High-solubility oat protein and preparation method thereof
Patent Information
- Application Number
- CN202411016208.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-27
- Publication Date
- 2024-10-11
AI Technical Summary
It is difficult to effectively improve the solubility of oat protein with existing technology, which limits its application in the field of food processing. Moreover, traditional solubilization methods are costly, complex, or unable to meet industrial production requirements.
The method of pH circulation combined with high-energy media milling is used to regulate the conformational changes of oat protein and improve its solubility and re-solubility through crushing, degreasing, extraction and spray drying processes.
It achieves the preparation of highly soluble oat protein with a solubility ≥85%, simplifies the process, reduces costs, is suitable for industrial production, and improves the emulsification and application scenarios of oat protein.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of food processing, and particularly relates to a highly soluble oat protein and a preparation method thereof. Background Art
[0002] As people pay more attention to healthy diet and pursue sustainable development, plant protein is favored by consumers due to its rich sources, high nutritional value, low price and low environmental pollution. Oats are rich in nutrients such as protein, fat, vitamins and dietary fiber, and are known as one of the best complete foods among cereals. The protein content in oats is about 16%, ranking first among cereals; the globulin content is as high as 70%, which is an oligomeric protein composed of 6 subunits through non-covalent bonds, and its tertiary structure is similar to soybean globulin. Oat protein has good nutritional properties, balanced amino acid composition, and a biological value of 72-75. It is a leader among plant proteins. However, the functional properties of oat protein such as solubility are poor, which limits its application in the field of food processing.
[0003] The current methods for solubilizing oat protein mainly include enzymatic method, chemical method and physical method. Among them, the enzymatic treatment cost is high and it is difficult to achieve industrialization; the chemical method has a complex process and has certain safety issues; although the physical method does not require additional chemical reagents, the traditional physical solubilization effect is limited and the processing capacity cannot match the requirements of industrial production. In addition, the solubilization technology research of some new oat proteins is also mostly concentrated in the experimental stage. Although oat protein solutions with good solubility can be obtained, the re-solubility after spray drying is still poor, making it difficult to achieve industrial production of oat protein. Therefore, the development of a simple, efficient, green, safe, and industrializable method for preparing highly soluble oat eggs is of great significance for expanding the oat protein market and breaking through the bottleneck of oat protein development. Summary of the invention
[0004] The purpose of the present invention is to solve the deficiencies of the prior art and provide a highly soluble oat protein and a preparation method thereof, which specifically adopts the following technical scheme: One aspect of the present invention provides a method for preparing highly soluble oat protein, comprising the following steps: S1: Grind oats to obtain oatmeal powder, then mix with 95% ethanol, centrifuge to obtain defatted oatmeal powder; S2: extracting oat protein from defatted oatmeal powder by alkali dissolution and acid precipitation; S3: Add water to the oat protein and mix well, add alkali to adjust the pH to 12.0-12.2, then grind in a high-energy medium mill for 40-60 min, add acid to adjust the pH to 6.8-7.0, spray dry, and finally obtain highly soluble oat protein.
[0005] The present invention adopts the method of pH cycle combined with high-energy medium mill, takes oats as raw materials, and prepares a highly soluble oat protein through the process of crushing, defatting, extraction, modification, drying and the like. The present invention mainly adopts low-temperature impact mill to crush oats, adds 95% ethanol to obtain defatted oat flour, extracts oat protein through alkali dissolution and acid precipitation, then adds alkali to adjust the solution environment to unfold the protein structure, and uses pH cycle combined with high-energy medium mill to regulate the conformational change of oat protein, and finally spray-dries to obtain oat protein. The experimental data results of the embodiment of the present invention show that compared with the oat protein powder directly obtained by high-energy medium milling, the oat protein prepared by this process can still maintain a high solubility after spray drying; compared with commercial oat protein, the oat protein prepared by the present invention has a solubility of ≥85%, and the method is simple to operate, has a short processing time, and has excellent physical and chemical properties. In short, the process framework of pH cycle combined with high-energy medium mill solves the difficulty of poor solubility of commercial oat protein, broadens the development scope and ideas of oat protein products, and meets the requirements of industrial production.
