Resistive Random Access Memory and Its Fabrication Method
By adjusting the grinding stop point and adding a metal layer in the resistive switching memory fabrication process, the problem of unevenness of the lower electrode via caused by chemical mechanical polishing in the prior art has been solved, improving the process window and the electrical and structural consistency of the resistive switching memory.
Patent Information
- Application Number
- CN202310450080.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-04-24
AI Technical Summary
In existing resistive switching memory fabrication processes, chemical mechanical polishing (CMP) results in uneven filling structures of the lower electrode vias, affecting photolithography alignment marking signals and process windows, leading to severe chip and wafer loading and increasing structural differences in the resistive switching layer.
A via-fill layer is deposited on the dielectric layer, and the grinding stop point is adjusted to a set thickness to avoid grinding different film structures at the same time. A metal layer is added to reduce the influence of the resistive switching layer, and the resistive switching memory structure is formed by etching.
This avoids the depressions or protrusions in the bottom electrode via filling structure, reduces the impact on the resistive switching layer, improves the process window, reduces chip and wafer loading, and improves the electrical and structural consistency of the resistive switching memory.
Smart Images

Figure CN116634853B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of resistive random access memory (RRAM) technology, and more specifically, to a RRAM and its fabrication method. Background Technology
[0002] Resistive Random Access Memory (ReRAM) has garnered increasing attention due to its advantages such as low voltage, high speed, low power consumption, simple structure, compatibility with traditional CMOS (Complementary Metal Oxide Semiconductor) processes, low cost, and high density. It is considered a new type of memory that may replace flash memory as the mainstream storage product. RRAM typically consists of a three-layer structure formed by stacking metal, resistive switching dielectric, and metal layers. It stores data by utilizing high and low resistance states. When different polarities and magnitudes of voltage are applied across the device, the resistance of the intermediate resistive switching thin film material switches. The key structure of RRAM is the resistive switching material structure, using a TiN / TaO / Ta / TiN structure. This structure allows the device to reversibly switch between high and low resistance states by forming and breaking conductive channels under positive and negative voltages, thereby storing data.
[0003] The existing fabrication process of resistive random access memory is as follows: Figure 1 As shown, the lower electrode (BE) via is first filled by thin film deposition, photolithography, etching, and chemical mechanical polishing (CMP) until the upper surface of the silicon carbide structure on both sides of the via is exposed, thus completing the fabrication of the lower electrode. Then, thin film deposition is performed to complete the fabrication of the gap film of the upper electrode (TE). Finally, the overall fabrication of the resistive switching memory is completed by photolithography and etching.
[0004] The drawbacks of existing fabrication processes are as follows: they affect the alignment mark signals and OVL Mark Damage required for photolithography, thereby affecting the process and reducing the process window.
[0005] Therefore, there is an urgent need for a method to fabricate resistive switching memory that can reduce the impact of grinding. Summary of the Invention
[0006] The purpose of this invention is to provide a resistive random access memory and its fabrication method to solve at least one problem existing in the prior art.
[0007] To achieve the above objectives, the present invention provides a method for fabricating a resistive random access memory (RRAM), the method comprising:
[0008] A via-fill layer is deposited on the dielectric layer to fill the via of the lower electrode;
[0009] Grind the via filler layer until the thickness of the via filler layer covering the dielectric layer reaches the set thickness threshold.
[0010] A resistive switching layer and an upper electrode are sequentially deposited on the via-filled layer;
[0011] The via filling layer, resistive switching layer and top electrode are etched to form the resistive switching structure of the resistive switching memory.
[0012] Furthermore, the preferred method includes, prior to the step of sequentially depositing a resistive switching layer and an upper electrode on the via-filling layer, the method further includes,
[0013] A metal layer is deposited on the via filling layer, and a resistive switching layer and an upper electrode are sequentially deposited on the metal layer.
[0014] Further, a preferred method includes the steps of depositing a metal layer on the via filling layer, and sequentially depositing a resistive switching layer and an upper electrode on the metal layer, including...
