Calcite coated microfluidic units and methods thereof
The manufacturing of calcite microfluidic equipment through 3D printing and atomic layer deposition technology has solved the problem of complex and time-consuming manufacturing methods in the prior art, and achieved simple and high-precision calcite microstructure manufacturing, suitable for carbonate reservoir research.
Patent Information
- Application Number
- CN202380034947.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-18
- Filing Date
- 2023-04-18
- Publication Date
- 2024-12-03
AI Technical Summary
The methods used in the prior art for manufacturing calcite microfluidic equipment are complex and time-consuming, and there is a lack of a simple manufacturing method.
3D printing technology is used to manufacture polymer substrates including microfluidic channels, and a calcite layer is deposited through atomic layer deposition technology to form calcite microfluidic equipment.
It provides a simple and high-precision method for manufacturing calcite microstructures, suitable for basic research on carbonate reservoirs, able to simulate pore structures in carbonate reservoirs, and improve research efficiency and accuracy.
Smart Images

Figure CN119072398A_ABST
Abstract
Description
Background Art
[0001] Microfluidic systems, also known as "lab-on-a-chip" devices, can be used to simulate reservoir environments to conduct basic enhanced oil recovery research. For example, the use of microfluidic systems can provide a mode to directly test wettability changes using different fluids to enhance oil recovery. Many conventional materials used in microfluidic devices, such as silicon, are not suitable for studying carbonate reservoir systems. Calcite microfluidics can be used to study reservoir properties; however, calcite microfluidic devices are not common and their fabrication technology is under development.
[0002] Few methods exist for fabricating calcite microfluidic devices, and these methods are often complex and time-consuming to perform. Thus, there exists a need for a facile method for fabricating calcite microfluidic devices. Summary of the invention
[0003] This summary is provided to introduce some concepts that are further described below in the detailed description. This summary is not intended to identify key or essential features of the claimed subject matter, nor is it intended to be used as an aid in limiting the scope of the claimed subject matter.
[0004] In one aspect, embodiments disclosed herein relate to a method comprising 3D printing a polymer substrate comprising microfluidic channels and then depositing calcite onto the polymer substrate using atomic layer deposition to form a calcite microfluidic device.
[0005] In another aspect, embodiments disclosed herein relate to a 3D-printed polymer substrate comprising a microfluidic channel. The 3D-printed polymer substrate has a calcite coating.
[0006] Other aspects and advantages of the claimed subject matter will be apparent from the following description and the appended claims. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 is a schematic diagram of a method for making a calcite microfluidic device according to one or more embodiments.
[0008] Figure 2 is a schematic diagram of a molten filament manufacturing apparatus according to one or more embodiments.
[0009] Figure 3A is a top view of a microfluidic device according to one or more embodiments.
[0010] Figure 3B is a cross-sectional view of a microfluidic device according to one or more embodiments.
[0011] Figure 4 is a cross-sectional view of a microfluidic device according to one or more embodiments. DETAILED DESCRIPTION
[0012] In one aspect, embodiments disclosed herein relate to a method for making a calcite (CaCO 3 ) microfluidic device. Figure 1 As depicted, a schematic diagram of a method 100 according to one or more embodiments includes designing a microfluidic device on a computer 102, printing a polymer substrate 104 including microfluidic channels, and coating calcite on the polymer substrate 106 using atomic layer deposition to form a calcite microfluidic device. Once the microfluidic device is fabricated, glass windows, inlets, and outlets 108 can be added to fabricate a working microfluidic device. The method according to the present invention provides a simple and high-precision method for making calcite microstructures, which is suitable for basic research on carbonate reservoirs.
[0013] As described above, the methods described herein include 3D printing a polymer substrate including a microfluidic channel. As used herein, "3D printing" (also referred to as additive manufacturing) refers to the process of building a three-dimensional (3D) object from 3D model (such as a computer-aided design (CAD) model) data. 3D printing is typically a layer-by-layer process in which a 3D object is built one layer at a time, and each successive layer is added to the previously built layer(s). 3D printing can be performed using any suitable method, and in one or more specific embodiments, a fused filament fabrication (FFF) method can be used.
