Array substrate and its fabrication method, display panel
By setting an undercut structure on the surface of the passivation layer, the pixel electrode is disconnected at the undercut structure to form a display electrode and a slit, which solves the problem of foreign matter residue at the edge of the pixel electrode in the array substrate and improves the display effect.
Patent Information
- Application Number
- CN202410128439.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-29
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-01-29
AI Technical Summary
In existing array substrates, bottom voids or fuzzy foreign matter residues are prone to appear at the edges of pixel electrode lines, leading to poor display quality.
Multiple undercut structures are formed on the surface of the passivation layer away from the substrate. The pixel electrode is disconnected at the undercut structure to form a spaced display electrode and slit. A velvety material is formed by ashing the photoresist layer and the passivation layer, and the stripping liquid is used to contact the undercut structure to improve the stripping efficiency.
It enhances the peeling effect of the photoresist layer, avoids the formation of burrs at both ends of the photoresist layer, improves the clarity and display effect of the display electrode, and reduces foreign matter residue at the edge of the pixel electrode.
Smart Images

Figure CN117991551B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of display technology, and in particular to an array substrate, its fabrication method, and a display panel. Background Technology
[0002] To save costs, existing amorphous silicon semiconductor processes are evolving towards 3-mask technology. The passivation layer and pixel electrode layer are fabricated using the same mask. Specifically, a flocking process is applied to the photoresist layer above the passivation layer. The undulating surface features of the flocked structure allow the pixel electrode layer covering it to fracture. Then, a stripping solution is used to simultaneously peel off the photoresist layer and the pixel electrode, forming the display electrode and the slit between adjacent display electrodes. However, because the photoresist layer has a gentle angle and a long trailing edge, burrs easily form at its ends during peeling. This can result in empty shells or flocking foreign matter residue at the edge of the pixel electrode, potentially causing display defects. Summary of the Invention
[0003] This invention provides an array substrate and its fabrication method, as well as a display panel, which can solve the technical problem that existing array substrates have bottom empty shells or fuzzy foreign matter residues at the edge of the pixel electrode lines, which easily cause display defects.
[0004] This invention provides an array substrate, comprising:
[0005] Substrate;
[0006] A driving circuit layer is disposed on one side of the substrate;
[0007] A passivation layer is disposed on the side of the driving circuit layer away from the substrate; and
[0008] A pixel electrode is disposed on the side of the passivation layer away from the substrate and electrically connected to the driving circuit layer through a via penetrating the passivation layer. The pixel electrode includes a plurality of spaced display electrodes and a slit located between two adjacent display electrodes. The passivation layer near the display electrode of the slit is recessed from the surface away from the substrate to the side closer to the substrate to form an undercut structure.
[0009] According to an embodiment of the present invention, the passivation layer of the array substrate includes a main body portion and a micro-oxidation portion located on the side of the main body portion away from the substrate, wherein one side surface of the main body portion is recessed toward the side closer to the substrate to form the undercut structure.
[0010] According to the array substrate provided in the embodiments of the present invention, the material of the micro-oxidation portion includes silicon oxide, and the material of the main body portion includes silicon nitride.
[0011] According to the array substrate provided in the embodiment of the present invention, the orthographic projection of each slit on the substrate covers the orthographic projection of the corresponding undercut structure on the substrate.
[0012] According to the array substrate provided in the embodiment of the present invention, in the thickness direction of the substrate, from the side of the passivation layer away from the substrate to the side of the passivation layer close to the substrate, the width dimension of the undercut structure gradually increases.
[0013] According to the array substrate provided in the embodiment of the present invention, the pixel electrode further includes a connection electrode disposed separately from the display electrode, and the connection electrode is electrically connected to the driving circuit layer through a via penetrating the passivation layer.
[0014] This invention provides a display panel including the array substrate described above;
[0015] Opposing substrate, disposed opposite to the array substrate; and
[0016] A liquid crystal layer, disposed between the array substrate and the opposing substrate, comprises a plurality of liquid crystal molecules.
[0017] This invention provides a method for fabricating an array substrate, comprising the following steps:
[0018] Provide a substrate;
[0019] A driving circuit layer is formed on one side of the substrate;
[0020] A passivation layer is formed on the side of the driving circuit layer away from the substrate; and
[0021] A pixel electrode is formed on the side of the passivation layer away from the substrate. The pixel electrode includes a plurality of display electrodes spaced apart, and a slit is provided between two adjacent display electrodes.
