Solid-state battery and method for manufacturing solid-state battery

By sequentially stacking the first solid electrolyte layer, the positive electrode and the second solid electrolyte layer on the negative electrode in the solid battery, and bonding them in the area that does not face the positive electrode and the positive electrode tabs, the problem of short circuit in the all-solid battery is solved and achieved It effectively isolates the positive and negative ends to prevent short circuit and falling off.

CN118738570APending Publication Date: 2024-10-01HONDA MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410201078.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-02-23
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing all-solid-state batteries do not have a partition wall that separates the ends of the positive and negative electrodes, which may lead to short circuits.

Method used

In a solid battery, the first solid electrolyte layer, the positive electrode, and the second solid electrolyte layer are sequentially stacked on the negative electrode and bonded in a region that does not face the positive electrode and the positive electrode tabs to ensure that the first solid electrolyte layer and the second solid electrolyte layer are The solid electrolyte layer is located further outside, thus separating the ends of the positive and negative electrodes and preventing short circuits.

Benefits of technology

It effectively suppresses the occurrence of short circuit and prevents the positive electrode from shifting and falling off.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738570A_ABST
    Figure CN118738570A_ABST
Patent Text Reader

Abstract

This solid-state battery is provided with an electrode laminate in which a first solid electrolyte layer, a positive electrode, and a second solid electrolyte layer are laminated in this order on a negative electrode, and is characterized in that: a positive electrode tab extends from the positive electrode, one of the first solid electrolyte layer and the second solid electrolyte layer contains a porous base material; the other of the first solid electrolyte layer and the second solid electrolyte layer does not contain a porous base material, and when the electrode laminate is viewed in plan, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are present further outside than the outer peripheral end of the positive electrode, and the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are present further outside than the outer peripheral end of the positive electrode. The first solid electrolyte layer and the second solid electrolyte layer are joined in a region that does not face the positive electrode and the positive electrode tab.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a solid battery and a method for manufacturing the solid battery. Background Art

[0002] In recent years, research and development of secondary batteries that contribute to improving energy efficiency have been conducted in order to ensure that affordable, reliable, sustainable, and advanced energy is available to the majority of people.

[0003] Patent Document 1 describes an all-solid-state battery having a positive electrode sheet formed by forming a positive electrode active material layer on a positive electrode collector layer, a negative electrode sheet formed by forming a negative electrode active material layer on a negative electrode collector layer, and a bag-shaped solid electrolyte layer containing the positive electrode sheet. Here, the positive electrode sheet contained in the bag-shaped solid electrolyte layer is stacked with the negative electrode sheet in a manner that overlaps when viewed from above, so that the positive electrode active material layer and the negative electrode active material layer are arranged opposite to each other through the solid electrolyte layer.

[0004] [Prior Technical Literature]

[0005] (Patent Document)

[0006] Patent Document 1: Japanese Patent Application Publication No. 2020-181668 Summary of the invention

[0007] [Problems to be solved by the invention]

[0008] However, the all-solid-state battery described in Patent Document 1 does not have a partition wall that separates the ends of the positive electrode sheet and the negative electrode sheet that are arranged with a bag-shaped solid electrolyte layer interposed therebetween, and therefore there is a possibility of short circuit.

[0009] An object of the present invention is to provide a solid battery capable of suppressing the occurrence of a short circuit.

[0010] [Technical means to solve the problem]

[0011] (1) A solid battery, comprising an electrode stack having a first solid electrolyte layer, a positive electrode, and a second solid electrolyte layer stacked in sequence on a negative electrode, a positive electrode tab extending from the positive electrode, one of the first solid electrolyte layer and the second solid electrolyte layer comprising a porous substrate, and the other of the first solid electrolyte layer and the second solid electrolyte layer not comprising a porous substrate, when the electrode stack is viewed from above, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are located further outward than the outer peripheral end of the positive electrode, and the first solid electrolyte layer and the second solid electrolyte layer are joined in a region that is not opposite to the positive electrode and the positive electrode tab.

[0012] (2) A solid battery according to (1), wherein in the aforementioned positive electrode, a positive electrode mixed material layer is formed on both sides of the positive electrode collector, and in the aforementioned electrode stack, the aforementioned first solid electrolyte layer, the aforementioned positive electrode, the aforementioned second solid electrolyte layer and the second negative electrode are stacked in sequence on the aforementioned negative electrode.

