Binder, electrode plate, secondary battery and electric equipment

By using fluorescent polymer binders in electrode pole pieces to monitor the dispersion of the binder, the problem of binder dispersion detection in the existing technology is solved, the production efficiency and yield rate of secondary batteries are improved, and the cost is reduced. .

CN118791990AInactive Publication Date: 2024-10-18HONOR DEVICE CO LTD +1

Patent Information

Application Number
CN202411263755.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

It is difficult to accurately detect the dispersion of the binder in the electrode plates with existing technology, resulting in limited improvements in secondary battery production yields, high detection costs, and poor sampling representativeness.

Method used

Develop a polymer binder with fluorescent properties. The binder is used to monitor the dispersion of the binder in the electrode plate. Through rapid detection of fluorescent signals, it can screen for uneven binder dispersion and optimize battery performance. .

Benefits of technology

Through fluorescence signal monitoring, the production yield of electrode pole pieces and the yield rate of secondary batteries are improved, the production cost is reduced, and the failure analysis during the battery charge and discharge cycle is assisted.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118791990A_ABST
    Figure CN118791990A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides a binder, an electrode plate, a secondary battery and electric equipment. The adhesive has the fluorescence characteristic while achieving the excellent adhesive property; when the device is applied to the electrode plate, the dispersing condition of the binder in the electrode plate and the manufacturing process of the electrode plate can be monitored, and the electrode plate with the non-uniformly dispersed binder can be judged and screened in time, so that the production yield of the electrode plate can be effectively improved, and the yield of a secondary battery can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of material technology, and in particular to adhesives, electrode plates, secondary batteries and electrical equipment. Background Art

[0002] The electrode plate is a key component of a secondary battery, which generally includes a current collector and an active material layer disposed on the current collector. In order to ensure the molding and structural stability of the active material layer, a binder is generally added to the active material layer, and the dispersion of the binder in the active material layer will affect the performance of the battery; therefore, monitoring the distribution of the binder in the active material layer during the production of the electrode plate can improve the production yield of the secondary battery. However, the binder used in the related art has similar component elements to other materials in the active material layer, and it is difficult to accurately detect the distribution of the binder through conventional detection methods, and the detection cost is high; the industry can only implement sampling detection at present, and the representativeness of the sampling inspection is poor, and the improvement of the production yield of the secondary battery is limited. Summary of the invention

[0003] In view of this, the embodiments of the present application provide a binder, an electrode sheet, a secondary battery and an electrical device. The binder has a fluorescent property while achieving a relatively good bonding performance; when it is applied to the electrode sheet, the manufacturing process of the electrode sheet and the dispersion of the binder in the electrode sheet can be monitored, and the electrode sheet with uneven binder dispersion can be timely judged and screened, thereby effectively improving the production yield of the electrode sheet and the yield of the secondary battery.

[0004] In a first aspect, an embodiment of the present application provides a binder, which is a polymer, and includes a fluorescent structural unit as shown in formula (I) and a viscous structural unit as shown in formula (II): Formula (I), Formula (II); Among them, R 11 is a single bond, any one of an alkylene group, an ester group, an ether bond, a ketocarbonyl group, and an amide group; R 12 is a fluorescent group; R2 is a group having adhesiveness.

[0005] The binder provided in the embodiment of the present application has both a fluorescent structural unit and a viscous structural unit in its molecular structure. Therefore, the binder has a bonding function, can form the active material layer of the electrode plate, and has a certain structural stability, while also having a fluorescent effect. In this way, the dispersion of the binder can be easily monitored during the manufacturing process of the electrode plate, so that the electrode plate with uneven binder dispersion can be judged and screened during the manufacturing process of the electrode plate, thereby effectively improving the production yield of the electrode plate, and can also effectively improve the yield of the secondary battery and reduce production costs. In addition, since the above-mentioned fluorescent performance is an inherent property of the binder, the failure analysis during the battery charge and discharge cycle can also be assisted by monitoring the distribution of the binder.

[0006] In some embodiments of the present application, the fluorescent group includes any one of a substituted or unsubstituted benzofuran group, a group containing isothiocyanate, a substituted or unsubstituted anthraquinone group, a group containing naphthalenesulfonic acid group, a substituted or unsubstituted pyridine group, a substituted or unsubstituted thiophene group, a substituted or unsubstituted indole group, a substituted or unsubstituted acridine group, and a substituted or unsubstituted rhodamine group. The above fluorescent groups have fluorescent signals under visible light excitation, which is beneficial to the rapid detection of the fluorescent signals of the binder.

[0007] In some embodiments of the present application, the R 12 Through the carbon atom and the R 11 In this way, the adhesive can be easily prepared.

[0008] In some embodiments of the present application, the fluorescent group is selected from any one of the structures shown in formula (1-1) to formula (1-19): Formula (1-1), Formula (1-2), (Formula 1-3), Formula (1-4), Formula (1-5), Formula (1-6), Formula (1-7), Formula (1-8), Formula (1-9), Formula (1-10), Formula (1-11), Formula (1-12), Formula (1-13), Formula (1-14), Formula (1-15), Formula (1-16), Formula (1-17), Formula (1-18), Formula (1-19); where Indicates the connection site.

[0009] In some embodiments of the present application, the fluorescent structural unit includes .

[0010] In some embodiments of the present application, the R2 includes -COOH, -COO - A + 、-CONH2、 , -SO3H; wherein A + Including Na + , Li + The above groups have strong viscosity, and the polymers they participate in forming can be dispersed in an aqueous system, which is beneficial to the application of the binder in the negative electrode of a secondary battery.

[0011] In some embodiments of the present application, the molar proportion of the fluorescent structural unit in the binder is ≥ 0.3%. In this way, the fluorescent effect signal of the binder is strong, which is easy to monitor the distribution of the binder in the battery process and battery failure analysis, and is more conducive to the application of the binder.