[0022] The step of forming a pixel electrode on the side of the passivation layer away from the substrate includes:
[0023] A photoresist layer is formed on the entire side of the passivation layer away from the substrate;
[0024] A photomask is provided to pattern the photoresist layer so that the thickness of the photoresist layer corresponding to the display electrode to be formed is greater than the thickness of the photoresist layer corresponding to the slit to be formed, and the portion of the photoresist layer corresponding to the via to be formed is removed to expose the passivation layer.
[0025] Oxygen is introduced to perform a first ashing treatment on the photoresist layer, so that the portion of the photoresist layer corresponding to the display electrode to be formed is thinned to form a photoresist portion, the portion of the photoresist layer corresponding to the slit to be formed is removed to expose the passivation layer, and the passivation layer not covered by the photoresist layer is etched away to form the via, wherein a velvety texture is formed on the photoresist portion, and the surface of the passivation layer located between two adjacent photoresist portions on the side away from the substrate is micro-oxidized;
[0026] A mixture of oxygen and sulfur hexafluoride is introduced to perform a second ashing treatment on the photoresist layer, so that the edge of the photoresist portion is etched away to expose the passivation layer, and the exposed passivation layer is etched to form multiple undercut structures.
[0027] A pixel electrode is formed on the photoresist layer, the passivation layer, and the driving circuit layer; the pixel electrode is disconnected at the undercut structure to form the display electrode and the slit; and
[0028] The photoresist layer is peeled off.
[0029] According to the method for fabricating an array substrate provided in an embodiment of the present invention, during the first ashing process, the surface of the drain electrode of the driving circuit layer exposed by the via, on the side away from the substrate, is micro-oxidized to form a metal sacrificial layer; and
[0030] During the second ashing process, the metal sacrificial layer is deoxidized.
[0031] According to the method for preparing an array substrate provided in an embodiment of the present invention, the ratio of oxygen to sulfur hexafluoride in the second ashing gas is in the range of 5:1 to 10:1.
[0032] Beneficial effects: In the array substrate and its preparation method and display panel provided in the embodiments of the present invention, by providing multiple undercut structures on the surface of the passivation layer away from the substrate, the pixel electrode is broken in the undercut structure to form multiple spaced display electrodes and slits located between two adjacent display electrodes, so that the pixel electrode has a clear slit boundary. When the photoresist layer with velvety material and the pixel electrode located on the photoresist layer are peeled off to form the display electrode and slit, the stripping liquid can easily contact the photoresist layer through the undercut structure, which increases the immersion path of the stripping liquid at the edge of the photoresist part, which is beneficial to improve the stripping effect and efficiency of the photoresist layer, and avoids the formation of burrs at both ends of the photoresist layer when it is peeled off, which would cause the bottom shell or velvety foreign matter residue to appear at the edge of the pixel electrode, thus improving the display effect. Attached Figure Description
[0033] To more clearly illustrate the technical solutions in the embodiments of the present invention, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0034] Figure 1 This is a schematic diagram of a first cross-sectional structure of an array substrate provided in an embodiment of the present invention;
[0035] Figure 2 This is a schematic diagram of a second cross-sectional structure of the array substrate provided in an embodiment of the present invention;
[0036] Figure 3 This is a schematic diagram of a third cross-sectional structure of the array substrate provided in an embodiment of the present invention;
[0037] Figure 4 This is a schematic flowchart of the method for fabricating an array substrate provided in an embodiment of the present invention;
[0038] Figure 5 for Figure 4 A flowchart illustrating step S40 in the process;
[0039] Figures 6A-6J A schematic diagram of the process structure of the array substrate fabrication method provided in the embodiment of the present invention;
[0040] Figure 7 This is a schematic diagram of the cross-sectional structure of a display panel provided in an embodiment of the present invention.
[0041] Explanation of reference numerals in the attached figures:
[0042] 10. Substrate; 11. Driving circuit layer; 110. Gate; 111. Gate insulating layer; 112. Semiconductor layer; 113. Source; 114. Drain; 115. Common electrode; 1141. Metal sacrificial layer; 12. Passivation layer; 120. Undercut structure; 121. Via; 122. Main body; 123. Micro-oxidation part; 13. Pixel electrode; 131. Display electrode; 132. Slit; 133. Connecting electrode; 20. Photoresist layer; 21. Photoresist part; 30. Photomask; 31. Transparent area; 32. Semi-transparent area; 33. Light-shielding area; 100. Array substrate; 200. Opposing substrate; 300. Liquid crystal layer; 301. Liquid crystal molecule. Detailed Implementation
[0043] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0044] In the description of this invention, it should be understood that the terms "length," "width," "thickness," "upper," "lower," etc., indicating orientation or positional relationships are based on the orientation or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. In the description of this invention, "a plurality of" means two or more, unless otherwise explicitly specified.
