A method and system for analyzing stray current corrosion of substation grounding grid

By calculating the grounding down conductor offset and current sequence analysis, the problem of selecting stray current corrosion detection points in the substation grounding grid is solved, efficient and accurate corrosion ratings are achieved, and resource waste and calculation errors are reduced.

CN118376883BActive Publication Date: 2024-10-18STATE GRID JIANGXI ELECTRIC POWER CO LTD RES INST +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410804946.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-21
Publication Date
2024-10-18
Estimated Expiration
2044-06-21

AI Technical Summary

Technical Problem

In the existing technology, the selection of stray current corrosion detection points in the substation grounding grid is vague and there is a lack of simple and effective methods, which results in difficulty in detection and waste of resources. Moreover, the corrosion situation in the corners of the grounding grid is difficult to accurately reflect the overall corrosion risk.

Method used

Determine the corrosion detection point by calculating the offset of the grounding down conductor, and use the corrosion probe to obtain the current sequence, divide the target current sub-sequence, calculate the average corrosion current and scattering density, combined with the data filtering and weight assignment of the current recorder, Accurately assess the corrosion risk of grounding grids.

Benefits of technology

It achieves simple and efficient detection point selection, reduces resource waste, accurately reflects the corrosion risk of the grounding grid, improves the accuracy of corrosion ratings, and avoids inaccurate calculations caused by current recorder failures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118376883B_ABST
    Figure CN118376883B_ABST
Patent Text Reader

Abstract

The present invention discloses a stray current corrosion analysis method and system for a transformer substation grounding grid, the method comprising: defining a certain detection grounding down conductor with the largest offset as a corrosion detection grounding down conductor; obtaining at least one current value of a corrosion probe at the corrosion detection grounding down conductor according to a preset detection frequency, and obtaining a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period; dividing the target current sequence into at least one target current subsequence based on a preset division rule, and calculating a target average corrosion current of the target current sequence according to the time length of at least one target current subsequence and the average corrosion current of at least one target current subsequence; and calculating an average stray current density according to the target average corrosion current and the surface area of ​​the corrosion probe. The detection point is determined by using the ground potential of the grounding down conductor, and the waste of resources caused by large-scale excavation is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of power engineering grounding grids, and in particular relates to a stray current corrosion analysis method and system for a substation grounding grid. Background Art

[0002] After the stray current invades the substation through cables, overhead ground wires, conductors, etc., it will propagate current to the earth through the grounding grid. When the current value is positive, it means that the grounding grid is dispersing current to the soil, and when the current value is negative, it means that the soil is converging to the grounding grid. When the grounding grid is dispersing current to the soil, the grounding metal material will lose electrons, resulting in stray current corrosion of the grounding grid.

[0003] The mechanism of stray current corrosion on grounding grid is relatively clear. The stray current corrosion rate of substation grounding grid is linearly related to the stray current density. Using Faraday's law, the corrosion rate can be accurately calculated according to the stray current density. Therefore, the stray current corrosion rating of substation grounding grid can be rated by measuring the average stray current density.

[0004] In the current regulations, the selection of detection points for the stray current density of the substation grounding grid is vague and lacks a simple and effective method. In fact, after the stray current is injected into the grounding grid, it is not evenly dispersed, but concentrated in the corners of the grounding grid. The middle of the grounding grid basically does not participate in the dispersion. Figure 1 Therefore, the closer to the corner of the grounding grid, the more serious the stray current corrosion will be.

[0005] However, it is difficult and meaningless to directly detect the scattered current in the corners of the grounding grid. On the one hand, the corners and edges of the grounding grid are difficult to locate at the substation site, and often require a lot of excavation to find, which is time-consuming and labor-intensive. On the other hand, the corners of the grounding grid are generally not connected to the equipment through the down conductor, so even if corrosion occurs, it will not have much impact on the overall function of the grounding grid. Summary of the invention

[0006] The present invention provides a stray current corrosion analysis method, system and readable storage medium for a transformer substation grounding grid, which are used to solve the technical problem that effective detection points cannot be selected simply and conveniently.

