the microlens array of the photosensitive chip component.

[0053] According to some embodiments of the present application, the camera module further includes:

[0054] A filter element, disposed on the packaging component and covering the window;

[0055] The lens assembly is mounted on the packaging component.

[0056] According to some embodiments of the present application, the carrying plate includes:

[0057] A circuit board, the electronic components and the photosensitive chip assembly are electrically connected to the carrier board;

[0058] or

[0059] A flexible circuit board, the electronic component and the photosensitive chip assembly are arranged on the flexible circuit board and are electrically connected to the flexible circuit board; and

[0060] A reinforcing plate, arranged below the flexible circuit board to support the flexible circuit board;

[0061] or

[0062] a circuit board having an opening, wherein the electronic component is arranged on the circuit board; and

[0063] A reinforcing plate is arranged below the circuit board, the photosensitive chip assembly is arranged on the reinforcing plate and is located in the opening, and the electronic component and the photosensitive chip assembly are electrically connected to the circuit board.

[0064] According to a third aspect of the present application, a terminal device is provided, comprising the above-mentioned camera module.

[0065] Additional aspects and advantages of the present application will be given in part in the description below, and in part will become apparent from the description below, or will be learned through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0066] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without exceeding the scope of protection required by the present application.

[0067] Figure 1 A schematic diagram of the deformation of the photosensitive chip is shown.

[0068] Figure 2 A schematic diagram showing the deformation direction of the photosensitive chip and the image plane of the lens.

[0069] Figure 3 A schematic diagram showing the process of die extrusion bending a photosensitive chip.

[0070] Figure 4 A schematic diagram of the structure of a conventional photosensitive chip is shown.

[0071] Figure 5 A schematic diagram showing the bending principle during the conventional photosensitive chip bonding and curing process.

[0072] Figure 6 A schematic diagram showing the bending process during conventional photosensitive chip bonding and curing.

[0073] Figure 7 A schematic diagram of the structure of a photosensitive chip assembly according to a first exemplary embodiment of the present application is shown.

[0074] Figure 8 A schematic diagram of the bending process of a photosensitive chip assembly according to an exemplary embodiment of the present application is shown.

[0075] Fig. 9 A schematic diagram showing the protrusion distance of the corresponding part of the photosensitive area of ​​the photosensitive chip according to an exemplary embodiment of the present application.

[0076] Fig.10 A schematic diagram showing that the curvature direction of the photosensitive chip is the same as the curvature direction of the lens image plane.

[0077] Fig.11 A schematic diagram of the structure of a photosensitive chip assembly according to a second exemplary embodiment of the present application is shown.

[0078] Fig.12 A second schematic diagram of the structure of a photosensitive chip assembly according to the third exemplary embodiment of the present application is shown.

[0079] Fig.13 A third schematic diagram of the structure of a photosensitive chip assembly according to the fourth exemplary embodiment of the present application is shown.

[0080] Fig.14 A schematic diagram of the fixing structure of the photosensitive chip assembly of an exemplary embodiment of the present application is shown.

[0081] Fig.15 A schematic diagram of the fixing structure of a photosensitive chip assembly according to another exemplary embodiment of the present application is shown.

[0082] Fig.16 A schematic diagram of the package structure of a camera module photosensitive chip assembly according to an example embodiment of the present application is shown.

[0083] Fig.17 A schematic diagram of the package structure of a camera module photosensitive chip assembly according to another example embodiment of the present application is shown.

[0084] Fig.18A second schematic diagram of the package structure of a camera module photosensitive chip assembly according to another example embodiment of the present application is shown.

[0085] Fig.19 A schematic diagram of the camera module structure according to an example embodiment of the present application is shown. DETAILED DESCRIPTION

[0086] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0087] First, the structure and connection process of the existing photosensitive chip will be combined to explain the reason why the deformation direction of the photosensitive chip is opposite to the image surface of the lens.

[0088] Figure 4 A schematic diagram of the structure of a conventional photosensitive chip is shown.

[0089] like Figure 4 As shown, the structure of the photosensitive chip 1100 is respectively a microlens array 111, a Bayer color filter array 112, a photosensitive area 113, a non-photosensitive area 114 such as a circuit layer, and a silicon substrate 115 from top to bottom. The Bayer color filter array 112, the photosensitive area 113, and the non-photosensitive area 114 such as a circuit layer are also referred to as active areas. For ease of description, the photosensitive area 113, the non-photosensitive area 114 such as a circuit layer, and the silicon substrate 115 are referred to as a silicon layer 116 below.