[0045] In this invention, unless otherwise expressly specified and limited, the first feature "above" or "below" the second feature may include direct contact between the first and second features, or contact between the first and second features not in direct contact but through another feature between them.
[0046] This invention provides an array substrate, a method for fabricating the same, and a display panel. These are described in detail below. It should be noted that the order of description of the following embodiments is not intended to limit the preferred order of the embodiments.
[0047] Please see Figure 1 This invention provides an array substrate 100, which includes:
[0048] Substrate 10;
[0049] A driving circuit layer 11 is disposed on one side of the substrate 10;
[0050] A passivation layer 12 is disposed on the side of the driving circuit layer 11 away from the substrate 10; and
[0051] A pixel electrode 13 is disposed on the side of the passivation layer 12 away from the substrate 10 and is electrically connected to the driving circuit layer 11 through a via 121 penetrating the passivation layer 12. The pixel electrode 13 includes a plurality of spaced display electrodes 131 and a slit 132 located between two adjacent display electrodes 131. The passivation layer 12 near the display electrode 131 of the slit 132 is recessed from the surface away from the substrate 10 to the side closer to the substrate 10 to form an undercut structure 120.
[0052] It is understood that in the array substrate 100 and its preparation method and display panel provided in the embodiments of the present invention, by providing a plurality of undercut structures 120 on the side surface of the passivation layer 12 away from the substrate 10, the pixel electrode 13 is broken at the undercut structure 120 to form a plurality of spaced display electrodes 131 and a slit 132 located between two adjacent display electrodes 131, so that the pixel electrode 13 has a clear boundary of the slit 132. When the photoresist layer 20 with the velvety material formed and the pixel electrode 13 located on the photoresist layer 20 are peeled off to form the display electrode 131 and the slit 132, the stripping liquid can easily contact the photoresist layer 20 through the undercut structure 120, which increases the immersion path of the stripping liquid at the edge of the photoresist portion 21, which is beneficial to improve the stripping effect and efficiency of the photoresist layer 20, and avoids the formation of burrs at both ends of the photoresist layer 20 when it is peeled off, which would cause the bottom shell or velvety foreign matter residue to appear at the edge of the pixel electrode 13, thus improving the display effect.
[0053] Specifically, the substrate 10 can be a rigid substrate, such as glass or transparent resin, or a flexible substrate, such as polyimide, polycarbonate, polyethersulfone, polyethylene terephthalate, polyethylene naphthalate, polyaryl compounds, or glass fiber reinforced plastic. The present invention does not limit the material of the substrate 10.
[0054] The driving circuit layer 11 provides multiple pixel driving circuits and multiple signal traces. Each pixel driving circuit includes a thin-film transistor electrically connected to a corresponding signal trace, used to transmit electrical signals to the corresponding pixel unit, thereby achieving image display. It should be noted that... Figure 1 The driving circuit layer 11 described herein is for illustrative purposes only and does not show a specific film structure. This part will be described in detail in the following embodiments.
[0055] The pixel electrodes 13 can all be made of transparent conductive materials, such as one or a combination of indium tin oxide (ITO) and indium zinc oxide (IZO). It should be noted that the display electrodes 131 are similar to branch electrodes in a multi-domain pixel electrode, with multiple branch electrodes electrically connected to the main electrode. The slits 132 are similar to the gap between two adjacent branch electrodes. That is, a certain gap needs to be left between two adjacent display electrodes 131 to form the slits 132. This invention utilizes a flocking process to form the display electrodes 131 and the slits 132, the details of which will be described in detail in the following embodiments regarding the fabrication method of the array substrate 100.
[0056] The passivation layer 12 is made of an inorganic insulating material. Optionally, the material of the passivation layer 12 includes any one or a combination of silicon oxide, silicon nitride, and silicon oxynitride. For example, the material of the passivation layer 12 is silicon nitride.
[0057] It is understood that the undercut structure 120 in this embodiment of the invention is a groove formed by recessing the surface of the passivation layer 12 away from the substrate 10 toward the side closer to the substrate 10. Specifically, the cross-sectional shape of the undercut structure 120 is a trapezoid, so that the pixel electrode 13 can be disconnected at the undercut structure 120.