[0012] In some embodiments of the present application, the molar proportion of the viscous structural unit in the binder is ≥ 60%. In this way, the bonding strength of the binder is better, which is beneficial to the forming of the electrode sheet and improves the structural stability of the electrode sheet.

[0013] In some embodiments of the present application, in a single molecular chain of the binder, the number of the fluorescent structural units is 100-10000. In this way, the fluorescent effect signal of the binder molecule under the excitation wavelength is strong, which is beneficial to the application of the binder.

[0014] In some embodiments of the present application, the number of the adhesive structural units is 100-10000. In this way, the adhesive has a better bonding strength, which is beneficial to the forming of the electrode sheet and improves the structural stability of the electrode sheet.

[0015] In some embodiments of the present application, the binder further comprises a third structural unit as shown in formula (III), In formula (III), R3 is selected from any one of a strongly polar group, a hydrogen atom, and a C1-C6 hydrocarbon group; the strongly polar group includes a hydroxyl group or a cyano group. When R3 is selected from a strongly polar group, the bonding performance of the adhesive molecule can be further improved; when R3 is a hydrogen atom or a C1-C6 hydrocarbon group, the production cost of the adhesive can be reduced.

[0016] In some embodiments of the present application, in a single molecular chain of the binder, the number of the third structural units is 100-10000.

[0017] In some embodiments of the present application, the number average molecular weight of the binder is 3×10 5 -50×10 5 In this way, the binder has better processability and better dispersibility in a solvent (eg, water), which is beneficial to the application of the binder in an electrode sheet.

[0018] In some embodiments of the present application, the binder has a fluorescent signal under visible light excitation. In this way, the distribution of the binder can be monitored by an optical microscope, which is easy to implement in industrial production.

[0019] In some embodiments of the present application, the binder is a random copolymer or a block copolymer.

[0020] A second aspect of the embodiments of the present application provides an electrode plate, including a current collector and an active material layer disposed on the current collector, wherein the active material layer includes the binder provided in the first aspect of the embodiments of the present application.

[0021] A third aspect of the embodiments of the present application provides a secondary battery, comprising the electrode plate provided in the embodiments of the present application, and an electrolyte.

[0022] The fourth aspect of the embodiment of the present application provides an electric device, including the secondary battery provided by the embodiment of the present application. Due to the use of the secondary battery provided by the embodiment of the present application, the electric device has a better market prospect. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 A, B, and C are optical microscope photographs of different magnifications of the adhesive prepared in Example 1 of the present application without visible light excitation; Figure 1 a, b, and c are Figure 1 A, B, and C in the figure correspond to optical microscope photographs of the adhesive after being excited by visible light; Figure 2A This is an optical photograph of the negative electrode sheet prepared in Example 1 of the present application; Figure 2B This is an optical microscope photograph of the negative electrode active layer of the negative electrode sheet prepared in Example 1 of the present application after being exposed to a visible light source for 0.5 s; Figure 2C This is an optical microscope photograph of the negative electrode active layer of the negative electrode sheet prepared in Example 1 of the present application after color development treatment. DETAILED DESCRIPTION

[0024] The electrode plate is one of the key components of a secondary battery, which generally includes a current collector and an active material layer disposed on the current collector. In order to ensure the molding and structural stability of the active material layer, a binder is generally added to the active material layer. The dispersion of the binder will affect the performance of the battery. For example, poor dispersion of the binder will affect the electrochemical performance and safety performance of the battery. It can be seen that if the dispersion of the binder in the electrode plate can be monitored during the battery manufacturing process, the electrode plate can be screened, thereby effectively improving the production yield of the battery, optimizing the production capacity, and reducing the cost of the battery. Taking the wet method for preparing the electrode plate as an example, the binder, active material particles, and optional conductive agents are generally dispersed in a solvent to obtain an active material layer slurry, and then the active material layer slurry is coated on the current collector. The electrode plate can be obtained through processes such as rolling, striping, baking, lithium supplementation, and die cutting. In some cases, the electrode plate process needs to undergo secondary or even multiple rolling. In any of the above links, there may be or induce uneven distribution of the binder, especially in the preparation, coating, and rolling of the active material layer slurry.

[0025] In addition, in high energy density battery systems, such as silicon-based negative electrode battery systems, the volume expansion of the negative electrode plates is serious during the battery's charge and discharge cycle; in situ characterization of the binder distribution in the negative electrode plates before and after the cycle is very important for clarifying the negative electrode expansion.

[0026] Since the elemental composition (carbon, nitrogen, oxygen, etc.) of the binder used in the relevant technology is very similar to other components in the electrode plate and is easy to be confused, it is difficult to characterize the binder distribution through a scanning electron microscope (SEM), an energy dispersive spectrometer (EDS), or a transmission electron microscope (TEM). Even though high-resolution methods are currently used to characterize local areas of the binder, only micro-nano level characterization can be detected at a time, and it is difficult to detect the overall binder distribution of the electrode plate.

[0027] In order to solve the above technical problems, an embodiment of the present application provides a binder, which is a polymer, and the binder includes a fluorescent structural unit as shown in formula (I) and a viscous structural unit as shown in formula (II): Formula (I), Formula (II); Among them, R 11 is a single bond, any one of an alkylene group, an ester group, an ether bond, a ketocarbonyl group, and an amide group; R 12 is a fluorescent group; R2 is a group having adhesiveness.

