Resistive Random Access Memory and Its Fabrication Method
By adding metal layer deposition during the fabrication of resistive switching memory and completing the deposition of both the metal layer and the resistive switching layer on the same machine, the problem of electrical instability after chemical mechanical polishing was solved, thereby improving the electrical properties and production efficiency of the resistive switching memory.
Patent Information
- Application Number
- CN202310450651.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-04-24
AI Technical Summary
In existing resistive switching memory fabrication processes, chemical residues on the film surface and environmental changes after chemical mechanical polishing lead to electrical instability, and the production process time is difficult to control precisely, affecting the electrical properties of the memory.
An additional metal layer is deposited before the resistive switching layer, and both the metal layer and the resistive switching layer are deposited on the same deposition machine to avoid the impact of environmental changes and the transfer of multiple machines.
It improves the electrical stability and controllability of the resistive switching memory, reduces the probability of chemical residues and compound formation, and increases production efficiency.
Smart Images

Figure CN116600631B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of resistive random access memory (RRAM) technology, and more specifically, to a RRAM and its fabrication method. Background Technology
[0002] Resistive Random Access Memory (ReRAM) has attracted increasing attention due to its advantages such as low voltage, high speed, low power consumption, simple structure, compatibility with traditional CMOS (Complementary Metal Oxide Semiconductor) processes, low cost, and high density. It is considered a new type of memory that may replace flash memory as the mainstream storage product. The existing fabrication process of ReRAM is as follows: Figure 1 As shown, the lower electrode (BE) is first fabricated through thin film deposition and chemical mechanical polishing (CMP). Then, the gap film for the upper electrode (TE) is fabricated through thin film deposition. Finally, the overall resistive switching memory (RSM) is fabricated through photolithography and etching. The disadvantages of performing the resistive switching layer and upper electrode deposition after the CMP step are as follows: 1) CMP can leave chemical residues on the film surface, affecting the electrical properties of the RSM. 2) Since CMP and deposition are performed on separate CMP and deposition machines, the environmental changes during wafer transfer between the two machines can easily lead to compound formation on the lower electrode surface. Furthermore, the wafer transfer from the CMP machine to the deposition machine involves a process of running between two different machines, making precise time control between CMP and deposition impossible. The increased production time also increases the probability of compound formation on the lower electrode surface, thus affecting the RSM's electrical properties.
[0003] Therefore, there is an urgent need for a resistive switching memory (RSM) fabrication process that can improve the production efficiency of RSMs. Summary of the Invention
[0004] The purpose of this invention is to provide a resistive random access memory and its fabrication method to solve at least one problem existing in the prior art.
[0005] To achieve the above objectives, the present invention provides a method for fabricating a resistive switching memory, the method comprising: generating two electrode layers, and generating a metal layer and a resistive switching layer, wherein the metal layer and the resistive switching layer are located between the two electrode layers.
[0006] Further, a preferred method involves generating two electrode layers, the two electrode layers including a first electrode layer and a second electrode layer; and generating a metal layer and a resistive switching layer, the metal layer and the resistive switching layer being located between the two electrode layers; the method includes:
[0007] A first electrode layer is formed on the substrate, and a metal layer is formed on the first electrode layer;
[0008] A resistive switching layer and a second electrode layer are formed on the metal layer.
[0009] Furthermore, a preferred method is that the metal layer includes a first metal layer and a second metal layer.
[0010] Furthermore, a preferred method further includes sequentially forming a second metal layer, a resistive switching layer, and a second electrode layer on the first metal layer.
[0011] In a second aspect, the present invention provides a resistive switching memory comprising a first electrode layer, a second electrode layer and a resistive switching layer located between the first electrode layer and the second electrode layer, wherein a metal layer is disposed between the first electrode layer and the resistive switching layer.
[0012] Furthermore, a preferred structure is that the metal layer includes a first metal layer and a second metal layer.
[0013] Furthermore, in a preferred structure, the material of the first metal layer is W, Lr, Ru, or Pt.
[0014] Furthermore, a preferred structure is that the thickness of the first metal layer is 20nm to 180nm.
[0015] Furthermore, in a preferred configuration, the material of the second metal layer is W, Lr, Ru, or Pt.
[0016] Furthermore, a preferred structure is that the thickness of the second metal layer is 10 nm to 100 nm.
