Cooling process for producing acfc with purified improved crystalline

By cooling the ACFC mixture at high temperature and optimizing catalyst and solvent selection, the problem of low purity and chromaticity in ACFC production in the prior art is solved, and the ACFC preparation of high-efficiency, low-carbon oxides is achieved.

CN119013263APending Publication Date: 2024-11-22EASTMAN CHEM CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380033857.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-13
Filing Date
2023-04-12
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

It is difficult to effectively produce 5-(alkoxycarbonyl)furan-2-formic acid (ACFC) of high purity and low chromaticity, and traditional methods have problems with carbon oxide formation and increased intermediate yield.

Method used

A mixture containing ACFC and solvent is provided above 70°C and cooled to 30°C or lower at a rate of 0.5°C/min to 10°C/min, using monocarboxylic acid having 2 to 6 carbon atoms as the solvent, The dried solid composition is prepared, the particle/crystal particle size distribution is controlled from 20 to 500 microns, and impurity formation and carbon oxide formation are reduced by optimizing the selection of oxidation catalyst and solvent.

Benefits of technology

Production of ACFC solid compositions with high purity and low chromaticity is achieved, reducing carbon oxide formation and intermediate yields, and improving yields and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119013263A_ABST
    Figure CN119013263A_ABST
Patent Text Reader

Abstract

Providing a dry solid composition comprising a compound of structural formula (I): # imgabs0 # wherein R2 is an alkyl group having from 1 to 6 carbon atoms, and wherein the composition has a particle / crystalline particle size distribution of from 20 to 500 microns; wherein the dried solid composition has a filter cake specific resistance of 5 * 10 < 9 > m / kg or less, or 4.3 * 10 < 9 > m / kg or less; wherein the particle size is in the range of 20 to 500 microns. In addition, a method of making the composition is also provided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates generally to the field of organic chemistry and in particular to a process for preparing 5-(alkoxycarbonyl)furan-2-carboxylic acid (ACFC) and a composition comprising the acid. Background Art

[0002] Aromatic dicarboxylic acids, such as terephthalic acid and isophthalic acid, can be used to produce various polyesters. Examples of such polyesters include polyethylene terephthalate (PET) and its copolymers. These aromatic dicarboxylic acids are usually synthesized by catalytic oxidation of the corresponding dialkyl aromatic compounds, which are obtained from fossil fuels.

[0003] There is a growing interest in using renewable resources as raw materials in the chemical industry, mainly due to the gradual reduction of fossil reserves and their associated environmental impact. Furan-2,5-dicarboxylic acid (FDCA) and ACFC are common intermediates that are considered to be the most promising and closest bio-based alternatives to terephthalic acid and isophthalic acid. Similar to aromatic diacids, ACFC and FDCA can be condensed with diols such as ethylene glycol to make polyester resins similar to PET.

[0004] Therefore, there is a need in the art to provide alternative and / or improved methods for producing carboxylic acid compositions, especially compositions containing ACFC. In addition, there is a need to provide ACFC compositions having high purity and low color.

[0005] The present invention addresses this need and other needs, which will become apparent from the following description and the appended claims. Summary of the invention

[0006] In one embodiment of the present invention, a method for increasing the crystal size of a compound of structural formula (I) is provided:

[0007]

[0008] The method includes

[0009] (a) providing a mixture comprising compound (I) and a solvent at a temperature of at least 70°C; and

[0010] (b) cooling the mixture from step (a) to a temperature of 30°C or less at a rate of 0.5°C / min to 10°C / min,

[0011] in

[0012] The solvent includes a monocarboxylic acid having 2 to 6 carbon atoms; and

[0013] R 2is an alkyl group having 1 to 6 carbon atoms.

[0014] In another embodiment of the present invention, there is provided a dry solid composition comprising a compound of structural formula (I):

[0015]

[0016] R 2 is an alkyl group having 1 to 6 carbon atoms, wherein the particle / crystal size distribution of the composition is 20 to 500 microns; wherein the dried solid composition has 5x10 9 m / kg or less, or 4.3x10 9 m / kg or less filter cake resistance; wherein the particle size range is 20 to 500 microns. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 Various embodiments of the present invention are shown in which a method of producing a dry carboxylic acid 410 is provided.

[0018] Figure 2 An embodiment of the invention is shown in which a purge stream is produced. Figure 1 Detailed description of the 700 area. DETAILED DESCRIPTION

[0019] In one aspect, the present invention provides a method for preparing a compound of formula (I):

[0020]

[0021] Where R 2 is an alkyl group having 1 to 6 carbon atoms. The alkyl group may be branched or straight-chain. Examples of such groups include methyl, ethyl, propyl, isopropyl, butyl, methylpropyl, pentyl, ethylpropyl, hexyl, methylpentyl and ethylbutyl.

[0022] In various embodiments, R 2 is an alkyl group having 1 to 3 carbon atoms.

[0023] In other various embodiments, R 2 It is methyl.

[0024] Compound (I) can be referred to as 5-(alkoxycarbonyl)furan-2-carboxylic acid (ACFC). 2 When it is a methyl group, compound (I) is 5-(methoxycarbonyl)furan-2-carboxylic acid (MCFC).

[0025] The method for preparing compound (I) comprises contacting a compound of formula (II) with an oxidizing agent in the presence of an oxidation catalyst and a solvent:

[0026]

[0027] R in formula (II) 1 is hydrogen, R 3 O- or R 3 C(O)O-, wherein R3 is hydrogen or an alkyl group having 1 to 6 carbon atoms. 2 Similar, R 3 The alkyl group in may be branched or linear.

[0028] In various embodiments, R 3 is hydrogen or an alkyl group having 1 to 3 carbon atoms.

[0029] In other various embodiments, R 1 For hydrogen.

[0030] In various other embodiments, R 1 For R 3 O-, where R 3 is hydrogen, methyl, ethyl, propyl or isopropyl.

[0031] In other various embodiments, R 1 For R 3 C(O)O-, where R 3 is hydrogen, methyl, ethyl, propyl or isopropyl.

[0032] R in formula (II) 2 The same as in formula (I), that is, an alkyl group or a methyl group having 1 to 6 carbon atoms or 1 to 3 carbon atoms.

[0033] Specific examples of compound (II) include the following:

[0034]

[0035] In various embodiments, compound (II) can be selected from methyl 5-methylfuran-2-carboxylate (MMFC), methyl 5-(hydroxymethyl)furan-2-carboxylate, methyl 5-(methoxymethyl)furan-2-carboxylate, methyl 5-(ethoxymethyl)furan-2-carboxylate, ethyl 5-methylfuran-2-carboxylate, ethyl 5-(hydroxymethyl)furan-2-carboxylate, 5-(methoxymethyl)furan-2-carboxylate 5-(ethoxymethyl)furan-2-carboxylic acid ethyl ester, 5-methylfuran-2-carboxylic acid propyl ester, 5-(hydroxymethyl)furan-2-carboxylic acid propyl ester, 5-(methoxymethyl)furan-2-carboxylic acid propyl ester, 5-(ethoxymethyl)furan-2-carboxylic acid propyl ester, 5-methylfuran-2-carboxylic acid isopropyl ester, 5-(hydroxymethyl)furan-2-carboxylic acid isopropyl ester, 5-(methoxymethyl)furan-2-carboxylic acid isopropyl ester ester, methyl 5-((formyloxy)methyl)furan-2-carboxylate, methyl 5-(acetoxymethyl)furan-2-carboxylate, methyl 5-((propionyloxy)methyl)furan-2-carboxylate, ethyl 5-((formyloxy)methyl)furan-2-carboxylate, ethyl 5-(acetoxymethyl)furan-2-carboxylate, ethyl 5-((propionyloxy)methyl)furan-2-carboxylate, ethyl 5-((formyloxy)methyl)furan-2-carboxylate, 5-((propionyloxy)methyl)furan-2-carboxylic acid propyl ester, 5-((formyloxy)methyl)furan-2-carboxylic acid isopropyl 5-(acetoxymethyl)furan-2-carboxylate, 5-((propionyloxy)methyl)furan-2-carboxylate, 5-((formyloxy)methyl)furan-2-carboxylic acid isopropyl ester, 5-(acetoxymethyl)furan-2-carboxylic acid isopropyl ester, 5-((propionyloxy)methyl)furan-2-carboxylic acid isopropyl ester, 5-(ethoxymethyl)furan-2-carboxylic acid isopropyl ester, and mixtures thereof.

[0036] In various other embodiments, compound (II) can be selected from methyl 5-methylfuran-2-carboxylate (MMFC), methyl 5-(hydroxymethyl)furan-2-carboxylate, methyl 5-(methoxymethyl)furan-2-carboxylate, methyl 5-(ethoxymethyl)furan-2-carboxylate, methyl 5-((formyloxy)methyl)furan-2-carboxylate, methyl 5-(acetoxymethyl)furan-2-carboxylate, methyl 5-((propionyloxy)methyl)furan-2-carboxylate, and mixtures thereof.

[0037] In other various embodiments, compound (II) comprises methyl 5-methylfuran-2-carboxylate (MMFC).

[0038] The compound (II) can be prepared from renewable raw materials by literature methods and / or can be obtained commercially, for example, from xF Technologies Inc.

[0039] The oxidant used in the present method is not particularly limited. It refers to the source of oxygen. Preferably, the oxidant is an oxygen-containing gas. Examples include molecular oxygen, air and other oxygen-containing gases. The oxygen-containing gas introduced into the reactor may have 5 to 80 mol %, 5 to 60 mol %, 5 to 45 mol % or 15 to 25 mol % of molecular oxygen. The remainder of the oxygen-containing gas may be one or more gases inert to oxidation, such as nitrogen and argon.

[0040] The oxidation catalyst comprises cobalt, manganese and bromine. Cobalt, manganese and bromine can be provided by any suitable source. The catalyst components are generally derived from compounds that are soluble in the solvent under the reaction conditions or that are soluble in the reactants fed to the oxidation zone. Preferably, the source of the catalyst components is soluble in the solvent at 25°C, 30°C or 40°C and 1 atm, and / or is soluble in the solvent under the reaction conditions.

[0041] The cobalt may be provided in ionic form as an inorganic cobalt salt, such as cobalt bromide, cobalt nitrate or cobalt chloride, or as an organic cobalt compound, such as a cobalt salt of an aliphatic or aromatic acid having 2 to 22 carbon atoms, including cobalt acetate, cobalt octoate, cobalt benzoate, cobalt acetylacetonate and cobalt naphthoate.

