Display panel, preparation method thereof and display device

By coating the sidewalls of the perforated structure of the display panel with a barrier layer and an electrostatic discharge structure, problems such as water and oxygen intrusion, peeling of the light-emitting device layer, and electrostatic induction are solved, thereby improving the high temperature and humidity resistance and lifespan of the display panel.

CN118973322APending Publication Date: 2024-11-15BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411022640.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing display panels are prone to display defects at the junction of the camera device and the display screen, such as water and oxygen intrusion, peeling of the light-emitting device layer, electrostatic induction, and electrochemical reactions, which affect display performance and lifespan.

Method used

A first barrier layer and a second barrier layer are coated on the sidewall of the opening structure of the display panel. The first barrier layer is made of a material that can block cations, and the second barrier layer is made of a hydrophobic conductive material. Combined with the support structure, static charge is released to form a complete encapsulation structure.

Benefits of technology

It effectively blocks water and oxygen intrusion, prevents the peeling of the light-emitting device layer and electrostatic induction, reduces electrochemical corrosion, and improves the high temperature and humidity resistance and lifespan of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973322A_ABST
    Figure CN118973322A_ABST
Patent Text Reader

Abstract

The invention provides a display panel, a preparation method thereof and a display device, belongs to the technical field of display, and can solve the problem that an existing display panel is easily eroded by water and oxygen to generate black spots. The display panel is divided into an installation area and a display area surrounding at least part of the outline of the installation area. The display panel comprises: a substrate; the light-emitting device layer is arranged on the substrate; the light-emitting device layer at least comprises a light-emitting device located in the display area; the opening structure is positioned in the mounting area; the opening structure at least penetrates through the substrate and the light-emitting device layer in the thickness direction of the display panel; the display panel further comprises a first barrier layer covering the side wall of the opening structure. The display panel disclosed by the invention can effectively avoid black spots and has good display quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of display technology, and in particular to a display panel and a preparation method thereof, and a display device. Background Art

[0002] In response to the demand for narrow bezels and high screen-to-body ratio in electronic terminal products, a relatively mature solution currently available is to form a hole on the display screen that matches the size of the camera device, thereby combining the camera device with the display area of ​​the display screen.

[0003] On the other hand, water and oxygen from the outside can easily enter the display screen through the hole, resulting in poor reliability. Therefore, how to improve the structure of the display device to improve the performance, quality and life of the display device is an urgent problem to be solved. Summary of the invention

[0004] The present invention aims to solve at least one of the technical problems existing in the prior art, and proposes a display panel and a manufacturing method thereof, and a display device.

[0005] On the one hand, the present invention provides a display panel, which is divided into an installation area and a display area surrounding at least a partial outline of the installation area; the display panel comprises: a base substrate; a light-emitting device layer, which is arranged on the base substrate; the light-emitting device layer at least includes a light-emitting device located in the display area; an opening structure, which is located in the installation area; the opening structure at least penetrates the base substrate and the light-emitting device layer along the thickness direction of the display panel; the display panel also includes a first barrier layer covering the side wall of the opening structure.

[0006] In some examples, the display panel also includes: a supporting structure located on the side of the base substrate away from the light-emitting device layer; a protective cover plate arranged on the side of the light-emitting device layer away from the base substrate; and a second barrier layer covering the first barrier layer; the opening structure also penetrates the supporting structure; the second barrier layer is in contact with the protective cover plate, extends to the supporting structure through the opening structure, and is electrically connected to the supporting structure.

[0007] In some examples, the support structure includes a backing film and a support layer stacked in sequence in a direction away from the substrate.

[0008] In some examples, the material of the second barrier layer is a hydrophobic conductive material.

[0009] In some examples, the material of the second barrier layer is graphene or carbon nanotubes.

[0010] In some examples, the material of the first barrier layer is selected to be a material capable of blocking the migration of cations.

[0011] In some examples, the display panel further includes a polarizer located in a direction of the light-emitting device layer away from the base substrate; and the opening structure also passes through the polarizer.

[0012] In some examples, the display panel further includes a touch layer located between the polarizer and the light-emitting device layer, and the opening structure also penetrates the touch layer.

[0013] In a second aspect, the present invention provides a display device, which includes the display panel described above.

[0014] In a third aspect, the present invention provides a method for preparing the display panel as described above, the method comprising:

[0015] providing a substrate base plate;

[0016] forming a light-emitting device layer on the base substrate; the light-emitting device layer at least includes a light-emitting device located in the display area;

[0017] forming an opening structure located in the mounting area and penetrating at least the base substrate and the light-emitting device layer in the thickness direction of the display panel;

[0018] A first barrier layer is formed on the sidewall of the open-pore structure; the first barrier layer covers the sidewall of the open-pore structure.

[0019] In some examples, the preparation method further comprises:

[0020] Forming a support structure and attaching it to a side of the base substrate away from the light-emitting device layer; the opening structure also penetrates the support structure;

[0021] forming a second barrier layer covering the first barrier layer;

[0022] A protective cover plate is disposed on a side of the light emitting device layer away from the base substrate; the second barrier layer contacts the protective cover plate, extends to the support structure through the opening structure, and is electrically connected to the support structure.

[0023] In some examples, the first barrier layer and the second barrier layer are formed using the same equipment and process.

[0024] In some examples, forming the support structure includes:

[0025] A support layer is provided, and a back film is formed on a side of the support layer close to the base substrate.

[0026] In some examples, the preparation method further comprises:

[0027] A touch layer is formed on a side of the light emitting device layer away from the base substrate; and the opening structure also penetrates the touch layer.