[0006] Among them, in the above preparation process, the pH of the system is adjusted to 12.0-12.2 by adding alkali. This is because when the pH is too low, the protein cannot be fully unfolded and the modification effect will be greatly weakened. If the pH is too high, the protein is easily hydrolyzed into peptides, thereby destroying the nutritional integrity of the protein and causing unpleasant flavors. In addition, too much alkali also increases the final salt content of the product. Then, hydrochloric acid is added to adjust the pH to 6.8-7.0. Too high a concentration of hydrochloric acid will cause local over-acidity in the system during the adjustment process, resulting in protein precipitation. A low concentration will increase the amount of acid used.
[0007] As a further preferred embodiment, in S1, a low-temperature impact mill is used to grind the oats to less than 300 meshes at a temperature of 15°C-25°C. Ultrafine grinding of oats is beneficial to the extraction of oat protein. Too large a particle size of oat powder will result in a low oat protein extraction rate. Low-temperature grinding is beneficial to protecting the components of oat powder and preventing the loss of its heat-sensitive components.
[0008] As a further preferred embodiment, the ratio of oatmeal powder to ethanol is 1g:15 mL-25 mL. A higher ethanol ratio is more conducive to the dissolution of fat, while a too low ratio may result in incomplete defatting.
[0009] As a further preferred embodiment, the specific process of extracting oat protein by the alkali dissolution and acid precipitation method in S2 is as follows: Dissolve defatted oatmeal powder in water, add alkali to adjust the pH to 10, then stir at 50 °C, centrifuge to obtain a supernatant, then add acid to adjust the pH to 4.5, centrifuge to obtain oat protein. Among them, the ratio of defatted oatmeal powder to water is 1:10-15. Too high or too low a ratio of oatmeal powder to water will affect the protein extraction rate. And the purpose of stirring at 50 °C in this process is that a higher water temperature is conducive to protein dissolution and improves the protein extraction rate, but when the temperature is higher than 60 °C, the protein is prone to denaturation. When adjusting the pH to alkaline, a lower pH is not conducive to protein dissolution, and too high a pH will also denature the protein, resulting in poor nutritional and functional properties.
[0010] As a further preferred embodiment, the base is sodium hydroxide, and the acid is citric acid or hydrochloric acid.
[0011] As a further preferred embodiment, the temperature of the oat protein solution is kept below 30° C. during grinding in the high-energy medium mill in S3 to prevent the oat protein from denaturing due to temperature rise during grinding.
[0012] As a further preferred embodiment, the specific process parameters of the high-energy medium mill in S3 are as follows: the rotation speed is 1200r / min, the diameter of the grinding beads is 0.6 mm, and the filling degree of the grinding chamber is 60%-75%. Among them, too high or too low filling of the grinding chamber will affect the grinding effect, resulting in poor modification of oat protein and no obvious improvement in its solubility. When the filling is too high (≥80%), the solubility will not only not increase but will decrease. The reason is that ① the filling rate is too high and affects the fluidity of the material in the cavity; ② the friction between the medium and the medium and the material increases, and the two together reduce the grinding efficiency.
[0013] As a further preferred embodiment, the spray drying in S3 adopts a mist drying tower atomizer, and the specific process parameters are as follows: frequency is 45 Hz-50 Hz, inlet air temperature is 160 ℃-175 ℃, and outlet air temperature is 75 ℃-85 ℃. Spray drying has high processing efficiency and large processing capacity, and is suitable for industrialization. The effect is better when the inlet air temperature and outlet air temperature are within the above range. If the temperature is too high, the protein is easy to denature and aggregate during the drying process, and if the temperature is too low, the production efficiency cannot be guaranteed.
