A high-moisture-retention vapor eye mask and a method of making the same
By using a highly moisturizing steam eye mask with hydrogel and sericin cotton layer, the problem of insufficient repair effect of traditional steam eye masks under sunlight is solved, and a steam eye mask with high comfort and moisturizing effect is achieved, which has antioxidant, anti-inflammatory and eye protection functions.
Patent Information
- Application Number
- CN202310752791.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-26
- Publication Date
- 2025-10-10
- Estimated Expiration
- 2043-06-26
AI Technical Summary
Existing steam eye masks cannot effectively repair eye damage caused by ultraviolet rays when working under sunlight, and traditional heating plates have unstable heating and overheating risks, and are insufficient in comfort and moisturizing effects.
Hydrogel is used instead of super absorbent resin, and a sericin cotton layer and traditional Chinese medicine ingredients are added. Combined with tea tree essential oil and rose essential oil, a highly moisturizing steam eye mask is prepared, which is heated using a heating sheet.
It effectively relieves problems such as dry eyes and eye pain caused by working in the sun for a long time, improves comfort and moisturizing effect, repairs UV damage, and has rich functions.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of eye masks and discloses a highly moisturizing steam eye mask and a preparation method thereof. Background Art
[0002] Steam eye mask is a new type of eye mask used to relieve eye fatigue and improve sleep quality. Its principle is similar to that of hot compress. It uses a heating pack to heat and generate steam. Combined with medicinal ingredients such as herbal essences added to the product, it provides warmth and moisture to the eyes, relieves fatigue, and improves blood circulation in the eyes.
[0003] Traditional steam eye masks use powdered bag heating packs, which have unstable heating locations and duration, and there is a risk of powder leakage or local overheating that can damage the skin. The use of thin heating sheets can solve this problem. The heating temperature of the heating sheet can be effectively controlled, the effective time is stable, the texture is comfortable and soft, and it will not irritate the skin. It is a current research hotspot.
[0004] Among the existing products, most steam eye masks use traditional Chinese medicine ingredients that can reduce swelling and relieve pain, nourish blood and calm the nerves, clear away heat and detoxify, or use essential oils to relieve eye fatigue and soothe the body and mind. Such products can effectively relieve problems such as intraocular congestion, fatigue, dryness, and pain caused by prolonged exposure to electronic products, but they ignore the damage caused to human eyes by ultraviolet rays when working in the sun for a long time. The repair effect of such products on eye damage caused by working in the sun needs to be improved.
[0005] Therefore, it is of great significance to prepare a steam eye mask that is highly moisturizing, has good skin and eye protection effects, is rich in functions, and is comfortable to wear. Summary of the Invention
[0006] The object of the present invention is to provide a highly moisturizing steam eye mask and a preparation method thereof to solve the problems raised in the above background technology.
[0007] In order to solve the above technical problems, the present invention provides the following technical solutions:
[0008] A highly moisturizing steam eye mask comprises a sericin cotton layer, a non-woven fabric layer, a heating sheet, a polyethylene layer, ear hooks, and essence.
[0009] More optimally, the preparation of the heating sheet includes the following steps: taking iron powder, activated carbon powder, hydrogel, vermiculite, polyethylene fiber, sodium chloride, sodium carboxymethyl cellulose, water, and traditional Chinese medicine ingredients, stirring evenly, standing for 5 to 7 hours, pressing into sheets, and drying at 100 to 120°C for 3 to 5 hours to obtain a heating sheet of 1 to 3 mm.
[0010] More optimally, the size of the heating sheet is 4.6 to 5.2 cm in length and 4.6 to 5.2 cm in width.
[0011] More optimally, the heating sheet includes the following raw materials, calculated by weight: 40-50 parts of iron powder, 10-15 parts of activated carbon powder, 0.1-0.5 parts of hydrogel, 0.1-4 parts of vermiculite, 2-5 parts of polyethylene fiber, 1-4 parts of sodium chloride, 1-6 parts of sodium carboxymethyl cellulose, 10-15 parts of water, and 15-20 parts of traditional Chinese medicine ingredients.
