Method for removing oxide layer on back surface of silicon carbide wafer
By applying film on the front of the silicon carbide wafer and removing the back oxide using corrosion method, the problems of damage and low efficiency of the front film layer when the back oxide layer of the silicon carbide wafer are removed in the prior art are solved, and the oxide removal is efficient and The effect of reducing wear ratio.
Patent Information
- Application Number
- CN202410972759.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-22
AI Technical Summary
The prior art is easy to damage the front mask layer when removing the back oxide layer of the silicon carbide wafer, and the grinding method is low and the wear ratio is high, resulting in warping and debris, affecting the subsequent process.
The oxide on the back of the silicon carbide wafer is removed by corrosion. By applying a film on the front and selecting the appropriate corrosion liquid and overcorrosion amount, the front film layer is protected, and the oxide is removed before thinning to reduce the wear ratio.
The efficiency of oxide removal is improved, warping and wear of the silicon carbide wafer is avoided, the front mask layer is protected, and the wear ratio of subsequent processes is reduced.
Smart Images

Figure CN119008525A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wafer processing, and in particular to a method for removing an oxide layer on the back side of a silicon carbide wafer. Background Art
[0002] For silicon carbide power devices, after completing the front process, the back of the silicon carbide wafer needs to be thinned to a certain thickness before making the back electrode. The existing back thinning process generally uses mechanical grinding. Due to the front process, such as thermal oxidation process, 100nm-500nm of oxide will be left on the back of the silicon carbide wafer. In the thinning process, it is generally required to remove the oxide on the back of the silicon carbide wafer. If there is residual oxide on the back of the silicon carbide wafer, the grinding rate will be particularly slow and the wear ratio will be particularly large. The wear ratio of the conventional back thinning process is 20% to 30%, and the wear ratio with oxide is as high as 60% to 80%.
[0003] Therefore, before thinning the back of the silicon carbide wafer, the residual oxide needs to be removed first. While removing the back oxide, it is also necessary to ensure that the front film layer is not affected. Due to the high temperature during the operation, the traditional dry process will melt the front metal layer. In addition, the traditional wet process may corrode the front film layer. Conventional grinding methods are generally used to remove residual oxides on the back of the silicon carbide wafer, but conventional grinding methods use low-mesh grinding wheels, which have a large grinding loss ratio and low grinding efficiency. It will also cause the silicon carbide wafer to have a large warping, resulting in fragments in the subsequent back process, and even making it impossible to carry out subsequent processes due to the large warping.
[0004] Therefore, a method is needed to remove the oxide layer on the back side of the silicon carbide wafer while protecting the front side film layer from being affected. Summary of the invention
[0005] In order to overcome the problems existing in the related art, the purpose of the present invention is to provide a method for removing the oxide layer on the back side of a silicon carbide wafer, which can protect the front film layer from being affected while removing the oxide layer on the back side of the silicon carbide wafer.
[0006] A method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0007] Performing front-side processing on the front side of the silicon carbide wafer;
[0008] Applying a film on the front side of the silicon carbide wafer;
[0009] Removing oxide from the back of the silicon carbide wafer by etching;
[0010] Removing the film on the front side of the silicon carbide wafer to obtain a wafer after the oxide is removed;
[0011] The back side of the wafer after oxide removal is thinned to obtain a thinned wafer.
[0012] In a preferred technical solution of the present invention, the process of attaching a film on the front side of the silicon carbide wafer comprises:
[0013] The UV film on the film sticking ring is stuck on the front side of the silicon carbide wafer.
[0014] In a preferred technical solution of the present invention, the etching method is used to remove the oxide on the back side of the silicon carbide wafer, comprising:
[0015] Selecting an etching solution and a preset over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer;
[0016] The back oxide layer is corroded using the corrosive solution according to the preset over-corrosion amount.
[0017] In a preferred technical solution of the present invention, the etching solution and the preset over-etching amount are selected according to the thickness of the back oxide layer of the silicon carbide wafer, including:
[0018] If the thickness of the back oxide layer is in the range of 100 nm-500 nm, the preset over-etching amount is in the range of 50%-100%, and the etching solution is hydrofluoric acid.