[0017] Furthermore, a preferred structure is that the thickness of the second metal layer is 20 nm to 40 nm.
[0018] Furthermore, a preferred structure further includes a via-filling layer, which is used to fill the vias of the first electrode layer; the metal layer, the resistive switching layer, and the second electrode layer are sequentially deposited on the via-filling layer.
[0019] Thirdly, the present invention provides a storage unit, which includes a gate and a resistive switching memory connected to the gate. The gate may be a three-terminal gate device.
[0020] Fourthly, the present invention provides a storage device, which includes a storage controller and a resistive random access memory (RRAM), wherein the storage controller is used to read and write data to the RRAM.
[0021] Fifthly, the present invention provides an electronic device, including a circuit board and a resistive random access memory connected to the circuit board.
[0022] As described above, the present invention provides a resistive switching memory (RSM), its fabrication method, memory cell, memory device, and electronic device. This invention adds a metal deposition step before the resistive switching layer deposition and adds a second metal layer, which is deposited on the first metal layer using the same deposition equipment as the resistive switching layer. The beneficial effects are as follows: 1) Since there are no other process flows between the resistive switching layer and the metal layer, the influence of other processes on the resistive switching layer is reduced. 2) Since the resistive switching layer and the metal layer deposition are completed using the same deposition equipment, environmental changes during wafer transfer between two equipments are avoided, preventing an increase in the probability of compound formation on the electrode surface. 3) Reducing the wafer transfer process between two different equipments before the resistive switching layer is formed makes the production process time controllable, preventing an increase in the probability of compound formation on the lower electrode surface due to prolonged production time, thereby ensuring the electrical properties of the RSM.
[0023] To achieve the foregoing and related objectives, one or more aspects of the invention include the features that will be described in detail below and particularly pointed out in the claims. The following description details certain exemplary aspects of the invention. However, these aspects indicate only a few of the various ways in which the principles of the invention can be used. Furthermore, the invention is intended to include all such aspects and their equivalents. Attached Figure Description
[0024] Figure 1 This is a schematic diagram of the existing resistive switching memory fabrication process.
[0025] Figure 2 This is a schematic diagram of the resistive random access memory provided in Embodiment 1 of the present invention;
[0026] Figure 3 This is a flowchart illustrating the manufacturing principle of the resistive random access memory provided in Embodiment 1 of the present invention;
[0027] Figure 4 This is a schematic diagram of the fabrication process of the resistive switching memory provided in Embodiment 2 of the present invention;
[0028] Figure 5 This is a schematic diagram of the resistive random access memory according to Embodiment 2 of the present invention;
[0029] Figure 6 This is a schematic diagram of the resistive random access memory according to Embodiment 3 of the present invention.
[0030] 1. Bottom electrode via; 2. Dielectric layer; 3. Metal layer; 4. Resistive switching layer; 5. Top electrode; 6. Sidewall protective layer; 7. Bottom electrode. Detailed Implementation
[0031] It should be understood that the specific embodiments described herein are for illustrative purposes only and are not intended to limit the scope of the invention. Where specific techniques or conditions are not specified in the embodiments, they should be performed in accordance with the techniques or conditions described in the literature in this field, or according to the product instructions. Reagents or instruments whose manufacturers are not specified can be purchased from legitimate channels as conventional products.
[0032] Memory is a storage device used in modern information technology to store information. Its main function is to store various types of data (such as business data and program data). Memory typically uses physical devices (e.g., memory cells) with two stable states (represented by "0" and "1" respectively) to achieve its storage function. Memory can characterize stored data based on the amount of stored charge. For example, Dynamic Random Access Memory (DRAM) and Flash Memory typically characterize stored data based on the amount of stored charge. Memory can also characterize stored data based on the magnitude of resistance. For example, Resistive Random Access Memory (RRAM) typically characterizes stored data based on the device's resistance. RRAM is a type of non-volatile memory with adjustable resistance. The RRAM cell structure uses a MIM capacitor structure, with an insulating layer or semiconductor functional material layer sandwiched between the upper and lower electrodes, also known as a sandwich structure. Specifically, RRAM can control the device resistance by controlling the movement of oxygen ions, thereby achieving its storage function. The memory array can adopt a crossbar array structure. This crossbar array structure has simple manufacturing process, high density, and good scaling capability.