[0007] In a first aspect, the present invention provides a method for analyzing stray current corrosion of a substation grounding grid, comprising:

[0008] Acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential;

[0009] Calculate the offset between the second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor;

[0010] At least one current value of the corrosion probe at the corrosion detection grounding down conductor is obtained according to a preset detection frequency, and a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period is obtained, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe is dispersing current to the soil, and when the current value is negative, it indicates that the soil is converging current to the corrosion probe;

[0011] Dividing the target current sequence into at least one target current subsequence based on a preset division rule, and calculating a target average corrosion current of the target current sequence according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence;

[0012] The average scattered current density is calculated based on the target average corrosion current and the surface area of ​​the corrosion probe.

[0013] In a second aspect, the present invention provides a stray current corrosion analysis system for a substation grounding grid, comprising:

[0014] A first acquisition module is configured to acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential;

[0015] A first calculation module is configured to calculate an offset between a second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor;

[0016] The second acquisition module is configured to acquire at least one current value of the corrosion probe at the corrosion detection grounding down conductor according to a preset detection frequency, and obtain a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe disperses the current to the soil, and when the current value is negative, it indicates that the soil converges the current to the corrosion probe;

[0017] a division module, configured to divide the target current sequence into at least one target current subsequence based on a preset division rule, and calculate a target average corrosion current of the target current sequence according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence;

[0018] The second calculation module is configured to calculate the average scattered current density according to the target average corrosion current and the surface area of ​​the corrosion probe.

[0019] According to a third aspect, an electronic device is provided, comprising: at least one processor, and a memory communicatively connected to the at least one processor, wherein the memory stores instructions executable by the at least one processor, and the instructions are executed by the at least one processor so that the at least one processor can perform the steps of the stray current corrosion analysis method for the substation grounding grid of any embodiment of the present invention.

[0020] In a fourth aspect, the present invention further provides a computer-readable storage medium having a computer program stored thereon, wherein when the program instructions are executed by a processor, the processor executes the steps of the stray current corrosion analysis method for a substation grounding grid according to any embodiment of the present invention.

[0021] The stray current corrosion analysis method and system of the substation grounding grid of the present application calculates the offset between the second ground potential and the first ground potential of at least one grounding down conductor, and defines a certain detection grounding down conductor with the largest offset as a corrosion detection grounding down conductor, thereby realizing the use of the ground potential of the grounding down conductor to determine the detection point, avoiding the waste of resources caused by large-scale excavation, and better reflecting the corrosion risk of weak and dangerous points of stray current corrosion in the grounding grid. If the number of target current subsequences with a time length less than the first preset threshold is not greater than the second preset threshold, the target current subsequence with a time length less than the first preset threshold is defined as an abnormal target The current subsequences are removed and the current values ​​obtained by the current recorder with sudden changes in positive and negative values ​​can be screened out, thereby reducing the occurrence of inaccurate calculation of the target average corrosion current due to faults in the current recorder itself. If the number of target current subsequences with time lengths less than the first preset threshold is greater than the second preset threshold, the weight of a target current subsequence is determined according to the ratio of the time length of a target current subsequence to the total time lengths of other target current subsequences. In this way, the weight influence of the target current subsequences with short time lengths can be reduced as much as possible, which may facilitate the accuracy of the calculation of the target average corrosion current. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0023] Figure 1 It is the distribution diagram of stray current of grounding grid;

[0024] Figure 2 A flowchart of a method for analyzing stray current corrosion of a substation grounding grid provided by an embodiment of the present invention;

[0025] Figure 3 A current waveform diagram of a stray current detection corrosion probe of a substation grounding grid is provided for one embodiment of the present invention;

[0026] Figure 4 A structural block diagram of a stray current corrosion analysis system for a substation grounding grid provided by an embodiment of the present invention;

[0027] Figure 5 It is a schematic diagram of the structure of an electronic device provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] A substation is responsible for supplying power to the subway system. During operation, it was found that the stray current generated by the subway invaded the substation through the cable sheath. The stray current is a very low frequency current, with both positive and negative currents, and disappears when the subway stops operating at night. Therefore, a stray current corrosion analysis method for the substation grounding grid is proposed to analyze the stray current corrosion of the substation grounding grid.