[0012] More optimally, the preparation of the hydrogel includes the following steps: S1: taking sodium hydroxide and water, stirring evenly, adding L-lysine, stirring to dissolve, adding 5% copper sulfate solution, cooling to 8-10°C, and simultaneously adding acryloyl chloride and sodium hydroxide solution dropwise for 30-35 minutes, stirring for 10-14 hours, centrifuging to remove the supernatant, taking the precipitate, washing with water, ethanol, and ether, and vacuum drying at 35-45°C for 6-7 hours to obtain a complex precipitate;
[0013] S2: Take the complex precipitate, water, and chloroform solution of 8-hydroxyquinoline, stir for 10-14 hours, remove the green precipitate by suction, extract with chloroform three times, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0014] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are prepared into solution A with an aldehyde-terminated polyethylene glycol concentration of 10-15% (w / v); acryloyl lysine and phosphate buffer are prepared into solution B with an acryloyl lysine concentration of 2-5% (w / v); solutions A and B are mixed in equal volumes to obtain a hydrogel.
[0015] More optimally, the phosphate buffer comprises potassium dihydrogen phosphate and sodium hydroxide.
[0016] More optimally, the concentration of the sodium hydroxide solution is 2M, with the remainder being water; and the concentration of 8-hydroxyquinoline in the chloroform solution of 8-hydroxyquinoline is 4%.
[0017] More optimally, the acryloyl lysine comprises the following raw materials, calculated by weight: 4 to 5 parts of complex precipitate, 25 to 35 parts of water, and 25 to 35 parts of 8-hydroxyquinoline chloroform solution; the complex precipitate comprises the following raw materials, calculated by weight: 1 to 2 parts of sodium hydroxide, 25 to 30 parts of water, 2 to 3 parts of L-lysine, 25 to 30 parts of copper sulfate solution, 1 to 2 parts of acryloyl chloride, and 7 to 8 parts of sodium hydroxide solution.
[0018] Preferably, the sericin cotton layer comprises sericin cotton protein, and the preparation method of sericin cotton protein comprises the following steps: S1: taking cotton fabric, adding it to a sodium periodate solution, oxidizing it at 40-50° C. in the dark for 1-2 hours, washing it with glycerol, washing it with water, and drying it to obtain an oxidized cotton fabric;
[0019] S2: Take oxidized cotton fabric and sericin solution, soak them at 40-50°C for 1-2 hours, pre-bake at 70-80°C for 40-60 seconds, bake at 120-130°C for 20-30 seconds, soak them in water for 24 hours, and dry them to obtain sericin cotton.
[0020] More optimally, the concentration of the sodium periodate solution is 4 g / L, and the rest is water; the sericin solution is prepared from sericin powder and water, the concentration of the sericin powder is 4%, and the rest is water.
[0021] More optimally, the sericin protein comprises the following raw materials, by weight: 1-2 parts of oxidized cotton fabric, 30-40 parts of sericin solution; the oxidized cotton fabric comprises the following raw materials, by weight: 1-2 parts of cotton fabric, 50-60 parts of sodium periodate solution.
[0022] More optimally, the Chinese medicinal ingredients include the following raw materials, calculated by weight: 10 to 12 parts of Glauber's salt, 1 to 2 parts of rhubarb, 1 to 2 parts of Polygonum multiflorum, and 1 to 2 parts of chrysanthemum.
[0023] A method for preparing a highly moisturizing steam eye mask comprises the following steps: pressing a polyethylene film and a non-woven fabric to obtain a layer A; pressing the non-woven fabric and sericin cotton to obtain a layer B; placing a heating element between layers A and B, and pressing them together to obtain a steam eye mask body; connecting ear hooks to both sides of the steam eye mask body; spraying 8-15 wt% tea tree essential oil and 5-10 wt% rose essential oil on one side of layer B that lies adjacent to layer A, drying the layer to obtain the highly moisturizing steam eye mask, and sealing the layer for storage.
[0024] More optimally, the thickness of the sericin cotton is 1.5-3 mm, the thickness of the non-woven fabric is 0.1-0.3 mm, and the thickness of the polyethylene film is 0.22-0.45 mm.
[0025] Compared with the prior art, the present invention has the following beneficial effects: (1) a heating sheet is prepared, wherein the hydrogel prepared by the present invention replaces the super absorbent resin in the conventional technology; the hydrogel is prepared by acryloyl lysine and aldehyde-terminated polyethylene glycol, and is obtained by cross-linking aldehyde groups with amino groups, and has better biocompatibility, good stability, and is easy to prepare; acryloyl lysine has antioxidant effects, eliminates free radicals generated by ultraviolet light, and relieves inflammation, and can effectively relieve problems such as dry eyes and eye pain caused by working under sunlight for a long time; at the same time, acryloyl lysine can repair the skin around the eyes damaged by ultraviolet radiation.
