Method for preparing lithium thiocyanate from coking desulfurization waste liquid and lithium hydroxide

By acidizing, filtration, heating and lithium hydroxide reaction in coking desulfurization waste liquid, lithium thiocyanate can be successfully extracted and generated, which solves the problem of large-scale production of lithium thiocyanate and achieves high value Recycling and industrial-grade production.

CN118908242APending Publication Date: 2024-11-08JIANGSU LIAOYUAN ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411205627.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Currently, there is a lack of large-scale production of lithium thiocyanate products that can be used as additives for lithium sulfur battery electrolytes, and there is no relevant literature to report the method of preparing lithium thiocyanate for ammonium thiocyanate. How to make full use of coking desulfurization waste liquid for resource utilization has become Technical issues that need to be solved urgently.

Method used

Acidified by adding dilute sulfuric acid to the coking desulfurization waste solution, then the acidified liquid is formed and ammonia water is added to neutralize excess sulfuric acid, filter and separate the elemental sulfur, then add activated carbon for stirring and heating, distillation under reduced pressure and concentrate and cool, and finally slowly add lithium hydroxide. to produce lithium thiocyanate.

Benefits of technology

It realizes effective extraction of thiocyanate, thiosulfate and sulfate in coking desulfurization waste liquid, and generates lithium thiocyanate that can be used as an electrolyte additive, providing an industrial-grade recycling and production method, which is different from small batches. Hydrate reagent.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of resourceful treatment of coking desulfurization waste liquid, in particular to a method for preparing lithium thiocyanate from coking desulfurization waste liquid and lithium hydroxide, which comprises the following steps: step S1, adding dilute sulphuric acid into the coking desulfurization waste liquid for acidification to obtain acidified liquid; s2, ammonia water is added into the acidizing fluid to neutralize excessive sulfuric acid, and filtrate is obtained; s3, adding activated carbon into the filtrate to obtain secondary filtrate; s4, carrying out reduced pressure distillation and concentration on the secondary filtrate, cooling, and centrifugally extracting ammonium sulfate to obtain primary mother liquor; s5, stirring and heating the primary mother liquor, and performing centrifugal separation to obtain secondary mother liquor; step S6, recycling the secondary mother liquor; according to the method, thiocyanate, thiosulfate and sulfate contained in the coking desulfurization waste liquid are effectively extracted through step-by-step reaction, meanwhile, lithium hydroxide is introduced into the reaction process, and lithium thiocyanate capable of being used as an electrolyte additive is generated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of resource treatment of coking desulfurization waste liquid, and in particular to a method for preparing lithium thiocyanate by utilizing coking desulfurization waste liquid and lithium hydroxide. Background Art

[0002] The national coking output is over 400 million tons, of which 70% of coking plants use HPF wet desulfurization and decyanation process. Because the desulfurization circulating fluid will have various side reactions in the desulfurization and decyanation process to generate thiocyanate, thiosulfate, and sulfate, when the content of side salts is too high, the desulfurization efficiency will be reduced. In order to ensure the desulfurization and decyanation effect, some desulfurization waste liquid will be discharged. About 10,000 tons of waste liquid is discharged every day. The effective treatment of these waste liquids is an inevitable requirement to ensure the healthy development of the coking industry, and the resource utilization of waste liquids is the industry's first choice.

[0003] Lithium-ion batteries have greatly promoted the rapid development of the new energy vehicle industry, so the research on new lithium-ion batteries has also been advancing rapidly, and lithium-sulfur batteries are one of them. According to a study by Jinkwan Jung et al. of the Korea Advanced Institute of Science and Technology in 2023, thiocyanate ions can prevent electrode passivation and are compatible with lithium metal electrodes, and their effect is better than Br − Therefore, the use of lithium thiocyanate as an electrolyte additive can solve the current problems of lithium-sulfur batteries and is a promising development path to promote the commercial application of lithium-sulfur batteries.

[0004] Currently, there is no large-scale supply of lithium thiocyanate products at home and abroad. The lithium thiocyanate on the market is mainly small-batch reagent grade, mostly lithium thiocyanate hydrate. If it is used as an electrolyte additive, it needs to be dehydrated first.