[0058] Specifically, the dimension of the undercut structure 120 in the thickness direction of the array substrate 100 is smaller than the thickness of the passivation layer 12. That is, the undercut structure 120 does not penetrate the passivation layer 12, so as to avoid the metal layer located on the upper layer of the driving circuit layer 11 being exposed by the undercut structure 120, resulting in display defects.
[0059] In an embodiment of the present invention, the passivation layer 12 includes a main body portion 122 and a micro-oxidation portion 123 located on the side of the main body portion 122 away from the substrate 10. One side surface of the main body portion 122 is recessed towards the side close to the substrate 10 to form the undercut structure 120. The micro-oxidation portion 123 is located between two adjacent undercut structures 120, and the display electrode 131 is located on the side of the micro-oxidation portion 123 away from the substrate 10.
[0060] It should be noted that, for the same type of ashing gas, the etching rate of the main body 122 is greater than the etching rate of the micro-oxidation portion 123. This is such that when the main body 122 forms the undercut structure 120, the micro-oxidation portion 123 has not yet started etching or has only been etched in a very small portion and is retained. This prevents the undercut structure 120 from spreading to the micro-oxidation portion 123, thereby allowing the display electrode 131 to be formed on the micro-oxidation portion 123.
[0061] In this embodiment of the invention, the orthographic projection of each slit 132 on the substrate 10 covers the orthographic projection of the corresponding undercut structure 120 on the substrate 10. That is, the undercut structure 120 is provided corresponding to the slit 132. Specifically, the undercut structure 120 is located on the side edge of the slit 132 near the micro-oxidation portion 123.
[0062] It should be noted that, in this embodiment of the invention, the size of the undercut structure 120 cannot be too large or too small. Specifically, if the size of the undercut structure 120 is too large, the pixel electrode 13 is easily formed within the undercut structure 120, while if the size of the undercut structure 120 is too small, the pixel electrode 13 may not be able to break at the undercut structure 120.
[0063] Specifically, the undercut structure 120 has a dimension in the thickness direction of the array substrate 100 ranging from 500 angstroms to 1000 angstroms, for example, it can be one of 500 angstroms, 550 angstroms, 600 angstroms, 650 angstroms, 700 angstroms, 750 angstroms, 800 angstroms, 850 angstroms, 900 angstroms, 950 angstroms, and 1000 angstroms. The width of the undercut structure 120 in the horizontal direction ranges from 1000 angstroms to 1500 angstroms, for example, it can be one of 1000 angstroms, 1100 angstroms, 1200 angstroms, 1300 angstroms, 1400 angstroms, and 1500 angstroms.
[0064] The inclination angle between the sidewall and the bottom surface of the undercut structure 120 is greater than 0 degrees and less than 90 degrees. Optionally, the inclination angle between the sidewall and the bottom surface of the undercut structure 120 is greater than 15 degrees and less than or equal to 45 degrees. For example, it can be one of 15 degrees, 20 degrees, 25 degrees, 30 degrees, 35 degrees, 40 degrees and 45 degrees.
[0065] In this embodiment of the invention, the micro-oxidation portion 123 and the main body portion 122 are integrally formed and are both part of the passivation layer 12. The main body portion 122 is the unoxidized portion of the passivation layer 12, and the micro-oxidation portion 123 is the oxidized portion of the passivation layer 12. Specifically, the material of the main body portion 122 includes silicon nitride, and the material of the micro-oxidation portion 123 includes silicon oxide.
[0066] Please see Figure 1 and Figure 2 The pixel electrode 13 further includes a connection electrode 133 disposed separately from the display electrode 131. The connection electrode 133 is electrically connected to the driving circuit layer 11 through the through-hole 121. The display electrode 131 and the connection electrode 133 can be electrically connected through other parts of the pixel electrode 13 to have the same pixel voltage.
[0067] like Figure 2 As shown, the bottom-cut structure 120 is provided on both sides of the connecting electrode 133. Similarly, this is to avoid the occurrence of bottom shells or foreign matter residues on the edges of the connecting electrode 133, which is beneficial to improving the display effect.