[0013] (3) A solid battery according to (1) or (2), wherein an insulating frame is provided on the outer periphery of the positive electrode, and when the electrode stack is viewed from above, the outer periphery ends of the first solid electrolyte layer and the second solid electrolyte layer are located on the outside compared to the outer periphery ends of the insulating frame, and the first solid electrolyte layer and the second solid electrolyte layer are joined in a region not facing the insulating frame.

[0014] (4) The solid battery according to any one of (1) to (3), wherein the negative electrode has a lithium metal layer.

[0015] (5) A method for manufacturing a solid battery, which is a method for manufacturing a solid battery described in any one of (1) to (4), the method comprising the following steps: a step of stacking the first solid electrolyte layer, the positive electrode and the second solid electrolyte layer in sequence; and a step of joining the first solid electrolyte layer and the second solid electrolyte layer by applying pressure from the other side of the first solid electrolyte layer and the second solid electrolyte layer.

[0016] (6) A solid battery, comprising an electrode stack having a first solid electrolyte layer, a negative electrode, and a second solid electrolyte layer stacked in sequence on a positive electrode, a negative electrode tab extending from the negative electrode, one of the first solid electrolyte layer and the second solid electrolyte layer comprising a porous substrate, and the other of the first solid electrolyte layer and the second solid electrolyte layer not comprising a porous substrate, when the electrode stack is viewed from above, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are present on the outside compared to the outer peripheral end of the negative electrode, and the first solid electrolyte layer and the second solid electrolyte layer are joined in a region that is not opposite to the negative electrode and the negative electrode tab.

[0017] (Effects of the Invention)

[0018] According to the present invention, a solid battery capable of suppressing the occurrence of a short circuit can be provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a perspective view showing an example of a solid battery according to this embodiment.

[0020] Figure 2 yes Figure 1 A magnified top view of a solid-state battery.

[0021] Figure 3 yes Figure 1 An exploded perspective view of a solid battery.

[0022] Figure 4 yes Figure 2 Cross-sectional view in the AA direction.

[0023] Figure 5 yes Figure 2 Cross-sectional view along the BB direction.

[0024] Figure 6 It is a cross-sectional view showing a variation of the stacking structure of the electrode stack. DETAILED DESCRIPTION

[0025] Hereinafter, embodiments of the present invention will be described with reference to the drawings.

[0026] Figures 1 to 3 An example of a solid state battery according to this embodiment is shown in FIG.

[0027] In the solid battery 100, the electrode stack 110 is packaged with a laminate film 120 as a packaging material, and the electrode stack 110 is stacked with a first solid electrolyte layer 112, a positive electrode 113, a second solid electrolyte layer 114 and a substrate 115 in sequence on the negative electrode 111. At this time, in the solid battery 100, a negative electrode tab 111A extends from the negative electrode 111, and a positive electrode tab 113A extends from the positive electrode 113. In addition, the direction in which the negative electrode tab 111A extends is opposite to the direction in which the positive electrode tab 113A extends. Furthermore, the first solid electrolyte layer 112 does not contain a porous substrate, and the second solid electrolyte layer 114 contains a porous substrate. In addition, when the electrode stack 110 is viewed from above, the outer peripheral ends of the first solid electrolyte layer 112 and the second solid electrolyte layer 114 are located further outside than the outer peripheral end of the positive electrode 113, and the first solid electrolyte layer 112 and the second solid electrolyte layer 114 are joined in a region that is not opposite to the positive electrode 113 and the positive electrode tab 113A (see Figure 4 , Figure 5 ). Therefore, since the end of the negative electrode 111 and the end of the positive electrode 113 are separated by the first solid electrolyte layer 112, the occurrence of a short circuit is suppressed. In addition, the positional displacement between the positive electrode 113 and the first solid electrolyte layer 112 and the detachment of the positive electrode 113 are suppressed.

[0028] Furthermore, when the positive electrode tab 113A is a porous body, the first solid electrolyte layer 112 and the second solid electrolyte layer 114 can be joined even in a region facing the positive electrode tab 113A.

[0029] The solid electrolytes constituting first solid electrolyte layer 112 and second solid electrolyte layer 114 may be different, but are preferably the same in consideration of the bonding properties between first solid electrolyte layer 112 and second solid electrolyte layer 114 .

[0030] The first solid electrolyte layer 112 is formed by, for example, a transfer method or a coating method.

[0031] The porous substrate constituting the second solid electrolyte layer 114 is not particularly limited as long as it can be filled with a solid electrolyte, and examples thereof include nonwoven fabrics.