[0005] There is no literature report on the preparation of lithium thiocyanate from ammonium thiocyanate. Therefore, how to make full use of coking desulfurization waste liquid and prepare lithium thiocyanate that can be used as an electrolyte additive is a technical problem that needs to be solved urgently in this field. Summary of the invention

[0006] The present invention provides a method for preparing lithium thiocyanate by utilizing coking desulfurization waste liquid and lithium hydroxide, which solves the technical problem that the existing process cannot produce lithium thiocyanate that can be used as an electrolyte additive on a large scale.

[0007] In order to solve the above technical problems, the present invention provides a method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide, comprising the following steps: step S1, adding dilute sulfuric acid to the coking desulfurization waste liquid for acidification, so that free ammonia in the waste liquid is converted into ammonium sulfate, ammonium thiosulfate is converted into ammonium sulfate, sulfur and sulfur dioxide, sulfur dioxide is absorbed by liquid alkali to generate sodium sulfite, and acidified liquid is obtained; step S2, adding ammonia water to the acidified liquid to neutralize excess sulfuric acid, so that the pH of the acidified liquid is controlled at 7-7.5, and then filtering and separating the acidified liquid. to obtain a primary filtrate; step S3, adding activated carbon to the primary filtrate, stirring, heating and keeping warm for a period of time, and then filtering to remove the activated carbon to obtain a secondary filtrate; step S4, concentrating the secondary filtrate by reduced pressure distillation and cooling, and extracting ammonium sulfate by centrifugation to obtain a primary mother liquor; step S5, stirring and heating the primary mother liquor, slowly adding lithium hydroxide, and after the reaction generates lithium thiocyanate, distilling under reduced pressure, cooling, centrifuging and drying to obtain a finished product of lithium thiocyanate, and centrifuging to obtain a secondary mother liquor; step S6, recycling the secondary mother liquor.

[0008] Furthermore, the coking desulfurization waste liquid is a salt-containing effluent liquid produced by HPF wet desulfurization.

[0009] Furthermore, the acidification in step S1 is specifically to first add a small amount of dilute sulfuric acid to neutralize ammonia in the waste liquid, control the pH at 6.5-7.5, then slowly add dilute sulfuric acid to decompose ammonium thiosulfate, stir for 0.5-1h, and use liquid alkali to absorb sulfur dioxide discharged during the acidification process; wherein the concentration of the dilute sulfuric acid is not higher than 50%; and the molar ratio of sulfuric acid to ammonium thiosulfate in the dilute sulfuric acid is 1-1.1:1.

[0010] Furthermore, the elemental sulfur separated in step S2 can enter the coking sulfur melting system or be used for acid production.

[0011] Furthermore, the mass of the activated carbon in step S3 is 0.3%-1% of the mass of the primary filtrate.

[0012] Furthermore, in step S4: concentration specifically involves concentrating the concentration of the secondary filtrate to 50%-75%; cooling specifically involves lowering the temperature of the secondary filtrate to 30-60°C.

[0013] Furthermore, in step S5, the molar ratio of lithium hydroxide to ammonium thiocyanate in the primary mother liquor is 0.9-1.1:1.

[0014] Furthermore, the reaction temperature after adding lithium hydroxide in step S5 is 70-130°C.

[0015] Furthermore, in step S5: the distillation is specifically to distill and concentrate the primary mother liquor to a concentration of 70%-85%; the cooling is specifically to reduce the temperature of the primary mother liquor to 30-60°C.

[0016] Furthermore, the content of lithium thiocyanate in the finished lithium thiocyanate in step S5 is not less than 98%.

[0017] In another aspect, the present invention further provides lithium thiocyanate, which is obtained by the method for preparing lithium thiocyanate by utilizing coking desulfurization waste liquid and lithium hydroxide as described above.

[0018] The beneficial effect of the present invention is that the method for preparing lithium thiocyanate by utilizing coking desulfurization waste liquid and lithium hydroxide of the present invention effectively extracts thiocyanate, thiosulfate and sulfate contained in the coking desulfurization waste liquid through step-by-step reaction, and simultaneously introduces lithium hydroxide into the reaction process to generate lithium thiocyanate which can be used as an electrolyte additive. While the coking desulfurization waste liquid is recycled and utilized at a high value, it is also different from the existing small-batch hydrate reagents and provides an industrial-grade recycling production method.

[0019] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention are realized and obtained by the structures particularly pointed out in the description.

