Molded resin product, camera, printer, and method of manufacturing molded resin product
By forming protrusions and grooves with specific height distribution on the outer surface of the resin product, using light reflection and curvature differences, the problem that resin molding in the prior art is difficult to achieve brightness, and the brightness effect without coating is achieved and suitable for use in the uncoated. Large-scale production.
Patent Information
- Application Number
- CN202410931556.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2020-04-07
- Filing Date
- 2021-04-02
- Publication Date
- 2024-11-05
AI Technical Summary
In the prior art, it is difficult to achieve the brightness of the outer surface of the resin product through the resin molding method in large-scale production, and there are limitations in uniformity, variation, time, productivity and cost using the coating method.
By forming a plurality of protrusions on the outer surface of the resin product, the histogram indicating its height distribution has two peaks, and a first protrusion and a second protrusion are formed in resin molding by mold design, using light reflection and curvature differences Achieve brightness and avoid differences in reflectivity between different materials.
It is achieved without coating in resin molding, providing the observer with a bright feeling similar to the surface of a coated glass bead or metal sheet mixed with fine glass beads or metal sheets, and can be reproducibly manufactured through mold design, suitable for large-scale production.
Smart Images

Figure CN118893786A_ABST
Abstract
Description
[0001] This application is a divisional application of the invention patent application with the application date of April 2, 2021, application number 202110358825.0, and invention name "Molded resin product, mold, manufacturing device and manufacturing method thereof". Technical Field
[0002] The present invention relates to a molded resin product having a glossiness adjusted on its outer surface by providing a fine surface structure, a method for manufacturing the same, and the like. Specifically, the present invention relates to a molded resin product that gives a bright feeling to an observer. Background Art
[0003] The exterior surfaces of resin components used in housings and casings for various products require highly comfortable designs. Examples of these products include electronic devices such as digital cameras and printers. For example, smoothing the component surface can impart a mirror-like sheen, creating an aesthetically pleasing glossy appearance. Conversely, a matte texture can be achieved by providing visually indistinguishable fine projections and depressions on the component surface.
[0004] Coating the outer surface of molded products has been used as a method to improve the texture of resin products or give them pleasing designs. However, since the coating is applied to each molded product, coating is not necessarily suitable for large-scale production due to factors such as uniformity, variation, time, productivity, and cost.
[0005] Therefore, attempts have been made to design the molding surface of a mold for resin molding so as to improve the texture of the outer surface by resin molding without coating.
[0006] For example, Japanese Patent Laid-Open No. H09-314569 proposes a method of manufacturing a mold for obtaining an embossed product having improved design and scratch resistance.
[0007] In recent years, there has been a desire for diversification in product design, and in some cases, a luxurious exterior surface with a bright feel is desired in order to particularly improve the design. For example, a texture in which glittering dots (i.e., fine areas with high reflectivity) are dispersed on a matte base is preferred as an exterior surface that imparts a sense of understated luxury.
[0008] As a method of imparting such a bright feeling to the outer surface, there is known a method of coating the outer surface of a molded product with a paint mixed with fine glass beads or metal flakes having high reflectivity and minute size.
[0009] However, as mentioned above, processing methods using coatings are not necessarily suitable for large-scale production in terms of uniformity, variation, time, productivity and cost.
[0010] However, by using the mold described in Japanese Patent Laid-Open No. H09-314569, it is possible to produce an embossed product in which fine grooves / protrusions are provided in the grooves of the embossed grooves / protrusions, and a smooth convex surface in which the fine grooves / protrusions are smooth is formed on the protrusions of the embossed grooves / protrusions.
[0011] However, the outer surface of the embossed product manufactured with the mold disclosed in Japanese Patent Laid-Open No. H09-314569 has a texture completely different from that of an outer surface coated with a paint mixed with fine glass beads or metal flakes, and does not provide the observer with a feeling of brilliance close to that given by the coated surface.
[0012] Therefore, it is desired to realize a resin product whose outer surface gives an observer a brightness similar to that of a case where the resin product is coated with a paint mixed with fine glass beads or metal flakes, by resin molding using a mold. Summary of the Invention
[0013] According to one aspect of the present disclosure, a molded resin product includes a plurality of protrusions formed in a predetermined region. A histogram indicating a height distribution of the plurality of protrusions has two peaks with a boundary height serving as a boundary therebetween. When a protrusion having a height equal to or less than the boundary height is a first protrusion among the plurality of protrusions and a protrusion having a height greater than the boundary height is a second protrusion, an arithmetic mean curvature of the first protrusion is smaller than an arithmetic mean curvature of the second protrusion.