[0068] Please see Figure 3The driving circuit layer 11 includes a first metal layer, a gate insulating layer 111, a semiconductor layer 112, and a second metal layer. Specifically, the first metal layer is disposed on one side of the substrate 10 and includes a gate 110 and a scan line (not shown in the figure). The gate insulating layer 111 covers the first metal layer, and the semiconductor layer 112 is disposed on the side of the gate insulating layer 111 away from the substrate 10. The second metal layer is disposed on the side of the semiconductor layer 112 away from the substrate 10 and includes a source 113, a drain 114, and a data line (not shown in the figure). The passivation layer 12 covers the semiconductor layer 112 and the source / drain metal layers, and the connection electrode 133 is electrically connected to the drain 114 through the via 121. The multiple signal traces include the data line and the scan line. The thin-film transistor is electrically connected to the data line and the scan line. The data line is used to transmit data signals to the pixel electrode 13, and the scan line is used to control the closing and closing of the thin-film transistor.
[0069] Specifically, the driving circuit layer 11 also includes a common electrode 115, and a storage capacitor can be formed between the pixel electrode 13 and the common electrode 115. The size of the storage capacitor is determined by the distance between the pixel electrode 13 and the common electrode 115 layer and the area opposite to each other.
[0070] In this embodiment of the invention, the orthogonal projection of the first metal layer on the substrate 10 lies within the orthogonal projection of the common electrode 115 on the substrate 10. This is because the common electrode 115 and the first metal layer are fabricated using the same photomask. Similarly, the orthogonal projection of the second metal layer on the substrate 10 lies within the orthogonal projection of the semiconductor layer 112 on the substrate 10. This is because the second metal layer and the semiconductor layer 112 are fabricated using the same photomask, which helps to save on manufacturing processes and reduce production costs.
[0071] Please see Figure 4 , Figure 5 and Figures 6A-6J The present invention also provides a method for fabricating an array substrate 100, comprising the following steps:
[0072] S10: Provides a substrate 10;
[0073] S20: A driving circuit layer 11 is formed on one side of the substrate 10;
[0074] S30: A passivation layer 12 is formed on the side of the driving circuit layer 11 away from the substrate 10; and
[0075] S40: A pixel electrode 13 is formed on the side of the passivation layer 12 away from the substrate 10. The pixel electrode 13 includes a plurality of display electrodes 131 arranged at intervals, and a slit 132 is provided between two adjacent display electrodes 131.
[0076] For details, please refer to Figure 6A In step S20, the step of forming the driving circuit layer 11 includes: forming a common electrode and a first metal layer on one side of the substrate 10 using a photomask, wherein the first metal layer is formed on the side of the common electrode away from the substrate 10; forming a gate insulating layer covering the first metal layer and the common electrode; and forming a semiconductor layer and a second metal layer on one side of the gate insulating layer using a photomask, wherein the second metal layer is formed on the side of the semiconductor layer away from the substrate, and the second metal layer includes a source and a drain.
[0077] For details, please refer to Figure 6B In step S30, the passivation layer 12 can be formed on the entire side of the second metal layer away from the substrate 10 by deposition, sputtering, or coating processes. Optionally, the material of the passivation layer 12 includes silicon nitride.
[0078] For further details, please refer to Figures 6C-6J The step of forming the pixel electrode 13 on the side of the passivation layer 12 away from the substrate 10 includes:
[0079] S401: A photoresist layer 20 is formed on the entire side of the passivation layer 12 away from the substrate 10.
[0080] For details, please refer to Figure 6C The photoresist layer 20 is an organic material layer that can be prepared by deposition, sputtering or coating processes, and the photoresist layer 20 has a uniform thickness.
[0081] S402: Provide a photomask 30 to pattern the photoresist layer 20 so that the thickness of the photoresist layer 20 corresponding to the display electrode 131 to be formed is greater than the thickness of the photoresist layer 20 corresponding to the slit 132 to be formed, and the portion of the photoresist layer 20 corresponding to the via 121 to be formed is removed to expose the passivation layer 12.
[0082] For details, please refer to Figure 6D and Figure 6EThe photomask 30 can be a halftone photomask, which includes a light-transmitting area 31, a semi-transmitting area 32, and a light-shielding area 33. The light-transmitting area 31 corresponds to the via 121 to be formed, which penetrates the passivation layer 12 and is used to electrically connect the pixel electrode 13 and the driving circuit layer 11. The semi-transmitting area 32 corresponds to the slit 132 to be formed between two adjacent display electrodes 131. The light-shielding area 33 corresponds to the display electrode 131 to be formed. The light transmittance of the light-transmitting area 31 is greater than that of the semi-transmitting area 32, and the light transmittance of the semi-transmitting area 32 is greater than that of the light-shielding area 33. For example, the light transmittance of the light-transmitting area 31 is 100%, the light transmittance of the semi-transmitting area 32 is 50%, and the light transmittance of the light-shielding area 33 is 0%. Thus, when the passivation layer 12 is exposed using the halftone photomask, the photoresist layer 20 corresponding to the light-transmitting area 31 is completely removed to expose the passivation layer 12, the photoresist layer 20 corresponding to the light-shielding area 33 is completely retained, and a portion of the photoresist layer 20 corresponding to the semi-transparent area 32 is etched away, thereby making the thickness of the photoresist layer 20 corresponding to the light-shielding area 33 greater than the thickness of the photoresist layer 20 corresponding to the semi-transparent area 32.