[0033] Figure 1 This diagram illustrates the fabrication process of existing resistive random access memory (RRAM); in the prior art, such as Figure 1 As shown, currently, resistive switching layer and upper electrode deposition are performed after chemical mechanical polishing (CMP) of film 4. Depositing the resistive switching layer on top of the CMP-treated film presents two problems: 1. Chemical residues on the film surface after CMP affect the electrical properties of the RRAM. 2. CMP and deposition are performed on different machines. During wafer transfer between the two machines, environmental changes can easily lead to compound formation on the lower electrode surface. Furthermore, the time interval between the CMP and deposition processes is increased due to the need for precise control of the CMP-to-deposition time. The longer the time, the more likely compounds are to form on the lower electrode surface, thus affecting the RRAM electrical properties. This invention adds a metal layer deposition (film 5) before resistive switching layer deposition to block the CMP-treated film surface (films 3 and 4), thereby improving the problem of the interface between the resistive switching layer and the lower electrode affecting the RRAM electrical properties.
[0034] Example 1
[0035] To illustrate the resistive random access memory, its manufacturing method, and electronic device provided by this invention. Figure 2 The structure of an RRAM according to Embodiment 1 of the present invention is shown. Figure 3 The flowchart of a method for manufacturing an RRAM structure according to Embodiment 1 of the present invention is shown.
[0036] like Figure 2 As shown, the present invention provides a resistive switching memory (RSM) comprising a first electrode layer, a second electrode layer, and a resistive switching layer located between the first electrode layer and the second electrode layer, wherein a metal layer 3 is disposed between the first electrode layer and the resistive switching layer. In this embodiment, the first electrode layer is a lower electrode 7; the second electrode layer is an upper electrode 5. Specifically, it includes a film 1, films 2 and 3 as dielectric layers, a lower electrode film 4 (i.e., film 4 fills the first electrode via 1 formed by films 2 and 3), a film 5 as a metal layer, a film 6 as a resistive switching layer, a film 7 as an upper electrode, and a film 8 as a sidewall protective layer.
[0037] The resistive switching material layer of the resistive switching memory can be one or more transition metal oxides such as Ni, Ti, Al, Ta, and Hf. The resistive switching mechanism of such materials is mainly due to the formation of oxygen vacancy conductive filaments by the movement of oxygen ions. Simultaneously, the number of defects in the resistive switching material layer directly affects the resistive switching characteristics of the device. Since nitrogen atoms have lower binding energy to metal atoms, nitrogen-containing transition metal oxides often exhibit better resistive switching performance. Based on this, the aforementioned resistive switching layer can be generated on the electrode layer by atomic layer deposition (ALD) or sputtering. The thickness of the resistive switching layer can be set according to actual needs. For example, an 8nm thick resistive switching layer can be generated on the lower electrode by ALD. The material of this resistive switching layer can be selected according to actual needs; for example, the material of the resistive switching layer can be any of the transition metal oxides such as HfOx, NiO, TiO2, Al2O3, and Ta2O5. The lower electrode is usually formed of a metallic material. This metallic material includes, but is not limited to, copper, aluminum, titanium, titanium nitride, silver, nickel, platinum, and palladium. Based on this, the lower electrode can be generated by PVD, and the upper electrode can be generated by sputtering. In some embodiments, the thickness of the upper electrode can be equal to the thickness of the lower electrode, for example, it can be 20 nm. In other embodiments, the thickness of the upper electrode may not be equal to the thickness of the lower electrode. Similarly, the material of the upper electrode can be the same as the material of the lower electrode, for example, both can be TiN. In some embodiments, the material of the upper electrode may also be different from the material of the lower electrode.
[0038] The material of the metal layer can be, but is not limited to, W, Lr, Ru, or Pt. The thickness of the via filling layer is set to be 20 nm to 180 nm, which is the same as the thickness of the first metal layer. In this invention, a metal deposition step is added before resistive switching deposition. That is, the resistive switching layer is minimized from the influence of environmental factors, thereby improving the electrical properties of the RRAM film and the stability of the process.
