Forging method of gearbox gear
Through hot isostatic pressing and CNC forging technology, combined with the assembly of intelligent manipulators, the problems of low material utilization and low production efficiency in gearbox gear forging are solved, and a high-precision and efficient forging process is achieved.
Patent Information
- Application Number
- CN202410961256.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-17
AI Technical Summary
Existing transmission gear forging methods have problems such as low material utilization, low processing accuracy, low production efficiency, and high energy consumption and cost.
High-strength alloy materials are used to prepare metal powder, and the forging billet is formed through hot isostatic pressing and CNC forging. It is precision processed and heat treated, and assembled with intelligent manipulators to ensure product quality and efficiency.
It improves material utilization and processing accuracy, reduces material waste and production costs, and improves the yield rate and production efficiency of gearbox gears.
Smart Images

Figure CN118752188A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of gearbox gear production, and in particular relates to a forging method for gearbox gears. Background Art
[0002] Train wheels are direct contact parts between the vehicle body and the railway track, and are responsible for vehicle starting, driving and braking. The gearbox gears, as the core transmission mechanism for wheel rotation, play a vital role in the power transmission and steering control of train vehicles. The strength and wear resistance of the gearbox gears directly affect the service life and maintenance cycle of the wheels. High-quality gearbox gears can withstand large loads and repeated stress cycles, thereby extending the service life of the wheels and reducing maintenance costs. They are crucial to ensuring the continuity and economy of railway transportation. Usually, the forging steps of gearbox gears include blanking, heating, billet making, pre-forging and trimming, heating, final forging and trimming, heat treatment, and shot blasting. The existing forging method of gearbox gears has the following disadvantages: (1) Low material utilization rate: Due to the complex structure of the gearbox gear, more waste and blanks will be generated in the traditional forging process, and the material utilization rate is low; (2) Low processing accuracy: The forging process itself has certain limitations, and it is difficult to achieve the strict dimensional tolerance and surface quality requirements required for gearbox gears; (3) Low production efficiency: The traditional single-piece forging method has low production efficiency and is not conducive to mass production; (4) High energy consumption and cost: High-temperature heating, repeated hammering and other processes consume a lot of energy. Combined with labor costs, the overall production cost is high. Summary of the invention
[0003] The present invention provides a forging method for a gearbox gear, so as to solve at least one of the above-mentioned technical problems.
[0004] In order to solve the above technical problems, the present invention discloses a forging method for a gearbox gear, comprising the following steps: S1. Material preparation: Select high-strength alloy material and prepare it into metal powder; S2. Hot isostatic pressing: hot isostatic pressing is performed on the metal powder to form a forging blank, which includes a sun gear forging blank, a plurality of planetary gear forging blanks and a ring gear forging blank; S3, CNC forging: placing the forging blank into the CNC forging equipment, performing forging plastic deformation, and finally forming a formed sun gear, a number of formed planetary gears and a formed ring gear; S4, precision machining and heat treatment: turning and grinding the formed sun gear, several formed planetary gears and formed ring gear, and performing quenching and tempering heat treatment to form a finished sun gear, several finished planetary gears and a finished ring gear; S5. Quality inspection: Conduct quality inspection on finished sun gears, several finished planetary gears and finished ring gears, and remove unqualified products; S6. Finished product assembly: The qualified finished sun gear, several finished planetary gears and finished ring gear are assembled and packaged by intelligent manipulators.
[0005] Preferably, step S1 comprises: S10, perform quality inspection on high-strength alloy materials and select qualified high-strength alloy materials; S11, after cleaning and cutting the qualified high-strength alloy material, put it into a smelting furnace for smelting to form a molten metal; S12, placing the molten metal into an atomizing device for atomization to finally form metal powder, and drying the metal powder.
[0006] Preferably, the atomization method adopted by the atomization device adopts any one of gas atomization or two-phase flow atomization.
[0007] Preferably, placing the molten metal into an atomizing device for atomization comprises: S120. Before atomization, the atomized particles are loaded into the solid particle discharge tank in advance, and the atomization equipment is inspected, calibrated and debugged; S121, during the atomization process, the atomizing gas in the high-pressure gas supply device generates a high-speed airflow under the action of the pressure device, and the high-speed airflow is sent into the solid particle discharge tank through the gas pipeline to form a two-phase flow together with the atomized particles in the solid particle discharge tank; S122, the two-phase flow is sprayed from the nozzle at the outlet end of the solid particle discharge tank into the atomization chamber, and at the same time, the molten metal is poured into the atomization chamber through the crucible; S123. The metal melt is formed into metal powder under the impact of the two-phase flow. The metal powder is cooled by the cooling water sprayed from the cooling water pipe and falls into the water at the bottom of the atomization chamber.