[0026] (2) Sericin cotton is used to replace the cotton layer used in traditional steam eye masks. Sericin has moisturizing and antibacterial effects. The softness and breathability of cotton modified with sericin are improved, which can help improve the wearing comfort of steam eye masks. Tea tree essential oil and rose essential oil are sprayed on the sericin cotton layer, which can be quickly absorbed by the skin, moisturizing the skin, protecting the eyes, and soothing the mood.
[0027] (3) Adding Chinese herbal ingredients to the heating plate, including at least one of Glauber's salt, rhubarb, Polygonum multiflorum, and chrysanthemum, has the effects of clearing away heat and detoxifying, relieving pain and reducing swelling. The Chinese herbal ingredients work together with the essence and hydrogel to repair problems such as intraocular congestion, fatigue, dryness, and pain caused by long-term exposure to electronic products. It can also relieve the damage to the human eye caused by ultraviolet rays when working in the sun for a long time, moisturize the skin around the eyes, and soothe the body and mind. It has complete functions. DETAILED DESCRIPTION
[0028] The following is a clear and complete description of the technical solutions in the embodiments of the present invention. Obviously, the embodiments described are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making any creative efforts are within the scope of protection of the present invention.
[0029] The following raw materials were included in the following examples: iron powder (YM-Fe005, Yumu New Materials Co., Ltd.), activated carbon powder (200 mesh, Shanghai Huzhen Industrial Co., Ltd.), vermiculite (Zhengzhou Huiju Chemical Co., Ltd.), polyethylene fiber membrane (model: DC-0555, Dongchen), non-woven fabric (material: PP, gram weight: 180 g / cm 2 ), cotton fabric (weight: ~170g / cm 2 ), sodium chloride (CAS: 7647-14-5), sodium carboxymethyl cellulose (CAS: 9004-32-4), 8-hydroxyquinoline (CAS: 148-24-3), chloroform (CAS: 67-66-3), sodium hydroxide (CAS: 1310-73-2), aldehyde-terminated polyethylene glycol (molecular weight ~3400, Chongqing Yusi Pharmaceutical Technology Co., Ltd.), phosphate buffer (pH ~7.2, Qingdao High-tech Industrial Park Haibo Biotechnology Co., Ltd.), L-lysine (CAS: 56-87-1), copper sulfate (CAS: 7758-98-7), acryloyl chloride (CAS: 814-68-6), sericin powder (Hubei Chengfeng Chemical Co., Ltd.), sodium periodate (CAS: 7790-28-5); Glauber's salt, rhubarb, Polygonum multiflorum vine, chrysanthemum (Chinese medicinal materials Chengshitong); tea tree essential oil, rose essential oil (Jiangxi Hairui Natural Plant Co., Ltd.).
[0030] The following parts are by mass;
[0031] Example 1: S1: Take 1.5 parts of sodium hydroxide and 30 parts of distilled water, stir evenly, add 3 parts of L-lysine, stir to dissolve, add 30 parts of 5% copper sulfate solution, cool to 10°C, and simultaneously add 1.5 parts of acryloyl chloride and 7.5 parts of sodium hydroxide solution dropwise for 30 minutes. Stir for 12 hours, centrifuge to remove the supernatant, take the precipitate, wash with water, ethanol, and ether, and dry in vacuo at 40°C for 6 hours to obtain a complex precipitate;
[0032] S2: Take 5 parts of the complex precipitate, 30 parts of water, and 30 parts of a chloroform solution of 8-hydroxyquinoline, stir for 12 hours, remove the green precipitate by suction, extract with chloroform three times to remove 8-hydroxyquinoline, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0033] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are mixed to prepare solution A with a 15% (w / v) concentration of aldehyde-terminated polyethylene glycol; acryloyl-lysine and phosphate buffer are mixed to prepare solution B with a 4% (w / v) concentration of acryloyl-lysine; and solutions A and B are mixed in equal volumes to obtain a hydrogel;
[0034] S4: Take 11 parts of Glauber's salt, 2 parts of Rhubarb, 1 part of Polygonum multiflorum, and 1 part of Chrysanthemum, mix them evenly to obtain a traditional Chinese medicine component;
[0035] S5: Take 2 parts of cotton fabric, add them to 50 parts of 4g / L sodium periodate solution, oxidize them at 50℃ in the dark for 1 hour, wash them with glycerol solution, wash them with water, and dry them to obtain oxidized cotton fabric;