[0028] In some examples, the preparation method further comprises:

[0029] A polarizer is formed on a side of the touch layer away from the base substrate; and the opening structure also penetrates the polarizer. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present invention but do not constitute a limitation of the present invention. In the accompanying drawings:

[0031] Figure 1A It is a plan view schematic diagram of a display panel in the related art;

[0032] Figure 1B for Figure 1A The schematic diagram of the film structure of the display panel along the AA section is shown;

[0033] Figure 1C for Figure 1A A schematic diagram of a partial film layer structure of a display panel display area is shown;

[0034] Figure 1D for Figure 1A A schematic diagram of a portion of the structure of the blocking area of ​​the display panel is shown;

[0035] Figure 1E for Figure 1A Another schematic diagram showing the structure of a portion of the blocking area of ​​the display panel;

[0036] Figure 2A A schematic diagram showing black spots appearing on the edge of the opening structure of the display panel;

[0037] Figure 2B A schematic diagram showing peeling and black spots on the light-emitting device layer of a display panel;

[0038] Figure 2C A schematic diagram showing the edges of the opening structure of the display panel are illuminated;

[0039] Figure 2D A schematic diagram of electrostatic induction phenomenon occurring in a display panel;

[0040] Figure 2E A schematic diagram showing a structure of an electrolytic cell formed in a display panel;

[0041] Figure 3 It is a schematic plan view of a display panel according to an embodiment of the present disclosure;

[0042] Figure 4A schematic diagram of coating a first barrier layer on the side wall of an open-pore structure;

[0043] Figure 5 is a schematic diagram of coating a second barrier layer on a first barrier layer;

[0044] Figure 6 A schematic diagram of the structure of an electrolytic cell formed in the display panel after the first barrier layer and the second barrier layer are formed;

[0045] The accompanying drawings are marked as follows:

[0046] 10-display panel; 11-opening structure; 12-display area; 13-barrier area; 120-display substrate; 101-base substrate; 124-driving circuit layer; 125-light-emitting device layer; 118-encapsulation layer; 127-touch layer; 128-polarizer; 129-optical adhesive; 180-protective cover; 121-support layer; 122-back film; 102-buffer layer; 105-first gate insulating layer; 108-second gate insulating layer; 103-interlayer dielectric layer; 116-planarization layer; 113-pixel defining part; 132-support part; 118a -first inorganic encapsulation layer; 118b-organic encapsulation layer; 118c-second inorganic encapsulation layer; 104-active layer; 106-gate; 110-source; 111-drain; 112-first electrode; 114a-light-emitting portion; 115-second electrode; 1d-light-emitting device; 130-first electrode plate; 131-second electrode plate; 202-first isolation column; 204-second isolation column; 203-first interception wall; 205-second interception wall; 206-first organic insulating layer; 801-first barrier layer; 802-second barrier layer; 210-support structure. DETAILED DESCRIPTION

[0047] The specific implementation of the present disclosure is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described herein is only used to illustrate and explain the present disclosure, and is not used to limit the present disclosure.

[0048] In order to make the purpose, technical solution and advantages of the embodiments of the present disclosure clearer, the technical solution of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.

[0049] Unless otherwise defined, the technical terms or scientific terms used in the embodiments of the present disclosure should be understood by people with ordinary skills in the field to which the present disclosure belongs. The "first", "second" and similar words used in the present disclosure do not represent any order, quantity or importance, but are only used to distinguish different components. Similarly, "including" or "comprising" and similar words mean that the elements or objects appearing in front of the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0050] As used herein, "parallel" and "perpendicular" include the described situation and the situation similar to the described situation, and the range of the similar situation is within the acceptable deviation range, wherein the acceptable deviation range is determined by a person of ordinary skill in the art taking into account the measurement in question and the error associated with the measurement of a specific quantity (i.e., the limitations of the measurement system). For example, "parallel" includes absolute parallelism and approximate parallelism, wherein the acceptable deviation range of approximate parallelism can be, for example, a deviation within 5°; "perpendicular" includes absolute perpendicularity and approximate perpendicularity, wherein the acceptable deviation range of approximate perpendicularity can also be, for example, a deviation within 5°.

[0051] It will be understood that when a layer or an element is referred to as being on another layer or substrate, it can be directly on the other layer or substrate, or intervening layers may be present between the layer or element and the other layer or substrate.

[0052] Exemplary embodiments are described herein with reference to cross-sectional views and / or plan views that are idealized exemplary drawings. In the drawings, the thickness of layers and regions are exaggerated for clarity. Therefore, variations in shape relative to the drawings due to, for example, manufacturing techniques and / or tolerances are conceivable. Therefore, the exemplary embodiments should not be interpreted as being limited to the shapes of the regions shown herein, but include deviations in shape due to, for example, manufacturing. Therefore, the regions shown in the drawings are schematic in nature, and their shapes are not intended to illustrate the actual shapes of regions of the device, and are not intended to limit the scope of the exemplary embodiments.

[0053] Figure 1A FIG. 1 shows a schematic plan view of a display panel used in a display device in the related art. Figure 1AAs shown, the display panel 10 can be divided into a display area 12 and a mounting area. The display area 12 includes a pixel array. The opening structure 11 located in the pixel array reserves a position for the camera device, so that the camera device can be integrated with the display area 12 through the opening structure 11.

[0054] Figure 1B for Figure 1A FIG. 1 is a schematic cross-sectional view of the display panel 10 along line AA. Figure 1B As shown, the display panel 10 includes a display substrate 120, a back film 122 and a support layer 121 attached below the display substrate 120, and a touch layer 127, a polarizer 128, an optical adhesive 129 and a protective cover plate 180 attached above the display substrate 120. The opening structure 11 runs through all film layers below the protective cover plate 180.

[0055] Figure 1C FIG. 1 is a partial cross-sectional schematic diagram of the display area 12 of the display substrate 120. Figure 1B and Figure 1C As shown, the display substrate 120 may include a base substrate 101 and a buffer layer 102. The display area 12 includes a pixel array for display operation, the pixel array includes a plurality of pixel units arranged in an array, each pixel unit includes a driving circuit layer 124 and a light emitting device layer 125 and the like.

[0056] Specifically, the driving circuit layer 124 includes a thin film transistor and a storage capacitor. Figure 1C The thin film transistor includes an active layer 104, a gate 106, a gate insulating layer (a first gate insulating layer 105 and a second gate insulating layer 108), an interlayer dielectric layer 103, a source 110 and a drain 111 arranged on a substrate 101; wherein the source 110 and the drain 111 may include a single-layer or multi-layer structure formed by a metal material or an alloy material, such as a three-layer metal layer structure such as titanium / aluminum / titanium, molybdenum / aluminum / molybdenum, titanium / copper / titanium or molybdenum / copper / molybdenum. The capacitor structure includes a first electrode 130 and a second electrode 131. wherein the first electrode 130 and the gate 106 are arranged in the same layer, and the second electrode 131 is between the second gate insulating layer 108 and the interlayer dielectric layer 103.