[0030] See also Figure 2 , which shows a flow chart of a stray current corrosion analysis method for a substation grounding grid of the present application.

[0031] like Figure 2 As shown, the stray current corrosion analysis method of the substation grounding grid specifically includes the following steps:

[0032] Step S101, obtaining a first ground potential of a reference grounding down conductor, wherein the first ground potential is equal to a natural potential.

[0033] In this step, determine the reference grounding down conductor: the neutral point grounding down conductor of the transformer in the substation is located at the center of the grounding grid, and its potential to the ground is constant. Combined with the stray current waveform, it can be considered that there is no stray current in the grounding grid at this location. The potential of this down conductor to the ground is equal to the natural potential and can be used as a reference grounding down conductor. Its potential to the ground is used as a reference potential for determining the corrosion monitoring grounding down conductor step.

[0034] Step S102, calculate the offset between the second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor.

[0035] In this step, the corrosion detection grounding down conductor is determined: a lightning arrester grounding down conductor is located at the corner of the substation wall, close to the corner of the grounding grid. Its peak deviation from the reference potential to the ground can reach 100mV, which is higher than other grounding down conductors. It is determined to be the corrosion detection grounding down conductor.

[0036] Bury the corrosion probe: dig a small pit about 30cm long, 30cm wide and 80cm deep next to the corrosion detection grounding lead, and bury the corrosion probe in the soil. The corrosion probe is made of Q235 carbon steel, the same material as the grounding grid, with a surface area of ​​6cm 2 The burial depth is consistent with the grounding grid (80cm), and the corrosion probe and the corrosion detection grounding lead are connected by a wire through a current recorder.

[0037] Step S103, obtaining at least one current value of the corrosion probe at the corrosion detection grounding down conductor according to a preset detection frequency, and obtaining a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period, wherein the current value includes the absolute value of the current value and the positive and negative sign of the current value. When the current value is positive, it indicates that the corrosion probe is dissipating current to the soil, and when the current value is negative, it indicates that the soil is converging to the corrosion probe.

[0038] In this step, the corrosion probe current data is obtained: the current recorder is used to detect the current flowing through the corrosion probe in real time, the detection frequency is 1Hz, and the positive value is the current flowing from the corrosion probe to the soil, and the negative value is the current flowing from the soil to the corrosion probe. The corrosion probe current detection time for the stray current corrosion evaluation of the grounding grid should be an integer multiple of 24 hours. This test obtained 72 hours of current data, such as Figure 3 shown.

[0039] Step S104, dividing the target current sequence into at least one target current subsequence based on a preset division rule, and calculating the target average corrosion current of the target current sequence according to the time length of the at least one target current subsequence and the average corrosion current of the at least one target current subsequence.

[0040] In this step, at least one current value with a negative current value in the target current sequence is taken as a critical node, and at least one target current sub-sequence is intercepted in the target current sequence according to each critical node, wherein at least one target current sub-sequence only contains current values ​​with positive current values, and the first node in any target current sub-sequence is a current value with a positive current value adjacent to a certain critical node, and the last node in a certain target current sub-sequence is another current value with a positive current value adjacent to another critical node, and a certain critical node and another critical node are two adjacent critical nodes.

[0041] It should be noted that the time length of each target current subsequence is obtained, and it is determined whether the number of target current subsequences whose time length is less than the first preset threshold is greater than the second preset threshold; if the number of target current subsequences whose time length is less than the first preset threshold is greater than the second preset threshold, the average corrosion current of at least one target current subsequence is calculated; the weight of a certain target current subsequence is determined according to the ratio of the time length of a certain target current subsequence to the sum of the time lengths of other target current subsequences, wherein the other target current subsequences are the target current subsequences excluding a certain target current subsequence from at least one target current subsequence; the target average corrosion current of the target current sequence is calculated according to the average corrosion current of at least one target current subsequence and the average corrosion current of at least one corresponding target current subsequence.