[0036] S6: Take 2 parts of oxidized cotton fabric and 40 parts of 4% sericin solution, treat at 50°C for 2 hours, pre-bake at 80°C for 40 seconds, bake at 120°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0037] S7: Take 45 parts of iron powder, 12 parts of activated carbon powder, 0.4 parts of hydrogel, 2 parts of vermiculite, 3 parts of polyethylene fiber, 2 parts of sodium chloride, 3 parts of binder, 18 parts of water, and 16 parts of traditional Chinese medicine ingredients, stir evenly, let it stand for 5 hours, press into sheets, and dry at 110°C for 4 hours to obtain a 2mm heating sheet;
[0038] S8: Press 0.4 mm polyethylene film and 0.2 mm non-woven fabric to obtain layer A; press 0.2 mm non-woven fabric and 2 mm sericin cotton to obtain layer B; place a heating element between layer A and layer B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 14 wt% tea tree essential oil and 8 wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0039] Example 2: S1: Take 1 part of sodium hydroxide and 25 parts of distilled water, stir evenly, add 2 parts of L-lysine, stir to dissolve, add 25 parts of 5% copper sulfate solution, cool to 10°C, and simultaneously add 1 part of acryloyl chloride and 7 parts of sodium hydroxide solution dropwise for 30 minutes. Stir for 10 hours, centrifuge to remove the supernatant, take the precipitate, wash with water, ethanol, and ether, and dry in vacuo at 35°C for 6 hours to obtain a complex precipitate;
[0040] S2: Take 4 parts of the complex precipitate, 30 parts of water, and 30 parts of a chloroform solution of 8-hydroxyquinoline, stir for 10 hours, remove the green precipitate by suction, extract with chloroform three times to remove 8-hydroxyquinoline, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0041] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are mixed to prepare solution A with a 10% (w / v) concentration of aldehyde-terminated polyethylene glycol; acryloyl-lysine and phosphate buffer are mixed to prepare solution B with a 2% (w / v) concentration of acryloyl-lysine; and solutions A and B are mixed in equal volumes to obtain a hydrogel;
[0042] S4: Take 10 parts of Glauber's salt, 1 part of Rhubarb, 1 part of Polygonum multiflorum, and 1 part of Chrysanthemum, mix them evenly to obtain a traditional Chinese medicine component;
[0043] S5: Take 1 part of cotton fabric, add it to 50 parts of 4g / L sodium periodate solution, oxidize it at 40℃ in the dark for 1 hour, wash it with glycerol solution, wash it with water, and dry it to obtain oxidized cotton fabric;
[0044] S6: Take 1 part of oxidized cotton fabric and 30 parts of 4% sericin solution, treat at 40°C for 2 hours, pre-bake at 70°C for 40 seconds, bake at 120°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0045] S7: Take 40 parts of iron powder, 10 parts of activated carbon powder, 0.1 parts of hydrogel, 0.1 parts of vermiculite, 2 parts of polyethylene fiber, 1 part of sodium chloride, 1 part of binder, 15 parts of water, and 15 parts of traditional Chinese medicine ingredients, stir evenly, let it stand for 5 hours, press it into a sheet, and dry it at 100°C for 3 hours to obtain a 3mm heating sheet;
[0046] S8: Press 0.22 mm polyethylene film and 0.3 mm non-woven fabric to obtain layer A; press 0.3 mm non-woven fabric and 1.5 mm sericin cotton to obtain layer B; place a heating element between layer A and layer B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 8 wt% tea tree essential oil and 5 wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0047] Example 3: S1: Take 2 parts of sodium hydroxide and 30 parts of distilled water, stir evenly, add 3 parts of L-lysine, stir to dissolve, add 30 parts of 5% copper sulfate solution, cool to 10°C, and simultaneously add 2 parts of acryloyl chloride and 8 parts of sodium hydroxide solution dropwise for 30 minutes. Stir for 14 hours, centrifuge to remove the supernatant, take the precipitate, wash with water, ethanol, and ether, and dry in vacuo at 45°C for 6 hours to obtain a complex precipitate;