[0019] In a preferred technical solution of the present invention, the etching solution is used to etch the back oxide layer according to the preset over-etching amount, comprising:
[0020] Spraying the etching liquid on the back oxide layer;
[0021] Detect whether the over-corrosion amount of the back oxide layer reaches the preset over-corrosion amount, and if so, stop corroding the back oxide layer.
[0022] In a preferred technical solution of the present invention, the back side of the wafer after the oxide is removed is thinned to obtain a thinned wafer, comprising:
[0023] Acquire a target thickness, and set a first thickness range according to the target thickness;
[0024] Roughly thinning the back side of the wafer after the oxide is removed until the thickness of the wafer after the oxide is removed is within the first thickness range;
[0025] The wafer after oxide removal is thinned to the target thickness to obtain a thinned wafer.
[0026] In a preferred technical solution of the present invention, before thinning the back side of the wafer after removing the oxide, the method further includes:
[0027] A high-viscosity film is pasted on the front side of the wafer after the oxide is removed, and the wafer after the oxide is removed is pasted on the thinning device through the high-viscosity film;
[0028] After thinning the back side of the wafer after oxide removal, the high-adhesion film is removed.
[0029] In a preferred technical solution of the present invention, after removing the oxide on the back side of the silicon carbide wafer by etching, the method further comprises:
[0030] The silicon carbide wafer is dried using an inert gas at a temperature of 60-80°C.
[0031] In a preferred technical solution of the present invention, after the UV film on the film-sticking ring is pasted on the front surface of the silicon carbide wafer, the method further includes:
[0032] The film-sticking ring is fixed on a processing device, and the processing device is a dicing machine or a cleaning machine.
[0033] In a preferred technical solution of the present invention, after obtaining the thinned wafer, the method further comprises:
[0034] The thinned wafer is subjected to back side processing, wherein the back side processing includes a back side ohmic contact process and a back side metal process.
[0035] The beneficial effects of the present invention are:
[0036] The method for removing the oxide layer on the back side of a silicon carbide wafer provided by the present invention comprises performing front process processing on the front side of the silicon carbide wafer, and pasting a film on the front side of the silicon carbide wafer, which can protect the front side of the silicon carbide wafer and can also play a role in fixing the silicon carbide wafer. The oxide on the back side of the silicon carbide wafer is removed by an etching method. Since the film is pasted on the front side of the silicon carbide wafer, the front film layer can be prevented from being corroded during the process of removing the oxide. The thin film on the front side of the silicon carbide wafer is removed to obtain a wafer after the oxide is removed, and the back side of the wafer after the oxide is removed is thinned to obtain a thinned wafer. Before the thinning process, the oxide on the back side of the silicon carbide wafer is first removed to reduce the wear ratio of the thinning process. Compared with the method of removing the oxide on the back side of the silicon carbide wafer by grinding, the method of removing the oxide on the back side of the silicon carbide wafer by etching can improve the efficiency of removing the oxide and avoid large warping of the silicon carbide wafer. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 It is a flow chart of the method for removing the oxide layer on the back side of a silicon carbide wafer of the present invention;
[0038] Figure 2 is a flow chart of the improved thinning process of the present invention;
[0039] Figure 3 It is a flow chart of the conventional thinning process;
[0040] Figure 4 It is a schematic diagram of a silicon carbide wafer attached to a UV film;
[0041] Figure 5 It is a schematic diagram of the film ring before film application;
[0042] Figure 6 It is a schematic diagram of the film ring after film application. DETAILED DESCRIPTION
[0043] The preferred embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although the preferred embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided to make the present invention more thorough and complete, and to fully convey the scope of the present invention to those skilled in the art.
[0044] Example 1
[0045] like Figure 1 As shown, this embodiment provides a method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0046] S1: Performing front-side processing on the front side of the silicon carbide wafer.
[0047] S2: Applying a film on the front side of the silicon carbide wafer.
[0048] S3: removing the oxide on the back side of the silicon carbide wafer by etching.
[0049] S4: removing the thin film on the front side of the silicon carbide wafer to obtain a wafer after oxide removal.