[0020] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below for detailed description as follows. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution of the present invention will be described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0022] At least one embodiment provides a method for preparing lithium thiocyanate using coking desulfurization waste liquid and lithium hydroxide, comprising the following steps: step S1, adding dilute sulfuric acid to the coking desulfurization waste liquid for acidification, so that free ammonia in the waste liquid is converted into ammonium sulfate, ammonium thiosulfate is converted into ammonium sulfate, sulfur and sulfur dioxide, and sulfur dioxide is absorbed by liquid alkali to generate sodium sulfite to obtain an acidified liquid; step S2, adding ammonia water to the acidified liquid to neutralize excess sulfuric acid, so that the pH of the acidified liquid is controlled at 7-7.5, and then filtering and separating the elemental sulfur in the acidified liquid to obtain a primary filtrate; step S3, adding activated carbon to the primary filtrate, stirring, heating and keeping warm for a period of time, and then filtering to remove the activated carbon to obtain a secondary filtrate; step S4, vacuum distilling and concentrating the secondary filtrate and cooling it, centrifuging to extract ammonium sulfate, and obtaining a primary mother liquor; step S5, stirring and heating the primary mother liquor, slowly adding lithium hydroxide, and after the reaction generates lithium thiocyanate, vacuum distilling, cooling, centrifuging, and drying to obtain a finished product of lithium thiocyanate, and centrifuging to obtain a secondary mother liquor; step S6, recycling the secondary mother liquor.

[0023] In this embodiment, specifically, the coking desulfurization waste liquid is a salt-containing effluent liquid generated by HPF wet desulfurization.

[0024] In this embodiment, specifically, the acidification in step S1 is to first add a small amount of dilute sulfuric acid to neutralize the ammonia in the waste liquid, control the pH at 6.5-7.5, then slowly add dilute sulfuric acid to decompose the ammonium thiosulfate, stir for 0.5-1h, and use liquid alkali to absorb the sulfur dioxide discharged during the acidification process; wherein the concentration of the dilute sulfuric acid is not higher than 50%; and the molar ratio of sulfuric acid to ammonium thiosulfate in the dilute sulfuric acid is 1-1.1:1.

[0025] In this embodiment, specifically, the elemental sulfur separated in step S2 can enter the coking sulfur melting system or be used for acid production.

[0026] In this embodiment, specifically, the mass of the activated carbon in step S3 is 0.3%-1% of the mass of the primary filtrate.

[0027] In this embodiment, specifically, in step S4: concentration specifically involves concentrating the concentration of the secondary filtrate to 50%-75%; cooling specifically involves lowering the temperature of the secondary filtrate to 30-60°C.

[0028] In this embodiment, specifically, the molar ratio of lithium hydroxide to ammonium thiocyanate in the primary mother liquor in step S5 is 0.9-1.1:1.

[0029] In this embodiment, specifically, the reaction temperature after adding lithium hydroxide in step S5 is 70-130°C.

[0030] In this embodiment, specifically, in step S5: distillation specifically includes distilling and concentrating the primary mother liquor to a concentration of 70%-85%; cooling specifically includes lowering the temperature of the primary mother liquor to 30-60°C.

[0031] In this embodiment, specifically, the content of lithium thiocyanate in the finished lithium thiocyanate in step S5 is not less than 98%.

[0032] At least one embodiment provides lithium thiocyanate, which is obtained by the method for preparing lithium thiocyanate using coking desulfurization waste liquid and lithium hydroxide as described above.

[0033] Example 1, 2200g of desulfurization waste liquid was added to a 3L flask, pH 8.6, content: ammonium thiocyanate 15.90%, ammonium thiosulfate 5.20%, ammonium sulfate 3.11%, stirred, and 50.6g of dilute sulfuric acid (concentration 30%) was added in batches to neutralize ammonia, pH 6.8. Then 265g of dilute sulfuric acid was slowly added for 0.5h, and stirring was continued for 45min after adding sulfuric acid. The generated sulfur dioxide was absorbed by liquid alkali. 7.3g of ammonia water (concentration 20%) was added to neutralize excess sulfuric acid, pH 7.3, and filtered to obtain 33g of filter cake (mainly sulfur, ammonium thiocyanate and ammonium sulfate were recovered by washing, and the remaining sulfur could be used for other resource utilization), and 2439g of primary filtrate. Add 7.5 g of activated carbon to the primary filtrate, stir for 0.5 h, and filter with suction to obtain 9.5 g of filter cake and 2436 g of secondary filtrate, with the contents of: 14.28% ammonium thiocyanate, 0.05% ammonium thiosulfate, and 8.00% ammonium sulfate.