[0028] It is understandable that in the embodiment of the present application, a single molecular chain of the binder includes structural units shown in formula (I) and formula (II) at the same time. In the embodiment of the present application, the binder may include only one fluorescent structural unit and one adhesive structural unit, for example: R 11 All are single bonds, R 12 The chemical formula of R is the same as that of R2; in other embodiments, the binder may include a plurality of different fluorescent structural units and a viscous structural unit, for example: R 11 All are single bonds, but R 12 The chemical structural formulas of the adhesive structural units are different, and the chemical structural formulas of R2 in the multiple adhesive structural units are the same; or, only one fluorescent structural unit is included, and multiple different adhesive structural units. In other embodiments, the adhesive includes multiple different fluorescent structural units and multiple different adhesive structural units at the same time. The above-mentioned "multiple" refers to two or more.

[0029] In the embodiments of the present application, the presence of fluorescent structural units and adhesive structural units in the binder can be determined by using X-ray photoelectron spectroscopy (XPS), infrared, or nuclear magnetic resonance testing methods.

[0030] The binder provided in the embodiment of the present application has both fluorescent structural units and viscous structural units in its molecular structure. Therefore, the binder has a bonding function, can make the active material layer of the electrode plate molded and have a certain structural stability, and also has a fluorescent effect. In this way, the dispersion of the binder can be easily monitored in the process of electrode plates; specifically, taking the wet preparation of electrode plates as an example: the dispersion of the binder in the active material layer slurry can be smoothly monitored, and the distribution of the binder in the active material layer of the prepared electrode plate can be monitored; therefore, in the process of electrode plates, not only can the dispersion of the binder in the active material layer slurry be adjusted in time, but also the electrode plates with uneven binder dispersion can be judged and screened in time, so as to effectively improve the production yield of the electrode plates, and can also effectively improve the yield of secondary batteries and reduce production costs. In addition, since the above-mentioned fluorescent properties are inherent properties of the binder, the failure analysis during the battery charge and discharge cycle can also be assisted by monitoring the distribution of the binder.

[0031] In some embodiments of the present application, R 11 is a single bond, that is, the structure shown in formula (1) can be In other embodiments, R 11is any one of an alkylene group, an ester group (-COO-), an ether bond (-COC-), a ketocarbonyl group (-CO-), and an amide bond (-CONH-), that is, R 12 R is bridged to the main chain through any one of alkylene, ester, ether, ketocarbonyl, and amide bonds; 12 Bridging the above groups with the main chain will not affect the fluorescence properties of the fluorescent group, and in some cases, it is beneficial to the preparation of the binder.

[0032] In some embodiments of the present application, the fluorescent group has a fluorescent signal under visible light excitation. In this way, the distribution of the binder can be monitored by an optical microscope, which is easy to implement in industrial production. In the embodiments of the present application, visible light refers to light with a wavelength within the range of 300 nm-700 nm. Specifically, the excitation wavelength of the fluorescent group can be, for example, 300 nm-450 nm, 350 nm-500 nm, 300 nm-500 nm, 350 nm-550 nm, 350 nm-600 nm, 400 nm-700 nm, etc.

[0033] In some embodiments of the present application, the fluorescent group includes any one of a substituted or unsubstituted benzofuran group, an isothiocyanate-containing group, a substituted or unsubstituted anthraquinone group, a naphthalenesulfonic acid-containing group, a substituted or unsubstituted pyridine group, a substituted or unsubstituted thiophene group, a substituted or unsubstituted indole group, a substituted or unsubstituted acridine group, and a substituted or unsubstituted rhodamine group. The above fluorescent groups have fluorescent signals under visible light excitation, which is beneficial to the rapid detection of the fluorescent signal of the binder. Specifically, the benzofuran group can be, for example, Formula (1-1), or The structure shown in formula (1-2), wherein The marked position indicates the attachment site of the benzofuran group; the attachment site of the benzofuran group can be any carbon atom on the carbon ring or oxygen heterocycle of benzofuran that can be used as the attachment site, and the present application does not limit this. In other specific embodiments, the above-mentioned benzofuran group can also be a benzofuran group substituted with a substituent, and the above-mentioned substituent includes but is not limited to weak polar groups such as hydrocarbon groups and ether bonds. In this way, the substituent will not destroy the electronic distribution of the benzofuran group, and thus the fluorescence signal of the fluorescent group can be ensured to be strong. Specifically, the hydrocarbon group can be, for example, a straight-chain alkyl or straight-chain alkyl such as methyl, ethyl, propyl, or a straight-chain alkenyl or straight-chain alkenyl such as vinyl and propenyl, or a cycloalkyl such as cyclopropyl and cyclobutyl, or a cycloalkenyl, but not limited thereto; the substituent can be located on any carbon atom that can be substituted by the benzofuran group, and the present application does not limit this.

[0034] In some embodiments of the present application, the fluorescent group may be a substituted or unsubstituted anthraquinone group. Specifically, the anthraquinone group may be, for example, any structure shown in formula (1-3) to formula (1-5), (Formula 1-3), Formula (1-4), Formula (1-5); where The marked position indicates the attachment site of the anthraquinone group; the attachment site of the anthraquinone group can be any carbon atom on the anthraquinone group that can serve as a attachment site, and the present application does not impose any restrictions on this. In other embodiments, the fluorescent group can also be an anthraquinone group substituted with a substituent, and the substituent on the anthraquinone group can be, for example, a weakly polar group such as a hydrocarbon group and an ether bond. In this way, the substituent will not destroy the electron distribution of the anthraquinone group, thereby ensuring that the fluorescent signal of the fluorescent group is strong. Specifically, the hydrocarbon group can be, for example, a straight-chain alkyl or straight-chain alkyl such as methyl, ethyl, propyl, or a straight-chain alkenyl or straight-chain alkenyl such as vinyl and propenyl, or a cycloalkyl such as cyclopropyl and cyclobutyl, or a cycloalkenyl, but is not limited thereto; the substituent can be located on any carbon atom that can be substituted for the anthraquinone group. In other words, in some embodiments of the present application, R 12 The attachment site is selected from R 12 The present application does not impose any restriction on this.