[0050] S5: Thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer.
[0051] The front side of the silicon carbide wafer is processed by front side processes, including thermal oxidation, deposition, etching, polishing and wiring. The thermal oxidation process refers to placing the silicon carbide wafer in an oxidation furnace for thermal oxidation treatment. The thermal oxidation process will leave 100nm-500nm of oxide on the back of the silicon carbide wafer. If there is residual oxide on the back of the silicon carbide wafer, the grinding rate will be extremely slow and the wear ratio will be particularly large. The wear ratio of the conventional back thinning process is 20% to 30%, and the wear ratio with oxide is as high as 60% to 80%. Therefore, in the thinning process of the silicon carbide wafer, the oxide on the back of the silicon carbide wafer needs to be removed.
[0052] Apply UV varnish on the film ring, and use UV lamp to irradiate the UV varnish to cure the UV varnish to form a UV film. The front side of the silicon carbide wafer is attached to the UV (Ultraviolet) film, which can protect the front side of the silicon carbide wafer. There is no film on the back side of the silicon carbide wafer.
[0053] The oxide on the back of the silicon carbide wafer is etched away by single-sided etching. Single-sided etching involves etching liquid and a device for spraying the etching liquid, which has the advantages of low cost and will not generate stress on the back of the silicon carbide wafer, thereby avoiding warping of the back of the silicon carbide wafer. After fully removing the oxide on the back of the silicon carbide wafer, wash the back of the silicon carbide wafer with clean water for 10 minutes to 30 minutes to fully wash away the etching liquid.
[0054] The UV film on the front side of the silicon carbide wafer is torn off, a thin film is attached to the front side of the silicon carbide wafer, and then the silicon carbide wafer is transported to the thinning equipment using a robotic arm to thin the back side of the wafer after removing the oxide to obtain a thinned wafer.
[0055] Figure 2 This is the flow chart of the improved thinning process. Figure 3 This is a flow chart of a conventional thinning process. In this embodiment, the oxide on the back side of the silicon carbide wafer is removed before thinning, and then the back side of the silicon carbide is thinned, which can reduce the wear ratio of the back side thinning process and prevent the back side of the silicon carbide wafer from warping.
[0056] The method for removing the oxide layer on the back of the silicon carbide wafer provided in this embodiment includes performing a front process on the front of the silicon carbide wafer, and pasting a film on the front of the silicon carbide wafer, which can protect the front of the silicon carbide wafer and can also play a role in fixing the silicon carbide wafer. The oxide on the back of the silicon carbide wafer is removed by etching. Since the film is pasted on the front of the silicon carbide wafer, the front film layer can be prevented from being corroded during the removal of the oxide. The thin film on the front of the silicon carbide wafer is removed to obtain a wafer after the oxide is removed, and the back of the wafer after the oxide is removed is thinned to obtain a thinned wafer. Before the thinning process, the oxide on the back of the silicon carbide wafer is removed first, which can reduce the wear ratio of the thinning process. Compared with the method of removing the oxide on the back of the silicon carbide wafer by grinding, the method of removing the oxide on the back of the silicon carbide wafer by etching can improve the efficiency of removing the oxide and avoid large warping of the silicon carbide wafer.
[0057] Example 2
[0058] like Figure 1 As shown, this embodiment provides a method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0059] S1: Performing front-side processing on the front side of the silicon carbide wafer.
[0060] S2: applying a film on the front side of the silicon carbide wafer.
[0061] S3: removing the oxide on the back side of the silicon carbide wafer by etching.
[0062] S4: removing the thin film on the front side of the silicon carbide wafer to obtain a wafer after oxide removal.
[0063] S5: Thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer.
[0064] The process of attaching a film to the front side of the silicon carbide wafer comprises:
[0065] The UV film on the film ring is pasted on the front side of the silicon carbide wafer.