[0014] Another aspect of the present invention provides a highly soluble oat protein prepared by the above preparation method, wherein the particle size of the highly soluble oat protein is 0.5 μm-10 μm. Compared with natural oat protein or oat protein dried after only high-energy medium treatment, the oat protein prepared by the present invention has a re-dissolved solubility of ≥85%, and an emulsification property improved by about 60%, which greatly expands its application scenarios.
[0015] The beneficial effects of the present invention are: The preparation method proposed in the present invention has a green and simple treatment process, is safe and controllable, and can be industrialized. The method regulates the conformational changes of oat protein by combining pH circulation with high-energy medium milling, thereby solving the problems of poor dispersibility and nutritional deficiencies of commercial oat protein. Among them, the physical modification equipment used in this method, the high-energy medium mill, has the characteristics of low-temperature grinding, large processing capacity, and good modification effect. It transfers energy to the stirring medium and protein through the rotating shaft. The violent movement between the grinding media produces shear, extrusion and friction forces, which cause the oat protein between the media to be deformed and broken by force, and promote the continuous development of the oat protein structure. High-energy medium milling treatment can dissociate large, irregular, and dense oat protein aggregates into uniform spherical proteins with a particle size of ≤10 μm, improve its anti-sedimentation and flocculation properties, and thus improve the dispersibility of oat protein in water (solubility ≥98%). DETAILED DESCRIPTION
[0016] The following will be combined with the embodiments to clearly and completely describe the concept, specific structure and technical effects of the present invention, so as to fully understand the purpose, scheme and effect of the present invention. It should be noted that the embodiments and features in the embodiments of this application can be combined with each other without conflict.
[0017] The model of the high energy medium mill in the embodiment of the present invention is XCFB-4T, and the manufacturer is Beijing Collaborative Innovation Food Technology Co., Ltd.
[0018] Example 1 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh; (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min and the supernatant was removed to obtain defatted oatmeal powder. (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and mix well. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge to obtain the precipitate as oat protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0019] (4) pH cycle combined with high-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the stirring tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w). Then, 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12. After grinding with the high-energy medium mill for 60 min, 1 M hydrochloric acid was added to adjust the pH to 7.0. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 75%, and the temperature of the entire system was maintained below 30 °C. The solubility of the modified oat protein was 99.01%, and the particle size was below 10 μm.
[0020] (5) Spray drying: The modified oat protein solution in step (4) was spray dried, with the spray tower atomizer motor frequency of 47 Hz, the air inlet temperature of 175°C, and the air outlet temperature of 80°C to obtain 0.67 kg of oat protein with a reconstituted solubility of 87.89%.
[0021] Example 2 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh; (2) Defatting: The oatmeal powder in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h, and the mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder; (3) Extracting protein by alkali dissolution and acid precipitation: The defatted oatmeal powder and deionized water in step (2) were mixed in a ratio of 1:10 (g / ml), the pH was adjusted to 10 with 1 M NaOH and stirred in a 50 °C water bath for 2 h, and the supernatant was obtained by centrifugation. The pH of the solution was then adjusted to 4.5 with 0.5 M HCl, and the oatmeal protein was obtained by centrifugation. The centrifugation parameters for both times were 4800 r / min and 20 min. (4) pH cycle combined with high-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), and then 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12, and stirred for 20 min. After grinding with a high-energy medium mill for 40 min, 1 M hydrochloric acid was added to adjust the pH to 7.0. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 75%, and the temperature of the entire system was kept below 30 °C. The solubility of the modified oat protein was 98.53%, and the particle size was below 10 μm.
[0022] (5) Spray drying: The modified oat protein solution in step (4) was spray dried. The frequency of the spray tower atomizer motor was 47 Hz, the air inlet temperature was 175°C, and the air outlet temperature was 80°C. 0.66 kg of oat protein was obtained, and the reconstituted solubility was 85.34%.