[0015] A first metal layer is deposited on the via filling layer;
[0016] A second metal layer, a resistive switching layer, and an upper electrode are sequentially deposited on the first metal layer.
[0017] Further, the preferred method includes, after the steps of depositing a metal layer on the via filling layer, and sequentially depositing a resistive switching layer and an upper electrode on the metal layer, the method further includes,
[0018] Photolithography and etching are performed on the resistive switching layer and the top electrode; a sidewall protective layer is deposited and grown on the side of the resistive switching layer, the surface and side of the top electrode, and the surface of the metal layer.
[0019] The via filling layer, metal layer, and sidewall protective layer are etched to form the resistive switching structure of the resistive switching memory.
[0020] Furthermore, a preferred method includes using TaN or W as the material for the via filling layer.
[0021] Furthermore, a preferred method includes using W, Lr, Ru, or Pt as the material of the metal layer.
[0022] Furthermore, a preferred method includes setting the thickness of the via filling layer to be 10 nm to 160 nm.
[0023] Furthermore, a preferred method includes setting the thickness of the via filling layer to be 10 nm to 90 nm.
[0024] Secondly, the present invention provides a resistive switching memory, comprising a dielectric layer having a lower electrode via and a via-filling layer for filling the lower electrode via; the via-filling layer is an insulating dielectric film of a predetermined thickness covering the dielectric layer; a resistive switching layer and an upper electrode are sequentially stacked on the via-filling layer. Further, a preferred structure is that a metal layer is disposed between the resistive switching layer and the via-filling layer. Further, a preferred structure is that the metal layer includes a first metal layer and a second metal layer.
[0025] Thirdly, the present invention provides a storage unit, which includes a gate and a resistive switching memory connected to the gate. The gate may be a three-terminal gate device.
[0026] Fourthly, the present invention provides a storage device, which includes a storage controller and a resistive random access memory (RRAM), wherein the storage controller is used to read and write data to the RRAM.
[0027] Fifthly, the present invention provides an electronic device, including a circuit board and a resistive random access memory connected to the circuit board.
[0028] As described above, the resistive switching memory, its fabrication method, memory cell, memory device, and electronic device of the present invention change the grinding stop point of the via filling layer. The beneficial effects are as follows:
[0029] Chemical mechanical polishing (CMP) only requires polishing the via filling layer to a preset thickness, avoiding the occurrence of depressions or protrusions in the filling structure of the lower electrode via, thereby reducing the impact on the resistive switching layer and avoiding the current severe loading of chips and wafers, as well as the severe loading of ISO and Density regions in the same chip; it also avoids the influence of alignment mark signals and OVL mark damage required for photolithography, thus achieving the technical effect of ensuring the process of resistive switching memory structure and improving the process window.
[0030] To achieve the foregoing and related objectives, one or more aspects of the invention include the features that will be described in detail below and particularly pointed out in the claims. The following description details certain exemplary aspects of the invention. However, these aspects indicate only a few of the various ways in which the principles of the invention can be used. Furthermore, the invention is intended to include all such aspects and their equivalents. Attached Figure Description
[0031] Figure 1 This is a schematic diagram of the existing resistive switching memory fabrication process;
[0032] Figure 2 This is a schematic diagram of the resistive random access memory provided in Embodiment 1 of the present invention;
[0033] Figure 3 This is a schematic flowchart of the resistive switching memory fabrication method provided in Embodiment 1 of the present invention;
[0034] Figure 4 This is a schematic diagram of the resistive random access memory according to Embodiment 2 of the present invention;
[0035] Figure 5 This is a schematic diagram of the fabrication process of the resistive switching memory according to Embodiment 2 of the present invention;
[0036] Figure 6 This is a schematic diagram of the resistive random access memory according to Embodiment 3 of the present invention.