[0042] In a specific embodiment, after obtaining the time length of each target current subsequence and determining whether the number of target current subsequences whose time length is less than a first preset threshold is greater than a second preset threshold, if the number of target current subsequences whose time length is less than the first preset threshold is not greater than the second preset threshold, the target current subsequence whose time length is less than the first preset threshold is defined as an abnormal target current subsequence and removed; the average corrosion current of at least one target current subsequence excluding the abnormal target current subsequence is calculated; the weight of a target current subsequence is determined based on the ratio of the time length of a target current subsequence to the sum of the time lengths of other target current subsequences, wherein the other target current subsequences are target current subsequences excluding a target current subsequence from at least one target current subsequence; and the target average corrosion current of the target current sequence is calculated based on the average corrosion current of at least one target current subsequence and the average corrosion current of at least one corresponding target current subsequence.

[0043] In this specific embodiment, since the current recorder may have a temporary fault, the current value obtained in a continuous period of acquisition time changes from negative or zero to positive, and then from positive to negative or zero. For example, in three consecutive moments, the current values ​​at the first moment and the previous moments are all negative, the current value at the second moment is positive, and the current values ​​at the third moment and the subsequent moments are all negative. At this time, the positive current value at the second moment may be caused by a temporary fault in the current recorder. If this situation only exists during the entire acquisition time period, the positive current value at the second moment will be regarded as an abnormal situation and removed. In this way, the accuracy of calculating the target average corrosion current can be improved.

[0044] Step S105, calculating the average scattered current density according to the target average corrosion current and the surface area of ​​the corrosion probe.

[0045] In this step, after the average scattered current density is calculated, the corresponding level is found in the preset substation grounding grid stray current corrosion risk table according to the average scattered current density, and recorded as the stray current corrosion analysis result of the substation grounding grid. Among them, the average scattered current density in the substation grounding grid stray current corrosion risk table is less than 0.01A / m 2 The corresponding level is the fourth level, and the average scattered current density is not less than 0.01A / m 2 And less than 0.05A / m 2 The corresponding level is the third level, and the average scattered current density is not less than 0.05A / m 2 And not more than 0.075A / m 2 The corresponding level is the second level and the average scattered current density is greater than 0.075A / m 2 The corresponding level is the first level, and the priorities of the first level, the second level, the third level, and the fourth level decrease in sequence.

[0046] Specifically, the stray current corrosion risk table of the substation grounding grid is:

[0047] ,

[0048] In summary, the method of the present application calculates the offset between the second ground potential and the first ground potential of at least one grounding down conductor, and defines a certain detection grounding down conductor with the largest offset as a corrosion detection grounding down conductor, so as to realize the use of the grounding down conductor ground potential to determine the detection point, avoid the waste of resources caused by large-scale excavation, and better reflect the corrosion risk of weak and dangerous points of stray current corrosion of the grounding grid. If the number of target current subsequences with a time length less than the first preset threshold is not greater than the second preset threshold, the target current subsequence with a time length less than the first preset threshold is defined as an abnormal target current subsequence and removed, and the current value obtained by the current recorder with a sudden change in positive and negative values ​​can be screened out, so as to minimize the occurrence of inaccurate calculation of the target average corrosion current caused by the failure of the current recorder itself. If the number of target current subsequences with a time length less than the first preset threshold is greater than the second preset threshold, the weight of a target current subsequence is determined according to the ratio of the time length of a target current subsequence to the sum of the time lengths of other target current subsequences. In this way, the weight influence of the target current subsequence with a short time length can be minimized, which may facilitate the accuracy of the target average corrosion current calculation.

[0049] See also Figure 4 , which shows a structural block diagram of a stray current corrosion analysis system for a substation grounding grid of the present application.