[0008] Preferably, the melting temperature of the smelting furnace is 1500°C-1650°C; The atomizing gas can be any one of nitrogen, inert gas and pure air; The atomized particles are metal particles having the same composition as the metal powder to be prepared.
[0009] Preferably, the method further comprises: performing real-time quality inspection on the metal powder during the atomization process and timely adjusting the atomization parameters of the atomization equipment, including the following steps: S124, performing a sampling quality inspection on the diameter of the metal powder, and if the quality inspection is qualified, the metal powder is dried, otherwise, executing step S125; S125. Calculate the regulated mass flow rate of the two-phase flow: S126. When the adjusted mass flow rate of the two-phase flow is calculated to be a positive value, the pressure of the two-phase flow is increased by adjusting the pressure-applying device so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank increases. When the adjusted mass flow rate of the two-phase flow is negative, the pressure of the two-phase flow is reduced by adjusting the pressure reducing valve, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank is reduced. , thus ensuring the quality of metal powder.
[0010] Preferably, step S125 includes: S1250. Calculate the Weber number of the current two-phase flow: (1); in, is the Weber number of the current two-phase flow, is the diameter of the nozzle at the outlet of the solid particle discharge tank, is the density of the atomizing gas in the two-phase flow, is the flow rate of the atomizing gas before it enters the solid particle discharge tank, is the flow rate of the molten metal in the crucible, It is the reference surface tension when the metal melt is broken. is the preset number of atomized particles sprayed out per unit time from the nozzle at the outlet of the solid particle discharge tank, is the reference mass of a single atomized particle, is the flow rate of atomized particles in two-phase flow, is the value of pi, which is 3.14. is the drag coefficient of two-phase flow; S1251. Calculate the regulated mass flow rate of the two-phase flow: (2); in, is the regulated mass flow rate of the two-phase flow, is the current mass flow rate of the molten metal, is the detection diameter of the i-th metal powder during sampling quality inspection, n is the number of metal powders sampled for quality inspection, is the preset reference diameter of the metal powder. is the kinematic viscosity of the two-phase flow, is the kinematic viscosity of the molten metal.
[0011] Preferably, hot isostatic pressing of the metal powder comprises: S20, putting the metal powder into the package, and extracting the gas adsorbed in the gaps between the metal powders and in the package; S21, vacuum-sealing the package and placing it into a pressure vessel of a hot isostatic press; S22, after sealing the pressure vessel, pumping inert gas into the pressure vessel to a preset pressure, and maintaining the pressure; S23, then heating the pressure vessel to a preset temperature, and completing hot isostatic pressing under the combined action of high temperature and high pressure; S24. Remove the sheathing mold by mechanical or acid leaching method to obtain the forging blank.
[0012] Preferably, step S5 includes dimensional inspection, surface quality inspection, material property inspection and preliminary meshing inspection of the finished sun gear, several finished planetary gears and the finished ring gear.
[0013] Preferably, step S6 comprises: S60, Parts cleaning: Check the cleanliness of the surface of the finished sun gear, several finished planetary gears and finished ring gear parts, and clean the contaminated areas; S61, Parts assembly: Use a multi-joint intelligent robotic arm to accurately grab finished parts and install the finished sun gear, several finished planetary gears and finished ring gear on the finished planetary gear carrier; S62, Parts lubrication: Apply lubricating grease to the meshing surfaces of gear parts of the gearbox; S63, Inspection and debugging: Carry out transmission test on the assembled gearbox gears to check whether they run smoothly and without abnormal noise, and make fine adjustments to the positions of various parts; S64. Packaging identification: Pack the qualified assembled gearbox gears and affix the identification information of the gearbox gears on the packaging.
