Reinforced film, optical member, and electronic member

By using an adhesive layer with a specific composition in the reinforcing film, the problems of insufficient flexural recovery and flexural retention are solved, and a suitable variation in light peel and adhesion is achieved, making it suitable for equipment subject to repeated bending.

CN116096570BActive Publication Date: 2026-06-09NITTO DENKO CORP

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
NITTO DENKO CORP
Filing Date
2021-07-27
Publication Date
2026-06-09

AI Technical Summary

Technical Problem

Existing reinforcing films are difficult to maintain good flexural resilience and flexural holding force under repeated bending or flexing, and the changes in adhesive force are not easy to control, which affects the yield and operability of the equipment.

Method used

An adhesive layer comprising polymer (A) and polymer (B) is used. Polymer (B) contains a polyorganosiloxane backbone and (meth)acrylic monomer units, with a surface elastic modulus in the range of 1 to 20 kPa and a weight-average molecular weight of 10,000 to 100,000. The change in adhesive force is controlled by adjusting the bulk elastic modulus and loss modulus.

Benefits of technology

It achieves light peeling resistance in the initial stage of application, and a significant increase in adhesion in the later stage. It has good flexural recovery and flexural retention, and is suitable for repeated bending environments where it is not prone to peeling or other defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116096570B_ABST
    Figure CN116096570B_ABST
Patent Text Reader

Abstract

This invention provides a reinforcing film that exhibits mild peel resistance in the initial stage of adhesion to an adherend, followed by a significant increase in adhesive strength, and possesses flexural recovery and flexural retention properties. The reinforcing film includes an adhesive layer. The adhesive layer comprises a polymer (A) and a polymer (B). The polymer (B) comprises monomer units having a polyorganosiloxane backbone and (meth)acrylic acid monomer units. Furthermore, the adhesive layer has a surface elastic modulus of 1–20 kPa at 23°C. Moreover, the polymer (B) has a weight-average molecular weight of 10,000–100,000.
Need to check novelty before this filing date? Find Prior Art