[0066] Figure 5 This is a schematic diagram of the film ring before film application. Figure 6 is a schematic diagram of the film ring after film application. Figure 6 As shown, the film ring is covered with a layer of UV film. The silicon carbide wafer is attached to the film ring, and the front of the silicon carbide wafer is attached to the UV film, and the back of the silicon carbide wafer is not filmed. The film ring is often used to fix the silicon carbide wafer on the dicing machine when the silicon carbide wafer is diced. You can also use UV film to fix the silicon carbide wafer on the film ring, and then fix the film ring on the cleaning equipment.
[0067] The method of removing the oxide on the back side of the silicon carbide wafer by etching comprises:
[0068] S31: Selecting etching solution and preset over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer.
[0069] S32: Corroding the back oxide layer using the etching solution according to the preset over-corrosion amount.
[0070] The preset over-corrosion amount is positively correlated with the thickness of the back oxide layer, that is, the greater the thickness of the back oxide layer, the greater the preset over-corrosion amount; and the smaller the thickness of the back oxide layer, the smaller the preset over-corrosion amount.
[0071] The etching liquid is used to corrode the back oxide layer of the silicon carbide wafer. The etching liquid can be hydrofluoric acid or other types of etching liquid. This embodiment takes hydrofluoric acid as the etching liquid as an example, and selects hydrofluoric acid of a corresponding concentration according to the thickness of the back oxide layer.
[0072] On the basis of using UV film to protect the front of the silicon carbide wafer, using hydrofluoric acid to corrode the back oxide layer of the silicon carbide wafer has the advantages of low cost and high efficiency, and can also prevent the back of the silicon carbide wafer from warping. Before thinning the back of the silicon carbide wafer, using hydrofluoric acid to remove the back oxide layer of the silicon carbide wafer can increase the grinding rate and reduce the wear ratio.
[0073] The present embodiment describes the step of attaching a film to the front side of the silicon carbide wafer, including attaching a UV film on a film-attaching ring to the front side of the silicon carbide wafer, and the step of removing the oxide on the back side of the silicon carbide wafer by etching, including selecting an etching solution and a preset over-etching amount according to the thickness of the back side oxide layer of the silicon carbide wafer, and using the etching solution to etch the back side oxide layer according to the preset over-etching amount. On the basis of using a UV film to protect the front side of the silicon carbide wafer, using hydrofluoric acid to etch the back side oxide layer of the silicon carbide wafer has the advantages of low cost and high efficiency, and can also prevent the back side of the silicon carbide wafer from warping. Using hydrofluoric acid to remove the back side oxide layer of the silicon carbide wafer before thinning the back side of the silicon carbide wafer can increase the grinding rate and reduce the wear ratio.
[0074] Example 3
[0075] like Figure 1 As shown, this embodiment provides a method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0076] S1: Perform front-side processing on silicon carbide wafers.
[0077] S2: applying a film on the front side of the silicon carbide wafer.
[0078] S3: removing the oxide on the back side of the silicon carbide wafer by a single-side etching method.
[0079] S4: removing the thin film on the front side of the silicon carbide wafer to obtain a wafer after oxide removal.
[0080] S5: Thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer.
[0081] The single-side etching method is used to remove the oxide on the back side of the silicon carbide wafer, comprising:
[0082] S31: Selecting etching solution and preset over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer.
[0083] S32: Corroding the back oxide layer using the etching solution according to the preset over-corrosion amount.
[0084] The method of selecting the etching solution and presetting the over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer comprises:
[0085] If the thickness of the back oxide layer is in the range of 100 nm-500 nm, the preset over-etching amount is in the range of 50%-100%, and the etching solution is hydrofluoric acid.
[0086] The step of using the etching solution to corrode the back oxide layer according to the preset over-corrosion amount includes:
[0087] S321: Spraying the etching liquid on the back oxide layer.
[0088] S322: Detect whether the over-corrosion amount of the back oxide layer reaches the preset over-corrosion amount, and if so, stop corroding the back oxide layer.