[0048] S2: Take 5 parts of the complex precipitate, 30 parts of water, and 30 parts of a chloroform solution of 8-hydroxyquinoline, stir for 14 hours, remove the green precipitate by suction, extract with chloroform three times to remove 8-hydroxyquinoline, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0049] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are mixed to prepare solution A with a 13% (w / v) aldehyde-terminated polyethylene glycol concentration; acryloyl-lysine and phosphate buffer are mixed to prepare solution B with a 5% (w / v) acryloyl-lysine concentration; solutions A and B are mixed in equal volumes to obtain a hydrogel;
[0050] S4: Take 12 parts of Glauber's salt, 2 parts of Rhubarb, 2 parts of Polygonum multiflorum, and 2 parts of Chrysanthemum, mix them evenly to obtain a traditional Chinese medicine component;
[0051] S5: Take 2 parts of cotton fabric, add them to 60 parts of 4g / L sodium periodate solution, oxidize them at 50℃ in the dark for 2h, wash them with glycerol solution, wash them with water, and dry them to obtain oxidized cotton fabric;
[0052] S6: Take 2 parts of oxidized cotton fabric and 40 parts of 4% sericin solution, treat at 50°C for 1 hour, pre-bake at 70°C for 60 seconds, bake at 130°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0053] S7: Take 50 parts of iron powder, 15 parts of activated carbon powder, 0.5 parts of hydrogel, 4 parts of vermiculite, 5 parts of polyethylene fiber, 4 parts of sodium chloride, 6 parts of binder, 20 parts of water, and 20 parts of traditional Chinese medicine ingredients, stir evenly, let it stand for 7 hours, press into sheets, and dry at 110°C for 5 hours to obtain a 3mm heating sheet;
[0054] S8: Press 0.45mm polyethylene film and 0.1mm non-woven fabric to obtain layer A; press 0.3mm non-woven fabric and 3mm sericin cotton to obtain layer B; place a heating plate between layer A and layer B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 15wt% tea tree essential oil and 10wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0055] Comparative Example 1 (increasing the amount of hydrogel added, and the remaining method steps are consistent with Example 1): S1: Take 1.5 parts of sodium hydroxide and 30 parts of distilled water, stir evenly, add 3 parts of L-lysine, stir to dissolve, add 30 parts of 5% copper sulfate solution, cool to 10°C, and simultaneously add 1.5 parts of acryloyl chloride and 7.5 parts of sodium hydroxide solution dropwise for 30 minutes. Stir for 12 hours, centrifuge to remove the supernatant, take the precipitate, wash with water, ethanol, and ether, and dry in vacuo at 40°C for 6 hours to obtain a complex precipitate;
[0056] S2: Take 5 parts of the complex precipitate, 30 parts of water, and 30 parts of a chloroform solution of 8-hydroxyquinoline, stir for 12 hours, remove the green precipitate by suction, extract with chloroform three times to remove 8-hydroxyquinoline, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0057] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are mixed to prepare solution A with a 15% (w / v) concentration of aldehyde-terminated polyethylene glycol; acryloyl-lysine and phosphate buffer are mixed to prepare solution B with a 4% (w / v) concentration of acryloyl-lysine; and solutions A and B are mixed in equal volumes to obtain a hydrogel;
[0058] S4: Take 11 parts of Glauber's salt, 2 parts of Rhubarb, 1 part of Polygonum multiflorum, and 1 part of Chrysanthemum, mix them evenly to obtain a traditional Chinese medicine component;
[0059] S5: Take 2 parts of cotton fabric, add them to 50 parts of 4g / L sodium periodate solution, oxidize them at 50℃ in the dark for 1 hour, wash them with glycerol solution, wash them with water, and dry them to obtain oxidized cotton fabric;
[0060] S6: Take 2 parts of oxidized cotton fabric and 40 parts of 4% sericin solution, treat at 50°C for 2 hours, pre-bake at 80°C for 40 seconds, bake at 120°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0061] S7: Take 45 parts of iron powder, 12 parts of activated carbon powder, 5 parts of hydrogel, 2 parts of vermiculite, 3 parts of polyethylene fiber, 2 parts of sodium chloride, 3 parts of binder, 18 parts of water, and 16 parts of traditional Chinese medicine ingredients, stir evenly, let it stand for 5 hours, press into sheets, and dry at 110°C for 4 hours to obtain a 2mm heating sheet;