[0014] Further features of the present disclosure will become apparent from the following description of exemplary embodiments with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1A is an enlarged schematic perspective view of a portion of an outer surface of a molded resin product according to an embodiment.
[0016] Figure 1B It is along Figure 1A A cross-sectional view taken along line A1-A2.
[0017] Figure 2A 3 is a histogram showing the height distribution of fine protrusions provided on the outer surface of the example.
[0018] Figure 2B It is a histogram from which fluctuations (high-frequency components) of the frequency distribution are removed.
[0019] Figure 3 is an enlarged schematic perspective view of the base surface on which only the first protrusions are provided.
[0020] Figure 4 is a schematic perspective view of an example of a molded resin product of an embodiment.
[0021] Figure 5 : is a diagram showing the result of observing the outer surface of the molded resin product according to the embodiment by using a laser microscope.
[0022] Figure 6 It is a monochrome image represented by normalizing the height distribution of the bumps and converting the height into a shade (grayscale).
[0023] Figure 7 is a black and white binary image in which the second protrusion is represented by white and the other parts are represented by black.
[0024] Figure 8 1 and 2 are diagrams for describing a method of manufacturing a mold according to an embodiment by using a laser processing machine.
[0025] Figure 9A It is a diagram showing the arrangement of an injection molding apparatus.
[0026] Figure 9B It is a diagram showing a mold clamping step.
[0027] Figure 9C It is a diagram showing the injection steps.
[0028] Figure 9D It is a diagram showing a pressure holding step and a cooling step.
[0029] Figure 9E It is a figure which shows the mold opening step and the mold releasing step.
[0030] Figure 10A is an external view of a camera including the molded resin product according to the embodiment.
[0031] Figure 10B is an external view of a printer including the molded resin product according to the embodiment. DETAILED DESCRIPTION
[0032] A molded resin product, a method of manufacturing the molded resin product, a mold, an apparatus including the molded resin product, and the like as embodiments of the present disclosure will be described with reference to the accompanying drawings.
[0033] It should be noted that the exterior surfaces of the molded resin products of the embodiments described below are not necessarily limited to those exposed to the outside of a device's housing or casing. For example, even if a surface is not always visually recognizable to a user, in some cases, if it is visually recognizable when a door, hatch, or lid portion of the device is open, then that surface should be considered an exterior surface. Therefore, in the following description, surfaces of resin parts or resin products that are visually recognizable to a user may sometimes be referred to simply as "exterior surfaces."
[0034] Note that, in the drawings to be referred to in the description of the following embodiments, elements denoted by the same reference numerals are assumed to have the same functions unless otherwise described.
[0035] Molded resin products
[0036] The shape of the outer surface of the molded resin product according to the embodiment, which serves as a predetermined area giving a sense of brightness to an observer, will be described. Figure 1A is a schematic enlarged perspective view of a portion of an outer surface of a predetermined area serving as a molded resin product according to an embodiment, and Figure 1B It is along Figure 1A The cross-sectional view of the outer surface taken along the line A1-A2 of FIG. 1 and FIG. 2 shows its shape. Figure 1A and Figure 1B As shown, according to the embodiment, many fine protrusions are provided on the outer surface. Figure 2A : is a histogram showing the height distribution of fine protrusions provided on the outer surface of the embodiment. The vertical axis of the histogram represents the number of protrusions used as frequency, and the horizontal axis of the histogram represents the protrusion height. In addition, Figure 2B This is done by applying a low-pass filter to Figure 2A A histogram of the frequency distribution is obtained by removing the fluctuation of the frequency distribution (ie, the high-frequency component).
[0037] From the diagram showing the height distribution of the protrusions provided on the outer surface of the molded resin product of the embodiment Figure 2A and Figure 2B , it can be seen that there are two peaks in the histogram. The boundary between the two peaks, that is, the bottom of the valley between the two peaks, will be referred to as height Hx (boundary height). The ridges with a height equal to or less than the boundary height Hx will be collectively referred to as first ridges CV1, and the ridges with a height greater than the height Hx will be collectively referred to as second ridges CV2.
