INS diaphragm and preparation method thereof
By setting the watermark pattern layer between the transparent film layer and the protective layer in the automotive decorative diaphragm, the watermark pattern layer is developed by using the difference in gloss value, the problem of visual conflict between LOGO pattern and decorative pattern is solved, and the decorative beauty and brand are enhanced Image and improves the durability of the diaphragm.
Patent Information
- Application Number
- CN202410975102.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-01
AI Technical Summary
The LOGO patterns and decorative patterns in existing automotive decorative diaphragms often have obvious visual conflicts, affecting the decorative effect.
By setting a watermark pattern layer between the transparent film layer and the protective layer, the watermark pattern layer is developed by using the difference in gloss value, thereby distinguishing it from the decorative pattern, reducing visual conflicts, and introducing brand attributes.
It effectively reduces the visual conflict between the watermark pattern layer and the decorative pattern layer, enhances the decorative beauty and brand image, and improves the durability and mechanical properties of the INS diaphragm.
Smart Images

Figure CN118876874A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of material technology, and in particular to an INS diaphragm and a preparation method thereof. Background Art
[0002] Car interior decoration is the finishing touch in the whole car design. Good decoration design effect can often improve the quality of the whole car, give people a sense of physical and mental pleasure, and increase brand premium. There are many kinds of car decoration technology, and INS film is one of the most commonly used decoration schemes. Usually, new patterns are designed in the decorative pattern layer to obtain new INS film appearance effects, including imitation wood grain patterns, technological patterns, and regular patterns, with different color combinations, presenting ever-changing design effects.
[0003] With the popularization of the Internet and technological advancement, in the digital age, it has become very easy to share and disseminate pictures. In daily life, in order to protect the copyright of images, it is a common practice to add watermarks. Adding watermarks can not only protect copyright and establish brand image, but also increase the beauty of decorative patterns.
[0004] The usual practice is to add a watermark LOGO pattern layer with brand attributes to the decorative pattern layer, but the LOGO pattern and the decorative pattern often produce obvious visual conflicts, affecting the decorative effect. Summary of the invention
[0005] The present application provides an INS film and a preparation method thereof, so as to solve the problem that existing LOGO patterns and decorative patterns often produce obvious visual conflicts and affect the decorative effect.
[0006] In a first aspect, the present application provides an INS membrane, comprising a transparent film layer, a watermark pattern layer, a protective layer and a decorative pattern layer arranged in sequence, wherein:
[0007] The gloss value of the protective layer is 18 to 22;
[0008] The gloss value of the watermark pattern layer is 12-15.
[0009] The present application sets the watermark pattern layer between the protective layer and the transparent film layer, so that the watermark pattern layer can be separated from the decorative pattern layer, reducing the visual conflict of the watermark pattern layer on the decorative pattern layer and reducing the impact on the decorative effect. At the same time, the gloss value of the protective layer is 18 to 22, and the gloss value of the watermark pattern layer is 12 to 15. In this way, there is a gloss difference between the watermark pattern layer and the protective layer, so that the watermark pattern layer is developed through the color difference, thereby distinguishing the watermark pattern from the decorative pattern without distinguishing the watermark from the decorative pattern by lines or colors, and reducing the impact of the watermark pattern layer on the decorative pattern layer. By developing the watermark layer through the difference in color value, brand attributes can be introduced into the INS diaphragm, copyright protection and brand image can be established, and the beauty and visual effect of the decorative pattern can be increased, which is beautiful and practical.
[0010] It should be noted that both the protective layer and the watermark pattern layer are transparent, and the watermark pattern is developed only through the gloss value of the film layer. The development principle of the watermark pattern is through the difference between the gloss of the ink and the PET film. When the LOGO pattern is printed, the corresponding pattern is produced on the PET film. The decorative pattern layer usually has certain colors and lines, which distinguishes it from the watermark pattern layer.
[0011] Gloss value refers to the mirror reflection ability of the surface of an object to light. It is a physical quantity that evaluates the ability of a material surface to reflect light. A high gloss value means a strong surface reflection ability, while a low gloss value means a weak surface reflection ability. Gloss value can be measured by a gloss meter. Generally, the smaller the gloss value, the more matte the material is.