[0014] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention adopts hot isostatic pressing technology to directly form metal powder materials into nearly formed parts under high temperature and high pressure, greatly reducing material waste. At the same time, compared with traditional machine combined with manual forging, the use of CNC forging can greatly improve the processing accuracy and material utilization rate, and at the same time improve production efficiency. Quality inspection of finished products can effectively improve the yield rate of finished gearbox gears. At the same time, after quality inspection, the intelligent manipulator assembles the gearbox gears to further confirm the yield rate of the finished products through assembly; 2. The present invention performs real-time quality inspection on metal powder during the atomization process, timely adjusts the atomization parameters of the atomization equipment, and adjusts the mass flow rate of the two-phase flow. When the mass flow rate of the two-phase flow is calculated to be a positive value, the pressure of the two-phase flow is increased by adjusting the pressure-applying device, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank increases. When the adjusted mass flow rate of the two-phase flow is negative, the pressure of the two-phase flow is reduced by adjusting the pressure reducing valve, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank is reduced. , thereby ensuring the quality of metal powder, and thus better ensuring the quality of gearbox gear forging. At the same time, the calculation of the regulated mass flow rate of the two-phase flow is applicable to both gas atomization and two-phase flow atomization. It has a wide range of applicability and can meet various manufacturing needs of gearbox gears. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings: Figure 1 It is a schematic diagram of the process flow of the present invention; Figure 2 A schematic diagram of the structure of the atomization device of the present invention; Figure 3 It is a hot isostatic pressing process flow chart of the present invention.
[0016] In the figure: 1. pressure device; 2. pressure gauge; 3. pressure reducing valve; 4. air valve; 5. solid particle discharge tank; 6. solid particles; 7. two-phase flow; 8. atomizer; 9. crucible; 10. cooling water pipe; 11. atomization chamber; 12. cooling water; 13. installation platform; 14. high-pressure gas supply device. DETAILED DESCRIPTION
[0017] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0018] In addition, in the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes, and do not specifically refer to the order or sequence, nor are they used to limit the present invention. They are only used to distinguish components or operations described with the same technical terms, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions and technical features between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0019] The present invention provides the following embodiments Example 1 The embodiment of the present invention provides a forging method for a gearbox gear, such as Figure 1-3 As shown, the following steps are included: S1. Material preparation: Select high-strength alloy material and prepare it into metal powder; S2. Hot isostatic pressing: hot isostatic pressing is performed on the metal powder to form a forging blank, which includes a sun gear forging blank, a plurality of planetary gear forging blanks and a ring gear forging blank; S3, CNC forging: placing the forging blank into the CNC forging equipment, performing forging plastic deformation, and finally forming a formed sun gear, a number of formed planetary gears and a formed ring gear; S4, precision machining and heat treatment: turning and grinding the formed sun gear, several formed planetary gears and formed ring gear, and performing quenching and tempering heat treatment to form a finished sun gear, several finished planetary gears and a finished ring gear; S5. Quality inspection: Conduct quality inspection on finished sun gears, several finished planetary gears and finished ring gears, and remove unqualified products; S6. Finished product assembly: The qualified finished sun gear, several finished planetary gears and finished ring gear are assembled and packaged by intelligent manipulators.
[0020] The working principle and beneficial effects of the above technical solution are as follows: a high-strength alloy material is selected and prepared into a metal powder, the metal powder is hot isostatically pressed to form a forging blank, the forging blank includes a sun gear forging blank, a plurality of planetary gear forging blanks and a ring gear forging blank, and then the forging blank is placed in a CNC forging device for forging plastic deformation to finally form a formed sun gear, a plurality of formed planetary gears and a formed ring gear, the formed sun gear, the plurality of formed planetary gears and the formed ring gear are turned and ground, and quenched and tempered to form a finished sun gear, a plurality of finished planetary gears and a finished ring gear, the finished sun gear, the plurality of finished planetary gears and the finished ring gear are quality inspected, unqualified products are removed, and finally the qualified finished sun gear, the plurality of finished planetary gears and the finished ring gear are assembled and packaged by an intelligent manipulator; The present invention adopts hot isostatic pressing technology to directly form metal powder materials into nearly formed parts under high temperature and high pressure, greatly reducing material waste. At the same time, compared with traditional machine combined with manual forging, CNC forging can greatly improve processing accuracy and material utilization, while improving production efficiency. Quality inspection of finished products can effectively improve the yield rate of finished gearbox gears. At the same time, after quality inspection, the intelligent manipulator assembles the gearbox gears to further confirm the yield rate of the finished products through assembly.