[0038] On the outer surface of the molded resin product of the embodiment, the total number N1 of the first protrusions CV1 is greater than the total number N2 of the second protrusions CV2. Figure 1A As shown, the second convexities CV2 are arranged in a dispersed manner, and each of the second convexities CV2 is roughly surrounded by a plurality of first convexities CV1. The arrangement density of the first convexities CV1 per unit area on the outer surface is higher than the arrangement density of the second convexities CV2.
[0039] Here, for the sake of convenience, Figure 3 The outer surface shape of the molded resin product on which only the first protrusion CV1 is provided is shown in the form of a schematic enlarged perspective view. Figure 3The outer surface shown as having only the first protrusions CV1 will be referred to as the base surface. The base surface is an embossed surface that visually gives a matte feel. The embossed surface is a surface obtained by forming a fine pattern consisting of grooves and protrusions on the surface of a mold (such as a casting mold or a press mold) and transferring this pattern to a molded resin product. The embossed surface is a matte surface without a mirror finish.
[0040] The outer surface of this embodiment has a shape in which second protrusions CV2 higher than the first protrusions CV1 are arranged in a dispersed manner on the base surface. In addition, the curvature radius of the second protrusions CV2 is smaller than the curvature radius of the first protrusions CV1. Here, the curvature radius is the radius of an approximate circle passing through the apex of the protrusion, such as Figure 1B As shown, and in the case where the curvature radius of the second convexity CV2 is R2 and the curvature radius of the first convexity is R1, R1>R2 holds. Figure 1A An embodiment may involve Figure 3 The shape of the base surface of the first protrusions CV1 is such that some of the first protrusions are replaced by second protrusions CV2 having a larger height and a smaller radius of curvature. It should be noted that when the statistics of the protrusion group on the outer surface are studied by using the inverse of the radius of curvature as the curvature, the arithmetic mean curvature spc1 of the first protrusions CV1 is smaller than the arithmetic mean curvature spc2 of the second protrusions CV2, and spc2>spc1 holds.
[0041] The molded resin product of this embodiment, having an outer surface of this shape, can give the observer a brightness similar to that of a surface coated with a paint mixed with fine glass beads or metal flakes. In the case of coating, by dispersing glass beads or metal flakes having high reflectivity in a matte paint and utilizing the difference in reflectivity between the materials, a brightness can be achieved in which glittering spots (i.e., fine areas of high reflectivity) are dispersed on a matte base.
[0042] In contrast, in the outer surface of the present embodiment, by utilizing molding to design the shape of the protrusions formed on the outer surface rather than utilizing the reflectivity difference between different materials, a bright feeling can be achieved in which the shiny spots (i.e., fine areas of high reflectivity) are arranged in a dispersed manner on a matte base.
[0043] Because light reflects so that the angle of incidence and the angle of reflection are equal, the angle distribution of reflected light is wider when the normal to the incident surface has a wider range of angles, such as when the incident surface is curved. For example, if light is incident on a perfectly flat surface such as a mirror at a certain angle of incidence, the light is reflected only in the direction of a certain reflection angle. In contrast, if the incident surface is uneven, the reflection angle is distributed in various directions.
[0044] In addition, in conventional interface reflection, the larger the incident angle, the higher the intensity of the reflected light. That is, when the surface has undulations, the diffusion of the reflected light increases, and there is an angle at which the reflection intensity is higher.
[0045] The base surface, on which the first protrusions CV1 have a relatively large radius of curvature, diffuses light more than a flat or mirrored surface, thus giving it a matte feel. Furthermore, by distributing second protrusions CV2 having a greater height and a smaller radius of curvature than the first protrusions CV1 in a dispersed manner on the base surface, a bright feeling can be achieved in which sparkling points are dispersed against a matte background.
[0046] The intensity of the specular reflection component is controlled by forming the base surface into an embossed surface with portions having a large radius of curvature. Furthermore, by distributing protrusions with a greater height and a smaller radius of curvature than the base surface, the base surface is imbued with glittering spots that have higher reflection intensity and diffuse light over a wider angle range. The differences in reflection intensity and diffusion angle between the base surface and the glittering spots create a bright reflection that varies depending on the viewing angle.