[0062] S8: Press 0.4 mm polyethylene film and 0.2 mm non-woven fabric to obtain layer A; press 0.2 mm non-woven fabric and 2 mm sericin cotton to obtain layer B; place a heating element between layer A and layer B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 14 wt% tea tree essential oil and 8 wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0063] Comparative Example 2 (using a super absorbent resin of model Chengfeng 001 instead of the hydrogel, and the remaining steps are the same as those in Example 1): S1: 11 parts of sodium sulfate, 2 parts of rhubarb, 1 part of Polygonum multiflorum, and 1 part of chrysanthemum are mixed uniformly to obtain a traditional Chinese medicine component;
[0064] S2: Take 2 parts of cotton fabric, add them to 50 parts of 4g / L sodium periodate solution, oxidize them at 50℃ in the dark for 1 hour, wash them with glycerol solution, wash them with water, and dry them to obtain oxidized cotton fabric;
[0065] S3: Take 2 parts of oxidized cotton fabric and 40 parts of 4% sericin solution, treat at 50°C for 2 hours, pre-bake at 80°C for 40 seconds, bake at 120°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0066] S4: Take 45 parts of iron powder, 12 parts of activated carbon powder, 0.4 parts of super absorbent resin, 2 parts of vermiculite, 3 parts of polyethylene fiber, 2 parts of sodium chloride, 3 parts of binder, 18 parts of water, and 16 parts of traditional Chinese medicine ingredients, stir evenly, let it stand for 5 hours, press into sheets, and dry at 110°C for 4 hours to obtain a 2mm heating sheet;
[0067] S5: Press a 0.4 mm polyethylene film and a 0.2 mm non-woven fabric to obtain layer A; press a 0.2 mm non-woven fabric and a 2 mm sericin cotton to obtain layer B; place a heating element between layers A and B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 14 wt% tea tree essential oil and 8 wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0068] Comparative Example 3 (using a cotton layer instead of a sericin cotton layer; the remaining steps are the same as in Example 1): S1: 1.5 parts of sodium hydroxide and 30 parts of distilled water are mixed and uniformly stirred. 3 parts of L-lysine are added and stirred to dissolve. 30 parts of a 5% copper sulfate solution are added, and the mixture is cooled to 10° C. Simultaneously, 1.5 parts of acryloyl chloride and 7.5 parts of a sodium hydroxide solution are added dropwise for 30 minutes. The mixture is stirred for 12 hours, and the supernatant is removed by centrifugation. The precipitate is collected, washed with water, ethanol, and ether, and dried in vacuo at 40° C. for 6 hours to obtain a complex precipitate.
[0069] S2: Take 5 parts of the complex precipitate, 30 parts of water, and 30 parts of a chloroform solution of 8-hydroxyquinoline, stir for 12 hours, remove the green precipitate by suction, extract with chloroform three times to remove 8-hydroxyquinoline, and freeze-dry the remaining liquid to obtain acryloyl lysine;
[0070] S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are mixed to prepare solution A with a 15% (w / v) concentration of aldehyde-terminated polyethylene glycol; acryloyl-lysine and phosphate buffer are mixed to prepare solution B with a 4% (w / v) concentration of acryloyl-lysine; and solutions A and B are mixed in equal volumes to obtain a hydrogel;
[0071] S4: Take 11 parts of mirabilite, 2 parts of rhubarb, 1 part of first wu, 1 part of chrysanthemum, mix evenly, get traditional Chinese medicine ingredients;
[0072] S5: Take 45 parts of iron powder, 12 parts of activated carbon powder, 0.4 parts of hydrogel, 2 parts of vermiculite, 3 parts of polyethylene fiber, 2 parts of sodium chloride, 3 parts of binder, 18 parts of water, 16 parts of traditional Chinese medicine ingredients, stir evenly, stand for 5h, press into sheet, dry at 110℃ for 4h, get 2mm heating sheet;
[0073] S6: 0.4mm polyethylene film and 0.2mm non-woven fabric are pressed together to get layer A; 0.2mm non-woven fabric and 2mm cotton fabric are pressed together to get layer B; the heating sheet is placed between layer A and layer B, and then pressed to get the steam eye mask body; ear hooks are connected on both sides of the steam eye mask body; 14wt% tea tree essential oil and 8wt% rose essential oil are sprayed on the silk sericin cotton layer, and then dried to get the high-moisture steam eye mask, which is sealed and stored.