[0023] Example 3 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0024] (2) Defatting: Select the oatmeal powder in step (1) and 95% ethanol at a ratio of 1:20 (g / ml), mix and stir for 2 h, centrifuge at 4800 r / min for 20 min, remove the supernatant, and obtain defatted oatmeal powder.
[0025] (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and mix well. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge to obtain the precipitate as oat protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0026] (4) pH cycle combined with high-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), and then 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12. After grinding with the high-energy medium mill for 60 min, 1 M hydrochloric acid was added to adjust the pH to 7.0. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 60%, and the temperature of the entire system was maintained below 30 °C. The solubility of the modified oat protein was 91.98%, and the particle size was below 10 μm.
[0027] (5) Spray drying: The modified oat protein solution in step (4) was spray dried, with the spray tower atomizer motor frequency of 47 Hz, the air inlet temperature of 175°C, and the air outlet temperature of 80°C to obtain 0.60 kg of oat protein with a reconstituted solubility of 85.06%.
[0028] Comparative Example 1 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0029] (2) Defatting: Select the oatmeal powder in step (1) and 95% ethanol at a ratio of 1:20 (g / ml), mix and stir for 2 h, centrifuge at 4800 r / min for 20 min, remove the supernatant, and obtain defatted oatmeal powder.
[0030] (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and mix well. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge to obtain the precipitate as oat protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0031] (4) pH cycle combined with high-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), and then 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12. After grinding with the high-energy medium mill for 60 min, 1 M hydrochloric acid was added to adjust the pH to 7.0. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 85%, and the temperature of the entire system was maintained below 30 °C. The solubility of the modified oat protein was 69.14%, and the particle size was below 35 μm.
[0032] (5) Spray drying: The modified oat protein solution in step (4) was spray dried, with the spray tower atomizer motor frequency of 47 Hz, the air inlet temperature of 175°C, and the air outlet temperature of 80°C to obtain 0.60 kg of oat protein with a reconstituted solubility of 58.26%.
[0033] Comparative Example 2 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh; (2) Defatting: The oatmeal powder in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h, and the mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder; (3) Extracting protein by alkali dissolution and acid precipitation: The defatted oatmeal powder and deionized water in step (2) were mixed in a ratio of 1:10 (g / ml), the pH was adjusted to 10 with 1 M NaOH and stirred in a 50 °C water bath for 2 h, and the supernatant was obtained by centrifugation. The pH of the solution was then adjusted to 4.5 with 0.5 M HCl, and the oatmeal protein was obtained by centrifugation. The centrifugation parameters for both times were 4800 r / min and 20 min. (4) pH cycle combined with high energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), and then 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12, stirred for 40 min, and then ground by high energy medium mill for 20 min, and 1 M hydrochloric acid was added to adjust the pH to 7.0; the operating conditions of the high energy medium mill were: 1200 r / min, grinding beads (zirconia) with a diameter of 0.6 mm, grinding chamber filling degree of 75%, and the temperature of the entire system was maintained below 30 °C. The solubility of the modified oat protein was 72.38%, and the particle size was below 25 μm.
[0034] (5) Spray drying: The modified oat protein solution in step (4) was spray dried, with the spray tower atomizer motor frequency of 47 Hz, the air inlet temperature of 175°C, and the air outlet temperature of 80°C to obtain 0.27 kg of oat protein with a reconstituted solubility of 44.72%.
[0035] Comparative Example 3 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0036] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0037] (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and stir evenly. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge again to obtain the precipitate as oatmeal protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0038] (4) High-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), which was then ground in the high-energy medium mill for 60 min. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 75%, and the temperature of the entire system was kept below 30 °C. The solubility of the modified oat protein was 98.12%, and the particle size was below 10 μm.