[0050] like Figure 4 As shown, the stray current corrosion analysis system 200 includes a first acquisition module 210 , a first calculation module 220 , a second acquisition module 230 , a division module 240 and a second calculation module 250 .

[0051] Among them, the first acquisition module 210 is configured to obtain the first ground potential of the reference grounding down conductor, and the first ground potential is equal to the natural potential; the first calculation module 220 is configured to calculate the offset between the second ground potential of at least one grounding down conductor and the first ground potential, and define a detection grounding down conductor with the largest offset as a corrosion detection grounding down conductor, wherein the grounding down conductor is any grounding down conductor except the reference grounding down conductor; the second acquisition module 230 is configured to obtain at least one current value of the corrosion probe at the corrosion detection grounding down conductor according to a preset detection frequency, and obtain the current value of the corrosion probe at the corrosion detection grounding down conductor within a preset time period. A target current sequence, wherein the current value includes the absolute value of the current value and the positive or negative sign of the current value. When the current value is positive, it indicates that the corrosion probe is dispersing current to the soil, and when the current value is negative, it indicates that the soil is converging to the corrosion probe; a division module 240 is configured to divide the target current sequence into at least one target current subsequence based on a preset division rule, and calculate the target average corrosion current of the target current sequence according to the time length of the at least one target current subsequence and the average corrosion current of the at least one target current subsequence; a second calculation module 250 is configured to calculate the average scattered current density according to the target average corrosion current and the surface area of ​​the corrosion probe.

[0052] It should be understood that Figure 4 Modules and references documented in Figure 1 Therefore, the operations and features described above for the method and the corresponding technical effects are also applicable to Figure 4 The modules in it will not be described in detail here.

[0053] In some other embodiments, the embodiments of the present invention further provide a computer-readable storage medium having a computer program stored thereon, wherein when the program instructions are executed by a processor, the processor is caused to execute the stray current corrosion analysis method for a substation grounding grid in any of the above method embodiments;

[0054] As an implementation mode, the computer-readable storage medium of the present invention stores computer-executable instructions, and the computer-executable instructions are configured as follows:

[0055] Acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential;

[0056] Calculate the offset between the second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor;

[0057] At least one current value of the corrosion probe at the corrosion detection grounding down conductor is obtained according to a preset detection frequency, and a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period is obtained, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe is dispersing current to the soil, and when the current value is negative, it indicates that the soil is converging current to the corrosion probe;

[0058] Dividing the target current sequence into at least one target current subsequence based on a preset division rule, and calculating a target average corrosion current of the target current sequence according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence;

[0059] The average scattered current density is calculated based on the target average corrosion current and the surface area of ​​the corrosion probe.

[0060] The computer-readable storage medium may include a program storage area and a data storage area, wherein the program storage area may store an operating system and application programs required for at least one function; the data storage area may store data created according to the use of the stray current corrosion analysis system of the substation grounding grid, etc. In addition, the computer-readable storage medium may include a high-speed random access memory, and may also include a memory, such as at least one disk storage device, a flash memory device, or other non-volatile solid-state storage device. In some embodiments, the computer-readable storage medium may optionally include a memory remotely arranged relative to the processor, and these remote memories may be connected to the stray current corrosion analysis system of the substation grounding grid via a network. Examples of the above-mentioned network include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof.

[0061] Figure 5 is a schematic diagram of the structure of an electronic device provided by an embodiment of the present invention, such as Figure 5 As shown, the device includes: a processor 310 and a memory 320. The electronic device may also include: an input device 330 and an output device 340. The processor 310, the memory 320, the input device 330 and the output device 340 may be connected via a bus or other means. Figure 5 In the example, the bus connection is used. The memory 320 is the above-mentioned computer-readable storage medium. The processor 310 executes various functional applications and data processing of the server by running the non-volatile software programs, instructions and modules stored in the memory 320, that is, the stray current corrosion analysis method of the substation grounding grid in the above-mentioned method embodiment is realized. The input device 330 can receive input digital or character information, and generate key signal input related to user settings and function control of the stray current corrosion analysis system of the substation grounding grid. The output device 340 may include display devices such as display screens.