[0074] Comparative example 4 (the heating material is not pressed into sheet, and the rest of the method steps are consistent with example 1)
[0075] S2: Take 5 parts of complex precipitate, 30 parts of water, 30 parts of 8-hydroxyquinoline chloroform solution, stir for 12h, remove the green precipitate by suction filtration, extract with chloroform for 3 times, remove 8-hydroxyquinoline, freeze-dry the remaining liquid to get acryloyl lysine;
[0076] S3: The aldehyde-terminated polyethylene glycol is configured with phosphate buffer to get A solution with aldehyde-terminated polyethylene glycol concentration of 15%(w / v); the acryloyl lysine is configured with phosphate buffer to get B solution with acryloyl lysine concentration of 4%(w / v); the A and B solutions are mixed in equal volume to get hydrogel;
[0077] S4: Take 11 parts of mirabilite, 2 parts of rhubarb, 1 part of first wu, 1 part of chrysanthemum, mix evenly, get traditional Chinese medicine ingredients;
[0078] S5: Take 2 parts of cotton fabric, add 50 parts of 4g / L sodium periodate solution, 50℃ avoid light oxidation for 1h, wash with glycerol solution, wash with water, dry to get oxidized cotton fabric;
[0079] S6: Take 2 parts of oxidized cotton fabric and 40 parts of 4% sericin solution, treat at 50°C for 2 hours, pre-bake at 80°C for 40 seconds, bake at 120°C for 20 seconds, soak in water for 24 hours, and dry to obtain sericin cotton;
[0080] S7: Take 45 parts of iron powder, 12 parts of activated carbon powder, 0.4 parts of hydrogel, 2 parts of vermiculite, 3 parts of polyethylene fiber, 2 parts of sodium chloride, 3 parts of binder, 18 parts of water, and 16 parts of traditional Chinese medicine ingredients, stir well to obtain a heating material;
[0081] S8: Press 0.4 mm polyethylene film and 0.2 mm non-woven fabric to obtain layer A; press 0.2 mm non-woven fabric and 2 mm sericin cotton to obtain layer B; place a heating material between layer A and layer B, and press them together to obtain a steam eye mask body; connect ear hooks on both sides of the steam eye mask body; spray 14 wt% tea tree essential oil and 8 wt% rose essential oil on the sericin cotton layer, dry it, and obtain a highly moisturizing steam eye mask, which is then sealed and stored.
[0082] Experiment: (1) The high-moisturizing steam eye masks prepared in Examples 1 to 3 and Comparative Examples 1 to 4 were measured, and the average temperature and the maximum temperature in the heating stage were measured; the moisturizing rate was tested by referring to the in vitro gravimetric method; the specific data are shown in Table 1;
[0083] Table 1:
[0084] Average temperature / ℃ Maximum temperature / ℃ Moisturizing rate / % Example 1 40 43 66 Example 2 41 44 66 Example 3 41 44 65 Comparative Example 1 37 40 65 Comparative Example 2 41 45 57 Comparative Example 3 40 44 61 Comparative Example 4 41 48 63
[0085] Conclusion: Table 1 shows that increasing the amount of hydrogel added has little effect on the steam mask's moisturizing rate, but it does affect the heating performance of the heating element, so the amount added needs to be controlled. The use of commercially available superabsorbent resin slightly decreased the steam mask's moisturizing rate. The use of cotton fabric untreated with sericin also decreased the steam mask's moisturizing rate. There is a risk of localized overheating when using heating powder packs.
[0086] (2) 100 highly moisturizing steam eye masks prepared in Example 1 were distributed to office workers aged 20 to 45 for trial wearing; the specific evaluation is shown in Table 2;
[0087] Table 2:
[0088] Comfort Satisfaction with eye protection effect Example 1 97% 98%
[0089] Conclusion: As shown in Table 2, the highly moisturizing steam eye mask prepared in Example 1 provides excellent comfort and eye protection satisfaction. This is due to the softness and good breathability of the sericin cotton layer, the excellent hydrating and eye-protecting effects of the hydrogel, and the combined effects of the traditional Chinese medicine ingredients and the essence. It can repair problems such as intraocular congestion, fatigue, dryness, and pain caused by prolonged use of electronic products. It can also relieve damage to the human eye caused by ultraviolet rays when working in the sun for a long time, moisturize the skin around the eyes, and soothe the body and mind. It is a comprehensive product.
[0090] In summary, the solution provided by the present invention can prepare a steam eye mask with high moisturizing, good comfort, and good eye and skin protection effects.
[0091] It should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that includes a list of elements includes not only those elements but also other elements not explicitly listed, or elements inherent to such process, method, article, or apparatus.
[0092] Finally, it should be noted that the above descriptions are merely preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art will be able to modify the technical solutions described in the aforementioned embodiments or substitute equivalents for some of the technical features. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention shall be included within the scope of protection of the present invention.