[0034] The secondary filtrate was distilled under reduced pressure until the concentration reached about 66%, and the temperature was lowered to 30°C. The kettle liquid was 822.9 g. After centrifugation, 207 g of filter cake was obtained (mainly ammonium sulfate, which was further purified to obtain ammonium sulfate product and ammonium thiocyanate was recovered). The primary mother liquor was 599 g, and the contents were: 55.35% ammonium thiocyanate, 0.18% ammonium thiosulfate, and 0.32% ammonium sulfate.

[0035] Add 599g of the primary mother liquor to a 1L flask, stir and heat to 90°C, drop 1736g of lithium hydroxide aqueous solution (concentration 10%) (the mol ratio of lithium hydroxide to ammonium thiocyanate is 0.95:1), gradually increase the temperature, add and distill while dropping, control the reaction solution to 700-800mL, the reaction temperature is 105-110°C at the end of the dropwise addition, and cool to ≤50°C. Change to vacuum distillation, concentrate to a concentration of about 76%, cool to 50°C, 379.5g of kettle liquid, centrifuge, get 140.4g of filter cake, vacuum dry, get 137g dry basis, lithium thiocyanate content 98.17%, calculated based on the mol number of ammonium thiocyanate in the primary mother liquor, the yield of a single batch of lithium thiocyanate is about 47.5%. 222g of the secondary mother liquor, content: 56.24% lithium thiocyanate, 6.58% ammonium thiocyanate, apply to the next batch of reaction to prepare lithium thiocyanate.

[0036] Example 2, 2200g of desulfurization waste liquid was added to a 3L flask, pH 8.6, content: ammonium thiocyanate 15.90%, ammonium thiosulfate 5.20%, ammonium sulfate 3.11%, stirred, and 50.6g of dilute sulfuric acid (concentration 30%) was added in batches to neutralize ammonia, pH 6.8. Then 265g of dilute sulfuric acid was slowly added for 0.5h, and stirring was continued for 45min after adding sulfuric acid. The generated sulfur dioxide was absorbed by liquid alkali. 6.8g of ammonia water (concentration 20%) was added to neutralize excess sulfuric acid, pH 7.1, and filtered to obtain 32.6g of filter cake (mainly sulfur, ammonium thiocyanate and ammonium sulfate were recovered by washing, and the remaining sulfur could be used for other resource utilization), and 2439.7g of primary filtrate. Add 8.5 g of activated carbon to the primary filtrate, stir for 0.5 h, and filter with suction to obtain 10.8 g of filter cake and 2436 g of secondary filtrate, with the contents of: 14.28% ammonium thiocyanate, 0.05% ammonium thiosulfate, and 8.00% ammonium sulfate.

[0037] The secondary filtrate was distilled under reduced pressure until the concentration reached about 74%, and the temperature was lowered to 40°C. The kettle liquid was 735g, and centrifuged to obtain 205.8g of filter cake (mainly ammonium sulfate, which was further purified to obtain ammonium sulfate product and ammonium thiocyanate was recovered), and 509.2g of primary mother liquor, with contents of 64.83% ammonium thiocyanate, 0.21% ammonium thiosulfate and 0.18% ammonium sulfate.

[0038] Add 509.2g of the primary mother liquor to a 1L flask, stir and heat to 90°C, drop 1838g of lithium hydroxide aqueous solution (concentration 10%) (the mol ratio of lithium hydroxide to ammonium thiocyanate is 1.01:1), gradually increase the temperature, drop and distill, control the reaction solution to 600-700mL, the reaction temperature is 105~115°C at the end of the dropwise addition, and cool to ≤50°C. Change to vacuum distillation, concentrate to a concentration of about 74%, cool to 40°C, kettle liquid 383.7g, centrifuge, get 140.2g of filter cake, vacuum dry, get 136.9g dry basis, lithium thiocyanate content 98.83%, calculated based on the mol number of ammonium thiocyanate in the primary mother liquor, the yield of a single batch of lithium thiocyanate is about 48%. The secondary mother liquor is 226.6g, with the content of 60.20% lithium thiocyanate and 0.04% lithium hydroxide, which is used to prepare lithium thiocyanate with the next batch of reactions.