[0021] Example 2 Based on Example 1, step S1 includes: S10, perform quality inspection on high-strength alloy materials and select qualified high-strength alloy materials; S11, after cleaning and cutting the qualified high-strength alloy material, put it into a smelting furnace for smelting to form a molten metal; S12, placing the molten metal into an atomizing device for atomization to finally form metal powder, and drying the metal powder.
[0022] Preferably, the atomization method adopted by the atomization device adopts any one of gas atomization or two-phase flow atomization.
[0023] The working principle and beneficial effects of the above technical solution are as follows: gas atomization is to impact the metal melt with a high-speed gas flow, convert the gas kinetic energy into the surface energy of the metal droplets, and the droplets are then rapidly cooled to finally form spherical powders. Compared with the traditional mechanical crushing process, the gas atomization method is simple and economical. Compared with the water atomization process, the gas atomized powder has better sphericity, smoother surface and lower oxygen content. The metal powder prepared by gas atomization has the advantages of fine particle size, high sphericity, low oxygen content, uniform composition, high solid solubility and low environmental pollution. Two-phase flow atomization is a method of using a mixture of gas and solid as the atomizing medium (two-phase flow), pressurizing the atomizing medium to form a high-speed two-phase flow to impact the metal melt, converting the high-speed two-phase flow energy into the surface energy of the metal droplets, and then rapidly cooling the droplets to eventually form spherical powders. In addition to having the same advantages as gas atomization, two-phase flow atomization can process metal particles with smaller particle sizes than gas atomization.
[0024] Example 3 On the basis of Example 2, placing the molten metal into an atomizing device for atomization includes: S120, before atomization, the atomized particles are loaded into the solid particle discharge tank 5 in advance, and the atomization equipment is inspected, calibrated and debugged; S121, during the atomization process, the atomizing gas in the high-pressure gas supply device 14 generates a high-speed airflow under the action of the pressure-applying device 1, and the high-speed airflow is sent into the solid particle discharge tank 5 through the gas pipeline to form a two-phase flow together with the atomized particles in the solid particle discharge tank 5; S122, the two-phase flow is sprayed from the nozzle at the outlet end of the solid particle discharge tank 5 into the atomization chamber 11, and at the same time, the molten metal is poured into the atomization chamber 11 through the crucible 9; S123. The metal melt is impacted into a fountain shape by the impact of the two-phase flow. The kinetic energy of the two-phase flow is converted into the surface energy of the metal melt. Under the action of the surface energy, the metal melt forms metal powder. The metal powder is cooled by the cooling water sprayed from the cooling water pipe 10 and falls into the water at the bottom of the atomization chamber 11.
[0025] Preferably, the melting temperature of the smelting furnace is 1500°C-1650°C; The atomizing gas can be any one of nitrogen, inert gas and pure air; The atomized particles are metal particles having the same composition as the metal powder to be prepared.
[0026] The working principle and beneficial effects of the above technical solution are as follows: wherein, the atomization pressure is adjusted by the pressure applying device 1 and the pressure reducing valve 3, wherein the pressure value is read by the indicator on the pressure reducing valve 3, and furthermore, the air pressure in the high-pressure gas supply device 14 is read by the barometer 2, and the high-pressure gas supply device 14 is connected to the inlet end of the solid particle discharge tank 5 through the barometer 2; During the atomization process, the molten metal is impacted into a fountain shape by the impact of the two-phase flow, and the kinetic energy of the two-phase flow is converted into the surface energy of the molten metal. Under the action of the surface energy, the molten metal is formed into metal powder.