[0012] It should be noted that since the watermark pattern is usually not laid out on the INS membrane as a whole, but only appears in special positions, there are many blank watermark-free areas in the watermark pattern layer. These areas are filled with the material of the protective layer, so that the watermark pattern layer is embedded in the protective layer to be fixed and protected, reducing the wear of the watermark layer.
[0013] In some embodiments, the material of the transparent film layer includes PET. PET material has high light transmittance, strong wear resistance and corrosion resistance, and good processing ductility, which is conducive to the processing of special-shaped INS diaphragms and reduces damage at sharp corners. It should be noted that in other embodiments of the present application, the material of the transparent film layer may also include PMMA, which is suitable for INS diaphragms with regular shapes and no sharp corners. When the material of the transparent film layer is PET, when the INS diaphragm is pasted on the vehicle, the PET transparent film layer is usually torn off as a release layer. When the material of the transparent film layer is PMMA, when the INS diaphragm is pasted on the vehicle, the PMMA transparent film layer is usually attached to the vehicle with the INS diaphragm and does not need to be torn off. PET material refers to polyethylene terephthalate, which is a thermoplastic polyester plastic. PMMA material refers to polymethyl methacrylate, commonly known as acrylic or plexiglass.
[0014] In some embodiments, the material of the watermark pattern layer includes transparent ink and matte powder. By adding matte powder to the transparent ink, the gloss value of the watermark pattern layer after the material forms the watermark pattern layer can be reduced, and the development effect of the watermark layer can be improved. The transparent ink can be Siegwerk 770-9515LM, and the matte powder can be Degussa TS100.
[0015] In some embodiments, the matte powder accounts for 8% to 12% of the material of the watermark pattern layer by mass. When the matte powder accounts for 8% to 12% of the material of the watermark pattern layer by mass, the gloss value of the watermark pattern layer can be controlled to 12 to 15, thereby improving the development effect of the watermark layer.
[0016] In some embodiments, the decorative pattern layer further includes an adhesive layer and a substrate layer disposed in sequence on the side away from the protective layer, wherein the material of the substrate layer includes ABS. The use of ABS material can significantly improve the performance of the INS diaphragm, improve the durability of the INS diaphragm, enhance the mechanical properties, and optimize the processing performance. ABS refers to acrylonitrile-butadiene-styrene copolymer, which is a thermoplastic polymer structural material with high strength, good toughness, and easy processing and molding. It is copolymerized by three monomers of acrylonitrile (Acrylonitrile), butadiene (Butadiene) and styrene (Styrene), and has high hardness, good toughness and excellent processing and molding characteristics.
[0017] In a second aspect, the present application provides a method for preparing an INS diaphragm, which is used to prepare the INS diaphragm of the first aspect, comprising the following steps:
[0018] S10, printing a watermark pattern slurry on the transparent film layer to obtain a watermark pattern layer;
[0019] S20, printing a protective layer slurry on the watermark pattern layer to obtain a protective layer;
[0020] S30, printing a decorative pattern layer slurry on the protective layer to obtain an INS membrane;
[0021] Wherein, the gloss value of the protective layer is 18 to 22;
[0022] The gloss value of the watermark pattern layer is 12-15.
[0023] By printing the watermark pattern layer between the protective layer and the transparent film layer, the watermark pattern layer can be separated from the decorative pattern layer, reducing the visual conflict of the watermark pattern layer on the decorative pattern layer and reducing the impact on the decorative effect. At the same time, the gloss value of the protective layer is 18 to 22, and the gloss value of the watermark pattern layer is 12 to 15. In this way, there is a gloss difference between the watermark pattern layer and the protective layer, so that the watermark pattern layer is developed through the color difference, thereby distinguishing the watermark pattern from the decorative pattern, without distinguishing the watermark from the decorative pattern by lines or colors, and reducing the impact of the watermark pattern layer on the decorative pattern layer. By developing the watermark layer through the difference in color value, brand attributes can be introduced into the INS film, copyright protection and brand image can be established, and the beauty and visual effect of the decorative pattern can be increased, which is beautiful and practical.