[0039] In summary, the method for preparing lithium thiocyanate using coking desulfurization waste liquid and lithium hydroxide of the present invention effectively extracts thiocyanate, thiosulfate and sulfate contained in the coking desulfurization waste liquid through step-by-step reaction, and introduces lithium hydroxide into the reaction process to generate lithium thiocyanate that can be used as an electrolyte additive. While the coking desulfurization waste liquid is recycled and utilized at a high value, it is also different from the existing small-batch hydrate reagents and provides an industrial-grade recycling production method.

[0040] In the several embodiments provided in this application, it should be understood that the disclosed systems, devices and methods can be implemented in other ways. The device embodiments described above are only schematic. For example, the division of the units is only a logical function division. There may be other division methods in actual implementation. For example, multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed.

[0041] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.

Claims

1. A method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide, It is characterized in that The steps include: Step S1, adding dilute sulfuric acid to the coking desulfurization waste liquid for acidification, so that free ammonia in the waste liquid is converted into ammonium sulfate, ammonium thiosulfate is converted into ammonium sulfate, sulfur and sulfur dioxide, and sulfur dioxide is absorbed by liquid alkali to generate sodium sulfite to obtain an acidified liquid; Step S2, adding ammonia water to the acidified liquid to neutralize excess sulfuric acid, so that the pH of the acidified liquid is controlled at 7-7.5, and then filtering and separating the elemental sulfur in the acidified liquid to obtain a primary filtrate; Step S3, adding activated carbon to the primary filtrate, stirring, heating and keeping warm for a period of time, and then filtering to remove the activated carbon to obtain a secondary filtrate; Step S4, distilling and concentrating the secondary filtrate under reduced pressure and cooling it, and extracting ammonium sulfate by centrifugation to obtain a primary mother liquor; Step S5, stirring and heating the primary mother liquor, slowly adding lithium hydroxide, and after the reaction generates lithium thiocyanate, performing reduced pressure distillation, cooling, centrifugation, and drying to obtain finished lithium thiocyanate, and centrifugally separating to obtain a secondary mother liquor; Step S6, recycling the secondary mother liquor.

2. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: The coking desulfurization waste liquid is a salt-containing effluent liquid produced by HPF wet desulfurization.

3. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: The acidification in step S1 specifically includes first adding a small amount of dilute sulfuric acid to neutralize the ammonia in the waste liquid, controlling the pH at 6.5-7.5, then slowly adding dilute sulfuric acid to decompose the ammonium thiosulfate, stirring for 0.5-1h, and using liquid alkali to absorb the sulfur dioxide discharged during the acidification process; wherein The concentration of the dilute sulfuric acid is not higher than 50%; The molar ratio of sulfuric acid to ammonium thiosulfate in the dilute sulfuric acid is 1-1.1:

1.

4. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: The mass of the activated carbon in step S3 is 0.3%-1% of the mass of the primary filtrate.

5. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, It is characterized in that In step S4: The concentration is specifically to concentrate the concentration of the secondary filtrate to 50%-75%; The cooling specifically includes lowering the temperature of the secondary filtrate to 30-60°C.

6. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: In step S5, the molar ratio of lithium hydroxide to ammonium thiocyanate in the primary mother liquor is 0.9-1.1:

1.

7. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: The reaction temperature after adding lithium hydroxide in step S5 is 70-130°C.

8. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, It is characterized in that In step S5: The distillation is specifically to distill and concentrate the primary mother liquor to a concentration of 70%-85%; The cooling specifically includes lowering the temperature of the primary mother liquor to 30-60°C.

9. The method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as claimed in claim 1, Features: The content of lithium thiocyanate in the finished lithium thiocyanate in step S5 is not less than 98%.

10. Lithium thiocyanate, It is characterized in that The lithium thiocyanate is obtained by using the method for preparing lithium thiocyanate by using coking desulfurization waste liquid and lithium hydroxide as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Method for extracting sodium thiocyanate from coking desulfurization waste liquid

    CN102259896A

  • Method for recovering thiocyanate from coke oven gas desulfuration and decyanation wastewater

    CN102424401A

  • Desulfurization waste liquid treatment method and treatment system

    CN114956418A

  • Application of lithium thiocyanate as lithium supplement material, lithium ion battery positive plate and preparation method of lithium ion battery positive plate

    CN118039909A

  • Method for recovering ammonium thiocianate

    JP1988282113A