[0039] like Figure 3 As shown, this invention provides a method for fabricating a resistive switching memory (RRAM). The method includes: generating two electrode layers, an upper electrode layer 5 and a lower electrode layer 7, and generating a metal layer 3 and a resistive switching layer 4, with the metal layer 3 and the resistive switching layer 4 located between the upper electrode layer 5 and the lower electrode layer 7. That is, the lower electrode layer 7 is generated first, then the metal layer 3 and the resistive switching layer 4 are generated sequentially, and finally the upper electrode layer 5 is generated. By adding a metal layer 3 before the resistive switching layer 4 is generated, the surface of the films (film 3 and film 4) after chemical mechanical polishing is blocked, thereby improving the problem of the interface between the resistive switching layer and the lower electrode affecting the electrical properties of the RRAM.
[0040] Specifically, the process includes the following steps: S110, forming a first electrode layer, i.e., the lower electrode 7, on the substrate; S120, forming a metal layer 3 on the lower electrode 7; S130, forming a resistive switching layer 4 and an upper electrode layer 5 on the metal layer 3. The metal layer can be, but is not limited to, being deposited separately by a single deposition equipment, or it can be simultaneously formed by the equipment used to grow the resistive switching layer. No specific limitations are imposed here.
[0041] In the specific implementation process, the operation steps include cleaning the substrate, sequentially growing film 1 and film 2 and film 3 as dielectric layer 2; depositing film 4 to fill the lower electrode via 1, and polishing film 4 (CMP) until the top surface of the via-filled structure is flush with the silicon dioxide structure layer (film 3) on both sides of the via, with film 4 serving as the lower electrode 7; depositing metal layer 3 on film 4; depositing resistive switching layer 4 and upper electrode 5 on metal layer 3; performing photolithography on resistive switching layer 4 and upper electrode 5; etching resistive switching layer 4 and upper electrode 5 after photolithography; depositing and growing sidewall protection layer 6 on the sides of metal layer 3 and resistive switching layer 4, and on the top and sides of upper electrode 5; etching metal layer 3 and sidewall protection layer 6 to obtain the resistive switching structure of resistive switching memory protruding on dielectric layer 2 and lower electrode 7.
[0042] In other words, this invention adds a metal layer to the polished film layer. Since all films 4 on film 3 need to be polished simultaneously (i.e., polishing both film 3 and film 4 simultaneously), this can easily cause depressions or protrusions in the lower electrode via filling structure (film 4). To isolate the effect of the smoothness of the polished film layer on the resistive switching layer, a metal layer is added. This achieves the technical effect of minimizing the influence of environmental factors on the resistive switching layer, thereby improving the electrical properties and process stability of the RRAM film.
[0043] Example 2
[0044] To illustrate the resistive random access memory and its manufacturing method provided by the present invention. Figure 4 The fabrication process of the RRAM structure according to Embodiment 2 of the present invention is shown. Figure 5 The structure of the resistive random access memory according to Embodiment 2 of the present invention is shown.
[0045] To further improve the stability of the resistive switching memory (RSM), this embodiment provides an RSM comprising two electrode layers and a resistive switching layer located between the two electrode layers, with multiple metal layers disposed between the two electrodes. The metal layer 3 includes a first metal layer 31 and a second metal layer 32, the second metal layer 32 and the resistive switching layer 4 being formed using the same deposition equipment. The thickness of the first metal layer is 20 nm to 180 nm, and the thickness of the second metal layer is 10 nm to 100 nm. In this embodiment, the first metal layer is formed using a separate deposition equipment, while the second metal layer, the resistive switching layer, and the upper electrode are formed using the same deposition equipment.
[0046] like Figure 5 As shown, a resistive switching memory includes a first electrode layer, a second electrode layer, and a resistive switching layer located between the first electrode layer and the second electrode layer. Multiple metal layers 3 are disposed between the first electrode layer and the resistive switching layer. In this embodiment, the first electrode layer is the lower electrode 7; the second electrode layer is the upper electrode 5. That is, films 2 and 3 form a dielectric layer 2. A lower electrode via 1 is formed in the dielectric layer 2, and the lower electrode via 1 is filled with the lower electrode metal to obtain the lower electrode 7 (film 4). The lower electrode 7 is provided with a first metal layer 31 of film 5, a second metal layer 32 of film 6, a resistive switching layer 4 of film 7, an upper electrode 5 of film 8, a barrier layer of film 9, and a sidewall protective layer 6 of film 10.