[0047] The shape of the outer surface of the molded resin product according to the embodiment can be appropriately set based on the desired brightness, within the range that allows for reproducible production of molded resin products using mold molding. For example, if the ratio of the area occupied by the second protrusions CV2 on the outer surface is less than 5% in plan view, the number of glittering points is too small and the reflection intensity is too low, thus failing to achieve a sufficient brightness. Therefore, it is preferred that the ratio of the area occupied by the second protrusions CV2 on the outer surface be 5% or higher. Meanwhile, if the ratio of the area occupied by the second protrusions CV2 on the outer surface is greater than 40% in plan view, the number of glittering points is too large, and the contrast difference between the base surface and the glittering points becomes insufficient. In this case, the brightness imparted to the observer is reduced, and therefore, the area occupied by the second protrusions CV2 is preferably 40% or less of the outer surface area.
[0048] In addition, regarding the surface roughness of the area where the first protrusion CV1 is formed only on the outer surface, the SPC value is preferably equal to or greater than 10 [1 / mm] and equal to or less than 30 [1 / mm], and the SDR (developed interface area ratio) value is preferably equal to or greater than 0.001 and equal to or less than 0.015.
[0049] Here, the spc value is the arithmetic mean curvature of the ridge line passing through the apex of the protrusion, that is, the average value of the reciprocal of the radius of the approximate circle of the ridge line passing through the apex of the protrusion, and is expressed by the following formula (1). In this formula (1), x and y represent the position on the outer surface in the coordinate system in the plan view, z represents the height direction component of the protrusion at that position, and n represents the number of apexes of the protrusion. A smaller value indicates that the shape of the protrusion is not steep and has a wide amplitude, and a larger value indicates that the shape of the protrusion is sharp and narrow.
[0050] Formula (1)
[0051]
[0052] When the arithmetic mean curvature spc of the base surface is less than 10 [1 / mm], the base surface is approximately a flat surface, and reflection close to specular reflection occurs depending on how light is incident. Meanwhile, when the arithmetic mean curvature spc of the base surface is greater than 30 [1 / mm], the diffuseness and reflection intensity of the base surface increase, so the contrast difference between the base surface and the second protrusions CV2 serving as the glittering points becomes insufficient, and a sense of brightness cannot be achieved.
[0053] Furthermore, sdr is the developed interface area ratio and is expressed by the following formula (2). In formula (2), x and y represent the position on the outer surface in the coordinate system in the plan view, z represents the height direction component of the protrusion at that position, and A represents the area of the defined area. Therefore, the developed interface area ratio sdr indicates how large the surface area is relative to the area of the defined area.
[0054] Formula (2)
[0055]
[0056] A smaller value of the developed interface area ratio sdr indicates that the outer surface is close to a flat surface, and a larger value of sdr indicates that there are many steep surfaces.
[0057] When the SDR of the base surface is less than 0.001, the base surface is approximately flat, and reflection close to specular reflection occurs depending on how light is incident. Meanwhile, when the SDR of the base surface is greater than 0.015, the diffuseness and reflection intensity of the base surface increase, so the contrast difference between the base surface and the second protrusions CV2 serving as the glittering point becomes insufficient, and a bright feeling cannot be achieved.
[0058] In addition, when the shape of the second protrusion CV2 serving as the flash point is statistically studied, the spc value is preferably equal to or greater than 15 [1 / mm] and equal to or less than 100 [1 / mm], and the sdr value is preferably equal to or greater than 0.020 and equal to or less than 0.080.
[0059] When the SPC of the second convex CV2 used as the glittering spot is less than 15 [1 / mm], the reflection intensity of the glittering spot is too low to achieve a sufficient contrast difference from the base surface, thus failing to achieve a sufficient sense of brightness. Meanwhile, when the SPC of the second convex CV2 used as the glittering spot is greater than 100 [1 / mm], the diffusion range of the glittering spot increases, and its function as a glittering spot deteriorates. When the SDR value of the second convex CV2 used as the glittering spot is less than 0.020, the difference between the diffusion at the glittering spot and the diffusion at the base surface becomes too small to achieve a sufficient sense of brightness. Meanwhile, when the SDR value of the second convex CV2 used as the glittering spot is greater than 0.080, although the diffusion and reflection intensity of the glittering spot increases, the reflection intensity becomes too high, causing the observer to perceive a strong sense of graininess from the glittering spot. In this case, the apparent graininess is exaggerated, and the intended texture may not be achieved.