[0083] S403: Oxygen is introduced to perform a first ashing treatment on the photoresist layer 20, so that the portion of the photoresist layer 20 corresponding to the display electrode 131 to be formed is thinned to form a photoresist portion 21, the portion of the photoresist layer 20 corresponding to the slit 132 to be formed is removed to expose the passivation layer 12, and the passivation layer 12 not covered by the photoresist layer 20 is etched away to form the via 121, wherein a velvety texture is formed on the photoresist portion 21, and the surface of the passivation layer 12 located between two adjacent photoresist portions 21 on the side away from the substrate 10 is micro-oxidized.
[0084] For details, please refer to Figure 6F The photoresist layer 20 is subjected to a first ashing treatment using a high concentration of oxygen. The passivation layer 12 at the drain electrode 114 is etched away to form the via 121. The exposed surface of the passivation layer 12 is also micro-oxidized to form micro-oxidized portions 123, while the remaining unoxidized portions of the passivation layer 12 form the main body 122. During this first ashing treatment, the photoresist layer 20 is flocked to form a velvety texture on its surface.
[0085] Furthermore, during the first ashing process, the surface of the drain 114 of the drive circuit layer 11 exposed by the via 121 away from the substrate 10 is micro-oxidized to form a metal sacrificial layer 1141, so as to prevent the lint falling off the photoresist layer 20 from falling onto the exposed drain 114, which would affect the process stability and optical quality.
[0086] S404: A mixture of oxygen and sulfur hexafluoride is introduced to perform a second ashing treatment on the photoresist layer 20, so that the edge of the photoresist portion 21 is etched away to expose the passivation layer 12, and the exposed passivation layer 12 is etched to form a plurality of undercut structures 120.
[0087] For details, please refer to Figure 6G and Figure 6H The mixed gas may also include helium. During the second ashing process, the edges of the photoresist portion 21 are further etched to expose a portion of the passivation layer 12. Since the oxygen content introduced during the second ashing process is significantly lower than that introduced during the first ashing process, the exposed passivation layer 12 is not oxidized. Sulfur hexafluoride gas acts as the material for the undercut structure 120. Its etching rate on the main body portion 122 is much higher than its etching rate on the micro-oxidized portion 123. The mixed gas etches the exposed passivation layer 12 (i.e., the main body portion 122) to form the undercut structure 120, while the micro-oxidized portion 123 is not etched or is only etched in a very small portion, which can be ignored. Furthermore, and more importantly, the trailing part of the photoresist 21 is further etched away, which increases the distance between the edge of the photoresist 21 and the micro-oxidation part 123, thereby avoiding the influence of burrs or foreign matter residues formed at both ends of the photoresist 21 when it is peeled off on the subsequently formed pixel electrode 13.
[0088] In this embodiment of the invention, the dimensions of the undercut structure 120 can be controlled by controlling the ratio of oxygen to sulfur hexafluoride in the mixed gas and the time of the ashing treatment. Specifically, the ratio of oxygen to sulfur hexafluoride in the second ashing gas ranges from 5:1 to 10:1. For example, the ratio of oxygen to sulfur hexafluoride in the second ashing gas can be one of 5:1, 6:1, 7:1, 8:1, 9:1, and 10:1.
[0089] Furthermore, during the second ashing process, such as Figure 6H As shown, the metal sacrificial layer 1141 is deoxidized to improve the contact performance between the pixel electrode 13 and the drain electrode 114, and to avoid increased resistance that would affect the electrical connection effect.
[0090] S405: A pixel electrode 13 is formed on the photoresist layer 20, the passivation layer 12 and the driving circuit layer 11. The pixel electrode 13 is disconnected at the undercut structure 120 to form the display electrode 131 and the slit 132.