[0057] Continue to refer to Figure 1CThe light-emitting device layer 125 is located in the display area 12, and may include a first electrode 112 and a pixel defining portion 113 sequentially formed on the interlayer dielectric layer 103. It can be understood that the light-emitting device layer 125 also includes a light-emitting portion 114a and a second electrode 115. The first electrode 112, the light-emitting portion 114a and the second electrode 115 form a light-emitting device 1d. In addition, when the thin film transistor is a top-gate type, before the light-emitting device layer 125 is made, a planarization layer 116 may also be made, which is formed between the interlayer dielectric layer 103 and the first electrode 112. The first electrode 112 may be electrically connected to the drain electrode 111 through a metal via, and the first electrode 112 may be an anode, and the anode may be made of materials such as ITO (indium tin oxide), indium zinc oxide (IZO), and zinc oxide (ZnO); the pixel defining portion 113 may cover the planarization layer 116, and the pixel defining portion 113 may be made of an organic material, such as an organic material such as a photoresist, and the portion of the pixel defining portion 113 located in the display area 10a may have a pixel opening exposing the first electrode 112; the light emitting portion 114a is located in the pixel opening and is formed on the first electrode 112, and the light emitting portion 114a may include a small The molecular organic material or polymer molecular organic material may be a fluorescent material or a phosphorescent material, and may emit red light, green light, blue light, or white light, etc.; and, according to different actual needs, in different examples, the light-emitting portion 114a may further include functional layers such as an electron injection layer, an electron transport layer, a hole injection layer, and a hole transport layer; the second electrode 115 covers the light-emitting portion 114a, and the polarity of the second electrode 115 is opposite to the polarity of the first electrode 112; the second electrode 115 may be a cathode, and the cathode may be made of metal materials such as lithium (Li), aluminum (Al), magnesium (Mg), and silver (Ag). In the related art, a support portion 132 may be provided on the side of the pixel defining portion 113 away from the interlayer dielectric layer 103, and the support portion 132 may play a role in supporting the protective film layer (not shown in the figure) to prevent the protective film layer from contacting the first electrode 112 or other wirings, thereby causing the first electrode 112 or other wirings to be easily damaged.

[0058] It should be noted that if Figure 1C As shown, the first electrode 112, the light-emitting portion 114a and the second electrode 115 may constitute a light-emitting device 1d. Among them, the portion of the display device located in the display area 12 may include a plurality of light-emitting devices 1d arranged in an array. In addition, it should be noted that the first electrodes 112 of each light-emitting device 1d are independent of each other, and the second electrodes 115 of each light-emitting device 1d are connected over the entire surface; that is, the second electrode 115 is a whole-surface structure disposed on the display substrate 120, and is a common electrode for multiple display devices.

[0059] like Figure 1B and 1CAs shown, the display substrate 120 also includes an encapsulation layer 118, and the encapsulation layer 118 may include a first inorganic encapsulation layer 118a, an organic encapsulation layer 118b, and a second inorganic encapsulation layer 118c stacked in sequence. The first inorganic encapsulation layer 118a and the second inorganic encapsulation layer 118b may be silicon nitride, silicon oxide, or silicon oxynitride and a stacked structure thereof, and may be made by a chemical vapor deposition process, but not limited thereto, and may also be made by a physical vapor deposition process, etc. The organic encapsulation layer 118b is used to absorb water vapor and flatten, and may be made of materials such as acrylic-based polymers and silicon-based polymers, and may be made by an inkjet printing process, but not limited thereto, and may also be made by a spraying process, etc.

[0060] Although the opening structure 11 can improve the screen-to-body ratio of the display device, it also provides a channel for impurities such as water and oxygen from the outside to enter the display area 12. The light-emitting device layer 125 is prone to progressive black spots under the erosion of water and oxygen, thereby affecting the display function. At the same time, the fluid encapsulation layer 118 is easy to flow into the opening area when encapsulating the display substrate 120, resulting in poor encapsulation reliability.

[0061] In order to solve the above problems in the related art, a relatively mature solution is to form a barrier area 13 between the display area 12 of the display substrate 120 and the opening structure 11, such as Figure 1A As shown, the barrier region 13 surrounds the open cell structure 11 . Figure 1D FIG. 1 is a partial cross-sectional schematic diagram of the barrier region 13. Figure 1D As shown, the barrier area 13 includes a first isolation column 202 , a first interception wall 203 and a second isolation column 204 which are arranged in sequence from the display area 12 to the opening structure 11 , and are all disposed around the opening structure 11 .

[0062] Reference Figure 1D, wherein the first isolation column 202 includes a metal layer structure, which has a notch on at least one side surrounding the opening structure 11, and the first isolation column 202 can disconnect the functional layer formed on the entire surface of the display substrate 120, such as the light-emitting portion 114a and the cathode 115 in the light-emitting device layer 125. The first interception wall 203 includes a stack of multiple insulating layers, which can intercept some functional layers formed in the display area 12, such as the organic encapsulation layer 118b, to prevent them from approaching or entering the opening structure 11. The second isolation column 204 has a similar structure to the first isolation column 202, and also includes a metal layer structure, which has a notch on at least one side surrounding the opening structure 11. Similarly, the second isolation column 204 can also disconnect the functional layer formed on the entire surface of the display substrate 120, thereby achieving a double barrier effect together with the first isolation column 202. In addition, the second isolation column 204 can also prevent the cracks generated when the opening structure 11 is formed from extending to the display area 12. Similarly, the blocking area 13 may also include a second interception wall 205 adjacent to the first interception wall 203. The second interception wall 205 is similar to the first interception wall 203 and includes a stack of multiple insulating layers, which together with the first interception wall 203 achieve a double interception effect. For example, the metal layer structures in the first isolation column 202 and the second isolation column 204 are both arranged in the same layer as the source 110 and the drain 111, that is, they can correspond one to one with the three metal layers of the source 110 and the drain 111 and have the same material. For example, in the direction away from the base substrate 101, the first interception wall 203 includes a first insulating layer and a second insulating layer, wherein the first insulating layer can be arranged in the same layer as the planarization layer 116, and the second insulating layer can be arranged in the same layer as the pixel defining portion 113. For example, in the direction away from the base substrate 101, the second intercepting wall 205 includes three insulating layers, respectively referred to as a third insulating layer, a fourth insulating layer and a fifth insulating layer, wherein the third insulating layer can be arranged on the same layer as the planarization layer 116, the fourth insulating layer can be arranged on the same layer as the pixel defining portion 113, and the fifth insulating layer can be arranged on the same layer as the supporting portion 132.

[0063] Typically, the encapsulation layer 118 encapsulates at least the first isolation column 202, for example, the display area 12 and the first isolation column 202 are encapsulated at the same time. Specifically, the first inorganic encapsulation layer 118a is formed on the entire display substrate 120, and due to the interception effect of the first interception wall 203, the first organic encapsulation layer 118b and the second inorganic encapsulation layer 118c are terminated at the first interception wall 203.