[0027] Example 4 On the basis of Example 3, the method further includes: performing real-time quality inspection on the metal powder during the atomization process and timely adjusting the atomization parameters of the atomization equipment, including the following steps: S124, performing a sampling quality inspection on the diameter of the metal powder, and if the quality inspection is qualified, the metal powder is dried, otherwise, executing step S125; S125. Calculate the regulated mass flow rate of the two-phase flow: S126, when the adjusted mass flow rate of the two-phase flow is calculated to be a positive value, the pressure of the two-phase flow is increased by adjusting the pressure applying device 1, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank 5 increases When the adjusted mass flow rate of the two-phase flow is negative, the pressure of the two-phase flow is reduced by adjusting the pressure reducing valve 3, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank 5 is reduced. , thus ensuring the quality of metal powder; Step S125 includes: S1250. Calculate the Weber number of the current two-phase flow: (1); in, is the Weber number of the current two-phase flow, is the diameter of the nozzle at the outlet of the solid particle discharge tank 5, is the density of the atomizing gas in the two-phase flow, is the flow rate of the atomizing gas before entering the solid particle discharge tank 5, is the flow rate of the molten metal in the crucible 9, It is the reference surface tension when the metal melt is broken. is the preset number of atomized particles sprayed out per unit time from the nozzle at the outlet end of the solid particle discharge tank 5, is the reference mass of a single atomized particle, is the flow rate of atomized particles in two-phase flow, is the value of pi, which is 3.14. is the drag coefficient of two-phase flow; S1251. Calculate the regulated mass flow rate of the two-phase flow: (2); in, is the regulated mass flow rate of the two-phase flow, is the current mass flow rate of the molten metal, is the detection diameter of the i-th metal powder during sampling quality inspection, n is the number of metal powders sampled for quality inspection, is the preset reference diameter of the metal powder, is the kinematic viscosity of the two-phase flow, is the kinematic viscosity of the molten metal.
[0028] The working principle and beneficial effects of the above technical solution: When aerosolization is used The value is 0, when two-phase flow atomization is used and Both are not 0. The density of the atomizing gas in the two-phase flow The flow rate of the atomized gas before entering the solid particle discharge tank 5 is obtained by the density sensor. The flow rate of atomized particles in two-phase flow is obtained by the flow rate sensor. = the flow rate of the atomized gas before entering the solid particle discharge tank 5 - the flow rate of the two-phase flow at the nozzle at the outlet end of the solid particle discharge tank 5, the flow rate of the molten metal in the crucible 9 is measured by a flow rate sensor, The value range is 20-35. The value is 1.03* -1.21* g, The value is 0.43-0.51; By performing real-time quality inspection on the metal powder during the atomization process, the atomization parameters of the atomization equipment are adjusted in time. Based on the adjusted mass flow rate of the two-phase flow, when the adjusted mass flow rate of the two-phase flow is calculated to be a positive value, the pressure of the two-phase flow is increased by adjusting the pressure-applying device 1, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank 5 increases. When the adjusted mass flow rate of the two-phase flow is negative, the pressure of the two-phase flow is reduced by adjusting the pressure reducing valve 3, so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank 5 is reduced. , thereby ensuring the quality of metal powder, and thus better ensuring the quality of gearbox gear forging. At the same time, the calculation of the regulated mass flow rate of the two-phase flow is applicable to both gas atomization and two-phase flow atomization. It has a wide range of applicability and can meet various manufacturing needs of gearbox gears.
[0029] Example 5 Based on Example 1, hot isostatic pressing of metal powder includes: S20, putting the metal powder into the package, and extracting the gas adsorbed in the gaps between the metal powders and in the package; S21, vacuum-sealing the package and placing it into a pressure vessel of a hot isostatic press; S22, after sealing the pressure vessel, pumping inert gas into the pressure vessel to a preset pressure, and maintaining the pressure; S23, then heating the pressure vessel to a preset temperature, and completing hot isostatic pressing under the combined action of high temperature and high pressure; S24. Remove the sheathing mold by mechanical or acid leaching method to obtain the forging blank.
[0030] The working principle and beneficial effects of the above technical solution are as follows: manufacturing the gearbox gears through hot isostatic pressing can effectively improve the density and uniformity of the gearbox gear parts. At the same time, hot isostatic pressing can process parts with complex shapes with higher flexibility. At the same time, it can enhance the strength, toughness, fatigue resistance and other properties of the gearbox gear parts. Moreover, compared with the traditional piece-by-piece pressing and sintering, the process time of hot isostatic pressing is shorter and the productivity is higher. At the same time, metal powder processing can greatly reduce the loss of raw materials in the traditional forging process.
[0031] Example 6 Based on Example 1, step S5 includes dimensional inspection, surface quality inspection, material property inspection and preliminary meshing inspection of the finished sun gear, several finished planetary gears and the finished ring gear.