[0039] (5) Spray drying: The modified oat protein solution in step (4) was spray dried, with the spray tower atomizer motor frequency of 47 Hz, the air inlet temperature of 175°C, and the air outlet temperature of 80°C to obtain 0.66 kg of oat protein with a reconstituted solubility of 23.02%.
[0040] Comparative Example 4 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0041] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0042] (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and mix well. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge to obtain the precipitate as oat protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0043] (4) High-energy medium mill modification: 0.9 kg of oat protein from step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), which was then ground in the high-energy medium mill for 40 min. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 75%, and the temperature of the entire system was kept below 30 °C. The solubility of the modified oat protein was 98.04%, and the particle size was below 10 μm.
[0044] (5) Spray drying: The modified oat protein solution in step (4) was spray dried at a spray tower atomizer motor frequency of 47 Hz, an air inlet temperature of 175°C, and an air outlet temperature of 80°C to obtain 0.66 kg of oat protein with a reconstituted solubility of 22.28%.
[0045] Comparative Example 5 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0046] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / ml) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0047] (3) Extracting protein by alkali dissolution and acid precipitation: Mix the defatted oatmeal powder and deionized water in step (2) in a ratio of 1:10 (g / ml) and mix well. Adjust the pH to 10 with 1 M NaOH and stir in a 50 °C water bath for 2 h. Centrifuge to obtain the supernatant. Adjust the pH of the solution to 4.5 with 0.5 M HCl and centrifuge to obtain the precipitate as oat protein. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0048] (4) High-energy medium mill modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), which was then ground in the high-energy medium mill for 20 min. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 75%, and the temperature of the entire system was kept below 30 °C. The solubility of the modified oat protein was 55.34%, and the particle size was below 25 μm.
[0049] (5) Spray drying: The modified oat protein solution in step (4) was spray dried at a spray tower atomizer motor frequency of 47 Hz, an air inlet temperature of 175°C, and an air outlet temperature of 80°C to obtain 0.37 kg of oat protein with a reconstituted solubility of 22.35%.
[0050] Comparative Example 6 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0051] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / mL) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0052] (3) Extracting protein by alkali dissolution and acid precipitation: The defatted oatmeal powder and deionized water in step (2) were mixed in a ratio of 1:10 (g / mL), the pH was adjusted to 10 with 1 M NaOH and stirred in a 50 °C water bath for 2 h. The supernatant was obtained by centrifugation. The pH of the solution was then adjusted to 4.5 with 0.5 M HCl and the oatmeal protein was obtained by centrifugation. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0053] (4) High-energy medium mill modification: 0.9 kg of oat protein from step (3) and 14.1 kg of deionized water were poured into the mixing tank of the high-energy medium mill and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w), which was then ground in the high-energy medium mill for 60 min. The operating conditions of the high-energy medium mill were: 1200 r / min, the diameter of the grinding beads (zirconia) was 0.6 mm, the filling degree of the grinding chamber was 60%, and the temperature of the entire system was kept below 30 °C. The solubility of the modified oat protein was 82.37%, and the particle size was below 10 μm.
[0054] (5) Spray drying: The modified oat protein solution in step (4) was spray dried at a spray tower atomizer motor frequency of 47 Hz, an air inlet temperature of 175°C, and an air outlet temperature of 80°C to obtain 0.56 kg of oat protein with a reconstituted solubility of 22.13%.
[0055] Comparative Example 7 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0056] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / mL) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0057] (3) Extracting protein by alkali dissolution and acid precipitation: The defatted oatmeal powder and deionized water in step (2) were mixed in a ratio of 1:10 (g / mL), the pH was adjusted to 10 with 1 M NaOH and stirred in a 50 °C water bath for 2 h. The supernatant was obtained by centrifugation. The pH of the solution was then adjusted to 4.5 with 0.5 M HCl and the oatmeal protein was obtained by centrifugation. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0058] (4) pH cycle modification: 0.9 kg of oat protein in step (3) and 14.1 kg of deionized water were poured into a stirring tank and mixed evenly to obtain an oat protein solution with a concentration of 6% (w / w). Then, 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12. After stirring for 60 min, 1 M hydrochloric acid was added to adjust the pH to 7.0. The solubility of the modified oat protein was 43.82%, and the average particle size was about 50 μm.