[0091] For details, please refer to Figure 6IThe pixel electrode 13 can be fabricated by deposition, sputtering, or coating processes. Because the velvety material formed above the photoresist portion 21 has undulating surface features, the pixel electrode 13 breaks at the velvety material, forming a fracture pattern on the photoresist portion 21. Furthermore, the pixel electrode 13 breaks at the undercut structure 120, isolating the pixel electrode 13 located above the micro-oxidation portion 123 from the pixel electrode 13 located on the photoresist portion 21, and the slit 132 has a distinct boundary.
[0092] Understandably, in order to disconnect the pixel electrode 13 at the undercut structure 120, the surface of the passivation layer 12 away from the substrate 10 protrudes from the sidewall of the undercut structure 120, and the angle between the sidewall of the undercut structure 120 and the surface of the passivation layer 12 away from the substrate 10 is an acute angle, thereby making the cross-sectional shape of the undercut structure 120 a regular trapezoid. Optionally, the angle between the sidewall of the undercut structure 120 and the surface of the passivation layer 12 away from the substrate 10 is less than 60 degrees. Specifically, in the thickness direction of the substrate 10, from the side of the passivation layer 12 away from the substrate 10 to the side of the passivation layer 12 close to the substrate 10, the width of the undercut structure 120 gradually increases. In addition, the depth of the undercut structure 120 should be controlled within a suitable range. If the depth is too large, it will penetrate the passivation layer 12, and if the depth is too small, the undercut structure 120 will not have a sufficient slope, causing the pixel electrode 13 to break at the sidewall of the undercut structure 120.
[0093] S406: Peel off the photoresist layer 20.
[0094] For details, please refer to Figure 6J A stripping solution is provided, which can enter through the undercut structure 120, allowing the pixel electrode 13 on the photoresist portion 21 to contact the stripping solution, thereby removing the photoresist portion 21 and forming the desired pixel electrode 13 pattern on the passivation layer 12. Compared to the prior art, this increases the immersion path of the stripping solution at the edge of the photoresist portion 21, increasing the contact area between the stripping solution and the photoresist portion 21, which is beneficial for improving stripping efficiency and avoiding incomplete photoresist stripping. Furthermore, as mentioned above, because the distance between the edge of the photoresist portion 21 and the micro-oxidation portion 123 is increased, the distance between the edge of the photoresist portion 21 and the display electrode 131 on the micro-oxidation portion 123 is also increased. Burrs falling from the photoresist portion 21 will not cause bottom shells or fuzzy foreign matter residues at the edge of the display electrode 131, which is beneficial for improving the display effect.
[0095] It is understood that the fabrication method of the array substrate 100 provided in the embodiments of the present invention uses the same photolithography process for the first metal layer and the common electrode 115, the same photolithography process for the second metal layer and the semiconductor layer 112, and the same photolithography process for the pixel electrode 13 and the passivation layer 12, which is beneficial to reduce the number of processes and reduce production costs.
[0096] Please see Figure 7 This invention also provides a display panel, which includes an array substrate 100 and a counter substrate 200. The counter substrate 200 is disposed opposite to the array substrate 100. A liquid crystal layer 300 is disposed between the array substrate 100 and the counter substrate 200 and includes a plurality of liquid crystal molecules 301. The counter substrate 200 may be a color filter substrate, which includes a color resist layer (not shown) and a black matrix layer (not shown). A driving voltage exists between the array substrate 100 and the color filter substrate to drive the liquid crystal molecules 301 to deflect, thereby realizing display.
[0097] Beneficial effects: In the array substrate and its preparation method and display panel provided in the embodiments of the present invention, by providing multiple undercut structures on the surface of the passivation layer away from the substrate, the pixel electrode is broken in the undercut structure to form multiple spaced display electrodes and slits located between two adjacent display electrodes, so that the pixel electrode has a clear slit boundary. When the photoresist layer with velvety material and the pixel electrode located on the photoresist layer are peeled off to form the display electrode and slit, the stripping liquid can easily contact the photoresist layer through the undercut structure, which increases the immersion path of the stripping liquid at the edge of the photoresist part, which is beneficial to improve the stripping effect and efficiency of the photoresist layer, and avoids the formation of burrs at both ends of the photoresist layer when it is peeled off, which would cause the bottom shell or velvety foreign matter residue to appear at the edge of the pixel electrode, thus improving the display effect.
[0098] In the above embodiments, the descriptions of each embodiment have different focuses. For parts not described in detail in a certain embodiment, please refer to the relevant descriptions in other embodiments.