[0032] The working principle and beneficial effects of the above technical solution are as follows: dimension inspection is carried out using a three-coordinate measuring machine, surface quality inspection is carried out through a surface defect judgment neural network model, material performance inspection includes hardness test, tensile test and metallographic analysis, hardness test is carried out using a Rockwell hardness tester, a Brinell hardness tester, etc., tensile test is carried out by carrying out a tensile test on a material testing machine, and strength parameters are measured for inspection, metallographic analysis uses a metallographic microscope to observe the organizational structure of the part material and evaluate its quality, gear meshing inspection is carried out by installing the parts on a special gear inspection table, the meshing of the gears is tested by driving, and the stability, noise, vibration and other performance indicators of the gear meshing are observed, and the above inspections are all carried out by sampling inspection.
[0033] Example 7 Based on Example 1, step S6 includes: S60, Parts cleaning: Check the cleanliness of the surface of the finished sun gear, several finished planetary gears and finished ring gear parts, and clean the contaminated areas; S61, Parts assembly: Use a multi-joint intelligent robotic arm to accurately grab finished parts and install the finished sun gear, several finished planetary gears and finished ring gear on the finished planetary gear carrier; S62, Parts lubrication: Apply lubricating grease to the meshing surfaces of gear parts of the gearbox; S63, Inspection and debugging: Carry out transmission test on the assembled gearbox gears to check whether they run smoothly and without abnormal noise, and make fine adjustments to the positions of various parts; S64. Packaging identification: Pack the qualified assembled gearbox gears and affix the identification information of the gearbox gears on the packaging.
[0034] The working principle and beneficial effects of the above technical solution are as follows: the finished product assembly process is highly automated, and the intelligent robotic arm is used to achieve precise positioning and assembly of parts, which greatly improves production efficiency and product quality consistency. At the same time, lubrication, sealing, inspection and debugging ensure the reliability and performance of the finished gear pair.
[0035] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A method for forging a gearbox gear, characterized in that: The following steps are involved: S1. Material preparation: Select high-strength alloy material and prepare it into metal powder; S2. Hot isostatic pressing: hot isostatic pressing is performed on the metal powder to form a forging blank, which includes a sun gear forging blank, a plurality of planetary gear forging blanks and a ring gear forging blank; S3, CNC forging: placing the forging blank into the CNC forging equipment, performing forging plastic deformation, and finally forming a formed sun gear, a number of formed planetary gears and a formed ring gear; S4, precision machining and heat treatment: turning and grinding the formed sun gear, several formed planetary gears and formed ring gear, and performing quenching and tempering heat treatment to form a finished sun gear, several finished planetary gears and a finished ring gear; S5. Quality inspection: Conduct quality inspection on finished sun gears, several finished planetary gears and finished ring gears, and remove unqualified products; S6. Finished product assembly: The qualified finished sun gear, several finished planetary gears and finished ring gear are assembled and packaged by intelligent manipulators.
2. A method for forging a gearbox gear according to claim 1, characterized in that: Step S1 includes: S10, perform quality inspection on high-strength alloy materials and select qualified high-strength alloy materials; S11, after cleaning and cutting the qualified high-strength alloy material, put it into a smelting furnace for smelting to form a molten metal; S12, placing the molten metal into an atomizing device for atomization to finally form metal powder, and drying the metal powder.
3. A method for forging a gearbox gear according to claim 2, characterized in that: The atomization method adopted by the atomization equipment is either gas atomization or two-phase flow atomization.
4. A method for forging a gearbox gear according to claim 2, characterized in that: Placing the molten metal into the atomizing equipment for atomization includes: S120, before atomization, the atomized particles are pre-loaded into the solid particle discharge tank (5), and the atomization equipment is inspected, calibrated and debugged; S121, during the atomization process, the atomizing gas in the high-pressure gas supply device (14) generates a high-speed airflow under the action of the pressure-applying device (1), and the high-speed airflow is sent into the solid particle discharge tank (5) through the gas pipeline to form a two-phase flow together with the atomized particles in the solid particle discharge tank (5); S122, the two-phase flow is sprayed from the nozzle at the outlet end of the solid particle discharge tank (5) into the atomization chamber (11), and at the same time, the molten metal is poured into the atomization chamber (11) through the crucible (9); S123. The metal melt is formed into metal powder under the impact of the two-phase flow. The metal powder is cooled by the cooling water sprayed from the cooling water pipe (10) and then falls into the water at the bottom of the atomization chamber (11).