[0024] In some embodiments, the step of printing a watermark pattern slurry on the transparent film layer to obtain a watermark pattern layer comprises:
[0025] The watermark pattern is carved into a flower roller, the slurry of the watermark pattern layer is coated on the flower roller, and the watermark pattern slurry is printed on the transparent film layer to obtain the watermark pattern layer.
[0026] Since the watermark pattern is usually not laid out on the INS film as a whole but only appears in a special position, the watermark pattern layer is obtained by carving the watermark pattern into a flower roller, coating the slurry of the watermark pattern layer on the flower roller, and printing the watermark pattern slurry on the transparent film layer. In this way, a lot of blank watermark-free areas can be obtained in the watermark pattern layer. These areas are filled with the material of the protective layer, so that the watermark pattern layer is embedded in the protective layer to be fixed and protected, thereby reducing the wear of the watermark layer.
[0027] In some embodiments, the watermark pattern is engraved into a flower roller, a slurry of the watermark pattern layer is coated on the flower roller, and the watermark pattern slurry is printed on the transparent film layer, so that the watermark pattern layer is printed in a manner including gravure printing. Gravure printing has the characteristics of bright and saturated colors, strong three-dimensional sense, strong light resistance, good anti-counterfeiting performance, and high production efficiency, and can further improve the service life and anti-counterfeiting performance of the watermark layer of the INS membrane.
[0028] In some embodiments, the step of printing the decorative pattern layer slurry on the protective layer to obtain the INS film comprises:
[0029] S301, printing a decorative pattern layer slurry on the protective layer to obtain a decorative pattern layer;
[0030] S302, printing a bonding layer slurry on the decorative pattern layer to obtain a bonding layer;
[0031] S303, compounding the substrate layer material on the bonding layer to obtain an INS membrane.
[0032] In some embodiments, the material of the transparent film layer includes PET, which has high light transmittance, strong wear resistance and corrosion resistance, and good processing ductility, which is conducive to the processing of special-shaped INS diaphragms and reduces damage at sharp corners; and / or,
[0033] The material of the watermark pattern layer includes transparent ink and matte powder. By adding matte powder to the transparent ink, the gloss value of the watermark pattern layer after the material forms the watermark pattern layer can be reduced, and the development effect of the watermark layer can be improved. The transparent ink can be Siegwerk 770-9515LM, and the matte powder can be Degussa TS100. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0035] Figure 1 It is a schematic diagram of the structure of the INS diaphragm of the prior art of this application.
[0036] Figure 2 Schematic diagram of the structure of an INS diaphragm according to an embodiment of the present application.
[0037] Figure 3 This is a schematic structural diagram of an INS diaphragm according to another embodiment of the present application.
[0038] Figure 4 FIG. 4 is a flow chart of a method for preparing an INS membrane according to an embodiment of the present application.
[0039] Figure 5 This is a flow chart of a method for preparing an INS membrane according to another embodiment of the present application.
[0040] Description of Figure Numbers:
[0041] 100INS film; 1 transparent film layer; 2 watermark pattern layer; 3 protective layer; 4 decorative pattern layer; 5 adhesive layer; 6 substrate layer. DETAILED DESCRIPTION
[0042] In order to make the purpose, technical solution and advantages of the present application clearer, the technical solution of the present application will be clearly and completely described below in combination with the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present application.
[0043] In order to meet the carbon neutrality goal, it is necessary to develop zero-carbon or low-carbon fuel internal combustion engines to meet the needs of different application scenarios. Ammonia, as a zero-carbon fuel and hydrogen-rich carrier, is gaining more and more attention. Without changing the engine structure, combining ammonia fuel with other highly active fuels and using highly active fuels to ignite the internal combustion engine is a more feasible technical solution. Oil filtration is a sub-application with lower filtration accuracy requirements and the highest aging resistance requirements among various automotive or mechanical oil filtration.