[0064] Before entering the market, display devices need to undergo a "double 85 reliability test", that is, the display devices are stored and operated in an environment with a temperature of up to 85 degrees Celsius and a humidity of up to 85% to verify the quality of the display devices. When the display devices described in the above-mentioned related technologies are operated under such extreme conditions of high temperature and high humidity, the following technical problems may occur, resulting in damage to the optical performance, display function and life of the display devices. Figure 1A-Figure 1D The display panel 10 shown is taken as an example to introduce possible technical problems thereof.

[0065] Question 1:

[0066] When the display panel 10 is placed in a high temperature and high humidity environment, the first isolation column 202 and the second isolation column 204 may fail, and external impurities such as water and oxygen may still enter the light-emitting device layer 125 and the packaging layer 118 through the opening structure 11, causing black spots to appear on the light-emitting portion 114a of the light-emitting device layer 125, resulting in poor display.

[0067] Question 2:

[0068] Figure 2A and Figure 2B FIG. 1 is a schematic diagram showing the peeling of the light emitting device layer 125 to produce black spots. Figure 2A and Figure 2B As shown, under high temperature and high humidity environment, the various film layers of the display panel 10 expand and contract multiple times under cyclic hot and cold shocks. The lateral shear force and longitudinal tensile force generated in this process can easily cause the light-emitting device layer 125 to peel off or fall off, and water and oxygen enter the light-emitting device layer 125 through the gaps caused by the peeling of the light-emitting device layer 125, causing black spots to appear on the light-emitting portion 114 of the light-emitting device layer 125, resulting in poor display.

[0069] Question 3:

[0070] Figure 2C It is a schematic diagram showing that the edge of the open hole structure 11 is bright. Figure 2D Schematic diagram of the induced negative charge generated by the open-pore structure 11 under the action of electrostatics. Figure 2D As shown, the opening structure 11 is prone to generate induced negative charges under the action of static electricity, which makes the threshold voltage V th Negative bias, thus the operating current increases, causing the edge of the opening structure 11 to glow.

[0071] Question 4:

[0072] When the display panel 10 is operated in a high temperature and high humidity environment, the first isolation column 202 and the second isolation column 204 located in the barrier area 13 are both turned on. When the first isolation column 202 and the second isolation column 204 are turned on, an external electric field is formed in the display panel 10 with the second electrode 115 of the light-emitting device layer 125 as the cathode and the edge of the open hole structure 11 as the anode, that is, Figure 2E Taking the second electrode 115 as an example, once the display panel 10 is formed as shown in FIG. Figure 2E In the electrolytic cell shown, the following reactions will occur:

[0073] 1) Water H2O is ionized under an electric field to form OH - and H + ;

[0074] 2) The silver Ag in the anode end of the electrolytic cell or in the display panel 10 material undergoes oxidation reaction to form Ag ions: 2Ag-2e→2Ag + ;

[0075] Afterwards, with OH - Reacts to form Ag2O and water: 2Ag + +2OH - →2AgOH→Ag2O+H2O; Ag2O migrates to the cathode end of the electrolytic cell, i.e., near the display area 12, under the action of the electric field;

[0076] 3) H at the cathode end of the electrolytic cell + Gain electrons and form hydrogen: 2H + +2e→H2↑; at the same time, the Ag2O that migrated to the cathode undergoes a reduction reaction and is reduced to Ag: Ag2O+2e+H2O→Ag+OH - ; Among them, the generated hydrogen easily forms holes in the light-emitting device layer 125, which provide transmission channels for water and oxygen, increasing the speed of water and oxygen invasion; and the Ag single substance generated at the cathode end will further accelerate the speed of the electrochemical reaction, providing positive feedback for water and oxygen invasion;

[0077] 4) In addition, the polarizer 128 material of most display panels 10 contains alkali metal ions. It should be noted that even COE display devices that do not contain polarizer 128 inevitably have alkali metal ions in their materials due to their special display module material requirements. Such ions will migrate rapidly under the action of the electric field, and their migration direction is similar to that of Ag. +The same, all move toward the direction near the display area 12. During their migration, they will react with the encapsulation layer 118, causing the first inorganic encapsulation layer 118a and the second inorganic encapsulation layer 118c to change in quality; at the same time, the alkali metal ions make the electrolytic cell solution alkaline, breaking the balance of the electrolytic cell and causing H2O to be continuously ionized, thereby causing the electrochemical reactions described in 1)-4) above to continue, ultimately corroding the encapsulation layer 118 and causing water and oxygen to invade the light-emitting device layer 125, causing black spots to form.

[0078] In summary, the above problems may cause the optical performance, display function or life of the display panel 10 to be damaged, and therefore need to be solved urgently.

[0079] In order to solve at least one of the above problems, on the one hand, an embodiment of the present disclosure provides a display panel 10 . Figure 3 is a schematic plan view of the display panel 10, Figure 4 FIG. 1 is a partial cross-sectional view of the display panel 10 along line AA.

[0080] like Figure 3 As shown, the display panel 10 is divided into a mounting area and a display area 12 surrounding at least a portion of the mounting area. Figure 4 As shown, the display panel 10 at least includes a display substrate 120. Specifically, the display substrate 120 includes a base substrate 101 and a light-emitting device layer 125 disposed on the base substrate 101 in the thickness direction. The light-emitting device layer 125 includes at least a light-emitting device 1d located in the display area 12. The display panel 10 also includes an opening structure 11 located in the mounting area. The opening structure 11 at least penetrates the base substrate 101 and the light-emitting device layer 125 in the thickness direction of the display panel 10. In addition, as shown in FIG. Figure 4 As shown, the display panel 10 further includes a first barrier layer 801 covering the side wall of the opening structure 11 .

[0081] The embodiment of the present disclosure can solve at least the above-mentioned problems 1 and 2 by coating the first barrier layer 801 on the side wall of the opening structure 11. On the one hand, the first barrier layer 801 coated on the side wall of the opening structure 11 can prevent external impurities such as water and oxygen from entering the light-emitting device layer 125 through the side wall of the opening structure 11; on the other hand, the first barrier layer 801 located on the side wall of the opening structure 11 completely covers the multiple stacked film layers at the opening structure 11, so that the interface of the opening structure 11 is transformed from a multi-film layer interface to a non-film layer interface, thereby preventing the light-emitting device layer 125 from peeling off or falling off due to the lateral shear force and longitudinal tensile force generated by the expansion and contraction of the various film layers of the display panel 10 under the cyclic hot and cold shocks in a high temperature and high humidity environment, and water and oxygen enter the light-emitting device layer 125 through the gaps generated by the peeling, resulting in black spots on the light-emitting portion 114 of the light-emitting device layer 125, causing poor display problems.