[0090] The microlens array 111 is generally made of an organic film, such as an acrylic thermosetting resin, an acrylic thermoplastic resin, etc. The materials of the photosensitive area 113, the non-photosensitive area 114 such as the circuit layer, and the silicon substrate 115 are mainly inorganic materials, mainly silicon. The photosensitive chip 1100 and the circuit board are usually fixed by applying an adhesive and curing it after heating.

[0091] Figure 5 A schematic diagram showing the bending principle during the conventional photosensitive chip bonding and curing process.

[0092] like Figure 5 As shown, the photosensitive chip 1100 needs to be heated during the bonding and curing process. The thermal expansion coefficient of the microlens array 111 is relatively large, about 30PPM. The thermal expansion coefficient of the silicon layer 116 is about 3PPM. The expansion coefficients of the microlens array 111 and the silicon layer 116 differ too much. During the temperature rise process, the expansion speed of the microlens array 111 is greater than the expansion speed of the silicon layer, causing the photosensitive chip 1100 to bend downward all around, that is, the central area of ​​the photosensitive chip 1100 bulges upward.

[0093] Figure 6 A schematic diagram showing the bending process during conventional photosensitive chip bonding and curing.

[0094] During the bonding and fixing process of the photosensitive chip 1100 and the carrier plate 1200, the adhesive 900 is first applied to the carrier plate 1200. Then, the photosensitive chip 1100 is attached to the carrier plate 1200 through the adhesive 900. Next, the temperature is raised to 100 to 120 degrees Celsius to cure the adhesive 900. In this process, the photosensitive chip 1100 is bent by the heat due to the above reasons, and the central area of ​​the photosensitive chip 1100 protrudes upward, and the adhesive 900 is gradually cured in this process. After the photosensitive chip 1100 is bent to a certain extent, it is fixed by the adhesive 900 and cannot be restored to flatness. Finally, the photosensitive chip 1100 is bent upward in this process, which is inconsistent with the curvature direction of the imaging surface of the lens assembly.

[0095] In order to solve this problem, the inventors have proposed a photosensitive chip assembly. By setting a stress layer on the back side of the photosensitive chip, the photosensitive chip is deformed toward the substrate of the photosensitive chip, so that the bending direction of the photosensitive chip is consistent with the bending direction of the lens imaging surface and maintains a stable bending, thereby improving the clarity of the imaging.

[0096] Figure 7 A schematic diagram of the structure of a photosensitive chip assembly according to the first exemplary embodiment of the present application is shown.

[0097] like Figure 7 As shown, the photosensitive chip assembly 1100 includes a photosensitive chip 1100 and a stress layer 130. The stress layer 130 is arranged on the back side of the photosensitive chip 1100. According to the first exemplary implementation of the present application, the stress layer 130 can be a compensation film whose thermal expansion coefficient is greater than or equal to the thermal expansion coefficient of the microlens array 111. Therefore, during the assembly process, the expansion speed of the compensation film 130 after being heated is greater than the expansion speed of the microlens array 111, and the periphery of the photosensitive chip 1100 will be slightly bent upward, and the central area of ​​the photosensitive chip 1100 will be concave downward, so that the bending direction of the photosensitive area of ​​the photosensitive chip 1100 is the same as the bending direction of the imaging surface of the lens.

[0098] According to some embodiments, the material of the compensation film 130 may be silicon oxide, aluminum oxide, titanium oxide, etc., or magnesium fluoride, etc. The compensation film 130 may include but is not limited to a PVD film and / or a CVD film. The PVD film includes but is not limited to at least one of a vacuum evaporation film, a magnetron sputtering film, and an atomic layer deposition film. The thickness of the compensation film 130 is 0.1um to 10um. The thickness of the photosensitive chip 1100 is generally 100um to 200um. The thickness of the microlens array 111 of the photosensitive chip 1100 is generally equivalent to the thickness of the compensation film 130, or less than the thickness of the compensation film 130.

[0099] In order to ensure that the thickness of the photosensitive chip assembly 1100 after adding the compensation film 130 meets the chip requirements of normal specifications, the thickness of the silicon substrate 115 on the bottom side of the photosensitive chip 1100 can be first ground to ensure that the thickness of the photosensitive chip assembly 1100 after adding the stress layer 130 will not increase.

[0100] Figure 8 A schematic diagram of the bending process of a photosensitive chip assembly according to an exemplary embodiment of the present application is shown.

[0101] like Figure 8 As shown, during the heating and fixing process of the photosensitive chip assembly 1100, since the thermal expansion coefficient of the compensation film 130 is greater than or equal to the thermal expansion coefficient of the microlens array 111 of the photosensitive chip 1100, and the compensation film 130 is located on the back side of the photosensitive chip 1100, and the microlens array 111 is located on the front side of the photosensitive chip 1100, when the photosensitive chip assembly 1100 is heated, the expansion speed of the compensation film 130 is greater than or equal to the microlens array 111.