5. A method for forging a gearbox gear according to claim 4, characterized in that: The melting temperature of the smelting furnace is 1500℃-1650℃; The atomizing gas can be any one of nitrogen, inert gas and pure air; The atomized particles are metal particles having the same composition as the metal powder to be prepared.
6. A method for forging a gearbox gear according to claim 4, characterized in that: Also includes: During the atomization process, the metal powder is inspected in real time and the atomization parameters of the atomization equipment are adjusted in time, including the following steps: S124, performing a sampling quality inspection on the diameter of the metal powder, and if the quality inspection is qualified, the metal powder is dried, otherwise, executing step S125; S125. Calculate the regulated mass flow rate of the two-phase flow: S126, when the regulated mass flow rate of the two-phase flow is calculated to be a positive value, the pressure of the two-phase flow is increased by adjusting the pressure applying device (1), so that the mass flow rate sensor value at the nozzle at the outlet end of the solid particle discharge tank (5) increases When the regulated mass flow rate of the two-phase flow is negative, the pressure of the two-phase flow is reduced by adjusting the pressure reducing valve (3), so that the mass flow rate sensor value at the nozzle at the outlet of the solid particle discharge tank (5) is reduced. , thus ensuring the quality of metal powder.
7. A method for forging a gearbox gear according to claim 6, characterized in that: Step S125 includes: S1250. Calculate the Weber number of the current two-phase flow: (1); in, is the Weber number of the current two-phase flow, is the diameter of the nozzle at the outlet of the solid particle discharge tank (5), is the density of the atomizing gas in the two-phase flow, is the flow rate of the atomizing gas before it enters the solid particle discharge tank (5), is the flow rate of the molten metal in the crucible (9), It is the reference surface tension when the metal melt is broken. is the preset number of atomized particles sprayed out per unit time from the nozzle at the outlet end of the solid particle discharge tank (5), is the reference mass of a single atomized particle, is the flow rate of atomized particles in two-phase flow, is the value of pi, which is 3.
14. is the drag coefficient of two-phase flow; S1251. Calculate the regulated mass flow rate of the two-phase flow: (2); in, is the regulated mass flow rate of the two-phase flow, is the current mass flow rate of the molten metal, is the detection diameter of the i-th metal powder during sampling quality inspection, n is the number of metal powders sampled for quality inspection, is the preset reference diameter of the metal powder. is the kinematic viscosity of the two-phase flow, is the kinematic viscosity of the molten metal.
8. The forging method of a gearbox gear according to claim 1, characterized in that: Hot isostatic pressing of metal powders includes: S20, putting the metal powder into the package, and extracting the gas adsorbed in the gaps between the metal powders and in the package; S21, vacuum-sealing the package and placing it into a pressure vessel of a hot isostatic press; S22, after sealing the pressure vessel, pumping inert gas into the pressure vessel to a preset pressure, and maintaining the pressure; S23, then heating the pressure vessel to a preset temperature, and completing hot isostatic pressing under the combined action of high temperature and high pressure; S24. Remove the sheathing die by mechanical or acid leaching method to obtain the forging blank.
9. The forging method of a gearbox gear according to claim 1, characterized in that: Step S5 includes a dimensional inspection, a surface quality inspection, a material property inspection and a preliminary meshing inspection of the finished sun gear, a plurality of finished planetary gears and a finished ring gear.
10. The forging method of a gearbox gear according to claim 1, characterized in that: Step S6 includes: S60, Parts cleaning: Check the surface cleanliness of the finished sun gear, several finished planetary gears and finished ring gear parts, and clean the contaminated areas; S61, Parts assembly: Use a multi-joint intelligent robotic arm to accurately grab finished parts and install the finished sun gear, several finished planetary gears and finished ring gear on the finished planetary gear carrier; S62, Parts lubrication: Apply lubricating grease to the meshing surfaces of gear parts of the gearbox; S63, Inspection and debugging: Carry out transmission test on the assembled gearbox gears to check whether they run smoothly and without abnormal noise, and make fine adjustments to the positions of various parts; S64. Packaging identification: Pack the qualified assembled gearbox gears and affix the identification information of the gearbox gears on the packaging.
Citation Information
Patent Citations
Forging technology for tap-position gear powder for automobile double-clutch transmission
CN105945290A
Cited By
Pre-forging equipment for gear forge piece production and pre-forging method of pre-forging equipment