Claims
1. A method for preparing a highly moisturizing steam eye mask, characterized in that: The following steps are involved: The method comprises the following steps: laminating a polyethylene film and a non-woven fabric to obtain a layer A; laminating the non-woven fabric and sericin cotton to obtain a layer B; placing a heating element between layers A and B, and laminating them to obtain a steam eye mask body; attaching ear hooks to both sides of the steam eye mask body; spraying 8-15 wt% tea tree essential oil and 5-10 wt% rose essential oil on the side of layer B away from layer A, drying the layer, and obtaining a highly moisturizing steam eye mask, which is then sealed and stored. The preparation of the heating sheet comprises the following steps: taking iron powder, activated carbon powder, hydrogel, vermiculite, polyethylene fiber, sodium chloride, sodium carboxymethyl cellulose, water, and traditional Chinese medicine components, stirring them evenly, letting them stand for 5 to 7 hours, pressing them into sheets, and drying them at 100 to 120° C. for 3 to 5 hours to obtain a heating sheet with a thickness of 1 to 3 mm; The heating sheet comprises the following raw materials, calculated by weight: 40-50 parts of iron powder, 10-15 parts of activated carbon powder, 0.1-0.5 parts of hydrogel, 0.1-4 parts of vermiculite, 2-5 parts of polyethylene fiber, 1-4 parts of sodium chloride, 1-6 parts of sodium carboxymethyl cellulose, 10-15 parts of water, and 15-20 parts of traditional Chinese medicine ingredients; The preparation of the hydrogel comprises the following steps: S1: Take sodium hydroxide and water, stir evenly, add L-lysine, stir to dissolve, add 5% copper sulfate solution, cool to 8-10°C, and simultaneously add acryloyl chloride and sodium hydroxide solution dropwise for 30-35 minutes. Stir for 10-14 hours, centrifuge to remove the supernatant, take the precipitate, wash with water, ethanol, and ether, and dry in a vacuum at 35-45°C for 6-7 hours to obtain a complex precipitate; S2: Take the complex precipitate, water, and chloroform solution of 8-hydroxyquinoline, stir for 10-14 hours, remove the green precipitate by suction, extract with chloroform three times, and freeze-dry the remaining liquid to obtain acryloyl lysine; S3: Aldehyde-terminated polyethylene glycol and phosphate buffer are prepared into solution A with an aldehyde-terminated polyethylene glycol concentration of 10-15%; acryloyl lysine and phosphate buffer are prepared into solution B with an acryloyl lysine concentration of 2-5%; solutions A and B are mixed in equal volumes to obtain a hydrogel.
2. The method for preparing a highly moisturizing steam eye mask according to claim 1, characterized in that: The acryloyl lysine comprises the following raw materials, calculated in parts by weight: 4-5 parts of complex precipitate, 25-35 parts of water, and 25-35 parts of 8-hydroxyquinoline chloroform solution; the complex precipitate comprises the following raw materials, calculated in parts by weight: 1-2 parts of sodium hydroxide, 25-30 parts of water, 2-3 parts of L-lysine, 25-30 parts of copper sulfate solution, 1-2 parts of acryloyl chloride, and 7-8 parts of sodium hydroxide solution.
3. The method for preparing a highly moisturizing steam eye mask according to claim 1, characterized in that: Preparation method of sericin cotton The following steps are involved: S1: Take cotton fabric, add it to sodium periodate solution, oxidize it at 40-50℃ in the dark for 1-2 hours, wash it with glycerol, wash it with water, and dry it to obtain oxidized cotton fabric; S2: Take oxidized cotton fabric and sericin solution, soak them at 40-50°C for 1-2 hours, pre-bake at 70-80°C for 40-60 seconds, bake at 120-130°C for 20-30 seconds, soak them in water for 24 hours, and dry them to obtain sericin cotton.
4. The method for preparing a highly moisturizing steam eye mask according to claim 3, characterized in that: The sericin cotton comprises the following raw materials, calculated by weight: 1-2 parts of oxidized cotton fabric and 30-40 parts of sericin solution; the oxidized cotton fabric comprises the following raw materials, calculated by weight: 1-2 parts of cotton fabric and 50-60 parts of sodium periodate solution.
5. The method for preparing a highly moisturizing steam eye mask according to claim 1, characterized in that: The thickness of the sericin cotton is 1.5-3 mm, the thickness of the non-woven fabric is 0.1-0.3 mm, and the thickness of the polyethylene film is 0.22-0.45 mm.
6. The method for preparing a highly moisturizing steam eye mask according to claim 1, characterized in that: The traditional Chinese medicine ingredients include at least two of Glauber's salt, rhubarb, Polygonum multiflorum and chrysanthemum.
7. A highly moisturizing steam eye mask obtained by the method for preparing a highly moisturizing steam eye mask according to any one of claims 1 to 6.
Citation Information
Patent Citations
Sericin linen product and preparation method thereof
CN105926291A
Novel self-heating eyeshade and preparation process
CN111568640A
An exothermic drug plaster
CN1864653A