[0082] like Figure 4 As shown, the display panel 10 further includes a support structure 210 located on the side of the base substrate 101 away from the light emitting device layer 125 and a protective cover plate 180 arranged on the side of the light emitting device layer 125 away from the base substrate 101 , and the opening structure 11 also passes through the above support structure 210 .

[0083] In some embodiments, Figure 5 As shown, the display panel 10 further includes a second barrier layer 802 covering the first barrier layer 801 , wherein the second barrier layer 802 contacts the protective cover plate 180 , extends to the support structure 210 through the opening structure 11 , and is electrically connected to the support structure 210 .

[0084] The above embodiment can solve at least problem 3 while solving problem 1 and problem 2 by coating the second barrier layer 802 on the first barrier layer 801. That is, on the one hand, the second barrier layer 802 can further avoid problem 1 and problem 2 by having the same function as the first barrier layer 801, which will not be described in detail here; on the other hand, by contacting the second barrier layer 802 with the protective cover plate 180 and extending to the support layer 210 to be electrically connected thereto, the support structure 210 is grounded, so that the static charge on the protective cover plate 180 can be conducted to the support structure 210 through the second barrier layer 802 and released. Figure 5 The direction indicated by the arrow in the middle is the conduction path of the static charge. Therefore, the above embodiment can prevent the opening structure 11 from generating induced negative charges under the action of static electricity, so that the threshold voltage V th Negative bias causes the working current to increase, resulting in the problem of shiny edges of the opening structure 11. On the other hand, compared with the solution of discharging electrostatic charge by setting a wire between the protective cover 180 and the supporting structure 210, the second barrier layer 802 of this embodiment can avoid the physical interference caused by the wire at the edge of the opening structure 11, affecting the installation effect of the components in the installation area (such as the camera module).

[0085] It should be noted that, in some embodiments, the support structure 210 includes a back film 122 and a support layer 121 stacked in sequence in a direction away from the base substrate 101 , wherein the support layer 121 may be a metal bottom plate.

[0086] Of course, the display panel 10 of the embodiment of the present disclosure further includes an encapsulation layer 118 located on the side of the light emitting device layer 125 away from the base substrate 101, and its specific structure and position are as described above ( Figure 1B and Figure 1C), including a first inorganic encapsulation layer 118a, an organic encapsulation layer 118b and a second inorganic encapsulation layer 118c, which will not be described in detail here. The opening structure 11 also penetrates the encapsulation layer 118, specifically, penetrates the first inorganic encapsulation layer 118a formed on the entire surface of the display substrate 120. In addition, there is a barrier area 13 between the opening structure 11 and the display area 12, and the display panel 10 also includes a first isolation column 202 and a second isolation column 204 located in the barrier area 13, and a first interception wall 203 and a second interception wall 205. The structure and number of the isolation columns, and the structure and number of the interception walls in the embodiment of the present disclosure can be as described above (see Figure 1D ), or other situations (for example, including a third barrier wall, etc.), which are not limited in the present application. For example, in some embodiments, the display panel 10 further includes: Figure 1E The first organic insulating layer 206 shown in the figure at least covers the second isolation column 204. For example, the first organic insulating layer 206 is disposed between the second intercepting wall 205 and the opening structure 11. The first organic insulating layer 206 can protect the second isolation column 204, and can also prevent impurities such as water and oxygen from entering the display area 12 from the opening structure 11; in addition, the first organic insulating layer 206 has a certain height. When the display substrate 120 is covered with structures such as the polarizer 128 and the protective cover plate 180, the first organic insulating layer 206 can support the structures such as the polarizer 128 and the protective cover plate 180 around the opening structure 11, and prevent the structures such as the polarizer 128 and the protective cover plate 180 from collapsing in the opening structure 11.

[0087] As a preferred embodiment, the material of the second barrier layer 802 is a hydrophobic conductive material. At this time, the second barrier wall 802 can release static charge while reducing the rate at which water vapor is transmitted along the second barrier layer 802 to the display substrate 120, thereby reducing the oxidation of the first inorganic encapsulation layer 118a, thereby reducing the probability of progressive black spot defects in the light-emitting device layer 125, and improving the quality of the display product.

[0088] The second barrier layer 802 can be a transparent material or a light-shielding material. In some examples, the second barrier layer 802 can be made of a hydrophobic acrylic material containing conductive materials such as carbon black, carbon nanotubes, graphene, and silver. As a preferred embodiment, the material of the second barrier layer 801 is graphene or carbon nanotubes, which can not only realize the extraction of static charges, but also perform light shielding on the open hole structure 11, thereby reducing the influence of ambient light on the thin film transistor characteristics of the driving circuit layer 124, and has a good effect on reducing low grayscale brightness.

[0089] As a preferred embodiment, the material of the first barrier layer 801 is selected from materials that can block the migration of cations, such as an anion exchange membrane or a cation barrier membrane, etc. Specifically, the first barrier layer 801 can be a polymer cation barrier membrane based on polypropylene (PS), polyolefin (PE / PP), polyisobutylene (PIB), etc., or a nanocellulose barrier membrane. Of course, various additives, such as anti-aging agents, etc., can also be added according to actual application scenarios.

[0090] In the above embodiment, the first barrier layer 801 is made of a material that can block the migration of cations, which can also solve the above problem 4. When the display panel 10 of this embodiment is operated in a high temperature and high humidity environment, the first isolation column 202 and the second isolation column 204 are turned on. At this time, the second electrode 115 of the light-emitting device layer 125 is still the cathode of the electrolytic cell, and the anode of the electrolytic cell is the second barrier layer 802, wherein the second barrier layer 802 is grounded and has a low potential (0V). Water H2O is ionized in the electrolytic cell: In the region between the first barrier layer 801 and the cathode (the second electrode 115), H + Directed migration toward the cathode, OH - In the region between the anode (second barrier layer 802) and the first barrier layer 801, since the first barrier layer has selective permeability, that is, cations are not allowed to pass through the first barrier layer 801 and move toward the cathode (second electrode 115), the cations (e.g., K + 、Ag + , H + The cations (such as Ag) cannot migrate through the first barrier layer 801 to the cathode, and the various reactions that occur at the cathode end of the electrolytic cell as described in question 4 will not occur at the cathode end of the electrolytic cell. For example, since the cations cannot migrate to the cathode end of the electrolytic cell, the chemical reaction described in point 3) of question 4 will not occur at the cathode end of the electrolytic cell, that is, more Ag will not be produced at the cathode end to accelerate the electrochemical reaction. More importantly, avoid the K in the material + By moving the first barrier layer 801 toward the encapsulation layer 118, the electrochemical reaction in point 4) of question 4 can be avoided, that is, the alkali metal ions can be prevented from reacting with the first inorganic encapsulation layer 118a and the second inorganic encapsulation layer 118c, thereby causing the first inorganic encapsulation layer 118a and the second inorganic encapsulation layer 118c to undergo qualitative changes; at the same time, the alkali metal ions are prevented from breaking the balance of the electrolytic cell, thereby not accelerating the electrochemical reaction. In short, this embodiment uses a material that can block cations as the first barrier layer 801, which can effectively prevent water and cations from electrochemically corroding the encapsulation layer 118, causing the encapsulation layer 118 to fail, thereby effectively preventing the light-emitting device layer 125 from having progressive black spots.