[0044] Car interior decoration is the finishing touch in the whole car design. Good decoration design effect can often improve the quality of the whole car, give people a sense of physical and mental pleasure, and increase brand premium. There are many kinds of car decoration technology, and INS film is one of the most commonly used decoration schemes. Usually, new patterns are designed in the decorative pattern layer to obtain new INS film appearance effects, including imitation wood grain patterns, technological patterns, and regular patterns, with different color combinations, presenting ever-changing design effects.
[0045] With the popularization of the Internet and technological advancement, in the digital age, it has become very easy to share and disseminate pictures. In daily life, in order to protect the copyright of images, it is a common practice to add watermarks. Adding watermarks can not only protect copyright and establish brand image, but also increase the beauty of decorative patterns.
[0046] like Figure 1 As shown, the structure of a common INS film is a transparent film layer, a protective layer, a watermark layer, a decorative pattern layer, an adhesive layer and a substrate layer arranged in sequence. The watermark layer is printed on the decorative pattern, and the LOGO is reflected by color lines. However, the LOGO pattern with color and lines often produces obvious visual conflicts with the decorative pattern, affecting the decorative effect.
[0047] In view of this, the present application provides an INS membrane and a preparation method thereof to solve the problem that existing LOGO patterns and decorative patterns often produce obvious visual conflicts, thereby affecting the decorative effect.
[0048] like Figure 2 As shown, in the first aspect, the present application provides an INS membrane 100, comprising a transparent film layer 1, a watermark pattern layer 2, a protective layer 3 and a decorative pattern layer 4 arranged in sequence, wherein:
[0049] The gloss value of the protective layer 3 is 18 to 22;
[0050] The gloss value of the watermark pattern layer 2 is 12-15.
[0051] The present application sets the watermark pattern layer 2 between the protective layer 3 and the transparent film layer 1, so that the watermark pattern layer 2 can be separated from the decorative pattern layer 4, reducing the visual conflict of the watermark pattern layer 2 on the decorative pattern layer 4 and reducing the impact on the decorative effect. At the same time, the gloss value of the protective layer 3 is 18-22, and the gloss value of the watermark pattern layer 2 is 12-15, so that there is a gloss difference between the watermark pattern layer 2 and the protective layer 3, so that the watermark pattern layer 2 is developed through the color difference, thereby distinguishing the watermark pattern from the decorative pattern, without distinguishing the watermark from the decorative pattern by lines or colors, and reducing the impact of the watermark pattern layer 2 on the decorative pattern layer 4. By developing the watermark layer through the difference in color value, brand attributes can be introduced into the INS diaphragm 100, copyright protection and brand image can be established, and the beauty and visual effect of the decorative pattern can be increased, which is beautiful and practical.
[0052] It should be noted that the protective layer 3 and the watermark pattern layer 2 are both transparent, and the watermark pattern is developed only through the gloss value of the film layer. The development principle of the watermark pattern is through the difference between the gloss of the ink and the PET film. When the LOGO pattern is printed, a corresponding pattern is produced on the PET film. The decorative pattern layer 4 usually has certain colors and lines, so as to distinguish it from the watermark pattern layer 2.
[0053] Gloss value refers to the mirror reflection ability of the surface of an object to light. It is a physical quantity that evaluates the ability of a material surface to reflect light. A high gloss value means a strong surface reflection ability, while a low gloss value means a weak surface reflection ability. Gloss value can be measured by a gloss meter. Generally, the smaller the gloss value, the more matte the material is.
[0054] It should be noted that, since the watermark pattern is usually not laid on the INS diaphragm 100 as a whole, but only appears in special positions, there are many blank watermark-free areas in the watermark pattern layer 2, and these areas are filled with the material of the protective layer 3, so that the watermark pattern layer 2 is embedded in the protective layer 3 to be fixed and protected, reducing the wear of the watermark layer.