[0032] The method of joining the first solid electrolyte layer 112 and the second solid electrolyte layer 114 is not particularly limited, and for example, a method of laminating the first solid electrolyte layer 112, the positive electrode 113, the second solid electrolyte layer 114, and the substrate 115 in order on the negative electrode 111 and then applying pressure from the first solid electrolyte layer 112 side, that is, the negative electrode 111 side. At this time, the pressure may be applied while heating as necessary.

[0033] The first solid electrolyte layer 112 and the second solid electrolyte layer 114 may be joined before or during packaging of the electrode stack 110 with the laminate film 120 .

[0034] The material constituting the substrate 115 is not particularly limited as long as it is a material with high rigidity, and an example thereof is stainless steel.

[0035] Alternatively, the order of stacking the first solid electrolyte layer 112 and the second solid electrolyte layer 114 may be reversed, and pressure may be applied from the first solid electrolyte layer 112 side, that is, the substrate 115 side.

[0036] Alternatively, after stacking the first solid electrolyte layer 112, the positive electrode 113, and the second solid electrolyte layer 114 in sequence, the first solid electrolyte layer 112 may be pressed to pre-fabricate the first solid electrolyte layer-positive electrode-second solid electrolyte layer stack. In this case, the order of stacking the first solid electrolyte layer 112 and the second solid electrolyte layer 114 may be reversed for the electrode stack 110.

[0037] The negative electrode 111 has a negative electrode mixed material layer 411b formed on one side of the negative electrode collector 411a, and the positive electrode 113 has a positive electrode mixed material layer 413b formed on one side of the positive electrode collector 413a. In addition, the negative electrode tab 111A is connected to the negative electrode tab lead 130, and the positive electrode tab 113A is connected to the positive electrode tab lead 140. Furthermore, the negative electrode tab lead 130 is bonded to the laminate film 120 by the sealant 150, and the positive electrode tab lead 140 is bonded to the laminate film 120 by the sealant 160.

[0038] The laminate film 120 includes, for example, a resin layer on the surface of which a metal layer is formed. Examples of the resin include polyethylene, polyvinyl fluoride, and polyvinylidene chloride, and examples of the metal include aluminum.

[0039] An insulating frame may also be provided on the outer periphery of the positive electrode 113. Thus, short circuits are suppressed. In this case, when the electrode stack 110 is viewed from above, the outer peripheries of the first solid electrolyte layer 112 and the second solid electrolyte layer 114 are located further outward than the outer peripheries of the positive electrode 113 and the insulating frame, and the first solid electrolyte layer 112 and the second solid electrolyte layer 114 are joined in an area that is not opposite to the positive electrode 113, the positive electrode tab 113A, and the insulating frame.

[0040] The material constituting the insulating frame is not particularly limited as long as it has electronic insulation properties, and examples thereof include insulating oxides such as alumina, resins such as polyvinylidene fluoride (PVDF), and rubbers such as styrene-butadiene rubber (SBR).

[0041] Furthermore, the insulating frame may also have ion conductivity.

[0042] Figure 6 2 shows a variation of the stacking structure of the electrode stack.

[0043] Electrode stack 610 is the same as electrode stack 110 except that positive electrode 613 is used instead of positive electrode 113 and negative electrode 111 is further disposed between second solid electrolyte layer 114 and substrate 115. Here, positive electrode 613 has positive electrode mixture layers formed on both sides of a positive electrode current collector.

[0044] Furthermore, the negative electrodes 111 disposed on both sides of the positive electrode 613 may be the same or different. Furthermore, the positive electrode mixture layers formed on both sides of the positive electrode current collector may be the same or different.

[0045] The solid battery of the present embodiment is not particularly limited, and examples thereof include all-solid lithium ion batteries and all-solid lithium metal batteries.

[0046] Furthermore, the solid battery of the present embodiment may include a plurality of electrode stacks.

[0047] Hereinafter, the case where the solid battery of the present embodiment is an all-solid-state lithium metal battery will be described.

[0048] The positive electrode current collector is not particularly limited, and an example thereof may be aluminum foil.

[0049] The positive electrode mixed material layer contains a positive electrode active material, and may further contain a solid electrolyte, a conductive auxiliary agent, and a binder.

[0050] The positive electrode active material is not particularly limited as long as it can absorb and release lithium ions, and examples thereof include LiCoO2, Li(Ni 5 / 10 Co 2 / 10 Mn 3 / 10 )O2、Li(Ni 6 / 10 Co 2 / 10 Mn 2 / 10 )O2、Li(Ni 8 / 10 Co 1 / 10 Mn 1 / 10 )O2、Li(Ni 0.8 Co 0.15 Al 0.05 )O2、Li(Ni 1 / 6 Co 4 / 6 Mn 1 / 6 )O2、Li(Ni 1 / 3 Co 1 / 3 Mn 1 / 3 )O2, LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, sulfur.