[0089] Figure 4 It is a schematic diagram of a silicon carbide wafer pasted on a UV film. Before removing the oxide on the back of the silicon carbide wafer, the silicon carbide wafer must first complete all front-side process processing, and then the front of the silicon carbide wafer must be fixed with a film before the oxide on the back of the silicon carbide wafer can be processed. A single-sided etching method is used here to remove the oxide on the back of the silicon carbide wafer, that is, a wet method is used to spray hydrofluoric acid solution to corrode the oxide on the back. According to the thickness of the back oxide layer, for example, the thickness is 100nm-500nm, the over-corrosion amount is 50%-100%, and the over-corrosion amount is preferably 50% or 75%. The actual thickness is based on the actual measured process film thickness on the production line to ensure that the oxide is fully removed. After corrosion, use clean water to wash for 10 minutes to 30 minutes to fully wash off the etching liquid on the back of the silicon carbide wafer.
[0090] A single-sided etching method is used to remove the oxide on the back of the silicon carbide wafer. This method only uses chemical corrosives and only processes the back of the silicon carbide wafer. The film layer on the front of the silicon carbide wafer will not be affected. It is not only low-cost but also helps to maintain the integrity and performance of the front process film layer.
[0091] This embodiment uses a single-sided etching method to remove the back oxide layer of the silicon carbide wafer. When the front process film layer of the silicon carbide wafer is not affected, the back oxide is wet-sprayed with hydrofluoric acid solution according to the preset over-corrosion amount according to the thickness of the back oxide. The etching solution and the preset over-corrosion amount are selected according to the thickness of the back oxide layer of the silicon carbide wafer, including if the thickness of the back oxide layer ranges from 100nm to 500nm, the preset over-corrosion amount ranges from 50% to 100%, and the etching solution uses hydrofluoric acid. The back oxide layer is corroded using the etching solution according to the preset over-corrosion amount, including spraying the etching solution on the back oxide layer, detecting whether the over-corrosion amount of the back oxide layer reaches the preset over-corrosion amount, and if so, stopping the etching of the back oxide layer. The single-sided etching method is not only low-cost, but also does not damage the front process film layer of the silicon carbide wafer.
[0092] Example 4
[0093] like Figure 1As shown, this embodiment provides a method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0094] S1: Perform front-side processing on silicon carbide wafers.
[0095] S2: applying a film on the front side of the silicon carbide wafer.
[0096] S3: removing the oxide on the back side of the silicon carbide wafer by a single-side etching method.
[0097] S4: removing the thin film on the front side of the silicon carbide wafer to obtain a wafer after oxide removal.
[0098] S5: Thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer.
[0099] The process of attaching a film to the front side of the silicon carbide wafer comprises:
[0100] The UV film on the film sticking ring is stuck on the front side of the silicon carbide wafer.
[0101] Before thinning the back side of the wafer after removing the oxide, the method further includes:
[0102] A high-viscosity film is pasted on the front side of the wafer after the oxide is removed, and the wafer after the oxide is removed is pasted on the thinning device through the high-viscosity film;
[0103] After thinning the back side of the wafer after oxide removal, the high-adhesion film is removed.
[0104] The high-viscosity film has strong viscosity and can firmly stick the wafer after the oxide is removed to the table of the thinning equipment. In the subsequent thinning process, the wafer after the oxide is removed will be subjected to stress and may be displaced. Use a high-viscosity film to fix the wafer after the oxide is removed to the table of the thinning equipment, thereby preventing the wafer from being displaced during the thinning process.
[0105] After thinning the back side of the wafer after oxide removal, the high-viscosity film is removed and the thinned wafer is sent to the next production line for the next process.
[0106] After the single-side etching method is used to remove the oxide on the back side of the silicon carbide wafer, the method further includes:
[0107] The silicon carbide wafer is dried using an inert gas at a temperature of 60-80°C.
[0108] After the UV film on the film-sticking ring is pasted on the front surface of the silicon carbide wafer, the method further includes:
[0109] The film-sticking ring is fixed on a processing device, and the processing device is a dicing machine or a cleaning machine.
[0110] After all front processes are completed, the silicon carbide wafer is first attached to the film ring, which is often used to fix the silicon carbide wafer on the wafer scribing machine during wafer scribing. The front of the silicon carbide wafer is attached to the UV film, and the back of the silicon carbide wafer is not filmed. In this embodiment, the silicon carbide wafer is fixed to the film ring using the UV film, and then the film ring is fixed to the cleaning equipment.