[0055] It should be noted that the gloss value of the protective layer 3 can be achieved by mapping the gloss value of the transparent film layer 1. To achieve a gloss value of 18 to 22 for the protective layer 3, it is necessary to select a transparent film layer 1 with a gloss value of 18 to 22. The matte pattern formed on the surface of the transparent film layer 1 with a gloss value of 18 to 22 is mapped to the protective layer 3 formed by the ink slurry of the transparent protective layer 3 when the ink slurry of the transparent protective layer 3 is coated. In this way, after the transparent film layer 1 is torn off, its matte effect remains on the protective layer 3, thereby achieving control of the matte value of the protective layer 3.
[0056] The glossiness value of the protective layer 3 includes, but is not limited to, 18, 19, 20, 21 or 22. The glossiness value of the watermark pattern layer 2 includes, but is not limited to, 12, 13, 14 or 15.
[0057] In combination with the first aspect, in some embodiments provided in the present application, the material of the transparent film layer 1 includes PET. PET material has high light transmittance, strong wear resistance and corrosion resistance, and good processing ductility, which is conducive to the processing of special-shaped INS diaphragm 100 and reduces damage at sharp corners. It should be noted that in other embodiments of the present application, the material of the transparent film layer 1 may also include PMMA, which is suitable for INS diaphragms 100 with regular shapes and no sharp corners. When the material of the transparent film layer 1 is PET, when the INS diaphragm 100 is pasted on the vehicle, the PET transparent film layer 1 is usually torn off as a release layer. When the material of the transparent film layer 1 is PMMA, when the INS diaphragm 100 is pasted on the vehicle, the PMMA transparent film layer 1 is usually attached to the vehicle with the INS diaphragm 100, and there is no need to tear it off. PET material refers to polyethylene terephthalate, which is a thermoplastic polyester plastic. PMMA material refers to polymethyl methacrylate, commonly known as acrylic or plexiglass.
[0058] In combination with the first aspect, in some embodiments provided in the present application, the material of the watermark pattern layer 2 includes transparent ink and matte powder. By adding matte powder to the transparent ink, the gloss value of the watermark pattern layer 2 after forming the watermark pattern layer 2 can be reduced, and the development effect of the watermark layer can be improved, wherein the transparent ink can be Siegwerk 770-9515LM, and the matte powder can be Degussa TS100.
[0059] In combination with the first aspect, in some embodiments provided in the present application, the mass proportion of the matte powder in the material of the watermark pattern layer 2 is 8% to 12%. When the mass proportion of the matte powder in the material of the watermark pattern layer 2 is within this range, the gloss value of the watermark pattern layer 2 can be controlled to be 12 to 15, thereby improving the development effect of the watermark layer. The mass proportion of the matte powder in the material of the watermark pattern layer 2 includes, but is not limited to, 8%, 9%, 10%, 11% or 12%.
[0060] like Figure 3As shown, in combination with the first aspect, in some embodiments provided in the present application, the decorative pattern layer further includes an adhesive layer 5 and a substrate layer 6 disposed in sequence on the side away from the protective layer 3, wherein the material of the substrate layer 6 includes ABS. The use of ABS material can significantly improve the performance of the INS diaphragm 100, improve the durability of the INS diaphragm 100, enhance the mechanical properties, and optimize the processing performance. ABS refers to acrylonitrile-butadiene-styrene copolymer, which is a thermoplastic polymer structural material with high strength, good toughness, and easy processing and molding. It is copolymerized by three monomers of acrylonitrile (Acrylonitrile), butadiene (Butadiene) and styrene (Styrene), and has high hardness, good toughness and excellent processing and molding characteristics.
[0061] like Figure 4 As shown, in a second aspect, the present application provides a method for preparing an INS diaphragm 100, which is used to prepare the INS diaphragm 100 of the first aspect, comprising the following steps:
[0062] S10, printing a watermark pattern slurry on the transparent film layer 1 to obtain a watermark pattern layer 2;
[0063] S20, printing a protective layer 3 slurry on the watermark pattern layer 2 to obtain a protective layer 3;
[0064] S30, printing the slurry of the decorative pattern layer 4 on the protective layer 3 to obtain the INS membrane 100;
[0065] Wherein, the gloss value of the protective layer 3 is 18 to 22;
[0066] The gloss value of the watermark pattern layer 2 is 12-15.