[0014] Figure 2 A schematic depiction of an FFF 3D printing apparatus 200 is shown. The apparatus includes a substrate 202 on which a 3D printed object 204 can be printed. The substrate 202 is configured to move in a vertical direction (indicated by an arrow) as the 3D printing process proceeds. The material to be printed is in the form of a filament 206, which is fed from a spool 212 through a roller 208 to a nozzle 210 through which the filament is extruded. The roller 208 is mounted on a horizontal platform 214 and can be configured to move in both horizontal and vertical directions, but is at least configured to move in a horizontal direction (indicated by an arrow) to generate a pattern of the 3D printed object 204.
[0015] To 3D print an object using the FFF device 200, a first layer of a polymer material (in the form of a filament 206) is printed directly onto a substrate 202. It is printed by extrusion through a nozzle 210, which is configured to heat the filament for printing. As the filament 206 is extruded through the heated nozzle, a continuous bead of polymer (also referred to as a "road") is deposited onto the substrate 202. The nozzle 210 moves over the substrate in a predetermined geometry to form the first layer of the object 204. Once the first layer is completed, the substrate 202 is lowered away from the nozzle 210, and a second layer of the polymer is deposited on the first layer. This process is repeated to build the object layer by layer until the object 204 is completed.
[0016] As will be appreciated by those skilled in the art, before 3D printing the substrate, a CAD model of the object to be printed having suitable dimensions may be generated. The CAD model may be designed using commercially available software, such as software provided by a commercially available 3D printer. Other readily available software, such as AutoCAD, Fusion360, or TinkerCAD may be used.
[0017] The 3D printer for printing the device according to the present disclosure is not particularly limited and can be any of various commercially available 3D printers known to those skilled in the art. In one or more specific embodiments, the Utilimaker 3D printer available from Dynamism (Chicago, Illinois, USA) can be used. In order to print the device disclosed herein, the printer can have a resolution of up to about 20 microns.
[0018] Any polymer suitable for FFF printing can be used to print the device disclosed herein. For example, the polymer filament can be selected from the group consisting of polylactic acid, acrylonitrile butadiene styrene, polyethyleneterephthalate glycol (also known as polyethylene terephthalate), polyethylene terephtathalate, high impact polystyrene, thermoplastic polyurethane, aliphatic polyamide, and combinations thereof. In a particular embodiment, the polymer filament can be polylactic acid.
[0019] The 3D-printed substrate may have suitable structures with microscale dimensions for creating calcite microfluidic devices. Figure 3A A top view of such a substrate 300 is shown. Figure 3BA cross-sectional view thereof is shown. The substrate 300 includes channels 302 with raised portions 304 between the channels 302. The raised portions 304 are made of the polymer described previously, and the channels 302 are empty spaces. Although the shapes of the channels are shown as circular, they can be any suitable shape, such as square, rectangular, and curved, as long as the shape can be easily 3D printed. Figure 3A and 3B The channels depicted in are also regularly repeated and of similar size. However, the pattern can be varied as desired. Both the shape and size of the pores may be irregular and are limited only by the capabilities of the 3D printer. When constructed at microscale dimensions, this structure forms a substrate or template for microfluidic devices.