[0059] (5) Spray drying: The modified oat protein solution in step (4) was spray dried at a spray tower atomizer motor frequency of 47 Hz, an air inlet temperature of 175°C, and an air outlet temperature of 80°C to obtain 0.29 kg of oat protein with a reconstituted solubility of 42.06%.
[0060] Comparative Example 8 A method for preparing highly soluble oat protein comprises the following steps: (1) Grinding: Grind the oats in a low-temperature impact mill, set the main machine frequency to 30 Hz, the induced draft fan frequency to 30 Hz, the air classifier frequency to 40 Hz, and the grinding temperature to 18±1°C, and grind to less than 300 mesh.
[0061] (2) Defatting: The oatmeal powder prepared in step (1) was mixed with 95% ethanol at a ratio of 1:20 (g / mL) and stirred for 2 h. The mixture was centrifuged at 4800 r / min for 20 min to remove the supernatant to obtain defatted oatmeal powder.
[0062] (3) Extracting protein by alkali dissolution and acid precipitation: The defatted oatmeal powder and deionized water in step (2) were mixed in a ratio of 1:10 (g / mL), the pH was adjusted to 10 with 1 M NaOH and stirred in a 50 °C water bath for 2 h. The supernatant was obtained by centrifugation. The pH of the solution was then adjusted to 4.5 with 0.5 M HCl and the oatmeal protein was obtained by centrifugation. The centrifugation parameters for both times were 4800 r / min and 20 min.
[0063] (5) pH cycle combined with colloid mill modification: 0.9 kg of oat protein in step (3) was uniformly mixed with 14.1 kg of deionized water to obtain an oat protein solution with a concentration of 6% (w / w). Then, 10 M sodium hydroxide solution was added to maintain the pH of the protein solution at 12. After multiple pulverization treatments using a colloid mill, 1 M hydrochloric acid was added after the alkaline treatment time was 60 min to adjust the pH to 7.0. Finally, the oat protein solution was sieved with a 1250 mesh to ensure that its particle size was less than 10 μm. The solubility of the modified oat protein was 49.27%.
[0064] (4) Spray drying: The oat protein solution modified and sieved in step (4) was spray dried at a spray tower atomizer motor frequency of 47 Hz, an air inlet temperature of 175°C, and an air outlet temperature of 80°C to obtain 0.12 kg of oat protein with a reconstituted solubility of 41.19%.
[0065] Embodiment 4: In this example, the oat proteins prepared in the above examples 1-3 and comparative examples 1-8 were tested and analyzed for solubility before drying, solubility after redissolution, foaming properties, and foaming properties. The specific process is as follows: (1) Determination of oat protein solubility: The solubility of the modified oat protein solution was determined by the Kjeldahl method. The experimental process was based on GB 5009.5-2016.
[0066] (2) Determination of emulsification and emulsification stability of oat protein: The emulsification and emulsion stability were determined by turbidimetry. 16 mL of oat protein solution was added with 4 mL of soybean oil and immediately dispersed with a disperser to obtain an emulsion. Then, 50 μL of the emulsion was accurately measured at 0.5 cm from the bottom of the container and dispersed in 10 mL of 0.1% SDS (w / v). The emulsion was vortexed and mixed. The absorbance values of the emulsion after 0 min and 10 min were measured at a wavelength of 500 nm, A0 and A1. 10 . The emulsifying activity index (EAI, m 2 / g) and emulsion stability index (ESI, min) to express emulsification; the calculation formula is as follows: In the formula: DF represents the dilution factor, C represents the protein concentration (g / mL), f Indicates the optical path (1cm), i Indicates the volume fraction of oil (v / v) Where: A0 represents the absorbance value at 0 min; A 10 Indicates the absorbance value after 10 min; Δt indicates the time difference The above measurement results are shown in Table 1: Table 1 Oat protein performance test results As can be seen from the table above, pH cycle combined with high-energy medium milling modification can increase the solubility of oat protein to 99.01%. After spray drying, the solubility of oat protein re-dissolved is greatly increased by up to about 7.1 times, and the emulsification is increased by up to about 2.6 times, which greatly improves the functional properties of oat protein overall. In addition, if only high-energy medium milling or pH cycle treatment is used, the functional properties of oat protein are not significantly improved.