[0060] Furthermore, the spc ratio between the first protrusions CV1, serving as the base surface, and the second protrusions CV2, serving as the sparkling dots, is preferably 1.5 or higher and 10.0 or lower. If the ratio is lower than 1.5, the contrast difference between the base surface and the sparkling dots is too small to achieve a sufficient sense of brightness. If the ratio is higher than 10.0, each sparkling dot becomes smaller, and the intensity of reflected light from the sparkling dots decreases, making them inadequate for use as sparkling dots. According to experiments conducted by the inventors, the spc ratio between the first protrusions CV1, serving as the base surface, and the second protrusions CV2, serving as the sparkling dots, is particularly preferably in the range of 3 to 8.
[0061] Next, Figure 4 1 is a perspective view of an example of a molded resin product according to an embodiment, showing its appearance. The first and second convexities CV1 and CV2 are formed on the surface area 42 of the molded resin product 41 to impart a sense of brightness. Note that since the first and second convexities CV1 and CV2 are very small, for ease of description, Figure 4 This is illustrated by adding a simple texture to the surface area 42 .
[0062] Next, the outer surface shape of the surface region 42 will be described in more detail.
[0063] Figure 5 Results of observing the outer surface of the molded resin product according to the embodiment by using a laser microscope are shown. The laser microscope used here is one of the 3D laser scanning confocal microscopes VK-X series manufactured by KEYENCE Corporation. Figure 5A microscopic image obtained by combining data obtained from a total of 24 measurements is shown, consisting of measurements of four rows and six columns using a 50x microscope lens. Note that Figure 2A The histogram shown in is obtained from Figure 5 The height distribution of the outer surface of the observation result. Therefore, by obtaining the reference Figure 2A and Figure 2B The boundary height Hx described can be obtained from Figure 5 The first and second bumps CV1 and CV2 are each extracted from the image. Once the first and second bumps CV1 and CV2 are obtained, the spc and sdr values of each can be determined using a multi-file analysis application equipped with a laser microscope. In the molded resin product of this example, the spc value of the second bump CV2, which serves as the glittering point, is 80.2, and the sdr value of the second bump CV2 is 0.045. The spc value of the first bump CV1, which serves as the base surface, is 12.3, and the sdr value of the first bump CV1 is 0.004.
[0064] Figure 6 A monochrome image is shown in which the height is expressed by normalizing the height distribution of a large number of protrusions formed on the outer surface and converting the height into shade or grayscale of the image, and a lighter color, ie, a color closer to white, indicates a larger height of the protrusion.
[0065] Figure 7 A black / white binary image is shown, in which the second convex portion CV2 is represented by white, while the other portions are represented by black. That is, Figure 7 Shown by reference Figure 2A and Figure 2B The described method distinguishes between a black / white binary image representing the first and second projections CV1 and CV2. In other words, the white portion represents the glittering point, and the black portion represents the base surface. By calculating the area of each of the white and black portions, the area ratio of the second projections CV2 on the outer surface, which imparts a sense of brightness to the viewer, can be determined, or the area ratio of the glittering point relative to the base surface can be determined. It should be noted that the area ratio of the second projections CV2 on the outer surface, which function as the glittering point, is 14%.
[0066] As described above, in the molded resin product according to the present embodiment, the shape of the protrusions formed on the outer surface is designed by molding using a mold instead of utilizing the reflectivity difference between different materials, thereby achieving a bright feeling in which the shiny spots (i.e., fine areas with high reflectivity) are arranged in a dispersed manner on the matte base.
[0067] mold
[0068] Next, a mold for forming the first and second convexities CV1 and CV2 on the outer surface of the resin material will be described in detail. A first groove for forming the first convexity CV1 and a second groove for forming the second convexity CV2 on the resin are defined in the molding surface of the mold.
[0069] The mold can be made of, for example, stainless steel or aluminum, which is suitable for reproducibly transferring fine shapes to resin. The mold surface of the mold defines grooves for forming the first and second projections CV1 and CV2 by transfer, creating a reverse mold. While such grooves can, in principle, be defined by cutting, sandblasting, or etching, laser machining is particularly preferred for quickly and accurately defining fine grooves.