[0091] In some examples, the display panel 10 further includes a touch layer 127 and a polarizer 128 located in a direction of the light emitting device layer 125 away from the base substrate 101, such as Figure 4 and Figure 5 As shown, the touch layer 127 is located between the light emitting device layer 125 and the polarizer 128. In addition, there is an optical glue 129 between the protective cover 180 and the polarizer 128. The opening structure 11 also penetrates the touch layer 127, the polarizer 128 and the optical glue 129.

[0092] In short, the display panel provided by the embodiment of the present disclosure can achieve at least the following beneficial effects compared with the prior art:

[0093] 1. By coating the first barrier layer 801 on the side wall of the open hole structure 11, on the one hand, it can physically prevent external impurities such as water and oxygen from entering the light-emitting device layer 125 through the side wall of the open hole structure 11; on the other hand, the first barrier layer 801 located on the side wall of the open hole structure 11 completely covers the multiple stacked film layers at the open hole structure 11, so that the interface of the open hole structure 11 is transformed from a multi-film layer interface to a non-film layer interface, thereby preventing the lateral shear force and longitudinal tensile force generated by the expansion and contraction of each film layer of the display panel 10 under the cyclic hot and cold shock under high temperature and high humidity environment, causing the light-emitting device layer 125 to peel off or fall off, and water and oxygen enter the light-emitting device layer 125 through the gaps generated by the peeling, resulting in black spots on the light-emitting portion 114 of the light-emitting device layer 125, causing poor display problems;

[0094] 2. By coating the second barrier layer 802 on the first barrier layer 801, on the one hand, it is possible to further isolate water and oxygen from entering the light-emitting device layer from the open-pored structure 11, and to prevent the light-emitting device layer 125 from being subjected to stress shedding caused by thermal expansion and contraction, thereby causing progressive black spots; on the other hand, the static charge on the protective cover plate 180 can be conducted to the support structure 210 through the second barrier layer 802 for release, thereby preventing the open-pored structure 11 from generating induced negative charge under the action of static electricity, thereby reducing the threshold voltage V th Negative bias, so the working current increases, resulting in the problem of the edge of the opening structure 11 being shiny; on the other hand, compared with the solution of discharging static charge by setting a wire between the protective cover 180 and the support structure 210, this embodiment can avoid the physical interference caused by the wire at the edge of the opening structure 11, affecting the installation effect of the device in the installation area (such as the camera module);

[0095] 3. By selecting the material of the second barrier layer 802 as a hydrophobic conductive material, it can release static charge while reducing the rate at which water vapor is transmitted along the second barrier layer 802 to the display substrate 120, thereby reducing the oxidation of the first inorganic encapsulation layer 118a, thereby reducing the probability of progressive black spot defects in the light-emitting device layer 125;

[0096] 4. By selecting the material of the second barrier layer 802 as graphene or carbon nanotubes, it is possible to realize the extraction of static charge and to perform light shielding treatment on the open hole structure 11, thereby reducing the influence of ambient light on the thin film transistor characteristics of the driving circuit layer 124, and having a good effect on reducing low grayscale brightness;

[0097] 5. By selecting the material of the first barrier layer 801 to be a material that can block the migration of cations, the electrochemical corrosion of the encapsulation layer 118 by water and cations can be effectively avoided, causing the encapsulation layer 118 to fail, thereby effectively avoiding the occurrence of progressive black spots in the light-emitting device layer 125.

[0098] In the second aspect, based on the same inventive concept, the embodiment of the present disclosure provides a display device, which includes the display panel described above. The display device can be any product or component with a display function, such as a mobile phone, a tablet computer, a television, a monitor, a notebook computer, a digital photo frame, a navigator, etc., and the embodiment of the present disclosure does not limit this.

[0099] In a third aspect, based on the same inventive concept, an embodiment of the present disclosure provides a method for preparing a display panel, which can prepare the display panel 10 described above, wherein the display panel 10 includes a mounting area and a display area 12 surrounding at least a portion of the outline of the mounting area.

[0100] Below Figure 1B-Figure 5 Taking the display panel 10 shown as an example, the preparation method provided by the embodiment of the present disclosure is introduced.

[0101] The preparation method comprises:

[0102] Step S100, providing a base substrate 101. For example, when the display panel 10 is a flexible display panel, the provided base substrate 101 may be a flexible substrate such as polyimide (PI), and when the display panel 10 is a rigid panel, the base substrate 101 may be a rigid substrate such as glass or quartz. This embodiment is described by taking the formation of a flexible display panel as an example.

[0103] Step S200 , forming a light-emitting device layer 125 located in the display area 12 on the base substrate 101 , wherein the light-emitting device layer 125 at least includes a light-emitting device 1 d located in the display area 12 .

[0104] Step S300 , forming an opening structure 11 located in the mounting area and penetrating at least the base substrate 101 and the light emitting device layer 125 along the thickness direction of the display panel 10 .

[0105] Step S400: forming a first barrier layer 801 on the sidewall of the open-pore structure 11. The first barrier layer 801 covers the sidewall of the open-pore structure 11. Figure 4 For example, the first barrier layer 801 can be formed by inkjet printing process.

[0106] In some embodiments, the preparation method further comprises:

[0107] Step S500 , forming a support structure 210 , and attaching it to a side of the base substrate 101 away from the light-emitting device layer 125 , and the opening structure 11 also penetrates the support structure 210 .

[0108] Step S600: forming a second barrier layer 802 covering the first barrier layer 801. For example, the second barrier layer 801 may be formed by inkjet printing.