[0042] When added as a compound to the reaction mixture, the oxidation state of the cobalt is not limited and includes the +2 and +3 oxidation states.

[0043] Manganese can be provided in the form of one or more inorganic manganese salts, such as manganese borate, manganese halide, manganese nitrate; or in the form of an organometallic manganese compound, such as manganese salts of lower aliphatic carboxylic acids, including manganese acetate; manganese salts of β-diketonates, including manganese acetylacetonate.

[0044] The bromine component can be added as elemental bromine, in a combined form or in an anionic form. Suitable bromine sources include hydrogen bromide, hydrobromic acid (sometimes referred to as aqueous hydrogen bromide or aqueous HBr), sodium bromide, potassium bromide, ammonium bromide and tetrabromoethane. Hydrobromic acid or sodium bromide may be preferred bromine sources.

[0045] Cobalt may be used in an amount ranging from 2 to 10,000 ppmw, 500 to 6,000 ppmw, 1,000 to 6,000 ppmw, 700 to 4,500 ppmw, or 1,000 to 4,000 ppmw.

[0046] Manganese may be used in an amount ranging from 2 to 10,000 ppmw, 2 to 600 ppmw, 20 to 400 ppmw, or 20 to 200 ppmw.

[0047] Bromine may be used in an amount ranging from 2 to 10,000 ppmw, 300 to 4,500 ppmw, 700 to 4,000 ppmw, or 1,000 to 4,000 ppmw.

[0048] These exemplary ranges for Co, Mn, and Br are based on the total weight of the reaction mixture.

[0049] Alternatively, the amount of catalyst can be expressed based on the weight of the raw material (i.e., compound (II)). In this case, the reaction can be carried out, for example, at a cobalt content of 0.50 to 5.0 weight % (wt%), a Mn content of 0.15 to 3.0 wt%, and a Br content of 0.11 to 3.2 wt%, based on the weight of compound (II).

[0050] In various embodiments, the cobalt content ranges from 0.50 to 1.0 wt%, the Mn content ranges from 1.5 to 2.3 wt%, and the bromine content ranges from 0.32 to 3.2 wt%, based on the weight of compound (II).

[0051] In various embodiments, the weight ratio of cobalt to manganese in the oxidation catalyst can be at least 0.01:1, at least 0.1:1, at least 1:1, at least 10:1, at least 20:1, at least 50:1, at least 100:1, or at least 400:1.

[0052] In other various embodiments, the weight ratio of Co:Mn in the oxidation catalyst may range from 1:1 to 400:1, 10:1 to 400:1, or 20:1 to 400:1.

[0053] In other various embodiments, the weight ratio of Co:Mn in the oxidation catalyst may range from 0.1:1 to 100:1, 0.1:1 to 10:1, 0.1:1 to 1:1, 1:1 to 100:1, 10:1 to 100:1, or 20:1 to 100:1.

[0054] In various embodiments, the weight ratio of cobalt to bromine may range from 0.7:1 to 3.5:1, 0.5:1 to 10:1, or 0.5:1 to 5:1.

[0055] The above-mentioned Co:Mn and Co:Br ratios can produce high-yield ACFCs, reduce the formation of impurities, including impurities that cause product discoloration (measured by b*), and / or keep the amount of CO and CO2 in the off-gas to a minimum.

[0056] The reaction solvent includes a monocarboxylic acid having 2 to 6 carbon atoms or 2 to 4 carbon atoms. Examples of such acids include acetic acid, propionic acid, n-butyric acid, isobutyric acid, n-pentanoic acid, trimethylacetic acid and caproic acid. A mixture of these acids and a mixture of one or more of the acids with water can be used. The solvent can be selected according to the ability of the solvent to dissolve the catalyst component under the reaction conditions. The solvent can also be selected according to the volatility of the solvent under the reaction conditions so that it is discharged from the oxidation reactor as a waste gas.

[0057] In various embodiments, the solvent includes anhydrous acetic acid, a mixture of peracetic acid and acetic acid, a mixture of acetic acid and water, or a mixture of peracetic acid, acetic acid, and water.

[0058] In other various embodiments, the solvent used for oxidation is an aqueous acetic acid solution, typically having a concentration of 50 to 99 wt%, 75 to 99 wt%, or 80 to 99 wt% acetic acid.

[0059] The solvent and catalyst used in the method can be recovered and reused. For example, the crude ACFC composition can be discharged from the oxidation reactor and subjected to various mother liquor exchange, separation, purification and / or recovery methods. These methods can provide recovered solvent and catalyst components for recycling back to the oxidation reactor. Therefore, a portion of the solvent introduced into the oxidation reactor can come from a recovery stream obtained by replacing, for example, 80 to 90 wt% of the mother liquor in the crude reaction mixture discharged from the oxidation reactor. The mother liquor can be replaced with fresh wet acetic acid, for example, acetic acid containing greater than 0 to 20 wt% or greater than 0 to 15 wt% of water.

[0060] Generally, the oxidation reaction can be conducted at a temperature of 50°C to 220°C, 75°C to 200°C, 75°C to 180°C, 100°C to 180°C, 110°C to 180°C, 130°C to 180°C, 100°C to 160°C, 110°C to 160°C, or 130°C to 160°C. A typical oxidation reactor is characterized by a lower portion where gas bubbles are dispersed in a continuous liquid phase. Solids may also be present in the lower portion. In the upper portion of the reactor, gas is the continuous phase, and entrained droplets may also be present therein. These oxidation temperatures refer to the temperature of the reaction mixture within the oxidation reactor where the liquid is present as the continuous phase.

[0061] In various embodiments, the liquid phase in the oxidation reactor has a pH of -4.0 to 2.0.

[0062] Typically, the oxidation reaction can be carried out at a pressure above the reaction mixture, such as 50 to 1,000 psig, 50 to 750 psig, 50 to 500 psig, 50 to 400 psig, 50 to 200 psig, 100 to 1000 psig, 100 to 750 psig, 100 to 500 psig, 100 to 400 psig, 100 to 300 psig, or 100 to 200 psig. The pressure is typically selected so that the solvent is primarily in the liquid phase.

[0063] The oxidation process can be carried out in batch, semi-continuous (sometimes referred to as semi-batch) or continuous mode. The batch process generally involves adding the entire amount of compound (II) starting material, catalyst and solvent to a reactor before starting the reaction, passing an oxidizing gas through the reaction mixture to initiate and carry out the reaction, and recovering the reaction mixture once at the end of the reaction.

[0064] The semi-continuous method generally involves adding the entire amount of catalyst and solvent into a reactor, continuously introducing the compound (II) raw material and an oxidizing gas into the reactor to carry out an oxidation reaction, and recovering the reaction mixture all at once at the end of the reaction.

[0065] The continuous process generally involves continuously introducing the feedstock, catalyst, solvent and oxidizing gas into a reactor to carry out the oxidation reaction, and continuously recovering the reaction mixture containing the product compound (I).

[0066] The oxidation reaction time may vary depending on various factors such as temperature, pressure and catalyst composition / concentration applied. However, in general, the reaction time may range from 1 to 6 hours or 1 to 3 hours.

[0067] The present process may produce Compound (I) in a yield of at least 50%, at least 60%, at least 70%, at least 80%, at least 85%, at least 90%, at least 95%, at least 98%, at least 99% or at least 99.5%.

[0068] The yield can be calculated by dividing the mass of the obtained ACFC (compound (I)) by the theoretical amount of the oxidizable raw material (compound (II)) that should be produced based on the amount of raw material consumed. For example, in the case of MMFC as compound (II), if one mole or 140.1 grams of MMFC are oxidized, theoretically one mole or 170.1 grams of MCFC will be produced. For example, if the actual amount of MCFC generated is only 150 grams, the MCFC yield of the reaction can be 88.2% (=150 / 170.1x100). The same calculation can be performed for oxidation reactions using other oxidizable compounds and other products / by-products.

[0069] In addition to compound (I), the present method may also produce one or more by-products. These by-products include furan-2,5-dicarboxylic acid (FDCA), 5-formylfuran-2-carboxylic acid (FFCA) and 5-formylfuran-2-carboxylic acid alkyl ester (AFFC). 2 When it is a methyl group, AFFC is methyl 5-formylfuran-2-carboxylate (MFFC). The structural formulas of FDCA, FFCA, AFFC and MFFC are as follows.

[0070]

[0071] In various embodiments, the present methods produce FDCA in a yield of less than 20%, less than 15%, less than 10%, less than 5%, less than 1%, or less than 0.5%.

[0072] In the process of the present invention, the extent of solvent burn and unusability can be the same as or even lower than that of a typical oxidation process, as estimated by the carbon oxide formation. Even though the absolute amount of carbon oxide formation can be reduced by known techniques, such reduction can be achieved without affecting acceptable conversion rates. Lower amounts of carbon oxide formation can generally be obtained by conducting the reaction at lower oxidation temperatures and / or using catalysts with lower levels of conversion or selectivity, but this generally results in reduced conversion and increased intermediate production. However, compared to other oxidation processes, the present process has the advantage of maintaining a lower ratio of solvent burn to conversion, thereby minimizing the effect on conversion to obtain lower solvent burn.

[0073] Thus, in various embodiments, the carbon oxide formation ratio (in terms of CO per mole of compound (II) feed) is x The moles of CO and CO2 represented by the formula (denoted by the formula (a)) may not exceed 1.0 mole of CO x , or not more than 0.5 mol CO x , or not more than 0.3 mol CO x , in each case relative to the number of moles of compound (II) fed to the reactor.

[0074] At the end of the reaction, the reaction mixture is usually decompressed and cooled to obtain a slurry comprising the product compound (I). The product slurry may be subjected to one or more solid-liquid separations (such as filtration and / or centrifugation) and washing steps to obtain a wet cake. The wet cake may then be dried (optionally at elevated temperature and vacuum) to obtain a dry solid product composition.

[0075] In various embodiments, the process of the present invention may comprise one or more steps to obtain a dry solid product composition comprising compound (I).