[0102] See also Figure 8 , when the thermal expansion coefficient of the compensation film 130 is equal to the thermal expansion coefficient of the microlens array 111, the expansion rates of the two are basically the same. Therefore, the photosensitive chip assembly 1100 basically does not bend. Since the thickness of the compensation film 130 is slightly greater than the thickness of the microlens array 111, the expansion amount of the compensation film 130 is slightly greater than the expansion amount of the microlens array 111. At this time, the photosensitive chip assembly 1100 will bend slightly upward on all sides, and its central area will be slightly concave downward, or basically will not bend. Therefore, the photosensitive chip basically does not bend here, which should be understood as the photosensitive chip assembly 1100 is flat or the central area is concave downward.

[0103] like Figure 8 As shown, when the thermal expansion coefficient of the compensation film 130 is greater than the thermal expansion coefficient of the microlens array 111, the expansion speed of the compensation film 130 is greater than the expansion speed of the microlens array 111. The periphery of the photosensitive chip assembly 1100 will bend upward and the central area will be concave downward. At this time, the bending direction of the photosensitive chip 1100 is consistent with the bending direction of the lens imaging surface.

[0104] According to other embodiments of the present application, Figure 7 As shown, the stress layer 130 may also be a stress film and have a predetermined thickness. The stress film 130 may generate stress during the molding process, so that the photosensitive area of ​​the photosensitive chip 110 is deformed toward its substrate (back side). That is, the stress film 130 is plated on the back surface of the silicon substrate, and stress is generated on the photosensitive chip 110 during the coating process, so that the photosensitive area of ​​the photosensitive chip 110 is deformed toward the back side. At this time, the predetermined thickness of the stress film 130 can be determined according to the size of the photosensitive chip 110 and the size that needs to be deformed.

[0105] The stress film 130 generates stress during the coating process, which is different from the prior art. The coating process can be understood as atoms or molecules being coated layer by layer on the surface of the coating body, and stress is generated during the coating process. Instead of only providing a stress film product, the stress film product is attached to the back of the photosensitive chip 110 to generate stress on the photosensitive chip 110.

[0106] The photosensitive chip 110 mainly generates field curvature during the heating and curing process. Figure 1 As shown in , the middle area of ​​the conventional photosensitive chip is arched toward the front, and the two sides are warped toward the back. Therefore, if the stress film 130 is plated on the photosensitive chip 110 before the photosensitive chip 110 is heated and cured, compressive stress will be generated on the back, causing the photosensitive chip 110 to deform toward the back in advance, that is, the photosensitive area of ​​the photosensitive chip 110 and the area below it are bent and arched downward. If the photosensitive chip 110 is heated and cured after the photosensitive chip 110 has undergone field curvature deformation, and the stress film 130 is plated on the photosensitive chip 110 at this time, a tensile stress opposite to the deformation of the photosensitive chip 110 will be generated. In principle, this is possible, but in actual production, the heating and curing process is the process of pasting the photosensitive chip on the circuit board or the reinforcement board, and the coated side needs to be pasted on the circuit board or the reinforcement board. Therefore, in actual operation, it is often chosen to coat the film first and then heat and cure.

[0107] The reason why the stress film 130 generates stress on the photosensitive chip 110 can be explained from a microscopic perspective. During the coating process of the photosensitive chip 110, as the microcrystals of the thin film grow, the effect of surface tension weakens, and the lattice constant of the microcrystal, that is, the side length of the unit cell, should gradually increase to the maximum lattice constant of the film. However, due to the binding effect of the back of the photosensitive chip 110 on the film, the increase in the lattice constant of the microcrystal is hindered. Even if the thickness of the film continues to increase, the lattice constant of the microcrystal is less than the maximum lattice constant of the film. Therefore, the stress film 130 generates stress on the photosensitive chip 110, and the stress causes the photosensitive chip to bulge toward one side of the film. The distance that the portion of the photosensitive chip 110 corresponding to the photosensitive area (that is, the portion of the photosensitive area within the vertical projection of the photosensitive chip 110) bulges toward one side of the stress film 130 can be achieved by controlling the temperature and pressure during the coating process.

[0108] The distance h of the corresponding part of the photosensitive area of ​​the photosensitive chip protruding toward the stress film is defined as: the height of the periphery of the photosensitive area minus the height of the center of the photosensitive area, such as Fig. 9 As shown. ( Fig. 9 (The microlens array is omitted in the figure) In this exemplary embodiment, by controlling the temperature and pressure during the coating process, the distance h by which a specific part of the photosensitive chip protrudes toward the stress film is controlled to be in the range of 2μm-10μm. In this embodiment, the stress film 130 is attached to the entire back side of the photosensitive chip 110, so as to generate as much stress as possible on the photosensitive chip 110. The specific size of the photosensitive chip, the thickness of the coating, and the thickness of the protrusion of the corresponding part of the photosensitive area in the photosensitive chip can all be set according to actual conditions, and this is not a limitation to this embodiment.