[0035] In some embodiments of the present application, the group containing naphthalenesulfonic acid group can be, for example Formula (1-6), Indicates the connection site; the above groups have strong fluorescence signals at an excitation wavelength of 300 nm-500 nm. At this time, the fluorescent structural unit can be expressed as .

[0036] In some embodiments of the present application, the fluorescent group is any one of a substituted or unsubstituted pyridine group, a substituted or unsubstituted thiophene group, a substituted or unsubstituted indole group, and a substituted or unsubstituted acridine group. Specifically, the structural formula of the pyridine group is Formula (1-7), the structural formula of the thiophene group is Formula (1-8); the structural formula of the indole group can be Formula (1-9), or Formula (1-10); The structural formula of the acridine group can be, for example Formula (1-11), or Formula (1-12), or Formula (1-13); In the above structural formulas, All represent connection sites, and the connection sites of the above-mentioned groups and the main chain can be any carbon atom in the above-mentioned groups that can serve as connection sites. In other embodiments, the above-mentioned pyridine group, thiophene group, indole group, and acridine group can be further substituted, and the substituents on the above-mentioned groups can be independently selected from weak polar groups such as hydrocarbon groups and ether bonds, so that the substituents will not destroy the electron distribution of the above-mentioned groups, thereby ensuring that the fluorescent signal of the fluorescent group is strong. Specifically, the hydrocarbon group can be, for example, a straight-chain alkyl or straight-chain alkyl such as methyl, ethyl, propyl, or a straight-chain alkenyl or straight-chain alkenyl such as vinyl and propenyl, or a cycloalkyl such as cyclopropyl and cyclobutyl, or a cycloalkenyl, but not limited thereto; the substituent can be located on any carbon atom that can be substituted by the above-mentioned groups, and this application does not limit this.

[0037] In some embodiments of the present application, the fluorescent group is a substituted or unsubstituted rhodamine group; specifically, the structural formula of the rhodamine group can be expressed as Formula (1-14), or Formula (1-15), or Formula (1-16), Indicates the attachment site. In some embodiments, the fluorescent group is a rhodamine group substituted with a substituent, and the substituent on the rhodamine group includes, but is not limited to, a hydrocarbon group, an ether bond and other weak polar groups, so that the substituent does not destroy the electron distribution of the above-mentioned rhodamine group, thereby ensuring that the fluorescent signal of the fluorescent group is strong. Specifically, the hydrocarbon group can be, for example, a straight-chain alkyl or straight-chain alkyl such as methyl, ethyl, propyl, or a straight-chain alkenyl or straight-chain alkenyl such as vinyl, propenyl, or a cycloalkyl such as cyclopropyl, cyclobutyl, or a cycloalkenyl, but is not limited thereto; the substituent can be located on any carbon atom that can be substituted by the above-mentioned rhodamine group, and this application does not limit this.

[0038] In some embodiments of the present application, the fluorescent group may be a group containing isothiocyanate, for example, a fluorescein isothiocyanate group, but is not limited thereto; specifically, the structural formula of the group containing isothiocyanate may be Formula (1-17), Formula (1-18), Formula (1-19), The marked position indicates the connection site. The connection site of the fluorescein isothiocyanate group can be any carbon atom in its structure that can serve as a connection site, and the present application does not impose any limitation on this.

[0039] In the embodiments of the present application, in addition to the fluorescent groups mentioned above, those skilled in the art can also select other groups that have fluorescent signals under visible light excitation, or modify fluorescent groups that are sensitive to other wavelengths to make them sensitive to visible light; specifically, the number of conjugated double bonds in the group can be adjusted, or the proportion of heteroatoms in the heterocyclic group can be adjusted to adjust the molecular transition energy band difference of the group to achieve the group excitation fluorescence in the visible light band. Of course, the fluorescent group can also be a group that has a fluorescent signal under excitation of other wavelengths.

[0040] In some embodiments of the present application, the sticky group R2 includes but is not limited to -COOH, -COO - A + 、-CONH2、 , -SO3H; wherein A + Including but not limited to Na + , Li + etc. are monovalent cations. Specifically, In the above, -COOH can be located on any substitutable carbon atom on the benzene ring. The above groups have strong viscosity, and the polymers they participate in can be dispersed in an aqueous system, which is beneficial to the application of the binder in the negative electrode of the secondary battery. At this time, the viscous structural unit includes but is not limited to the structures shown in formula (2-1) to formula (2-6): Formula (2-1), Formula (2-2), Formula (2-3), Formula (2-4), Formula (2-5) Formula (2-6).

[0041] In some embodiments of the present application, the molar ratio of the fluorescent structural unit in the binder is ≥0.3%. In this way, the fluorescent signal of the binder is strong, which is easy to monitor the distribution of the binder in the battery process and battery failure analysis, and is more conducive to the application of the binder. In the embodiment of the present application, the molar ratio of the fluorescent structural unit in the binder can be, for example, 0.3%, 0.5%, 1%, 2%, 5%, 8%, 10%, 12%, 15%, 18%, 20%, 22%, 25%, 28%, 30%, 32%, 35%, 38%, etc. In the embodiment of the present application, the carbon spectrum of nuclear magnetic resonance spectroscopy (NMR) can be used to test the molar ratio of the fluorescent structural unit in the binder.

[0042] In some embodiments of the present application, in the molecular chain of a single adhesive, the number of fluorescent structural units is 100-10000. In this way, the fluorescent signal of the adhesive molecule at the excitation wavelength is strong, which is conducive to the application of the adhesive. Specifically, in the molecular chain of a single adhesive, the number of fluorescent structural units can be, for example, 100, 200, 500, 1000, 1500, 2000, 2500, 3000, 3500, 4000, 4500, 5000, 5500, 6000, 6500, 7000, 7500, 8000, 8500, 9000, 9500, 10000. In the embodiment of the present application, gel permeation chromatography (GPC) can be used to test the molecular weight of the adhesive, and then the molar proportion of the fluorescent structural unit in the adhesive is calculated according to the carbon spectrum of NMR, and then the number of viscous structural units is calculated.