[0076] These steps include passing at least a portion of the oxidation reaction mixture through a crystallization zone at the end of the oxidation reaction to form a crystal slurry. Generally, the crystallization zone includes at least one crystallizer. In the crystallization zone, the reaction mixture can be cooled to a temperature of 20°C to 175°C, 40°C to 175°C, 50°C to 170°C, 60°C to 165°C, 25°C to 100°C or 25°C to 50°C to form a crystal slurry. The steam from the crystallization zone can be condensed in at least one condenser and then returned to the crystallization zone or discharged from the crystallization zone. Alternatively, the steam in the crystallization zone can also be directly recycled without condensation, or sent to an energy recovery facility. As another option, the crystallizer vapor can be extracted and transported to a recovery system, in which the solvent is removed and recovered, and any volatile organic compounds (VOCs) can be treated, for example, by incineration in a catalytic oxidation device.

[0077] The crystal slurry can be further cooled in a cooling zone to generate a cooled crystal slurry. Cooling can be accomplished by any method known in the art. The cooling zone typically includes a flash tank. The temperature range of the cooled crystal slurry is 20°C to 160°C, 35°C to 160°C, 20°C to 140°C, 50°C to 140°C, 20°C to 120°C, 25°C to 120°C, 45°C to 120°C, 70°C to 120°C, 55°C to 95°C, 75°C to 95°C, or 20°C to 70°C.

[0078] In various embodiments, at least a portion (up to 100%) of the oxidation mixture may be conveyed directly to the cooling zone without prior passage through a crystallization zone.

[0079] In other various embodiments, at least a portion (up to 100%) of the crystallization slurry may be directly conveyed to the solid-liquid separation zone without prior passage through a cooling zone.

[0080] The cooled crystal slurry may enter a solid-liquid separation zone. The solid-liquid separation zone typically includes one or more solid-liquid separation devices configured to separate solids from liquids. In the solid-liquid separation zone, the solids may be washed with a wash solvent and dehydrated by reducing the moisture content of the washed solids to less than 30 wt%, less than 25 wt%, less than 20 wt%, less than 15 wt%, or less than 10 wt%.

[0081] Apparatus suitable for the solid-liquid separation zone typically include centrifuges, cyclone separators, rotary drum filters, belt filters, pressure leaf filters, candle filters, and the like.

[0082] In various embodiments, the solid-liquid separation zone comprises a rotary pressure drum filter.

[0083] The wash solvent comprises a liquid suitable for displacing and washing the mother liquor from the solid.

[0084] In various embodiments, the wash solvent comprises acetic acid and water.

[0085] In other various embodiments, the wash solvent comprises water (up to 100%).

[0086] The temperature of the wash solvent ranges from 20°C to 135°C, 40°C to 110°C, 50°C to 90°C, or 20°C to 70°C. The amount of wash solvent that can be used can be characterized by a wash ratio, which corresponds to the mass of wash liquid divided by the mass of the batch or continuous solids. The wash ratio ranges from 0.3 to 5, 0.4 to 4, or 0.5 to 3.

[0087] After the solids are washed in the solid-liquid separation zone, they are typically dewatered to produce a purified wet cake. Dewatering involves reducing the moisture content of the solids to less than 30 wt%, less than 25 wt%, less than 20 wt%, less than 15 wt% or less than 10 wt%.

[0088] In various embodiments, dehydration is accomplished in a filter by passing a gas stream through the solids to displace free liquid after the solids have been washed with a wash solvent.

[0089] In other various embodiments, dewatering is achieved by centrifugal force in a perforated or solid bowl centrifuge.

[0090] The filtrate produced in the solid-liquid separation zone is a mother liquor containing the oxidation solvent, catalyst and some impurities / oxidation by-products. The filtrate can be sent to a purge zone or returned to the oxidation reactor, or both.

[0091] In the purification zone, a portion of the impurities present in the mother liquor can be separated and removed. The remaining solvent and catalyst can be separated and recycled to the oxidation reactor.

[0092] In various embodiments, the remaining solvent from the purification zone may contain greater than 30%, greater than 50%, greater than 70%, or greater than 90% of the catalyst entering the purification zone continuously or batchwise.

[0093] The washing liquid from the solid-liquid separation zone usually contains a part of mother liquor and washing solvent. The ratio of the mother liquor mass to the washing solvent mass can be less than 3 or less than 2.

[0094] The purified wet cake from the solid-liquid separation zone may enter a drying zone to generate a dry solid product and a vapor stream. The vapor stream may include scrubbing solvent vapor and / or oxidation solvent vapor.

[0095] The drying zone typically comprises one or more dryers capable of evaporating at least 10% of the volatiles remaining in the purified wet cake. Examples of such dryers include indirect contact dryers such as rotary steam tube dryers, single shaft Porcupine dryers,TM Dryer and Bepex Solidaire TM Dryers, as well as direct contact dryers such as fluidized bed dryers and conveyor-equipped drying ovens.

[0096] In various embodiments, a vacuum system may be used to draw the steam stream from the drying zone. If a vacuum system is used in this manner, the pressure of the steam stream at the dryer outlet may range from 760 mm Hg to 400 mm Hg, 760 mm Hg to 600 mm Hg, 760 mm Hg to 700 mm Hg, 760 mm Hg to 720 mm Hg, or 760 mm Hg to 740 mm Hg, where the pressure is measured in mm Hg above absolute vacuum.

[0097] The process according to the invention can produce a dry solid product containing compound (I) which is unexpectedly pure and low in color without the need for reactive purification steps such as secondary oxidation (sometimes referred to as post-oxidation), hydrogenation and / or treatment with an oxidizing agent (such as sodium hypochlorite and / or hydrogen peroxide).

[0098] In a batch process, secondary oxidation refers to the step of continuing to feed the oxidizing gas into the reactor after the absorption of oxygen in the reaction medium has ceased. In a semi-continuous or continuous process, secondary oxidation refers to the step of continuing to feed the oxidizing gas into the reaction zone after the supply of the compound (II) starting material has ceased.

[0099] Thus, in a second aspect, the present invention provides a dry solid composition comprising at least 70 wt% of a compound of formula (I):

[0100]

[0101] Where R 2 In the above definition, the wt% of compound (I) is based on the total weight of the composition.

[0102] In various embodiments, the dry solid composition comprises at least 80 wt%, at least 90 wt%, at least 95 wt%, at least 97 wt%, at least 98 wt%, at least 99 wt%, or at least 99.5 wt% of Compound (I), based on the total weight of the composition.

[0103] In various embodiments, the dry solid composition comprises less than 30 wt%, less than 20 wt%, less than 10 wt%, less than 5 wt%, less than 3 wt%, less than 2 wt%, less than 1 wt%, or less than 0.05 wt% furan-2,5-dicarboxylic acid (FDCA), based on the total weight of the composition. In each case, the FDCA content may be greater than 0 wt%.

[0104] In various embodiments, the dry solid composition comprises less than 1 wt%, less than 0.5 wt%, less than 0.3 wt%, less than 0.1 wt%, less than 500 ppmw, less than 400 ppmw, less than 300 ppmw, less than 200 ppmw, less than 100 ppmw, less than 50 ppmw, less than 10 ppmw, less than 5 ppmw, or less than 1 ppmw of 5-formylfuran-2-carboxylic acid (FFCA), based on the total weight of the composition. In each case, the content of FFCA may be greater than 0 wt%.

[0105] In various embodiments, the dry solid composition comprises less than 1 wt%, less than 0.5 wt%, less than 0.3 wt%, less than 0.1 wt%, less than 500 ppmw, less than 400 ppmw, less than 300 ppmw, less than 200 ppmw, less than 100 ppmw, less than 50 ppmw, or less than 10 ppmw of alkyl 5-formylfuran-2-carboxylate (AFFC), based on the total weight of the composition. In each case, the AFFC content may be greater than 0 wt%.

[0106] When R 2 When methyl, the dry solid composition contains less than 1 wt%, less than 0.5 wt%, less than 0.3 wt%, less than 0.1 wt%, less than 500 ppmw, less than 400 ppmw, less than 300 ppmw, less than 200 ppmw, less than 100 ppmw, less than 50 ppmw or less than 10 ppmw of 5-formylfuran-2-carboxylic acid methyl ester (MFFC), based on the total weight of the composition. In each case, the content of MFFC may be greater than 0 wt%.

[0107] In various embodiments, the dried solid composition may have a b* value of less than 4, less than 2, less than 1, from -1 to +1, or from -0.5 to +0.5.

[0108] The b* value is one of the three color properties measured on an instrument based on spectral reflectance. Chroma can be measured by any device known in the art. The Hunter Ultrascan XE instrument is a typical measurement device. Positive readings indicate the degree of yellowness (or blue absorbance) and negative readings indicate the degree of blueness (or yellow absorbance).

[0109] In one embodiment, the dry solid composition comprises

[0110] (a) at least 70% by weight of compound (I);

[0111] (b) less than 30 wt% furan-2,5-dicarboxylic acid (FDCA);

[0112] (c) less than 500 ppmw of 5-formylfuran-2-carboxylic acid (FFCA); and

[0113] (d) less than 1000 ppmw of alkyl 5-formylfuran-2-carboxylate (AFFC),

[0114] All amounts are based on the total weight of the composition, and

[0115] Wherein the composition has a b* value of less than 4.

[0116] In another embodiment, the dry solid composition comprises

[0117] (a) at least 70 wt% of 5-(methoxycarbonyl)furan-2-carboxylic acid (MCFC);

[0118] (b) less than 30 wt% furan-2,5-dicarboxylic acid (FDCA);

[0119] (c) less than 500 ppmw of 5-formylfuran-2-carboxylic acid (FFCA); and

[0120] (d) less than 500 ppmw of methyl 5-formylfuran-2-carboxylate (MFFC);

[0121] All amounts are based on the total weight of the composition, and

[0122] Wherein the composition has a b* value of less than 4.

[0123] In another embodiment, the dry solid composition comprises

[0124] (a) at least 99 wt % of 5-(methoxycarbonyl)furan-2-carboxylic acid (MCFC);

[0125] (b) less than 500 ppmw of furan-2,5-dicarboxylic acid (FDCA);

[0126] (c) less than 10 ppmw of 5-formylfuran-2-carboxylic acid (FFCA); and

[0127] (d) less than 100 ppmw of methyl 5-formylfuran-2-carboxylate (MFFC);

[0128] All amounts are based on the total weight of the composition, and

[0129] Wherein the composition has a b* value from -1 to +1.