[0020] The size of the channel of the polymer substrate can be selected to simulate the pores in the carbonate reservoir. For example, in one or more embodiments, the channel of the polymer substrate can have a width ranging from 10 to 500 microns. The width of the channel can have a lower limit of one of 10, 15, 20, 30, 50, 75, 100, 125, 150, 200 and 250 microns, and an upper limit of one of 100, 125, 150, 175, 200, 250, 300, 350, 400, 450 and 500 microns, wherein any lower limit can be paired with any mathematically compatible upper limit. The height of the channel can be about 75 to 250 microns. For example, the height of the channel may have a lower limit of any one of 75, 80, 90, 100, 110, 125, 150 and 175 microns and an upper limit of any one of 125, 150, 175, 200, 225 and 250, wherein any lower limit can be paired with any mathematically compatible upper limit. The length of the channel can be selected based on the overall size required for the microfluidic device. The channel of one or more embodiments may have a length in the range of 2.0 mm (millimeter) to 5.0 mm. The length of the channel may have a lower limit of one of 2.0, 2.25, 2.5, 2.75, 3.0, 3.25 and 3.5 mm and an upper limit of one of 3.75, 4.0, 4.25, 4.5, 4.75 and 5.0, wherein any lower limit can be paired with any mathematically compatible upper limit. As described above, the size of the channel in the microfluidic device may change.
[0021] After 3D printing the polymer substrate, a layer of calcite can be deposited on the polymer substrate using an atomic layer deposition (ALD) process. Atomic layer deposition is a thin film deposition technique in which a sequence of vapor deposition processes is used to deposit layers of certain materials to build a thin film. ALD is a self-limiting process in which a gas is introduced into a deposition chamber and a monoatomic layer of gaseous material is deposited on the surface to form a monoatomic layer. Once the monolayer is formed, the gas is purged from the deposition chamber and another gas is introduced to form another layer on top of the previous layer. This process is repeated until the final material is formed.
[0022] According to one or more embodiments, a calcite layer having a thickness of 50 to 150 nm (nanometers) may be formed using the following parameters. The temperature during deposition may be between 250 and 325° C., and in particular, may be around 300° C. The gaseous precursors may be 2,2,6,6-tetramethyl-3,5-heptanedione calcium (Ca(thd)2), carbon dioxide (CO2), and ozone (O3). The calcite coating may be made by, for example, flowing a Ca(thd)2 precursor through a polymer substrate to form a calcium layer, purging with nitrogen, flowing an O3 precursor through a polymer substrate to form an oxygen layer, purging with nitrogen, flowing a CO2 precursor through a polymer substrate to form an oxygen layer, purging with nitrogen, and repeating the foregoing steps until a calcite layer is formed. A non-limiting example of a single deposition cycle for forming calcium carbonate may include a 3 second Ca(thd)2 pulse followed by a 2 second nitrogen purge, a 3 second O3 pulse followed by a 2 second nitrogen purge, and a 3 second CO2 pulse followed by a 2 second nitrogen purge. The deposition cycle may be repeated enough times to achieve a thickness of 50 to 150 nm. Specifically, the process may include about 1,000 to about 3,000 cycles.
[0023] Once a suitable calcite coating has been formed, scanning electron microscopy (and in some cases focused ion beam scanning electron microscopy) can be used to confirm the uniformity of the calcite layer.
[0024] The 3D-printed channels with calcite coating can be encapsulated into housings and ultimately used as microfluidic devices. Figure 4 A cross-sectional view of a final microfluidic device 400 according to one or more embodiments is shown. The microfluidic device includes a calcite coated 3D printed channel 402 as described above. The device also includes a top portion including a window 404. The window may be transparent to allow visual inspection of the channel during use. The device has a bottom portion 406 for housing the device. The bottom portion 406 may be any type of housing to provide stability to the device and allow the window 404 and fluid connections 408, 410 to connect properly. Figure 4 As shown, the device includes an inlet 408 configured to allow fluid to enter the device and an outlet 410 configured to allow fluid to leave the device. The inlet 408 can be connected to a pump configured to introduce fluid at a specific pressure and flow rate. The outlet 410 can be connected to a waste collection system to collect waste fluid after use. Figure 4 The inlet and outlet are shown on opposite sides of the device. However, their positions are not particularly limited. They can be located on any side of the device.