[0111] After the front side of the silicon carbide wafer is fixed with a film, the oxide on the back side of the silicon carbide wafer is removed by single-sided etching. The temperature is controlled at 60-80°C, and the silicon carbide wafer is dried in an environment filled with inert gas such as nitrogen. The inert gas will not chemically react with the silicon carbide wafer, thereby avoiding the introduction of impurities or oxidation.
[0112] After drying the silicon carbide wafer, tear off the UV film on the front of the silicon carbide wafer. Stick a high-viscosity film with a thickness of 100-200um on the front of the silicon carbide wafer, and use a robotic arm to transport the silicon carbide wafer to the thinning equipment for operation. Get the target thickness, and set the first preset range and the second preset range according to the target thickness. First, roughly thin the back of the silicon carbide wafer to within the first preset range. The lower limit of the first preset range is the target thickness + 20um, and the upper limit of the first preset range is the target thickness + 30um. For example, if it needs to be thinned to 180um, first thin the back of the silicon carbide wafer to 200um-210um to obtain a roughly thinned wafer. The rough thinning uses a grinding wheel of model SD600. Finely thin the wafer after removing the oxide to the target thickness to obtain a thinned wafer. For example, if the thickness of the wafer after rough thinning is 200um, the wafer after rough thinning is finely thinned by 20um; if the thickness of the wafer after rough thinning is 210um, the wafer after rough thinning is finely thinned by 30um, and the fine thinning adopts the grinding wheel of model SD2000 or 50D. The back side of the wafer after oxide removal can be rough thinned first, and then the back side of the wafer after rough thinning is finely thinned; or only the back side of the wafer after oxide removal can be rough thinned or fine thinned.
[0113] After thinning the back of the wafer after oxide removal, the thinned wafer is cleaned with deionized water to obtain a cleaned silicon carbide wafer. The cleaned silicon carbide wafer is dried, and then the high-viscosity film on the front of the cleaned silicon carbide wafer is torn off.
[0114] This embodiment thins the back side of the wafer after oxide removal to obtain a thinned wafer, including obtaining a target thickness and setting a first thickness range according to the target thickness. Rough thinning is performed on the back side of the wafer after oxide removal until the thickness of the wafer after oxide removal is within the first thickness range. Fine thinning is performed on the wafer after oxide removal to the target thickness to obtain a thinned wafer. Rough thinning is performed on the back side of a silicon carbide wafer using a rough grinding wheel, and fine thinning is performed on the back side of a silicon carbide wafer using a fine grinding wheel. In the case of removing the oxide on the back side of the silicon carbide wafer, the silicon carbide wafer can be thinned to the target thickness by combining two thinning steps.
[0115] Example 5
[0116] like Figure 1 As shown, this embodiment provides a method for removing an oxide layer on the back side of a silicon carbide wafer, comprising:
[0117] S1: Performing front-side processing on the front side of the silicon carbide wafer.
[0118] S2: Applying a film on the front side of the silicon carbide wafer.
[0119] S3: removing the oxide on the back side of the silicon carbide wafer by etching.
[0120] S4: removing the thin film on the front side of the silicon carbide wafer to obtain a wafer after oxide removal.
[0121] S5: Thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer.
[0122] After obtaining the thinned wafer, the method further includes:
[0123] The thinned wafer is subjected to back-side processing, and the back-side process includes a back-side ohmic contact process and a back-side metal process. The back side of the thinned wafer is subjected to back-side ohmic contact processing to form an ohmic contact on the back side of the thinned wafer. The back-side ohmic contact process is divided into ion implantation and epitaxy. Ion implantation is to generate positively charged impurity ions from the source material, and epitaxy is to grow a single crystal layer on the substrate. Ohmic contact means that the metal and the semiconductor are a resistor at the contact point, and the smaller the resistance value of the resistor, the better.
[0124] The above-mentioned back metal process refers to metallizing the back of the silicon carbide wafer, the main purpose of which is to reduce resistance. The metal on the back of the silicon carbide wafer is usually evaporated using an evaporation table or sputtered using a sputtering table, and metals such as Ti, Ni, Ag and Au are deposited on the back of the wafer under high vacuum process conditions.