[0130] In another embodiment, the dry solid composition comprises

[0131] (a) at least 99 wt % of 5-(methoxycarbonyl)furan-2-carboxylic acid (MCFC);

[0132] (b) less than 500 ppmw of furan-2,5-dicarboxylic acid (FDCA);

[0133] (c) less than 10 ppmw of 5-formylfuran-2-carboxylic acid (FFCA); and

[0134] (d) less than 100 ppmw of methyl 5-formylfuran-2-carboxylate (MFFC),

[0135] All amounts are based on the total weight of the composition, and

[0136] Wherein the composition has a b* value of -0.5 to +0.5.

[0137] In various embodiments, a dry solid composition is obtained without performing or undergoing a reaction purification step.

[0138] In other various embodiments, the dried solid composition is obtained without performing or undergoing a secondary oxidation step, a hydrogenation step, and / or a treatment step with an oxidizing agent.

[0139] In other various embodiments, the dried solid composition is polymer grade, ie, it is of sufficient purity to be used in making polymers without performing or undergoing reactive purification steps, such as secondary oxidation steps, hydrogenation steps, and / or treatment steps with oxidizing agents.

[0140] To eliminate any doubt, the present invention includes and explicitly considers and discloses any and all combinations of the embodiments, features, characteristics, parameters and / or ranges mentioned herein. That is, the subject matter of the present invention can be defined by any combination of the embodiments, features, characteristics, parameters and / or ranges mentioned herein.

[0141] Any component, ingredient or step not specifically identified or identified as part of the invention may be considered to be expressly excluded.

[0142] Any method, device, compound, composition, embodiment, or component of the present invention may be modified by the transition terms "comprising," "consisting essentially of," or "composed of," or variations of these terms.

[0143] As used herein, the indefinite articles "a" and "an" refer to one or more, unless the context clearly indicates otherwise. Likewise, singular forms of nouns include their plural forms and vice versa, unless the context clearly indicates otherwise.

[0144] Although precision is sought herein, the values ​​and ranges described herein should be considered approximate unless the context indicates otherwise. These values ​​and ranges may differ from the numbers they describe, depending on the desired properties sought to be obtained by the present disclosure and the variations caused by standard deviations found in the measurement techniques. In addition, the ranges described herein are intended and specifically contemplated to include all subranges and values ​​within the described ranges. For example, a range of 50 to 100 is intended to include all values ​​within that range, including subranges such as 60 to 90, 70 to 80, etc.

[0145] Any two numbers of the same property or parameter recorded in the working examples can define a range. These numerical values ​​can be rounded to the nearest thousandth, hundredth, tenth, integer, ten, hundredth or thousand to define the range.

[0146] All the contents of the literature cited herein, including patents and non-patent literature, are incorporated into this specification in their entirety by reference. If any incorporated subject matter conflicts with the content disclosed herein, the content disclosed herein takes precedence over the incorporated content.

[0147] The present invention can be further illustrated by the following working examples, but it should be understood that these examples are only for illustrative purposes and are not intended to limit the scope of the present invention.

[0148] It should be understood that the following is not an exclusive list of defined terms. Other definitions may also be provided in the foregoing description, for example, when the defined terms are used in the context. When appropriate starting materials are used, the present method may also be used for MCFC and ACFC as described above. Suitable starting materials are also described above.

[0149] As used herein, the terms "a," "an," and "the" refer to one or more.

[0150] As used herein, the term "and / or" when used with a list of two or more items means that any one of the listed items can be used alone, or any combination of two or more of the listed items can be used. For example, if a composition is described as containing components A, B, and / or C, the composition can contain A alone; B alone; C alone; A and B in combination; A and C in combination; B and C in combination; or A, B, and C in combination.

[0151] As used herein, the terms “comprising,” “including,” and “comprising” are open transition terms used to transition from an object listed before the term to one or more elements listed after the term, where the one or more elements listed after the transition term are not necessarily the only elements making up the object.

[0152] As used herein, the terms "having," "having," and "having" have the same open-ended meaning as "comprising," "including," and "comprising" provided above.

[0153] As used herein, the terms "comprising," "including," and "comprising" have the same open-ended meaning as "comprises," "comprising," and "including" provided above.

[0154] This specification uses numerical ranges to quantify certain parameters associated with the present invention. It should be understood that when numerical ranges are provided, these ranges should be interpreted as literally supporting claim limitations that only list the lower limit of the range and claim limitations that only list the upper limit of the range. For example, a public numerical range of 10 to 100 provides literal support for a claim that lists "greater than 10" (no upper limit) and a claim that lists "less than 100" (no lower limit).

[0155] This specification uses specific numerical values ​​to quantify certain parameters related to the present invention, wherein the specific numerical values ​​are not explicitly part of the numerical range. It should be understood that each specific numerical value provided herein should be interpreted as providing literal support for wide, medium and narrow ranges. The wide range associated with each specific numerical value is 60% of the numerical value plus and minus the numerical value, rounded to two significant digits. The medium range associated with each specific numerical value is 30% of the numerical value plus and minus the numerical value, rounded to two significant digits. The narrow range associated with each specific numerical value is 15% of the numerical value plus and minus the numerical value, rounded to two significant digits. For example, if this specification describes a specific temperature of 62°F, this description provides literal support for the wide numerical range of 25°F to 99°F (62°F+ / -37°F), the medium numerical range of 43°F to 81°F (62°F+ / -19°F), and the narrow numerical range of 53°F to 71°F (62°F+ / -9°F). These broad, medium, and narrow ranges should apply not only to the specific values, but also to the differences between these specific values. Thus, if the specification describes a first pressure of 110 psia and a second pressure of 48 psia (a difference of 62 psi), the broad, medium, and narrow ranges for the pressure difference between the two streams would be 25 to 99 psi, 43 to 81 psi, and 53 to 71 psi, respectively.

[0156] One embodiment of the present invention is as follows Figure 1 and Figure 2 The present invention provides a method for recovering a portion of the oxidation solvent, a portion of the oxidation catalyst and removing a portion of the oxidation by-products and raw material impurities from a solvent stream produced in a process for producing furan-2,5-dicarboxylic acid (FDCA). The methods discussed below can be combined with the previous methods in any logical order.

[0157] Step (a) comprises feeding an oxidation solvent, a catalyst system, a gas stream comprising oxygen, and an oxidizable raw material comprising at least one compound selected from the group consisting of 5-(hydroxymethyl)furfural (5-HMF), 5-(chloromethyl)furfural (5-CMF), 2,5-dimethylfuran (2,5-DMF), 5-HMF esters (5-R(CO)OCH2-furfural, wherein R = alkyl, cycloalkyl and aryl), 5-HMF ethers (5-R'OCH2-furfural, wherein R' = alkyl, cycloalkyl and aryl), 5-alkylfurfurals (5-R"-furfural, wherein R" = alkyl, cycloalkyl and aryl), alkyl), alkyl carboxylates of methylfuran (5-R"'O(CO)-methylfuran, wherein R"'=alkyl, cycloalkyl), alkyl carboxylates of alkoxyfuran (5-R""O(CO)-OR""'furan, wherein R""=alkyl, cycloalkyl and aryl, and R""'=alkyl, cycloalkyl and aryl), a mixed raw material of 5-HMF and 5-HMF ester, a mixed raw material of 5-HMF and 5-HMF ether, a mixed raw material of 5-HMF and 5-alkylfuran, a mixed raw material of 5-HMF and 5-CMF, a mixed raw material of 5-HMF and 2,5-DMF, a mixed raw material of 5-HMF and alkyl carboxylates of methylfuran, and a mixed raw material of 5-HMF and alkyl carboxylates of alkoxyfuran.

[0158] The structures of preferred oxidizable starting compounds are summarized below:

[0159] Preferred 5-HMF derivative feedstocks

[0160]

[0161] 5-HMF feed is oxidized with elemental O2 in a multi-step reaction to form FDCA containing 5-formylfuran-2-carboxylic acid (FFCA) as a key intermediate (Formula 1). Oxidation of 5-(acetoxymethyl)furfural (5-AMF), which contains oxidizable ester and aldehyde moieties, produces FDCA, FFCA, and acetic acid (Formula 2). Similarly, oxidation of 5-(ethoxymethyl)furfural (5-EMF) produces FDCA, FFCA, 5-(ethoxycarbonyl)furan-2-carboxylic acid (EFCA), and acetic acid (Formula 3).

[0162]

[0163] The feed stream sent to the primary oxidation zone 100 includes a gas stream 10 containing oxygen, and a stream 30 containing an oxidation solvent, and a stream 20 containing an oxidizable raw material. In another embodiment, the feed stream sent to the oxidation zone 100 includes a gas stream 10 containing oxygen, and a stream 20 containing an oxidation solvent, a catalyst, and an oxidizable raw material. In yet another embodiment, the oxidation solvent, oxygen-containing gas, catalyst system, and oxidizable raw material can be fed to the oxidation zone 100 as separate and individual streams, or mixed in any combination before entering the oxidation zone 100, wherein the feed streams can enter the oxidizer zone 100 at a single location or at multiple locations.

[0164] A suitable catalyst system is at least one compound selected from, but not limited to, cobalt, bromine and manganese compounds, which is soluble in the selected oxidation solvent. A preferred catalyst system comprises cobalt, manganese and bromine, wherein the weight ratio of cobalt to manganese in the reaction mixture is from about 10 to about 400, and the weight ratio of cobalt to bromine is from about 0.7 to about 3.5. The data shown in Table 1 show that very high FDCA yields can be obtained using 5-HMF or a derivative thereof and using the above catalyst composition.

[0165] Suitable oxidation solvents include, but are not limited to, aliphatic monocarboxylic acids, preferably containing 2 to 6 carbon atoms, and mixtures thereof, and mixtures of these compounds with water. In one embodiment, the oxidation solvent comprises acetic acid, wherein the weight % of acetic acid in the oxidation solvent is greater than 50%, greater than 75%, greater than 85%, and greater than 90%. In another embodiment, the oxidation solvent comprises acetic acid and water, wherein the ratio of acetic acid to water is greater than 1:1, greater than 6:1, greater than 7:1, greater than 8:1, and greater than 9:1.

[0166] The temperature of the oxidation zone may range from 100°C to 220°C, or 100°C to 200°C, or 130°C to 180°C, or 100°C to 180°C, preferably in the range of 110°C to 160°C. In another embodiment, the temperature of the oxidation zone may range from 105°C to 140°C.