[0067] By printing the watermark pattern layer 2 between the protective layer 3 and the transparent film layer 1, the watermark pattern layer 2 can be separated from the decorative pattern layer 4, reducing the visual conflict of the watermark pattern layer 2 on the decorative pattern layer 4 and reducing the impact on the decorative effect. At the same time, the gloss value of the protective layer 3 is 18-22, and the gloss value of the watermark pattern layer 2 is 12-15, so that there is a gloss difference between the watermark pattern layer 2 and the protective layer 3, so that the watermark pattern layer 2 is developed through the color difference, thereby distinguishing the watermark pattern from the decorative pattern, without distinguishing the watermark from the decorative pattern by lines or colors, and reducing the impact of the watermark pattern layer 2 on the decorative pattern layer 4. By developing the watermark layer through the difference in color value, brand attributes can be introduced into the INS diaphragm 100, copyright protection and brand image can be established, and the beauty and visual effect of the decorative pattern can be increased, which is beautiful and practical.
[0068] In combination with the second aspect, in some embodiments provided in the present application, the watermark pattern slurry is printed on the transparent film layer 1 to obtain the watermark pattern layer 2, comprising:
[0069] The watermark pattern is engraved into a flower roller, the slurry of the watermark pattern layer 2 is coated on the flower roller, and the watermark pattern slurry is printed on the transparent film layer 1 to obtain the watermark pattern layer 2.
[0070] Since the watermark pattern is usually not laid out on the INS film 100 as a whole, but only appears at a special position, the watermark pattern layer 2 is obtained by engraving the watermark pattern into a pattern roller, coating the slurry of the watermark pattern layer 2 on the pattern roller, and printing the watermark pattern slurry on the transparent film layer 1. In this way, a lot of blank areas without watermarks can be obtained in the watermark pattern layer 2. These areas are filled with the material of the protective layer 3, so that the watermark pattern layer 2 is embedded in the protective layer 3 to be fixed and protected, thereby reducing the wear of the watermark layer.
[0071] In combination with the second aspect, in some embodiments provided in the present application, the watermark pattern is engraved into a flower roller, the slurry of the watermark pattern layer 2 is coated on the flower roller, and the watermark pattern slurry is printed on the transparent film layer 1, and the printing method of the watermark pattern layer 2 includes gravure printing. Gravure printing has the characteristics of bright and saturated colors, strong three-dimensional sense, strong light resistance, good anti-counterfeiting performance, and high production efficiency, which can further improve the service life and anti-counterfeiting performance of the watermark layer of the INS diaphragm 100.
[0072] like Figure 5 As shown, in combination with the second aspect, in some embodiments provided in the present application, the INS membrane 100 obtained by printing the decorative pattern layer 4 slurry on the protective layer 3 includes:
[0073] S301, printing a slurry of a decorative pattern layer 4 on the protective layer 3 to obtain a decorative pattern layer 4;
[0074] S302, printing a slurry of an adhesive layer 5 on the decorative pattern layer 4 to obtain an adhesive layer 5;
[0075] S303 , compound the material of the substrate layer 6 on the adhesive layer 5 to obtain the INS membrane 100 .
[0076] In combination with the second aspect, in some embodiments provided in the present application, the material of the transparent film layer 1 includes PET. The PET material has high light transmittance, strong wear resistance and corrosion resistance, and good processing ductility, which is conducive to the processing of the special-shaped INS diaphragm 100 and reduces damage at sharp corners.
[0077] In combination with the second aspect, in some embodiments provided in the present application, the material of the watermark pattern layer 2 includes transparent ink and matte powder. By adding matte powder to the transparent ink, the gloss value of the material of the watermark pattern layer 2 after forming the watermark pattern layer 2 can be reduced, and the development effect of the watermark layer can be improved. The transparent ink can be Siegwerk 770-9515LM, and the matte powder can be Degussa TS100.