[0062] The electronic device can execute the method provided by the embodiment of the present invention, and has the functional modules and beneficial effects corresponding to the execution method. For technical details not described in detail in this embodiment, please refer to the method provided by the embodiment of the present invention.

[0063] As an implementation mode, the electronic device is applied to a stray current corrosion analysis system of a substation grounding grid, and is used for a client, and includes: at least one processor; and a memory connected to the at least one processor in communication; wherein the memory stores instructions executable by the at least one processor, and the instructions are executed by the at least one processor so that the at least one processor can:

[0064] Acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential;

[0065] Calculate the offset between the second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor;

[0066] At least one current value of the corrosion probe at the corrosion detection grounding down conductor is obtained according to a preset detection frequency, and a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period is obtained, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe is dispersing current to the soil, and when the current value is negative, it indicates that the soil is converging current to the corrosion probe;

[0067] Dividing the target current sequence into at least one target current subsequence based on a preset division rule, and calculating a target average corrosion current of the target current sequence according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence;

[0068] The average scattered current density is calculated based on the target average corrosion current and the surface area of ​​the corrosion probe.

[0069] Through the description of the above implementation modes, those skilled in the art can clearly understand that each implementation mode can be implemented by means of software plus a necessary general hardware platform, or of course by hardware. Based on such an understanding, the above technical solution can essentially or in other words be embodied in the form of a software product that contributes to the prior art. The computer software product can be stored in a computer-readable storage medium, such as ROM / RAM, a magnetic disk, an optical disk, etc., and includes a number of instructions for a computer device (which can be a personal computer, a server, or a network device, etc.) to execute the methods of each embodiment or some parts of the embodiment.

[0070] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for analyzing stray current corrosion of a substation grounding grid, characterized in that: include: Acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential; Calculate the offset between the second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor; At least one current value of the corrosion probe at the corrosion detection grounding down conductor is obtained according to a preset detection frequency, and a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period is obtained, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe is dispersing current to the soil, and when the current value is negative, it indicates that the soil is converging current to the corrosion probe; The target current sequence is divided into at least one target current subsequence based on a preset division rule, and a target average corrosion current of the target current sequence is calculated according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence, wherein the target current sequence is divided into at least one target current subsequence based on a preset division rule, comprising: At least one current value with a negative current value in the target current sequence is used as a critical node, and at least one target current subsequence is intercepted in the target current sequence according to each critical node, wherein the at least one target current subsequence only includes current values ​​with positive current values, and the first node in any target current subsequence is a current value with a positive current value adjacent to a certain critical node, and the last node in a certain target current subsequence is another current value with a positive current value adjacent to another critical node, and the certain critical node and the other critical node are two adjacent critical nodes; Calculating the target average corrosion current of the target current sequence according to the time length of the at least one target current subsequence and the average corrosion current of the at least one target current subsequence comprises: Obtaining the time length of each target current subsequence, and determining whether the number of target current subsequences whose time length is less than a first preset threshold is greater than a second preset threshold; If the number of target current subsequences whose time length is less than the first preset threshold is greater than the second preset threshold, the average corrosion current of the at least one target current subsequence is calculated; Determine the weight of a certain target current subsequence according to the ratio of the time length of a certain target current subsequence to the sum of the time lengths of other target current subsequences, wherein the other target current subsequences are target current subsequences excluding the certain target current subsequence from the at least one target current subsequence; Calculating a target average corrosion current of the target current sequence according to an average corrosion current of the at least one target current subsequence and a corresponding weight of the at least one target current subsequence; After obtaining the time length of each target current subsequence and determining whether the number of target current subsequences whose time length is less than the first preset threshold is greater than the second preset threshold, the method further includes: If the number of target current subsequences whose time length is less than the first preset threshold is not greater than the second preset threshold, the target current subsequence whose time length is less than the first preset threshold is defined as an abnormal target current subsequence and removed; calculating an average corrosion current of at least one target current subsequence excluding an abnormal target current subsequence; Determine the weight of a certain target current subsequence according to the ratio of the time length of a certain target current subsequence to the sum of the time lengths of other target current subsequences, wherein the other target current subsequences are target current subsequences excluding the certain target current subsequence from the at least one target current subsequence; Calculating a target average corrosion current of the target current sequence according to an average corrosion current of the at least one target current subsequence and a corresponding weight of the at least one target current subsequence; The average scattered current density is calculated based on the target average corrosion current and the surface area of ​​the corrosion probe.