[0037] In the attached figures, 1 is the lower electrode via; 2 is the dielectric layer; 3 is the via filling layer; 4 is the metal layer; 5 is the resistive switching layer; 6 is the upper electrode; 7 is the sidewall protective layer; 41 is the first metal layer; and 42 is the second metal layer. Detailed Implementation
[0038] It should be understood that the specific embodiments described herein are for illustrative purposes only and are not intended to limit the scope of the invention. Where specific techniques or conditions are not specified in the embodiments, they should be performed in accordance with the techniques or conditions described in the literature in this field, or according to the product instructions. Reagents or instruments whose manufacturers are not specified can be purchased from legitimate channels as conventional products.
[0039] Memory is a storage device used in modern information technology to store information. Its main function is to store various types of data (such as business data and program data). Memory typically uses physical devices (e.g., memory cells) with two stable states (represented by "0" and "1" respectively) to achieve its storage function. Memory can characterize stored data based on the amount of stored charge. For example, Dynamic Random Access Memory (DRAM) and Flash Memory typically characterize stored data based on the amount of stored charge. Memory can also characterize stored data based on the magnitude of resistance. For example, Resistive Random Access Memory (RRAM) typically characterizes stored data based on the device's resistance. RRAM is a type of non-volatile memory with adjustable resistance. The RRAM cell structure uses a MIM capacitor structure, with an insulating layer or semiconductor functional material layer sandwiched between the upper and lower electrodes, also known as a sandwich structure. Specifically, RRAM can control the device resistance by controlling the movement of oxygen ions, thereby achieving its storage function. The memory array can adopt a crossbar array structure. This crossbar array structure has simple manufacturing process, high density, and good scaling capability.
[0040] Figure 1 This diagram illustrates the fabrication process of existing resistive random access memory (RRAM); in the prior art, such as Figure 1As shown, in the polishing step, the surface of the filling structure of the lower electrode via needs to be polished until the upper surface of the silicon carbide structure (i.e., film 3) on both sides of the via is exposed. Since chemical mechanical polishing requires polishing both the filling structure layer (i.e., film 4) and the silicon carbide structure layer (i.e., film 3) on both sides of the via, the difference in materials to be polished can easily lead to uneven polishing, resulting in depressions or protrusions in the filling structure of the lower electrode via; the resistive switching structure composed of resistive switching layers is disposed immediately above the lower electrode via. The impact on resistive switching memory (RSM) is as follows: 1) It leads to a smaller process window for chemical mechanical polishing (CMP). Currently, loading is severe in both in-die and in-wafer applications, and even within the same chip, loading in the ISO and Density regions is severe; 2) This in turn causes alignment mark / OVL mark damage, resulting in OVL shift, which also affects the structural function of the RSM structure; 3) It also increases the functional and structural differences between RSM structures on the same wafer; 4) It also leads to damage to the alignment mark signal (Alignment Mark) and OVL mark used in photolithography, thereby affecting the process and reducing the process window.
[0041] Example 1
[0042] To illustrate the resistive switching memory, its fabrication method, and electronic device diagram provided by this invention. Figure 2 The structure of an RRAM according to Embodiment 1 of the present invention is shown. Figure 3 The flowchart of the method for preparing the RRAM structure according to Embodiment 1 of the present invention is shown.
[0043] like Figure 2 As shown, the present invention provides a resistive switching memory including a dielectric layer 2 having a lower electrode via 1 and a via filling layer 3 for filling the lower electrode via 1; the via filling layer 3 is an isolation dielectric film with a set thickness covering the dielectric layer 2; a resistive switching layer 5 and an upper electrode 6 are sequentially stacked on the via filling layer 3.