[0043] In some embodiments of the present application, the molar ratio of the viscous structural unit in the binder is ≥ 60%. In this way, the bonding strength of the binder is better, which is conducive to the molding of the electrode sheet and improves the structural stability of the electrode sheet. Specifically, the molar ratio of the viscous structural unit in the binder can be, for example, 60%, 62%, 65%, 68%, 70%, 72%, 75%, 78%, 80%, 82%, 85%, 88%, 90%, 92%, 95%, 98%, 99%, etc.

[0044] In some embodiments of the present application, in the molecular chain of a single binder, the number of viscous structural units is 100-10000. In this way, the molecular weight of the binder molecule is more suitable and the bonding performance is good, which is beneficial to the application of the binder and is more conducive to improving the production yield of the secondary battery. Specifically, in the molecular chain of a single binder, the number of viscous structural units can be, for example, 100, 200, 500, 1000, 1500, 2000, 2500, 3000, 3500, 4000, 4500, 5000, 5500, 6000, 6500, 7000, 7500, 8000, 8500, 9000, 9500, 10000. In the embodiment of the present application, the molecular weight of the binder can be tested by gel permeation chromatography, and then the molar proportion of the viscous structural unit in the binder is calculated according to the carbon spectrum of NMR, and then the number of viscous structural units is calculated.

[0045] In the embodiment of the present application, the binder may be a random copolymer or a block copolymer.

[0046] In some specific embodiments of the present application, the binder is a block copolymer, and the binder includes a structure as shown in formula (A), Formula (A); Specifically, in the fluorescent group of the binder, R 11 -R12 It can be connected to the carbon atom position marked by 1 or the carbon atom position marked by 2; in the adhesive structural unit of the adhesive, R2 can be connected to the carbon atom position marked by a or the carbon atom position marked by b, R 11 -R 12 And the connection position of R2 will not destroy the fluorescence activity and bonding performance of the adhesive. In some specific embodiments, n1 is a positive integer of 100-10000, and n2 is a positive integer of 100-10000.

[0047] In some specific embodiments of the present application, the binder is a random copolymer, and the binder includes a structure as shown in formula (B), Formula (B); Similarly, in the fluorescent group of the binder, R 11 -R 12 It can be connected to the carbon atom position marked by 1 or the carbon atom position marked by 2; in the adhesive structural unit of the adhesive, R2 can be connected to the carbon atom position marked by a or the carbon atom position marked by b, R 11 -R 12 The connection position of R2 will not destroy the fluorescent activity and bonding performance of the adhesive. In some specific embodiments, n1×m is a positive integer of 100-10000, and n2×m is a positive integer of 100-10000. Taking the structure shown in formula (B) as an example, when R 11 -R 12 When connected to the carbon atom position marked by 2, other groups may be connected to the carbon atom marked by 1, as long as the fluorescence and bonding properties of the binder are not damaged. Similarly, when R2 is connected to the carbon atom position marked by b, other groups may be connected to the carbon atom marked by a, as long as the fluorescence and bonding properties of the binder are not damaged.

[0048] Considering that the binder needs a certain molecular weight to meet the application requirements of the active material layer slurry, in some embodiments of the present application, the binder further includes a third structural unit as shown in formula (III), In formula (III), R3 is selected from any one of a strong polar group, a hydrogen atom, and a C1-C6 hydrocarbon group; the strong polar group includes a hydroxyl group (-OH) or a cyano group (-CN). Specifically, in some embodiments, R3 is selected from a hydroxyl group or a cyano group, so that the bonding performance of the binder molecule can be further improved (for example, the bonding strength can be improved), or the mass proportion of the binder in the active material layer can be appropriately reduced without affecting the safety performance and structural stability of the electrode plate, and the energy density of the final secondary battery can be improved. Taking into account different application scenarios, when the bonding requirements of the binder are not strict, and in order to control the production cost of the binder, in other specific embodiments, R3 is selected from a hydrogen atom or a C1-C6 hydrocarbon group; at this time, the binder is easy to prepare and has better fluorescence and bonding properties. Specifically, the C1-C6 hydrocarbon group can be a C1-C6 alkyl, C2-C6 alkenyl, C2-C6 alkynyl or C3-C6 cycloalkyl; the above alkyl, alkenyl, alkynyl can be linear or branched, for example, methyl, ethyl, propyl, butyl, pentyl, hexyl, vinyl, propenyl, butenyl, ethynyl, propynyl, cyclopropyl, cyclobutyl, but not limited to this. In the embodiment of the present application, the adhesive molecule can include only one R3, for example, R3 is a hydroxyl group, or R3 is a methyl group; or, the adhesive molecule can include multiple R3, wherein a part of R3 is selected from the above-mentioned strong polar groups, and a part of R3 is selected from hydrogen atoms; or, the adhesive molecule includes multiple R3, wherein a part of R3 is selected from hydroxyl groups, and another part of R3 is selected from cyano groups; but not limited to this.

[0049] In some embodiments of the present application, the binder is a block copolymer, and the binder includes a structure as shown in formula (C), Formula (C). In this case, n1 and n2 are each independently a positive integer of 100-10000, and n3 is a positive integer; n1 / (n1+n2+n3)×100%≥0.3%, n2 / (n1+n2+n3)×100%≥60%. In some specific embodiments, n3 is a positive integer of 100-10000. Similarly, R 11 -R 12 can be connected to the carbon atom position marked by 1 or 2; in the adhesive structural unit of the binder, R2 can be connected to the carbon atom position marked by a or b; in the third structural unit of the binder, R3 can be connected to the carbon atom position marked by x or y; R 11 -R 12 The connection positions of R2 and R3 will not destroy the fluorescence activity and bonding performance of the adhesive. It can be understood that, taking the structure shown in formula (C) as an example, when R 11 -R 12When connected to the carbon atom position marked by 2, the carbon atom marked by 1 may also be connected to other groups, as long as the fluorescence and bonding properties of the binder are not damaged. Similarly, when R2 is connected to the carbon atom position marked by b, the carbon atom marked by a may also be connected to other groups, as long as the fluorescence and bonding properties of the binder are not damaged; the third structural unit is similar and will not be described in detail here.