[0099] The above provides a detailed description of an array substrate, its preparation method, and a display panel provided by the embodiments of the present invention. Specific examples have been used to illustrate the principles and implementation methods of the present invention. The descriptions of the above embodiments are only for the purpose of helping to understand the technical solutions and core ideas of the present invention. Those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for manufacturing an array substrate, characterized by, Includes the following steps: Provide a substrate; A driving circuit layer is formed on one side of the substrate; A passivation layer is formed on the side of the driving circuit layer away from the substrate; as well as A pixel electrode is formed on the side of the passivation layer away from the substrate. The pixel electrode includes a plurality of display electrodes spaced apart, and a slit is provided between two adjacent display electrodes. The step of forming a pixel electrode on the side of the passivation layer away from the substrate includes: A photoresist layer is formed on the entire side of the passivation layer away from the substrate; A photomask is provided to pattern the photoresist layer so that the thickness of the photoresist layer corresponding to the display electrode to be formed is greater than the thickness of the photoresist layer corresponding to the slit to be formed, and the portion of the photoresist layer corresponding to the via to be formed is removed to expose the passivation layer. Oxygen is introduced to perform a first ashing treatment on the photoresist layer, so that the portion of the photoresist layer corresponding to the display electrode to be formed is thinned to form a photoresist portion, the portion of the photoresist layer corresponding to the slit to be formed is removed to expose the passivation layer, and the passivation layer not covered by the photoresist layer is etched away to form the via, wherein a velvety texture is formed on the photoresist portion, and the surface of the passivation layer located between two adjacent photoresist portions on the side away from the substrate is micro-oxidized; A mixture of oxygen and sulfur hexafluoride is introduced to perform a second ashing treatment on the photoresist layer, so that the edge of the photoresist portion is etched away to expose the passivation layer, and the exposed passivation layer is etched to form multiple undercut structures. A pixel electrode is formed on the photoresist layer, the passivation layer, and the driving circuit layer; the pixel electrode is disconnected at the undercut structure to form the display electrode and the slit; and The photoresist layer is peeled off.
2. The method of manufacturing an array substrate according to claim 1, wherein During the first ashing process, the surface of the drain of the drive circuit layer exposed by the via on the side away from the substrate is micro-oxidized to form a metal sacrificial layer. as well as During the second ashing process, the metal sacrificial layer is deoxidized.
3. The method of manufacturing an array substrate according to claim 1, wherein The ratio of oxygen to sulfur hexafluoride in the second ashing process is in the range of 5:1 to 10:
1.
4. An array substrate, characterized by, The array substrate is prepared by the method for preparing an array substrate as described in any one of claims 1-3, and the array substrate comprises: Substrate; A driving circuit layer is disposed on one side of the substrate; A passivation layer is disposed on the side of the driving circuit layer away from the substrate; and A pixel electrode is disposed on the side of the passivation layer away from the substrate and electrically connected to the driving circuit layer through a via penetrating the passivation layer. The pixel electrode includes a plurality of spaced display electrodes and a slit located between two adjacent display electrodes. The passivation layer near the display electrode of the slit is recessed from the surface away from the substrate to the side closer to the substrate to form an undercut structure.
5. The array substrate of claim 4, wherein, The passivation layer includes a main body portion and a micro-oxidation portion located on the side of the main body portion away from the substrate, wherein one side surface of the main body portion is recessed toward the side closer to the substrate to form the undercut structure.
6. The array substrate of claim 5, wherein, The material of the micro-oxidation part includes silicon oxide, and the material of the main body part includes silicon nitride.
7. The array substrate according to claim 5, characterized in that, The orthographic projection of each slit on the substrate overlaps the orthographic projection of the corresponding undercut structure on the substrate.
8. The array substrate according to claim 7, characterized in that, In the thickness direction of the substrate, from the side of the passivation layer away from the substrate to the side of the passivation layer closer to the substrate, the width dimension of the undercut structure gradually increases.
9. The array substrate according to claim 1, characterized in that, The pixel electrode also includes a connection electrode that is separately disposed from the display electrode, and the connection electrode is electrically connected to the driving circuit layer through a via penetrating the passivation layer.
10. A display panel, characterized in that, Includes the array substrate as described in any one of claims 4-9; The opposing substrate is disposed opposite to the array substrate; as well as A liquid crystal layer, disposed between the array substrate and the opposing substrate, comprises a plurality of liquid crystal molecules.
Citation Information
Patent Citations
Drawing Pixel structure and display panel
CN105446044A
Liquid crystal display and method of fabricating the same
US20100091228A1