[0078] In summary, by setting the watermark pattern layer between the protective layer and the transparent film layer, the watermark pattern layer can be separated from the decorative pattern layer, reducing the visual conflict of the watermark pattern layer on the decorative pattern layer and reducing the impact on the decorative effect. At the same time, the gloss value of the protective layer is 18-22, and the gloss value of the watermark pattern layer is 12-15. In this way, there is a gloss difference between the watermark pattern layer and the protective layer, so that the watermark pattern layer is developed through the color difference, thereby distinguishing the watermark pattern from the decorative pattern, without distinguishing the watermark from the decorative pattern by lines or colors, and reducing the impact of the watermark pattern layer on the decorative pattern layer. By developing the watermark layer through the difference in color value, brand attributes can be introduced into the INS membrane, copyright protection and brand image can be established, and the beauty and visual effect of the decorative pattern can be increased, which is beautiful and practical.
[0079] In the description of this specification, the description with reference to the terms "one embodiment / method", "some embodiments / methods", "example", "specific example" or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment / method or example are included in at least one embodiment / method or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment / method or example. Moreover, the specific features, structures, materials or characteristics described may be combined in a suitable manner in any one or more embodiments / methods or examples. In addition, those skilled in the art may combine and combine the different embodiments / methods or examples described in this specification and the features of the different embodiments / methods or examples, unless they are contradictory.
[0080] It should be noted that, in the present application, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that the process, method, article or equipment including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or equipment. In the absence of more restrictions, the elements defined by the sentence "comprise one..." do not exclude the existence of other identical elements in the process, method, article or equipment including the elements. In the present application, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically stipulated.
[0081] The above description is only a specific implementation of the present application, so that those skilled in the art can understand or implement the present application. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present application. Therefore, the present application will not be limited to the embodiments shown herein, but will conform to the widest range consistent with the principles and novel features applied for herein.
Claims
1. An INS diaphragm, characterized in that: It includes a transparent film layer, a watermark pattern layer, a protective layer and a decorative pattern layer arranged in sequence, wherein: The gloss value of the protective layer is 18 to 22; The gloss value of the watermark pattern layer is 12-15.
2. The INS diaphragm according to claim 1, characterized in that: The material of the transparent film layer includes PET.
3. The INS diaphragm according to claim 1, characterized in that: The material of the watermark pattern layer includes transparent ink and matte powder.
4. The INS diaphragm according to claim 3, characterized in that: The matte powder accounts for 8% to 12% by weight of the material of the watermark pattern layer.
5. The INS diaphragm according to claim 1, characterized in that: A bonding layer and a substrate layer are sequentially arranged on the side of the decorative pattern away from the protective layer, wherein the material of the substrate layer includes ABS.
6. A method for preparing an INS membrane according to any one of claims 1 to 5, characterized in that: The following steps are involved: Printing a watermark pattern slurry on the transparent film layer to obtain a watermark pattern layer; Printing a protective layer slurry on the watermark pattern layer to obtain a protective layer; Printing a decorative pattern layer slurry on the protective layer to obtain an INS film; Wherein, the gloss value of the protective layer is 18 to 22; The gloss value of the watermark pattern layer is 12-15.
7. The method for preparing the INS membrane according to claim 6, characterized in that: The watermark pattern slurry is printed on the transparent film layer to obtain the watermark pattern layer, comprising: The watermark pattern is carved into a flower roller, the slurry of the watermark pattern layer is coated on the flower roller, and the watermark pattern slurry is printed on the transparent film layer to obtain the watermark pattern layer.
8. The method for preparing the INS membrane according to claim 7, characterized in that: Printing methods include gravure printing.
9. The method for preparing the INS membrane according to claim 6, characterized in that: The INS membrane obtained by printing the decorative pattern layer slurry on the protective layer comprises: Printing a decorative pattern layer slurry on the protective layer to obtain a decorative pattern layer; Printing a bonding layer slurry on the decorative pattern layer to obtain a bonding layer; The substrate layer material is compounded on the bonding layer to obtain an INS membrane.
10. The method for preparing the INS membrane according to claim 6, characterized in that: The material of the transparent film layer includes PET; and / or, The material of the watermark pattern layer includes transparent ink and matte powder.