[0109] It should be noted that the coating method includes but is not limited to vacuum evaporation, magnetron sputtering, and other physical vapor deposition methods or other chemical vapor deposition methods. The preferred methods are vacuum evaporation and magnetron sputtering. The coating material needs to be selected with good adhesion and large surface energy (that is, the extra energy on the surface of the material relative to the interior) so that the film can be firmly attached to the photosensitive chip 110 and can generate greater stress. Therefore, the material of the stress film 130 may include at least one of silicon dioxide, magnesium fluoride, silicon nitride, and aluminum nitride. The specific method and material of the coating are not intended to limit this embodiment.

[0110] Before coating the stress film 130, the back side of the photosensitive chip 110, i.e., the substrate, needs to be polished. In this embodiment, the thickness of the photosensitive chip can be polished to a range of 100 μm-200 μm. Correspondingly, the coating thickness of the stress film 130 is 0.1 μm-10 μm, and the area of ​​the photosensitive chip 110 is 5 mm2-40 mm2.

[0111] By setting a stress layer on the back side of the photosensitive chip, the photosensitive chip can have two situations after the final deformation: First, the part of the photosensitive chip corresponding to the photosensitive area and the part corresponding to the non-photosensitive area are basically flush, that is, the back side of the entire photosensitive chip component forms a plane (such as Figure 8 Second, the part corresponding to the photosensitive area in the photosensitive chip bulges toward the stress layer, and the bulging direction is the same as the direction of the image plane curvature of the lens (such as Figure 8 shown on the right).

[0112] Fig.10 A schematic diagram showing that the curvature direction of the photosensitive chip is the same as the curvature direction of the lens image plane.

[0113] like Fig.10 For example, the image plane J of the lens is shaped like a smiling face with its mouth facing upwards. Because the image plane of the lens is a smiling face, the shape of the chip should also be made into a smiling face, that is, the photosensitive chip or the photosensitive area of ​​the photosensitive chip is convex downwards, so that the shape of the photosensitive chip corresponds to the shape of the lens image plane, receiving more light information, thereby avoiding the situation where the middle is clear and the sides are blurred.

[0114] Assuming that the actual field curvature of the lens assembly is A, when the stress layer adopts a compensation film, the field curvature of the photosensitive chip 1100 can be controlled to B by adjusting the thermal expansion coefficient, heating temperature, heating time and other parameters of the compensation film, so that B is close to A and in the same direction. When the stress layer adopts a stress film, the field curvature of the photosensitive chip can be controlled to B by adjusting the heating temperature, heating time, heating pressure and other parameters of the stress film during the coating process, so that B is close to A and in the same direction. According to some embodiments of the present application, the difference between B and A can be controlled within ±10um. According to other embodiments of the present application, the difference between B and A can be controlled within ±5um. Thereby, the field curvature of the photosensitive chip 1100 can match the field curvature of the lens, so that the overall field curvature of the camera module can be reduced, thereby improving the photo quality of the camera module.

[0115] Furthermore, according to some embodiments of the present application, the thickness of the stress layer is 0.1 μm to 10 μm, and the stress layer can be formed by coating processes such as physical vapor deposition and chemical vapor deposition. Traditional photosensitive chips need to be bonded with a compensation layer before being attached to the circuit board. In comparison, setting a stress layer can save a glue coating process, thereby reducing the field curvature caused by the difference in thermal expansion coefficients between multiple layers of different media, reducing the risk of chip protrusions caused by uneven adhesive coating, and at the same time does not significantly increase the chip thickness.

[0116] In addition, traditional compensation layers are generally made of metal materials. The thermal expansion coefficient of metal materials is generally 10-20ppm / ℃, which can easily cause thermal mismatch with materials such as photosensitive chips and circuit boards, resulting in problems such as mechanical fracture between the compensation layer and the chip and circuit board. In the embodiment of the present application, the thermal expansion coefficient of the compensation film is greater than or equal to the thermal expansion coefficient of the microlens array, and the thermal expansion coefficient of the stress film is close to the thermal expansion coefficient of the microlens array, both of which can compensate for the field curvature caused by the difference in thermal expansion coefficients inside the photosensitive chip. At the same time, it can also effectively alleviate the warping and field curvature problems of the photosensitive chip in the subsequent process of attaching the photosensitive chip to the circuit board.