[0047] In other words, based on the chemically ground film layer with an insulating metal layer, to further reduce the impact of other processes on the resistive switching layer and thus ensure the electrical properties of the resistive switching memory, this invention adds a metal deposition step after the formation of the first metal layer, before the formation of the resistive switching layer, to form a second metal layer. This shortens the overall formation time of the resistive switching structure, makes the timing easier to control, and reduces the time for the surface of the second metal layer to react with components in the environment, thereby achieving the technical effect of improving the electrical properties of the resistive switching memory.
[0048] To achieve the above objectives, the present invention provides a method for fabricating a resistive switching memory, the method comprising: S110, forming a first electrode layer on a substrate; S120, forming a first metal layer on the first electrode layer; S130, forming a second metal layer, a resistive switching layer, and a second electrode layer on the first metal layer; the second metal layer and the resistive switching layer are formed using the same deposition equipment. In this embodiment, the first electrode layer is a lower electrode 7; the second electrode layer is an upper electrode 5.
[0049] As an improvement to this embodiment, the specific steps of etching multiple metal layers, resistive switching layers, and top electrodes to form a resistive switching memory structure include: performing photolithography and etching on the metal layers, resistive switching layers, and top electrodes so that the tops of the resistive switching layers and top electrodes protrude from the metal layers; depositing and growing sidewall protective layers on the metal layer plane and on the tops of the resistive switching layers and top electrodes protruding from the metal layer plane; and etching the metal layers and sidewall protective layers to form a resistive switching memory structure.
[0050] Specifically, such as Figure 4 As shown, the substrate is cleaned, and films 1, 2, and 3 are grown sequentially, with films 2 and 3 serving as dielectric layers. The lower electrode metal fills the lower electrode via 1 to form the lower electrode (film 4), wherein the grinding stop point of film 4 is when the top surface of film 4 is flush with the upper surface of film 3. A first metal layer (film 5) is deposited on film 4. The first metal layer (film 5) is ground. A second metal layer (film 6), a resistive switching layer (film 7), an upper electrode (film 8), and a barrier layer (film 9) are sequentially deposited on the first metal layer (film 5). The resistive switching layer (film 7), the upper electrode (film 8), and the barrier layer (film 9) are photolithographically etched. The photolithographically etched resistive switching layer (film 7), the upper electrode (film 8), and the barrier layer (film 9) are etched. Then, a sidewall protective layer (film 10) is deposited and grown, and the first metal layer (film 5), the second metal layer (film 6), and the sidewall protective layer (film 10) are etched to obtain a resistive switching memory structure protruding on the lower electrode.
[0051] In the specific implementation process, this embodiment also includes the following steps: after generating the dielectric layer composed of film 2 and film 3, the lower electrode metal fills the lower electrode via 1 to obtain the lower electrode (film 4); instead of generating the first metal layer on film 3 and film 4, the second metal layer, resistive switching layer and upper electrode are directly deposited and photolithography and etching are performed, and then the sidewall protective layer is deposited.
[0052] Specifically, in this embodiment, to further improve the impact of the interface between the resistive switching layer and the metal layer on the electrical properties of the resistive switching memory, the metal layer is configured as two layers; that is, a metal layer is added to the film composition of the resistive switching layer and the top electrode. In other words, a first metal layer is grown on the dielectric layer and the bottom electrode; a second metal layer is formed on the first metal layer; and the resistive switching layer and the top electrode are formed on the second metal layer. The second metal layer, the resistive switching layer, and the top electrode are grown simultaneously on the same equipment. To ensure the thickness uniformity of the film deposited on the same equipment, the second metal layer should be thinner, while the first metal layer should be thicker. In specific implementation, the metal layer can be formed through a deposition process. This deposition process includes one or more of physical vapor deposition (PVD), chemical vapor deposition (CVD), or atomic layer deposition (ALD). The thickness of the second metal layer is 20 nm to 40 nm. It should be noted that the material of the metal layer should be a metal material with strong oxidation resistance and good thermal conductivity, which can be, but is not limited to, W, Pt, Lr and Ru.
[0053] This invention enables the resistive switching layer to be less affected by other processes and environmental factors, thereby improving the electrical properties and process stability of RRAM Film.
[0054] Example 3
[0055] To further illustrate the resistive random access memory and its manufacturing method provided by the present invention. Figure 6 The structure of the resistive random access memory according to Embodiment 3 of the present invention is shown.