2. A method for analyzing stray current corrosion of a substation grounding grid according to claim 1, characterized in that: The reference grounding down conductor is a transformer neutral point grounding down conductor of a substation located at the center of the grounding grid.

3. The method for analyzing stray current corrosion of a substation grounding grid according to claim 1, characterized in that: The at least one grounding down conductor comprises a lightning arrester grounding down conductor located at a corner of a transformer substation wall.

4. The method for analyzing stray current corrosion of a substation grounding grid according to claim 1, characterized in that: After calculating the average scattered current density according to the target average corrosion current and the surface area of ​​the corrosion probe, the method further includes: According to the average scattered current density, the corresponding level is searched in the preset stray current corrosion risk table of the substation grounding grid, and recorded as the stray current corrosion analysis result of the substation grounding grid, wherein the average scattered current density in the stray current corrosion risk table of the substation grounding grid is less than 0.01A / m 2 The corresponding level is the fourth level, and the average scattered current density is not less than 0.01A / m 2 And less than 0.05A / m 2 The corresponding level is the third level, and the average scattered current density is not less than 0.05A / m 2 And not more than 0.075A / m 2 The corresponding level is the second level and the average scattered current density is greater than 0.075A / m 2 The corresponding level is the first level, and the priorities of the first level, the second level, the third level, and the fourth level decrease in sequence.

5. A stray current corrosion analysis system of a stray current corrosion analysis method for a substation grounding grid according to any one of claims 1 to 4, characterized in that: include: A first acquisition module is configured to acquire a first ground potential of the reference grounding down conductor, wherein the first ground potential is equal to the natural potential; A first calculation module is configured to calculate an offset between a second ground potential of at least one ground down conductor and the first ground potential, and define a detection ground down conductor with the largest offset as a corrosion detection ground down conductor, wherein the ground down conductor is any ground down conductor except the reference ground down conductor; The second acquisition module is configured to acquire at least one current value of the corrosion probe at the corrosion detection grounding down conductor according to a preset detection frequency, and obtain a target current sequence of the corrosion probe at the corrosion detection grounding down conductor within a preset time period, wherein the current value includes the absolute value of the current value and the positive and negative of the current value. When the current value is positive, it indicates that the corrosion probe disperses the current to the soil, and when the current value is negative, it indicates that the soil converges the current to the corrosion probe; a division module, configured to divide the target current sequence into at least one target current subsequence based on a preset division rule, and calculate a target average corrosion current of the target current sequence according to a time length of the at least one target current subsequence and an average corrosion current of the at least one target current subsequence; The second calculation module is configured to calculate the average scattered current density according to the target average corrosion current and the surface area of ​​the corrosion probe.

6. An electronic device, characterized in that: include: At least one processor, and a memory communicatively connected to the at least one processor, wherein the memory stores instructions executable by the at least one processor, and the instructions are executed by the at least one processor to enable the at least one processor to perform the method described in any one of claims 1 to 4.

7. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the program is executed by a processor, the method according to any one of claims 1 to 4 is implemented.

Citation Information

Patent Citations

  • Method and device for detecting corrosion of grounding grid of power transmission line

    CN118091321A

  • Current density integrated testing device for evaluating corrosion rate of pipe network

    CN217443132U