[0044] In other words, the lower electrode layer is first deposited on the surface of the dielectric layer and in the lower electrode via using physical vapor deposition or atomic layer deposition (ALD). A via-hole filling layer, serving as an isolation medium, is then deposited on the surface of the lower electrode layer using chemical vapor deposition (CVD). In existing technologies, chemical mechanical polishing (CMP) is used to planarize the via-hole filling layer until the film layer above the dielectric layer is removed, leaving only the filling structure in the lower electrode via. In this invention, the polishing stop point of the via-hole filling layer is changed, and CMP is used to polish the via-hole filling layer until the thickness of the via-hole filling layer covering the dielectric layer reaches a set thickness. The resistive switching material layer of the resistive switching memory can be one or more transition metal oxides such as Ni, Ti, Al, Ta, and Hf. The resistive switching mechanism of such materials is mainly due to the formation of oxygen vacancy conductive filaments by the movement of oxygen ions. Simultaneously, the number of defects in the resistive switching material layer directly affects the resistive switching characteristics of the device. Based on this, the aforementioned resistive switching layer can be generated on the electrode layer by atomic layer deposition or sputtering. The thickness of the resistive switching layer can be set according to actual needs. For example, an 8 nm thick resistive switching layer can be formed on the lower electrode using atomic layer deposition (ALD). The material of this resistive switching layer can be selected according to actual needs; for example, the material can be any of the transition metal oxides such as HfOx, NiO, TiO2, Al2O3, and Ta2O5. The lower electrode is typically formed of a metallic material. This metallic material includes, but is not limited to, copper, aluminum, titanium, titanium nitride, silver, nickel, platinum, and palladium. Based on this, the lower electrode can be formed by PVD, or the upper electrode can be formed by sputtering. In some embodiments, the thickness of the upper electrode can be equal to the thickness of the lower electrode, for example, it can be 20 nm. In other embodiments, the thickness of the upper electrode may not be equal to the thickness of the lower electrode. Similarly, the material of the upper electrode can be the same as the material of the lower electrode, for example, both can be TiN. In some embodiments, the material of the upper electrode may also be different from the material of the lower electrode.
[0045] The filling material of the via filling layer 3 can be, but is not limited to, TaN and W. The thickness of the via filling layer is set to be 10 nm to 160 nm, with a preferred choice of 10 nm to 90 nm. In this invention, the via filling layer (i.e., film 4) with the same height as the silicon carbide structural layer (i.e., film 3) on the top surface and both sides of the via is changed to a via filling layer of a certain thickness that covers the entire film 3 and the lower electrode.
[0046] like Figure 3 As shown, the present invention provides a method for fabricating a resistive random access memory (RRAM), the method comprising:
[0047] S110. Deposit a via filling layer 3 on the dielectric layer 2 to fill the lower electrode via 1;
[0048] S120, grind the via filling layer 3 until the thickness of the via filling layer 3 covering the dielectric layer 2 reaches the set thickness threshold.
[0049] S130. A resistive switching layer 5 and an upper electrode 6 are sequentially deposited on the via filling layer 3.
[0050] S140. The via filling layer 3, the resistive switching layer 5 and the upper electrode 6 are etched to form the resistive switching structure of the resistive switching memory.
[0051] In the specific implementation process, obtain Figure 2 The operation steps of the resistive switching memory shown include cleaning the substrate, sequentially growing film 1 and film 2 and film 3 as dielectric layer 2; depositing film 4 to fill the via 1 of the lower electrode, and polishing film 4 (CMP) until the thickness of the via filling structure reaches a preset thickness threshold; sequentially depositing resistive switching layer 5 (film 5) and upper electrode 6 (film 6) on film 4; performing photolithography on resistive switching layer 5 and upper electrode 6; etching resistive switching layer 5 and upper electrode 6 after photolithography; depositing and growing sidewall protection layer 7 (film 7) on the side of resistive switching layer 5, the surface and side of upper electrode 6; etching sidewall protection layer 7 to obtain the resistive switching memory structure protruding on dielectric layer 2 and lower electrode.