[0117] According to some embodiments of the present application, during use, the stress layer and the photosensitive chip may have a large performance difference and poor "affinity", that is, the adhesion between the two is poor, causing the stress layer to fall off the photosensitive chip, which is not conducive to maintaining the bending direction. Therefore, the inventors propose a second photosensitive chip assembly structure based on the photosensitive chip assembly of the first exemplary embodiment.

[0118] Fig.11 A schematic diagram of the structure of a photosensitive chip assembly according to a second exemplary embodiment of the present application is shown.

[0119] like Fig.11 As shown, the photosensitive chip assembly 1100 includes a photosensitive chip 110, a stress layer 130 and a first intermediate layer 120. The stress layer 130 is disposed on the back side of the photosensitive chip 110. The first intermediate layer 120 is disposed between the photosensitive chip 110 and the stress layer 130. The material properties of the first intermediate layer 120 are between the bottom material of the photosensitive chip 110 and the material of the stress layer 130, which can neutralize the incompatible properties of the two, play a role similar to a "bridge", and increase the bonding force between the two.

[0120] The material of the first intermediate layer 120 has little or no effect on the bending of the photosensitive chip assembly 1100, or has the same effect on the bending of the chip as the stress layer 130. Specifically, the material of the first intermediate layer 120 can be one or more of silicon and silicon dioxide, but the present application is not limited thereto.

[0121] According to some embodiments, the first intermediate layer 120 has a thickness of 10-20 nm and can be formed by using a coating process such as physical vapor deposition, chemical vapor deposition, such as vacuum evaporation, magnetron sputtering, etc., or by using a process such as atomic layer deposition.

[0122] Similarly, when the photosensitive chip assembly is attached to the circuit board through an adhesive, the stress layer and the adhesive may not be suitable for each other and may not be easy to bond. For this reason, the inventor proposes a third and a fourth photosensitive chip assembly structure based on the photosensitive chip assembly of the first and second exemplary embodiments.

[0123] Fig.12 A second schematic diagram of the structure of a photosensitive chip assembly according to the third exemplary embodiment of the present application is shown; Fig.13 A third schematic diagram of the structure of a photosensitive chip assembly according to the fourth exemplary embodiment of the present application is shown.

[0124] Fig.12 The photosensitive chip assembly structure shown does not include the first intermediate layer 120; Fig.13 The photosensitive chip assembly structure shown includes a first intermediate layer 120. Fig.12 , 13 Combined for illustration.

[0125] like Fig.12 As shown, the photosensitive chip assembly 1100 includes a photosensitive chip 110, a stress layer 130 and a second intermediate layer 140. The stress layer 130 is disposed on the back side of the photosensitive chip 110. The second intermediate layer 140 is disposed on the side of the stress layer 130 opposite to the photosensitive chip 110. Fig.13 As shown, the photosensitive chip assembly 1100 includes a photosensitive chip 110, a stress layer 130, a first intermediate layer 120, and a second intermediate layer 140. The stress layer 130 is disposed on the back side of the photosensitive chip 110. The first intermediate layer 120 is disposed between the photosensitive chip 110 and the stress layer 130. The second intermediate layer 140 is disposed on the side of the stress layer 130 opposite to the photosensitive chip 110.

[0126] The material of the second intermediate layer 140 is suitable for stably bonding with the stress layer 130 and the adhesive, wherein the adhesive serves to bond the photosensitive chip 110 to the circuit board. At the same time, it does not affect the bending of the photosensitive chip 110 and the stress layer 130, or its influence is consistent with the influence of the stress layer 130 on the bending of the photosensitive chip 110. At this time, the bending of the photosensitive chip assembly 1100 is the result of the combined influence of the stress layer 130 and the second intermediate layer 140.

[0127] Specifically, the bonding performance between the second intermediate layer 140 and the stress layer 130 and the adhesive is better than the bonding performance between the stress layer 130 and the adhesive. The material of the second intermediate layer 140 can be a nano coating that increases the bonding force between the stress layer 130 and the adhesive, which is generally a hydrophilic material, such as porous silicon dioxide, titanium dioxide, a hydrophilic silicon coating liquid, etc., but the present application is not limited thereto.

[0128] According to some embodiments, the thickness of the second intermediate layer is 10-20 nm, and can be formed by coating processes such as physical vapor deposition, chemical vapor deposition, such as vacuum evaporation, magnetron sputtering, etc., or by atomic layer deposition and other processes to form the second intermediate layer 140.