[0167] One advantage of the disclosed oxidation conditions is low carbon combustion, as shown in Table 1. The oxidizer off-gas stream 120 is sent to the oxidizer off-gas treatment zone 800 to produce an inert gas stream 810, a liquid stream 820 comprising water, and a recovered oxidation solvent stream 830 comprising a condensed solvent. In one embodiment, in order to wash the solids present in the solid-liquid separation zone, at least a portion of the recovered oxidation solvent stream 830 is sent to the washing solvent stream 320 to become part of the washing solvent stream 320. In another embodiment, the inert gas stream 810 can be discharged to the atmosphere. In yet another embodiment, at least a portion of the inert gas stream 810 can be used as an inert gas in the process of inerting the container and / or a conveying gas for solids in the process. In another embodiment, at least a portion of the energy in the stream 120 is recovered in the form of steam and / or electricity.

[0168] In another embodiment of the present invention, a method for producing furan-2,5-dicarboxylic acid (FDCA) in high yield by liquid phase oxidation is provided, which minimizes solvent and raw material losses due to carbon combustion. The method includes oxidizing at least one oxidizable compound in an oxidizable raw material stream 30 in the presence of an oxidizing gas stream 10, an oxidizing solvent stream 20, and at least one catalyst system in an oxidation zone 100; wherein the oxidizable compound is 5-(hydroxymethyl)furfural (5-HMF); wherein the solvent stream comprises acetic acid in the presence or absence of water; wherein the catalyst system comprises cobalt, manganese, and bromine, wherein the weight ratio of cobalt to manganese in the reaction mixture is from about 10 to about 400. In the method, the temperature can vary from about 100°C to about 220°C, from about 105°C to about 180°C, and from about 110°C to about 160°C. The catalyst system may have a cobalt concentration of about 1000 ppm to about 6000 ppm, and manganese in an amount of about 2 ppm to about 600 ppm, and bromine in an amount of about 300 ppm to about 4500 ppm, relative to the total weight of liquid in the reaction medium.

[0169] Step (b) comprises sending the crude carboxylic acid stream 110 comprising FDCA to a cooling zone 200 to produce a cooled crude carboxylic acid slurry stream 210 and a first steam stream 220 comprising oxidation solvent steam. The cooling of the crude carboxylic acid slurry stream 110 can be accomplished by any method known in the art. The cooling zone 200 typically comprises flashing or evaporation of the solvent. The cooling zone 200 can be operated in batches or continuously. In one embodiment, the cooling zone 200 uses a vacuum to control the solvent cooling rate. In another embodiment, the cooling zone 200 is conducted through a jacketed container and an internal cooling coil. The crude carboxylic acid stream 110 comprises FDCA and a solvent, wherein the FDCA is supersaturated. Supersaturation refers to a state in which the liquid (solvent) comprises more dissolved FDCA solids (solutes) than those dissolved in a normal solution at that temperature. The temperature range of the crude carboxylic acid stream 110 is 35°C to 210°C, 55°C to 120°C, preferably 75°C to 95°C. The crude carboxylic acid stream 110 is cooled in the cooling zone 200 to produce a cooled crude carboxylic acid slurry stream 210 having a temperature in the range of 5°C to 65°C, 10°C to 50°C, 15°C to 40°C, preferably 15°C to 30°C. The cooling rate is controlled so that the solvent remains supersaturated with FDCA throughout the cooling cycle, but is allowed to drop below supersaturation when the final temperature of the cooled crude carboxylic acid slurry stream 210 is reached. The cooling rate in the cooling zone 200 may range from 0.1°C / min to 20°C / min, 0.3°C / min to 15°C / min, preferably 0.5°C / min to 10°C / min. FDCA crystals are produced in the cooling zone 200. The average particle size of the FDCA solids present in the crude carboxylic acid slurry stream 210 ranges from 20 microns to 500 microns, 25 microns to 250 microns, 25 microns to 75 microns, preferably 25 microns to 60 microns. In another embodiment, at least 90% of the FDCA solids present in the crude carboxylic acid slurry stream 210 may have an average particle size ranging from 20 microns to 500 microns, 25 microns to 250 microns, 25 microns to 75 microns, preferably 25 microns to 60 microns. In another embodiment, at least 80% of the FDCA solids present in the crude carboxylic acid slurry stream 210 may have an average particle size ranging from 20 microns to 500 microns, 25 microns to 250 microns, 25 microns to 75 microns, preferably 25 microns to 60 microns.

[0170] In another embodiment, a portion (up to 100%) of the crude carboxylic acid slurry stream 110 is directly sent to the solid-liquid separation zone 300, and thus the portion (up to 100%) does not need to be cooled in the cooling zone 200. The temperature of the stream 110 may range from 35°C to 210°C, 55°C to 120°C, and preferably from 75°C to 95°C.

[0171] Step (c) comprises separating, washing and dehydrating the solids present in the cooled crude carboxylic acid slurry stream 210 in a solid-liquid separation zone 300 to produce a crude carboxylic acid wet cake stream 310 comprising FDCA. These functions can be achieved in a single solid-liquid separation device or multiple solid-liquid separation devices. The solid-liquid separation zone comprises at least one solid-liquid separation device capable of separating solids and liquids, washing the solids with a washing solvent stream 320, and reducing the moisture % in the washed solids to less than 30 wt%, less than 20 wt%, less than 15 wt%, and preferably less than 10 wt%.

[0172] Suitable equipment for the solid-liquid separation zone can generally be at least one of the following types of devices: centrifuge, cyclone separator, drum filter, belt filter, pressure blade filter, candle filter, etc. The preferred solid-liquid separation device for the solid-liquid separation zone is a rotary pressure drum filter.

[0173] The temperature of the cooled crude carboxylic acid slurry stream 210 sent to the solid-liquid separation zone 300 can be 35°C to 210°C, 55°C to 120°C, and preferably 75°C to 95°C. The washing solvent stream 320 comprises a liquid suitable for displacing and washing mother liquor from the solid. In one embodiment, a suitable washing solvent comprises acetic acid. In another embodiment, a suitable washing solvent comprises acetic acid and water. In yet another embodiment, a suitable washing solvent comprises water and can be 100% water. The temperature of the washing solvent can be 20°C to 160°C, 40°C to 110°C, and preferably 50°C to 90°C.

[0174] The amount of wash solvent used is defined as the wash ratio and is equal to the mass of wash divided by the mass of solids (on an intermittent or continuous basis). The wash ratio can be from about 0.3 to about 5, from about 0.4 to about 4, and preferably from about 0.5 to 3. After the solids are washed in the solid-liquid separation zone, they are dehydrated. Dehydration involves reducing the mass of water present with the solids to less than 30 wt%, less than 25 wt%, less than 20 wt%, and most preferably less than 15 wt%, resulting in the production of a crude carboxylic acid wet cake stream 310 comprising FDCA.

[0175] In one embodiment, after washing the solids with the wash solvent, dewatering is accomplished in a filter by passing a gas-containing stream through the solids to displace free liquid. In one embodiment, dewatering of the wet cake solids in the solid-liquid separation zone 300 can be performed before and after the wet cake solids in the wash zone 300 to minimize the amount of oxidant solvent present in the wash liquid stream 340. In another embodiment, dewatering is accomplished by centrifugal force in a porous or solid drum centrifuge.

[0176] The mother liquor stream 330 generated in the solid-liquid separation zone 300 contains the oxidation solvent, the catalyst, and the impurities. 5 wt % to 95 wt %, 30 wt % to 90 wt %, and most preferably 40 wt % to 80 wt % of the mother liquor present in the crude carboxylic acid slurry 110 is separated in the solid-liquid separation zone 300 to generate the mother liquor stream 330 so that dissolved materials containing impurities present in the mother liquor stream 330 no longer enter the process.

[0177] In one embodiment, a portion of mother liquor stream 330 is sent to mother liquor purification zone 700, wherein the portion is at least 5 weight percent, at least 25 weight percent, at least 45 weight percent, at least 55 weight percent, at least 75 weight percent, or at least 90 weight percent. In another embodiment, at least a portion of mother liquor stream 330 is sent back to oxidation zone 100, wherein the portion is at least 5 weight percent. In yet another embodiment, at least a portion of mother liquor stream 330 is sent to mother liquor purification zone 700 and oxidation zone 100, wherein the portion is at least 5 weight percent. In one embodiment, mother liquor purification zone 700 includes an evaporation step to separate the oxidation solvent from stream 330 by evaporation. Solids may be present in mother liquor stream 330 at about 5 weight percent to about 0.5 weight percent. In another embodiment, any portion of the mother liquor stream 330 sent to the mother liquor purification zone is first subjected to a solid-liquid separation device to control the solids present in the stream 330 to less than 1 wt%, less than 0.5 wt%, less than 0.3 wt%, or less than 0.1 wt%. Suitable solid-liquid separation equipment includes a disc centrifuge and an intermittent filter press solid-liquid separation device. Preferred solid-liquid separation devices for use in the present application include intermittent candle filters.

[0178] Wash liquor stream 340 is generated in solid-liquid separation zone 300 and comprises a portion of the mother liquor present in stream 210 and a wash solvent, wherein the ratio of the mass of mother liquor to the mass of wash solvent is less than 3 and preferably less than 2. In one embodiment, at least a portion of wash liquor stream 340 is sent to oxidation zone 100, wherein the portion is at least 5 wt%. In one embodiment, at least a portion of wash liquor stream is sent to mother liquor purification zone 700, wherein the portion is at least 5 wt%. In another embodiment, at least a portion of wash liquor stream 340 is sent to oxidation zone 100 and mother liquor purification zone 700, wherein the portion is at least 5 wt%.