[0052] In other words, this invention adjusts the grinding stop point from grinding all the films on film 3 to not grinding all the films on film 3; this invention does not require grinding different film structures at the same time, and the remaining films are etched out in subsequent processes, which improves the problems caused by loading, increases the process window, and optimizes the differences between the functions of RRAM cell structure and RRAM cell structure. By changing the grinding stop point, a via-fill layer of preset thickness is set before the resistive switching layer deposition in the resistive switching memory. This allows chemical mechanical polishing (CMP) to only grind the via-fill layer to the preset thickness, avoiding the situation where, during CMP planarization of the via-fill layer to remove the film layer above the dielectric layer, leaving only the filling structure in the lower electrode via, grinding reaches film 3, or the filling structure in the lower electrode via protrudes from the plane of film 3 due to insufficient grinding. This reduces the impact on the resistive switching layer, avoiding severe loading on the current chip and wafer, as well as severe loading in the ISO and Density regions of the same chip. It also avoids the influence of alignment mark signals and OVL Mark Damage required for photolithography, thereby ensuring the resistive switching memory structure process and improving the process window. This achieves the technical effect of reducing the differences in function and structure between resistive switching structures on the same wafer.
[0053] Example 2
[0054] To illustrate the resistive switching memory and its fabrication method provided by the present invention. Figure 4 The structure of the RRAM according to Embodiment 2 of the present invention is shown. Figure 5The preparation process of RRAM according to Embodiment 2 of the present invention is shown.
[0055] like Figure 4 As shown, to further improve the stability of the resistive switching memory, this embodiment provides a resistive switching memory including a dielectric layer 2 with a lower electrode via 1 and a via filling layer 3 for filling the lower electrode via 1; the via filling layer 3 is an isolation dielectric film with a set thickness covering the dielectric layer 2; a resistive switching layer 5 and an upper electrode 6 are sequentially stacked on the via filling layer 3; a metal layer 4 is disposed between the resistive switching layer 5 and the via filling layer 3. Dielectric layers 2 and 3 are formed on film 1, and a lower electrode and via filling layer 3 (film 4) are formed in the dielectric via 1; a metal layer (film 5) is formed on film 4; a resistive switching layer (film 6), an upper electrode (film 7), a barrier layer (film 8), and a sidewall protection layer (film 9) are sequentially deposited on the metal layer. The material of the via filling layer is TaN or W; the material of the metal layer is W, Lr, Ru, or Pt; the material of the via filling layer and the material of the metal layer can be the same or different, and no specific limitation is made here.
[0056] In other words, by changing the via-filled layer 3, which is flush with the top of the dielectric film 3, to a via-filled layer of a certain thickness disposed above the dielectric film 3, and further reducing the impact of other processes on the resistive switching layer to ensure the electrical performance of the resistive switching memory, this invention deposits a metal layer on the via-filled layer, and then sequentially deposits the resistive switching layer and the top electrode on the metal layer. This shortens the time between the entire generation process, makes the timing easier to control, and reduces the time for the surface of the metal layer 4 to react with components in the environment, thereby achieving the technical effect of improving the electrical performance of the resistive switching memory.
[0057] To achieve the above objectives, this embodiment provides a method for fabricating a resistive switching memory, the method comprising: depositing a via-filling layer 3 for filling a lower electrode via 1 on a dielectric layer 2; grinding the via-filling layer 3 until the thickness of the via-filling layer 3 covering the dielectric layer 2 reaches a set thickness threshold; depositing a metal layer 4 on the via-filling layer 3, and sequentially depositing a resistive switching layer 5 and an upper electrode 6 on the metal layer 4; and etching the via-filling layer 3, the metal layer 4, the resistive switching layer 5 and the upper electrode 6 to form a resistive switching structure of the resistive switching memory.
[0058] As an improvement to this embodiment, such as Figure 5 As shown, the specific steps for etching the via filling layer 3, resistive switching layer 5, and upper electrode 6 to form the resistive switching structure of the resistive switching memory include: photolithography and etching of the resistive switching layer 5 and the upper electrode 6; depositing and growing a sidewall protective layer on the side of the resistive switching layer 5, the surface and side of the upper electrode 6, and the surface of the metal layer 4; and etching the via filling layer 3, the metal layer 4, and the sidewall protective layer 7 to form the resistive switching structure of the resistive switching memory.