[0050] In some other embodiments of the present application, the binder is a random copolymer, and the binder includes a structure as shown in formula (D), Formula (D). In this case, similarly, n1 and n2 are each independently a positive integer of 100-10000, and n3 is a positive integer; n1 / (n1+n2+n3)×100%≥0.3%, n2 / (n1+n2+n3)×100%≥60%. In some specific embodiments, n3 is a positive integer of 100-10000. Similarly, R 11 -R 12 can be connected to the carbon atom position marked by 1 or 2; in the adhesive structural unit of the binder, R2 can be connected to the carbon atom position marked by a or b; in the third structural unit of the binder, R3 can be connected to the carbon atom position marked by x or y; R 11 -R 12 The connection positions of R2, R3 and R4 will not destroy the fluorescent activity and bonding performance of the adhesive.

[0051] In some embodiments of the present application, the number average molecular weight of the binder is 3×10 5 -50×10 5 In this way, the binder has better processability and good dispersibility in solvents (e.g., water), which is conducive to the application of the binder in electrode plates. Specifically, the number average molecular weight of the binder can be, for example, 3×10 5 , 5×10 5 , 8×10 5 , 10×10 5 , 15×10 5 , 20×10 5 , 25×10 5 ,30×10 5 ,35×10 5 , 40×10 5 45×10 5 , 50×10 5 In the examples of the present application, GPC can be used to test the number average molecular weight of the binder.

[0052] In some embodiments of the present application, the room temperature viscosity of the aqueous solution of the aforementioned binder with a solidification amount of 6wt% is ≥7000cps. In this way, the binder has good processability, which is conducive to the application of the binder in the electrode plate. In the embodiment of the present application, a rotational rheometer can be used to test the room temperature viscosity of the binder solution, and the rotation speed during the test is 60 rpm.

[0053] In the embodiments of the present application, the binder can be obtained directly by monomer polymerization or by modifying the side chain of the polymer. The skilled person in the art can determine the method according to the actual production situation. , The polymerization reaction conditions are not limited in the present embodiment, and the polymerization of monomers that can be achieved is sufficient. When the third structural unit is contained, the monomer to be polymerized also includes .

[0054] In some embodiments of the present application, the polymer is modified to obtain the aforementioned binder provided in the embodiments of the present application; wherein, one embodiment is used as an example for explanation: The binder matrix is ​​obtained by free radical polymerization of acrylic acid, acrylonitrile and acrylamide monomers, and then the binder matrix is ​​modified as follows:

[0055] Among them, n1 and n2 are positive integers between 100 and 10000 respectively, and n 3-1 and n 3-2 The sum of is a positive integer between 100 and 1000, and n 3-1 and n 3-2 are also positive integers, R 3-1 -CN, R 3-2 is -CONH2; EDC is 1-ethyl-(3-dimethylaminopropyl)carbodiimide, and DFM is dimethylformamide. The above binder is easily dispersed in water and has good adhesion to negative electrode active materials such as silicon-based negative electrode materials and graphite; wherein silicon-based negative electrode materials include but are not limited to silicon-oxygen negative electrode materials, silicon-carbon composite materials, silicon single substance, etc. It should be noted that the above is only an exemplary synthesis route, and technicians in the field can replace the binder matrix and the reagents needed in the reaction according to actual production needs.

[0056] The embodiment of the present application further provides an electrode plate, comprising a current collector and an active material layer disposed on the current collector, wherein the active material layer comprises the aforementioned binder provided in the embodiment of the present application.

[0057] Due to the use of the binder provided in the embodiment of the present application, the electrode plate has a fluorescence signal at the excitation wavelength corresponding to the binder, and the dispersion of the binder in the active material layer can be detected by detecting the fluorescence distribution of the active material layer; in addition, the electrode plate has good formability and can also achieve better structural stability. Therefore, the electrode plate has high commercial value, and its application in secondary batteries can effectively improve the product yield of secondary batteries.

[0058] In the embodiment of the present application, one side surface of the current collector may have an active material layer, and the active material layer includes the aforementioned binder; or both opposite sides of the current collector may have the aforementioned active material layer, and the active material layer includes the aforementioned binder.

[0059] In some embodiments of the present application, the binder in the electrode plate has a fluorescent signal under visible light excitation. In this case, an optical microscope can be used to monitor the dispersion of the binder in the active material layer, which is more convenient and has high production efficiency.

[0060] In some embodiments of the present application, the electrode plate is a negative electrode plate. In some specific embodiments, the electrode plate includes a current collector and a negative electrode active material layer disposed on the current collector, and the negative electrode active material layer includes the aforementioned binder and the negative electrode active material. In the embodiment of the present application, the negative electrode active material can be any negative electrode active material known in the art that is suitable for the corresponding secondary battery type. For example, the negative electrode active material includes negative electrode active materials with high energy density such as graphite and silicon-based negative electrode materials, or includes other negative electrode active materials with a large cycle volume change rate; wherein, the silicon-based negative electrode material includes silicon-oxygen negative electrode material, silicon-carbon composite material, and silicon element, etc. In this way, the fluorescent signal distribution of the binder can also be used to assist in analyzing the cause of battery failure.