[0179] In another embodiment, at least a portion (up to 100 wt%) of the crude carboxylic acid slurry stream 110 is sent directly to the solid-liquid separation zone 300, whereby the portion will bypass the cooling zone 200. In this embodiment, the feed to the solid-liquid separation zone 300 comprises at least a portion of the crude carboxylic acid slurry stream 110 and a wash solvent stream 320 to produce a crude carboxylic acid wet cake stream 310 comprising FDCA. The solids in the feed slurry are separated, washed and dehydrated in the solid-liquid separation zone 300. These functions can be achieved in a single solid-liquid separation device or in multiple solid-liquid separation devices. The solid-liquid separation zone includes at least one solid-liquid separation device capable of separating solids and liquids, washing solids with a wash solvent stream 320, and reducing the moisture % in the washed solids to less than 30 wt%, less than 20 wt%, less than 15 wt%, and preferably less than 10 wt%. The equipment suitable for the solid-liquid separation zone can generally be at least one of the following types of devices: centrifuge, cyclone separator, drum filter, belt filter, pressure leaf filter, candle filter, etc. The preferred solid-liquid separation device for the solid-liquid separation zone 300 is a continuous drum filter press. The temperature of the crude carboxylic acid slurry stream sent to the solid-liquid separation zone 300 can be 40°C to 210°C, 60°C to 170°C, and preferably 80°C to 160°C. The washing stream 320 contains a liquid suitable for replacing and washing mother liquor from the solid. In one embodiment, a suitable washing solvent comprises acetic acid and water. In another embodiment, a suitable washing solvent comprises water with up to 100% water. The temperature of the washing solvent can be 20°C to 180°C, 40°C to 150°C, and preferably 50°C to 130°C. The amount of washing solvent used is defined as the washing ratio, and is equal to the mass of the detergent (mass of wash) divided by the mass of the solid on an intermittent or continuous basis. The wash ratio may be about 0.3 to about 5, about 0.4 to about 4, and preferably about 0.5 to 3.

[0180] After washing the solids in the solid-liquid separation zone, they are dehydrated. Dehydration includes reducing the mass of water present with the solids to less than 30% by weight, less than 25% by weight, less than 20% by weight, and most preferably less than 15% by weight, resulting in the generation of a crude carboxylic acid wet cake stream 310. In one embodiment, after washing the solids with a washing solvent, dehydration is achieved in a filter by passing a gas stream through the solids to displace free liquid. In another embodiment, dehydration of the wet cake in the solid-liquid separation zone 300 can be implemented before and after the solids in the washing zone 300 by any method known in the art to minimize the amount of oxidant solvent present in the wash liquid stream 340. In yet another embodiment, dehydration is achieved by centrifugal force in a porous or solid drum centrifuge. The mother liquor stream 330 generated in the solid-liquid separation zone 300 comprises an oxidation solvent, a catalyst, and impurities. 5 wt % to 95 wt %, 30 wt % to 90 wt %, and most preferably 40 wt % to 80 wt % of the mother liquor present in the crude carboxylic acid slurry stream 110 is separated in the solid-liquid separation zone 300 to generate a mother liquor stream 330, resulting in dissolved materials including impurities present in the mother liquor stream 330 not advancing in the process. In one embodiment, a portion of the mother liquor stream 330 is sent to the mother liquor purification zone 700, wherein the portion is at least 5 wt %, at least 25 wt %, at least 45 wt %, at least 55 wt %, at least 75 wt %, or at least 90 wt %. In another embodiment, at least a portion is sent back to the oxidation zone 100, wherein the portion is at least 5 wt %. In yet another embodiment, at least a portion of the mother liquor stream 330 is sent to the mother liquor purification zone and the oxidation zone 100, wherein the portion is at least 5 wt %. In one embodiment, the mother liquor purification zone 700 includes an evaporation step to separate the oxidation solvent from the stream 330 by evaporation.

[0181] Wash liquor stream 340 is generated in solid-liquid separation zone 300 and comprises a portion of the mother liquor present in stream 210 and a wash solvent, wherein the ratio of the mass of mother liquor to the mass of wash solvent is less than 3 and preferably less than 2. In one embodiment, at least a portion of wash liquor stream 340 is sent to oxidation zone 100, wherein the portion is at least 5 wt%. In one embodiment, at least a portion of wash liquor stream 340 is sent to mother liquor purification zone 700, wherein the portion is at least 5 wt%. In another embodiment, at least a portion of wash liquor stream 340 is sent to oxidation zone 100 and mother liquor purification zone 700, wherein the portion is at least 5 wt%.

[0182] The mother liquor stream 330 comprises an oxidation solvent, a catalyst, soluble intermediates, and soluble impurities. It is desirable to recycle at least a portion of the catalyst and the oxidation solvent present in the mother liquor stream 330 directly or indirectly back to the oxidation zone 100, wherein the portion is at least 5 weight percent, at least 25 weight percent, at least 45 weight percent, at least 65 weight percent, at least 85 weight percent, or at least 95 weight percent. Directly recycling at least a portion of the catalyst and the oxidation solvent present in the mother liquor stream 330 includes sending a portion of the stream 330 directly to the oxidizer zone 100. Indirectly recycling at least a portion of the catalyst and the oxidation solvent present in the mother liquor stream 330 to the oxidation zone 100 includes sending at least a portion of the stream 330 to at least one intermediate zone, wherein the stream 330 is treated to generate one or more streams comprising the oxidation solvent and / or the catalyst, and sent to the oxidation zone 100.

[0183] Step (d) comprises separating components of the mother liquor stream 330 in the mother liquor purification zone 700 for recycling to the process, while also separating those components that are not recycled, including impurities. The impurities in the stream 330 may originate from one or more sources. In one embodiment of the invention, the impurities in the stream 330 include impurities introduced into the process by feeding a stream containing impurities to the oxidation zone 100. The mother liquor impurities include at least one impurity selected from the group consisting of: 2,5-diformylfuran in an amount of about 5 ppm to 800 ppm, 20 ppm to about 1500 ppm, 100 ppm to about 5000 ppm, 150 ppm to about 2.0 wt %; levulinic acid in an amount of about 5 ppm to 800 ppm, 20 ppm to about 1500 ppm, 100 ppm to about 5000 ppm, 150 ppm to about 2.0 wt %; succinic acid in an amount of about 5 ppm to 800 ppm, 20 ppm to about 1500 ppm, 100 ppm to about 5000 ppm, 150 ppm to about 2.0 wt %; acetoxyacetic acid in an amount of about 5 ppm to 800 ppm, 20 ppm to about 1500 ppm, 100 ppm to about 5000 ppm, 150 ppm to about 2.0 wt %.

[0184] Impurities refer to any molecules that are not required for the proper operation of oxidation zone 100. For example, an oxidation solvent, a catalyst system, an oxygen-containing gas, and an oxidizable feedstock, wherein the oxidizable feedstock comprises at least one compound selected from the group consisting of 5-(hydroxymethyl)furfural (5-HMF), 5-(chloromethyl)furfural (5-CMF), 2,5-dimethylfuran (2,5-DMF), 5-HMF esters (5-R(CO)OCH2-furfural, where R = alkyl, cycloalkyl, and aryl), 5-HMF ethers (5-R'OCH2-furfural, where R' = alkyl, cycloalkyl, and aryl), 5-alkylfurfurals (5-R"-furfural, where R" = alkyl, cycloalkyl, and aryl), alkylcarboxylates of methylfuran (5-R"'O(CO)-methylfuran, where R" '=alkyl, cycloalkyl), alkyl carboxylates of alkoxyfurans (5-R""O(CO)-OR""'furans, where R""=alkyl, cycloalkyl and aryl, and R""'=alkyl, cycloalkyl and aryl), a mixed feed of 5-HMF and 5-HMF esters, a mixed feed of 5-HMF and 5-HMF ethers, a mixed feed of 5-HMF and 5-alkylfurans, a mixed feed of 5-HMF and 5-CMF, a mixed feed of 5-HMF and 2,5-DMF, a mixed feed of 5-HMF and alkyl carboxylates of methylfurans, and a mixed feed of 5-HMF and alkyl carboxylates of alkoxyfurans are all molecules required for the proper operation of oxidation zone 100 and are not considered impurities. Likewise, chemical intermediates formed in oxidation zone 100 that lead to or contribute to chemical reactions that produce desired products are not considered impurities. Oxidation byproducts that do not produce desired products are defined as impurities. Impurities may enter the oxidation zone 100 via a recycle stream sent to the oxidation zone 100 or via an impure feed stream fed to the oxidation zone 100 .

[0185] In one embodiment, it is contemplated that a portion of the impurities are separated from the oxidant mother liquor stream 330 and purified or removed from the process as a purge stream 751. In one embodiment of the present invention, 5 to 100 weight percent of the mother liquor stream 330 generated in the solid-liquid separation zone 300 is sent to the mother liquor purge zone 700, where a portion of the impurities present in the stream 330 are separated and leave the process as a purge stream 751. The portion of the stream 330 entering the mother liquor purge zone 700 may be 5 weight percent or greater, 25 weight percent or greater, 45 weight percent or greater, 65 weight percent or greater, 85 weight percent or greater, or 95 weight percent or greater. The recycled oxidation solvent stream 711 comprises the oxidation solvent separated from the stream 330 and may be recycled into the process. The raffinate stream 742 comprises the oxidation catalyst separated from the stream 330, which may optionally be recycled into the process. In one embodiment, raffinate stream 742 is recycled to oxidation zone 100 and contains greater than 30 weight percent, greater than 50 weight percent, greater than 80 weight percent, or greater than 90 weight percent of the catalyst that entered mother liquor cleanup zone 700 in stream 330. In another embodiment, at least a portion of mother liquor stream 330 is sent directly to oxidation zone 100 without first being treated in mother liquor cleanup zone 700. In one embodiment, mother liquor cleanup zone 700 includes an evaporation step to separate the oxidation solvent from stream 330 by evaporation.

[0186] One embodiment of the mother liquor purification zone 700 includes sending at least a portion of the oxidant mother liquor stream 330 to the solvent recovery zone 710 to generate a recycled oxidation solvent stream 711 containing oxidation solvent and an impurity-rich waste stream 712 containing oxidation byproducts and catalyst. Any technology known in the art that can separate volatile solvents from the stream 330 can be used. Examples of suitable unit operations include, but are not limited to, intermittent and continuous evaporation equipment operating above atmospheric pressure, at atmospheric pressure, or under vacuum. Single or multiple evaporation steps can be used. In one embodiment of the present invention, sufficient oxidation solvent is evaporated from the stream 330 to obtain a stream 712, which exists as a slurry having a solid weight percentage of greater than 10%, 20%, 30%, 40%, or 50% by weight. At least a portion of the impurity-rich stream 712 can be sent to the catalyst recovery zone 760 to generate a catalyst-rich stream 761. Examples of unit operations suitable for the catalyst recovery zone 760 include, but are not limited to, incineration or burning of the stream to recover the non-combustible metal catalyst in the stream 761.