[0070] Figure 8 This figure is used to describe a method for manufacturing a mold according to an embodiment using a laser processing machine. The laser processing machine 51 includes a laser head 53 capable of emitting laser light 52 for processing, and a processing table 55 on which a mold block 54 serving as a processing target can be placed. The relative positions of the laser head 53 and the mold block 54 can be changed by an X-axis movement mechanism, a Y-axis movement mechanism, and a Z-axis movement mechanism, allowing the laser light 52 used for processing to be irradiated at any position on the mold block 54.
[0071] The laser light emitted from the laser head 53 is converged and focused to a predetermined focal position by an optical system (not shown). Therefore, when irradiating the processing area with laser light, the movement mechanisms of the various axes are driven to maintain a state in which the laser head 53 and the irradiation point are always separated from each other by a focal distance. Furthermore, as a method for reducing the irradiation energy density to control the processed shape (such as the curvature and depth of the groove), laser irradiation can be performed while maintaining a defocused state in which the distance between the laser head 53 and the irradiation point deviates by a certain amount from the focal distance.
[0072] The laser head 53 includes a two-axis galvano scanner and an fθ lens, and can scan the irradiation position at high speed by driving a galvano mirror. Galvano mirror scanning can be performed faster than stage driving, and therefore, from the perspective of reducing processing time, controlling the irradiation position by moving the stage in combination with scanning with the galvano mirror is advantageous.
[0073] As the laser light source for laser processing, a continuous wave laser (CW laser) that continuously irradiates, as well as a pulsed laser that repeatedly irradiates for short periods of time, can be used. In this embodiment, a laser light source with a pulse width on the nanosecond order is preferably used. It is preferable to use a laser whose conditions, such as irradiation intensity, pulse length, and pulse interval, can be arbitrarily selected. For example, a nanosecond pulse laser manufactured by AMPLITUDE SYSTEMS can be used as a laser oscillator. In this embodiment, the wavelength of the laser light used for processing, generated by the nanosecond pulse laser oscillator, was set to 1030 nanometers, the pulse width was set to 30 nanoseconds, and the average output was set to 15 W.
[0074] Laser irradiation is performed by setting irradiation conditions according to the shapes of the first and second grooves for transferring the first and second projections CV1 and CV2 onto the resin material, and thus a large number of grooves are defined in the surface of the mold.
[0075] Manufacturing method
[0076] Next, a method of manufacturing the molded resin product in this embodiment by using the above-mentioned mold will be described. Figures 9A to 9E is a schematic diagram for describing a manufacturing process of a molded resin product according to an embodiment by using an injection molding machine.
[0077] Figure 9A 6 is a schematic diagram showing the arrangement of an injection molding apparatus, and shows molds 61 and 62, a cylinder 63 for injecting resin into the molds, and a hopper 64 for loading the resin material into the cylinder 63. First and second recesses for transferring first projections CV1 and second projections CV2 onto the resin material are defined in the molding surface of the mold 61 and / or the mold 62. In this embodiment, a reinforced polycarbonate resin is used as the resin material, and the reinforced polycarbonate resin is black and has a glass filler mixed therein at approximately 30%.
[0078] The cylinder 63 includes a screw not shown herein, and the screw is rotated by the motor 65 to convey the resin material to the distal end of the cylinder 63. In addition, the cylinder 63 is provided with a heater not shown, and the solid resin material charged from the hopper 64 is melted by being heated to a temperature equal to or higher than its melting point when conveyed to the distal end of the cylinder 63, and is retained in the space in the distal end portion of the cylinder 63.
[0079] Next, execute Figure 9BThe mold clamping step shown in FIG. Molds 61 and 62 are positioned by a moving mechanism (not shown) and then closed to form the cavity. Molds 61 and 62 are also heated by a heater (not shown). Typically, a channel for flowing a high-temperature liquid is defined in the mold, and the mold temperature is regulated by controlling the flow rate and temperature of the liquid. It should be noted that the mold heating temperature in this step will be referred to as the mold temperature.
[0080] Next, execute Figure 9C The injection step shown. The nozzle at the distal end of the cylinder 63 is pressed against the injection hole portion provided in the mold 62. Then, the motor 65 is operated to rotate the screw (not shown), thereby injecting the molten resin 66 into the cavity defined by the molds 61 and 62. It should be noted that the temperature of the molten resin 66 in this step will be referred to as the resin temperature.