[0059] Specifically, the substrate is cleaned, and films 1, 2, and 3 are grown sequentially, with films 2 and 3 serving as dielectric layers. The lower electrode metal fills the lower electrode via 1 to form the lower electrode, and a via-filling layer film 4 is deposited. Film 4 is then polished (CMP) until the thickness of the via-filling structure reaches a preset thickness threshold. A metal layer (film 5), a resistive switching layer 5 (film 6), an upper electrode 6 (film 7), and a barrier layer (film 8) are sequentially deposited on film 4. The resistive switching layer 5 (film 6), the upper electrode 6 (film 7), and the barrier layer (film 8) are then photolithographically etched and etched. A sidewall protection layer 7 (film 9) is deposited and grown on the side of the resistive switching layer 5, the surface of the upper electrode 6, and the side of the barrier layer. The sidewall protection layer 7 (film 9), the metal layer (film 5), and the via-filling layer (film 4) are then etched to obtain a resistive switching memory structure protruding from the dielectric layer 2 and the lower electrode.
[0060] Example 3
[0061] Furthermore, as an improvement to this embodiment, in order to further improve the influence of the interface formed by the resistive switching layer 5 and the metal layer 4 on the electrical properties of the resistive switching memory, the metal layer 4 is configured as two layers.
[0062] like Figure 6 As shown, to further improve the stability of the resistive switching memory, this embodiment provides a resistive switching memory including a dielectric layer 2 with a lower electrode via 1 and a via filling layer 3 for filling the lower electrode via 1; the via filling layer 3 is an isolation dielectric film with a set thickness covering the dielectric layer 2; a first metal layer 41 is deposited on the via filling layer 3, and a second metal layer 42, a resistive switching layer 5, and an upper electrode 6 are sequentially deposited on the first metal layer 41. Dielectric layer film 2 and film 3 are formed on film 1, and a lower electrode and via filling layer 3 (film 4) are formed in the dielectric layer via 1; a first metal layer (film 5) is formed on film 4; a second metal layer (film 6), a resistive switching layer (film 7), an upper electrode (film 8), and a sidewall protective layer (film 9) are sequentially deposited on the first metal layer.
[0063] A method for fabricating a resistive switching memory includes depositing a via-filling layer on a dielectric layer for filling a via hole of the lower electrode; grinding the via-filling layer until the thickness of the via-filling layer covering the dielectric layer reaches a set thickness threshold; depositing a first metal layer on the via-filling layer; and sequentially depositing a second metal layer, a resistive switching layer, and an upper electrode on the first metal layer.
[0064] Specifically, in this embodiment, to further improve the impact of the interface between the resistive switching layer and the metal layer on the electrical properties of the resistive switching memory, the metal layer is configured as two layers; that is, a first metal layer is grown on the dielectric layer and the lower electrode; a second metal layer is formed on the first metal layer; and a resistive switching layer and an upper electrode are formed on the second metal layer. The second metal layer, the resistive switching layer, and the upper electrode are grown simultaneously on the same equipment. To ensure the thickness uniformity of the film deposited on the same equipment, the second metal layer should be thinner, while the first metal layer should be thicker. In specific implementation, the metal layer can be formed through a deposition process. The first and second metal layers can be deposited on the same equipment or on different equipment; no specific limitation is made here. The deposition process includes one or more of physical vapor deposition (PVD), chemical vapor deposition (CVD), or atomic layer deposition (ALD). The thickness of the second metal layer is 20 nm to 40 nm. It should be noted that the material of the metal layer should be a metal material with strong oxidation resistance and good thermal conductivity, which can be, but is not limited to, W, Pt, Lr and Ru.
[0065] This invention improves the electrical properties and process stability of RRAM Film by adding multiple metal layers, which reduces the resistance switching layer's susceptibility to other processes and environmental factors.