[0187] Another embodiment of the mother liquor purification zone 700 includes sending at least a portion of the mother liquor stream 330 to the solvent recovery zone 710 to generate a recycled oxidation solvent stream 711 containing oxidation solvent and an impurity-rich waste stream 712 containing oxidation byproducts and catalyst. Any technology known in the art that can separate volatile solvents from the stream 330 can be used. Examples of suitable unit operations include, but are not limited to, intermittent and continuous evaporation equipment operating above atmospheric pressure, at atmospheric pressure or under vacuum. Single or multiple evaporation steps can be used. Evaporate enough oxidation solvent from the stream 330 to obtain an impurity-rich waste stream 712, which exists as a slurry with a solid weight percentage greater than 5%, 10%, 20% and 30% by weight. At least a portion of the impurity-rich waste stream 712 is sent to the solid-liquid separation zone 720 to generate a purified mother liquor stream 723 and a wet cake stream 722 containing impurities. In another embodiment of the present invention, all streams 712 are sent to the solid-liquid separation zone 720. Stream 722 may be removed from the process as a waste stream. Wash stream 721 may also be sent to solid-liquid separation zone 720, which will result in the presence of wash liquid in stream 723. It should be noted that zone 720 is a separate and distinct zone from zone 300.

[0188] Any technique known in the art capable of separating solids from the slurry may be used. Examples of suitable unit operations include, but are not limited to, intermittent or continuous filters, intermittent or continuous centrifuges, filter presses, vacuum belt filters, vacuum drum filters, continuous pressure drum filters, candle filters, leaf filters, disc centrifuges, sedimentation centrifuges, basket centrifuges, and the like. Continuous pressure drum filters are preferred equipment for solid-liquid separation zone 720.

[0189] The purified mother liquor stream 723 containing catalyst and impurities and the stream 731 containing catalyst solvent are sent to the mixing zone 731 to allow for sufficient mixing to generate the extraction feed stream 732. In one embodiment, the stream 731 contains water. The mixing is allowed to proceed for at least 30 seconds, 5 minutes, 15 minutes, 30 minutes, or 1 hour. Any technology known in the art can be used for the mixing operation, including in-line static mixers, continuous stirred tanks, mixers, high shear in-line mechanical mixers, etc.

[0190] The extraction feed stream 732, the recycled extraction solvent stream 752 and the fresh extraction solvent stream 753 are sent to the liquid-liquid extraction zone 740 to generate an extract stream 741 comprising impurities and an extraction solvent, and a raffinate stream 742 comprising a catalyst solvent and an oxidation catalyst, which can be directly or indirectly recycled to the oxidation zone 100. The liquid-liquid extraction zone 740 can be implemented in a single or multiple extraction units. The extraction unit can be intermittent and or continuous. Examples of equipment suitable for the extraction zone 740 include multiple single-stage extraction units. Another example of equipment suitable for the extraction zone 740 is a single multi-stage liquid-liquid continuous extraction tower. The extract stream 741 is sent to the distillation zone 750, where the extraction solvent is separated by evaporation and condensation to generate a recycled extraction solvent stream 752. A purge stream 751 is also generated and can be removed from the process as a waste purge stream. Intermittent or continuous distillation can be used in the distillation zone 750.

[0191] In another embodiment, the source of the oxidant mother liquor stream 330 fed to the mother liquor purification zone 700 may be derived from any mother liquor stream containing an oxidation solvent, an oxidation catalyst, and impurities generated during the production of furan-2,5-dicarboxylic acid (FDCA). For example, a solvent exchange zone downstream of the oxidation zone 100 that separates at least a portion of the FDCA oxidation solvent from the stream 110 may be the source of the stream 330. Suitable equipment for the solvent exchange zone includes a solid-liquid separation facility, which includes a centrifuge and a filter. Examples of facilities suitable for solvent exchange include, but are not limited to, a disc centrifuge or a continuous pressure drum filter.

[0192] Air oxidation of methyl 5-methylfuran-2-carboxylate (MMFC) of Formula 1 in acetic acid solvent using a Co / Mn / Br catalyst system at 132°C and 130 psig produces a slurry product consisting primarily of 5-(methoxycarbonyl)furan-2-carboxylic acid (MCFC) monomer. The slurry is heated to about 70°C to completely dissolve the solids. After controlled cooling to room temperature, the solids break up and the particle size improves. The filterability of this recrystallized slurry is significantly improved compared to the slurry reaction product that has not undergone this process.

[0193]

[0194] General steps for oxidation:

[0195] In Example 1, glacial acetic acid (125.7 g) and the catalyst components in the amounts described in Table 1A were transferred to a 300 ml titanium autoclave equipped with a high pressure condenser, a throttle plate and an Isco pump. Cobalt, manganese and ionic bromine were respectively prepared as cobalt (II) acetate tetrahydrate, manganese (II) acetate and aqueous hydrobromic acid solution (48.7 wt% in water). The autoclave was pressurized with nitrogen at about 50 psig, and then the homogeneous mixture was heated to the desired temperature under stirring in a closed system (i.e., without gas flow). At the reaction temperature, a gas flow of 1500 sccm was introduced at the bottom of the solution, and the reaction pressure was adjusted to the desired pressure. Liquid MMFC was injected at a rate of 0.20 mL / min by a high pressure Isco pump (reaction time at this time was t=0). 30 seconds after the start of the reactant feed, 1.0 g of peracetic acid (32 wt% in acetic acid) and 5.0 g of acetic acid were added using a blow bottle to start the reaction. The feed was stopped after 1 hour, and the reaction was continued for 1 hour under the same gas flow, temperature and pressure conditions. After the reaction time is over, the gas flow is stopped, the autoclave is cooled to room temperature and depressurized. The multiphase mixture is filtered to separate the white product. The mass of the filtrate is recorded. The white product is washed twice with 60 ml of acetic acid. The washed white product is dried overnight in a vacuum oven at 110°C and then weighed. The solid product, filtrate and acetic acid washings are analyzed by liquid chromatography.

[0196] The exhaust gas was analyzed with ND-1R (ABB, Advanced Optima) for CO and CO2 and O2 by a paramagnetic detection system (Servomex, 1440 Model).

[0197]

[0198] analyze

[0199] Liquid chromatography for sample analysis:

[0200] The samples were analyzed using an Agilent 1260LC device, which contained a four-stage pump, an autosampler (3uL injection volume), a thermostatic column compartment (35°C), and a diode array UV / vis detector (280nm). The chromatograph was equipped with a 150 mm x 4.6 mm Thermo Aquasil C18 column filled with 3 micron particles. The solvent flow rate program is shown in the following table: channel A is 0.1% phosphoric acid in water, channel B is acetonitrile, and channel C is tetrahydrofuran (THF)

[0201]

[0202] EZChrom elite was used to control the HPLC and process the data. A 5-point linear calibration was performed for FFCA, FDCA, MCFC, and MMFC in the (approximate) range of 0.25 to 100 ppm. Solid samples were prepared by dissolving approximately 0.05 g of sample (weighed to 0.0001 g) in 10 mL of 50:50 DMF / THF solution to detect FFCA in the ppm range. For purity analysis, 100 μL of sample was transferred to a 10 mL volumetric flask and diluted to volume with 50:50 DMF / THF. Ultrasonication was used to ensure that the sample was completely dissolved in the solvent. For liquid samples, 0.1 g of sample was weighed and diluted to 10 mL with 50:50 DMF / THF. A small portion of the prepared sample was transferred to an autosampler vial for injection into the LC.

[0203] Colorimetry

[0204] 1) Assemble the engraving machine die as directed in the instruction manual - place the die on the base with the bottom 40mm cylinder polished side facing up.

[0205] 2) Place a 40 mm plastic cup (Chemplex Plasticup, 39.7 x 6.4 mm) into the mold.

[0206] 3) Pour the sample to be analyzed into the cup. The exact amount of sample added is not important.

[0207] 4) Place the top 40 mm cylinder with the polished surface facing down on the sample.

[0208] 5) Insert the piston into the mold. The assembled mold should not appear "tilted".

[0209] 6) Place the mold into the engraving machine, making sure the mold is close to the center of the lower platen. Close the safety door.

[0210] 7) Raise the mold until the upper platen contacts the plunger. Apply >10,000 lbs of pressure. Then hold the mold under pressure for approximately 30 seconds (the exact time is not critical).

[0211] 8) Release the pressure and lower the lower pressure plate that fixes the mold.

[0212] 9) Remove the mold and remove the cup. Place the cup in a labeled plastic bag (Nasco Whirl-Pak 4 oz).

[0213] 10) Using a HunterLab UltraScan Pro colorimeter, create the following method (Hunterlab EasyMatchQC software, version 3.6.2 or higher)

[0214] Mode: RSIN-LAV( R eflectance S pecular In (not included)

[0215] Area View: 0.78 inches

[0216] UV filter position: Nominal

[0217] Measurement

[0218] CIE L*a*b*

[0219] CIE XYZ

[0220] 11) Following the software prompts, standardize the instrument using the light trap accessory and the certified white tile accessory and press it onto the reflection port.

[0221] 12) Run the Green Tile Standard with the Certified White Tile and compare the CIE X, Y, and Z values ​​obtained with the certified values ​​for the tile. The values ​​obtained should be ±0.15 units on each scale of the stated values.

[0222] 13) Press the sample in the bag onto the reflectance port for analysis and obtain the spectrum and L*, a*, b* values. Take duplicate readings and average them for your records.

[0223] As above Figure 1As shown, the particle / crystal size distribution of the dried solid product is 20 microns to 500 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 30 microns to 500 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 40 microns to 500 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 50 microns to 500 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 60 microns to 490 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 70 microns to 480 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 30 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 40 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 50 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 60 microns to 450 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 300 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 350 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 200 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 100 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 90 microns. In another embodiment of the present invention, the particle / crystal size distribution of the dried solid product is 20 microns to 80 microns.