[0081] Next, execute Figure 9D The holding pressure step and cooling step are shown. During the holding pressure step, the pressure applied to the molten resin 66 injected into the cavity is maintained at a predetermined value by controlling the oil pressure in cylinder 63. It should be noted that this predetermined pressure value will be referred to as the holding pressure. It should be noted that various values can be selected as the holding pressure to allow the molten resin 66 to fill all corners of the space in the cavity. In other words, applying an appropriate holding pressure to the molten resin 66 allows the resin to be injected into and around the grooves and protrusions on the molding surface of the mold without gaps, thereby forming the first and second protrusions CV1 and CV2 with high shape accuracy.
[0082] In the cooling step after the holding step, Figure 9D A cooling mechanism (not shown in the illustrated arrangement) cools molds 61 and 62, cooling the resin within the cavity to a temperature equal to or lower than the glass transition temperature of the resin and thereby solidifying it. For example, a method of providing a refrigerant passage around the mold and cooling the mold by circulating the refrigerant can be used as the cooling mechanism.
[0083] After the resin in the cavity is solidified, Figure 9E First, in the mold opening step, the mold 61 and / or the mold 62 is moved by a not-shown driving mechanism to separate the molds 61 and 62 from each other.
[0084] In the subsequent demolding step, the molded resin product 67 adhered to one of the molds is separated from the mold by, for example, protruding ejector pins (not shown). Note that, if necessary, the gate mark formed on the removed molded resin product 67, which is a burr left at the injection gate position, can be removed.
[0085] According to the manufacturing method described above, in the present embodiment, it is possible to manufacture a molded resin product on the outer surface of which the first protrusions CV1 and the second protrusions CV2 are formed with high shape accuracy.
[0086] Other embodiments
[0087] It is to be noted that the present disclosure is not limited to the above-described embodiments, and various modifications and combinations are possible within the technical concept of the present disclosure.
[0088] For example, the method for forming the first and second convexities CV1 and CV2 is not limited to the above-mentioned injection molding method, and various types of transfer molding methods that transfer the shape of the mold surface to the resin material may be used. For example, the first and second convexities CV1 and CV2 may be formed on the resin by an appropriate transfer method such as roll molding or press molding.
[0089] In addition, the molded resin product according to the embodiment is not limited to Figure 4 According to the present invention, a sense of brightness can be imparted to molded resin products of various shapes and functions.
[0090] For example, brightness can be given to Figure 10A The outer part 121 of the camera body of the camera shown or the outer part 122 of the lens barrel of the camera. Alternatively, for example, a sense of brightness may be imparted to Figure 10B The external part 131 of the top plate of the printer or the external part 132 of the side surface of the printer is shown. Note that the examples of the camera are not limited to Figure 10A Examples of the printer are shown, and include SLR cameras with interchangeable lenses, mirrorless cameras, compact cameras, and smartphones with image capture functions. In addition, examples of the printer are not limited to Figure 10B The examples shown include various embodiments such as a device having only a printing function, a copier, and a multifunction device having a reading function. Examples of the recording system are not particularly limited and include an electrophotographic system, an inkjet system, and a thermal transfer system.
[0091] Furthermore, the present disclosure is applicable not only to molded resin products for cameras and printers but also to any molded resin product that is desired to be visually perceived by an observer as bright, such as automotive interior parts and cosmetic packaging. The molded resin product may have a thin flat plate shape such as a sheet or film, or a three-dimensional shape with a curved surface, or may have flexibility.
[0092] As the main component of the resin material for molded resin products, for example, thermoplastic resins such as polyethylene, polystyrene, polypropylene, polyvinyl chloride, polyester, polyamide and polycarbonate can be preferably used, but the main component is not limited to these. In addition, although opaque resin materials are preferably used because they give a bright feeling by using surface reflection, the color is not limited. By mixing appropriate pigments into the resin material, the resin material can be colored as needed. In addition, the present disclosure is also applicable to reinforced resins obtained by adding glass fillers or carbon fillers to the resin, as well as functional resins such as conductive resins.
[0093] While the present disclosure has been described with reference to exemplary embodiments, it is to be understood that the present disclosure is not limited to the disclosed exemplary embodiments.The scope of the following claims is to be accorded the broadest interpretation so as to encompass all such modifications and equivalent structures and functions.