[0109] Step S700: a protective cover plate 180 is disposed on the side of the light emitting device layer 125 away from the base substrate 101. The second barrier layer 802 is in contact with the protective cover plate 180, and extends to the support structure 210 through the opening structure 11, and is electrically connected to the support structure 210. Figure 5 shown.

[0110] In this embodiment, the first barrier layer 801 and the second barrier layer 802 are formed by using the same equipment and process, and no additional equipment or process is required.

[0111] In some examples, before forming the light emitting device layer 125, the preparation method further includes a step SS1 of forming a driving circuit layer 124 in the display area 12. Specifically, forming the driving circuit layer 124 in the display area 12 includes: forming a thin film transistor and a storage capacitor in the display area 12. More specifically, step SS1 includes:

[0112] An active layer 104 is formed on a substrate 101 by a patterning process; a first gate insulating layer 105 is formed on the active layer 104 by deposition or the like; a gate 106 and a first electrode 130 are simultaneously formed on the first gate insulating layer 105 by a patterning process; a second gate insulating layer 108 is formed on the gate 106 and the first electrode 130 by deposition or the like; a second electrode 131 is formed by a patterning process; an interlayer dielectric layer 103 is formed on the second electrode 131 by deposition or the like; the interlayer dielectric layer 103, the second gate insulating layer 108 and the first gate insulating layer 105 are etched to form a via hole exposing the active layer 104; and a source electrode 110 and a drain electrode 111 are formed. Figure 1C shown.

[0113] For example, the active layer 104 may be made of materials such as polysilicon and metal oxide, the first gate insulating layer 105 may be made of inorganic insulating materials such as silicon oxide, silicon nitride or silicon oxynitride, the second electrode 131 may be made of metal or alloy materials such as aluminum, titanium, cobalt, etc., the interlayer dielectric layer 103 may be made of inorganic insulating materials such as silicon oxide, silicon nitride or silicon oxynitride, and the source 110 and the drain 111 may be formed into a multi-layer metal structure, such as a three-layer metal layer structure. For example, in one example, a titanium material layer, an aluminum material layer and a titanium material layer may be formed in sequence by sputtering or evaporation, and then the three material layers may be patterned by the same patterning process, thereby forming a titanium / aluminum / titanium three-layer metal structure constituting the source 110 and the drain 111.

[0114] In some examples, after the film layers of the thin film transistor and the storage capacitor are formed, a step SS2 of sequentially forming a planarization layer, a first electrode 112, a pixel defining portion 113 and a supporting portion 132 is further included. Step SS2 specifically includes:

[0115] A planarization layer is formed in the display area 12 through a deposition process, and the planarization layer has a via hole, so that the first electrode 112 formed later is electrically connected to the drain electrode 111 through the via hole; a pixel defining portion 113 is formed through a patterning process, and the pixel defining portion 113 has an opening exposing the first electrode 112, so that the light emitting portion 114a and the second electrode 115 of the light emitting device 1d are formed later; and a support portion 132 is formed by a patterning process. Figure 1C shown.

[0116] For example, the material of the planarization layer 116 can be an organic insulating material such as polyimide, epoxy resin, etc., the material of the first electrode 112 includes metal oxides such as ITO, IZO, or metals such as Ag, Al, Mo or their alloys, and the material of the pixel defining portion 113 and the supporting portion 132 can include organic insulating materials such as polyimide, epoxy resin, etc.

[0117] In some examples, step S200 of forming the light emitting device layer 125 specifically includes:

[0118] After the planarization layer, the first electrode 112, the pixel defining portion 113 and the support portion 132 are sequentially formed, the light emitting portion 114a and the second electrode 115 are formed in the opening of the pixel defining portion 113 by inkjet printing or evaporation. Figure 1C shown.

[0119] For example, an auxiliary light-emitting layer (not shown) may be formed between the light-emitting portion 114a and the first electrode 112 or between the light-emitting portion 114a and the second electrode 115, and the auxiliary light-emitting layer may include, for example, one or more of an electron injection layer, an electron transport layer, a hole injection layer, and a hole transport layer. For example, the material of the light-emitting portion 114a and the auxiliary light-emitting layer are organic materials, and the material of the light-emitting portion 114a may be selected as a light-emitting material that can emit a certain color of light (e.g., red light, blue light, or green light, etc.) according to demand. The material of the second electrode 115 may include metals such as Mg, Ca, Li, or Al, or metal oxides such as IZO and ZTO, or organic materials with conductive properties such as PEDOT / PSS (poly 3,4-ethylenedioxythiophene / polystyrene sulfonate).

[0120] In some examples, the display panel 10 also has Figure 1A The barrier area 13 shown in FIG. 1 is located between the mounting area and the display area 12. Figure 1D As shown, the display panel 10 further includes a first isolation column 202 , a second isolation column 204 , a first interception wall 203 and a second interception wall 205 located in the blocking area 13 .

[0121] like Figure 1D As shown, the first isolation column 202 and the second isolation column 204 both include a metal layer structure, and the preparation method of the first isolation column 202 and the second isolation column 204 includes:

[0122] While forming the source 110 and the drain 111 , the metal layer structure of the first isolation column 202 and the second isolation column 204 is formed; and by using an etching process, recesses are formed on the side surfaces of the metal layer structure of the first isolation column 202 and the second isolation column 204 .

[0123] like Figure 1D As shown, the first interception wall 203 includes a first insulating layer and a second insulating layer, and the second interception wall 205 includes a third insulating layer, a fourth insulating layer and a fifth insulating layer. The steps of preparing the first interception wall 203 and the second interception wall 205 include:

[0124] While forming the planarization layer 116, the first insulating layer of the first intercepting wall 203 and the third insulating layer of the second intercepting wall 205 are formed; while forming the pixel defining portion 113, the second insulating layer of the first intercepting wall 203 and the fourth insulating layer of the second intercepting wall 205 are formed; while forming the supporting portion 132, the fifth insulating layer of the second intercepting wall 205 is formed.

[0125] In some examples, after forming the light emitting device layer 125, an encapsulation layer 118 may be formed in the display area 12, and step SS3 of forming the encapsulation layer 118 specifically includes:

[0126] A first inorganic encapsulation layer 118a is formed on the display area 12 and the first isolation column 202 by deposition or the like; an organic encapsulation layer 118b is formed on the first inorganic encapsulation layer 118a by inkjet printing, and the organic encapsulation layer 118b terminates at the first interception wall 203; a second inorganic encapsulation layer 118c is formed on the organic encapsulation layer 118b by deposition or the like.