[0224] The cooling rate of the cooling zone can also be controlled. The material stream in the pipeline 110 is cooled to a temperature of 30°C or less at a rate of 0.5°C / min to 10°C / min. The cooling rate of the cooling zone can also be controlled. The material stream in the pipeline 110 is cooled to a temperature of 30°C or less at a rate of 0.4°C / min to 10°C / min. The cooling rate of the cooling zone can also be controlled. The material stream in the pipeline 110 is cooled to a temperature of 30°C or less at a rate of 0.2°C / min to 10°C / min. The material stream in the pipeline 110 is cooled to a temperature of 30°C or less at a rate of 0.1°C / min to 10°C / min, and the cooling rate of the cooling zone can also be controlled. The material stream in the pipeline 110 is cooled to a temperature of 40°C or less at a rate of 0.5°C / min to 10°C / min, and the cooling rate of the cooling zone can also be controlled. The material stream in the pipeline 110 is cooled to a temperature of 0°C or less at a rate of 0.5°C / min to 10°C / min. The cooling rate of the cooling zone can also be controlled. The stream in line 110 is cooled to a temperature of 30° C. or less at a rate of 0.5° C. / min to 10° C. / min.

[0225] Example

[0226] Analytical techniques

[0227] Liquid chromatography for sample analysis

[0228] The samples were analyzed using an Agilent 1260LC device equipped with a quadrupole pump, autosampler (3 μL injection), thermostatic column compartment (35°C), and diode array UV / vis detector (280 nm). The chromatograph was equipped with a 150 mm x 4.6 mm Thermo Aquasil C18 column filled with 3 micron particles. The solvent flow rate program is shown in the table below. Channel A was 0.1% phosphoric acid in water, channel B was acetonitrile, and channel C was tetrahydrofuran (THF).

[0229]

[0230] EZChrom elite was used to control the HPLC and process the data. A 5-point linear calibration was performed over the range of 0.25 to 100 ppm (approximately) for FFCA, FDCA, MCFC, MMFC, and MFFC. Solid samples were prepared by dissolving ~0.05 g (weighed to 0.0001 g) in 10 mL of 50:50 DMF / THF solution to measure the ppm level of FFCA and MFFC. For purity analysis, 100 μL of sample was transferred to a 10 mL volumetric flask and diluted to volume with 50:50 DMF / THF. Ultrasonication was used to ensure that the sample was completely dissolved in the solvent. For liquid samples, 0.1 g of sample was weighed and diluted to 10 mL with 50:50 DMF / THF. A small portion of the prepared sample was transferred to a vial in the autosampler for injection into the LC.

[0231] Colorimetry

[0232] 1) Assemble the engraving machine die as directed in the instruction manual - place the die on the base with the bottom 40mm cylinder polished side facing up.

[0233] 2) Place a 40 mm plastic cup (Chemplex Plasticup, 39.7 x 6.4 mm) into the mold.

[0234] 3) Pour the sample to be analyzed into the cup. The exact amount of sample added is not important.

[0235] 4) Place the top 40 mm cylinder with the polished surface facing down on the sample.

[0236] 5) Insert the piston into the mold. The assembled mold should not appear "tilted".

[0237] 6) Place the mold into the engraving machine, making sure the mold is close to the center of the lower platen. Close the safety door.

[0238] 7) Raise the mold until the upper platen contacts the plunger. Apply >10,000 lbs of pressure. Then hold the mold under pressure for approximately 30 seconds (the exact time is not critical).

[0239] 8) Release the pressure and lower the lower pressure plate that fixes the mold.

[0240] 9) Remove the mold and remove the cup. Place the cup in a labeled plastic bag (Nasco Whirl-Pak 4 oz).

[0241] 10) Using a HunterLab UltraScan Pro colorimeter, create the following method (Hunterlab EasyMatchQC software, version 3.6.2 or higher)

[0242] Mode: RSIN-LAV( R eflectance S pecular In (not included)

[0243] Area View: 0.78 inches

[0244] UV filter position: Nominal

[0245] Measurement

[0246] CIE L*a*b*

[0247] CIE XYZ

[0248] 11) Following the software prompts, standardize the instrument using the light trap accessory and the certified white tile accessory and press it onto the reflection port.

[0249] 12) Run the Green Tile Standard with the Certified White Tile and compare the CIE X, Y, and Z values ​​obtained with the certified values ​​for the tile. The values ​​obtained should be ±0.15 units on each scale of the stated values.

[0250] 13) Press the sample in the bag onto the reflectance port for analysis and obtain the spectrum and L*, a*, b* values. Take duplicate readings and average them for your records.

[0251] Examples

[0252] Air Oxidation of Methyl 5-Methylfuran-2-carboxylate (MMFC)

[0253] The air oxidation reaction of MMFC in acetic acid solvent is carried out according to the following general steps, using a catalyst system containing cobalt, manganese and bromine. The reaction is shown in Formula 1:

[0254]

[0255] General steps

[0256] Glacial acetic acid (125.7 g) and the amounts of catalyst components described in Table 1A were transferred to a 300 ml titanium autoclave equipped with a high pressure condenser, a throttle plate and an Isco pump. Cobalt, manganese and ionic bromine were prepared as cobalt (II) acetate tetrahydrate, manganese (II) acetate and aqueous hydrobromic acid (48.7 wt% in water), respectively.

[0257] The autoclave was pressurized with about 50 psig of nitrogen and the homogeneous mixture was then heated to the desired temperature with stirring in a closed system (ie, no gas flow).

[0258] At the desired reaction temperature, a gas flow of 1500 sccm was introduced at the bottom of the solution, and the reaction pressure was adjusted to the desired pressure. The liquid MMFC was injected at a rate of 0.20 mL / min by a high-pressure Isco pump (reaction time at this time was t=0).

[0259] 30 seconds after the start of the reactant feed, 1.0 g of peracetic acid (32 wt% in acetic acid) and 5.0 g of acetic acid were added using a blow bottle to start the reaction.

[0260] After 1 hour, the feed was stopped and the reaction was continued for 1 hour under the same conditions of gas flow, temperature and pressure.

[0261] After the reaction time was over, the gas flow was stopped and the autoclave was cooled to room temperature and depressurized.

[0262] The multiphase mixture was filtered to separate the white product. The mass of the filtrate was recorded. The white product was washed twice with 60 ml of acetic acid. The washed white product was dried overnight in a vacuum oven at 110°C and then weighed. The solid product, filtrate and acetic acid wash were analyzed by liquid chromatography.

[0263] For CO and CO2, the exhaust gas was analyzed with ND-1R (ABB, Advanced Optima); and O2 was analyzed by a paramagnetic detection system (Servomex, 1440 Model).

[0264] The results are summarized in Table 1. The LC chromatogram of the white solid product of Example 3 is shown in the attached figure.

[0265] Table 1 Results of MMFC semi-batch oxidation under different conditions

[0266]

[0267]

[0268] a = 48.7 wt% in water; b = 97.8wt% purity; c = in solid, in filtrate, in AA washing liquid

[0269] As can be seen in Table 1, the oxidation reaction produces mainly MCFC rather than FDCA. The reaction produces water as a byproduct, but surprisingly, under certain conditions, water has very little effect on the hydrolysis of the methyl ester bond to produce FDCA.

[0270] Also noteworthy in Table 1 is that in one (primary) oxidation step, a high purity product with a FFCA level of only 1.71 ppmw, a MFFC level of only 95.7 ppmw and a b* level of -0.11 can be produced. FFCA and MFFC are known chain terminators in polymerization processes. With such low levels of impurities and pigments, this product can be used directly to make polymers without further purification. Polymer grade monomers can be made without the need for additional purification steps, which has significant economic advantages.

[0271] The invention has been described in detail and with particular reference to specific embodiments thereof, but it will be understood that variations and modifications can be effected within the spirit and scope of the invention.

Claims

1. A method for increasing the crystal size of a compound of formula (I): The method comprises: (a) providing a mixture comprising the compound (I) and a solvent at a temperature of at least 70° C.; and (b) cooling the mixture from step (a) to a temperature of 30° C. or less at a rate of 0.5° C. / min to 10° C. / min; in: The solvent comprises a monocarboxylic acid having 2 to 6 carbon atoms; and R 2 is an alkyl group having 1 to 6 carbon atoms.

2. The method according to claim 1, wherein R 2 is an alkyl group having 1 to 3 carbon atoms.

3. The method according to claim 1, wherein R 2 It is methyl.

4. The method of any one of claims 1-3, wherein the solvent comprises acetic acid.

5. The method according to any one of claims 1 to 4, wherein the cooled mixture from step (b) has a 9 m / kg or less, or 4.3x10 9 m / kg or lower filter cake resistance.

6. The method according to any one of claims 1 to 5, further comprising: (a) filtering the cooled mixture to obtain a wet cake; and (b) drying the wet cake to obtain a dry solid product comprising the compound (I).

7. The process of claim 6, wherein the dried solid product has a particle / crystallite size distribution of 20 microns to 500 microns.

8. The process according to any one of claims 6-7, wherein the dried solid product comprises at least 70 wt% of Compound (I), based on the total weight of the product.

9. The process of any one of claims 6-8, wherein the dried solid product comprises less than 30 wt% furan-2,5-dicarboxylic acid (FDCA), based on the total weight of the product.

10. The process of any one of claims 6-9, wherein the dried solid product comprises less than 500 ppmw 5-formylfuran-2-carboxylic acid (FFCA), based on the total weight of the product.

11. The method of any one of claims 6-10, wherein the b* value of the dried solid product is less than 4.

12. The process according to any one of claims 1 to 11, wherein the mixture of step (a) is obtained by an oxidation reaction.

13. The method according to claim 12, comprising cooling the mixture from the oxidation reaction to a temperature of 30° C. or less; and The cooled mixture is reheated to a temperature of at least 70°C to provide the mixture of step (a).

14. The process of claim 6, wherein the dried solid product is suitable for polymerization without further purification steps.

15. The method according to claims 1-14, wherein said steps (a) and (b) are produced using facilities previously used in industrial processes, such as TPA and / or IPA.

16. A dry solid composition comprising a compound of formula (I): Where R 2 is an alkyl group having 1 to 6 carbon atoms, and wherein the composition has a particle / crystal size distribution of 20 to 500 microns; wherein the dried solid composition has a particle / crystal size distribution of 5 x 10 9 m / kg or less, or 4.3x 10 9 m / kg or less filter cake specific resistance; wherein the particle size is in the range of 20 to 500 microns.

17. The composition of compound (I) according to claim 16, based on the total weight of the composition.

18. The composition of any one of claims 16-17, comprising less than 30 wt. %, based on the total weight of the composition.

19. The composition of any one of claims 16-18 comprising less than 500 ppmw, based on the total weight of the composition.

20. The composition of any one of claims 16-19 having a b* value of less than 4.