Claims
1. A molded resin product comprising: A plurality of protrusions are formed in a predetermined area, the plurality of protrusions include a first protrusion and a second protrusion, the height of the second protrusion is smaller than the height of the first protrusion, An arithmetic mean curvature of the first protrusion is smaller than an arithmetic mean curvature of the second protrusion.
2. The molded resin product according to claim 1, wherein In the predetermined area, an arrangement density of the first protrusions is higher than an arrangement density of the second protrusions.
3. The molded resin product according to claim 1, wherein In the predetermined region, an area occupied by the first protrusion is larger than an area occupied by the second protrusion. 4 . The molded resin product according to claim 1 , wherein the second protrusion occupies 5% to 40% of the area of the predetermined region. 5 . The molded resin product according to claim 1 , wherein an arithmetic mean curvature of the first protrusion is 10 [1 / mm] or more and 30 [1 / mm] or less. 6 . The molded resin product according to claim 1 , wherein an arithmetic mean curvature of the second protrusions is 15 [1 / mm] or more and 100 [1 / mm] or less. 7 . The molded resin product according to claim 1 , wherein a ratio of an arithmetic mean curvature of the second protrusions to an arithmetic mean curvature of the first protrusions is 1.5 or more and 10.0 or less. 8 . The molded resin product according to claim 1 , wherein a developed interface area ratio of the first protrusion is 0.001 or more and 0.015 or less. 9 . The molded resin product according to claim 1 , wherein a developed interface area ratio of the second protrusion is 0.020 or more and 0.080 or less. 10 . The molded resin product according to claim 1 , wherein the second protrusions include a first second protrusion and a second second protrusion, and wherein the first protrusion is provided between the first second protrusion and the second second protrusion.
11. The molded resin product according to claim 1, wherein the second protrusions include a first second protrusion and a second second protrusion, and The first second protrusion and the second second protrusion are in contact with each other. 12 . The molded resin product according to claim 1 , wherein the first protrusion and the second protrusion are disposed on the same plane.
13. The molded resin product according to claim 1, wherein the second protrusions include a first second protrusion and a second second protrusion, and The height of the first second protrusion is different from the height of the second second protrusion. 14 . The molded resin product according to claim 1 , wherein each of the second protrusions is surrounded by the first protrusions.
15. A camera comprising the molded resin product according to claim 1.
16. A printer comprising the molded resin product according to claim 1.
17. A method for manufacturing a molded resin product, the molded resin product having a plurality of protrusions formed in a predetermined area, the plurality of protrusions comprising a first protrusion and a second protrusion, the height of the second protrusion being smaller than the height of the first protrusion, The method comprises: providing a mold, the mold comprising a first groove portion corresponding to the first protrusion and a second groove portion corresponding to the second protrusion; as well as forming the molded resin product by using the mold, The first groove portion and the second groove portion of the mold are defined by laser processing.
18. The method for manufacturing a molded resin product according to claim 17, wherein the first groove portion and the second groove portion of the mold are formed by setting irradiation conditions of a laser processing machine.
19. The method for manufacturing a molded resin product according to claim 17, wherein In the predetermined region, an arithmetic mean curvature of the first protrusions formed in the forming is smaller than an arithmetic mean curvature of the second protrusions formed in the forming.
20. The method for manufacturing a molded resin product according to claim 17, wherein In the predetermined region, an arrangement density of the first protrusions formed in the forming is higher than an arrangement density of the second protrusions formed in the forming.
21. The method for manufacturing a molded resin product according to claim 17, wherein In the predetermined region, an area occupied by the first protrusions formed in the forming is larger than an area occupied by the second protrusions formed in the forming.
22. A method for manufacturing a molded resin product, the molded resin product having a plurality of protrusions formed in a predetermined area, the plurality of protrusions comprising a first protrusion and a second protrusion, the height of the second protrusion being smaller than the height of the first protrusion, The method comprises: providing a mold, the mold comprising a first groove portion corresponding to the first protrusion and a second groove portion corresponding to the second protrusion; as well as forming the molded resin product by using the mold, Wherein, in the molding surface of the mold, an arithmetic mean curvature of the first groove portion is smaller than an arithmetic mean curvature of the second groove portion.