[0129] like Figure 10-13 As shown, the thickness of the photosensitive chip assembly 1100 increases due to the addition of the stress layer 130, the first intermediate layer 120, and the second intermediate layer 140. Therefore, before forming the stress layer 130, the first intermediate layer 120, and the second intermediate layer 140, the thickness of the silicon substrate at the bottom of the photosensitive chip 110 may be ground to reduce the thickness of the chip after molding to meet the usual chip requirements.

[0130] When the above-mentioned photosensitive chip assembly is used in a camera module, it is usually fixed on a carrier board together with the electronic components. According to some embodiments of the present application, the carrier board can be a separate circuit board, and the electronic components and the photosensitive chip assembly are electrically connected to the carrier board. According to other embodiments of the present application, such as Fig.14 As shown, the carrier board 1200 may further include a flexible circuit board 1210 and a reinforcement board 1220. The electronic component 1300 and the photosensitive chip assembly 1100 are disposed on the flexible circuit board 1210 and are electrically connected to the flexible circuit board 1210, and the stress layer 130 is located between the sensing chip 110 and the flexible circuit board 1210. The reinforcement board 1220 is disposed under the flexible circuit board 1210 to support the flexible circuit board 1210.

[0131] Alternatively, if Fig.15 As shown, the carrier plate 1200 also includes a circuit board 1210 and a reinforcement plate 1220, the circuit board 1210 has an opening 1211, and the electronic component 1300 is arranged on the circuit board 1210. The reinforcement plate 1220 is arranged below the circuit board 1210, and the photosensitive chip assembly 1100 is arranged on the reinforcement plate 1220 and located in the opening 1211. The electronic component 1300 and the photosensitive chip assembly 1100 are electrically connected to the circuit board 1220, and the stress layer 1300 is located between the sensing chip 110 and the circuit board 1210. In this embodiment, the photosensitive chip assembly 1100 is arranged on the reinforcement plate 1220 and located in the opening 1211. Such a setting can reduce the thickness of the entire camera module.

[0132] The above fixing scheme is introduced by taking the photosensitive chip assembly of the first exemplary embodiment of the present application as an example, and is also applicable to the photosensitive chip assemblies in other exemplary embodiments.

[0133] Fig.16 A schematic diagram of the packaging structure of a camera module photosensitive component according to an exemplary embodiment of the present application is shown.

[0134] like Fig.16 As shown, the camera module photosensitive component package 1000 includes a photosensitive chip component 1100, a carrier board 1200, an electronic component 1300, a packaging component 1400, and a filter element 1500.

[0135] The photosensitive chip assembly 1100 is adhered to the carrier board 1200 by the adhesive 900. The carrier board 1200 is electrically connected to the photosensitive chip assembly 1100 to transmit digital signals. The electronic component 1300 is arranged on the carrier board 1200 and is electrically connected to the carrier board 1200 to provide an auxiliary circuit for the transmission and processing of digital signals.

[0136] The packaging component 1400 is disposed on the carrier board 1200. The packaging component 1400 and the carrier board 1200 surround a cavity 1441 for accommodating the photosensitive chip assembly 1100 and the electronic component 1300. The packaging component 1400 has a light-transmitting window 1442 that exposes the microlens array 111 of the photosensitive chip assembly 1100. The filter element 1500 is disposed on the packaging component 1400 and covers the light-transmitting window 1442, and is used to filter out infrared light to improve the camera effect.

[0137] When the photosensitive chip assembly 1100 is attached to the carrier board 1200 through the adhesive 900 and needs to be heated to solidify the adhesive 900, the central area of ​​the photosensitive chip 110 remains flat or concave downward, which can improve the field curvature compared to the central area of ​​the photosensitive chip 110 protruding upward in the prior art. As a result, the camera module can take clear photos of the center and the surrounding areas. This package has a simple structure and a simple packaging process.

[0138] The packaging structure provided in this embodiment can prevent contamination of photosensitive chips, electronic components, circuit boards, etc.

[0139] Fig.17 A schematic diagram of the package structure of a camera module photosensitive component according to another example embodiment of the present application is shown.

[0140] Optionally, the packaging component 1400 is integrally formed on the carrier board 1200 by transfer molding, injection molding, or compression molding. The packaging component 1400 covers the photosensitive chip assembly 1100 and the electronic component 1300, and the packaging component 1400 has a light-transmitting window 1442 that exposes the microlens array 111 of the photosensitive chip assembly 1100.

[0141] The dimensions of this packaging structure are reduced in length, width and height, which prevents the adhesive from precipitating, and the packaging component 1400 further protects the electronic components and connecting wires.

[0142] Fig.18 A second schematic diagram of the structure of a camera module photosensitive component package according to another example embodiment of the present application is shown.