[0056] To further improve the stability of the resistive switching memory (RSM), this embodiment provides an RSM that also includes a via-filling layer. The via-filling layer is used to fill the vias of the first electrode layer. A metal layer, a resistive switching layer, and a second electrode layer are sequentially deposited on the via-filling layer. That is, an RSM includes a first electrode layer, a second electrode layer, and a resistive switching layer located between the first electrode layer and the second electrode layer. A plurality of metal layers 3 are disposed between the first electrode layer and the resistive switching layer. In this embodiment, the first electrode layer is the lower electrode 7; the second electrode layer is the upper electrode 5. Dielectric layer 2 is formed by films 2 and 3. A lower electrode via 1 is formed on dielectric layer 2. The lower electrode via 1 is filled with lower electrode metal to obtain lower electrode 7 (film 4). It should be noted that film 4 is a film layer of a predetermined thickness disposed above film 3, i.e., a via filling layer. That is, the grinding stop point of film 4 is adjusted so that film 4 not only exists in the lower electrode via but also covers dielectric layer 2. Film 5 is disposed on film 4, namely, first metal layer 31, film 6 (second metal layer 32), film 7 (resistive switching layer 4), film 8 (upper electrode 5), and film 9 (sidewall protection layer 6). The material of the via filling layer is TaN or W; the predetermined thickness of the via filling layer is 10nm to 160nm. The material of the via filling layer can be the same as or different from the material of the metal layer, and no specific limitation is made here.
[0057] By changing the grinding stop point of film 4, chemical mechanical polishing only needs to grind the via filling layer to a preset thickness, avoiding the occurrence of depressions or protrusions in the filling structure of the lower electrode via, thereby reducing the impact on the resistive switching layer; thus achieving the technical effect of reducing the differences in function and structure between resistive switching structures on the same wafer.
[0058] In summary, this invention achieves improved RRAM electrical properties by adding a metal deposition step before the resistive switching layer deposition, and by completing the deposition of the resistive switching layer and the second metal layer on the same machine. This eliminates the need for other processes between the resistive switching layer and the second metal layer, reducing the impact of other processes. The process time between the resistive switching structure steps is shorter and easier to control. The time available for the surface of the second metal layer, which is close to the resistive switching layer, to react with components in the environment is reduced.
[0059] Get according to Figure 1 The current-voltage characteristic curves of the resistive switching memory (RSM) prepared by the process shown, as well as those prepared in Examples 1, 2, and 3 (multiple current-voltage characteristic curves were measured for each example, and the most representative curve was selected for comparison) show that, compared with the RSM prepared according to the process shown, the current-voltage characteristic curves of the RSM prepared according to Example 2 and Example 3 are as follows: Figure 1 Compared to the resistive switching memory prepared by the process shown, the resistive switching memory prepared in Examples 1, 2 and 3 has better current-voltage characteristics.
[0060] The following section will introduce memory cells, memory devices, and electronic devices, including resistive random access memory (RRAM).
[0061] This application also provides a memory cell, including: a selector and a resistive random access memory (RRAM) device connected to the selector. The selector can be a three-terminal selector, such as a transistor, or a two-terminal selector, such as a bidirectional threshold switch. Taking a transistor as an example, a plug is formed between the transistor and the RRAM device, and the transistor and the RRAM device are electrically connected through the plug.
[0062] Specifically, a transistor includes a source, a drain, and a gate, with the resistive random access memory (RRAM) device connected between the drain and the bit line. Furthermore, the source of the transistor can be connected to a source line, and the gate can be connected to a word line.
[0063] This application embodiment also provides a storage device, including a storage controller and a resistive random access memory (RRAM) device, wherein the storage controller is used to read and write data to the RRAM device. Specifically, the storage controller can provide a write voltage or a read voltage to the RRAM device, thereby writing data to or reading data from the RRAM device. For example, the storage controller can control the voltages of the word line, bit line, and source line to control the operating state of the selector (such as a transistor) in the storage cell, thereby providing a write voltage or a read voltage between the upper and lower electrodes of the RRAM device. The write voltage and read voltage can cause a change in the resistance of the RRAM device, thereby changing the storage state.