[0127] For example, the first inorganic encapsulation layer 118a and the second inorganic encapsulation layer 118c can be formed of inorganic materials such as silicon nitride, silicon oxide, silicon oxynitride, etc., and the organic encapsulation layer 118b can be formed of organic materials such as polyimide (PI) and epoxy resin. Thus, the first inorganic encapsulation layer 118a, the organic encapsulation layer 118b and the second inorganic encapsulation layer 118c form a composite encapsulation layer 118, which can provide multiple protections for the functional structure of the display area 12 and the first isolation column 202 and other structures, and has a better encapsulation effect.

[0128] In some examples, the display panel 10 further includes a touch layer 127, a polarizer 128, an optical adhesive 129, and a protective cover plate 130 on the side of the light emitting device layer 125 facing away from the base substrate 101, as shown in FIG. Figure 4-Figure 5 .

[0129] The method for preparing the display panel 10 further includes:

[0130] A touch layer 127 and a polarizer 128 are sequentially formed on the side of the encapsulation layer 118 away from the base substrate, and an optical adhesive 129 for attaching the protective cover 180 is applied on the side of the polarizer 128 away from the base substrate 101. For example, the touch layer 127 includes structures such as touch electrodes.

[0131] The opening structure 11 penetrates all the film layer structures except the protective cover plate 180, that is, the opening structure 11 penetrates the optical glue 129, the polarizer 128, the touch layer 127, the encapsulation layer 118, the optical device layer 125, the drive circuit layer 124, the base substrate 101, the back film 122 and the support layer 121 along the thickness direction of the display panel 10. For example, the opening structure 11 can be formed by laser cutting or mechanical stamping, and structures such as image sensors and infrared sensors can be installed at the opening structure 11, and connected to signals such as a central processing unit. For example, the image sensor or infrared sensor can be arranged on the side of the base substrate 101 away from the light-emitting device 1d (i.e., the non-display side of the display panel 10), and various functions such as taking pictures, facial recognition, and infrared sensing can be realized through the opening structure 11.

[0132] In some examples, the display panel 10 further includes Figure 1EThe first organic insulating layer 206 shown in the figure at least covers the second spacer 204. The steps of preparing the display panel 10 in this example also include:

[0133] A first organic insulating layer 206 is formed on the second isolation column 204 by coating or other methods, and the first organic insulating layer 206 at least covers the second isolation column 204. For example, the first organic insulating layer 206 is formed between the second intercepting wall 205 and the opening structure 11. The first organic insulating layer 206 can protect the second isolation column 204, and the first organic insulating layer 206 can also prevent impurities such as water and oxygen from entering the display area 12 from the opening structure 11; in addition, the first organic insulating layer 206 has a certain height, which can support the polarizer 128 and the protective cover plate 180 and other structures formed on the display substrate 120 later, and prevent the polarizer 128 and the protective cover plate 180 and other structures from collapsing in the opening structure 11.

[0134] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the present invention, but the present invention is not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and essence of the present invention, and these modifications and improvements are also considered to be within the scope of protection of the present invention.

Claims

1. A display panel, divided into a mounting area and a display area surrounding at least a portion of the mounting area; the display panel comprising: substrate substrate; A light emitting device layer is arranged on the base substrate; The light emitting device layer at least includes a light emitting device located in the display area; An opening structure, located in the installation area; The opening structure at least penetrates the base substrate and the light emitting device layer along the thickness direction of the display panel; Characterized in that the display panel further comprises a first barrier layer covering the side walls of the opening structure.

2. The display panel according to claim 1, characterized in that: Also includes: A support structure located on a side of the substrate away from the light-emitting device layer; A protective cover plate disposed on a side of the light emitting device layer away from the base substrate; and, a second barrier layer covering the first barrier layer; The open hole structure also penetrates the support structure; The second barrier layer contacts the protection cover plate, extends to the support structure through the opening structure, and is electrically connected to the support structure.

3. The display panel according to claim 2, characterized in that: The support structure includes a back film and a support layer which are stacked in sequence in a direction away from the substrate.

4. The display panel according to claim 2, characterized in that: The material of the second barrier layer is a hydrophobic conductive material.

5. The display panel according to claim 2, characterized in that: The material of the second barrier layer is graphene or carbon nanotubes.

6. The display panel according to any one of claims 1 to 5, characterized in that: The material of the first barrier layer is selected to be a material capable of blocking the migration of cations.

7. The display panel according to any one of claims 1 to 5, characterized in that: It also includes a polarizer located in a direction where the light-emitting device layer is away from the substrate; and the opening structure also passes through the polarizer.

8. The display panel according to claim 7, characterized in that: It also includes a touch layer located between the polarizer and the light-emitting device layer, and the opening structure also penetrates the touch layer.

9. A display device, characterized in that: A display panel comprising any one of claims 1 to 8.

10. A method for preparing a display panel according to any one of claims 1 to 8, wherein the display panel is divided into a mounting area and a display area surrounding at least a portion of the mounting area; characterized in that: The preparation method comprises: providing a substrate base plate; Forming a light-emitting device layer on the base substrate; the light-emitting device layer at least includes a light-emitting device located in the display area; forming an opening structure located in the mounting area and penetrating at least the base substrate and the light-emitting device layer in the thickness direction of the display panel; A first barrier layer is formed on the sidewall of the open-pore structure; the first barrier layer covers the sidewall of the open-pore structure.

11. The preparation method according to claim 10, characterized in that: The preparation method further comprises: Forming a support structure and attaching it to a side of the base substrate away from the light-emitting device layer; the opening structure also penetrates the support structure; forming a second barrier layer covering the first barrier layer; A protective cover plate is disposed on a side of the light emitting device layer away from the base substrate; the second barrier layer contacts the protective cover plate, extends to the support structure through the opening structure, and is electrically connected to the support structure.

12. The preparation method according to claim 11, characterized in that: The first barrier layer and the second barrier layer are formed by using the same equipment and process.

13. The preparation method according to claim 10, characterized in that: The forming of the support structure comprises: A support layer is provided, and a back film is formed on a side of the support layer close to the base substrate.

14. The preparation method according to any one of claims 10 to 13, characterized in that: The preparation method further comprises: A touch layer is formed on a side of the light emitting device layer away from the base substrate; and the opening structure also penetrates the touch layer.

15. The preparation method according to claim 14, characterized in that: The preparation method further comprises: A polarizer is formed on a side of the touch layer away from the base substrate; and the opening structure also penetrates the polarizer.