[0061] In the embodiments of the present application, the mass proportion of the binder in the active material layer is not limited, as long as the electrode plate can be formed and the structural stability that meets safety standards can be achieved. In some embodiments, in the active material layer, the mass proportion of the aforementioned binder provided in the embodiments of the present application can be, for example, 0.5%-10%, or 2%-5%.

[0062] In some embodiments of the present application, the active material layer also includes a conductive agent. The present application embodiment does not limit the mass ratio of the conductive agent in the active material layer, nor does it limit the specific type of the conductive agent. Those skilled in the art can choose according to common knowledge and actual production conditions.

[0063] In the embodiments of the present application, the active material layer of the electrode plate is sampled and the presence of the binder is characterized. In some cases, the active material layer can be sampled and dispersed in a reagent, and then subjected to ultrasound, centrifugation, filtration, and dialysis to remove the active material and conductive agent in the active material layer, and then dried and purified to separate the binder, and then infrared or XPS is used to perform structural analysis on the separated binder. The above reagents can be, for example, N-methylpyrrolidone (NMP), acetone, acetonitrile, etc.

[0064] In the embodiment of the present application, the electrode plate also includes a pole ear.

[0065] In some embodiments of the present application, the preparation of the electrode plate includes: S01. Disperse the active material particles, the binder provided by the present application, and the conductive agent in a solvent, mix, and adjust the viscosity to obtain a uniform active material layer slurry; specifically, the fluorescence signal can be used to detect and analyze whether the binder is uniformly dispersed in the slurry. For the negative electrode active material layer slurry, the solvent can be water. The above-mentioned mixing and viscosity adjustment operations can be any process known to technicians in the field.

[0066] S02. Apply a uniform active material layer slurry on the current collector, and obtain an electrode plate by rolling, slitting, baking, and die-cutting. Specifically, the above-mentioned rolling may include a primary rolling and a secondary rolling; lithium supplementation may also be performed after the above-mentioned baking and before die-cutting. The above-mentioned rolling, slitting, baking, die-cutting, and lithium supplementation processes that may be involved may all adopt processes well known to technicians in the field, and this application does not limit this. It can be understood that in any of the above-mentioned processes, the dispersion of the binder can be analyzed by detecting the fluorescent signal.

[0067] The embodiment of the present application also provides a secondary battery, comprising the aforementioned electrode plate provided in the embodiment of the present application, and an electrolyte.

[0068] The secondary battery provided in the embodiment of the present application may be before formation, after formation and capacity expansion, or in any stage of the charge and discharge cycle.

[0069] It can be understood that the secondary battery includes both positive and negative electrodes. The positive electrode active material layer of part or all of the positive electrode sheet may include the binder provided in the embodiments of the present application, and the negative electrode sheet may be a negative electrode sheet known in the art for use with the positive electrode sheet. The negative electrode active material layer of part or all of the negative electrode sheet may include the binder provided in the embodiments of the present application, and the positive electrode sheet may be a positive electrode sheet known in the art for use with the negative electrode sheet. The positive electrode active material of all or part of the positive electrode sheet may include the binder provided in the embodiments of the present application, and the negative electrode active material layer of all or part of the negative electrode sheet may include the aforementioned binder provided in the embodiments of the present application.

[0070] In some embodiments of the present application, the active material layer of the negative electrode sheet in the secondary battery includes the aforementioned binder provided in the embodiments of the present application.

[0071] In the embodiment of the present application, the secondary battery may be a lithium ion battery, or a sodium ion battery or other alkali metal secondary battery.

[0072] In the embodiments of the present application, the secondary battery may be a liquid battery using a liquid electrolyte, a solid-state battery using a solid electrolyte, or a semi-solid-state battery using other electrolyte types such as a gel electrolyte.

[0073] In some embodiments of the present application, when the secondary battery is a liquid battery, the secondary battery includes a positive electrode sheet, a negative electrode sheet, and a separator and an electrolyte located between the positive electrode sheet and the negative electrode sheet.

[0074] In some embodiments of the present application, the secondary battery is a liquid battery, and its preparation includes: The positive electrode sheets and the negative electrode sheets are stacked, and then hot pressed, the tabs are welded, packaged, baked, and the electrolyte is injected. Then, they are left to stand, formed, clamped, shaped, vacuumed, sealed, folded, and divided.

[0075] The embodiment of the present application also provides an electric device, including the secondary battery provided in the embodiment of the present application. Due to the use of the secondary battery provided in the embodiment of the present application, the electric device has a better market prospect.

[0076] In the embodiments of the present application, electrical equipment includes but is not limited to vehicles, consumer electronic products, energy storage systems, etc.; specifically, vehicles include but are not limited to new energy vehicles, rail trains, power-assisted bicycles, etc.; consumer electronic products include but are not limited to mobile phones, laptops, tablet computers, as well as electronic wearable devices such as smart watches and smart glasses.

[0077] The technical solution of the present application is further described below with reference to the embodiments.

[0078] Example 1 The binder matrix is ​​obtained by free radical polymerization of acrylic acid, acrylonitrile and acrylamide monomers, and then the binder matrix is ​​modified as follows:

[0079] Among them, n1 and n2 are positive integers between 100 and 10000 respectively, and n 3-1 and n 3-2 The sum of is a positive integer between 100 and 1000, and n 3-1 and n 3-2 are also positive integers, R 3-1 -CN, R3-2 is -CONH2; EDC is 1-ethyl-(3-dimethylaminopropyl)carbodiimide, and DFM is dimethylformamide.

[0080] The room temperature viscosity of the binder matrix aqueous solution and the binder aqueous solution was tested by a rotational rheometer. The solid content of the binder matrix aqueous solution and the binder aqueous solution was 6wt%, and the test rotation speed was 60 rpm. The room temperature viscosity of the binder matrix aqueous solution was 11000 cps, and the room temperature viscosity of the binder aqueous solution was 10600 cps, indicating that the binder prepared in the embodiment of the present application has excellent bonding performance.