[0064] This application also provides an electronic device. The electronic device may include a circuit board and a resistive random access memory (RRAM) device connected to the circuit board. The circuit board and the RRAM device are electrically connected, and the RRAM device cooperates with the circuit board to achieve data storage functionality. The various embodiments in this specification are described in a progressive manner; similar or identical parts between embodiments can be referred to mutually. Each embodiment focuses on describing the differences from other embodiments. In particular, embodiments of storage units, storage devices, and electronic devices are basically similar in structure to the RRAM device embodiments, so the descriptions are relatively simple; relevant parts can be referred to the descriptions of the structural embodiments.
[0065] Resistive random access memory (RRAM) devices can be used in memory chips or in-memory computing (IMC) chips. IMC chips refer to chips that integrate storage and computation. For ease of understanding, this application uses an IMC chip as an example. An IMC chip includes a control circuit, a decoding circuit, a read / write circuit, and a memory array. The control circuit provides control signals for the entire chip. The memory array stores data; further, the memory array in the IMC chip also performs data computation. The decoding circuit selects rows and columns of the memory array. The read / write circuit performs read or write operations on the selected memory cells.
[0066] The memory array includes multiple memory cells. Each memory cell includes a transistor disposed on a substrate and a resistive random access memory (RRAM) device located on the transistor. The structure of the RRAM device can be described in the accompanying description. The transistor may be a MOS transistor, which may include a source (S), a drain (D), and a gate (G). The RRAM device may specifically be disposed on the gate. The RRAM device is electrically connected to the gate of the transistor. In some embodiments, the RRAM device may also be electrically connected to the drain via a plug. The plug may be a metallic material, such as a tungsten plug.
[0067] Specifically, the control circuit provides control signals, which include address signals and command signals. The decoding circuit receives the address signals and command signals, decodes them according to the address signals, and selects the memory cell in the memory array corresponding to the address signals. The read / write circuit performs read and write operations on the selected memory cell according to the command signals. For example, when the read / write circuit performs a write operation on the selected memory cell, it can output the data stored in the selected memory cell.
[0068] Furthermore, it is clear that the word "comprising" does not exclude other units or steps, and the singular does not exclude the plural. Multiple units or devices recited in a system claim may also be implemented by a single unit or device through software or hardware. The term "second class" is used to indicate names and does not indicate any specific order.
[0069] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit it. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the spirit and scope of the technical solutions of the present invention.
Claims
1. A method for fabricating a resistive random access memory, characterized in that, The method includes: A first electrode layer is formed on the substrate; A first metal layer is formed on the first electrode layer; A second metal layer, a resistive switching layer, and a second electrode layer are formed on the first metal layer; wherein... The second metal layer and the resistive switching layer are deposited using the same deposition equipment.
2. A resistive random access memory, characterized in that, It includes a first electrode layer, a second electrode layer, and a resistive switching layer located between the first electrode layer and the second electrode layer. A first metal layer and a second metal layer are disposed between the first electrode layer and the resistive switching layer. The first metal layer is disposed on the first electrode layer, and the second metal layer is disposed on the first metal layer. The second metal layer and the resistive switching layer are deposited using the same deposition equipment.
3. The resistive random access memory according to claim 2, characterized in that, The material of the first metal layer is W, Lr, Ru or Pt.
4. The resistive random access memory according to claim 3, characterized in that, The thickness of the first metal layer is 20nm to 180nm.
5. The resistive random access memory according to claim 2, characterized in that, The material of the second metal layer is W, Lr, Ru or Pt.
6. The resistive random access memory according to claim 5, characterized in that, The thickness of the second metal layer is 10 nm to 100 nm.
7. The resistive random access memory of claim 6, wherein, The thickness of the second metal layer is 20 nm to 40 nm.
8. The resistive random access memory according to claim 2, characterized in that, It also includes a via filling layer, which is used to fill the vias of the first electrode layer; the metal layer, the resistive switching layer and the second electrode layer are sequentially deposited on the via filling layer.
9. A storage unit, characterized in that, The storage unit includes a gate and a resistive switching memory as described in any one of claims 2-8 connected to the gate.
10. A storage device, comprising: The storage device includes a storage controller and a resistive switching memory as described in any one of claims 2-8, wherein the storage controller is used to read and write data to the resistive switching memory.
11. An electronic device, comprising: It includes a circuit board and a resistive switching memory as described in any one of claims 2-8 connected to the circuit board.
Citation Information
Patent Citations
Rram retention by depositing ti capping layer before hk hfo