[0143] Optionally, the packaging component 1400 includes a molding part 1443 and a supporting part 1444. The molding part 1443 is disposed on the carrier board 1200 and covers the electronic component 1300. The supporting part 1444 is disposed on the molding part 1443, and the molding part 1443 and the supporting part 1444 surround a cavity for accommodating the photosensitive chip component 1100 and the electronic component 1300, and the supporting part 1444 has a light-transmitting window 1442 for exposing the microlens array 111 of the photosensitive chip component 1100.

[0144] This packaging structure has a simple packaging process, produces less warping and dirt during the packaging process, and has reduced dimensions in both length and width.

[0145] It should be noted that Figure 16-18 The schematic diagram of the photosensitive component package structure shown in the figure is illustrated by taking the photosensitive chip component of the first exemplary embodiment of the present application as an example, and is also applicable to the photosensitive chip components of other exemplary embodiments of the present application.

[0146] In addition, the present application also provides a camera module, including the above-mentioned photosensitive chip component package.

[0147] Fig.19 A schematic diagram of the camera module structure according to an example embodiment of the present application is shown.

[0148] like Fig.19 As shown, the camera module 2000 also includes a lens assembly 1600, which is configured and mounted on the packaging component 1400, and is used to capture and focus the target object to be photographed to transmit it to the photosensitive chip assembly 1100. The lens assembly 1600 includes a lens 1610, a lens carrier or a motor 1620. The field curvature of the photosensitive chip assembly 1100 is in the same direction as the field curvature of the lens 1610, and the difference is controlled within ±10um.

[0149] It should be noted that Fig.19 The schematic diagram of the camera module structure shown in the figure takes the photosensitive chip component of the first exemplary embodiment of the present application as an example for explanation, and is also applicable to the photosensitive chip components of other exemplary embodiments of the present application.

[0150] The photosensitive chip assembly provided by the present application controls the bending direction and degree of the photosensitive chip by setting a stress layer on the back of the traditional photosensitive chip, so as to control the field curvature of the photosensitive chip, so that the bending direction of the photosensitive chip is consistent with the field curvature direction of the lens, thereby improving the clarity of the imaging. In addition, in order to ensure a good combination between the stress layer and the photosensitive chip or between the circuit boards, a first intermediate layer and / or a second intermediate layer are set in the photosensitive chip assembly, so that the curvature of the photosensitive chip can be maintained for a long time.

[0151] The embodiments of the present application are described in detail above. Specific examples are used herein to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method and its core idea of ​​the present application. At the same time, changes or deformations made by those skilled in the art based on the ideas of the present application, the specific implementation methods and the scope of application of the present application, all belong to the scope of protection of the present application. In summary, the content of this specification should not be construed as a limitation on the present application.

Claims

1. A photosensitive chip assembly, comprising: A photosensitive chip having a photosensitive area and a non-photosensitive area located at the edge of the photosensitive area; A stress layer is arranged on the back side of the photosensitive chip, and a portion corresponding to the photosensitive area protrudes toward the stress layer; as well as The first intermediate layer is arranged between the photosensitive chip and the stress layer, and the bonding performance between the first intermediate layer and the substrate of the photosensitive chip and the stress layer is better than the bonding performance between the substrate of the photosensitive chip and the stress layer.

2. The photosensitive chip assembly according to claim 1, wherein: The thickness of the stress layer is 0.1um to 10um.

3. The photosensitive chip assembly according to claim 2, wherein: The thickness of the photosensitive chip is 100um to 200um.

4. The photosensitive chip assembly according to claim 3, wherein: The stress layer comprises: a compensation film, wherein the thermal expansion coefficient of the compensation film is greater than or equal to the thermal expansion coefficient of the microlens array.

5. The photosensitive chip assembly according to claim 4, wherein: The thickness of the compensation film is greater than or equal to the thickness of the microlens array.

6. The photosensitive chip assembly according to claim 4, wherein: The material of the compensation film includes at least one of silicon oxide, magnesium fluoride, aluminum oxide and titanium oxide.

7. The photosensitive chip assembly according to claim 4, wherein: The compensation film includes a PVD film and / or a CVD film.

8. The photosensitive chip assembly according to claim 7, wherein: The PVD film includes at least one of a vacuum evaporation film, a magnetron sputtering film, and an atomic layer deposition film.

9. The photosensitive chip assembly according to claim 3, wherein: The photosensitive chip further includes an active area located on the substrate and a microlens array located on the active area. The active area also includes a photosensitive area, which is arranged below the microlens array to receive light from the outside world reaching the front of the photosensitive chip. The stress layer includes a stress film, and the stress film has a predetermined thickness. The stress generated during the coating process causes the photosensitive area of ​​the photosensitive chip to deform toward the substrate of the photosensitive chip.