[0067] In summary, under the conditions of the present invention, the preparation of highly soluble oat protein can be achieved through pH circulation combined with high-energy medium milling, and the product has excellent physical and chemical properties, the process is simple and easy to realize industrial production, and has broad application prospects.
[0068] Although the description of the present invention has been quite detailed and specifically describes several described embodiments, it is not intended to be limited to any of these details or embodiments or any particular embodiment, but should be regarded as providing a broad possible interpretation of these claims in view of the prior art by reference to the appended claims, thereby effectively covering the intended scope of the present invention. In addition, the above description of the present invention is based on the embodiments foreseeable by the inventor, and its purpose is to provide a useful description, and those non-substantial changes to the present invention that have not yet been foreseen may still represent equivalent changes to the present invention.
Claims
1. A method for preparing highly soluble oat protein, characterized in that: The following steps are involved: S1: Grind oats to obtain oatmeal powder, then mix with 95% ethanol, centrifuge to obtain defatted oatmeal powder; S2: extracting oat protein from defatted oat flour by alkali dissolution and acid precipitation; S3: Add water to the oat protein and mix well, add alkali to adjust the pH to 12.0-12.2, then grind in a high-energy medium mill for 40-60 minutes, add acid to adjust the pH to 6.8-7.0, spray dry, and finally obtain highly soluble oat protein.
2. The preparation method according to claim 1, characterized in that: In S1, a low temperature impact mill is used to grind oats to less than 300 meshes at a temperature of 15°C-25°C.
3. The preparation method according to claim 2, characterized in that: The dosage ratio of oatmeal powder to ethanol is 1g:15mL-25mL.
4. The preparation method according to claim 1, characterized in that: The specific process of extracting oat protein by alkali dissolution and acid precipitation in S2 is as follows: Dissolve defatted oatmeal powder in water, add alkali to adjust the pH to 10, then stir at 50°C, centrifuge to obtain a supernatant, then add acid to adjust the pH to 4.5, centrifuge to obtain oat protein.
5. The preparation method according to claim 1, characterized in that: The base is sodium hydroxide and the acid is citric acid or hydrochloric acid.
6. The preparation method according to claim 1, characterized in that: The temperature of the oat protein solution was kept below 30°C during grinding in the high energy media mill in S3.
7. The preparation method according to claim 6, characterized in that: The specific process parameters of the S3 medium-high energy medium mill are as follows: the rotation speed is 1200 r / min, the grinding bead diameter is 0.6 mm, and the filling degree of the grinding chamber is 60%-75%.
8. The preparation method according to claim 1, characterized in that: The spray drying in S3 adopts a mist drying tower atomizer, and the specific process parameters are as follows: frequency is 45 Hz-50 Hz, inlet air temperature is 160 ℃-175 ℃, and outlet air temperature is 75 ℃-85 ℃.
9. A highly soluble oat protein, characterized in that: The invention is prepared by the preparation method according to any one of claims 1 to 8.
10. The highly soluble oat protein according to claim 9, characterized in that The particle size of highly soluble oat protein is 0.5 μm-10 μm.
Citation Information
Cited By
Preparation method and application of oat protein-pectin-procyanidine compound
CN119184195A
Preparation method and application of oat protein-pectin-proanthocyanidin complex
CN119184195B