[0025] The device disclosed herein can be used to study the fluid dynamics in calcite microchannels, which are configured to simulate the pores in carbonate reservoirs. Carbonate reservoirs are usually treated with acid to increase pore connectivity and ultimately improve the oil recovery rate in the reservoir. Acid achieves this effect by dissolving carbonate rocks. The device disclosed herein can be used to visually observe the dissolution dynamics of various acid-treated mixtures to sedimentary calcite, thereby providing information about fluid flow dynamics. These observations can be used to quantify the acid dissolution of carbonate rocks and predict the migration of brine through aquifers (such as calcite formations). Such observations can be performed according to any technology known in the art. In particular, an optical microscope equipped with a CCD camera can be used to observe the dissolution dynamics.
[0026] Although only a few example embodiments have been described in detail above, those skilled in the art will readily appreciate that many modifications may be made to the example embodiments without materially departing from the present invention. Therefore, all such modifications are intended to be included within the scope of the present disclosure as defined by the appended claims. In the claims, means-plus-function clauses are intended to cover structures described herein as performing the recited functions, and not only structural equivalents, but also equivalent structures. Thus, while nails and screws may not be structural equivalents because nails employ cylindrical surfaces to secure wooden parts together, while screws employ helical surfaces, nails and screws may be equivalent structures in the context of fastening wooden parts. It is the applicant's express intent not to invoke 35 U.S.C. §112(f) for any limitation of any claim herein unless the claim expressly uses the term "means for..." and the associated function.
Claims
1. A method comprising: 3D printing a polymer substrate, the polymer substrate comprising a microfluidic channel; as well as Using atomic layer deposition, calcite was deposited onto the polymer substrate to form a calcite microfluidic device.
2. The method of claim 1, wherein the 3D printing is performed using fused filament fabrication.
3. The method of claim 2, wherein the molten filament manufacturing comprises: feeding a polymer filament through a heated nozzle to deposit a first layer of the polymer onto a substrate; depositing a second layer of the polymer onto the first layer; as well as The above steps are repeated until the polymer substrate is formed.
4. The method of claim 3, wherein the polymer filaments are selected from the group consisting of polylactic acid, acrylonitrile butadiene styrene, polyethylene terephthalate, polyethylene terephthalate, high impact polystyrene, thermoplastic polyurethane, aliphatic polyamide, and combinations thereof.
5. The method according to any one of the preceding claims, wherein the polymer of the polymer substrate is polylactic acid.
6. A method according to any one of the preceding claims, wherein the microfluidic channel has a width in the range of 10 to 500 microns.
7. A method according to any one of the preceding claims, wherein the microfluidic channel has a length in the range of 2 mm to 5 mm.
8. A method according to any one of the preceding claims, wherein the calcite has a thickness of 50 to 150 nm.
9. The method of any one of the preceding claims, wherein using the atomic layer deposition comprises: flowing a Ca(thd)2 precursor through the polymer substrate to form a calcium layer; Purging with nitrogen; flowing an O3 precursor through the polymer substrate to form an oxygen layer; Purging with nitrogen; flowing a CO2 precursor through the polymer substrate to form a carbon layer; Purging with nitrogen; and Repeat the above steps until a calcite layer is formed.
10. The method according to any one of the preceding claims, further comprising: The calcite microfluidic device is enclosed in a housing, wherein the housing comprises a top portion comprising a window, a bottom portion configured to receive the device, an inlet portion configured to allow fluid to enter the device, and an outlet portion configured to allow the fluid to exit the device.
11. A device comprising: A 3D-printed polymer substrate comprising a microfluidic channel, wherein the 3D-printed polymer substrate comprises a calcite coating.
12. The apparatus of claim 11, wherein the polymer substrate is selected from the group consisting of polylactic acid, acrylonitrile butadiene styrene, polyethylene terephthalate, polyethylene terephthalate, high impact polystyrene, thermoplastic polyurethane, aliphatic polyamide, and combinations thereof.
13. The device of claim 11 or 12, wherein the microfluidic channel has a width in the range of 10 to 500 microns.
14. The device according to any one of claims 11 to 13, wherein the microfluidic channel has a length in the range of 2 mm to 5 mm.
15. The device according to any one of claims 11 to 14, wherein the thickness of the calcite coating is 50 to 150 nm.