[0066] This invention improves the polishing process. Current mechanochemical polishing requires simultaneously polishing film structures with different filling structures (film 3 and lower electrode vias), which leads to uneven polishing of these structures. Since the RRAM cell structure sits directly above the lower electrode via, this significantly impacts the functionality of the RRAM cells. This results in increased functional and structural differences between RRAMs on the same wafer. Furthermore, this same issue also affects photolithography (alignment mark signals) and OVL mark damage, impacting the process and reducing the process window. This invention eliminates the need to simultaneously polish film structures with different filling structures (film 3 and lower electrode vias), thus mitigating this problem. By changing the polishing stop point of the via filling layer and adding multiple metal layers, the impact on the resistive switching layer is reduced, thereby minimizing the functional and structural differences between resistive switching structures on the same wafer.
[0067] Get according to Figure 1The current-voltage characteristic curves of the resistive switching memory (RSM) prepared by the process shown, as well as those prepared in Examples 1 and 2 (multiple current-voltage characteristic curves were measured for each example, and the most representative curve was selected for comparison), show that compared with the RSM prepared according to the process shown, the current-voltage characteristic curves of the RSM prepared according to Example 1 and Example 2 are significantly different. Figure 1 Compared to the resistive switching memory prepared by the process shown, the resistive switching memory prepared in Examples 1 and 2 has better current-voltage characteristics.
[0068] The following section will introduce memory cells, memory devices, and electronic devices, including resistive random access memory (RRAM).
[0069] This application also provides a memory cell, including: a selector and a resistive random access memory (RRAM) device connected to the selector. The selector can be a three-terminal selector, such as a transistor, or a two-terminal selector, such as a bidirectional threshold switch. Taking a transistor as an example, a plug is formed between the transistor and the RRAM device, and the transistor and the RRAM device are electrically connected through the plug.
[0070] Specifically, a transistor includes a source, a drain, and a gate, with the resistive random access memory (RRAM) device connected between the drain and the bit line. Furthermore, the source of the transistor can be connected to a source line, and the gate can be connected to a word line.
[0071] This application embodiment also provides a storage device, including a storage controller and a resistive random access memory (RRAM) device, wherein the storage controller is used to read and write data to the RRAM device. Specifically, the storage controller can provide a write voltage or a read voltage to the RRAM device, thereby writing data to or reading data from the RRAM device. For example, the storage controller can control the voltages of the word line, bit line, and source line to control the operating state of the selector (such as a transistor) in the storage cell, thereby providing a write voltage or a read voltage between the upper and lower electrodes of the RRAM device. The write voltage and read voltage can cause a change in the resistance of the RRAM device, thereby changing the storage state.
[0072] This application also provides an electronic device. The electronic device may include a circuit board and a resistive random access memory (RRAM) device connected to the circuit board. The circuit board and the RRAM device are electrically connected, and the RRAM device cooperates with the circuit board to achieve data storage functionality. The various embodiments in this specification are described in a progressive manner; similar or identical parts between embodiments can be referred to mutually. Each embodiment focuses on describing the differences from other embodiments. In particular, embodiments of storage units, storage devices, and electronic devices are basically similar in structure to the RRAM device embodiments, so the descriptions are relatively simple; relevant parts can be referred to the descriptions of the structural embodiments.
[0073] Resistive random access memory (RRAM) devices can be used in memory chips or in-memory computing (IMC) chips. IMC chips refer to chips that integrate storage and computation. For ease of understanding, this application uses an IMC chip as an example. An IMC chip includes a control circuit, a decoding circuit, a read / write circuit, and a memory array. The control circuit provides control signals for the entire chip. The memory array stores data; further, the memory array in the IMC chip also performs data computation. The decoding circuit selects rows and columns of the memory array. The read / write circuit performs read or write operations on the selected memory cells.