[0081] Fluorescence signal test The adhesive prepared in Example 1 was observed under an optical microscope, and the optical microscope photos at different magnifications are as follows: Figure 1 As shown in A, B, and C in FIG, the optical microscope photograph after exposure to a visible light source for 0.5 seconds is shown in FIG. Figure 1 As shown in a, b, and c.

[0082] The binder prepared in Example 1, the negative electrode active material (specifically, a mixture of silicon carbide and graphite in a mass ratio of 1:8) and the conductive agent (specifically, Super P) were dispersed in water in a mass ratio of 5:90:5, and stirred evenly to obtain a uniform negative electrode slurry; the negative electrode slurry was coated on the current collector, and the negative electrode sheet was obtained by rolling, drying and cutting. The optical photograph of the negative electrode sheet is shown in FIG. Figure 2A As shown, from Figure 2A It can be seen from the figure that the binder provided in the embodiment of the present application has excellent processing performance, and the structure of the prepared negative electrode sheet is complete; the distribution of the fluorescent signal in the negative electrode active layer of the negative electrode sheet is observed using an optical microscope, and the photo after exposure to a visible light source for 0.5 s is as shown in FIG. Figure 2B As shown in the figure, the photos after color adjustment by software are as follows Figure 2C shown.

[0083] The above is an exemplary embodiment of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made thereto without departing from the principles of the present application. These improvements and modifications are also considered to be within the scope of protection of the present application.

Claims

1. A binder, characterized in that: The binder is a polymer; the binder includes a fluorescent structural unit as shown in formula (I) and a viscous structural unit as shown in formula (II): Formula (I), Formula (II); Among them, R 11 is a single bond, any one of an alkylene group, an ester group, an ether bond, a ketocarbonyl group, and an amide bond; R 12 is a fluorescent group; R2 is a group having adhesiveness.

2. The adhesive according to claim 1, characterized in that The fluorescent group includes any one of a substituted or unsubstituted benzofuran group, an isothiocyanate-containing group, a substituted or unsubstituted anthraquinone group, a naphthalenesulfonic acid-containing group, a substituted or unsubstituted pyridine group, a substituted or unsubstituted thiophene group, a substituted or unsubstituted indole group, a substituted or unsubstituted acridine group, and a substituted or unsubstituted rhodamine group.

3. The adhesive according to claim 2, characterized in that The R 12 Through the carbon atom and the R 11 connect.

4. The adhesive according to claim 2, characterized in that The fluorescent group is selected from any one of the structures shown in formula (1-1) to formula (1-19): Formula (1-1), Formula (1-2), (Formula 1-3), Formula (1-4), Formula (1-5), Formula (1-6), Formula (1-7), Formula (1-8), Formula (1-9), Formula (1-10), Formula (1-11), Formula (1-12), Formula (1-13), Formula (1-14), Formula (1-15), Formula (1-16), Formula (1-17), Formula (1-18), Formula (1-19); where Indicates the connection site.

5. The adhesive according to claim 4, characterized in that The fluorescent structural unit comprises .

6. The adhesive according to claim 1, characterized in that The R2 includes -COOH, -COO - A + 、-CONH2、 , -SO3H; wherein A + Including Na + , Li + .

7. The adhesive according to any one of claims 1 to 6, characterized in that: The molar proportion of the fluorescent structural unit in the binder is ≥0.3%.

8. The adhesive according to any one of claims 1 to 6, characterized in that: The molar proportion of the adhesive structural unit in the binder is ≥60%.

9. The adhesive according to any one of claims 1 to 6, characterized in that: In a single molecular chain of the binder, the number of the fluorescent structural units is 100-10000, and the number of the adhesive structural units is 100-10000.

10. The adhesive according to any one of claims 1 to 6, characterized in that: The binder further comprises a third structural unit as shown in formula (III), In formula (III), R3 is selected from any one of a strongly polar group, a hydrogen atom, and a C1-C6 hydrocarbon group; the strongly polar group includes a hydroxyl group or a cyano group.

11. The adhesive according to claim 10, characterized in that In a single molecular chain of the binder, the number of the third structural units is 100-10000.

12. The adhesive according to any one of claims 1 to 6, characterized in that: The binder is a random copolymer or a block copolymer; the number average molecular weight of the binder is 3×10 5 -50×10 5 .

13. The adhesive according to any one of claims 1 to 6, characterized in that: The binder has a fluorescent signal under visible light excitation.

14. An electrode plate, characterized in that: The invention comprises a current collector and an active material layer arranged on the current collector, wherein the active material layer comprises the binder according to any one of claims 1 to 13.

15. A secondary battery, characterized in that: It comprises the electrode plate as claimed in claim 14, and an electrolyte.

16. An electrical equipment, characterized in that: Comprising the secondary battery as claimed in claim 15.

Citation Information

Patent Citations

  • Fluorescent functional monomer, pressure-sensitive adhesive enabling timely detection of coating defects and preparation method of pressure-sensitive adhesive

    CN113735772A

  • Hexamethylene diisocyanate amine ester adhesive containing fluorescent molecular cage as well as preparation method and application of hexamethylene diisocyanate amine ester adhesive

    CN115231983A

  • Water-soluble binder, battery pole piece and application of water-soluble binder

    CN117720869A

  • Conductive binder composition, preparation method thereof, negative electrode paste, secondary battery and electric device

    CN118299568A

  • Adhesive with differential optical properties and its application for substrate processing

    US20060189093A1

Cited By

  • One-day polymer binder for use in electrochemical cells

    DE102024139726A1

  • POLYMER BINDER WITH A MARKING FOR USE IN ELECTROCHEMICAL CELLS

    DE102025100175A1