[0125] After obtaining the thinned wafer described in this embodiment, the back side process of the thinned wafer is further included, and the back side process includes a back side ohmic contact process and a back side metal process. The back side ohmic contact process can form an ohmic contact on the back side of the thinned wafer, and the back side metal process can metallize the back side of the thinned wafer to reduce the resistance of the thinned wafer.
[0126] Unless otherwise specifically stated, the relative arrangement, numerical expressions and numerical values of the parts and steps set forth in these embodiments do not limit the scope of the application. In all examples shown and discussed here, any specific value should be interpreted as being merely exemplary, rather than as a restriction. Therefore, other examples of exemplary embodiments can have different values. It should be noted that similar reference numerals and letters represent similar items in the following drawings, and therefore, once a certain item is defined in an accompanying drawing, it does not need to be further discussed in the subsequent accompanying drawings.
[0127] It should be understood that spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. For example, if the device in the figures is inverted, a device described as "above" or "above" other devices or structures would then be positioned "below" or "below" the other devices or structures. Thus, the exemplary term "above" can include both the orientations of "above" and "below." The device may also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatially relative descriptions used herein should be interpreted accordingly.
[0128] In addition, it should be noted that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. Unless otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of this application.
[0129] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for removing an oxide layer on the back side of a silicon carbide wafer, characterized in that: include: Performing front-side processing on the front side of the silicon carbide wafer; Applying a film on the front side of the silicon carbide wafer; Removing oxide from the back of the silicon carbide wafer by etching; Removing the film on the front side of the silicon carbide wafer to obtain a wafer after the oxide is removed; The back side of the wafer after oxide removal is thinned to obtain a thinned wafer.
2. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: The process of attaching a film to the front side of the silicon carbide wafer comprises: The UV film on the film sticking ring is stuck on the front side of the silicon carbide wafer.
3. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: The method of removing the oxide on the back side of the silicon carbide wafer by etching comprises: Selecting an etching solution and a preset over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer; The back oxide layer is corroded using the corrosive solution according to the preset over-corrosion amount.
4. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 3, characterized in that: The method of selecting the etching solution and presetting the over-etching amount according to the thickness of the back oxide layer of the silicon carbide wafer comprises: If the thickness of the back oxide layer is in the range of 100 nm-500 nm, the preset over-etching amount is in the range of 50%-100%, and the etching solution is hydrofluoric acid.
5. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 3, characterized in that: The method of using the etching solution to etch the back oxide layer according to the preset over-etching amount includes: Spraying the etching liquid on the back oxide layer; Detect whether the over-corrosion amount of the back oxide layer reaches the preset over-corrosion amount, and if so, stop corroding the back oxide layer.
6. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: The step of thinning the back side of the wafer after the oxide is removed to obtain a thinned wafer comprises: Acquire a target thickness, and set a first thickness range according to the target thickness; Roughly thinning the back side of the wafer after the oxide is removed until the thickness of the wafer after the oxide is removed is within the first thickness range; The wafer after oxide removal is thinned to the target thickness to obtain a thinned wafer.
7. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: Before thinning the back side of the wafer after removing the oxide, the method further includes: A high-viscosity film is pasted on the front side of the wafer after the oxide is removed, and the wafer after the oxide is removed is pasted on the thinning device through the high-viscosity film; After thinning the back side of the wafer after oxide removal, the high-adhesion film is removed.
8. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: After removing the oxide on the back side of the silicon carbide wafer by etching, the method further includes: The silicon carbide wafer is dried using an inert gas at a temperature of 60-80°C.
9. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 2, characterized in that: After the UV film on the film-sticking ring is pasted on the front surface of the silicon carbide wafer, the method further includes: The film-sticking ring is fixed on a processing device, and the processing device is a dicing machine or a cleaning machine.
10. The method for removing the oxide layer on the back side of a silicon carbide wafer according to claim 1, characterized in that: After obtaining the thinned wafer, the method further includes: The thinned wafer is subjected to back side processing, wherein the back side processing includes a back side ohmic contact process and a back side metal process.