[0051] The solid electrolyte constituting the solid electrolyte layer is not particularly limited as long as it is a material capable of conducting lithium ions, and examples thereof include oxide-based electrolytes and sulfide-based electrolytes (eg, argyrodite-type sulfide solid electrolytes).

[0052] The negative electrode mixed material layer is a lithium metal layer.

[0053] The negative electrode current collector is not particularly limited, and examples thereof include copper foil.

[0054] The above is a description of the embodiments of the present invention, but the present invention is not limited to the above embodiments, and the above embodiments may be appropriately changed within the scope of the subject matter of the present invention. For example, the configuration of the positive electrode and the negative electrode in the solid battery may also be reversed. In this case, the solid battery has an electrode stack in which a first solid electrolyte layer, a negative electrode, and a second solid electrolyte layer are stacked in sequence, and a negative electrode tab extends from the negative electrode. Here, one of the first solid electrolyte layer and the second solid electrolyte layer includes a porous substrate, and the other of the first solid electrolyte layer and the second solid electrolyte layer does not contain a porous substrate. In addition, when looking down at the electrode stack, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer exist on the outside compared to the outer peripheral end of the negative electrode, and the first solid electrolyte layer and the second solid electrolyte layer are joined in an area that is not opposite to the negative electrode and the negative electrode tab.

[0055] Reference numerals

[0056] 100 solid battery

[0057] 110, 610 electrode stack

[0058] 111 negative electrode

[0059] 111A negative electrode tab

[0060] 112 First solid electrolyte layer

[0061] 113, 613 positive electrode

[0062] 113A positive electrode tab

[0063] 114 Second solid electrolyte layer

[0064] 115 substrate

[0065] 120 Laminated Film

[0066] 130 negative pole ear lead

[0067] 140 positive pole ear lead

[0068] 150, 160 sealant

[0069] 411a negative electrode collector

[0070] 411b negative electrode mixed material layer

[0071] 413a positive electrode collector

[0072] 413b Positive electrode mixed material layer

Claims

1. A solid battery comprising an electrode stack having a first solid electrolyte layer, a positive electrode and a second solid electrolyte layer stacked in this order on a negative electrode, A positive electrode ear extends from the positive electrode. One of the first solid electrolyte layer and the second solid electrolyte layer includes a porous substrate. The other of the first solid electrolyte layer and the second solid electrolyte layer does not contain a porous substrate, When the electrode stack is viewed from above, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are located outside the outer peripheral end of the positive electrode. The first solid electrolyte layer and the second solid electrolyte layer are joined in a region that does not face the positive electrode and the positive electrode tab.

2. The solid battery according to claim 1, wherein: In the positive electrode, positive electrode mixed material layers are formed on both sides of the positive electrode collector. In the electrode stack, the first solid electrolyte layer, the positive electrode, the second solid electrolyte layer, and the second negative electrode are stacked in this order on the negative electrode.

3. The solid battery according to claim 1, wherein: An insulating frame is provided on the outer periphery of the positive electrode. When the electrode stack is viewed from above, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are located outside the outer peripheral end of the insulating frame. The first solid electrolyte layer and the second solid electrolyte layer are joined in a region not facing the insulating frame.

4. The solid battery according to claim 1, wherein: The negative electrode has a lithium metal layer.

5. A method for manufacturing a solid battery, which is a method for manufacturing the solid battery according to any one of claims 1 to 4, comprising the following steps: The step of sequentially stacking the first solid electrolyte layer, the positive electrode, and the second solid electrolyte layer; and a step of bonding the first solid electrolyte layer and the second solid electrolyte layer by applying pressure from the other side of the first solid electrolyte layer and the second solid electrolyte layer.

6. A solid battery comprising an electrode stack having a first solid electrolyte layer, a negative electrode and a second solid electrolyte layer stacked in this order on a positive electrode, A negative electrode tab extends from the negative electrode. One of the first solid electrolyte layer and the second solid electrolyte layer includes a porous substrate. The other of the first solid electrolyte layer and the second solid electrolyte layer does not contain a porous substrate, When the electrode stack is viewed from above, the outer peripheral ends of the first solid electrolyte layer and the second solid electrolyte layer are located outside the outer peripheral end of the negative electrode. The first solid electrolyte layer and the second solid electrolyte layer are joined in a region that does not face the negative electrode and the negative electrode tab.