[0074] The memory array includes multiple memory cells. Each memory cell includes a transistor disposed on a substrate and a resistive random access memory (RRAM) device disposed on the transistor. The structure of the RRAM device can be described in the accompanying description. The transistor may be a MOS transistor, which may include a source (S), a drain (D), and a gate (G). The RRAM device may specifically be disposed on the gate. The RRAM device is electrically connected to the gate of the transistor. In some embodiments, the RRAM device may also be electrically connected to the drain via a plug. The plug may be a metallic material, such as a tungsten plug.
[0075] Specifically, the control circuit provides control signals, which include address signals and command signals. The decoding circuit receives the address signals and command signals, decodes them according to the address signals, and selects the memory cell in the memory array corresponding to the address signals. The read / write circuit performs read and write operations on the selected memory cell according to the command signals. For example, when the read / write circuit performs a write operation on the selected memory cell, it can output the data stored in the selected memory cell.
[0076] Furthermore, it is clear that the word "comprising" does not exclude other units or steps, and the singular does not exclude the plural. Multiple units or devices recited in a system claim may also be implemented by a single unit or device through software or hardware. The term "second class" is used to indicate names and does not indicate any specific order.
[0077] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit it. Although the present invention has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solutions of the present invention without departing from the spirit and scope of the technical solutions of the present invention.
Claims
1. A method for fabricating a resistive random access memory, characterized in that, The method includes: A via-fill layer is deposited on the dielectric layer to fill the via of the lower electrode; The via filling layer is subjected to chemical mechanical polishing, so that the polished via filling layer retains a set thickness above the dielectric layer; A first metal layer is deposited on the milled via-fill layer; a second metal layer is deposited on the first metal layer, wherein the thickness of the first metal layer is greater than the thickness of the second metal layer; A resistive switching layer and an upper electrode are sequentially deposited on the second metal layer; The via filling layer, the first metal layer, the second metal layer, the resistive switching layer, and the upper electrode are etched to form the resistive switching structure of the resistive switching memory.
2. The method for fabricating a resistive random access memory according to claim 1, characterized in that, After the step of sequentially depositing the resistive switching layer and the upper electrode on the second metal layer, the method further includes, Photolithography and etching are performed on the resistive switching layer and the top electrode; a sidewall protective layer is deposited and grown on the side of the resistive switching layer, the surface and side of the top electrode, and the surface of the second metal layer. The via filling layer, the first metal layer, the second metal layer, and the sidewall protective layer are etched to form the resistive switching structure of the resistive switching memory.
3. The method for fabricating a resistive random access memory according to claim 1, characterized in that, The material of the through-hole filling layer is TaN or W.
4. The method for fabricating a resistive random access memory according to claim 1, characterized in that, The materials of the first metal layer and the second metal layer are W, Lr, Ru or Pt.
5. The method for fabricating a resistive random access memory according to claim 1, characterized in that, The thickness of the via filling layer is set to be 10 nm to 160 nm.
6. The method for fabricating a resistive random access memory according to claim 5, characterized in that, The thickness of the via filling layer is set to be 10 nm to 90 nm.
7. A resistive random access memory, characterized in that, It includes a dielectric layer with a lower electrode via, a via filling layer for filling the lower electrode via, a first metal layer disposed on the via filling layer, a second metal layer disposed on the first metal layer, and a resistive switching layer and an upper electrode disposed sequentially on the second metal layer; wherein, the thickness of the first metal layer is greater than the thickness of the second metal layer, and the via filling layer is an insulating dielectric film with a set thickness covering the dielectric layer.
8. A storage unit, characterized in that, The storage unit includes a gate and a resistive switching memory as described in claim 7, which is connected to the gate.
9. A storage device, characterized in that, The storage device includes a storage controller and a resistive switching memory as described in claim 7, wherein the storage controller is used to read and write data to the resistive switching memory.
10. An electronic device, characterized in that, Includes a circuit board and a resistive switching memory as described in claim 7 connected to the circuit board.
Citation Information
Patent Citations
Rram retention by depositing ti capping layer before hk hfo