10. The photosensitive chip assembly according to claim 9, wherein: The stress film includes at least one of a silicon dioxide film, a magnesium fluoride film, a silicon nitride film, and an aluminum nitride film.

11. The photosensitive chip assembly as described in claim 9, before the stress film is coated, the back side of the photosensitive chip is a flat surface.

12. The photosensitive chip assembly according to claim 9, wherein: The portion of the photosensitive chip corresponding to the photosensitive area is substantially flush with the back side of the photosensitive chip.

13. The photosensitive chip assembly according to claim 9, wherein: A portion of the photosensitive chip corresponding to the photosensitive area protrudes toward the stress film, and a distance of the protrusion ranges from 2 μm to 10 μm.

14. The photosensitive chip assembly according to claim 9, wherein: The stress film is attached to the entire back side of the photosensitive chip.

15. The photosensitive chip assembly as claimed in claim 9, wherein: The area of ​​the photosensitive chip is 5mm 2 -40mm 2 .

16. The photosensitive chip assembly according to claim 1, wherein: The photosensitive chip assembly also includes: a second intermediate layer, which is arranged on the side of the stress layer opposite to the photosensitive chip, and the second intermediate layer bonds the photosensitive chip assembly to a carrier board on which the photosensitive chip assembly is mounted through an adhesive.

17. The photosensitive chip assembly according to any one of claims 4 to 8, wherein: The photosensitive chip assembly also includes: a second intermediate layer, which is arranged on the side of the stress layer opposite to the photosensitive chip, and the second intermediate layer bonds the photosensitive chip assembly to a carrier board on which the photosensitive chip assembly is mounted through an adhesive.

18. The photosensitive chip assembly according to claim 17, wherein: The bonding performance between the second intermediate layer and the stress layer and the adhesive is better than the bonding performance between the stress layer and the adhesive.

19. The photosensitive chip assembly according to claim 1, wherein: The material of the first intermediate layer includes one or more of silicon and silicon dioxide.

20. The photosensitive chip assembly according to claim 17, wherein: The material of the second intermediate layer includes one or more of porous silicon dioxide, titanium dioxide, and hydrophilic silicon coating liquid.

21. The photosensitive chip assembly according to claim 17, wherein: The thickness of the first intermediate layer or the second intermediate layer is 10-20 nm.

22. The photosensitive chip assembly according to claim 17, wherein: The first intermediate layer or the second intermediate layer includes a physical vapor deposition layer and / or a chemical vapor deposition layer.

23. A camera module, comprising: A lens assembly, including a lens; The photosensitive chip assembly as described in any one of claims 1-22 is connected to the lens assembly, and the field curvature of the photosensitive chip assembly is in the same direction as the field curvature of the lens and the difference is within ±10um.

24. The camera module according to claim 23, wherein: The camera module also includes: a carrier board, on which the photosensitive chip assembly is arranged; and an electronic component, which is arranged on the carrier board.

25. The camera module according to claim 24, wherein: The camera module also includes: A packaging component is disposed on the carrier plate, wherein the packaging component and the carrier plate surround a cavity for accommodating the photosensitive chip assembly and the electronic element, and the packaging component has a window for exposing the microlens array of the photosensitive chip assembly; or A packaging component, covering the photosensitive chip assembly and the electronic component, and the packaging component has a window exposing the microlens array of the photosensitive chip assembly; and the packaging component is integrally formed on the carrier board by transfer molding, injection molding, or compression molding; or The packaging component includes a molding portion, which is arranged on the carrier board and covers the electronic component; and a supporting portion, which is arranged on the molding portion. The molding portion and the supporting portion surround a cavity for accommodating the photosensitive chip component and the electronic component, and the supporting portion has a window that exposes the microlens array of the photosensitive chip component.

26. The camera module according to claim 25, wherein: The camera module also includes: a filter element, which is arranged on the packaging component and covers the window; and the lens assembly is installed on the packaging component.

27. The camera module according to claim 24, wherein: The bearing plate comprises: A circuit board, the electronic components and the photosensitive chip assembly are electrically connected to the carrier board; or A flexible circuit board, the electronic components and the photosensitive chip assembly are arranged on the flexible circuit board and are electrically connected to the flexible circuit board; and a reinforcing plate is arranged under the flexible circuit board to support the flexible circuit board; or a circuit board having an opening, wherein the electronic component is arranged on the circuit board; and A reinforcing plate is arranged below the circuit board, the photosensitive chip assembly is arranged on the reinforcing plate and is located in the opening, and the electronic component and the photosensitive chip assembly are electrically connected to the circuit board.

28. A terminal device, comprising a camera module as described in any one of claims 23-27.